Heater element assembly

The heater element assembly with resin-protected honeycomb structures addresses the issues of size and inefficiency by using resin frames to enhance protection and reduce heat loss, providing a compact and efficient heating solution for vehicle air conditioning systems.

JP2024144204APending Publication Date: 2024-10-11NGK INSULATORS LTD

Patent Information

Application Number
JP2024037395
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2023-03-30
Filing Date
2024-03-11
Publication Date
2024-10-11

AI Technical Summary

Technical Problem

Existing heater elements with honeycomb structures for vehicle air conditioning systems are large and inefficient, leading to space constraints and heat loss, and there is a need for a more compact and protective design that reduces heat loss while maintaining performance.

Method used

A heater element assembly comprising a honeycomb structure with PTC characteristics, sandwiched by resin frames on both ends, which provide protection and reduce heat loss through the use of resin materials with specific properties such as low thermal conductivity and Rockwell hardness.

Benefits of technology

The resin frames effectively protect the heater element from damage and reduce heat loss, allowing for a more compact and efficient heating solution suitable for vehicle air conditioning systems.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024144204000001_ABST
    Figure 2024144204000001_ABST
Patent Text Reader

Abstract

To provide a heater element assembly including a heater element having a honeycomb structure with PTC characteristics and a frame, which has excellent protective performance for the heater element and also contributes to reducing heat loss.SOLUTION: A heater element assembly includes a heater element and a frame, the heater element includes a honeycomb structure capable of generating heat when electrically energized, including an outer peripheral wall and partition walls that are arranged on an inner peripheral side of the outer peripheral wall, define a plurality of cells forming flow paths extending from a first end face to a second end face, and contain a material having PTC characteristics, and the frame includes a first frame portion made of resin and a second frame portion made of resin for sandwiching the heater element from the first end face side and the second end face side.SELECTED DRAWING: Figure 2A
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a heater element assembly comprising a heater element and a frame. [Background technology]

[0002] There is an increasing demand for improving the cabin environment in various vehicles such as automobiles. Specific demands include reducing CO2 in the cabin to suppress drowsiness of the driver, controlling humidity in the cabin, and removing harmful volatile components such as odor components and allergy-inducing components from the cabin. Ventilation is an effective measure to meet such demands, but ventilation causes a large loss of heater energy in winter, leading to a deterioration in energy efficiency in winter. In particular, electric vehicles (BEVs: Battery Electric Vehicles) have a problem in that the energy loss significantly reduces the driving range.

[0003] Therefore, Patent Documents 1 and 2 disclose a vehicle interior purification system in which components to be removed, such as water vapor and CO2, in the air in the vehicle interior are captured by a functional material such as an adsorbent, and then the components to be removed are reacted or desorbed by heating and released outside the vehicle, thereby regenerating the functional material. In such a vehicle interior purification system, it is required that the air and the functional material come into contact as much as possible in order to ensure the capturing performance of the components to be removed, and that the functional material can be heated to a predetermined temperature in order to promote the regeneration of the functional material. Regeneration is performed, for example, by a method of removing substances adsorbed on the functional material by an oxidation reaction, or a method of desorbing and discharging substances adsorbed on the functional material, but in either case, it is necessary to heat the functional material to an appropriate temperature depending on the adsorbed substance.

[0004] As a heating means, a vapor compression heat pump is superior in terms of thermal efficiency, but there are problems with the vapor compression heat pump, such as difficulty in operating when the outside air temperature is extremely low, and difficulty in rapidly heating the passenger compartment when starting the vehicle. Therefore, it is considered practical to use the vapor compression heat pump as the main heating device, while supplementarily using a heater element that utilizes Joule heat when rapid heating is required when starting the vehicle or when the outside air temperature is very low.

[0005] However, heater elements that utilize Joule heat tend to be large in size, which occupies space inside the vehicle. For this reason, it is desirable to provide a more compact heater element. In this regard, it is known that heater elements that include a honeycomb structure with PTC characteristics are advantageous because they can increase the heat transfer area per unit volume and prevent excessive heat generation (Patent Document 3).

[0006] Patent Document 3 describes a heater element having a columnar honeycomb structure having an outer peripheral side wall and partition walls having PTC characteristics that are disposed inside the outer peripheral side wall and define a plurality of cells that form a flow path from a first bottom surface to a second bottom surface. Patent Document 3 also describes that a pair of electrodes is joined to the heater element and a voltage is applied between the pair of electrodes to generate heat.

[0007] Patent Document 4 describes a heating device in which the heating element is entirely or partially made of a positive characteristic porcelain having a large number of through holes, and which is provided with a means for convecting gas or liquid through the through holes. It also describes that the positive characteristic porcelain (PTCR) and a fan are placed opposite each other in a cylindrical frame, and the PTCR is fixed to the frame with a heat-resistant insulating support. [Prior art documents] [Patent documents]

[0008] [Patent Document 1] JP 2020-104774 A [Patent Document 2] JP 2020-111282 A [Patent Document 3] International Publication No. 2020 / 036067 [Patent Document 4] Japanese Unexamined Patent Publication No. 49-114130 Summary of the Invention [Problem to be solved by the invention]

[0009] When a heater element having a honeycomb structure with PTC characteristics is installed in a vehicle, it is assumed that the heater element is installed in an air passage in the HVAC, which is the air conditioning system of the vehicle. In this case, it is considered preferable to install the heater element while protecting it with a frame. In this regard, although Patent Document 4 describes that the PTCR is fixed to the frame with a heat-resistant insulating support, the consideration is insufficient from the viewpoint of protecting the PTCR and reducing heat loss.

[0010] The present invention has been created in consideration of the above circumstances, and an object of the present invention is to provide, in one embodiment, a heater element assembly including a heater element having a honeycomb structure portion with PTC characteristics and a frame body, which has excellent protective performance for the heater element and also contributes to reducing heat loss. [Means for solving the problem]

[0011] The inventors of the present invention have conducted extensive research to solve the above problems and have found that it is advantageous to clamp a heater element having a honeycomb structure with PTC characteristics from the end face side with a resin frame having a predetermined structure. The present invention, which was completed based on this finding, is exemplified as follows.

[0012] [1] A heater element assembly comprising a heater element and a frame, The heater element is a honeycomb structure portion capable of generating heat when electrically connected, the honeycomb structure portion having an outer peripheral wall, and partition walls disposed on an inner peripheral side of the outer peripheral wall, partitioning a plurality of cells that form flow paths extending from a first end face to a second end face, the partition walls containing a material having a PTC property; a first electrode layer covering a part or the whole of a surface of the partition wall forming the first end surface; a second electrode layer covering a part or the whole of a surface of the partition wall forming the second end face; a first terminal connected to an outer surface of the first electrode layer; and a second terminal connected to an exterior surface of the second electrode layer; having The frame body is for clamping the heater element from the first end surface side and the second end surface side, a first frame portion made of resin and arranged on the first end surface side, the first frame portion having a flange portion arranged on the outer peripheral side of an outer peripheral contour of the first end surface, and a retaining portion arranged on the inner peripheral side of the outer peripheral contour of the first end surface and applying pressure to at least a part of an outer periphery of the first end surface; and a second frame portion made of resin and arranged on the second end surface side, the second frame portion having a flange portion arranged on the outer peripheral side of an outer peripheral contour of the second end surface, and a retaining portion arranged on the inner peripheral side of the outer peripheral contour of the second end surface and applying pressure to at least a part of an outer periphery of the second end surface; having Heater element assembly. [2] The heater element assembly according to [1], wherein the resin constituting the first frame portion and / or the second frame portion has a Rockwell hardness of 150 HRR or less and / or 120 HRM or less, as measured in accordance with ASTM D785-2008 R15. [3] The heater element assembly according to [1] or [2], wherein the resin constituting the first frame portion and / or the second frame portion has a deflection temperature under load of 145°C or higher as measured in accordance with JIS K7191-1:2015. [4] The heater element assembly according to any one of [1] to [3], wherein the resin constituting the first frame and / or the second frame has a melting point of 250° C. or higher. [5] The heater element assembly according to any one of [1] to [4], wherein the resin constituting the first frame portion and / or the second frame portion has a thermal conductivity of 0.5 W / m / K or less at 25°C measured in accordance with JIS R1611:2010. [6] The resin constituting the first frame and / or the second frame has a volume resistivity of 1.0×10 at 25° C. as measured in accordance with JIS C2139:2008. 16 The heater element assembly according to any one of [1] to [5], wherein the thermal conductivity is Ω·cm or more. [7] The heater element assembly according to any one of claims [1] to [6], wherein the resin constituting the first frame portion and / or the second frame portion contains one or two types selected from polyether ether ketone (PEEK) and polybutylene terephthalate (PBT). [8] A ratio of an area of ​​the first end face to which pressure is applied by the holding portion of the first frame portion to an area of ​​the first end face is 10% or less, and / or A ratio of an area of ​​the second end face to which pressure is applied by the holding portion of the second frame portion to an area of ​​the second end face is 10% or less. A heater element assembly according to any one of [1] to [7]. [9] A ratio of an area of ​​the first end face to which pressure is applied by the holding portion of the first frame portion to an area of ​​the first end face is 2% or less, and / or A ratio of an area of ​​the second end face to which pressure is applied by the holding portion of the second frame portion to an area of ​​the second end face is 2% or less. A heater element assembly according to any one of [1] to [7].

[10] the holding portion of the first frame portion has a portion that presses the first terminal toward the first end surface, and / or the holding portion of the second frame portion has a portion that presses the second terminal toward the second end surface, A heater element assembly according to any one of [1] to [9].

[11] A cushioning material is interposed between the holding portion of the first frame portion and the first end surface, and / or A cushioning material is interposed between the holding portion of the second frame portion and the second end surface. A heater element assembly according to any one of [1] to

[10] .

[12] The heater element assembly according to any one of [1] to

[11] , wherein the frame has a third frame portion made of resin that surrounds the outer peripheral surface of the outer peripheral wall of the heater element.

[13] A heater element assembly as described in

[12] , wherein a cushioning material is interposed between the third frame portion and the outer peripheral wall.

[14] The heater element assembly of any one of [1] to

[13] , wherein the first frame portion and the second frame portion are separated from each other and connected by a fastener.

[15] The heater element assembly according to any one of [1] to

[13] , wherein the first frame portion and the second frame portion are separated from each other and connected by a fitting structure.

[16] The heater element assembly according to any one of [1] to

[13] , wherein the first frame portion and the second frame portion are separated from each other and connected with an adhesive.

[17] and / or, an average value of the thickness of the first electrode layer at an outer periphery of the first end surface and at a connection point with the first terminal is greater than an average value of the thickness of the first electrode layer at other portions. an average value of a thickness of the second electrode layer at an outer circumferential portion of the second end face and at a connection portion between the second terminal and the second end face is greater than an average value of a thickness of the second electrode layer at other portions; A heater element assembly according to any one of [1] to

[16] .

[18] and / or, the average thickness of the first electrode layer over the entire outer periphery of the first end surface is greater than the average thickness of the first electrode layer over the remaining portion. an average thickness of the second electrode layer over the entire outer periphery of the second end face is greater than an average thickness of the second electrode layer over the other portion; A heater element assembly according to any one of [1] to

[17] . Effect of the Invention

[0013] According to the heater element assembly of the present invention, a resin frame protects a heater element having a honeycomb structure with PTC characteristics by clamping both end faces. Since resin is generally softer than metal, by making the frame out of resin, the portion of the heater element that contacts the frame is less likely to be damaged. Furthermore, since resin generally has a lower thermal conductivity than metal, it also contributes to reducing heat loss. [Brief description of the drawings]

[0014] [Figure 1A] FIG. 2 is a schematic diagram of a heater element according to one embodiment of the present invention as viewed from a first end surface side. [Figure 1B] FIG. 1B is a schematic cross-sectional view taken along line XX in FIG. 1A. [Figure 1C] FIG. 4 is a schematic diagram of a heater element according to another embodiment of the present invention, viewed from a first end surface side. [Figure 1D] FIG. 2 is a schematic cross-sectional view taken along line XX in FIG. 1C. [Figure 2A] 1 is a schematic diagram of an example of a heater element assembly having a frame that clamps a heater element from a first end surface side and a second end surface side, as viewed from the first end surface side. FIG. [Figure 2B] FIG. 2B is a schematic cross-sectional view taken along line XX in FIG. 2A. [Figure 3A] 13 is a schematic diagram of another example of a heater element assembly having a frame that clamps a heater element from a first end surface side and a second end surface side, as viewed from the first end surface side. FIG. [Figure 3B]FIG. 3B is a schematic cross-sectional view taken along line XX in FIG. 3A. [Figure 4A] 13 is a schematic diagram of yet another example of a heater element assembly having a frame that clamps a heater element from a first end surface side and a second end surface side, viewed from the first end surface side. FIG. [Figure 4B] FIG. 4B is a schematic cross-sectional view taken along line XX in FIG. 4A. [Figure 5A] 13 is a schematic diagram of yet another example of a heater element assembly having a frame that clamps a heater element from a first end surface side and a second end surface side, viewed from the first end surface side. FIG. [Figure 5B] FIG. 5B is a schematic cross-sectional view taken along line XX in FIG. 5A. [Figure 6] 1 is a schematic diagram showing a configuration example of an air conditioning system according to an embodiment of the present invention;

[0015] Hereinafter, the embodiments of the present invention will be described in detail with reference to the drawings. The present invention is not limited to the following embodiments, and it should be understood that modifications and improvements to the following embodiments, which are made based on the ordinary knowledge of those skilled in the art, fall within the scope of the present invention, without departing from the spirit of the present invention.

