Duplex stainless steel plate
By reducing the ferrite-austenite phase interface density in duplex stainless steel sheets to 0.50-0.70 pieces/μm, the sheets exhibit improved deep drawing formability and critical drawing ratios, addressing the limitations of conventional sheets in deep drawing applications.
Patent Information
- Application Number
- JP2024028906
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-30
- Filing Date
- 2024-02-28
- Publication Date
- 2024-10-11
AI Technical Summary
Conventional duplex stainless steel sheets containing a ferrite phase and an austenite phase lack sufficient deep drawing formability, particularly for applications requiring large drawing ratios, such as battery cases, due to inadequate critical drawing ratios and susceptibility to cracking during deep drawing processes.
The duplex stainless steel sheet is engineered to reduce the density of ferrite-austenite phase interfaces in the cross-section parallel to the rolling and plate thickness directions, with an interface density between 0.50 and 0.70 pieces/μm, achieved through controlled rolling and annealing processes to enhance deep drawing formability.
The solution results in a duplex stainless steel sheet with improved critical drawing ratio and reduced likelihood of cracking during deep drawing, demonstrating enhanced deep drawability and formability compared to conventional sheets.
Smart Images

Figure 2024144173000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a duplex stainless steel sheet containing a ferrite phase and an austenite phase, and a method for producing the same. [Background technology]
[0002] A duplex stainless steel sheet containing a ferrite phase and an austenite phase has high corrosion resistance and high strength, and is suitable for reducing the weight of molded products. In order to apply a duplex stainless steel sheet containing a ferrite phase and an austenite phase to deep-draw molded products such as battery cases, it is necessary to improve the deep-draw formability. Conventionally, techniques for improving the drawability of a duplex stainless steel sheet containing a ferrite phase and an austenite phase have been considered. Hereinafter, a duplex stainless steel sheet containing a ferrite phase and an austenite phase is also referred to as a "duplex stainless steel sheet".
[0003] In Patent Document 1, the r-value, which indicates the anisotropy of a stainless steel sheet, is defined as r0 for the r-value parallel to the rolling direction of the stainless steel sheet, and r for the r-value perpendicular to the rolling direction. 90 , r value in the direction at 45° to the rolling direction is r 45 Then, r 45 <r0<r 90 The present invention discloses a ferritic-austenitic duplex stainless steel sheet having improved square tube formability by adjusting the relationship between the sizes of the two.
[0004] Patent Document 2 discloses a ferritic-austenitic stainless steel sheet for press forming in which the difference in 0.2% yield strength between the 0° direction and the 90° direction relative to the rolling direction is kept to less than 20 MPa, thereby reducing the amount of earrings that occur during deep drawing, and a method for manufacturing the same. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Patent Publication No. 2018-127685 [Patent Document 2] Patent Publication No. 2011-208244 Summary of the Invention [Problem to be solved by the invention]
[0006] The limit drawing ratio is an index of drawing formability. The limit drawing ratio is a value obtained by dividing the maximum blank diameter that can be drawn without cracking by the diameter of the punch used in deep drawing. For example, in order to apply a duplex stainless steel sheet to a deep drawing product that requires a large drawing ratio, such as a battery case, it is necessary to improve the limit drawing ratio. The duplex stainless steel sheet described in Patent Document 1 has improved square tube formability, and the limit drawing ratio is not described. The duplex stainless steel sheet described in Patent Document 2 contributes to improving the yield by reducing the earrings.
[0007] In view of the above problems, an object of the present invention is to provide a duplex stainless steel sheet having excellent deep drawability compared to conventional duplex stainless steel sheets. [Means for solving the problem]
[0008] The present inventors have conducted extensive research to solve the above problems, and have found that by reducing the density of the ferrite-austenite interface in cross sections parallel to both the rolling direction and the sheet thickness direction, it is possible to reduce the possibility of fracture due to cracks occurring between the ferrite and austenite phases during deep drawing, thereby enabling an improvement in the limiting drawing ratio, and have completed the present invention.
[0009] In order to solve the above problems, a duplex stainless steel according to one embodiment of the present invention is a duplex stainless steel sheet containing a ferrite phase and an austenite phase, and when a cross section of the duplex stainless steel sheet parallel to both the rolling direction and the sheet thickness direction is observed, the number of intersections between an imaginary line segment drawn in the sheet thickness direction and a ferrite phase-austenite phase interface (excluding interfaces where the austenite phase has a thickness of less than 1 μm in the sheet thickness direction) is counted, and the number of intersections is divided by the length of the line segment to obtain the number of interfaces per unit length, which is defined as an interface density d. The interface density d is calculated at multiple different positions in the same sample, and the average value is calculated as d ave. When 0.50 particles / μm≦d ave. Satisfies ≦0.70 particles / μm. Effect of the Invention
[0010] According to one aspect of the present invention, a duplex stainless steel sheet having a larger limit drawing ratio and excellent deep drawability compared to conventional duplex stainless steel sheets can be provided. [Brief description of the drawings]
[0011] [Figure 1] 1 is a micrograph of an L cross section of the duplex stainless steel sheet of Example 1. [Diagram 2] 1 is a micrograph of an L cross section of the duplex stainless steel sheet of Comparative Example 2. [Diagram 3] 1 is an image of the surface of a deep-drawn product made from the duplex stainless steel sheet of Example 1, taken with a scanning electron microscope. [Figure 4] 1 is an image taken with a scanning electron microscope of the surface of a deep-drawn product made using the duplex stainless steel sheet of Comparative Example 2. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] One aspect of the present invention will be described in detail. The duplex stainless steel sheet in this embodiment is a stainless steel sheet containing a ferrite phase and an austenite phase. In this specification, the unit “%” of the content of each component element means “mass %” unless otherwise specified. Also, in this application, “A to B” indicates that it is A or more and B or less.
