Scanning antenna and method for manufacturing the same

By incorporating an organic rigid layer with higher hardness than the adhesive layer and an inorganic insulating film, the scanning antenna addresses the issue of conductive particle penetration, enhancing reliability and stability.

JP2024141649AInactive Publication Date: 2024-10-10TOPPAN HOLDINGS INC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023053417
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-29
Publication Date
2024-10-10
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The issue with existing scanning antennas is that the conductive particles in the anisotropic conductive film can break through the thin inorganic oxide electrode wiring, leading to insufficient electrical contact due to the soft adhesive layer.

Method used

The solution involves using a base material with an adhesive layer, a first metal wiring, an organic rigid layer with higher hardness than the adhesive layer, and an inorganic oxide wiring, all covered by an inorganic insulating film, to prevent penetration and ensure stable electrical connections.

Benefits of technology

This configuration prevents the inorganic oxide electrode from being penetrated, enhances alignment of phase shifters, reduces manufacturing costs, and improves reliability by minimizing cracks and peeling, thus ensuring stable electrical connections.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024141649000001_ABST
    Figure 2024141649000001_ABST
Patent Text Reader

Abstract

To provide a scanning antenna which does not break through an electrode (wiring) made of an inorganic oxide and does not cause disturbance in the orientation of liquid crystal in a phase shifter, even when the phase shifter is connected via an anisotropic conductive film.SOLUTION: A scanning antenna 1 includes a substrate 10, an adhesive layer 20 provided on the substrate 10, a first wiring 30 provided on a portion of the adhesive layer 20, an organic rigid layer 40 provided on another portion of the adhesive layer 20, a second wiring 50 provided across a portion of the first wiring 30 and a portion of the organic rigid layer 40, and an inorganic insulating film 60 provided across the first wiring 30, the second wiring 50 and the organic rigid layer 40, and the hardness of the organic rigid layer is greater than the hardness of the adhesive layer.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a scanning antenna and a method for manufacturing a scanning antenna. [Background technology]

[0002] 2. Description of the Related Art A phased array antenna having antenna units is known as an antenna (scanning antenna) having a function of changing the radiation direction of a beam.

[0003] Phased array antennas require phase shifters. In order to make phased array antennas possible to manufacture at low cost, phase shifters using liquid crystal are becoming practical.

[0004] Patent Document 1 describes a scanning antenna that utilizes liquid crystal display technology and includes a low-resistance metal electrode (wiring) and a high-resistance inorganic oxide electrode (wiring). The low-resistance metal electrode (wiring) is surrounded by a relatively soft adhesive layer, and the high-resistance inorganic oxide electrode (wiring) is provided across a part of the metal electrode (wiring) and a part of the adhesive layer, and the phase shifter is physically and electrically connected to the high-resistance inorganic oxide electrode (wiring) arranged on the adhesive layer via an anisotropic conductive film. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] International Publication No. 2020 / 121876 Summary of the Invention [Problem to be solved by the invention]

[0006] The inorganic oxide electrodes (wiring) are formed by a vapor phase film forming method such as sputtering, and are thin, about 10 nm to 100 nm, and the adhesive layer is soft, with a pencil hardness of about HB to 2H.

[0007] On the other hand, the anisotropic conductive film contains conductive particles, and when this anisotropic conductive film is pressed against an inorganic oxide electrode (wiring) on ​​an adhesive layer to bond it, the adhesive layer is soft, so the conductive particles in the anisotropic conductive film may break through the inorganic oxide electrode (wiring) and sink into the adhesive layer. When the conductive particles in the anisotropic conductive film sink into the adhesive layer in this way, the electrical contact between the conductive particles and the inorganic oxide electrode (wiring) becomes insufficient.

[0008] Therefore, an object of the present invention is to provide a scanning antenna that does not break through electrodes (wiring) made of inorganic oxide even when a phase shifter is connected via an anisotropic conductive film. [Means for solving the problem]

[0009] A first aspect of the present invention is a scanning antenna comprising: a substrate; an adhesive layer provided on the substrate; a first metallic wiring provided on a portion of the adhesive layer; an organic rigid layer provided on another portion of the adhesive layer; a second wiring made of an inorganic oxide provided across a portion of the first wiring and a portion of the organic rigid layer; and an inorganic insulating film provided across the first wiring, the second wiring, and the organic rigid layer, wherein the hardness of the organic rigid layer is greater than the hardness of the adhesive layer.

[0010] A second aspect of the present invention is a substrate, an adhesive layer provided on the substrate, and a coating layer provided on the adhesive layer. the scanning antenna comprising: an organic rigid layer disposed between the adhesive layer and the first wiring; a first wiring made of a metal disposed on a portion of the organic rigid layer; a second wiring made of an inorganic oxide disposed across the organic rigid layer and the first wiring; and an inorganic insulating film disposed across the first wiring, the second wiring, and the organic rigid layer, wherein the hardness of the organic rigid layer is greater than the hardness of the adhesive layer.

[0011] A third aspect of the present invention is a method for manufacturing a scanning antenna.

[0012] This manufacturing method includes a first step of bonding a metal foil onto a base material via an adhesive layer, a second step of patterning the metal foil to form a first wiring on a part of the adhesive layer, a third step of forming a pre-organic rigid layer on the adhesive layer and the first wiring, a fourth step of patterning the pre-organic rigid layer to form an organic rigid layer on the adhesive layer, a fifth step of forming an inorganic oxide layer on the first wiring and the organic rigid layer, a sixth step of patterning the inorganic oxide layer to form a second wiring, and a seventh step of forming an inorganic insulating film provided across the first wiring, the second wiring, and the organic rigid layer, wherein the organic rigid layer has a hardness greater than that of the adhesive layer.