[0016] (1. Heater element) The heater element according to the embodiment of the present invention can be suitably used to improve the indoor environment in various vehicles such as automobiles. Examples of the vehicle include, but are not limited to, automobiles and trains. Examples of the automobile include, but are not limited to, gasoline vehicles, diesel vehicles, gas-fueled vehicles using CNG (compressed natural gas) or LNG (liquefied natural gas), fuel cell vehicles, electric vehicles, and plug-in hybrid vehicles. The heater element according to the embodiment of the present invention can be suitably used in vehicles that do not have an internal combustion engine, such as electric vehicles and trains.

[0017] In addition, the heater element according to the embodiment of the present invention can be used to improve the interior space of buildings such as houses, offices, factories, stores, warehouses, and freezers, as well as vehicles such as ships and airplanes, other than vehicles.

[0018] The heater element according to the embodiment of the present invention can be used for heating purposes, and can also be added with a function of removing components to be removed from the air, which can contribute to improving the indoor environment. For example, the heater element can be added with a layer containing a functional material having a function of adsorbing components to be removed from the air, such as water vapor, carbon dioxide, and odor components, on the surface of the partition wall that forms the flow path inside the cell of the heater element.

[0019] Fig. 1A shows a schematic diagram of a heater element 100 according to one embodiment of the present invention as viewed from a first end surface side. Fig. 1B shows a schematic cross-sectional view of line XX in Fig. 1A. Fig. 1C shows a schematic diagram of a heater element 100 according to another embodiment of the present invention as viewed from a first end surface side. Fig. 1D shows a schematic cross-sectional view of line XX in Fig. 1C.

[0020] The heater element 100 comprises a honeycomb structure having an outer peripheral wall 103 and partition walls 106 arranged on the inner peripheral side of the outer peripheral wall 103 and defining a plurality of cells 104 that form flow paths extending from a first end face 101a to a second end face 101b. The heater element 100 includes a first electrode layer 102a covering a part or all of the surface of the partition wall 106 that forms the first end face 101a, and a second electrode layer 102b covering a part or all of the surface of the partition wall 106 that forms the second end face 101b. The heater element 100 comprises a first functional material-containing layer 107a covering a portion of the outer surface of the first electrode layer 102a (thereby indirectly covering the first end face 101a), and a second functional material-containing layer 107b covering a portion of the outer surface of the second electrode layer 102b (thereby indirectly covering the second end face 101b). The heater element 100 comprises a first terminal 109a connected to the outer surface of the first electrode layer 102a (if a first functional material-containing layer 107a is provided, it is preferable that the first terminal 109a is a portion of the outer surface of the first electrode layer 102a that is not covered by the first functional material-containing layer 107a), and a second terminal 109b connected to the outer surface of the second electrode layer 102b (if a second functional material-containing layer 107b is provided, it is preferable that the second terminal 109b is a portion of the outer surface of the second electrode layer 102b that is not covered by the second functional material-containing layer 107b). The heater element 100 includes a third functional material-containing layer 111a that covers a portion of the outer surface of the first terminal 109a, and a fourth functional material-containing layer 111b that covers a portion of the outer surface of the second terminal 109b. The heater element 100 includes a fifth functional material-containing layer 113 that covers a part or the whole of the surface of the partition wall 106 that forms the flow path inside the cell 104 . The configuration of the heater element 100 will be described in detail below.

[0021] (1-1. Honeycomb structure) The shape of the honeycomb structure is not particularly limited. For example, the outer shape of the cross section perpendicular to the direction in which the flow channels of the honeycomb structure extend (the direction in which the cells 104 extend) can be polygonal (quadrilateral (rectangle, square), pentagon, hexagon, heptagon, octagon, etc.), round (circular, elliptical, oval, egg-shaped, oval, rounded quadrangle (each side and each corner is formed by a curve, the radius of curvature of each side is larger than the radius of curvature of each corner, and a quadrangle formed by curves as a whole), etc.). In addition, when the outer shape of the cross section is polygonal, the corners may be chamfered. For the reasons of preventing damage to the honeycomb structure and making it easier to wrap a cushioning material around the outer peripheral surface, it is preferable that the corners are particularly R-chamfered, and it is more preferable that there are no corners with a radius of curvature of 5 mm or less, and even more preferable that the radius of curvature of the corners is 10 mm or more, and even more preferable that it is 20 mm or more. The upper limit of the radius of curvature of the corner is not limited, but can be 40 mm or less, and is typically 30 mm or less. The end faces (first end face 101a and second end face 101b) have the same shape as the cross section. In the heater element 100 shown in Figures 1A and 1B, the cross section of the honeycomb structure part has a circular outer shape, and the overall outer shape of the honeycomb structure part is cylindrical. In the heater element 100 shown in Figures 1C and 1D, the cross section of the honeycomb structure part has a rectangular outer shape with R-chamfered edges, and the overall outer shape of the honeycomb structure part is a square prism with R-chamfered edges.

[0022] The opening shape of the cells 104 is not particularly limited, and may be polygonal (quadrilateral (rectangle, square), pentagon, hexagon, heptagon, octagon, etc.), round (circular, elliptical, oval, egg, oval, etc.), etc. in a cross section perpendicular to the direction in which the flow path of the honeycomb structure extends. These shapes may be a single shape or a combination of two or more shapes. Among these shapes, a quadrangle or hexagon is preferable. By providing cells 104 of such a shape, the pressure loss during air circulation can be reduced. When the opening shape of the cells 104 is polygonal, the corners may be rounded. In the heater element 100 shown in the figure, the opening shape of the cells 104 is square.

[0023] The honeycomb structure may be a honeycomb bonded body having a plurality of honeycomb segments and a bonding layer bonding the outer peripheral surfaces of the plurality of honeycomb segments to each other. By using the honeycomb bonded body, it is possible to increase the total cross-sectional area of ​​the cells 104, which is important for ensuring the flow rate of air, while suppressing the occurrence of cracks. The bonding layer can be formed using a bonding material. The bonding material is not particularly limited, but a paste made by adding a solvent such as water to a ceramic material can be used. The bonding material may contain a material having PTC properties, or may contain the same material as the outer peripheral wall 103 and the partition wall 106. In addition to the role of bonding the honeycomb segments to each other, the bonding material can also be used as an outer peripheral coating material after bonding the honeycomb segments.

[0024] From the standpoints of ensuring the strength of the honeycomb structure, reducing pressure loss when air passes through the cells 104, ensuring the amount of functional material carried, ensuring the contact area with the air flowing within the cells 104, electrical resistance between the end faces, etc., it is desirable to suitably combine the thickness of the partition walls 106, the cell density, and the cell pitch (or the cell opening rate). In this specification, the thickness of the partition wall 106 refers to the length of a line segment that crosses the partition wall 106 when the line segment connects the centers of gravity of adjacent cells 104 in a cross section perpendicular to the extension direction of the flow channel. The thickness of the partition wall 106 refers to the average value of the thicknesses of all the partition walls 106. In this specification, the cell density is a value obtained by dividing the number of cells by the area of ​​one end face of the honeycomb structure part (the total area of ​​the partition walls 106 and the cells 104 excluding the outer peripheral wall 103). In this specification, the cell pitch refers to a value calculated by the following calculation. First, the area per cell is calculated by dividing the area of ​​one end face of the honeycomb structure (the total area of ​​the partition walls 106 and the cells 104 excluding the outer peripheral wall 103) by the number of cells. Next, the square root of the area per cell is calculated, and this is defined as the cell pitch. In this specification, the aperture ratio of the cells 104 is a value obtained by dividing the total area of ​​the cells 104 partitioned by the partition walls 106 in a cross section perpendicular to the extension direction of the flow paths of the honeycomb structure section, by the area of ​​one end face (the total area of ​​the partition walls 106 and the cells 104 excluding the outer peripheral wall 103). Note that when calculating the aperture ratio of the cells 104, layers provided on the partition walls 106, such as the electrode layer and the functional material-containing layer, are not taken into consideration.

[0025] In an embodiment advantageous from the viewpoint of carrying a sufficient amount of functional material, the partition wall thickness is 0.180 mm or less, and the cell density is 100 cells / cm 2 In a preferred embodiment, the partition wall thickness is 0.130 mm or less, and the cell density is 70 cells / cm. 2 In a more preferred embodiment, the partition wall thickness is 0.100 mm or less, and the cell density is 65 cells / cm. 2 and the cell pitch is 1.3 mm or more.

[0026] In each of the above embodiments, from the viewpoint of ensuring the strength of the honeycomb structure and keeping the electrical resistance low, the lower limit of the partition wall thickness is preferably 0.010 mm or more, more preferably 0.020 mm or more, and even more preferably 0.030 mm or more. In each of the above embodiments, in order to ensure the strength of the honeycomb structure, to keep the electrical resistance low, and to increase the surface area to promote reaction, adsorption, and desorption by the functional material, the lower limit of the cell density is set to 30 cells / cm. 2 Preferably, 35 cells / cm or more. 2 More preferably, 40 cells / cm or more. 2 It is even more preferable that the above is true. In each of the above embodiments, from the viewpoints of ensuring the strength of the honeycomb structure, maintaining low electrical resistance, and increasing the surface area to promote reaction, adsorption, and separation by the functional material, the upper limit of the cell pitch is preferably 2.0 mm or less, more preferably 1.8 mm or less, and even more preferably 1.6 mm or less.

[0027] In an embodiment advantageous from the viewpoint of achieving both a reduction in pressure loss and a maintenance of strength, the thickness of the partition wall is 0.08 mm or more and 0.36 mm or less, and the cell density is 2.54 cells / cm 2 More than 140 cells / cm 2 In a preferred embodiment, the thickness of the partition wall is 0.09 mm or more and 0.35 mm or less, and the cell density is 15 cells / cm. 2 More than 100 cells / cm 2 In a more preferred embodiment, the thickness of the partition wall is 0.10 mm or more and 0.30 mm or less, and the cell density is 20 cells / cm. 2 More than 90 cells / cm 2 Hereinafter, the cell aperture ratio is 0.77 or more.

[0028] In each of the above-mentioned embodiments, from the viewpoint of ensuring the strength of the honeycomb structure portion, the upper limit of the cell opening ratio is preferably 0.94 or less, more preferably 0.92 or less, and even more preferably 0.90 or less.

[0029] The thickness of the outer peripheral wall 103 is not particularly limited, but is preferably determined based on the following viewpoints. First, from the viewpoint of reinforcing the honeycomb structure, the thickness of the outer peripheral wall 103 is preferably 0.05 mm or more, more preferably 0.06 mm or more, and even more preferably 0.08 mm or more. On the other hand, from the viewpoint of increasing the electrical resistance to suppress the initial current, and from the viewpoint of reducing the pressure loss when air flows, the thickness of the outer peripheral wall 103 is preferably 1.0 mm or less, more preferably 0.5 mm or less, even more preferably 0.4 mm or less, and even more preferably 0.3 mm or less. In this specification, the thickness of the outer peripheral wall 103 refers to the length in the normal direction of the outer peripheral surface from the boundary between the outer peripheral wall 103 and the outermost cell 104 or partition wall 106 to the outer peripheral surface of the honeycomb structure section in a cross section perpendicular to the extension direction of the flow path.