[0013] (Component composition) The duplex stainless steel sheet in this embodiment has, as a steel component composition, in mass %, C: 0.080% or less, Si: 2.00% or less, Mn: 4.00% or less, P: 0.040% or less, S: 0.0300% or less, Ni: 1.50 to 8.00%, Cr: 17.00 to 28.00%, Mo: 5.00% or less, Cu: 0.05 to 3.00%, and N: 0.080 to 0.320%, and the balance consists of Fe and impurities. The significance and content of these elements will be described in detail below.
[0014] <C: 0.080% or less> When the C content exceeds 0.080%, the corrosion resistance decreases due to the precipitation of Cr carbides. Therefore, it is desirable that the C content be low, but it can be tolerated up to 0.080%, so this is set as the upper limit. From the viewpoint of improving corrosion resistance, the upper limit of the preferable C content is 0.030%, and more preferably, it is 0.025%. The lower limit of the C content is not particularly limited, but from the viewpoint of cost, it is preferably 0.001%, and more preferably, it is 0.007%.
[0015] <Si: 2.00% or less> Si acts as a deoxidizer and a desulfurizer. When the Si content exceeds 2.00%, the toughness decreases, so the Si content is set to 2.00% or less. The upper limit of the Si content is preferably 0.65%. For Si to sufficiently act as a deoxidizer and a desulfurizer, the lower limit of the Si content is preferably 0.05%. A more preferable lower limit of the Si content is 0.30%.
[0016] <Mn: 4.00% or less> Although Mn is a relatively inexpensive element, it increases the amount of austenite phase in the stainless steel sheet and further raises the solid solubility of nitrogen, thereby having the effect of suppressing the precipitation of Cr nitrides. On the other hand, if it is contained in excess, it will cause deterioration of corrosion resistance, so the upper limit is set at 4.00%. The upper limit of the Mn content is preferably 3.50%. The lower limit of the Mn content is preferably 0.85%, and more preferably 2.00%.
[0017] <P: 0.040% or less> P is an element that is inevitably contained in the stainless steel sheet, but since it deteriorates hot workability, the P content is set to 0.040% or less. The upper limit of the P content is preferably 0.035%. The lower limit is not particularly limited, but from the viewpoint of cost, it is preferably 0.005%.
[0018] <S: 0.0300% or less> Similar to P, S is an element that is inevitably contained in the stainless steel sheet, but since it deteriorates hot workability, toughness, and corrosion resistance, the upper limit of the S content is set to 0.030%. The upper limit of the S content is preferably 0.020%. The lower limit of the S content is not particularly limited, but from the viewpoint of cost, it is preferably 0.0001%. A more preferable lower limit of the S amount is 0.0005%.
[0019] <Ni: 1.50 - 8.00%> Ni is an element that improves the crevice corrosion resistance of the stainless steel sheet. Crevice corrosion is corrosion that occurs when the pH inside the crevice decreases and the passive film cannot be maintained. Ni suppresses the dissolution of the stainless steel sheet in a low pH environment. When the Ni content is too low, the effect of improving crevice corrosion resistance cannot be obtained. Therefore, the Ni content is set to 1.50% or more. The lower limit of the Ni content is preferably 2.00%. On the other hand, if the Ni content is excessive, not only will the cost increase significantly, but the austenite phase will be excessive and the hot workability will decrease. Therefore, the Ni content is 8.00% or less. The upper limit of the Ni content is preferably 6.80%, and more preferably 2.50%.
[0020] <Cr: 17.00~28.00%> Cr is an element that improves the corrosion resistance of the stainless steel sheet. From the perspective of corrosion resistance, the lower limit of the Cr content is 17.00%. The lower limit of the Cr content is preferably 20.00%. On the other hand, Cr is an element that increases the ferrite phase. When the stainless steel sheet contains an excessive amount of Cr, the ferrite phase becomes excessive and the toughness decreases. Therefore, the upper limit of the Cr content is set at 28.00%. The upper limit of the Cr content is preferably 24.50%, and more preferably 22.00%.
[0021] <Mo: 5.00% or less> Mo has a high effect of improving corrosion resistance exceeding Cr, but it is a very expensive element. When the Mo content is excessive, the manufacturing cost increases. Also, when the Mo content is excessive, it causes hardening of the stainless steel sheet and deteriorates the workability. Therefore, the upper limit of the Mo amount is set at 5.00%. The upper limit of the Mo content is preferably 2.95%, and more preferably 0.60%. The effect of improving corrosion resistance that Mo has is poor in terms of its additive effect when the Mo content is less than 0.01%. Therefore, the Mo content is preferably 0.01% or more. The lower limit of the Mo content is preferably 0.05%, and more preferably 0.20%.
[0022] <Cu: 0.05~3.00%> Cu is an element that suppresses the dissolution of the stainless steel sheet in a low pH environment, similar to Ni. However, when the stainless steel sheet contains an excessive amount of Cu, the hot workability is significantly impaired. Therefore, the upper limit of the Cu content is set at 3.00%. The upper limit of the Cu content is preferably 1.40%. On the other hand, the effect of suppressing the dissolution of the stainless steel sheet in a low pH environment cannot be expected much when the Cu content is less than 0.50%. Therefore, the lower limit of the Cu content is set at 0.50%. The lower limit of the Cu content is preferably 0.60%, and more preferably 0.70%.