[0013] A fourth aspect of the present invention is a method for manufacturing a scanning antenna.

[0014] This manufacturing method includes a first step of forming an organic rigid layer on a metal foil, a second step of forming an adhesive layer on the organic rigid layer, a third step of bonding the metal foil onto a base material via the adhesive layer and the organic rigid layer, a fourth step of patterning the metal foil to form a first wiring on a part of the organic rigid layer, a fifth step of forming an inorganic oxide layer on the organic rigid layer and the first wiring, a sixth step of patterning the inorganic oxide layer to form a second wiring, and a seventh step of forming an inorganic insulating film provided across the first wiring, the second wiring, and the organic rigid layer, wherein the organic rigid layer has a hardness greater than that of the adhesive layer. Effect of the Invention

[0015] According to the present invention, it is possible to provide a scanning antenna that does not break through electrodes (wiring) made of inorganic oxide even when a phase shifter is connected via an anisotropic conductive film, and a method for manufacturing the scanning antenna. [Brief description of the drawings]

[0016] [Figure 1] 1 is a cross-sectional view showing a scanning antenna according to a first embodiment of the present invention. [Diagram 2]5 is a flowchart showing a method for manufacturing the scanning antenna according to the first embodiment of the present invention. [Diagram 3] 2A to 2C are diagrams illustrating different steps in the manufacture of a scanning antenna according to a first embodiment of the present invention. [Figure 4] FIG. 6 is a cross-sectional view showing a scanning antenna according to a second embodiment of the present invention. [Diagram 5] 10 is a flowchart showing a method for manufacturing a scanning antenna according to a second embodiment of the present invention. [Figure 6] 5A-5C are diagrams illustrating different stages in the manufacture of a scanning antenna according to a second embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0017] First Embodiment A first embodiment of the present invention will be described with reference to FIGS.

[0018] 1 is a cross-sectional view showing a scanning antenna 1 according to the present embodiment. The scanning antenna 1 includes a base material 10, an adhesive layer 20 provided on the base material 10, a first wiring 30 provided on a portion of the adhesive layer 20, an organic rigid layer 40 provided on another portion of the adhesive layer 20, and a second wiring 30 on the first wiring 30. a second wiring 50 provided across a portion of the first wiring 30 and a portion of the organic rigid layer 40; and an inorganic insulating film 60 provided across the first wiring 30, the second wiring 50 and the organic rigid layer 40.

[0019] In this specification, each part of the scanning antenna 1 and the manufacturing method will be described with the direction in which the adhesive layer 20 is provided on the base material 10 being the upper side. However, the position of the scanning antenna 1 in this specification is merely an example, and the position of the scanning antenna 1 during use and the position during manufacturing are not limited to the position shown in this specification.

[0020] The substrate 10 is made of an insulating material. A typical material for the substrate 10 is glass, but flexibility can be imparted to the substrate 10 by using various plastic films. In this embodiment, the material for the substrate 10 is glass.

[0021] The adhesive layer 20 is provided on the substrate 10. The adhesive layer 20 is a layer formed from a known adhesive. This adhesive layer 20 is generally relatively soft and has a pencil hardness of HB to 2H. In order to bond the adhesive layer 20 to the first wiring 30, it is necessary to use an adhesive layer 20 that is relatively soft, and it is difficult to use an adhesive layer 20 with high hardness.

[0022] In this embodiment, the thickness of the adhesive layer 20 is about 5 μm, and the maximum height roughness Rz is 0.5 μm.

[0023] The first wiring 30 is provided on a part of the adhesive layer 20. The first wiring 30 is formed in a predetermined pattern shape. The first wiring 30 is attached to the base material 10 via the adhesive layer 20. In the scanning antenna 1, the first wiring 30 plays a role of a low resistance wiring.

[0024] The first wiring 30 is made of a metal. In this embodiment, the first wiring 30 is made of copper. The first wiring 30 may be made of a metal with a low resistivity, such as silver or aluminum.

[0025] From the viewpoint of reducing resistance, it is desirable for the first wiring 30 to be a thick film, and the thickness of the first wiring 30 can be, for example, about 1 μm to 30 μm. In this embodiment, the thickness of the first wiring 30 is 2 μm.

[0026] The organic rigid layer 40 is provided on a portion of the adhesive layer 20 where the first wiring 30 is not provided. The organic rigid layer 40 is formed in a predetermined pattern shape.

[0027] The organic rigid layer 40 has a role of receiving the conductive particles contained in the anisotropic conductive film and preventing the conductive particles from breaking through the second wiring 50 and embedding in the adhesive layer when the anisotropic conductive film is pressed against the second wiring 50 arranged thereon to physically and electrically connect the two. Therefore, it is desirable that the hardness of the organic rigid layer 40 is greater than that of the adhesive layer 20. As described above, the pencil hardness of the adhesive layer 20 is generally about HB to 2H, so it is desirable that the organic rigid layer 40 has a pencil hardness of 4H to 7H.

[0028] Such an organic rigid layer 40 can be formed of a thermosetting resin or a photocurable resin, such as cardo, polyimide, polyamic acid, epoxy, siloxane, urethane, etc. In this embodiment, the main component of the organic rigid layer 40 is a photocurable acrylic resin after curing.

[0029] The thickness of the organic rigid layer 40 is desirably 1 to 5 μm from the viewpoint of reducing the load applied to the inorganic insulating film 60 due to the thermal expansion, thermal contraction, and thermal flow of the adhesive layer 20. In this embodiment, the thickness of the organic rigid layer 40 is approximately 3 μm.

