Inner surface smoothing structure and inner surface smoothing method for corrugated steel pipe

The use of flexible inner sheets on corrugated steel pipes addresses issues of temperature sensitivity and high construction costs by providing a smooth inner surface that maintains flow rates and reduces assembly time and material waste.

JP2024141702APending Publication Date: 2024-10-10NIPPON STEEL METAL PROD CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023053492
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-29
Publication Date
2024-10-10

AI Technical Summary

Technical Problem

Existing corrugated steel pipes coated with bituminous materials face issues such as softening in hot weather, peeling due to gravity, cracking in cold weather, increased weight, and high construction costs due to on-site assembly and bolted connections, which affect construction efficiency and increase manufacturing costs.

Method used

A smooth inner surface structure for corrugated steel pipes using flexible sheets made of rubber, resin, or cloth that are attached via hooks or ring springs, eliminating the need for on-site bolted connections and reducing roughness coefficient.

Benefits of technology

The solution reduces construction costs, improves construction efficiency, and ensures consistent performance across temperature variations, while maintaining high flow rates and reducing material waste.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024141702000001_ABST
    Figure 2024141702000001_ABST
Patent Text Reader

Abstract

To provide an inner surface smoothing structure and an inner surface smoothing method for a corrugated steel pipe capable of securing a flow rate by reducing a roughness coefficient of an inner surface, having good construction efficiency and capable of shortening a construction period.SOLUTION: In an inner surface smoothing structure 1 for a corrugated steel pipe that reduces a roughness coefficient by smoothing an inner surface of the corrugated steel pipe 2 having a corrugation shape, an inner surface smoothing sheet 3 comprising a rubber sheet or a resin sheet having flexibility is attached to the inner surface of the corrugated steel pipe 2. The inner surface smoothing sheet 3 is a material that is not softened or hardened at 5°C-35°C of a room temperature.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an inner surface smoothing structure and an inner surface smoothing method for a corrugated steel pipe in which a corrugated steel sheet is corrugated and formed into a circular or U-shaped cross section. [Background technology]

[0002] In corrugated pipes used as drainage pipes, a method is used in which, in order to increase the flow rate inside the pipe, a paving material made of bituminous material is attached to the corrugated inner surface of the pipe to reduce the roughness coefficient.

[0003] For example, Patent Document 1 describes an asphalt-coated corrugated steel plate 1 for waterways, in which the inner surface of a curved corrugated steel plate 2 is coated with an asphalt mixture 3 so as to form a smooth inner surface. The asphalt mixture 3 is an asphalt mixture material that contains substantially no aggregate but is 75±2% by weight of blown asphalt and the remainder is a filler, and the asphalt mixture is mixed with the asphalt mixture and is then applied to the asphalt mixture. 3 An asphalt-coated corrugated steel sheet 1 using an asphalt mixture 3 mixed with 2 to 6 kg of short fibers per sheet is disclosed (see claim 1 in the claims of Patent Document 1, paragraphs

[0022] to

[0032] of the specification, and Figures 1 and 3 of the drawings, etc.).

[0004] However, the paving material used in the asphalt-coated corrugated steel plate described in Patent Document 1 is bituminous, and is therefore often affected by temperature, and there is a problem that it softens during the hot summer months, causing dents where it interferes with other members. In addition, when such an asphalt-coated corrugated steel plate is inverted, there is a problem that the corrugated steel plate and the paving material may peel off due to gravity. Furthermore, there is a problem that the paving material may crack due to impact during the cold winter months, and therefore care must be taken when storing it on site and handling it during construction.

[0005] In addition, the asphalt-coated corrugated steel plate described in Patent Document 1 aims to make the inner surface smooth, but the weight is significantly increased because a block of bitumen is attached, which increases the load of on-site assembly work. In addition, since the bolted joints that join the corrugated steel plates together cannot be pre-attached with paving material, it is necessary to fill the grooves in the bolted joints with a field repair material called a joint material after assembly. Furthermore, melted asphalt is used to bond the paving material and the corrugated steel (steel material), but in order to firmly bond the two together, the entire surface of the corrugated steel needs to be lined with asphalt in advance, which is very time-consuming.