[0023] <N: 0.080~0.320%> N is an element that significantly improves corrosion resistance and increases the amount of austenite phase. To obtain this effect, the lower limit of the N content is set to 0.080%. The lower limit of the N content is preferably 0.150%, and more preferably 0.155%. On the other hand, if the N content exceeds 0.320%, nitrides are formed in the steel, which reduces the corrosion resistance and toughness, so the upper limit of the N content is set to 0.320%. The upper limit of the N content is preferably 0.200%.
[0024] Here, the term "impurities" refers to impurity elements that are mixed in from raw materials such as ore and scrap, or from the manufacturing environment, during industrial production of the duplex stainless steel sheet of this embodiment, and are contained within a range that does not adversely affect the duplex stainless steel sheet of this embodiment. For example, 0.0070% or less of O may be contained as an impurity.
[0025] An example of the basic components of the duplex stainless steel sheet in this embodiment has been described above, but the duplex stainless steel sheet in this embodiment may further contain one or more of the elements described below in place of a portion of Fe.
[0026] <Al:0.003~0.050%> Al is an element with a strong deoxidizing effect, and is contained as necessary. In order to obtain the deoxidizing effect of Al, the Al content is preferably 0.003% or more. The lower limit of the Al content is more preferably 0.005%. On the other hand, Al easily forms nitrides together with N, and when nitrides are formed, the toughness is significantly reduced. Therefore, the upper limit of the Al content is preferably 0.050%. The upper limit of the Al content is preferably 0.040%.
[0027] <Nb:0.005~0.20%> Nb is an element that fixes C and N to prevent a decrease in corrosion resistance due to precipitation of Cr carbides and improves corrosion resistance, and is therefore included as necessary. If the Nb content is 0.005% or more, the effect is manifested, so the lower limit of the Nb content is preferably 0.005%. On the other hand, if the Nb content exceeds 0.20%, the α phase becomes hard due to solid solution strengthening, which may reduce workability, so the upper limit of the Nb content is preferably 0.20%.
[0028] <Ti:0.003~0.20%> Ti is an element that fixes C and N to prevent sensitization due to Cr carbide precipitation and improves corrosion resistance, and is therefore included as necessary. If the Ti content is 0.003% or more, the effect is manifested, so the lower limit of the Ti content is preferably 0.003%. On the other hand, if the Ti content exceeds 0.20%, the ferrite phase is hardened, the toughness is reduced, and furthermore, the surface roughness may be reduced due to Ti-based precipitates, so the upper limit of the Ti content is preferably 0.20%.
[0029] <Co:0.005~0.25%> Co is an element that suppresses the precipitation of Cr carbides and suppresses the deterioration of corrosion resistance, and is therefore included as necessary. If the Co content is 0.005% or more, Co exerts the above effects, so the lower limit of the Co content is preferably 0.005%. On the other hand, since Co is a rare element and expensive, the upper limit of the Co content is preferably 0.25%.
[0030] <V:0.005~0.15%> V is a strong carbide-forming element. When V, which easily forms carbides in high temperature regions, is contained, the precipitation of Cr carbides is suppressed, and the deterioration of corrosion resistance can be suppressed. For this reason, V is contained as necessary. Since V exerts the above-mentioned effect when the V content is 0.005% or more, the lower limit of the V content is preferably 0.005%. On the other hand, since a high V content leads to hardening, the upper limit of the V content is preferably 0.15%.
[0031] <Sn:0.005~0.20%、Sb:0.005~0.20%> Since Sn and Sb are elements that improve corrosion resistance, they are contained as necessary. When the content of either Sn or Sb is 0.005% or more, the effect of improving corrosion resistance is exerted, so the content of each of Sn and Sb is preferably 0.005% or more. The lower limit of each of the contents of Sn and Sb is more preferably 0.030%. On the other hand, Sn and Sb are also solid solution strengthening elements of the ferrite phase. For this reason, the upper limit of each of the contents of Sn and Sb is preferably 0.20%. The upper limit of each of the contents of Sn and Sb is more preferably 0.10%.
[0032] <Ga:0.001~0.050%> Ga is an element that contributes to improving corrosion resistance, and is therefore included as necessary. If the Ga content is 0.001% or more, the effect of improving corrosion resistance is exhibited, so the Ga content is preferably 0.001% or more. On the other hand, if the Ga content exceeds 0.050%, the effect of improving corrosion resistance is saturated, and this only leads to an increase in costs. Therefore, the upper limit of the Ga content is preferably 0.050%.
[0033] <Zr:0.005~0.50%> Zr is an element that contributes to improving corrosion resistance, and is therefore included as necessary. If the Zr content is 0.005% or more, the effect of improving corrosion resistance is exhibited, so the lower limit of the Zr content is preferably 0.005%. If the Zr content is more than 0.50%, the effect is saturated, so the upper limit of the Zr content is preferably 0.50%.
[0034] <Ta:0.005~0.100%> Ta is an element that improves corrosion resistance by modifying inclusions, and is therefore included as necessary. If the Ta content is 0.005% or more, the above effects are exhibited, so the lower limit of the Ta content is preferably 0.005%. On the other hand, if the Ta content exceeds 0.100%, it may lead to a decrease in ductility and toughness at room temperature. Therefore, the upper limit of the Ta content is preferably 0.100%. The upper limit of the Ta content is more preferably 0.050%.