[0030] In this embodiment, it is desirable that the surface of the organic rigid layer 40 is smoother than the surface of the adhesive layer 20. If the surface of the organic rigid layer 40 is smoother than the surface of the adhesive layer 20, the alignment disorder of the liquid crystal in the phase shifter can be improved. In this embodiment, since the maximum height roughness Rz of the adhesive layer 20 is 0.5 μm, it is desirable that the maximum height roughness Rz of the organic rigid layer 40 is 0.1 μm or less. In this embodiment, the maximum height roughness Rz of the organic rigid layer 40 is 0.03 μm.

[0031] In order to reduce the load applied to the inorganic insulating film 60 due to the thermal expansion and contraction of the organic rigid layer 40, it is preferable that the linear expansion coefficient of the organic rigid layer 40 is smaller than that of the inorganic insulating film 60. In this embodiment, the linear expansion coefficient of the organic rigid layer 40 is 3.5×10 -6 / K or less.

[0032] The second wiring 50 is provided across a part of the first wiring 30 and a part of the organic rigid layer 40. This connects the first wiring 30 and the second wiring 50. The second wiring 50 is formed in a predetermined pattern shape. In the scanning antenna 1, the second wiring 50 plays the role of a high resistance wiring.

[0033] The second wiring 50 is made of an inorganic oxide. In this embodiment, the second wiring 50 is made of indium tin oxide (ITO) which has a high resistivity. The second wiring 50 may be made of an inorganic oxide having a high resistivity, such as indium zinc oxide (IZO).

[0034] From the viewpoint of increasing resistance, the second wiring 50 is desirably a thin film, and the thickness of the second wiring 50 can be, for example, about 10 nm to 100 nm. In this embodiment, the thickness of the second wiring 50 is 60 nm.

[0035] The inorganic insulating film 60 is provided across the first wiring 30, the second wiring 50 and the organic rigid layer 40.

[0036] In this embodiment, the inorganic insulating film 60 is made of SiNx. The inorganic insulating film 60 has high gas barrier properties and insulating properties. In the scanning antenna 1, the inorganic insulating film 60 plays the role of a barrier layer that suppresses the oxidation of the first wiring 30 and the oxidative decomposition of the adhesive layer 20. In addition, in the scanning antenna 1, the inorganic insulating film 60 plays the role of an insulating layer that insulates the first wiring 30 and the second wiring 50. Since the inorganic insulating film 60 made of SiNx is fragile and has low bending resistance, it is necessary to suppress the load applied to the inorganic insulating film 60 in order to suppress the occurrence of cracks in the inorganic insulating film 60. The inorganic insulating film 60 may be made of a material having high gas barrier properties and insulating properties, such as SiO2, SiON, and SiOF.

[0037] In this embodiment, the linear expansion coefficient of the inorganic insulating film 60 is 3.5×10 -6 / K. As described above, the linear expansion coefficient of the organic rigid layer 40 is 3.5×10 -6 / K or less. In other words, the linear expansion coefficient of the organic rigid layer 40 is smaller than the linear expansion coefficient of the inorganic insulating film 60.

[0038] An example of a method for manufacturing the scanning antenna 1 of this embodiment having the above-mentioned configuration will be described.

[0039] As shown in FIG. 2, the manufacturing method of the scanning antenna 1 of this embodiment includes a first sub-step S111, a first step S11, a second step S12, a third step S13, a fourth step S14, a fifth step S15, a sixth step S16, and a seventh step S17.

[0040] The first sub-step S111 is a step of applying a liquid adhesive to the entire surface 130a of the metal foil 130 facing one side shown in FIG. 3(a) to form an adhesive layer 20. It is formed on a surface 130a facing one side of the substrate 130 by roll coating.

[0041] In this embodiment, the metal foil 130 is a copper foil formed in a sheet shape. The metal foil 130 can be formed by sputtering or electrolytic plating. In this embodiment, the metal foil 130 is formed by electrolytic plating and has a thickness of 2 μm.

[0042] The first step S11 is a step of bonding the metal foil 130 onto the substrate 10 via the adhesive layer 20. In the first step S11, the adhesive layer 20 formed on the entire surface 130a of the metal foil 130 facing one side is first brought into contact with the substrate 10. Next, the adhesive layer 20 is dried while the metal foil 130 and the substrate 10 are pressed together with a predetermined pressure. This allows the metal foil 130 and the substrate 10 to be bonded together via the adhesive layer 20.

[0043] As described above, in this embodiment, in the sub-first step S111, the adhesive layer 20 is formed on the entire surface 130a facing one side of the metal foil 130, and then in the first step S11, the metal foil 130 and the base material 10 are bonded together, but the procedure for bonding the metal foil 130 and the base material 10 is not limited to this. For example, in the sub-first step, an adhesive may be applied to the entire surface 10b facing the other side of the base material 10 to form the adhesive layer 20, and in the first step, the metal foil 130 may be brought into contact with the adhesive layer 20, and then the above-mentioned pressure bonding and drying may be performed to bond the metal foil 130 and the base material 10 together. In this case, the adhesive layer 20 is formed on the surface 10b facing the other side of the base material 10 by a coating method such as a die coating method or a slit & spin coating method.

[0044] The second step S12 is a step of patterning the metal foil 130 to form the first wiring 30 on a part of the adhesive layer 20. The patterning of the metal foil 130 is performed by photolithography.

[0045] In the second step S12, first, a photoresist layer is formed on the metal foil 130. In this embodiment, a novolac resin, which is a positive photoresist, is used as the photoresist. The photoresist is applied onto the metal foil 130 by a general spin coater, and a photoresist layer is formed.