[0006] In order to solve such problems, Patent Document 2 discloses an inner-coated corrugated steel pipe in which an auxiliary metal fitting 3 is attached to the inner surface of a corrugated steel pipe formed into a circular or U-shaped cross section by combining corrugated steel pipe materials 2a and 2b, and then an abrasion-resistant paving sheet 1 is attached and covered, the paving sheet being made by impregnating a sheet-like glass fiber with a thermoplastic resin and cutting the sheet to substantially the same shape as the corrugated steel pipe material (see claims 1 and 2 in the claims of Patent Document 2, paragraphs

[0011] to

[0027] in the specification, Figure 3 in the drawings, etc.).

[0007] Patent Document 3 discloses a method for covering the inner surface of a corrugated steel pipe, in which a wear-resistant paving sheet 1 made of a fiber-reinforced thermoplastic resin composite cut to approximately the same shape as the corrugated steel pipe material is attached by fastening means 3 to cover a lower 1 / 4 to 1 / 2 circumference of the inner surface of a corrugated steel pipe formed into a circular cross section by combining corrugated steel pipe materials 2a, 2b (see claim 1 in the claims of Patent Document 3, paragraphs

[0010] to

[0027] of the specification, Figures 1 to 6 of the drawings, etc.).

[0008] Furthermore, Patent Document 4 discloses a corrugated pipe for drainage comprising a corrugated pipe body 1 and a planar member 2 provided within the corrugated pipe body 1, the planar member 2 being provided along the inner wall surface of the corrugated pipe body 1 and being divided into multiple pieces in the axial direction of the corrugated pipe body 1 (see claim 1 in the claims of Patent Document 4, paragraphs

[0015] to

[0019] of the specification, Figures 1 to 5 of the drawings, etc.).

[0009] The paving sheets described in Patent Documents 2 and 3 and the flat material described in Patent Document 4 can reduce the roughness coefficient of the inner surface of the corrugated steel pipe. However, the paving sheets described in Patent Documents 2 and 3 and the flat material described in Patent Document 4 are plate-shaped and therefore need to be fastened to the corrugated steel pipe with bolts, which is a problem in that it takes time and effort to fasten all of these bolts on-site, increasing construction costs. In addition, the increase in the number of bolt fastening points naturally increases the processing costs of the bolt holes and the material costs of the bolts themselves. [Prior art documents] [Patent documents]

[0010] [Patent Document 1] JP 2009-275353 A [Patent Document 2] Japanese Patent Application Publication No. 7-158775 [Patent Document 3] Japanese Patent Application Publication No. 8-270840 [Patent Document 4] Japanese Patent Application Publication No. 7-252818 Summary of the Invention [Problem to be solved by the invention]

[0011] Therefore, the present invention has been devised in consideration of the above-mentioned problems, and an object of the present invention is to provide an inner surface smoothing structure and an inner surface smoothing method for a corrugated steel pipe which can reduce the roughness coefficient of the inner surface to ensure flow rate, improve construction efficiency, and shorten the construction period. [Means for solving the problem]

[0012] The first aspect of the present invention relates to an inner surface smooth structure of a corrugated steel pipe, which smoothes the inner surface of a corrugated corrugated steel pipe to reduce the roughness coefficient, and is characterized in that an inner surface smooth sheet made of a flexible rubber sheet, resin sheet, or cloth sheet is attached to the inner surface of the corrugated steel pipe.

[0013] The smooth inner surface structure of a corrugated steel pipe according to a second aspect of the present invention is characterized in that in the first aspect, the smooth inner surface sheet is made of a material that does not soften or harden at room temperatures of 5°C to 35°C.

[0014] The third invention relates to an inner surface smooth structure of a corrugated steel pipe, which is characterized in that, in the first or second invention, a slit or mounting hole is formed in either the inner surface of the corrugated steel pipe or the inner surface smooth sheet, and a mounting hook is formed in the other, and the hook is hung in the slit or mounting hole, thereby fixing the inner surface smooth sheet to the inner surface of the corrugated steel pipe.

[0015] The fourth invention relates to an inner surface smooth structure of a corrugated steel pipe according to the first or second invention, characterized in that the inner surface smooth sheet is tubular, and the tubular inner surface smooth sheet is pressed against the corrugated steel pipe from the inside by a ring spring, thereby fixing the inner surface smooth sheet to the inner surface of the corrugated steel pipe.

[0016] The fifth aspect of the present invention relates to a method for smoothing the inner surface of a corrugated steel pipe, which smoothes the inner surface of a corrugated corrugated steel pipe to reduce the roughness coefficient, and is characterized in that it includes an inner surface smoothing sheet attachment step of attaching an inner surface smoothing sheet made of a flexible rubber sheet or resin sheet to the inner surface of the corrugated steel pipe.