[0035] <B:0.0002~0.0050%> Since B is an element that has the effect of suppressing secondary work embrittlement and deterioration of hot workability, it is contained as necessary. If the B content is 0.0002% or more, B has the above effect, so the lower limit of the B content is preferably 0.0002%. On the other hand, B is an element that does not affect corrosion resistance, and if the B content exceeds 0.0050%, hot workability may deteriorate, so the upper limit of the B content is preferably 0.0050%. The upper limit of the B content is more preferably 0.0020%.
[0036] (interface density) In the duplex stainless steel of this embodiment, the density of the interface between the ferrite phase and the austenite phase in cross sections parallel to both the rolling direction and the plate thickness direction is within a predetermined range as shown below, so that the limiting drawing ratio is large. This will be described in detail below.
[0037] The method for calculating the interface density of the ferrite phase-austenite phase is as follows. A test piece is cut out from the prepared duplex stainless steel sheet, and a cross section parallel to both the rolling direction and the thickness direction of the duplex stainless steel sheet (so-called L cross section) is exposed, then embedded in resin and polished. Then, the piece is etched with an arbitrary agent to reveal the ferrite phase and the austenite phase.
[0038] Next, a structural photograph obtained by photographing the L-section of the test piece at a magnification of 500 to 1000 times is subjected to line analysis. Specifically, in the structural photograph of the L-section, the number of intersections between a virtual line drawn in the sheet thickness direction and the interface between the ferrite phase and the austenite phase is measured, and the number of intersections is divided by the length (μm) of the line to calculate the interface density d (pieces / μm), which is the number of interfaces (pieces) per unit length. However, since an interface where the thickness of the austenite phase in the sheet thickness direction is less than 1 μm has almost no effect on deep drawability, the interface density d is calculated using the number of interfaces excluding the interface. The above line analysis is performed at multiple different positions in the same sample, and the average value is taken as the average interface density d d. ave. The length of the line segment may be at least as long as it does not cause large variations in the line analysis results, for example, at least 50 μm.
[0039] The duplex stainless steel in this embodiment has an average interface density d ave. However, 0.50 pieces / μm≦d ave. The inventors have determined that the average interface density d ave. Through extensive research, we have found that duplex stainless steel sheets with an average interfacial density of 0.70 particles / μm or less have excellent deep drawability. ave. By keeping the density of interface d below 0.70 / μm, the number of two-phase interfaces that are the starting points of cracks is reduced, and the possibility of fracture due to cracks occurring during deep drawing can be reduced. ave. If the density is higher than 0.70 / μm, the number of two-phase interfaces that are the starting points of cracks increases, making the duplex stainless steel sheet more susceptible to fracture during deep drawing. On the other hand, if the interface density is too low, that is, if the content of the austenite phase is too low, the strength of the duplex stainless steel sheet decreases. ave. The number of grains / μm is 0.50 or more. From the viewpoint of increasing the ratio of the austenite phase and securing a certain level of strength, d ave. It is preferable that d is 0.51 / μm or more. ave. From the viewpoint of reducing breakage during deep drawing, it is preferable that the number of particles is 0.69 particles / μm or less.
[0040] (Method of manufacturing duplex stainless steel) The manufacturing method of the duplex stainless steel sheet in this embodiment will be described. The manufacturing method of the duplex stainless steel sheet in this embodiment includes a steelmaking process, a hot rolling process, a hot-rolled sheet pickling process, and a sheet thickness reduction process. For the processes other than the hot rolling process and the sheet thickness reduction process, the manufacturing conditions are not particularly limited, and known methods can be applied.
[0041] The hot rolling process is a process in which a steel sheet having the above-mentioned composition is hot-rolled to a thickness of less than 4.0 mm. The thickness of the sheet after hot rolling in this process is preferably 3.9 mm or less. The lower limit of the thickness after hot rolling is not particularly limited, but may be, for example, 3.0 mm. In the hot rolling process, the hot-rolled steel sheet may be annealed.
[0042] The thickness reduction step is a step of reducing the thickness of a hot-rolled sheet, the thickness of which has been reduced to less than 4.0 mm by the hot rolling step, to 0.50 mm to 1.60 mm. For example, the processing rate in the thickness reduction step (when the thickness is reduced by cold rolling, the cold rolling rate) may be 60% or more and 74% or less. This reduces the average value d ave. However, 0.50 pieces / μm≦d ave. It is possible to manufacture duplex stainless steel sheets that satisfy the requirement of ≦0.70 particles / μm.
[0043] The method for reducing the plate thickness is typically cold rolling, but the plate thickness may also be reduced by compression processing, for example. When the plate thickness is reduced by cold rolling, annealing may be performed after the cold rolling.
[0044] In the plate thickness reduction step, if the plate thickness is reduced to less than 0.50 mm, there is a risk that the steel plate will break due to localized thickness reduction during processing. Therefore, in the plate thickness reduction step, the plate thickness is reduced to 0.50 mm or more.
[0045] In the plate thickness reduction process, if the plate thickness is processed to be greater than 1.60 mm, the deformation resistance of the steel plate will increase, the load during forming will increase, and there is a risk of damage to the die. Therefore, in the plate thickness reduction process, the plate thickness is reduced to 1.60 mm or less.