[0046] Next, the photoresist layer is prebaked. In this embodiment, the photoresist layer is prebaked in a chamber under reduced pressure to dry it. This can shorten the drying time of the photoresist layer. The pressure in the chamber is 130 Pa. The baking temperature is 120° C. The baking time is 2 minutes.

[0047] Next, the photoresist layer was exposed to ultraviolet light through a photomask on which a pattern shape corresponding to the first wiring 30 was drawn. The exposure amount was set to 35 mJ.

[0048] Next, the photoresist layer after exposure is developed. A positive developer was used as the developer. A spray development method was used as the development method. The developer pressure was 0.1 MPa. The developer temperature was 25° C. The development time was 25 seconds.

[0049] Next, the metal foil 130 is etched to remove the portions of the metal foil 130 from which the photoresist layer has been removed, and the metal foil 130 is patterned into a pattern shape corresponding to the first wiring 30. The etching solution was a mixed aqueous solution of hydrogen peroxide, sulfuric acid, and water. The concentration of the hydrogen peroxide was about 2% to 20%. The concentration of the sulfuric acid was about 2% to 20%. The liquid temperature of the etching solution was 40° C. The etching time was about 2 minutes.

[0050] Next, the photoresist layer remaining on the first wiring 30 is stripped off. The temperature of the film-stripping solution was 40° C. The film-stripping time was 180 seconds.

[0051] Next, the first wiring 30 is post-baked. In this embodiment, the post-baking is performed in a chamber with a nitrogen atmosphere. The baking temperature is 250° C. The baking time is 90 minutes. When the post-baking of the first wiring 30 is completed, the second step S12 is completed, and the first wiring 30 having a predetermined pattern shape is formed on a part of the adhesive layer 20, as shown in FIG. 3(b).

[0052] The third step S13 is a step of forming a pre-organic rigid layer 140 on the adhesive layer 20 and the first wiring 30. The pre-organic rigid layer 140 is formed on the adhesive layer 20 and the first wiring 30 by a liquid application forming technique using a general coater such as spin coater or bar coater. In this embodiment, the main component of the liquid to be applied is a photocurable acrylic resin.

[0053] 3(b), a pre-organic rigid layer 140 is formed on the adhesive layer 20 and the first wiring 30. In this embodiment, the pre-organic rigid layer 140 has a thickness of about 3 μm.

[0054] The fourth step S14 is a step of patterning the pre-organic rigid layer 140 to form the organic rigid layer 40 on the adhesive layer 20. The pre-organic rigid layer 140 is patterned by photolithography. The pre-organic rigid layer 140 may also be patterned by laser drawing.

[0055] In the fourth step S14, first, the pre-organic rigid layer 140 is irradiated with ultraviolet light through a photomask on which a pattern shape corresponding to the organic rigid layer 40 is drawn, thereby exposing the pre-organic rigid layer 140. The exposure amount was set to 600 mJ.

[0056] Next, the pre-organic rigid layer 140 is developed to remove the uncured portion of the pre-organic rigid layer 140 that is not exposed to the ultraviolet light, i.e., the portion of the pre-organic rigid layer 140 located above the first wiring 30. A negative developer was used as the developer. The development time was 60 seconds.

[0057] Next, the organic rigid layer 40 is post-baked. In this embodiment, the post-baking is performed in a chamber with a nitrogen atmosphere. The baking temperature is 230° C. The baking time is 30 minutes. When the post-baking of the organic rigid layer 40 is completed, the fourth step S14 is completed, and the organic rigid layer 40 having a predetermined pattern shape is formed on the adhesive layer 20, as shown in FIG. 3(c).

[0058] The fifth step S15 is a step of forming an inorganic oxide layer 150 on the first wiring 30 and the organic rigid layer 40. The inorganic oxide layer 150 is formed by stacking indium tin oxide (ITO) on the first wiring 30 and the organic rigid layer 40 by sputtering. The power value of the sputtering was 5.6 kW. The conveying speed of the substrate 10 was 495 nm / sec. When the fifth step S15 is completed, as shown in FIG. 3(d), the inorganic oxide layer 150 is formed on the first wiring 30 and the organic rigid layer 40. In this embodiment, the thickness of the inorganic oxide layer 150 is 60 nm.

[0059] The sixth step S16 is a step of patterning the inorganic oxide layer 150 to form the second wiring 50. The inorganic oxide layer 150 is patterned by photolithography.

[0060] In the sixth step S16, first, a photoresist layer is formed on the inorganic oxide layer 150. In this embodiment, a novolac resin, which is a positive photoresist, is used as the photoresist. Ta.

[0061] Next, the photoresist layer is prebaked. In this embodiment, the prebaking is performed in a chamber under reduced pressure. The pressure in the chamber is 130 Pa. The baking temperature is 120° C. The baking time is 2 minutes.

[0062] Next, the photoresist layer is exposed to ultraviolet light through a photomask on which a pattern shape corresponding to the second wiring 50 is drawn. In this embodiment, the exposure amount is set to 70 mJ.

[0063] Next, the photoresist layer after exposure is developed. A positive developer was used as the developer. A spray development method was used as the development method. The developer pressure was 0.15 MPa. The developer temperature was 25° C. The development time was 100 seconds.

[0064] Next, the inorganic oxide layer 150 is etched to remove the portion of the inorganic oxide layer 150 from which the photoresist layer has been removed, and the inorganic oxide layer 150 is patterned into a pattern shape corresponding to the second wiring 50. The etching liquid was an aqueous solution of oxalic acid. The liquid temperature of the etching liquid was 40° C. The etching time was 60 seconds.