[0030] The length of the honeycomb structure in the flow path extension direction and the cross-sectional area perpendicular to the flow path extension direction may be adjusted according to the required size of the heater element, and are not particularly limited. For example, when used in a compact heater element while ensuring a predetermined function, the honeycomb structure has a length in the flow path extension direction of 2 to 50 mm, typically 5 to 50 mm, and a cross-sectional area perpendicular to the flow path extension direction of 30 to 400 cm. 2 , typically 50-150 cm 2 It can be said that:

[0031] The partition walls 106 constituting the honeycomb structure are made of a material capable of generating heat when electricity is applied, specifically, made of a material having a PTC (Positive Temperature Coefficient) characteristic. If necessary, the outer peripheral wall 103 may also be made of a material having a PTC characteristic like the partition walls 106.

[0032] When a functional material-containing layer is provided on the partition wall 106, it is possible to heat the functional material-containing layer by heat transfer from the partition wall 106 (and the outer peripheral wall 103, if necessary). In addition, a material having a PTC characteristic has a property that when the temperature rises and exceeds the Curie point, the resistance value rises suddenly and it becomes difficult for electricity to flow. Therefore, when the heater element 100 becomes hot, the partition wall 106 (and the outer peripheral wall 103, if necessary) limits the current flowing therethrough, thereby suppressing excessive heat generation of the heater element 100. Therefore, it is also possible to suppress thermal deterioration of the functional material-containing layer caused by excessive heat generation.

[0033] The lower limit of the volume resistivity of the material having the PTC characteristics at 25°C is preferably 0.5 Ω·cm or more, more preferably 1 Ω·cm or more, even more preferably 5 Ω·cm or more, and even more preferably 10 Ω·cm or more, from the viewpoint of obtaining a suitable heat generation. The upper limit of the volume resistivity of the material having the PTC characteristics at 25°C is preferably 30 Ω·cm or less, preferably 20 Ω·cm or less, more preferably 18 Ω·cm or less, and even more preferably 16 Ω·cm or less, from the viewpoint of generating heat at a low driving voltage. Therefore, the range of the volume resistivity of the material having the PTC characteristics at 25°C can be, for example, 10 Ω·cm or more and 30 Ω·cm or less. In this specification, the volume resistivity of the material having the PTC characteristics at 25°C is measured according to JIS K6271:2008.

[0034] From the viewpoint of being able to generate heat when electricity is applied and having PTC characteristics, the outer peripheral wall 103 and the partition wall 106 are preferably made of a material mainly composed of barium titanate (BaTiO3), and more preferably made of ceramics composed of a material mainly composed of barium titanate (BaTiO3)-based crystal particles in which part of Ba is replaced with a rare earth element. In this specification, the term "main component" means a component that accounts for more than 50 mass% of the total components. The content of BaTiO3-based crystal particles can be determined by fluorescent X-ray analysis. Other crystal particles can also be measured in the same manner.

[0035] The composition formula of BaTiO3-based crystal particles in which part of Ba is replaced by rare earth elements is (Ba 1-x A x )TiO3, where A represents one or more rare earth elements and 0.0001≦x≦0.010. A is not particularly limited as long as it is a rare earth element, but is preferably one or more selected from the group consisting of La, Ce, Pr, Nd, Eu, Gd, Dy, Ho, Er, Y and Yb, and more preferably La. x is preferably 0.001 or more, more preferably 0.0015 or more, from the viewpoint of suppressing the electrical resistance at room temperature from becoming too high. On the other hand, x is preferably 0.009 or less, from the viewpoint of suppressing the electrical resistance at room temperature from becoming too high due to insufficient sintering.

[0036] The content of BaTiO3-based crystal particles in the ceramics, in which a portion of Ba has been replaced with a rare earth element, is not particularly limited as long as it is the amount that serves as the main component, but is preferably 90 mass% or more, more preferably 92 mass% or more, and even more preferably 94 mass% or more. The upper limit of the content of BaTiO3-based crystal particles is not particularly limited, but is generally 99 mass% or less, preferably 98 mass% or less.

[0037] From the viewpoint of reducing the environmental load, it is desirable that the material used for the outer peripheral wall 103 and the partition wall 106 does not substantially contain lead (Pb). Specifically, the Pb content of the outer peripheral wall 103 and the partition wall 106 is preferably 0.01 mass% or less, more preferably 0.001 mass% or less, and even more preferably 0 mass%. With a low Pb content, for example, air heated by contacting the partition wall 106 during heat generation can be safely applied to living organisms such as humans. Note that the Pb content of the outer peripheral wall 103 and the partition wall 106, calculated as PbO, is preferably less than 0.03 mass%, more preferably less than 0.01 mass%, and even more preferably 0 mass%. The lead content can be determined by ICP-MS (inductively coupled plasma mass spectrometry).

[0038] The lower limit of the Curie point of the material constituting the outer peripheral wall 103 and the partition wall 106 is preferably 100° C. or higher, more preferably 110° C. or higher, and even more preferably 125° C. or higher, from the viewpoint of efficient heating of air. The upper limit of the Curie point is preferably 250° C. or lower, more preferably 225° C. or lower, even more preferably 200° C. or lower, even more preferably 150° C. or lower, and even more preferably 130° C. or lower, from the viewpoint of safety as a part placed inside a room, particularly in the vehicle compartment or in the vicinity of the vehicle compartment. Therefore, the Curie point range of the material constituting the outer peripheral wall 103 and the partition wall 106 can be, for example, 100° C. or higher and 130° C. or lower.

[0039] The Curie point of the material constituting the outer peripheral wall 103 and the partition walls 106 can be adjusted by the type and amount of the shifter added. For example, the Curie point of barium titanate (BaTiO3) is about 120°C, but by substituting a part of Ba and Ti with one or more of Sr, Sn, and Zr, the Curie point can be shifted to the lower temperature side.

[0040] In this specification, the Curie point is measured by the following method. A sample is attached to a sample holder for measurement and placed in a measurement tank (e.g., MINI-SUBZERO MC-810P, manufactured by Espec Corporation), and the change in electrical resistance of the sample relative to the temperature change when the temperature is raised from 10°C is measured using a DC resistance meter (e.g., multimeter 3478A, manufactured by Yokogawa Hewlett Packard, Ltd.). The temperature at which the resistance value is twice the resistance value at room temperature (20°C) based on the electrical resistance-temperature plot obtained by the measurement is taken as the Curie point.

[0041] (1-2. Electrode layer) The first electrode layer 102a is provided on the first end face 101a, and the second electrode layer 102b is provided on the second end face 101b. By applying a voltage between the first electrode layer 102a and the second electrode layer 102b, it becomes possible to generate heat in the honeycomb structure portion by Joule heat.

[0042] Specifically, the first electrode layer 102a covers a part or the whole of the surface of the partition wall 106 forming the first end face 101a. The second electrode layer 102b covers a part or the whole of the surface of the partition wall 106 forming the second end face 101b. In order to easily spread the current over the entire first end face 101a, the first electrode layer 102a preferably covers 80% or more, more preferably covers 90% or more, and even more preferably covers 99% or more of the area of ​​the portion of the first end face 101a excluding the opening of the cell 104 (partition wall portion and outer peripheral wall portion). Similarly, in order to easily spread the current over the entire second end face 101b, the second electrode layer 102b preferably covers 80% or more, more preferably covers 90% or more, and even more preferably covers 99% or more of the area of ​​the portion of the second end face 101b excluding the opening of the cell 104 (partition wall portion and outer peripheral wall portion).

[0043] The first electrode layer 102a and the second electrode layer 102b are not particularly limited, and may be, for example, a metal or alloy containing at least one selected from Cu, Ag, Al, Ni, and Si. In a preferred embodiment, the first electrode layer 102a and the second electrode layer 102b contain pure aluminum and / or an aluminum alloy. An ohmic electrode capable of making ohmic contact with the outer peripheral wall 103 and / or the partition wall 106 having PTC characteristics may also be used. The ohmic electrode may be, for example, an ohmic electrode containing at least one selected from Al, Au, Ag, and In as a base metal and at least one selected from Ni, Si, Zn, Ge, Sn, Se, and Te for n-type semiconductors as a dopant. The first electrode layer 102a and the second electrode layer 102b may have a single-layer structure or a laminated structure of two or more layers. When the first electrode layer 102a and the second electrode layer 102b have a laminated structure of two or more layers, the materials of the layers may be the same or different. In a preferred embodiment, the first electrode layer 102a and the second electrode layer 102b have a single layer of pure aluminum, a two-layer structure of an Al-Ni alloy layer and a pure silver layer, or a two-layer structure of an Al-Ni alloy layer and a pure aluminum layer.

[0044] The thickness of the first electrode layer 102a and the second electrode layer 102b is not particularly limited, and can be appropriately set depending on the method for forming the first electrode layer 102a and the second electrode layer 102b. Examples of the method for forming the first electrode layer 102a and the second electrode layer 102b include metal deposition methods such as sputtering, vapor deposition, electrolytic deposition, and chemical deposition. The electrode layer can also be formed by applying an electrode paste and then baking it, or by thermal spraying. Furthermore, the electrode layer may be formed by joining a metal plate or alloy plate such as a punching metal having a through hole at a position corresponding to the opening of the cell.

[0045] The average thickness of the first electrode layer 102a and the second electrode layer 102b is not limited, but may be, for example, 5 μm or more and 100 μm or less. When the lower limit of the average thickness of the first electrode layer 102a and the second electrode layer 102b is 5 μm or more, preferably 10 μm or more, and more preferably 20 μm or more, an advantage is obtained that abnormal heat generation in the electrode layer can be avoided. When the upper limit of the average thickness of the first electrode layer 102a and the second electrode layer 102b is 100 μm or less, preferably 80 μm or less, and more preferably 60 μm or less, an advantage is obtained that the rigidity of the electrode layer can be suppressed and the electrode layer is less likely to peel off from the end face of the honeycomb structure section.

[0046] The average thickness of the first electrode layer 102a is measured by the following procedure. First, a cross-sectional image of the first electrode layer is obtained at about 50 times magnification using a scanning electron microscope or the like. The cross section is a cross section parallel to the direction in which the flow passage of the honeycomb structure section extends. In the cross-sectional image, as exemplified in the partially enlarged view of FIG. 1B, the first electrode layer is visible for each partition wall, so that for each first electrode layer, the thickness T1 at the center position of the length in the direction perpendicular to the direction in which the flow passage of the partition wall forming the first end face covered by the first electrode layer is measured at two points per cross-sectional image. The thickness direction is a direction parallel to the direction in which the flow passage extends. In this way, a large number of cross-sectional images of the first electrode layer are obtained without bias from the vicinity of the first end face of the heater element, and the thickness T1 of the first electrode layer is measured at 10 or more points in total. The average value of all the measured thicknesses T1 is taken as the average thickness of the first electrode layer. The average thickness of the second electrode layer 102b is also measured by the same procedure.

[0047] The terminals are preferably disposed on the outer periphery. For this reason, the electrode layer is preferably thicker at the connection points with the outer periphery and the terminals, so that the material of the electrode layer melts during bonding, making it possible to secure a sufficient bonding area with the terminals and increase the bonding strength with the terminals. Furthermore, since a sufficient bonding area with the terminals can be secured, it is possible to increase the conductivity between the electrode layer and the terminals. Therefore, it is preferable that the heater element 100 satisfies at least one of the following conditions (1) and (2), and it is more preferable that it satisfies both conditions. (1) The average thickness of first electrode layer 102a at the outer periphery of first end face 101a and at the connection portion with first terminal 109a is greater than the average thickness of first electrode layer 102a in other portions. (2) The average thickness of second electrode layer 102b at the outer periphery of second end face 101b and at the connection portion with second terminal 109b is greater than the average thickness of second electrode layer 102b in other portions.

[0048] The average thickness of the first electrode layer 102a (second electrode layer 102b) at the outer periphery of the first end surface 101a (second end surface 101b) and at the connection point with the first terminal 109a (second terminal 109b) is preferably 1.1 to 2.0 times, and more preferably 1.5 to 1.6 times, the average thickness of the first electrode layer 102a (second electrode layer 102b) in other portions.

[0049] The average thickness of the first electrode layer 102a (second electrode layer 102b) at the outer periphery of the first end face 101a (second end face 101b) and the connection point with the first terminal 109a (second terminal 109b) is not limited, but can be, for example, 5.5 μm or more and 200 μm or less. When the lower limit of the average value is 5.5 μm or more, preferably 11 μm or more, and more preferably 22 μm or more, an advantage is obtained in that good conductive performance can be ensured. When the upper limit of the average value is 200 μm or less, preferably 160 μm or less, and more preferably 120 μm or less, an advantage is obtained in that the openings of the cells 104 are ensured, thereby reducing pressure loss during air blowing.