[0046] As described above, the method for producing a duplex stainless steel sheet according to one embodiment of the present disclosure is a method for producing a duplex stainless steel sheet containing a ferrite phase and an austenite phase, and includes a hot rolling step of producing a hot rolled sheet having a thickness of less than 4.0 mm by hot rolling, and a thickness reducing step of reducing the thickness of the hot rolled sheet having a thickness of less than 4.0 mm to 0.50 mm to 1.60 mm. The method for producing a duplex stainless steel sheet according to one embodiment of the present disclosure may be configured such that the thickness reducing step reduces the thickness of the hot rolled sheet by cold rolling.
[0047] The duplex stainless steel sheet in the present invention may have a steel composition comprising: C: 0.001 to 0.050%, Si: 0.01% or more and less than 0.50%, Mn: 1.0 to 4.5%, P: 0.050% or less, S: 0.030% or less, Ni: 1.5 to 3.5%, Cr: 19.6 to 24.0%, Mo: 0.01 to 1.00%, Cu: 0.01 to 1.20%, and N: 0.010 to 0.090%, with the remainder being Fe and impurities, and C+N being less than 0.130%. In this case, the duplex stainless steel sheet may further contain one or more elements selected from Nb: 0.010-0.500%, Ti: 0.010-0.500%, V: 0.01-0.50%, W: 0.05-0.50%, Co: 0.01-0.30%, B: 0.0002-0.0050%, Sn: 0.010-0.500%, Al: 0.010-0.050%, Mg: 0.0002-0.0100%, Ca: 0.0002-0.0100%, Ta: 0.050% or less, Ga: 0.050% or less, Zr: 0.01-0.50%, and REM: 0.0002-0.0100% as required. The significance of including these elements and their contents will be described in detail below.
[0048] <C:0.001~0.050%> C is an element that has a great influence on the stability of the austenite phase. If the C content is too high, the ductility (workability) may decrease, or the precipitation of Cr carbides may be promoted, leading to intergranular corrosion. Therefore, the C content is set to 0.050% or less, preferably 0.045% or less, more preferably 0.040% or less. Also, from the perspective of corrosion resistance, a lower C content is better, but reducing the C content too much will cause an increase in cost. Therefore, the C content is set to 0.001% or more, preferably 0.002% or more, more preferably 0.005% or more.
[0049] <Si: 0.01% or more and less than 0.50%> Si is added as a deoxidizing element and is also useful for improving oxidation resistance. However, if the Si content is too high, it will become hardened and the ductility will decrease. Therefore, the Si content is set to less than 0.50%, preferably 0.45% or less, more preferably 0.40% or less. Also, reducing Si excessively will increase the cost during steelmaking. Therefore, the Si content is set to 0.01% or more, preferably 0.02% or more, more preferably 0.05% or more.
[0050] <Mn: 1.0 - 4.5%> Mn is an element that plays an important role in concentrating in the austenite phase and stabilizing the austenite phase. However, if the Mn content is too high, in addition to ductility, corrosion resistance and hot workability will also decrease. Therefore, the Mn content is set to 4.5% or less, preferably 4.0% or less, more preferably 3.5% or less. Also, reducing Mn excessively will increase the cost during steelmaking. Therefore, the Mn content is set to 1.0% or more, preferably 1.1% or more, more preferably 1.2% or more.
[0051] <P: 0.050% or less> P is an element contained in raw materials such as Cr. When the content of P is high, the formability decreases. Therefore, the content of P is set to 0.050% or less, preferably 0.045% or less, more preferably 0.040%. On the other hand, although it is preferable that the content of P is lower, there is a limit to reducing the content of P. The lower limit of the content of P is generally 0.001%, preferably 0.002%, more preferably 0.003%.
[0052] <S: 0.030% or less> S is an element contained in various raw materials. Since S combines with Mn to form inclusions and may become a starting point for rusting, the lower the content of S, the better the corrosion resistance. Therefore, the content of S is set to 0.030% or less, preferably 0.025% or less, more preferably 0.020% or less. On the other hand, there is a limit to reducing the content of S. The lower limit of the content of S is generally 0.0001%, preferably 0.0005%.
[0053] <Ni: 1.5 - 3.5%> Ni is an austenite-forming element and is an important element for adjusting the stability of the austenite phase. Also, Ni has the effect of suppressing the precipitation of nitrides and improving the corrosion resistance. To exert these effects, the content of Ni is set to 1.5% or more, preferably 1.6% or more, more preferably 1.7% or more, still more preferably 1.8% or more. On the other hand, if the content of Ni is too high, it will not only lead to an increase in raw material costs, but also problems such as stress corrosion cracking may occur due to the high proportion of the austenite phase. Therefore, the content of Ni is set to 3.5% or less, preferably 3.4% or less, more preferably 3.0% or less.
[0054] <Cr: 19.6 - 24.0%> Cr is an element necessary for ensuring corrosion resistance. To achieve this effect, the Cr content is set to 19.6% or more, preferably 20.0% or more, and more preferably 20.4% or more. On the other hand, if the Cr content is too high, it may cause hot working cracks or increase the cost of the refining process. Therefore, the Cr content is set to 24.0% or less, preferably 23.5% or less, and more preferably 23.0% or less.
[0055] <Mo:0.01~1.00%> Mo is an element that improves corrosion resistance. To achieve this effect, the Mo content is set to 0.01% or more, preferably 0.03% or more, and more preferably 0.05% or more. On the other hand, if the Mo content is too high, the raw material cost increases. Therefore, the Mo content is set to 1.00% or less, preferably 0.80% or less, and more preferably 0.50% or less.