[0017] The sixth invention relates to a method for smoothing an inner surface of a corrugated steel pipe, and is characterized in that in the inner surface smoothing sheet mounting step, a mounting hook formed on either the inner surface of the corrugated steel pipe or the inner surface smooth sheet is hooked onto a slit or mounting hole formed on the other one of the inner surface of the corrugated steel pipe to mount the inner surface smooth sheet to the inner surface of the corrugated steel pipe.

[0018] The seventh invention relates to a method for smoothing an inner surface of a corrugated steel pipe, which is characterized in that in the inner surface smoothing sheet mounting step, the inner surface smoothing sheet is tubular, and the tubular inner surface smoothing sheet is pressed and fixed against the corrugated steel pipe from the inside with a ring spring to mount the inner surface smoothing sheet on the inner surface of the corrugated steel pipe. Effect of the Invention

[0019] According to the first to seventh inventions, the roughness coefficient of the inner surface of the corrugated steel pipe can be reduced by the inner surface smoothing sheet, thereby ensuring the flow rate of the drainage pipe made of the corrugated steel pipe. Also, according to the first to seventh inventions, compared to the conventional method of attaching a paving material made of bituminous material to the inner surface of the corrugated steel pipe, construction and manufacturing costs can be reduced because a lining material is not required.

[0020] Moreover, according to the first to seventh inventions, compared to conventional paving materials made of bituminous materials, it is easier to remove the inner smooth sheet from the corrugated steel pipe, making it possible to recover costs through waste disposal and steel scrap. Furthermore, according to the first to seventh inventions, compared to conventional paving materials made of bituminous materials, it is not necessary to adhere the paving material to the corrugated steel pipe, and normal hot-dip galvanized steel sheets can be used for the corrugated steel pipe, making inventory management easier and reducing the manufacturing cost of the corrugated steel pipe.

[0021] In particular, according to the second invention, since the inner smooth sheet is made of a material that does not soften or harden at room temperature, it is possible to suppress the occurrence of defects caused by temperature, such as softening in the hot summer months and hardening in the winter months, causing the sheet to crack when subjected to impact.

[0022] In particular, according to the third, fourth, sixth and seventh inventions, compared with the conventional method of bolting a vaporizing material or a steel plate to a corrugated steel pipe, the on-site installation work of the inner surface smoothing sheet can be easily performed in a short time. Therefore, the construction efficiency of the installation work of the drainage pipe made of the corrugated steel pipe is improved, and the construction period can be shortened. [Brief description of the drawings]

[0023] [Figure 1] FIG. 1 is a perspective view showing an inner smooth structure of a corrugated steel pipe according to a first embodiment of the present invention. [Diagram 2] FIG. 2 is a perspective view showing the corrugated steel pipe having a smooth inner surface structure of the corrugated steel pipe of the same embodiment. [Diagram 3] FIG. 3 is a perspective view showing an inner smooth sheet of the inner smooth structure of the corrugated steel pipe. [Figure 4] FIG. 4 is an enlarged view of part A in FIG. 1, mainly showing the joint between the corrugated steel pipe having the smooth inner structure and the smooth inner sheet. [Diagram 5] FIG. 5 is a perspective view showing an inner smooth structure of a corrugated steel pipe according to a second embodiment of the present invention. [Figure 6] FIG. 6 is a vertical cross-sectional view taken along the pipe axis, showing the smooth structure of the inner surface of the corrugated steel pipe. [Figure 7] FIG. 7(a) is a schematic diagram showing an overview of the corrugated steel pipe having an inner smooth structure of the above-mentioned corrugated steel pipe, and FIG. 7(b) is a schematic diagram showing another example of the corrugated steel pipe having an inner smooth structure of the above-mentioned corrugated steel pipe. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0024] Hereinafter, an inner surface smooth structure of a corrugated steel pipe according to an embodiment of the present invention will be described in detail with reference to the drawings.