[0050] The average thickness of the first electrode layer 102a at the outer periphery of the first end face 101a and the connection point with the first terminal 109a is measured by the following procedure. First, a cross-sectional image of the first electrode layer at about 50 times the outer periphery of the first end face and the connection point with the first terminal is obtained by a scanning electron microscope or the like. The cross section is a cross section parallel to the direction in which the flow path of the honeycomb structure part extends. In the cross-sectional image, as exemplified in the partial enlarged view of FIG. 1B, the first electrode layer is visible for each partition wall, so that the thickness T1 at the center position of the length in the direction perpendicular to the direction in which the flow path of the partition wall forming the first end face covered by the first electrode layer extends is measured at two points per cross-sectional image for each first electrode layer at the outer periphery of the first end face and the connection point with the first terminal. The thickness direction is a direction parallel to the direction in which the flow path extends. In this way, a large number of cross-sectional images of the first electrode layer at the outer periphery of the first end face and the connection point with the first terminal are obtained without bias from the vicinity of the first end face of the heater element, and the thickness T1 of the first electrode layer is measured at 10 points or more in total. The average value of all the measured thicknesses T1 is defined as the average thickness of the first electrode layer 102a at the outer periphery of the first end face 101a and at the connection point with the first terminal 109a. The average thickness of the second electrode layer 102b at the outer periphery of the second end face 101b and at the connection point with the second terminal 109b is also measured in the same manner. The definition of the outer periphery will be described later.

[0051] The average value of the thickness of the first electrode layer 102a in the portion other than the outer periphery of the first end face 101a and the connection portion with the first terminal 109a is measured by the following procedure. First, a cross-sectional image of the first electrode layer at about 50 times the magnification of the portion other than the outer periphery of the first end face and the connection portion with the first terminal is obtained by a scanning electron microscope or the like. The cross section is a cross section parallel to the direction in which the flow path of the honeycomb structure portion extends. In the cross-sectional image, as exemplified in the partial enlarged view of FIG. 1B, the first electrode layer is visible for each partition wall, so that for each first electrode layer in the portion other than the outer periphery of the first end face and the connection portion with the first terminal, the thickness T1 at the center position of the length in the direction perpendicular to the direction in which the flow path extends of the partition wall forming the first end face covered by the first electrode layer is measured at two points per cross-sectional image. The thickness direction is a direction parallel to the direction in which the flow path extends. In this way, a large number of cross-sectional images of the first electrode layer in the portion other than the outer periphery of the first end face and the connection portion with the first terminal are obtained without bias from the vicinity of the first end face of the heater element, and the thickness T1 of the first electrode layer is measured at 10 or more points in total. The average value of all the measured thicknesses T1 is set as the average thickness of the first electrode layer 102a in the portion other than the outer periphery of the first end face 101a and the connection portion with the first terminal 109a. The average thickness of the second electrode layer 102b in the portion other than the outer periphery of the second end face 101b and the connection portion with the second terminal 109b is also measured in the same manner. The definition of the outer periphery will be described later.

[0052] As described above, the thicker the electrode layer is at the connection points with the outer periphery and the terminals, the stronger the connection of the terminals to the electrode layer, and the higher the electrical conductivity between the electrode layer and the terminals. On the other hand, in order to increase the degree of freedom of the area where the terminals are connected, it is preferable to increase the thickness of the electrode layer over the entire outer periphery. Therefore, it is preferable for the heater element 100 to satisfy at least one of the following conditions (3) and (4), and it is more preferable for it to satisfy both conditions. (3) The average thickness of the first electrode layer 102a over the entire outer periphery of the first end face 101a is greater than the average thickness of the first electrode layer 102a in other portions. (4) The average thickness of the second electrode layer 102b over the entire outer periphery of the second end face 101b is greater than the average thickness of the second electrode layer 102b in other portions.

[0053] The average thickness of the first electrode layer 102a in the entire outer periphery of the first end face 101a is measured by the following procedure. First, a cross-sectional image of the first electrode layer at about 50 times the size of an arbitrary location in the outer periphery of the first end face is obtained using a scanning electron microscope or the like. The cross section is parallel to the direction in which the flow channels of the honeycomb structure section extend. In the cross-sectional image, the first electrode layer is visible for each partition wall, as exemplified in the partial enlarged view of FIG. 1B, so that for each first electrode layer in the outer periphery of the first end face, the thickness T1 at the center position of the length in the direction perpendicular to the direction in which the flow channels of the partition walls forming the first end face covered by the first electrode layer are measured at two points per cross-sectional image. The thickness direction is parallel to the direction in which the flow channels extend. In this way, cross-sectional images of the first electrode layer in the outer periphery of the first end face are obtained at equal intervals in the circumferential direction from the vicinity of the first end face of the heater element, and the thickness T1 of the first electrode layer is measured at 10 or more points in total. The average value of all the measured thicknesses T1 is defined as the average thickness of the first electrode layer 102a over the entire outer periphery of the first end face 101a. The average thickness of the second electrode layer 102b over the entire outer periphery of the second end face 101b is also measured in the same manner. The definition of the outer periphery will be described later.

[0054] The average value of the thickness of the first electrode layer 102a in the portion other than the outer periphery of the first end face 101a is measured by the following procedure. First, a cross-sectional image of the first electrode layer in the portion other than the outer periphery of the first end face is obtained by a scanning electron microscope or the like at a magnification of about 50 times. The cross section is a cross section parallel to the direction in which the flow path of the honeycomb structure portion extends. In the cross-sectional image, as exemplified in the partial enlarged view of FIG. 1B, the first electrode layer is visible for each partition wall, so that for each first electrode layer in the portion other than the outer periphery of the first end face, the thickness T1 at the center position of the length in the direction perpendicular to the direction in which the flow path of the partition wall forming the first end face covered by the first electrode layer is measured at two points per cross-sectional image. The thickness direction is a direction parallel to the direction in which the flow path extends. In this way, a large number of cross-sectional images of the first electrode layer in the portion other than the outer periphery of the first end face are obtained without bias from the vicinity of the first end face of the heater element, and the thickness T1 of the first electrode layer is measured at 10 points or more in total. The average value of all the measured thicknesses T1 is defined as the average thickness of the first electrode layer 102a in the portion other than the outer periphery of the first end face 101a. The average thickness of the second electrode layer 102b in the portion other than the outer periphery of the second end face 101b is also measured in the same manner. The definition of the outer periphery will be described later.

[0055] The lower limit of the volume resistivity of the first electrode layer 102a and the second electrode layer 102b at 25° C. is not particularly limited, but the normally achievable range is 1.0×10 -7 The upper limit of the volume resistivity of the first electrode layer 102a and the second electrode layer 102b at 25° C. is 1.0×10 -5 It is preferable that the resistance is Ω·cm or less, and 1.0×10 -6 It is preferable that the resistance is 5.0×10 -7 More preferably, it is 3.0×10 -7 It is more preferable that the volume resistivity of the first electrode layer 102a and the second electrode layer 102b at 25° C. is in the range of, for example, 1.0×10 -7 Ω cm or more 1.0×10 -5In this specification, the volume resistivity at 25° C. of the first electrode layer 102a and the second electrode layer 102b is measured in accordance with JIS K6271:2008.

[0056] (1-3. First and second functional material-containing layers) The first functional material-containing layer 107a may cover a part of the outer surface of the first electrode layer 102a, and the second functional material-containing layer 107b may cover a part of the outer surface of the second electrode layer 102b. The functional material-containing layer may be present on the end surface side of the heater element, thereby imparting the function of the functional material to the heater element. For example, when the first functional material-containing layer 107a and the second functional material-containing layer 107b contain a moisture absorbent, it is possible to suppress the migration of metal components in the electrode layers and the short circuit between the electrode layers. The outer surface of the first electrode layer 102a refers to the surface opposite to the surface where the first electrode layer 102a contacts the first end surface 101a. The outer surface of the second electrode layer 102b refers to the surface opposite to the surface where the second electrode layer 102b contacts the second end surface 101b.

[0057] The reason why the first functional material-containing layer 107a covers a "part" of the outer surface of the first electrode layer 102a is that the part of the outer surface of the first electrode layer 102a to which the first terminal 109a is connected should not be covered by the first functional material-containing layer 107a, and therefore does not cover the entirety. Similarly, the reason why the second functional material-containing layer 107b covers a "part" of the outer surface of the second electrode layer 102b is that the part of the outer surface of the second electrode layer 102b to which the second terminal 109b is connected should not be covered by the second functional material-containing layer 107b, and therefore does not cover the entirety.

[0058] In order to improve the performance of the functional material, the first functional material-containing layer 107a preferably covers 80% or more, more preferably covers 90% or more, and even more preferably covers 99% or more of the area of ​​the outer surface of the first electrode layer 102a where the first terminal 109a is not connected. Similarly, the second functional material-containing layer 107b preferably covers 80% or more, more preferably covers 90% or more, and even more preferably covers 99% or more of the area of ​​the outer surface of the second electrode layer 102b where the second terminal 109b is not connected.

[0059] The first functional material-containing layer 107a and the second functional material-containing layer 107b are preferably insulating. Foreign flying objects are likely to adhere to the vicinity of the first end face 101a and the vicinity of the second end face 101b, and if the flying objects are conductive, they may cause a short circuit. By making the first functional material-containing layer 107a and the second functional material-containing layer 107b insulating, it is possible to prevent a short circuit caused by the flying objects. In this specification, the first functional material-containing layer 107a and the second functional material-containing layer 107b being insulating means that the first functional material-containing layer 107a and the second functional material-containing layer 107b each satisfy the following conditions regarding electrical resistance.

[0060] The coordinate value of the center of gravity O of the first end surface 101a (second end surface 101b) is set to 0, the coordinate axis is set in the direction from the center of gravity O toward the outer peripheral contour C of the first end surface 101a (second end surface 101b), and the coordinate value at the outer peripheral contour C is set to 1.00R. Then, the electrical resistance at 25°C between two points on the outer surface of the first functional material-containing layer 107a (second functional material-containing layer 107b) that are the furthest apart between the line segment connecting the center of gravity O and an arbitrary point D with a coordinate value of 0.90R is measured by a shunt method (see FIG. 1A). The outer surface of the first functional material-containing layer 107a (second functional material-containing layer 107b) refers to the surface opposite to the surface where the first functional material-containing layer 107a (second functional material-containing layer 107b) contacts the first electrode layer 102a (second electrode layer 102b). Next, the point D is rotated 30° around the center of gravity O, and the electrical resistance is measured in the same manner. In this way, the electrical resistance between the center of gravity O and point D is measured around the circumference (12 points) while rotating point D by 30°. The lower limit of the electrical resistance at the 12 points obtained is 1.0×10 4 When the resistance is Ω or more, the first functional material-containing layer 107a (second functional material-containing layer 107b) is defined as being insulating. In addition, if the first terminal 109a (second terminal 109b) is present between the line segment connecting the point D to the center of gravity O, point D is further rotated and moved to a position where the first terminal 109a (second terminal 109b) is not present, and then measurement is performed.

[0061] The first functional material-containing layer 107a and the second functional material-containing layer 107b have a lower limit of electrical resistance of 1.0×10 5 Ω or more is preferable, and 5.0×10 5 The upper limit of the electrical resistance is not particularly set for the first functional material-containing layer 107a and the second functional material-containing layer 107b, but the range of electrical resistance when the electrical resistance is measured according to the above procedure is 1.0×10 5 Ω~1.0×10 7 Ω, usually 2.0×10 5 Ω~1.0×10 6 A typical example is Ω.

[0062] The first functional material-containing layer 107a and the second functional material-containing layer 107b preferably contain a moisture-absorbing material. In this specification, the moisture-absorbing material refers to a substance that has the property of being able to adsorb 5 g / g or more of water mass (g) per 1 g of its dry mass when left for one hour in an environment of room temperature (25°C) and relative humidity of 50%. The moisture-absorbing material preferably has a function of being able to adsorb moisture at -20 to 40°C and desorb it at a high temperature of 60°C or higher, preferably 70 to 180°C. In this way, when the moisture-absorbing material has the function of adsorbing moisture at a low temperature and desorbing it at a high temperature, the moisture-absorbing material can be used many times by repeatedly applying and de-applying electricity.