[0065] Next, the photoresist layer remaining on the second wiring 50 is stripped off. A silicate solution was used as the stripping liquid. The temperature of the stripping liquid was 40° C. The stripping time was 180 seconds. When the stripping of the photoresist layer is completed, the sixth step S16 is completed, and the second wiring 50 having a predetermined pattern shape is formed as shown in FIG. 3(e). The second wiring 50 is formed across the first wiring 30 and the organic rigid layer 40. As a result, the first wiring 30 and the second wiring 50 are connected to each other. In the portion where the inorganic oxide layer 150 has been removed, the first wiring 30 or the organic rigid layer 40 is exposed.

[0066] The seventh step S17 is a step of forming an inorganic insulating film 60 extending over the first wiring 30, the second wiring 50, and the organic rigid layer 40. The inorganic insulating film 60 is provided by forming a SiNx film on the first wiring 30, the second wiring 50, and the organic rigid layer 40 by a film forming method such as a chemical vapor deposition method. When the seventh step S17 is completed, the inorganic insulating film 60 extending over the first wiring 30, the second wiring 50, and the organic rigid layer 40 is provided as shown in FIG. 1. As described above, the inorganic insulating film 60 has high gas barrier properties and insulating properties, and therefore the inorganic insulating film 60 can suppress oxidation of the first wiring 30 and oxidative decomposition of the adhesive layer 20.

[0067] In the above-mentioned seventh step S17, the base material 10, the adhesive layer 20, the first wiring 30, the organic rigid layer 40, and the second wiring 50 are each heated by heat generated when the inorganic insulating film 60 is formed. Therefore, a load is applied to the organic rigid layer 40 provided directly on the adhesive layer 20, particularly due to thermal expansion, thermal contraction, and thermal flow of the adhesive layer 20.

[0068] Through the above steps, the scanning antenna 1 of this embodiment is completed.

[0069] According to this embodiment, the scanning antenna 1 includes a base material 10, an adhesive layer 20 provided on the base material 10, a first wiring 30 made of metal provided on a portion of the adhesive layer 20, an organic rigid layer 40 provided on another portion of the adhesive layer 20, a second wiring 50 made of inorganic oxide provided across a portion of the first wiring 30 and a portion of the organic rigid layer 40, and an inorganic insulating film 60 provided across the first wiring 30, the second wiring 50, and the organic rigid layer 40, and further, the hardness of the organic rigid layer 40 is greater than the hardness of the adhesive layer 20. Therefore, even when a phase shifter is connected via an anisotropic conductive film, it is possible to prevent the electrode (wiring) made of inorganic oxide from being broken through.

[0070] In the present embodiment, the inorganic insulating film 60 is made of any one of materials SiNx, SiO2, SiON, and SiOF. Therefore, a part of the inorganic insulating film 60 contacts the adhesive layer 20 via the organic rigid layer 40, so that the load caused by the thermal expansion, thermal contraction, and thermal flow of the adhesive layer 20 due to the heat generated when forming the inorganic insulating film 60 is indirectly applied to the inorganic insulating film 60 from the adhesive layer 20 via the organic rigid layer 40. This reduces the load applied to the inorganic insulating film 60, so that the occurrence of cracks in the inorganic insulating film 60 made of a brittle material such as SiNx and having low bending resistance can be suppressed, and the barrier properties of the inorganic insulating film 60 can be suppressed from decreasing. Therefore, the oxidation of the first wiring 30 and the oxidative decomposition of the adhesive layer 20 can be suppressed, so that the deterioration of the electrical properties of the first wiring 30 and the deterioration of the weather resistance of the adhesive layer 20 can be suppressed, and the reliability of the scanning antenna 1 can be improved.

[0071] Furthermore, in this embodiment, as described above, the surface shape of the organic rigid layer 40 is smoother than the surface shape of the adhesive layer 20. Therefore, compared to the case where the second wiring 50 is provided directly on the adhesive layer 20, the occurrence of cracks, breaks, and the like in the second wiring 50 can be suppressed. Therefore, the reliability of the scanning antenna 1 can be further improved.

[0072] In this embodiment, the first wiring 30 is bonded to the substrate 10 via the adhesive layer 20. The internal stress of the first wiring 30 formed in a thick film is large, and the adhesive force between the first wiring 30 made of metal and the substrate 10 is small. Therefore, when the first wiring 30 is directly provided on the substrate 10, the first wiring 30 is likely to float and peel off from the substrate 10. However, in this embodiment, the first wiring 30 is bonded to the substrate 10 via the adhesive layer 20 made of an adhesive that has high adhesiveness to both the first wiring 30 and the substrate 10, so that the first wiring 30 is prevented from floating and peeling off from the substrate 10. Therefore, the reliability of the scanning antenna 1 can be further improved.

[0073] In this embodiment, the second wiring 50 is provided across a part of the first wiring 30 and a part of the organic rigid layer 40. If the organic rigid layer 40 is not provided and the second wiring 50 is provided across the first wiring 30 and the adhesive layer 20, the part of the second wiring 50 that contacts the boundary between the side wall of the first wiring 30 and the adhesive layer 20 is likely to break. However, in this embodiment, since the side wall of the first wiring 30 is covered with the organic rigid layer 40, it is possible to prevent the second wiring 50 from contacting the boundary between the side wall of the first wiring 30 and the adhesive layer 20, and it is possible to suppress the second wiring 50 from breaking. Therefore, the reliability of the scanning antenna 1 can be further improved.

[0074] According to the present embodiment, the linear expansion coefficient of the organic rigid layer 40 is smaller than the linear expansion coefficient of the inorganic insulating film 60. This reduces the load applied to the inorganic insulating film 60 due to the thermal expansion and contraction of the organic rigid layer 40. This more effectively prevents cracks from occurring in the inorganic insulating film 60, thereby further improving the reliability of the scanning antenna 1.