[0025] <Smooth inner surface structure of corrugated steel pipe> [First embodiment] First, an explanation will be given of an inner surface smooth structure 1 of a corrugated steel pipe according to a first embodiment of the present invention with reference to Fig. 1 to Fig. 4. Fig. 1 is a perspective view showing an inner surface smooth structure 1 of a corrugated steel pipe according to this embodiment. Fig. 2 is a perspective view showing a corrugated steel pipe having the inner surface smooth structure 1 of a corrugated steel pipe, and Fig. 3 is a perspective view showing an inner surface smooth sheet of the inner surface smooth structure 1 of a corrugated steel pipe. And Fig. 4 is an enlarged view of part A in Fig. 1 mainly showing a joint between the corrugated steel pipe and the inner surface smooth sheet.

[0026] As shown in FIG. 1, the inner surface smoothing structure 1 of the corrugated steel pipe according to this embodiment is composed of a corrugated steel pipe 2 formed into a corrugated shape from a thin steel plate, and an inner surface smoothing sheet 3 attached to the inner surface of this corrugated steel pipe 2.

[0027] (Corrugated steel pipe) The corrugated steel pipe 2 is a corrugated steel pipe made by bending a corrugated steel plate formed from a 1.6 mm to 7.0 mm thick thin steel plate such as hot-rolled mild steel plate SPHC (steel plate hot commercial) or general structural rolled steel material SS400 into a U-shape or a half-cylindrical shape, as shown in Figures 1 and 2. Of course, the corrugated steel pipe 2 is not limited to a half-cylindrical shape, and may be appropriately bent into a predetermined shape such as an ellipse or a cylinder.

[0028] In addition, because the corrugated steel pipe 2 does not have a paving material made of bituminous material bonded to it, it can be treated with normal hot-dip zinc plating as an anti-rust treatment. This makes it possible to ensure durability at low cost. In addition, it is no longer necessary to distinguish and manage special corrugated steel pipes that are not hot-dip zinc plating from normal corrugated steel pipes that are hot-dip zinc plating, making inventory management easier and reducing the manufacturing cost of the corrugated steel pipes.

[0029] As shown in Fig. 2, this corrugated steel pipe 2 is composed of a U-shaped flume body 20 having a generally U-shaped cross section, and a flange 21 that protrudes outward along the upper edge of this U-shaped flume body 20. Further, a long hole 22 for bolt connection is drilled in the peak portion, which is the corrugated upper portion of the flange 21.

[0030] 2, a hanging plate 23 made of a strip-shaped steel plate for hanging an inner smooth sheet 3 (described later) is joined by welding or the like along the flange 21 of the corrugated steel pipe 2. The hanging plate 23 is a slit plate having slits 24 formed therein, which are cuts for hanging button hooks 31 (described later).

[0031] (Smooth inner surface sheet) The inner surface smooth sheet 3 is mainly composed of a sheet body 30 made of a lightweight rubber sheet having a thickness of about 1 to 2 mm. However, the inner surface smooth sheet according to the present invention is not particularly limited as long as it is a sheet-like material such as a resin sheet or a cloth sheet that has a predetermined rigidity and flexibility and can reduce the roughness coefficient of the inner surface of the corrugated steel sheet.

[0032] This is because, unlike hardened plate-like materials such as the steel plate and FRP sheet described in the background art, a sheet-like material having a predetermined rigidity and flexibility does not need to be fixed at many points with bolts or the like, and can reduce the roughness coefficient of the inner surface of the corrugated steel plate by being swept away by the flow of fluid flowing through the corrugated steel pipe 2. However, using a rubber sheet as the inner surface smooth sheet 3 is preferable because it has a predetermined rigidity due to rubber elasticity and does not follow the corrugated shape of the corrugated steel plate, and therefore the degree to which the roughness coefficient can be reduced is large.

[0033] Furthermore, it is preferable that the inner surface smooth sheet 3 is made of a material that does not soften or harden at room temperature. This is because it is possible to prevent problems caused by temperature, such as softening in the hot summer months and hardening in the winter months, leading to cracking due to impact. Note that room temperature here is assumed to be 20°C, as in the Japanese Industrial Standards, and refers to a range of 20°C ±15°C, i.e., a range of 5°C to 35°C.

[0034] In addition, as shown in Fig. 3, a number of button hooks 31, which are mounting hooks, are attached along the edge of the sheet body 30. Therefore, as shown in Fig. 4, simply by hooking the button hooks 31 into the slits 24 of the above-mentioned hanging plate 23, the inner surface smooth sheet 3 can be fixed to the inner surface of the corrugated steel pipe 2 easily and in a short time, compared to the case of bolting a steel plate or FRP sheet as described in the background art.

