Packaging sheet, individually-packaged absorbent article obtained by packaging absorbent article individually in the packaging sheet, and manufacturing method of packaging sheet

The packaging sheet for absorbent articles addresses tearing and operability issues by maintaining a specific tensile strength and ink application ratio, ensuring smooth printing and easy opening, thus enhancing usability and hygiene.

JP2024143328APending Publication Date: 2024-10-11DAIO PAPER CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023055944
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-30
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

Conventional packaging sheets made of paper materials for absorbent articles face issues with tearing during printing and poor operability due to insufficient tensile strength and high paper weight, which affects usability and hygiene.

Method used

A packaging sheet with a tensile strength of 16N to 25N in the fiber direction, a specific ink and heat seal application ratio of 8.45≦X×(1-Y/100), and a surface MMD of 0.050 or less to prevent tearing during printing and improve appearance, combined with a paper weight of 30 gsm or less to enhance operability.

Benefits of technology

The solution prevents tearing during printing, ensures uniform printing, reduces material costs, and maintains usability by avoiding sharp edges and rustling sounds, while allowing easy opening and disposal of absorbent articles.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024143328000001_ABST
    Figure 2024143328000001_ABST
Patent Text Reader

Abstract

To avoid breakage when printing is performed on a surface.SOLUTION: Provided is a packaging sheet made of paper for individually packaging an absorbent article. Printing is performed on a surface of the packaging sheet while the packaging sheet is conveyed in a fiber direction. The packaging sheet has a tensile strength in the fiber direction of 16 N or more and 25 N or less. When the tensile strength in the predetermined direction before printing is performed on the packaging sheet is X(N), and a ratio of the area applied with at least one of ink for the printing and a heat seal agent for bonding the packaging sheets to the area of the entire packaging sheet is Y(%), 8.45≤X×(1-Y / 100) is satisfied.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a packaging sheet, an individually packaged absorbent article obtained by packaging an absorbent article in the packaging sheet, and a method for producing the packaging sheet. [Background technology]

[0002] Many absorbent articles, such as sanitary napkins, panty liners, incontinence pads, etc., are provided as individually packaged absorbent articles (individually packaged bodies) in which they are individually wrapped and sealed in a wrapping sheet for reasons such as hygiene during storage and convenience during carrying.

[0003] Such individually packaged absorbent articles are carried in a state in which the absorbent article is contained in a packaging sheet, and therefore it may be preferable to print on the surface of the packaging sheet so that the absorbent article is not recognized as an absorbent article at first glance.

[0004] Patent Document 1 discloses an absorbent article package that is configured to include an absorbent article and a packaging material for packaging the absorbent article, and has a pattern that is visible from the outside. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] International Publication No. 2020 / 095764 Summary of the Invention [Problem to be solved by the invention]

[0006] In recent years, from the viewpoint of environmental issues, packaging sheets are being made of paper materials instead of conventional nonwoven fabrics or plastic films. When packaging sheets are made of paper materials, it is necessary to prevent the packaging sheet from breaking during printing, etc.

[0007] The present invention has been made in consideration of the problems associated with the conventional technology as described above, and aims to provide a packaging sheet that can prevent tearing when printing is applied to the surface, an individually packaged absorbent article in which an absorbent article is individually packaged in the packaging sheet, and a method for manufacturing the packaging sheet. [Means for solving the problem]

[0008] In order to achieve the above object, the present invention provides A paper packaging sheet that is printed on its surface while being transported in the fiber direction and that individually packages absorbent articles, The packaging sheet has a tensile strength in the fiber direction of 16 N or more and 25 N or less, When the tensile strength in the fiber direction of the packaging sheet before printing is X (N) and the ratio of the area to which at least one of the ink for printing and the heat seal agent for bonding the packaging sheets is applied to the entire area of ​​the packaging sheet is Y (%), 8.45≦X×(1−Y / 100) Meet the following.

[0009] In the present invention configured as described above, the tensile strength of the packaging sheet in the conveying direction is 16 N or more and 25 N or less, and by making the tensile strength of the packaging sheet before printing and the ratio of the area to which at least one of the ink for printing and the heat sealant is applied to the total area of ​​the packaging sheet satisfy the above conditions, tearing can be avoided when printing is applied to the surface.