[0056] <Cu:0.01~1.20%> Cu, like Mn and Ni, is an austenite-forming element and has the effect of suppressing the precipitation of nitrides and improving corrosion resistance. In order to exert these effects, the Cu content is set to 0.01% or more, preferably 0.05% or more, and more preferably 0.10% or more. On the other hand, if the Cu content is too high, it will not only increase the raw material cost but also reduce the hot workability. Therefore, the Cu content is set to 1.20% or less, preferably 1.00% or less, and more preferably 0.80% or less.
[0057] <N:0.010~0.090%> Like C, N is an element that has a large effect on the stability of the austenite phase. N is also an element that dissolves in solid solution to improve corrosion resistance. In order to achieve these effects, the N content is set to 0.010% or more, preferably 0.020% or more. On the other hand, if the N content is too high, the ductility decreases and the corrosion resistance also decreases due to the precipitation of Cr nitrides. Therefore, the N content is set to 0.090% or less, preferably 0.080% or less.
[0058] <Less than 0.130% of C + N> When the total content of C and N increases, the corrosion resistance decreases due to sensitization, or the ductility decreases due to high strength. Therefore, the total content of C and N is less than 0.130%, preferably 0.120% or less. The lower limit of the total content of C and N is not particularly limited, but is preferably 0.010%, preferably 0.020%, more preferably 0.030%.
[0059] <0.010 - 0.500% of Nb> Nb forms nitrides (NbN) and carbides (NbC) and has the effect of improving workability. To exert this effect, the content of Nb is 0.010% or more, preferably 0.015% or more, more preferably 0.020% or more. On the other hand, if the content of Nb is too high, the ductility decreases. Therefore, the content of Nb is 0.500% or less, preferably 0.300% or less, more preferably 0.200% or less.
[0060] <0.010 - 0.500% of Ti> Similar to Nb, Ti also forms nitrides (TiN) and carbides (TiC) and has the effect of improving workability. To exert this effect, the content of Ti is 0.010% or more, preferably 0.015% or more, more preferably 0.020% or more. On the other hand, if the content of Ti is too high, the ductility decreases. Therefore, the content of Nb is 0.500% or less, preferably 0.300% or less, more preferably 0.200% or less.
[0061] <0.01 - 0.50% of V> V forms nitrides and has the effect of improving workability. To exert this effect, the content of V is 0.01% or more, preferably 0.03% or more, more preferably 0.05% or more. On the other hand, if the content of V is too high, the ductility and hot workability will decrease. Therefore, the content of V is 0.50% or less, preferably 0.45% or less, more preferably 0.40% or less.
[0062] <0.05 - 0.50% of W> W is an element effective in improving corrosion resistance. To achieve this effect, the W content is set to 0.05% or more, preferably 0.08% or more, and more preferably 0.10% or more. On the other hand, if the W content is too high, the ductility decreases. Therefore, the W content is set to 0.50% or less, preferably 0.45% or less, and more preferably 0.40% or less.
[0063] <Co:0.01~0.30%> Co is an element effective in increasing high-temperature strength and improving hot workability. In order to exert these effects, the Co content is set to 0.01% or more, preferably 0.03% or more, and more preferably 0.05% or more. On the other hand, if the Co content is too high, the toughness decreases. Therefore, the Co content is set to 0.30% or less, preferably 0.25% or less, and more preferably 0.20% or less.
[0064] <B:0.0002~0.0050%> B is an element that segregates at grain boundaries to improve hot workability. To achieve this effect, the B content is set to 0.0002% or more, preferably 0.0010% or more, and more preferably 0.0015% or more. On the other hand, if the B content is too high, the corrosion resistance is significantly reduced. Therefore, the B content is set to 0.0050% or less, preferably 0.0040% or less, and more preferably 0.0030% or less.
[0065] <Sn:0.010~0.500%> Sn is an element that improves corrosion resistance. To achieve this effect, the Sn content is set to 0.010% or more, preferably 0.020% or more, and more preferably 0.030% or more. On the other hand, if the Sn content is too high, the hot workability is reduced. Therefore, the Sn content is set to 0.500% or less, preferably 0.450% or less, and more preferably 0.400% or less.
[0066] <Al:0.010~0.050%> Al is an element effective for desulfurization and deoxidation. To exert these effects, the Al content is set to 0.010% or more, preferably 0.015% or more, more preferably 0.020% or more. On the other hand, if the Al content is too high, it will lead to an increase in manufacturing defects and raw material costs. Therefore, the Al content is set to 0.050% or less, preferably 0.045% or less, more preferably 0.040% or less.
[0067] <Mg: 0.0002~0.0100%> Mg is an element that not only deoxidizes but also has the effect of refining the solidification structure. To exert these effects, the Mg content is set to 0.0002% or more, preferably 0.0005% or more, more preferably 0.0010% or more. On the other hand, if the Mg content is too high, it will lead to an increase in raw material costs. Therefore, the Mg content is set to 0.0100% or less, preferably 0.0095% or less, more preferably 0.0090% or less.
[0068] <Ca: 0.0002~0.0100%> Ca is an element effective for desulfurization and deoxidation. To exert this effect, the Ca content is set to 0.0002% or more, preferably 0.0005% or more, more preferably 0.0010% or more. On the other hand, if the Ca content is too high, hot working cracks are likely to occur and the corrosion resistance also decreases. Therefore, the Ca content is set to 0.0100% or less, preferably 0.0080% or less, more preferably 0.0050% or less.