[0035] 1 illustrates an example in which substantially the entire inner surface of the U-shaped flume body 20 is covered with the inner surface smooth sheet 3, but it is also possible to cover only the lower part of the U-shaped flume body 20 depending on the designed water volume of the drain pipe, etc. This is because when the amount of water flowing through the drain pipe is small, only the lower part is sufficient.

[0036] Also, although the example has been given of a case in which the hanging plate 23 with slits 24 is attached to the inner surface of the corrugated steel pipe 2, and the button hook 31 serving as a mounting hook is provided on the inner surface smooth sheet 3, these may be reversed. That is, the slit or mounting hole may be provided on the inner surface smooth sheet 3 side, and the button hook 31 serving as a mounting hook may be provided on the inner surface of the corrugated steel pipe 2. In short, it is sufficient that the slit 31 or mounting hole is formed on either the inner surface of the corrugated steel pipe 2 or the inner surface smooth sheet 3, and the mounting hook (button hook 31) is formed on the other. This is because hanging can be easily performed in a short time in either case.

[0037] [Second embodiment] Next, an inner surface smooth structure 1' of a corrugated steel pipe according to a second embodiment of the present invention will be described with reference to Fig. 5 to Fig. 7. Fig. 5 is a perspective view showing the inner surface smooth structure 1' of a corrugated steel pipe according to this embodiment, and Fig. 6 is a vertical cross-sectional view along the pipe axis showing the inner surface smooth structure 1' of a corrugated steel pipe. Fig. 7(a) is a schematic diagram showing an overview of a corrugated steel pipe having the inner surface smooth structure 1', and Fig. 7(b) is a schematic diagram showing another example of a corrugated steel pipe having the inner surface smooth structure 1'.

[0038] The corrugated steel pipe inner surface smooth structure 1' of the second embodiment is composed of a corrugated steel pipe 2' formed into a corrugated shape from a thin steel plate, and an inner surface smooth sheet 3' attached to the inner surface of this corrugated steel pipe 2'.

[0039] (Corrugated steel pipe) The corrugated steel pipe 2' is a corrugated steel pipe made by bending corrugated steel plates formed into a corrugation having a predetermined pitch (e.g., 68 mm) and a predetermined wave depth (e.g., 13 mm) from thin steel plates of 1.6 mm to 7.0 mm, such as hot-rolled mild steel plate SPHC (steel plate hot commercial) or general structural rolled steel material SS400, into half cylindrical shapes as shown in Figures 5 and 6, and combining these into a cylindrical shape. Of course, it goes without saying that the corrugated steel pipe 2' may be formed into a predetermined shape, such as an ellipse or a cylinder, by appropriately bending the corrugated steel plates.

[0040] As shown in Figures 5 and 6, the corrugated steel pipe 2' is composed of a semi-cylindrical arc-shaped steel plate 20' and a flange 21' that is bent up along the edge of the end of this arc-shaped steel plate 20' and protrudes outward. In addition, a long hole 22' for bolt connection is drilled in the peak portion, which is the corrugated upper part of the flange 21'.

[0041] The corrugated steel pipe 2' is not limited to one in which the ends of a semicircular section (arc-shaped steel plate 20') are bent up to form a flange 21' and the upper and lower sections are joined together by means of bolts, as shown in FIG. 7(a). It may also be a corrugated steel pipe 2" in which the cross section is formed by combining several arc-shaped sections 20", the circumference of which is divided into a number of arcs, and each section is joined together by bolts using a lap method to form a cylindrical shape, as shown in FIG. 7(b).

[0042] (Smooth inner surface sheet) The smooth-inner-surface sheet 3' in the second embodiment is made of a lightweight rubber sheet having a thickness of approximately 1 to 2 mm, similar to the smooth-inner-surface sheet 3 described above, but unlike the smooth-inner-surface sheet 3, it is made of a rubber tube 30' having a diameter of 800 mm to 3000 mm.

[0043] 5 and 6, the tubular inner surface smooth sheet 3' is fixed to the inner surface of the corrugated steel pipe 3' by being pressed against the corrugated steel pipe 3' from the inside by a ring spring 4. Therefore, the work of attaching the inner surface smooth sheet 3' to the corrugated steel pipe 2' can be completed easily in a short time.