[0075] According to this embodiment, the manufacturing method of the scanning antenna 1 includes a first step S11 of bonding the metal foil 130 onto the base material 10 via the adhesive layer 20, a second step S12 of patterning the metal foil 130 to form the first wiring 30 on a part of the adhesive layer 20, a third step S13 of forming a pre-organic rigid layer 140 on the adhesive layer 20 and the first wiring 30, a fourth step S14 of patterning the pre-organic rigid layer 140 to form an organic rigid layer 40 on the adhesive layer 20, a fifth step S15 of forming an inorganic oxide layer 150 on the first wiring 30 and the organic rigid layer 40, a sixth step S16 of patterning the inorganic oxide layer 150 to form the second wiring 50, and a seventh step S17 of forming an inorganic insulating film 60 that is provided across the first wiring 30, the second wiring 50, and the organic rigid layer 40 and is made of any one of SiNx, SiO2, SiON, and SiOF. Generally, when a thick-film wiring pattern is formed by plating, the adhesion between the substrate and the wiring pattern is not sufficient. As a method for increasing the adhesion between the substrate and the thick-film wiring pattern, there is a method for forming a thick-film wiring pattern using a conductive paste, but this method requires firing the conductive paste under an inert gas atmosphere, which increases the manufacturing cost. However, in this embodiment, in the first step S11, the metal foil 130 is bonded to the substrate 10 via the adhesive layer 20, and then in the second step S12, the metal foil 130 is patterned to form the first wiring 30. Therefore, the manufacturing cost of the thick-film first wiring 30 can be prevented from increasing.

[0076] Generally, when forming a first wiring made of metal by plating, if the first wiring has a complex shape, the current density is likely to be biased, and the first wiring is likely to have a large unevenness in thickness, which may cause the operation of the scanning antenna 1 to become unstable. However, in this embodiment, as described above, since the shape of the metal foil 130 is a sheet shape, which is a simple shape, the unevenness in thickness of the metal foil 130 formed by plating can be reduced. Also, in this embodiment, in the first step S11, the metal foil 130 is bonded to the base material 10 via the adhesive layer 20, and then in the second step S12, the metal foil 130 is patterned to form the first wiring 30. Therefore, the unevenness in thickness of the first wiring 30 can be reduced, and the reliability of the scanning antenna 1 can be improved.

[0077] Generally, when a metal foil is provided on a substrate by plating, there is a risk of the substrate cracking or chipping when the substrate is immersed in a plating tank or transported. However, in the present embodiment, in the first step S11, the metal foil 130 is bonded to the substrate 10 via the adhesive layer 20, so that the substrate 10 is prevented from cracking or chipping. Therefore, the manufacturing steps and manufacturing costs of the scanning antenna 1 can be prevented from increasing. Also, the reliability of the scanning antenna 1 can be improved.

[0078] Generally, the adhesiveness between the glass substrate 10 and the copper first wiring 30 is low, so when the first wiring is provided on the substrate by plating, the first wiring is likely to float and peel off from the substrate. However, in the present embodiment, in the first step S11, the first wiring 30 is bonded to the substrate 10 via the adhesive layer 20, so that the first wiring 30 can be prevented from floating and peeling off from the substrate 10. Therefore, the reliability of the scanning antenna 1 can be improved.

[0079] <Second embodiment> A second embodiment of the present invention will be described with reference to Figures 4 to 6. In the following description, the same components as those in the first embodiment described above are denoted by the same reference numerals, and the description thereof may be omitted.

[0080] 4 is a cross-sectional view showing a scanning antenna 201 according to this embodiment. The scanning antenna 201 includes a base material 10, an adhesive layer 20 provided on the base material 10, an organic rigid layer 240 provided on the adhesive layer 20, a first wiring 30 provided on a part of the organic rigid layer 240, a second wiring 50 provided across the organic rigid layer 240 and the first wiring 30, and an inorganic insulating film 260 provided across the first wiring 30, the second wiring 50, and the organic rigid layer 240.

[0081] The aspect of the substrate 10 of this embodiment is the same as that of the substrate 10 of the first embodiment.

[0082] The aspect of the adhesive layer 20 of this embodiment is the same as the aspect of the adhesive layer 20 of the first embodiment.

[0083] The organic rigid layer 240 is provided entirely on the adhesive layer 20. Other aspects of the organic rigid layer 240 are the same as those of the organic rigid layer 240 in the first embodiment.

[0084] The first wiring 30 is provided on a part of the organic rigid layer 240. Other aspects of the first wiring 30 are the same as those of the first wiring 30 of the first embodiment.

[0085] The aspect of the second wiring 50 of this embodiment is the same as the aspect of the second wiring 50 of the first embodiment.

[0086] The inorganic insulating film 260 is provided across the first wiring 30, the second wiring 50, and the organic rigid layer 240. Other aspects of the inorganic insulating film 260 are the same as other aspects of the inorganic insulating film 60 of the first embodiment. The inorganic insulating film 260 may be made of a material having high gas barrier properties and insulating properties, such as SiO2, SiON, or SiOF.

[0087] An example of a method for manufacturing the scanning antenna 201 of this embodiment having the above-mentioned configuration will be described.

[0088] As shown in FIG. 5, the manufacturing method of the scanning antenna 201 of this embodiment includes a first step S21, a second step S22, a third step S23, a fourth step S24, a fifth step S25, a sixth step S26, and a seventh step S27.