[0010] The surface on which printing is performed may have an MMD (mean coefficient of friction variation) of 0.050 or less.

[0011] In such a configuration, printing on the surface is made uniform, improving the appearance.

[0012] The paper weight may be 30 gsm or less.

[0013] With this configuration, problems such as an increase in material costs due to a high paper weight and poor operability and loud noises when opening due to the stiffness of the paper can be avoided.

[0014] Also, there is provided an individually packaged absorbent article in which an absorbent article is individually packaged in the packaging sheet, The packaging sheet is folded and the edges are sealed to individually package the absorbent articles, The seal strength at the edge may be smaller than the tensile strength of the packaging sheet.

[0015] In such a configuration, the packaging sheet is less likely to tear when the sealed portion is peeled off to remove the absorbent article.

[0016] Also, there is provided a method for producing a packaging sheet for individually packaging absorbent articles, comprising the steps of: a printing step of printing on a surface of the packaging sheet while conveying the packaging sheet in a fiber direction; and a coating step of coating a surface of the packaging sheet with a heat-sealing agent while conveying the packaging sheet in a fiber direction, The packaging sheet has a tensile strength in the fiber direction of 16 N or more and 25 N or less, When the tensile strength in the fiber direction of the packaging sheet before printing is X (N) and the ratio of the area to which at least one of the ink for printing and the heat sealant is applied to the entire area of ​​the packaging sheet is Y (%), 8.45≦X×(1−Y / 100) The above configuration may be adopted. Effect of the Invention

[0017] According to the present invention, it is possible to prevent the sheet from being torn when printing is performed on the surface. [Brief description of the drawings]

[0018] [Figure 1]1 is a plan view showing one embodiment of an individually packaged absorbent article of the present invention. [Diagram 2] 2 is a plan view of the individually packaged absorbent article shown in FIG. 1 in an unfolded state. [Diagram 3] FIG. 2 is a cross-sectional view of II shown in FIG. [Figure 4] FIG. 2 is an enlarged view of part II shown in FIG. [Diagram 5] FIG. 4 is a diagram for explaining a printing method for the packaging sheet shown in FIGS. 1 to 3. [Figure 6] FIG. 4 is a diagram showing a detailed configuration of a printed surface of the packaging sheet shown in FIGS. 1 to 3. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In each drawing, unless otherwise specified, the same or corresponding components are denoted by the same reference numerals and the description thereof will be omitted.

[0020] <Overall configuration of individually packaged absorbent article> Fig. 1 is a plan view showing one embodiment of an individually packaged absorbent article of the present invention. Fig. 2 is a plan view of the individually packaged absorbent article 100 shown in Fig. 1 in an unfolded state, as viewed from the inner surface of the packaging sheet 10 or from the skin side of the absorbent article 1. Fig. 3 is a cross-sectional view taken along line II shown in Fig. 1.

[0021] 1 to 3, the present embodiment is an individually packaged absorbent article 100 including a packaging sheet 10 and an absorbent article 1 individually packaged by the packaging sheet 10. As shown in Fig. 2, the packaging sheet 10 has an elongated shape, for example, in an unfolded state, and has a longitudinal direction (vertical direction) D1 and a lateral direction (lateral direction) D2 perpendicular to the longitudinal direction. The longitudinal direction D1 and the lateral direction D2 of the packaging sheet 10 also correspond to the longitudinal direction and the lateral direction of the absorbent article 1, respectively.

[0022] <Absorbent articles> The absorbent article 1 packaged in the packaging sheet 10 has a shape for being worn so as to face the excretion opening of bodily fluids (menstrual blood, vaginal discharge, urine, etc.), and is, for example, a flat and elongated article. Specific examples of the absorbent article 1 include sanitary napkins, panty liners (discharge sheets), and light incontinence pads. In this specification, the absorbent article will be mainly described as a sanitary napkin.

[0023] As shown in FIG. 2, for example, the absorbent article 1 has a liquid-permeable top sheet 3, a liquid-impermeable back sheet (not shown), and an absorbent body 4 disposed between the top sheet 3 and the back sheet.