[0069] <Ta: 0.050% or less> Ta is an element that improves corrosion resistance by modifying inclusions. However, if the Ta content is too high, it will lead to a decrease in normal temperature ductility and toughness. Therefore, the Ta content is 0.050% or less, preferably 0.045% or less, more preferably 0.040% or less. On the other hand, the lower limit value of the Ta content is not particularly limited, but to exert the effect of Ta, it is preferably 0.001%, more preferably 0.003%.
[0070] <Ga: 0.050% or less> Ga is an element that improves corrosion resistance and suppresses hydrogen embrittlement. However, if the Ga content is too high, workability decreases. Therefore, the Ga content is set to 0.050% or less, preferably 0.040% or less, and more preferably 0.030% or less. On the other hand, the lower limit of the Ga content is not particularly limited, but in order to exert the effect of Ga, it is preferably 0.001%, more preferably 0.003%.
[0071] <Zr:0.01~0.50%> Zr has a similar effect to Nb and Ti and is an element that improves oxidation resistance. In order to exert these effects, the Zr content is set to 0.01% or more, preferably 0.03% or more, and more preferably 0.05% or more. On the other hand, if the Zr content is too high, it will not only reduce ductility but also increase raw material costs. Therefore, the Zr content is set to 0.50% or less, preferably 0.40% or less, and more preferably 0.30% or less.
[0072] <REM:0.0002~0.0100%> REM (rare earth) is an element effective in improving hot workability. To achieve this effect, the REM content is set to 0.0002% or more, preferably 0.0005% or more, and more preferably 0.0010% or more. On the other hand, if the REM content is too high, it impairs manufacturability and increases costs. Therefore, the REM content is set to 0.0100% or less, preferably 0.0090% or less, and more preferably 0.0080% or less.
[0073] REM is a general term for Sc, Y, and 15 elements from La to Lu (lanthanoids). These elements can be used alone or in combination of two or more kinds as REM.
[0074] The present invention is not limited to the above-described embodiments, and various modifications are possible within the scope of the claims. Embodiments obtained by appropriately combining the technical means disclosed in different embodiments are also included in the technical scope of the present invention. EXAMPLES
[0075] An embodiment of the present invention will now be described.
[0076] The duplex stainless steel sheet of Example 1 was produced as follows. First, a steel sheet having the composition shown in Table 1 was produced. Next, the produced steel sheet was hot rolled to a thickness of 3.5 mm, and then annealed. Thereafter, the steel sheet was cold rolled to a thickness of 0.99 mm, and then annealed to produce a cold-rolled annealed duplex stainless steel sheet of Example 1.
[0077] The duplex stainless steel sheets of Examples 2 to 14 and Comparative Examples 1 to 11 were produced in the same manner as Example 1, except that the compositions, the thicknesses of the steel sheets after hot rolling and annealing (hot rolled and annealed sheet thickness), and the thicknesses of the steel sheets after cold rolling and annealing (cold rolled and annealed sheet thickness) were different. For Examples 1 to 14 and Comparative Examples 1 to 11, the compositions of the steel sheets are shown in Table 1, and the hot rolled and cold rolled annealed sheet thicknesses are shown in Table 2. Table 2 also shows the cold rolling reduction ratios. [Table 1] [Table 2] (Average interfacial density d ave. ) Next, for the duplex stainless steel sheets of Examples 1 to 14 and Comparative Examples 1 to 11, the average interface density d ave. was calculated as follows. A test piece was cut from the center of the plate thickness (1 / 2 of the plate thickness) of the prepared duplex stainless steel plate, and after exposing the L-shaped cross section, it was embedded in resin and polished. The L-shaped cross section was then etched with an etching agent suitable for revealing the phases, revealing the ferrite phase and the austenite phase.
[0078] Next, an arbitrary field (observation field) in the L-section of the test piece in which the ferrite phase and the austenite phase were revealed by etching was photographed at a magnification of 500 times using an optical microscope (Olympus Corporation, model number BX53M) to take a structural photograph of the L-section. FIG. 1 is a structural photograph of the L-section of the duplex stainless steel sheet of Example 1. FIG. 2 is a structural photograph of the L-section of the duplex stainless steel sheet of Comparative Example 2. Next, as shown in FIG. 1 and FIG. 2, three imaginary line segments L of length l were drawn parallel to the sheet thickness direction so as to divide the structural photograph of the L-section of the steel sheet into four equal parts in the rolling direction, and the number of intersections I of each line segment L1, L2, and L3 with the ferrite phase-austenite phase interface was measured. The numerical values shown in FIG. 1 and FIG. 2 are the number of intersections I1, I2, and I3 of each line segment L1, L2, and L3 with the ferrite phase-austenite phase interface. Next, the measured intersection counts I1, I2, and I3 were divided by the line length l to calculate the interface densities d1, d2, and d3, which are the number of interfaces per unit length. The interface density d can be expressed by the following formula.
[0079] d(pieces / μm)=I(pieces) / l(μm) At this time, the interface density d was calculated using the number of interfaces I excluding interfaces where the thickness of the austenite phase in the plate thickness direction was less than 1 μm. In the example shown in Figures 1 and 2, the field area of the observation field was 9900 μm 2 The length of the line segment was equal to the vertical length of the observation field, 99 μm. The same line analysis was performed in three different fields, and the average value d of the nine calculated interface densities (3 lines per field × 3 fields) was calculated. ave. The average value of the calculated interface density d ave. is shown in Table 2.