[0089] The first step S21 is a step of forming an organic rigid layer 240 on the surface 130a facing one side of the metal foil 130 shown in Fig. 6(a). The organic rigid layer 240 is formed on the surface 130a facing one side of the metal foil 130 by a liquid coating formation technique using a general coater such as spin coater or bar coater. When the first step S21 is completed, the organic rigid layer 240 is formed on the surface 130a facing one side of the metal foil 130.

[0090] The second step S22 is a step of applying a liquid adhesive onto the organic rigid layer 240 to form the adhesive layer 20. The adhesive layer 20 is formed on the organic rigid layer 240 by using a roll coating method. When the second step S22 is completed, the adhesive layer 20 is formed on the organic rigid layer 240, as shown in FIG. 6(a).

[0091] The third step S23 is a step of bonding the metal foil 130 onto the substrate 10 via the adhesive layer 20 and the organic rigid layer 240. In the third step S23, first, the organic rigid layer 240 and the substrate 10 are brought into contact with each other. Next, the metal foil 130 and the substrate 10 are bonded together at a predetermined pressure while the adhesive layer 20 is dried, thereby bonding the metal foil 130 and the substrate 10 together. When the third step S23 is completed, the metal foil 130 is bonded onto the substrate 10 via the adhesive layer 20 and the organic rigid layer 240, as shown in FIG. 6(a).

[0092] The fourth step S24 is a step of patterning the metal foil 130 to form the first wiring 30 on a part of the organic rigid layer 240. The patterning of the metal foil 130 is performed by photolithography. The work content of the fourth step S24 is the same as the work content of the second step S12 in the first embodiment. When the fourth step S24 is completed, the first wiring 30 having a predetermined pattern shape is formed on a part of the organic rigid layer 240, as shown in FIG. 6(b).

[0093] The fifth step S25 is a step of forming an inorganic oxide layer 150 on the organic rigid layer 240 and the first wiring 30. The inorganic oxide layer 150 is formed by stacking indium tin oxide (ITO) on the first wiring 30 and the organic rigid layer 240 by sputtering. The work content of the fifth step S25 is similar to the work content of the fifth step S15 in the first embodiment. When the fifth step S25 is completed, the inorganic oxide layer 150 is formed on the organic rigid layer 240 and the first wiring 30, as shown in FIG. 6(b).

[0094] The sixth step S26 is a step of patterning the inorganic oxide layer 150 to form the second wiring 50. The inorganic oxide layer 150 is patterned by photolithography. , is performed. The work content of the sixth step S26 is the same as the work content of the sixth step S16 in the first embodiment. When the sixth step S26 is completed, the second wiring 50 having a predetermined pattern shape is formed as shown in FIG. 6(c). The second wiring 50 is formed across the organic rigid layer 240 and the first wiring 30. As a result, the first wiring 30 and the second wiring 50 are connected to each other. Furthermore, the first wiring 30 or the organic rigid layer 240 is exposed in the portion where the inorganic oxide layer 150 has been removed.

[0095] The seventh step S27 is a step of forming an inorganic insulating film 260 extending over the first wiring 30, the second wiring 50, and the organic rigid layer 240. The inorganic insulating film 260 is provided by forming a SiNx film on the first wiring 30, the second wiring 50, and the organic rigid layer 240 by a film forming method such as chemical vapor deposition. The work content of the seventh step S27 is similar to the work content of the seventh step S17 of the first embodiment. When the seventh step S27 is completed, as shown in FIG. 4, the inorganic insulating film 260 extending over the first wiring 30, the second wiring 50, and the organic rigid layer 240 is provided. As described above, the inorganic insulating film 260 has high gas barrier properties and insulating properties, so that the inorganic insulating film 260 can suppress oxidation of the first wiring 30 and oxidative decomposition of the adhesive layer 20.

[0096] With the above steps, the scanning antenna 201 of this embodiment is completed.

[0097] According to this embodiment, the scanning antenna 1 includes a base material 10, an adhesive layer 20 provided on the base material 10, a first wiring 30 made of metal provided on a portion of the adhesive layer 20, an organic rigid layer 40 provided on another portion of the adhesive layer 20, a second wiring 50 made of inorganic oxide provided across a portion of the first wiring 30 and a portion of the organic rigid layer 40, and an inorganic insulating film 60 provided across the first wiring 30, the second wiring 50, and the organic rigid layer 40, and the hardness of the organic rigid layer 40 is greater than the hardness of the adhesive layer 20. Therefore, even when a phase shifter is connected via an anisotropic conductive film, the inorganic oxide electrode (wiring) is not broken, and it is possible to prevent the liquid crystal of the phase shifter from being disoriented.

[0098] In the present embodiment, the inorganic insulating film 60 is made of any one of materials SiNx, SiO2, SiON, and SiOF. Therefore, since the inorganic insulating film 260 contacts the adhesive layer 20 via the organic rigid layer 240, the load caused by the thermal expansion, thermal contraction, and thermal flow of the adhesive layer 20 due to the heat generated when forming the inorganic insulating film 260 is indirectly applied to the inorganic insulating film 260 from the adhesive layer 20 via the organic rigid layer 240. This reduces the load applied to the inorganic insulating film 260, so that it is possible to suppress the occurrence of cracks in the inorganic insulating film 260 made of a brittle material such as SiNx and having low bending resistance, and it is possible to suppress the deterioration of the barrier properties of the inorganic insulating film 260. Therefore, it is possible to suppress the oxidation of the first wiring 30 and the oxidative decomposition of the adhesive layer 20, so that it is possible to suppress the deterioration of the electrical properties of the first wiring 30 and the deterioration of the weather resistance of the adhesive layer 20, and it is possible to improve the reliability of the scanning antenna 201.