[0024] The back sheet may be a sheet material having at least water impermeability, such as an olefin resin sheet, such as polyethylene or polypropylene. A laminated nonwoven fabric in which a nonwoven fabric is laminated on a polyethylene sheet, or a laminated sheet of nonwoven fabric in which a waterproof film is interposed to ensure substantial liquid impermeability may be used. A material having moisture permeability may also be used.

[0025] A porous or non-porous nonwoven fabric, a porous plastic sheet, etc. are preferably used as the top sheet 3. Examples of material fibers constituting the nonwoven fabric include olefins such as polyethylene and polypropylene, synthetic fibers such as polyester and polyamide, regenerated fibers such as rayon and cupra, and blends of these fibers, as well as natural fibers such as cotton, which may be used alone or in combination of two or more kinds.

[0026] The absorbent body 4 is not limited as long as it is a material capable of absorbing and retaining body fluids, but preferably contains cotton-like pulp and a water-absorbing polymer. As the water-absorbing polymer, superabsorbent polymer granular powder (superabsorbent polymer (SAP)), superabsorbent fiber (SAF)), and a combination thereof can be used. As the pulp, there can be mentioned chemical pulp obtained from wood, cellulose fiber such as dissolving pulp, and artificial cellulose fiber such as rayon and acetate. As the pulp, hardwood pulp obtained from hardwoods, softwood pulp obtained from softwoods, or a mixture thereof can be used. Furthermore, the pulp can be recycled pulp regenerated from used pulp.

[0027] The thickness of the absorbent body 4 may be 0.5 to 25 mm. The absorbent body 4 may have a bulging structure in an area corresponding to the bodily fluid discharge outlet (area corresponding to the bodily fluid discharge outlet) and an area behind the area corresponding to the bodily fluid discharge outlet facing the gluteal crease. The absorbent body 4 has a size and shape that does not protrude from the top sheet 3 and the back sheet, and at the front and rear edge portions of the absorbent body, the outer edges of the back sheet and the top sheet 3 are joined by an adhesive such as hot melt, heat sealing, ultrasonic sealing, or other adhesive means.

[0028] 2, side sheets 7 may be provided along the longitudinal direction D1 on both ends in the short side direction D2 on the outer lateral sides of the absorbent body 4. As the side sheets 7, a water-repellent treated nonwoven fabric or a hydrophilic treated nonwoven fabric may be used.

[0029] 1 to 3, the absorbent article 1 is a so-called wingless type without wings, but it may be configured as an article with wings that extend to each side. The wings may be formed by joining the side sheet and the back sheet.

[0030] Furthermore, an anti-slip adhesive portion may be provided on the back sheet side (non-skin side, i.e., the side facing the underwear when worn) of the absorbent article 1 to prevent the absorbent article 1 from slipping off the underwear when attached to the underwear. The anti-slip adhesive portion is formed, for example, in the shape of multiple strips extending in the longitudinal direction D1 or the lateral direction D2.

[0031] The overall length of the absorbent article 1 can be 140 to 430 mm, and the width of the absorbent article 1 (the width of the main body excluding the wings if the absorbent article has wings) can be 40 to 130 mm.

[0032] <Wrapping sheet> The packaging sheet 10 in this embodiment is paper. Using a paper packaging sheet 10 can contribute to reducing plastic use and achieving the Sustainable Development Goals. Paper can also impart a unique texture, such as the appearance and feel of a natural material.

[0033] The packaging sheet 10 is composed of 50% or more pulp fiber, and has a design printed on its exposed surface that is exposed when the absorbent article 1 is individually packaged. Detailed conditions of the packaging sheet 10 will be described later.

[0034] The dimensions of the packaging sheet 10 depend on the size and shape of the absorbent article 1 to be packaged, and for example, when the packaging sheet 10 is fully unfolded (not folded back), the length in the longitudinal direction D1 (sometimes simply referred to as the length) can be 100 to 450 mm, and the length in the transverse direction D2 (sometimes simply referred to as the width) can be 70 to 250 mm. In the illustrated example, the packaging sheet 10 has a rectangular shape when unfolded, but may have a shape such as an oblong shape.