[0063] The type of moisture absorbent is not particularly limited, but examples thereof include silica gel, sepiolite, calcium oxide, diatomaceous earth, activated carbon, activated clay, zeolite, white carbon, calcium chloride, magnesium chloride, potassium acetate, dibasic sodium phosphate, sodium citrate, water-absorbing polymers, crystalline aluminum silicate, and amorphous aluminum silicate. Among these, zeolite and amorphous aluminum silicate are preferred, and amorphous aluminum silicate is more preferred, because they can release moisture in a relatively low temperature range. One type of moisture absorbent may be used alone, or two or more types may be used in combination. The above moisture absorbents are examples and are not limited to these.

[0064] The first functional material-containing layer 107a and the second functional material-containing layer 107b may contain a binder. Examples of binders include both organic binders and inorganic binders, but inorganic binders are preferred. There are no particular limitations on the type of inorganic binder, but examples include alumina sol, silica sol, montmorillonite, boehmite, gamma alumina, and attapulgite. These may be used alone or in combination of two or more types. Among these, alumina sol and silica sol are preferred, and silica sol is more preferred, because they are easy to ensure adhesive strength.

[0065] The first functional material-containing layer 107a and the second functional material-containing layer 107b may contain a functional material having a function of adsorbing components to be removed in the air, such as carbon dioxide and / or organic gas components, in addition to or instead of the moisture absorbent. In particular, it is preferable to contain a functional material having a function of adsorbing carbon dioxide and / or organic gas components at -20 to 40°C and desorbing them at a high temperature of 60°C or higher, preferably 70 to 180°C. In this way, when the functional material has the function of adsorbing components to be removed in the air at low temperatures and desorbing them at high temperatures, the functional material can be used many times by repeatedly applying and de-energizing it.

[0066] Organic gas components contained in the air that can be the subject of removal include, for example, volatile organic compounds (VOCs), odor components, etc. Specific examples of harmful volatile components include ammonia, acetic acid, isovaleric acid, nonenal, formaldehyde, toluene, xylene, paradichlorobenzene, ethylbenzene, styrene, chlorpyrifos, di-n-butyl phthalate, tetradecane, di-2-ethylhexyl phthalate, diazinon, acetaldehyde, N-methylcarbamate-2-(1-methylpropyl)phenyl, etc.

[0067] Some of the above-mentioned moisture absorbents have both of these functions, and the description will be repeated, but examples of the types of functional materials include zeolite, silica gel, activated carbon, alumina, silica, low-crystalline clay, and amorphous aluminum silicate complexes. The type of functional material may be appropriately selected depending on the type of components to be removed. The functional materials may be used alone or in combination of two or more types.

[0068] The first functional material-containing layer 107a and the second functional material-containing layer 107b may further contain a catalyst for the purpose of purifying the components to be removed or enhancing the function of the functional material (including the moisture absorbent) to capture the components to be removed. The catalyst preferably has a function capable of promoting an oxidation-reduction reaction. Examples of catalysts having such a function include metal catalysts such as Pt, Pd, and Ag, and oxide catalysts such as CeO2 and ZrO2. The catalyst may be used alone or in combination of two or more types.

[0069] The average thickness of at least one of the first functional material-containing layer 107a and the second functional material-containing layer 107b, preferably both, is not limited, but can be, for example, 10 μm or more and 500 μm or less. By setting the lower limit of the average thickness of at least one of the first functional material-containing layer 107a and the second functional material-containing layer 107b, preferably both, to 10 μm or more, preferably 30 μm or more, more preferably 50 μm or more, the advantage is that insulation can be ensured and the function of the functional material can be easily exerted. By setting the upper limit of the average thickness of the first functional material-containing layer 107a and the second functional material-containing layer 107b to 500 μm or less, preferably 300 μm or less, more preferably 200 μm or less, the advantage is that the rigidity of the functional material-containing layer can be reduced and it is difficult to peel off.

[0070] The average thickness of the first functional material-containing layer 107a is measured by the following procedure. First, a cross-sectional image of the first functional material-containing layer is obtained at about 50 times magnification using a scanning electron microscope or the like. The cross section is a cross section parallel to the direction in which the flow channels of the honeycomb structure section extend. In the cross-sectional image, as illustrated in the partially enlarged view of FIG. 1B, the first functional material-containing layer is visually recognized for each partition wall, so that for each first functional material-containing layer, the thickness T2 at the center position of the length in the direction perpendicular to the direction in which the flow channels extend of the partition wall forming the first end face indirectly covered by the first functional material-containing layer is measured at two points per cross-sectional image. The thickness direction is a direction parallel to the direction in which the flow channels extend. Then, a large number of cross-sectional images of the first functional material-containing layer are obtained without bias from the vicinity of the first end face of the heater element, and the thickness T2 of the first functional material-containing layer is measured at 10 or more points. The average value of all the measured thicknesses T2 is taken as the average thickness of the first functional material-containing layer. The average thickness of the second functional material-containing layer 107b is also measured by the same procedure.

[0071] The first functional material-containing layer 107a preferably covers not only the outer surface of the first electrode layer 102a but also a part or the whole of other exposed surfaces of the first electrode layer 102a (e.g., surfaces parallel to the thickness direction of the first electrode layer 102a), and more preferably covers the whole. Similarly, the second functional material-containing layer 107b preferably covers not only the outer surface of the second electrode layer 102b but also a part or the whole of other exposed surfaces of the second electrode layer 102b (e.g., surfaces parallel to the thickness direction of the second electrode layer 102b), and more preferably covers the whole.

[0072] (1-4. Terminals) The first terminal 109a is connected to the outer surface of the first electrode layer 102a (when the first functional material-containing layer 107a is provided, it is preferably a portion of the outer surface of the first electrode layer 102a that is not covered by the first functional material-containing layer 107a). The second terminal 109b is connected to the outer surface of the second electrode layer 102b (when the second functional material-containing layer 107b is provided, it is preferably a portion of the outer surface of the second electrode layer 102b that is not covered by the second functional material-containing layer 107b). It is preferable that at least a portion of the first terminal 109a (second terminal 109b) is disposed on the outer periphery of the first end face 101a (second end face 101b), and it is more preferable that the entire terminal is disposed on the outer periphery.

[0073] The method of connection between the first electrode layer 102a and the first terminal 109a, and between the second electrode layer 102b and the second terminal 109b is not particularly limited as long as they are conductive, and can be connected by, for example, welding, brazing, or mechanical contact. The material of the first terminal 109a and the second terminal 109b is not particularly limited, and can be, for example, a metal. As the metal, a simple metal or an alloy can be adopted, but from the viewpoint of selecting a material that is difficult to oxidize in a humid environment, difficult to cause migration or electrolytic corrosion even under wet conditions, and easy to join with the electrode, it is preferable to contain one or more types selected from pure aluminum, aluminum alloy, and stainless steel, and for example, it can be made of pure aluminum, aluminum alloy, or stainless steel. In addition, an alloy containing at least one type selected from the group consisting of Cr, Fe, Co, Ni, Cu, and Ti can also be used, and among them, Fe-Ni alloy and phosphor bronze can be suitably used. It is preferable that the terminal is made of a material similar to that of the electrode layer on the end face from the viewpoint of avoiding electrolytic corrosion. For example, it is preferable that both the electrode layer and the terminal are made of pure aluminum and / or aluminum alloy.

[0074] The shape of the first terminal 109a and the second terminal 109b is not limited, but may be, for example, a flat plate shape. In this case, the plate thickness of the terminal is not limited, but may be, for example, 0.1 to 4 mm, and is preferably 0.3 to 2 mm.

[0075] Since the first terminal 109a is connected to the first electrode layer 102a, there is no particular limit to the area of ​​the portion of the first end face 101a that is (indirectly) covered by the first terminal 109a. However, if the first terminal 109a is too small, it becomes difficult to connect a current-carrying component to the first terminal 109a. Conversely, if the first terminal 109a is too large, the area that blocks the opening of the cell 104 becomes large, and the flow rate of air that can be passed through the heater element 100 decreases. Therefore, the lower limit of the ratio of the area of ​​the first end face 101a covered by the first terminal 109a to the area of ​​the first end face 101a is preferably 0.5% or more, more preferably 1% or more, and even more preferably 2% or more. Moreover, the upper limit of the ratio of the area of ​​the first end face 101a covered by the first terminal 109a to the area of ​​the first end face 101a is preferably 10% or less, more preferably 8% or less, and even more preferably 5% or less. Therefore, the ratio of the area of ​​first end face 101a covered by first terminal 109a to the area of ​​first end face 101a can be in the range of, for example, 0.5% to 10%. The same applies to the ratio of the area of ​​second end face 101b covered by second terminal 109b to the area of ​​second end face 101b.

[0076] The lower limit of the volume resistivity of the first terminal 109a and the second terminal 109b at 25° C. is not particularly limited, but the normally achievable range is 1.0×10 -7 The upper limit of the volume resistivity of the first terminal 109a and the second terminal 109b at 25° C. is 1.0×10 -6 It is preferable that the resistance is 5.0×10 -7 It is preferable that the resistance is Ω·cm or less, and 3.0×10 -7 It is more preferable that the resistance is 2.0×10 -7 Therefore, the range of the volume resistivity of the first terminal 109a and the second terminal 109b at 25° C. is, for example, 1.0×10 -7 Ω cm or more 1.0×10 -6In this specification, the volume resistivity of the first terminal 109a and the second terminal 109b at 25° C. is measured in accordance with JIS K6271:2008.

[0077] (1-5. Third and fourth functional material-containing layers) The third functional material-containing layer 111a may cover a part of the outer surface of the first terminal 109a, and the fourth functional material-containing layer 111b may cover a part of the outer surface of the second terminal 109b. The presence of the functional material-containing layer on the outer surface of the terminal can impart the function provided by the functional material to the heater element. For example, when the third functional material-containing layer 111a and the fourth functional material-containing layer 111b contain a moisture absorbent, it is possible to suppress the migration of metal components in the terminal and short-circuiting. The outer surface of the first terminal 109a refers to the surface opposite to the surface where the first terminal 109a contacts the first electrode layer 102a. The outer surface of the second terminal 109b refers to the surface opposite to the surface where the second terminal 109b contacts the second electrode layer 102b.

[0078] The reason why the third functional material-containing layer 111a covers a "part" of the outer surface of the first terminal 109a is that the part of the outer surface of the first terminal 109a to which the current-carrying component 105a is connected should not be covered by the third functional material-containing layer 111a, and therefore does not cover the entirety. Similarly, the reason why the fourth functional material-containing layer 111b covers a "part" of the outer surface of the second terminal 109b is that the part of the outer surface of the second terminal 109b to which the current-carrying component 105b is connected should not be covered by the fourth functional material-containing layer 111b, and therefore does not cover the entirety.

[0079] In order to improve the performance of the functional material, the third functional material-containing layer 111a preferably covers 80% or more, more preferably 90% or more, and even more preferably 99% or more of the area of ​​the outer surface of the first terminal 109a where the current-carrying component 105a is not connected. Similarly, the fourth functional material-containing layer 111b preferably covers 80% or more, more preferably 90% or more, and even more preferably 99% or more of the area of ​​the outer surface of the second terminal 109b where the current-carrying component 105b is not connected.

[0080] The third functional material-containing layer 111a and the fourth functional material-containing layer 111b are preferably insulating for the same reasons as the first functional material-containing layer 107a and the second functional material-containing layer 107b. The third functional material-containing layer 111a and the fourth functional material-containing layer 111b being insulating means that the third functional material-containing layer 111a and the fourth functional material-containing layer 111b each satisfy the following conditions regarding electrical resistance.

[0081] The electrical resistance at 25°C between any two points 3 mm apart on the outer surface of the third functional material-containing layer 111a (fourth functional material-containing layer 111b) is measured by the shunt method. The two points are selected so that the current-carrying component 105a does not exist between the line segment connecting the two points. When measurements are taken at three points by shifting the measurement points, the lower limit of the obtained electrical resistance is 1.0×10 4 When the resistance is Ω or more, the third functional material-containing layer 111a (fourth functional material-containing layer 111b) is defined as being insulating.