[0044] Although the case where the inner surface smooth sheet 3' is shaped like a tube and covers the entire inner surface of the corrugated steel pipe 2' has been illustrated, the button hooks 31 and the slits 24 of the inner surface smooth structure 1 of the corrugated steel pipe may be applied to cover the lower half of the corrugated steel pipe 2' through which the wastewater from the corrugated steel pipe 2' is expected to flow, or to cover only the lower one-third. This is because it is clear that the roughness coefficient can be reduced even by only partially covering the inner surface of the corrugated steel pipe 2' with the inner surface smooth sheet 3.

[0045] <Method of smoothing the inner surface of corrugated steel pipes> Next, a method for smoothing the inner surface of a corrugated steel pipe according to an embodiment of the present invention will be described.

[0046] (Corrugated steel pipe assembly and installation process) First, in the method for smoothing the inner surface of a corrugated steel pipe according to this embodiment, a corrugated steel pipe assembly and installation step is performed in which a corrugated steel pipe is assembled and installed.

[0047] For example, in the case of the above-mentioned smooth inner surface structure 1 of the corrugated steel pipe, a groove is excavated and the corrugated steel pipe 2 consisting of the U-shaped flume body 20 is installed.

[0048] In the case of the above-mentioned corrugated steel pipe with smooth inner surface 1', the flanges 21' of the upper and lower semi-cylindrical arc-shaped steel plates 20' are bolted together to assemble the corrugated steel pipe 2', and then the corrugated steel pipe 2' is inserted into a culvert or the like for installation.

[0049] (Inner surface smoothing sheet installation process) Thereafter, in the method for smoothing the inner surface of a corrugated steel pipe according to this embodiment, an inner surface smoothing sheet attachment step is carried out in which the above-mentioned inner surface smoothing sheet is attached to the inner surface of the corrugated steel pipe.

[0050] For example, in the case of the above-mentioned smooth inner surface structure 1 of the corrugated steel pipe, a slit 24 is formed on the inner surface of the corrugated steel pipe 2, the above-mentioned hanging plate 23 is attached in advance, and the button hook 31 protruding from the smooth inner surface sheet 3 is fitted into the slit 24 and hung, thereby attaching the smooth inner surface sheet 3 to the inner surface of the corrugated steel pipe 2 (see Figure 4).

[0051] In the case of the aforementioned corrugated steel pipe inner surface smooth structure 1', a tubular inner surface smooth sheet 3' is pressed and fixed from the inside against the corrugated steel pipe 2' with a ring spring 4 to attach the inner surface smooth sheet 3' to the inner surface of the corrugated steel pipe 2' (see Figure 6).

[0052] According to the inner surface smoothing structure 1, 1' of a corrugated pipe according to an embodiment of the present invention and the inner surface smoothing method of a corrugated pipe according to an embodiment of the present invention described above, the roughness coefficient of the inner surface of the corrugated steel pipe 2, 2' can be reduced by the inner surface smoothing sheet 3, 3', thereby ensuring the flow rate of a drainage pipe consisting of the corrugated steel pipe 2, 2'.

[0053] Furthermore, according to the corrugated pipe inner surface smoothing structure 1, 1' and the method for smoothing the inner surface of a corrugated pipe according to this embodiment, construction and manufacturing costs can be reduced because lining material is not required, compared to attaching conventional paving material made of bituminous material to the inner surface of a corrugated steel pipe.

[0054] Moreover, according to the corrugated pipe smooth inner surface structure 1, the smooth inner surface sheet 3 is attached to the inner surface of the corrugated steel pipe 2 simply by fitting the button hooks 31 protruding from the smooth inner surface sheet 3 into the slits 24 and hooking them, so that the on-site installation work of the smooth inner surface sheet can be easily performed in a short time compared to the conventional case where a vaporizing material made of a plate material or a steel plate is bolted to the corrugated steel pipe. Therefore, the construction efficiency of the installation work of the drainage pipe made of the corrugated steel pipe is improved and the construction period can be shortened.

[0055] Similarly, according to the corrugated pipe smooth inner surface structure 1', the smooth inner surface sheet 3' is simply attached to the inner surface of the corrugated steel pipe 2' by pressing and fixing the tubular smooth inner surface sheet 3' from the inside with the ring spring 4 against the corrugated steel pipe 2' from the inside, so that the on-site installation work of the smooth inner surface sheet can be easily performed in a short time compared to the conventional case where a vaporizing material made of a plate material or a steel plate is bolted to the corrugated steel pipe. This improves the efficiency of the installation work for drainage pipes made of corrugated steel pipes and shortens the construction period.