[0080] As shown in Table 2, in the duplex stainless steel sheets of Examples 1 to 14 in which the thickness of the hot-rolled sheet was reduced to 0.50 mm to 1.60 mm from the hot-rolled sheet having a thickness of less than 4.0 mm in the hot-rolling process, the average value of the interface density d ave.In contrast, in the duplex stainless steel sheets of Comparative Examples 1 to 11 in which the thickness was reduced to 0.50 mm to 1.60 mm from the hot-rolled sheet having a thickness of 4 mm or more in the hot rolling process, the average interface density was d ave. was greater than 0.70 particles / μm.
[0081] (Deep drawing test) Next, a deep drawing test was performed using the duplex stainless steel sheets of Examples 1 to 14 and Comparative Examples 1 to 11. The deep drawing test was performed with a punch diameter of 40 mm, a punch R of 4 mm, a die diameter set arbitrarily according to the sheet thickness of the workpiece, a blank holding force of 10 kN, and a punch speed of 20 mm / min. Castrol's Iloform CFX300 was used as the lubricant, and the lubricant was applied to the surface of the material with a brush. The limit drawing ratio LDR was calculated from the deep drawing test results. The calculated limit drawing ratio LDR is shown in Table 2. As shown in Table 2, the duplex stainless steel sheets of Examples 1 to 14 had limit drawing ratios LDR that were about 5% higher than those of the duplex stainless steel sheets of Comparative Examples 1 to 11.
[0082] The surface of the formed product after the deep drawing test was observed using a scanning electron microscope (manufactured by JEOL Ltd., model number JSM-IT510). FIG. 3 is an image of the surface of the formed product deep-drawn using the duplex stainless steel sheet of Example 1, taken with a scanning electron microscope. FIG. 4 is an image of the surface of the formed product deep-drawn using the duplex stainless steel sheet of Comparative Example 2, taken with a scanning electron microscope. As shown in FIG. 3, when the duplex stainless steel sheet of Example 1 was used for forming, no cracks were confirmed on the surface. In contrast, when the duplex stainless steel sheet of Comparative Example 2 was used for forming, as shown in FIG. 4, microcracks along the rolling direction were observed. Even when the duplex stainless steel sheets of Examples 2 to 14 were used, no cracks were observed on the surface of the formed product after the deep drawing test, as in the case of the duplex stainless steel sheet of Example 1 shown in FIG. 3. On the other hand, when the duplex stainless steel sheets of Comparative Examples 1 and 3 to 11 were used, cracks were observed on the surface of the formed product after the deep drawing test, as in the case of the duplex stainless steel sheet of Comparative Example 2 shown in FIG.
Claims
1. A duplex stainless steel sheet containing a ferrite phase and an austenite phase, When the duplex stainless steel sheet is observed in a cross section parallel to both the rolling direction and the sheet thickness direction, the number of intersections between an imaginary line drawn parallel to the sheet thickness direction and a ferrite phase-austenite phase interface (excluding interfaces where the austenite phase has a thickness of less than 1 μm in the sheet thickness direction) is measured, and the number of intersections is divided by the length of the line to obtain the number of interfaces per unit length, which is defined as an interface density d. The interface density d is calculated at multiple different positions in the same sample, and the average value is calculated as d ave. When 0.50 pieces / μm≦d ave. A duplex stainless steel sheet satisfying a grain size distribution of ≦0.70 particles / μm.
2. The duplex stainless steel sheet according to claim 1, containing, by mass%, C: 0.080% or less, Si: 2.00% or less, Mn: 4.00% or less, P: 0.040% or less, S: 0.0300% or less, Ni: 1.50 to 8.00%, Cr: 17.00 to 28.00%, Mo: 5.00% or less, Cu: 0.05 to 3.00%, and N: 0.080 to 0.320%, with the balance being Fe and impurities.
3. The duplex stainless steel sheet according to claim 1, containing, by mass%, C: 0.001 to 0.050%, Si: 0.01% or more and less than 0.50%, Mn: 1.0 to 4.5% or less, P: 0.050% or less, S: 0.030% or less, Ni: 1.5 to 3.5%, Cr: 19.6 to 24.0%, Mo: 0.01 to 1.00%, Cu: 0.01 to 1.20%, and N: 0.010 to 0.090%, with the balance being Fe and impurities, and C + N being less than 0.130%.
4. The duplex stainless steel sheet according to claim 3, further comprising at least one selected from, by mass%, Nb: 0.010 to 0.500%, Ti: 0.010 to 0.500%, V: 0.01 to 0.50%, W: 0.05 to 0.50%, Co: 0.01 to 0.30%, B: 0.0002 to 0.0050%, Sn: 0.010 to 0.500%, Al: 0.010 to 0.050%, Mg: 0.0002 to 0.0100%, Ca: 0.0002 to 0.0100%, Ta: 0.050% or less, Ga: 0.050% or less, Zr: 0.01 to 0.50%, and REM: 0.0002 to 0.0100%.
Citation Information
Patent Citations
Ferritic-austenitic stainless steel sheet to be press-formed causing small earring, and method for manufacturing the same
JP2011208244A
Ferrite austenite two-phase stainless steel sheet and manufacturing method therefor