[0082] The third functional material-containing layer 111a and the fourth functional material-containing layer 111b have a lower limit of electrical resistance of 1.0×10 5 Ω or more is preferable, and 5.0×10 5 The third functional material-containing layer 111a and the fourth functional material-containing layer 111b do not have a particular upper limit for the electrical resistance, but the range of electrical resistance when the electrical resistance is measured according to the above procedure is 5.0×10 5 Ω~1.0×10 7 Ω is usually 1.0×106 Ω~5.0×10 6 A typical example is Ω.

[0083] The functional materials contained in the third functional material-containing layer 111a and the fourth functional material-containing layer 111b are as described in the first functional material-containing layer 107a and the second functional material-containing layer 107b, including preferred embodiments.

[0084] The third functional material-containing layer 111a and the fourth functional material-containing layer 111b may contain a binder. The binder is as described in the first functional material-containing layer 107a and the second functional material-containing layer 107b, including preferred embodiments.

[0085] The third functional material-containing layer 111a and the fourth functional material-containing layer 111b may further contain a catalyst for the purpose of purifying the components to be removed or enhancing the function of the functional material (including the moisture absorbent) to capture the components to be removed, etc. The catalyst is as described in the explanation of the first functional material-containing layer 107a and the second functional material-containing layer 107b, including the preferred embodiments.

[0086] The average thickness of the third functional material-containing layer 111a and the fourth functional material-containing layer 111b is not limited, but can be, for example, 10 μm or more and 500 μm or less. By setting the lower limit of the average thickness of the third functional material-containing layer 111a and the fourth functional material-containing layer 111b to 10 μm or more, preferably 20 μm or more, and more preferably 30 μm or more, the advantage is obtained that the insulation properties can be ensured and the function of the functional material can be easily exerted. By setting the upper limit of the average thickness of the third functional material-containing layer 111a and the fourth functional material-containing layer 111b to 500 μm or less, preferably 300 μm or less, and more preferably 200 μm or less, the rigidity of the functional material-containing layer can be reduced, and the layer is less likely to peel off.

[0087] The average thickness of the third functional material-containing layer 111a is defined as the average value of thicknesses measured at any five or more points of the third functional material-containing layer using a cross-sectional method conforming to JIS K5600-1-7: 2014. The average thickness of the fourth functional material-containing layer 111b is also measured using the same procedure.

[0088] The third functional material-containing layer 111a preferably covers not only the outer surface of the first terminal 109a but also a part or the whole of other exposed surfaces of the first terminal 109a (for example, surfaces parallel to the plate thickness direction when the first terminal 109a is flat), and more preferably covers the whole. Similarly, the fourth functional material-containing layer 111b preferably covers not only the outer surface of the second terminal 109b but also a part or the whole of other exposed surfaces of the second terminal 109b (for example, surfaces parallel to the plate thickness direction when the second terminal 109b is flat), and more preferably covers the whole.

[0089] (1-6.Fifth functional material containing layer) It is preferable to have a fifth functional material-containing layer 113 that covers a part or all of the surface of the partition walls 106 that form the flow paths inside the cells 104. Since air containing the components to be removed passes through the flow paths inside the cells 104, by covering the surface of the partition walls 106 that form the flow paths with a functional material, it is possible to improve the performance of the functional material for the heater element 100 as a whole.

[0090] In order to improve the performance of the functional material, the fifth functional material-containing layer 113 preferably covers 80% or more, more preferably 90% or more, and even more preferably 99% or more of the surface area of ​​the partition walls 106 that form the flow paths inside the cells 104. The proportion of the surface area of ​​the partition walls 106 that form the flow paths inside the cells 104 that is covered by the fifth functional material-containing layer 113 is measured by the following procedure. (1) A cross section passing through the center of gravity O of the first end surface 101a (second end surface 101b) and parallel to the extension direction of the cells 104 is cut out from the heater element 100. (2) The obtained cross section is imaged, and the ratio of the length of the portion of the partition wall 106 forming the flow path inside the cell 104 in the cell extension direction to the portion of the length covered by the fifth functional material-containing layer 113 is obtained by image analysis. The average value of the ratio measured for all cells 104 in the cross section is regarded as the ratio of the area covered by the fifth functional material-containing layer 113 to the area of ​​the surface of the partition wall 106 forming the flow path inside the cell 104. For the image analysis, a method can be adopted in which the brightness of each pixel constituting the fifth functional material-containing layer and the partition wall is measured on an image obtained by photographing with an optical microscope (magnification 50 times), and the average value is used as a threshold value to perform binarization processing to distinguish the fifth functional material-containing layer and the partition wall regions. The length of the portion of the partition wall covered by the fifth functional material-containing layer is specified, and the ratio of the length of the portion covered by the fifth functional material-containing layer can be obtained by dividing it by the length of the cell (the length of the honeycomb structure).

[0091] The fifth functional material-containing layer 113 is preferably insulating for the same reasons as the first functional material-containing layer 107a and the second functional material-containing layer 107b. The fifth functional material-containing layer 113 being insulating means that the fifth functional material-containing layer 113 satisfies the following conditions. A cross section parallel to the extension direction of the flow channels of the honeycomb structure is cut out from the heater element 100, and the fifth functional material-containing layer 113 covering the surface of the partition wall 106 is exposed. For the surface of the fifth functional material-containing layer 113 covering any one of the cells 104, the electrical resistance at 25°C is measured by a shunt method between any five two points spaced 3 mm apart in the extension direction of the cell 104. If the obtained electrical resistance is 1.0×10 4 When the resistance is Ω or more, the fifth functional material-containing layer 113 covering the cell is defined as having insulating properties. The fifth functional material-containing layers 113 covering other cells can be measured in the same manner, but if it is clear that the material forming the fifth functional material-containing layers 113 is substantially the same, the results will be the same and therefore the measurement may be omitted.

[0092] The fifth functional material-containing layer 113 has a lower limit of electrical resistance of 1.0×105 Ω or more is preferable, and 5.0×10 5 The fifth functional material-containing layer 113 has no particular upper limit on the electrical resistance. However, when the electrical resistance is measured according to the above procedure, the range of the electrical resistance is preferably 5.0×10 5 Ω~1.0×10 7 Ω is usually 1.0×10 6 Ω~5.0×10 6 A typical example is Ω.

[0093] The functional material contained in the fifth functional material-containing layer 113, including the preferred embodiments, is as described in the explanation of the first functional material-containing layer 107a and the second functional material-containing layer 107b.

[0094] The fifth functional material-containing layer 113 may contain a binder. The binder, including the preferred embodiments, is as described in the description of the first functional material-containing layer 107a and the second functional material-containing layer 107b.

[0095] The fifth functional material-containing layer 113 may further contain a catalyst for the purpose of purifying the components to be removed, or for the purpose of enhancing the function of the functional material (including the moisture absorbent) in capturing the components to be removed, etc. The catalyst is as described in the explanation of the first functional material-containing layer 107a and the second functional material-containing layer 107b, including the preferred embodiments.

[0096] The average thickness of the fifth functional material-containing layer 113 is not limited, but can be, for example, 10 μm or more and 500 μm or less. By setting the lower limit of the average thickness of the fifth functional material-containing layer 113 to 10 μm or more, preferably 20 μm or more, and more preferably 30 μm or more, the advantage of easily exerting the function of the functional material is obtained. By setting the upper limit of the average thickness of the fifth functional material-containing layer 113 to 500 μm or less, preferably 300 μm or less, and more preferably 200 μm or less, the opening area of ​​the cells can be kept large, and therefore the advantage of keeping the airflow resistance low is obtained.

[0097] The average thickness of the fifth functional material-containing layer 113 is measured by the following procedure. First, a cross-sectional image of the fifth functional material-containing layer 113 is obtained at about 50 times magnification using a scanning electron microscope or the like. The cross section is parallel to the direction in which the flow channels of the honeycomb structure section extend. In the cross-sectional image, as illustrated in the partially enlarged view of FIG. 1B, two fifth functional material-containing layers 113 sandwiching each partition wall are visible, and the thickness of each fifth functional material-containing layer 113 is calculated by dividing the entire cross-sectional area from the first end face 101a to the second end face 101b of each fifth functional material-containing layer 113 by the length from the first end face 101a to the second end face 101b of the partition wall covered by the fifth functional material-containing layer. Then, a large number of cross-sectional images of the fifth functional material-containing layer 113 are obtained from the heater element without bias, and the thickness of the fifth functional material-containing layer 113 at five or more locations is measured. The average value of all the measured thicknesses of the fifth functional material-containing layer 113 is defined as the average thickness of the fifth functional material-containing layer.

[0098] The above-mentioned classification of the functional material-containing layers into the first to fifth categories is for convenience, and it is not necessary that each layer is formed independently. There is no prohibition on different types of functional material-containing layers being continuous, and there is no prohibition on different types of functional material-containing layers being simultaneously formed in a single process.

[0099] (1-7. Electrically conductive parts) The first terminal 109a and the second terminal 109b can connect the current-carrying components 105a and 105b, respectively. Examples of conductive materials constituting the current-carrying components 105a and 105b include stainless steel, aluminum, aluminum alloy, copper alloy, and copper. The method of connecting the first terminal 109a and the current-carrying component 105a and the second terminal 109b and the current-carrying component 105b is not particularly limited as long as they are conductive, and can be connected by, for example, welding, brazing, mechanical contact, or the like. In one embodiment, the current-carrying components 105a and 105b may be the electric wire itself between the power source and the first terminal 109a (second terminal 109b), that is, a copper wire, a copper alloy wire, an aluminum wire, an aluminum alloy wire, or a stainless steel wire. In another embodiment, the current-carrying components 105a and 105b may be intermediate components that connect the electric wire and the first terminal 109a (second terminal 109b). The interface piece may be connected to the wires by, for example, welding, soldering, brazing, crimping, bolting, or other methods.

[0100] (2. Heater element assembly with end clamping type frame) The heater element according to one embodiment of the present invention is provided as a heater element assembly held by a frame. The protective effect of the frame makes the heater element less susceptible to damage when the heater element is installed in the air passage, and the heater element can be shaped to be easily installed in the air conditioning system while ensuring electrical insulation from surrounding components. Figures 2A and 2B show an example of a heater element assembly including a frame 120 that clamps the heater element 100 from the first end surface 101a side and the second end surface 101b side.

[0101] The frame 120 has a first frame portion 121 and a second frame portion 122 for sandwiching the heater element from the first end face 101a side and the second end face 101b side. The first frame portion is a resin-made first frame portion 121 arranged on the first end face 101a side, and has a flange portion 121b arranged on the outer periphery side of the outer periphery contour C of the first end face 101a, and a holding portion 121a arranged on the inner periphery side of the outer periphery contour C of the first end face 101a and applying pressure to at least a part of the outer periphery of the first end face 101a. The second frame portion 122 is a resin-made second frame portion 122 arranged on the second end face 101b side, and has a flange portion 122b arranged on the outer periphery side of the outer periphery contour C of the second end face 101b, and a holding portion 122a arranged on the inner periphery side of the outer periphery contour C of the second end face 101b and applying pressure to at least a part of the outer periphery of the second end face 101b.

[0102] In this specification, if the coordinate value of the center of gravity O of first end face 101a (second end face 101b) is set to 0, a coordinate axis is drawn in the direction from the center of gravity O toward the outer peripheral contour C of first end face 101a (second end face 101b), and the coordinate value on the outer peripheral contour C is set to 1.00R, the set of points located between 0.90R and 1.00R is defined as the outer periphery of first end face 101a (second end face 101b).

[0103] In one embodiment, the outer shape of the first frame portion 121 (the second frame portion 122) is annular. The specific shape and dimensions of the first frame portion 121 (the second frame portion 122) may be designed to match the shape and dimensions of the first end surface 101a (the second end surface 101b) of the heater element 100.

[0104] The retaining portion 121a (122a) may apply pressure to the first end face 101a (second end face 101b) located on the inner circumferential side of the outer circumferential portion, but if the retaining portion 121a (122a) expands, it will be more likely to impede the flow of air entering and exiting the heater element 100. For this reason, it is preferable that the retaining portion 121a (122a) apply pressure only to the outer circumferential portion of the first end face 101a (second end face 101b).