[0056] In addition, according to the corrugated pipe inner surface smoothing structure 1, 1' and the corrugated pipe inner surface smoothing method of this embodiment, the inner surface smoothing sheets 3, 3' can be easily removed from the corrugated steel pipes 2, 2' compared to conventional paving materials made of bituminous material, making it possible to recover costs through waste disposal and steel scrap.

[0057] Furthermore, according to the corrugated pipe inner surface smoothing structure 1, 1' and the corrugated pipe inner surface smoothing method of this embodiment, compared to conventional paving materials made of bituminous material, there is no need to glue the paving material to the corrugated steel pipe, and ordinary hot-dip galvanized steel sheets can be used for the corrugated steel pipes 2, 2', making inventory management easier and reducing the unit manufacturing cost of the corrugated steel pipes.

[0058] Although the inner surface smoothing structure 1, 1' of a corrugated pipe according to an embodiment of the present invention and the inner surface smoothing method of a corrugated pipe according to an embodiment of the present invention have been described in detail above, the above-mentioned and illustrated embodiments are merely specific embodiments for carrying out the present invention, and therefore the technical scope of the present invention should not be interpreted as being limited by them. [Explanation of symbols]

[0059] 1,1': Smooth inner surface structure of corrugated steel pipe 2,2': Corrugated steel pipe 20: U-shaped flume body 20': Arc-shaped steel plate 20”: Arc section 21,21': Flange 22,22': Long hole 23: Hanging plate 24: Slit 3,3': Smooth inner surface sheet 30: Seat body 30': Rubber tube 31: Button hook 4: Ring spring

Claims

1. A smooth inner surface structure of a corrugated steel pipe that smooths the inner surface of a corrugated steel pipe to reduce the roughness coefficient, A smooth inner surface sheet made of a flexible rubber sheet, resin sheet, or cloth sheet is attached to the inner surface of the corrugated steel pipe. The smooth inner surface structure of the corrugated steel pipe is characterized by the above.

2. The inner smooth sheet is made of a material that does not soften or harden at room temperature of 5°C to 35°C.

2. The smooth inner surface structure of a corrugated steel pipe according to claim 1.

3. A slit or an attachment hole is formed in either the inner surface of the corrugated steel pipe or the inner surface smooth sheet, and an attachment hook is formed in the other, and the hook is hooked into the slit or the attachment hole, thereby fixing the inner surface smooth sheet to the inner surface of the corrugated steel pipe.

3. The smooth inner surface structure of a corrugated steel pipe according to claim 1 or 2.

4. The inner smooth sheet is tubular, and the tubular inner smooth sheet is pressed against the corrugated steel pipe from the inside by a ring spring, so that the inner smooth sheet is fixed to the inner surface of the corrugated steel pipe.

3. The smooth inner surface structure of a corrugated steel pipe according to claim 1 or 2.

5. A method for smoothing the inner surface of a corrugated steel pipe, which smooths the inner surface of a corrugated steel pipe to reduce the roughness coefficient, comprising the steps of: The method further comprises the step of attaching an inner smooth sheet made of a flexible rubber sheet or a resin sheet to the inner surface of the corrugated steel pipe. A method for smoothing the inner surface of a corrugated steel pipe, comprising the steps of:

6. In the inner surface smooth sheet mounting step, a mounting hook formed on one of the inner surface of the corrugated steel pipe and the inner surface smooth sheet is hooked onto a slit or mounting hole formed on the other of the inner surface of the corrugated steel pipe to mount the inner surface smooth sheet on the inner surface of the corrugated steel pipe.

6. The method for smoothing the inner surface of a corrugated steel pipe according to claim 5,

7. In the inner surface smooth sheet mounting step, the inner surface smooth sheet is tubular, and the tubular inner surface smooth sheet is pressed against the corrugated steel pipe from the inside by a ring spring to fix the inner surface smooth sheet to the inner surface of the corrugated steel pipe.

6. The method for smoothing the inner surface of a corrugated steel pipe according to claim 5,

Citation Information

Patent Citations

  • Inner surface-covered corrugated steel pipe, method for covering inner surface, and wear resisting paving sheet used therefor

    JP1995158775A

  • Corrugated pipe for drainage channel

    JP1995252818A

  • Inner surface covering method of inner surface covered corrugated steel pipe

    JP1996270840A

  • Asphalt-coated and corrugated steel plate for water way

    JP2009275353A