[0035] <Packaging structure of individually packaged absorbent articles> As shown in Figs. 1 to 3, the absorbent article 1 is folded together with the packaging sheet 10 to be packaged, and an individually packaged absorbent article 100 is formed. When folding, as shown in Fig. 2, the absorbent article 1 is first placed on the inner surface of the packaging sheet 10 so that the back sheet side of the absorbent article 1 faces the inner surface of the packaging sheet 10. Then, the packaging sheet 10 and the absorbent article 1 are both folded in the longitudinal direction D1 at a first fold line F1 and a second fold line F2 along the width direction D2. More specifically, a first region R1 including one end 11 of the packaging sheet 10 in the longitudinal direction D1 is folded back in the longitudinal direction D1 at the first fold line F1, and a second region R2 including the other end 12 of the packaging sheet 10 in the longitudinal direction D1 is folded back at the second fold line F2. The region between the first region R1 and the second region R2 of the packaging sheet 10 is a third region R3. In the illustrated example, the packaging sheet 10 is folded so that the second region R2 is folded first and the first region R1 overlaps the outer surface of the second region R2 (FIGS. 1 and 2), but the folding order of the first region R1 and the second region R2 may be reversed. After the packaging sheet 10 and the absorbent article 1 are thus folded in three together (inner three fold) to wrap the absorbent article 1, both edges in the short direction D2 are sealed along the long direction D1, and the sealed portion 15 is formed.

[0036] Such a packaging format in which the absorbent article is folded in three or more can be formed relatively easily, can hygienically wrap the absorbent article 1, and also allows easy removal of the absorbent article 1. Note that the folding format is not limited to folding in three, and may be folded in four or more, or may be folded in half.

[0037] <Sealing section> 1, in the individually packaged absorbent article 100, the areas on both edges in the short-side direction D2 where the absorbent article 1 is not present are sealed to form a sealed portion 15. In this embodiment, this sealed portion 15 is formed by applying a heat sealant to the surface to be sealed of the packaging sheet 10, and then passing the packaging sheet 10 through a pair of heated rolls to press the packaging sheets 10 together in the thickness direction.

[0038] 1, the sealed portion 15 is formed, for example, over the entire length in the longitudinal direction D1 of the individually packaged absorbent article 100. This is preferable from the viewpoint of preventing dirt, dust, or accidentally fingers or small objects from entering through the short edge (obtaining a sealable property).

[0039] The range in the short side direction D2 in which the seal portion 15 is provided is, for example, a range up to 20 mm from the edge in the short side direction D2. The seal portion 15 may be formed over the entire range, or may be formed in a portion of the range, for example, at a position away from the edge in the short side direction D2. The length (width) of the seal portion 15 itself in the short side direction D2 is preferably 3 to 15 mm.

[0040] FIG. 4 is an enlarged view of part II shown in FIG.

[0041] As shown in FIG. 4, the seal portion 15 includes, for example, a plurality of pressure-bonded portions (or joint portions) 15a that are spaced apart from each other in a plan view. Each pressure-bonded portion 15a is a portion in which packaging sheets 10 are joined together by pressure bonding in the thickness direction. In the illustrated example, the portion other than the plurality of pressure-bonded portions 15a is a non-joined portion in which the packaging sheets 10 are not joined together. In this way, since the plurality of pressure-bonded portions 15a are scattered apart from each other, the packaging sheets can be easily peeled apart from each other when opening the package, and the ease of opening can be improved, compared to, for example, a case in which the packaging sheets 10 are joined together continuously over the entire surface of the seal portion 15. In addition, it is possible to prevent both edges of the individually packaged absorbent article 100 from becoming excessively hard and impairing the feel.

[0042] In addition, the planar shape of each of the compression parts 15a is a square in the example shown in Fig. 4, but is not limited to the illustrated shape, and may be, for example, a quadrangle other than a square such as a rectangle or a parallelogram, a polygon other than a quadrangle, a circle, an ellipse, a heart, a star, a teardrop, etc. In addition, the size of each of the compression parts 15a may be, for example, a square with one side of 0.25 to 2.5 mm, or a size having an area equivalent thereto. In addition, the arrangement of the multiple compression parts 15a may be in a lattice shape as shown in Fig. 4, or in a staggered shape.