[0105] Moreover, the area of ​​the portion of the first end face 101a (second end face 101b) to which pressure is applied by the holding portion 121a (122a) is preferably 10% or less of the entire area of ​​the first end face 101a (second end face 101b) from the viewpoint of not impeding the flow of air entering and exiting the heater element 100, more preferably 8% or less, even more preferably 5% or less, even more preferably 2% or less, even more preferably 1.8% or less, and even more preferably 1.6% or less. Moreover, the area of ​​the portion of the first end face 101a (second end face 101b) to which pressure is applied by the holding portion 121a (122a) is preferably 1% or more of the entire area of ​​the first end face 101a (second end face 101b) from the viewpoint of improving the holding performance for the heater element 100, more preferably 1.2% or more, and even more preferably 1.4% or more. Therefore, the ratio of the area of ​​the portion of first end face 101a (second end face 101b) that is subjected to pressure by holding portion 121a (122a) to the entire area of ​​first end face 101a (second end face 101b) can be, for example, 1% or more and 10% or less.

[0106] The upper limit of the width W of the holding portion 121a (122a) is preferably 7 mm or less, more preferably 5 mm or less, and even more preferably 4 mm or less, from the viewpoint of not hindering the flow of gas entering and exiting the heater element 100. The lower limit of the width W of the holding portion 121a (122a) is preferably 1 mm or more, more preferably 2 mm or more, and even more preferably 3 mm or more, from the viewpoint of improving the holding performance for the heater element 100. Therefore, the range of the width W of the holding portion 121a (122a) can be, for example, 1 mm or more and 7 mm or less. Here, the width W of the holding portion 121a (122a) means the length of the holding portion 121a (122a) in the direction from the outer peripheral contour C of the first end face 101a (second end face 101b) toward the center of gravity O of the first end face 101a (second end face 101b).

[0107] It is desirable that the resin constituting at least one of the first frame portion 121 and the second frame portion 122, preferably both, has a certain degree of softness so that the heater element 100 is less likely to be damaged. Therefore, in one embodiment, the resin constituting at least one of the first frame portion 121 and the second frame portion 122, preferably both, has an upper limit of Rockwell hardness measured in accordance with ASTM D785-2008 R15 of preferably 150 HRR or less, more preferably 130 HRR or less, and even more preferably 120 HRR or less. In another embodiment, the resin constituting at least one of the first frame portion 121 and the second frame portion 122, preferably both, has an upper limit of Rockwell hardness measured in accordance with ASTM D785-2008 R15 of preferably 120 HRM or less, more preferably 100 HRM or less, and even more preferably 90 HRM or less. The resin constituting at least one of the first frame portion 121 and the second frame portion 122, and preferably both, can satisfy the condition regarding the upper limit of either the above-mentioned Rockwell hardness HRR or HRM, and it is desirable to satisfy both conditions.

[0108] On the other hand, from the viewpoint of improving the holding performance for the heater element 100, it is desirable that the resin constituting at least one of the first frame portion 121 and the second frame portion 122, preferably both, has a certain degree of hardness. Therefore, in one embodiment, the resin constituting at least one of the first frame portion 121 and the second frame portion 122, preferably both, has a lower limit of Rockwell hardness measured in accordance with ASTM D785-2008 R15 of preferably 70 HRR or more, more preferably 80 HRR or more, and even more preferably 90 HRR or more. In another embodiment, the resin constituting at least one of the first frame portion 121 and the second frame portion 122, preferably both, has a lower limit of Rockwell hardness measured in accordance with ASTM D785-2008 R15 of preferably 40 HRM or more, more preferably 50 HRM or more, and even more preferably 70 HRM or more. The resin constituting at least one of, and preferably both of, the first frame portion 121 and the second frame portion 122 can satisfy the condition regarding the lower limit of either the above-mentioned Rockwell hardness HRR or HRM, and it is desirable to satisfy both conditions.

[0109] Therefore, in one embodiment, the resin constituting at least one of, and preferably both of, the first frame 121 and the second frame 122 has a Rockwell hardness in the range of, for example, 70 HRR to 150 HRR, as measured in accordance with ASTM D785-2008 R15. In another embodiment, the resin constituting at least one of, and preferably both of, the first frame 121 and the second frame 122 has a Rockwell hardness in the range of, for example, 40 HRM to 120 HRM.

[0110] There are no particular limitations on the type of resin constituting the first frame portion 121 and the second frame portion 122, but from the standpoint of heat resistance, it is preferable that the resin constituting at least one, and preferably both, of the first frame portion 121 and the second frame portion 122 contains one or both of polyether ether ketone (PEEK) and polybutylene terephthalate (PBT), and it is more preferable that the resin contains a total of 80 mass% or more of polyether ether ketone (PEEK) and polybutylene terephthalate (PBT), even more preferable that the resin contains 90 mass% or more, and may contain 100 mass%.

[0111] The resin constituting the first frame portion 121 and the second frame portion 122 is desirably heat resistant. Therefore, the resin constituting at least one of the first frame portion 121 and the second frame portion 122, preferably both, has a lower limit of a deflection temperature under load measured in accordance with JIS K7191-1:2015 of preferably 145°C or more, more preferably 160°C or more, and even more preferably 180°C or more. The upper limit of the deflection temperature under load is not particularly set, but from the viewpoint of availability, it is usually 300°C or less, typically 250°C or less. Therefore, the resin constituting at least one of the first frame portion 121 and the second frame portion 122, preferably both, has a deflection temperature under load in the range of, for example, 145°C or more and 300°C or less.

[0112] The resin constituting the first frame portion 121 and the second frame portion 122 desirably has a high melting point so as not to melt when heated. Therefore, the lower limit of the melting point of the resin constituting at least one of the first frame portion 121 and the second frame portion 122, preferably both, is preferably 250°C or higher, more preferably 280°C or higher, and even more preferably 300°C or higher. There is no particular upper limit for the melting point, but from the viewpoint of availability, it is usually 400°C or lower, typically 350°C or lower. Therefore, the melting point of the resin constituting at least one of the first frame portion 121 and the second frame portion 122, preferably both, is in the range of, for example, 250°C or higher and 400°C or lower.

[0113] In this specification, the melting point of a resin refers to the minimum temperature at which an endothermic peak due to melting is observed when TG-DTA (thermogravimetry-differential thermal analysis) measurement is carried out.

[0114] The resin constituting the first frame portion 121 and the second frame portion 122 desirably has a low thermal conductivity in order to reduce heat loss. Therefore, the resin constituting at least one of the first frame portion 121 and the second frame portion 122, preferably both, has an upper limit of thermal conductivity at 25°C measured in accordance with JIS R1611:2010 of preferably 0.5 W / m / K or less, more preferably 0.3 W / m / K or less, and even more preferably 0.2 W / m / K or less. The lower limit of the thermal conductivity is not particularly set, but from the viewpoint of availability, it is usually 0.1 W / m / K or more, typically 0.15 W / m / K or more. Therefore, the resin constituting at least one of the first frame portion 121 and the second frame portion 122, preferably both, has a thermal conductivity range of, for example, 0.1 W / m / K or more and 0.5 W / m / K or less.

[0115] In order to prevent short circuits, the resin constituting the first frame portion 121 and the second frame portion 122 is preferably insulating. Therefore, the resin constituting at least one of the first frame portion 121 and the second frame portion 122, and preferably both of them, has a lower limit of volume resistivity of 1.0×10 at 25° C. as measured in accordance with the bridge method of JIS C2139:2008. 16 It is preferable that the resistance is Ω·cm or more, and 2.0×10 16 It is preferable that the resistance is 5.0×10 Ω·cm or more. 16 It is more preferable that the volume resistivity is Ω·cm or more. Although there is no particular upper limit for the volume resistivity, from the viewpoint of availability, it is usually 1.0×10 18 Ω cm or less, typically 1.0×10 17 Therefore, the volume resistivity of the resin constituting at least one of the first frame portion 121 and the second frame portion 122, and preferably both of them, is in the range of, for example, 1.0×10 16 Ω cm or more 1.0×10 18Ω·cm or less.

[0116] The holding portion 121a (122a) may apply pressure directly to the first end face 101a (second end face 101b), but it is preferable to apply pressure indirectly via the buffer material 127. By the holding portion 121a (122a) applying pressure indirectly to the first end face 101a (second end face 101b) via the buffer material 127, the first end face 101a (second end face 101b) is less likely to be damaged. In addition, the buffer material 127 deforms in response to the thermal deformation of the heater element 100, and can also relieve thermal stress. This makes it possible to suppress the occurrence of cracks in the heater element 100.

[0117] The thickness of the cushioning material 127 compressed by receiving pressure from the holding portion 121a (122a) in the compression direction is preferably 0.5 mm or more, more preferably 1.0 mm or more, and even more preferably 2.0 mm or more, from the viewpoint of ensuring a deformation margin for obtaining a sufficient cushioning effect. The thickness of the cushioning material 127 compressed by receiving pressure from the holding portion 121a (122a) in the compression direction is preferably 7.0 mm or less, more preferably 5.0 mm or less, and even more preferably 4.0 mm or less, because it is necessary to ensure the holding surface pressure of the heater element and hold the heater element without destroying it. Therefore, the range of the thickness of the cushioning material 127 compressed by receiving pressure from the holding portion 121a (122a) in the compression direction can be, for example, 0.5 mm or more to 7.0 mm or less.

[0118] The lower limit of the pressure that the buffer material 127 receives from the holding portion 121a (122a) is preferably 0.002 MPa or more, and more preferably 0.005 MPa or more. The upper limit of the pressure that the buffer material 127 receives from the holding portion 121a (122a) is preferably 0.2 MPa or less, and more preferably 0.1 MPa or less. Therefore, the pressure that the buffer material 127 receives from the holding portion 121a (122a) is preferably, for example, 0.002 MPa to 0.2 MPa, and more preferably 0.005 MPa to 0.1 MPa. The pressure that the buffer material 127 receives from the holding portion 121a (122a) is calculated from the Young's modulus and the amount of displacement of the buffer material 127.

[0119] From the viewpoint of ensuring the holding surface pressure against the honeycomb heater element, the Young's modulus of the buffer material 127 is preferably at least 0.05 MPa, more preferably at least 0.06 MPa, and even more preferably at least 0.1 MPa. From the viewpoint of ensuring a deformation allowance for obtaining a sufficient buffer effect, the Young's modulus of the buffer material 127 is preferably at most 0.3 MPa, more preferably at most 0.25 MPa, and even more preferably at most 0.2 MPa. Therefore, the range of the Young's modulus of the buffer material 127 can be, for example, at least 0.05 MPa and not more than 0.3 MPa.

[0120] The Young's modulus of the cushioning material 127 is determined from the relationship between the surface pressure and the change in thickness (amount of displacement) when a sheet-like cushioning material is compressed by gradually applying a surface pressure.

[0121] There is no particular restriction on the type of material constituting the buffer material 127, but from the viewpoint of ensuring sufficient deformation, it is preferably made of rubber, and more preferably made of rubber sponge. Sponge means a porous body. Rubber and rubber sponge can contain various rubbers such as natural rubber, styrene-butadiene rubber, butadiene rubber, chloroprene rubber, ethylene-propylene rubber, butyl rubber, fluororubber, acrylonitrile-butadiene rubber, silicone rubber, isoprene rubber, urethane rubber, chlorosulfonated polyethylene, hydrogenated nitrile rubber, epichlorohydrin rubber, acrylic rubber, ethylene acrylic rubber, and norbornene rubber, and these may be contained alone or in a mixture of two or more types. Among these, it is more preferable that the buffer material 127 is made of silicone rubber sponge containing silicone rubber as the main component (preferably 60% by mass or more, more preferably 80% by mass or more).

[0122] In one embodiment, the first frame portion 121 and the second frame portion 122 can be provided in a state in which they are separated from each other. In that case, the first frame portion 121 and the second frame portion 122 can be connected by a fastener 124. By connecting by the fastener 124, it is possible to obtain an advantage that the pressure applied by the holding portion 121a (122a) to the first end surface 101a (second end surface 101b) can be easily adjusted. The fastener 124 can be fixed to the flange portion 121b (flange portion 122b). The fastener 124 can be, but is not limited to, a combination of a bolt and a nut. The first frame portion 121 and the second frame portion 122 may be provided with a recess 125 for accommodating the fastener 124. By providing the recess 125, the fastener 124 is less likely to come off accidentally. The number and positions of the points at which the first frame portion 121 and the second frame portion 122 are connected by the fasteners 124 may be set appropriately so as to stably hold the heater element 100, but, for example, it is preferable to install the fasteners at 4 to 8 points at equal intervals around the circumferential direction of the flange portion 121b (flange portion 122b) when the heater element assembly is viewed from the first end face 101a (second end face 101b) side (see Figure 2A).

[0123] When the first frame portion 121 and the second frame portion 122 are separated from each other, other methods for joining the two include, but are not limited to, a method of connecting them using an interlocking structure and a method of connecting them using an adhesive.