[0099] According to this embodiment, the manufacturing method of the scanning antenna 201 includes a first step S21 of forming an organic rigid layer 240 on the metal foil 130, a second step S22 of forming an adhesive layer 20 on the organic rigid layer 240, a third step S23 of bonding the metal foil 130 onto the base material 10 via the adhesive layer 20 and the organic rigid layer 240, a fourth step S24 of patterning the metal foil 130 to form a first wiring 30 on a part of the organic rigid layer 240, a fifth step S25 of forming an inorganic oxide layer 150 on the organic rigid layer 240 and the first wiring 30, a sixth step S26 of patterning the inorganic oxide layer 150 to form a second wiring 50, and a seventh step S27 of forming an inorganic insulating film 260 that is provided across the first wiring 30, the second wiring 50, and the organic rigid layer 240 and is made of any one of SiNx, SiO2, SiON, and SiOF. Therefore, compared to the manufacturing method of the scanning antenna 1 of the first embodiment, there is no need for a step of patterning the organic rigid layer 240 to form the organic rigid layer 240 into a predetermined pattern shape. As a result, the manufacturing process of the scanning antenna 201 can be simplified, and the reliability of the scanning antenna 201 can be improved.

[0100] Although the embodiment of the present invention has been described above, the specific configuration is not limited to this embodiment, and configuration changes and combinations within the scope of the gist of the present invention are also included. Some examples of changes are shown below, but these are not all inclusive, and other changes are also possible. These changes can be freely combined.

[0101] In the method for manufacturing a scanning antenna of the present invention, the order of the steps may be changed. For example, the metal layer may be patterned before bonding the metal foil coated with the adhesive layer to the substrate.

[0102] The cross-sectional shape of the first wiring is not limited to a substantially rectangular shape, and may be a tapered shape that gradually shrinks with increasing distance from the adhesive layer. In this case, the normal to the side surface of the first wiring faces upward, so that the inorganic oxide layer can be stably formed on the side surface of the first wiring by sputtering. Therefore, the film thickness of the second wiring can be made uniform on the first wiring, and the reliability of the scanning antenna can be improved. [Explanation of symbols]

[0103] 1,201 Scanning Antennas 10 Base material 20 Adhesive layer 30 1st wiring 40,240 Organic Rigid Layer 50 2nd wiring 60,260 Inorganic insulating film 130 Metal foil 140 Pre-Organic Rigid Layer 150 Inorganic oxide layer S11,S21 1st process S12,S22 2nd process S13,S23 3rd process S14,S24 4th process S15,S25 5th process S16,S26 6th process S17,S27 7th process

Claims

1. A substrate; An adhesive layer provided on the substrate; a first wiring made of metal and provided on a portion of the adhesive layer; an organic rigid layer provided on another portion of the adhesive layer; a second wiring made of an inorganic oxide provided across a portion of the first wiring and a portion of the organic rigid layer; an inorganic insulating film provided across the first wiring, the second wiring, and the organic rigid layer; Equipped with A scanning antenna, wherein the hardness of the rigid organic layer is greater than the hardness of the adhesive layer.

2. A substrate; An adhesive layer provided on the substrate; an organic rigid layer provided on the adhesive layer; a first wiring made of metal and provided on a part of the organic rigid layer; a second wiring made of an inorganic oxide provided across the organic rigid layer and the first wiring; an inorganic insulating film provided across the first wiring, the second wiring, and the organic rigid layer; Equipped with A scanning antenna, wherein the hardness of the rigid organic layer is greater than the hardness of the adhesive layer.

3. The scanning antenna of claim 1 or 2, wherein the organic rigid layer has a pencil hardness of 4H to 7H.

4. 3. The scanning antenna of claim 1 or 2, wherein the adhesive layer has a pencil hardness of HB to 2H.

5. 3. A scanning antenna as claimed in claim 1 or 2, wherein said rigid organic layer is made of a thermosetting resin or a photosetting resin.

6. 3. The scanning antenna according to claim 1, wherein the organic rigid layer has a thickness of 1 to 5 μm.

7. 3. A scanning antenna according to claim 1, wherein the organic rigid layer has a maximum height roughness Rz of 0.1 μm or less.

8. A first step of bonding a metal foil onto a substrate via an adhesive layer; A second step of patterning the metal foil to form a first wiring on a part of the adhesive layer; a third step of forming a pre-organic rigid layer on the adhesive layer and the first wiring; A fourth step of patterning the pre-organic rigid layer to form an organic rigid layer on the adhesive layer; a fifth step of forming an inorganic oxide layer on the first wiring and on the organic rigid layer; A sixth step of patterning the inorganic oxide layer to form a second wiring; a seventh step of forming an inorganic insulating film provided across the first wiring, the second wiring, and the organic rigid layer; having A method for manufacturing a scanning antenna, comprising the step of: forming the organic rigid layer with a hardness greater than that of the adhesive layer;

9. A first step of forming an organic rigid layer on a metal foil; A second step of forming an adhesive layer on the organic rigid layer; A third step of bonding a metal foil onto the substrate via an adhesive layer and an organic rigid layer; a fourth step of patterning the metal foil to form a first wiring on a portion of the organic rigid layer; a fifth step of forming an inorganic oxide layer on the organic rigid layer and on the first wiring; A sixth step of patterning the inorganic oxide layer to form a second wiring; a seventh step of forming an inorganic insulating film provided across the first wiring, the second wiring, and the organic rigid layer; having A method for manufacturing a scanning antenna, comprising the step of: forming the organic rigid layer with a hardness greater than that of the adhesive layer;

Citation Information

Patent Citations

  • Scanning antenna and method for manufacturing scanning antenna

    WO2020121876A1