[0043] (Fastening tape) 1 to 3, the individually packaged absorbent article 100 may be provided with a fastening tape 30 in the center in the short-side direction D2 near the edge of the first region R1 (one end 11 of the packaging sheet 10). The fastening tape 30 may be provided across the first region R1 and the second region R2 so as to straddle the one end 11 of the packaging sheet 10, as shown in Fig. 1. The fastening tape 30 has, in a plan view, a base portion 31 attached to the first region R1 and a tip portion 32 attached to the second region R2.

[0044] By providing the fastening tape 30, when opening the individually packaged absorbent article 100, the user can hold the fastening tape 30 (more specifically, the tip portion 32 of the fastening tape 30) and lift and pull the first region R1, making opening easier. Furthermore, by providing the fastening tape 30, when replacing the absorbent article, the used absorbent article can be wrapped in a packaging sheet obtained from a newly opened individually packaged absorbent article, and the end of the packaging sheet can be fastened to another location on the packaging sheet. This makes it possible to prevent the packaging sheet from opening and exposing the used absorbent article, and allows the used absorbent article to be disposed of hygienically.

[0045] The width (length in the short direction D2) of the fastening tape 30 may be preferably 5 to 30 mm, more preferably 10 to 20 mm. The entire length of the fastening tape 30 may be preferably 10 to 50 mm, more preferably 15 to 40 mm.

[0046] <Packaging sheet strength and ink coating area ratio> When manufacturing the individually packaged absorbent article 100 configured as above, first, printing is applied to the packaging sheet 10.

[0047] FIG. 5 is a diagram for explaining a printing method for the packaging sheet 10 shown in FIGS.

[0048] When manufacturing the packaging sheet 10 shown in Fig. 1, in a printing process, printing is performed on the surfaces of a plurality of packaging sheets 10 connected together in the fiber direction (MD: machine direction) which is the short side direction, as shown in Fig. 5. At that time, the packaging sheet 10 is printed while being transported with the short side direction as the transport direction A. However, if the tensile strength of the packaging sheet 10 is weak, the packaging sheet may tear during printing, i.e., a so-called paper break may occur.

[0049] Furthermore, when the packaging sheet 10 is printed, the ink from the printing penetrates the packaging sheet 10, causing the fiber structure to loosen and weakening the bonds between the fibers. This also weakens the tensile strength and causes the sheet to break. This phenomenon is not limited to the ink from the printing, but can also occur when a heat sealant is applied to the packaging sheet 10 in a coating process in which the heat sealant is applied to seal the packaging sheets 10 together, whether or not a printing process is performed.

[0050] FIG. 6 shows examples of printing on the packaging sheet 10 shown in FIGS. 1 to 3, where (a) is a plan view of an individually packaged absorbent article, and (b) is an enlarged view of part B in the case of dot printing.

[0051] When printing is performed on the packaging sheet 10, as shown in FIG. 6(a), there are colored areas 41 that are colored by printing and non-colored areas 42 that are not printed. Here, in the case of so-called solid printing by gravure printing, ink is applied to the entire colored area 41. Therefore, the application area ratio of ink to the entire packaging sheet 10 is (area of ​​colored region 41) / (total area of ​​packaging sheet 10) It becomes.

[0052] On the other hand, when printing is performed by dot printing, as shown in FIG. 6(b), the colored area 41 formed by printing includes a coated area 41a where ink is applied and a non-coated area 41b where ink is not applied. Therefore, the coating area ratio of the ink to the entire packaging sheet 10 is (area of ​​coated region 41a) / {(area of ​​non-colored region 42)+(area of ​​non-coated region 41b)}. That is, in dot printing, even if printing is performed on the entire packaging sheet 10, it is possible to prevent the ink coating area ratio to the entire packaging sheet 10 from becoming 100%.

[0053] Therefore, various papers that can be used as the packaging sheet 10 were examined for suitability for printing operation based on the tensile strength and the coating area ratio of the ink and heat sealant to the entire packaging sheet 10. In this embodiment, the packaging sheet 10 is printed while being transported in the fiber direction of the paper, so the tensile strength was measured in the fiber direction of the packaging sheet 10. In this examination, the measurement was performed at room temperature using a Tensilon tensile tester. As for the measurement conditions, the paper base material to be the packaging sheet 10 was cut into individual pieces of 120 mm in the fiber direction and 25 mm in the direction perpendicular to the fiber direction, and the tensile strength was measured while pulling in the fiber direction at a speed of 500 mm / sec. The chuck distance was 50 mm.

[0054] [Table 1] As shown in Table 1, in Example 1, Unryu paper (manufactured by Marubishi Paper Tech Co., Ltd.) with a basis weight of 14 gsm was used, in which the heat seal agent was not applied to the packaging sheet 10, and the coating area ratio of the ink to the entire packaging sheet 10 was 20%. In addition, in Example 2, Unryu paper (manufactured by Marubishi Paper Tech Co., Ltd.) with a basis weight of 14 gsm was used, in which the ink was not applied to the packaging sheet 10, and the coating area ratio of the heat seal agent to the entire packaging sheet 10 was 50%. In addition, in Example 3, crepe paper (manufactured by Daio Paper Co., Ltd.) with a basis weight of 18 gsm was used, in which the ink was not applied to the packaging sheet 10, and the coating area ratio of the heat seal agent to the entire packaging sheet 10 was 100%. In addition, in Example 4, crepe paper (manufactured by Daio Paper Co., Ltd.) with a basis weight of 18 gsm was used, in which the heat seal agent was not applied to the packaging sheet 10, and the coating area ratio of the ink to the entire packaging sheet 10 was 12%. As Example 5, crepe paper (manufactured by Daio Paper Co., Ltd.) with a basis weight of 18 gsm was used, in which the heat seal agent was not applied to the packaging sheet 10, and the coating area ratio of the ink to the entire packaging sheet 10 was 35%. As Comparative Example 1, Unryu paper (manufactured by Marubishi Paper Tech Co., Ltd.) with a basis weight of 17 gsm was used, in which the coating area ratio of the heat seal agent to the entire packaging sheet 10 was 100%, and the coating area ratio of the ink to the entire packaging sheet 10 was 72%. As Comparative Example 2, rayon PM (manufactured by Marubishi Paper Tech Co., Ltd.) with a basis weight of 14 gsm was used, in which the coating area ratio of the heat seal agent to the entire packaging sheet 10 was 100%, and the coating area ratio of the ink to the entire packaging sheet 10 was 72%. As Comparative Example 3, Unryu paper (manufactured by Marubishi Paper Tech Co., Ltd.) with a basis weight of 25 gsm was used. As Comparative Example 4, Kinshachi paper (manufactured by Daio Paper Co., Ltd.) with a basis weight of 24.4 gsm was used, in which the application area ratio of the heat sealant to the entire packaging sheet 10 was 100% and the application area ratio of the ink to the entire packaging sheet 10 was 72%.In addition, as Comparative Example 5, Kinshachi paper (manufactured by Daio Paper Co., Ltd.) with a basis weight of 30 gsm was used, in which the coating area ratio of the heat seal agent to the entire packaging sheet 10 was 100%, and the coating area ratio of the ink to the entire packaging sheet 10 was 72%. Note that Rayon PM is a paper composed of 15% rayon and 85% pulp.

[0055] In Table 1, for the printing suitability, a "◯" is given to products that could be printed without breaking, and an "×" is given to products that broke and were unable to be printed. Additionally, for usability, we determined whether the hardness of the paper caused any problems in use, such as sharp edges of the individual packaging or rustling noises. Products that had no problems in use were given an "◯", products that were hard and made noises when used were given an "×", and products that had problems with only one of the hardness or the sound were given a "△".

[0056] As a result, in Comparative Example 3 and Comparative Example 5, the individual packaging ends became sharp and the rustling sound during use became louder. As a result, it was found that when the tensile strength exceeded 54N, the individual packaging ends became sharp and the rustling sound during use became louder. In addition, when the paper used in Examples 3 to 5 had a tensile strength of 17.7N, there were cases where the paper broke during printing. On the other hand, in Comparative Example 1, which used paper with a tensile strength of 25.7N, no paper break occurred. As a result, it was found that when the tensile strength was 25N or less, there was a possibility that the paper would break during printing.

[0057] Therefore, for papers with a tensile strength of 25 N or less, the coating area ratio of the ink and heat sealant to the entire packaging sheet 10 was checked. For paper with a tensile strength of 17.7 N, paper breaks occurred during printing in Example 3, where the coating area ratio of the heat sealant to the entire packaging sheet 10 was 100%. On the other hand, for paper with a tensile strength of 17.7 N, paper breaks did not occur during printing in Example 5, where the coating area ratio of the ink to the entire packaging sheet 10 was 35%.

[0058] In addition, in Example 2 in which the application area ratio of the heat seal to the entire ink packaging sheet 10 was 50% for paper having a tensile strength of 16.9 N, no paper breaks occurred during printing.

[0059] Here, the ink application area ratio that enables printing operation increases proportionally to the strength of the paper. In other words, the higher the tensile strength of the paper, the larger the ink application area ratio that enables printing operation can be. Therefore, the threshold value for enabling printing operation is (Tensile strength) x (1 - ink (heat sealant) coating area ratio) is a constant value.

[0060] Therefore, based on the above results, for the paper used in Example 2, which had the weakest tensile strength among the papers verified this time, 50% of the heat seal coating area rate for which the printing operation suitability was rated "good" was substituted into the above formula, and 16.9 N was substituted for the tensile strength. 16.9×(1-0.50)=8.45 If this value is set as the lower limit, paper breaks will not occur during printing.

[0061] As a result, if the tensile strength is X (N) and the ratio of the area where at least one of the ink and the heat sealant is applied to the entire area of ​​the packaging sheet is Y (%), 8.45≦X×(1−Y / 100) It was found that in cases where the above condition is satisfied, no paper breaks occur during printing. The above formula holds even if any of the cases where the printing operation suitability was "○" is substituted into the algebras X and Y.

[0062] As for Unryu paper, Rayon PM, and Kinshachi, they are suitable for printing even when the coating area rate of the heat seal agent is 100%, so there is no need to restrict the coating area for papers with a tensile strength of over 25 N. Also, those with a tensile strength of less than 16 N are poorly suited for printing regardless of the coating area rate of the ink or heat seal agent, and are also likely to lead to individual packages tearing when opened.

[0063] From these results, it was determined that the tensile strength of the packaging sheet 10 in the conveying direction during printing is 16 N or more and 25 N or less. If the tensile strength of the packaging sheet 10 before printing is X (N) and the ratio of the area to the entire area of ​​the packaging sheet 10 where at least one of the ink for printing and the heat seal agent for bonding the packaging sheets together is applied is Y (%), 8.45≦X×(1−Y / 100) If a material that satisfies the above requirement is used, it is possible to prevent the packaging from being torn when printing is performed on the surface, and at the same time, it is possible to prevent the individual packaging edges from becoming sharp and to prevent a loud rustling sound during use.

[0064] This allows printing to be applied to the packaging sheet 10 using thin paper while ensuring operability and usability, and makes it possible to provide an individually packaged absorbent article 100 using a paper packaging sheet 10 with a highly designable design.

[0065] Furthermore, if the surface of the packaging sheet 10 is rough, the printing will not be uniform and the appearance will be poor. Therefore, an experiment was conducted to measure the MMD (mean coefficient of friction variation), which is an index of the smoothness of the paper surface, and to determine whether the paper is suitable for printing. As a result, it was found that paper with an MMD of 0.050 or less on the surface before printing is suitable for printing, and that by using this paper, it is possible to print on the surface of the packaging sheet 10 and improve the design.

[0066] In addition, if the paper weight is high, the material cost will increase. In addition, the paper will become stiff, which will lead to poor operability and problems such as loud noises when opening the package. Therefore, the paper weight is preferably 30 gsm or less.

[0067] <Seal strength> As described above, in the individually packaged absorbent article 100, the packaging sheet 10 together with the absorbent article 1 is folded in three (inner three fold) to wrap the absorbent article 1, and then both edge portions in the short direction D2 are sealed along the longitudinal direction D1 to form a sealed portion 15. Then, the packaging sheets 10 joined at the sealed portion 15 are peeled away from each other, whereby the individually packaged absorbent article 100 is opened and the absorbent article 1 is taken out.

[0068] Here, if the seal strength at the sealed portion 15 is too high, there is a risk that the packaging sheet 10 will tear when the packaging sheets 10 are peeled away from each other at the sealed portion 15 in order to remove the absorbent article 1.

[0069] Therefore, the relationship between the tensile strength of the sealed portion and the seal strength was examined for a configuration in which the packaging sheet 10 was not torn when peeled away from itself. In this examination, measurements were performed at room temperature using a Tensilon tensile tester. The measurement conditions were as follows: the packaging sheet 10 was cut into a 25 mm width including the sealed portion 15 (seal width 6 mm) in the longitudinal direction of the packaging sheet 10, and the tensile strength was measured by pulling the sealed portion of the cut sample in the longitudinal direction of the packaging sheet 10. The pulling speed was 100 mm / sec, and the chuck distance was 10 mm. The maximum point load (N / measurement width) was taken as the strength of the sealed portion 15.

[0070] [Table 2] As shown in Table 2, crepe paper (manufactured by Daio Paper Co., Ltd.) with a basis weight of 18 gsm was used as Example 1. Unryu paper (manufactured by Marubishi Paper Tech Co., Ltd.) with a basis weight of 17 gsm was used as Comparative Example 1. Rayon PM (manufactured by Marubishi Paper Tech Co., Ltd.) with a basis weight of 14 gsm was used as Comparative Example 2. As a result of verification of these, the seal strength of the sealed portion 15 was smaller than the tensile strength of the packaging sheet 10 for the paper of Example 1 and the papers of Comparative Examples 1 and 2.

[0071] This shows that if the seal strength at the sealed portion 15 is smaller than the tensile strength of the packaging sheet 10, the packaging sheet 10 is less likely to tear when peeling the packaging sheets 10 apart at the sealed portion 15 to remove the absorbent article 1.

[0072] Although the present invention has been described above based on the embodiments, the present invention is not limited to these embodiments. The above-mentioned embodiments can be variously changed, modified, substituted, added, deleted, and combined within the scope of the claims, and these also belong to the technical scope of the present invention. In addition, the above-mentioned components can be arbitrarily combined. [Explanation of symbols]

[0073] 1. Absorbent articles 3 Top sheet 4. Absorber 7 Side seat 10 Packaging Sheet 11 Longitudinal end 12 Other end in the longitudinal direction 15 Seal part 15a Crimping part 30 Fastening Tape 31 Base 32 Tip 41 Colored area 41a Coating area 41b Non-coating area 42 Uncolored area 100 individually packaged absorbent articles D1 Longitudinal direction of packaging sheet D2 Short side of packaging sheet F1 First fold line F2 Second fold line R1 1st area R2 2nd area R3 3rd area

Claims

1. A paper packaging sheet that is printed on its surface while being transported in the fiber direction and that individually packages absorbent articles, The packaging sheet has a tensile strength in the fiber direction of 16 N or more and 25 N or less, When the tensile strength in the fiber direction of the packaging sheet before printing is X (N) and the ratio of the area to which at least one of the ink for printing and the heat seal agent for bonding the packaging sheets is applied to the entire area of ​​the packaging sheet is Y (%), 8.45≦X×(1-Y / 100) Meet the packaging sheet.

2. The packaging sheet according to claim 1 , wherein the MMD of the surface on which the printing is performed is 0.050 or less.

3. The packaging sheet according to claim 1 or 2, having a basis weight of 30 gsm or less.

4. An individually packaged absorbent article comprising the absorbent article individually packaged in the packaging sheet according to claim 1 or 2, the packaging sheet is folded and the edges are sealed to individually package the absorbent articles; An individually packaged absorbent article, wherein the seal strength at said edge is less than said tensile strength.

5. A method for manufacturing a packaging sheet for individually packaging absorbent articles, comprising the steps of: a printing step of printing on a surface of the packaging sheet while conveying the packaging sheet in a fiber direction; and a coating step of coating a surface of the packaging sheet with a heat-sealing agent while conveying the packaging sheet in a fiber direction, The packaging sheet has a tensile strength in the fiber direction of 16 N or more and 25 N or less, When the tensile strength in the fiber direction of the packaging sheet before printing is X (N) and the ratio of the area to which at least one of the ink for printing and the heat sealant is applied to the entire area of ​​the packaging sheet is Y (%), 8.45≦X×(1-Y / 100) A manufacturing method of a packaging sheet that satisfies the above requirements.

Citation Information

Patent Citations

  • Absorbent article wrapper and package of absorbent article wrapper

    WO2020095764A1