[0124] 3A and 3B show another example of a heater element assembly including a frame 120 that clamps the heater element 100 from the first end surface 101a side and the second end surface 101b side. The holding portion 121a of the first frame portion 121 of the frame 120 shown in Fig. 3A and 3B has a portion that presses the first terminal 109a toward the first end surface 101a. Similarly, the holding portion 122a of the second frame portion 122 of the frame 120 shown in Fig. 3A and 3B has a portion that presses the second terminal 109b toward the second end surface 101b.

[0125] The holding portion 121a (holding portion 122a) has a portion that presses the first terminal 109a (second terminal 109b) toward the first end surface 101a (second end surface 101b), which provides an effect of preventing the first terminal 109a (second terminal 109b) from falling off. In addition, there is also an advantage that the electrical connection characteristics between the first terminal 109a (second terminal 109b) and the first electrode layer 102a (second electrode layer 102b) are improved.

[0126] In order to enhance the effect of preventing the first terminal 109a from falling off, it is preferable that the holding portion 121a of the first frame portion 121 has a portion 126a that locally protrudes toward the inner periphery, and the protruding portion 126a constitutes at least a part of the portion that presses the first terminal 109a toward the first end face 101a. Similarly, in order to enhance the effect of preventing the second terminal 109b from falling off, it is preferable that the holding portion 122a of the second frame portion 122 has a portion 126b that locally protrudes toward the inner periphery, and the protruding portion 126b constitutes at least a part of the portion that presses the second terminal 109b toward the second end face 101b.

[0127] The larger the area ratio of the portion of the outer surface of the first terminal 109a (second terminal 109b) that is pressed toward the first end face 101a (second end face 101b) by the portion 126a (126b) of the holding portion 121a (122a) that locally protrudes toward the inner periphery, the higher the effect of preventing the first end face 101a (second end face 101b) from falling off. For this reason, the lower limit of the area ratio is preferably 10% or more, more preferably 15% or more, and even more preferably 20% or more. On the other hand, the smaller the area ratio is, the easier it is to ensure space for the current-carrying component, and to easily join the current-carrying component 105a (105b). For this reason, the upper limit of the area ratio is preferably 80% or less, more preferably 75% or less, and even more preferably 70% or less. Therefore, the range of the area ratio can be, for example, 10 to 80%.

[0128] Since the holding portion 121a (holding portion 122a) only locally protrudes toward the inner periphery, it is possible to reduce the area blocking the opening of the cell 104. When the portion 126a (126b) locally protruding toward the inner periphery to press the first terminal 109a (second terminal 109b) toward the first end face 101a (second end face 101b) is observed from the first end face 101a (second end face 101b) side (see FIG. 3A), the upper limit of the ratio of the area of ​​the portion 126a (126b) locally protruding toward the inner periphery (when there are a plurality of portions 126a (126b) locally protruding toward the inner periphery, the total area of ​​the portions 126a (126b)) to the area of ​​the first end face 101a (second end face 101b) is preferably 10% or less, more preferably 5% or less, and even more preferably 3% or less. On the other hand, from the viewpoint of enhancing the effect of preventing the first terminal 109a (second terminal 109b) from falling off, the lower limit of the ratio of the area of ​​the portion 126a (126b) locally protruding inward to the area of ​​the first end face 101a (second end face 101b) is preferably 0.5% or more, more preferably 1% or more, and even more preferably 2% or more. Therefore, the range of the ratio of the area of ​​the portion 126a (126b) locally protruding inward to the area of ​​the first end face 101a (second end face 101b) can be, for example, 0.5% to 10%.

[0129] In the heater element assembly in Figures 3A and 3B, the components represented by the same symbols as those in Figures 2A and 2B are the same as those described with respect to the heater element assembly in Figures 2A and 2B, so their explanations will be omitted.

[0130] In the heater element assembly shown in Figures 2A and 2B and the heater element assembly shown in Figures 3A and 3B, there is a gap between the first frame 121 and the second frame 122, and the outer peripheral surface of the outer peripheral wall 103 of the heater element 100 is exposed. Therefore, as shown in Figures 4A and 4B, in order to improve the protective performance of the frame 120 for the heater element 100, the frame 120 can have a third frame 123 made of resin that surrounds the outer peripheral surface 103e of the outer peripheral wall 103.

[0131] The third frame portion 123 may be connected to the first frame portion 121 or the second frame portion 122, or may be integrally formed with the first frame portion 121 or the second frame portion 122. In addition, the third frame portion 123 may have a through hole for passing the fastener 124 therethrough.

[0132] The materials of the resin constituting the third frame portion 123, such as its Rockwell hardness, type, deflection temperature under load, melting point, thermal conductivity, and volume resistivity, are as described in the explanation of the first frame portion 121 and the second frame portion 122, including the preferred embodiments.

[0133] The third frame 123 may not be in contact with the outer peripheral wall 103. From the viewpoint of stably holding the heater element 100 in the frame 120, the third frame 123 may be in contact with the outer peripheral wall 103. From the viewpoint of improving the protection performance for the heater element 100, a buffer material 131 may be interposed between the third frame 123 and the outer peripheral wall 103. When the buffer material 131 is interposed between the third frame 123 and the outer peripheral wall 103, from the viewpoint of stably holding the heater element 100 in the frame 120 while improving the protection performance for the heater element 100, it is preferable that the buffer material 131 is in a compressed state by being sandwiched between the third frame 123 and the outer peripheral wall 103.

[0134] The thickness of the cushioning material 131 compressed by being sandwiched between the third frame 123 and the outer peripheral wall 103 in the compression direction is preferably 0.5 mm or more, more preferably 1.0 mm or more, and even more preferably 2.0 mm or more, from the viewpoint of ensuring a deformation margin for obtaining a sufficient cushioning effect. The thickness of the cushioning material 131 compressed by being sandwiched between the third frame 123 and the outer peripheral wall 103 in the compression direction is preferably 7.0 mm or less, more preferably 5.0 mm or less, and even more preferably 4.0 mm or less, because it is necessary to ensure the holding surface pressure of the heater element and hold the heater element without destroying it. Therefore, the range of the thickness of the cushioning material 131 compressed by being sandwiched between the third frame 123 and the outer peripheral wall 103 in the compression direction can be, for example, 0.5 mm or more and 7.0 mm or less.

[0135] The lower limit of the pressure that the buffer material 131 receives by being sandwiched between the third frame portion 123 and the outer peripheral wall 103 is preferably 0.002 MPa or more, and more preferably 0.005 MPa or more. The upper limit of the pressure that the buffer material 131 receives is preferably 0.2 MPa or less, and more preferably 0.1 MPa or less. Therefore, the pressure that the buffer material 131 receives is preferably, for example, 0.002 MPa to 0.2 MPa, and more preferably 0.005 MPa to 0.1 MPa. The pressure that the buffer material 131 receives is determined from the Young's modulus and the amount of displacement of the buffer material 131.

[0136] From the viewpoint of ensuring the holding surface pressure against the honeycomb heater element, the Young's modulus of the buffer material 131 is preferably at least 0.05 MPa, more preferably at least 0.06 MPa, and even more preferably at least 0.1 MPa. From the viewpoint of ensuring a deformation allowance for obtaining a sufficient buffer effect, the Young's modulus of the buffer material 131 is preferably at most 0.3 MPa, more preferably at most 0.25 MPa, and even more preferably at most 0.2 MPa. Therefore, the range of the Young's modulus of the buffer material 131 can be, for example, at least 0.05 MPa and not more than 0.3 MPa.

[0137] The method for measuring the Young's modulus of the buffer material 131 is as described in the description of the buffer material 127 .

[0138] The materials constituting the cushioning material 131 are as described in the description of the cushioning material 127, including the preferred embodiment.

[0139] In the heater element assembly in Figures 4A and 4B, the components represented by the same symbols as those in Figures 3A and 3B are the same as those described with respect to the heater element assembly in Figures 3A and 3B, so their explanations will be omitted.

[0140] 5A and 5B show another example of a heater element assembly including a frame 120 that clamps the heater element 100 from the first end face 101a side and the second end face 101b side. The holding portion 121a of the first frame portion 121 of the frame 120 shown in Fig. 5A and Fig. 5B has a plurality of portions 126a that locally protrude toward the inner periphery. Similarly, the holding portion 122a of the second frame portion 122 of the frame 120 shown in Fig. 5A and Fig. 5B has a plurality of portions 126b that locally protrude toward the inner periphery.

[0141] 5A and 5B, only the portion 126a protruding locally to the inner periphery constitutes the retaining portion 121a that applies pressure to at least a part of the outer periphery of the first end face 101a. Similarly, in the second frame portion 122 of the frame 120 shown in Fig. 5A and 5B, only the portion 126b protruding locally to the inner periphery constitutes the retaining portion 122a that applies pressure to at least a part of the outer periphery of the second end face 101b.

[0142] When only the portion 126a protruding locally toward the inner periphery constitutes the holding portion 121a that applies pressure to at least a part of the outer periphery of the first end face 101a, the protruding portion 126a is preferably provided at a plurality of locations in order to stably hold the heater element 100. Similarly, when only the portion 126b protruding locally toward the inner periphery constitutes the holding portion 122a that applies pressure to at least a part of the outer periphery of the second end face 101b, the protruding portion 126b is preferably provided at a plurality of locations in order to stably hold the heater element 100.

[0143] When the protruding portions 126a (126b) are installed in multiple locations, it is preferable to install them at 4 to 8 locations at equal intervals in the circumferential direction of the first frame portion 121 (second frame portion 122) when the heater element assembly is viewed from the first end face 101a (second end face 101b) side and / or point-symmetrically with respect to the center of gravity O (see Figure 5A).

[0144] At least one of the protruding portions 126a (126b) preferably has a portion that presses the first terminal 109a (second terminal 109b) toward the first end face 101a (second end face 101b). The other protruding portions 126a (126b) do not need to play the role of pressing the first terminal 109a (109b) toward the first end face 101a (second end face 101b), and it is sufficient for them to play the role of holding portions 121a (121b) that apply pressure to at least a part of the outer periphery of the first end face 101a (second end face 101b).

[0145] When only the portion 126a (126b) protruding locally toward the inner circumference constitutes the retaining portion 121a (122a) that applies pressure to at least a portion of the outer periphery of the first end face 101a (second end face 101b), when the protruding portion 126a (126b) is observed from the first end face 101a (second end face 101b) side (see FIG. 5A), the upper limit of the ratio of the area of ​​the portion 126a (126b) protruding locally toward the inner circumference (if there are multiple portions 126a (126b) protruding locally toward the inner circumference, this refers to the total area of ​​those portions) to the area of ​​the first end face 101a (second end face 101b) is preferably 1.0% or less, more preferably 0.8% or less, and even more preferably 0.5% or less. On the other hand, from the viewpoint of enhancing the effect of preventing the first terminal 109a (second terminal 109b) from falling off, the lower limit of the ratio of the area of ​​the portion 126a (126b) locally protruding inward (when there are a plurality of portions 126a (126b) locally protruding inward, the total area of ​​the portions) to the area of ​​the first end face 101a (second end face 101b) is preferably 0.1% or more, more preferably 0.3% or more, and even more preferably 0.4% or more. Therefore, the range of the ratio of the area of ​​the portion 126a (126b) locally protruding inward to the area of ​​the first end face 101a (second end face 101b) can be, for example, 0.1% or more and 1.0% or less.

[0146] 5A and 5B, the first frame portion 121 (second frame portion 122) has a passage 130a (130b) for the current-carrying part 105a (105b) that penetrates from the inner circumference side to the outer circumference side. The current-carrying part 105a (105b) is inserted into the passage 130a (130b) and has an end portion 105c (105d) on the outer circumference side of the first frame portion 121 (second frame portion 122) that can be electrically connected to an electric wire.

[0147] 5A and 5B is divided into two parts, which are connected by a connecting portion 150 having a fitting structure. In the illustrated embodiment, the division point 154 is located in the second frame portion 122, but there is no particular limitation on the position of the division point 154. For example, the division point 154 can be freely set at the second frame portion 122, the first frame portion 121, the third frame portion 123, the boundary between the first frame portion 121 and the third frame portion 123, the boundary between the second frame portion 122 and the third frame portion 123, etc.

[0148] The illustrated connecting portion 150 has a press-fit type protrusion 151 and a recess 152. When the protrusion 151 is pressed into the recess 152 while being elastically deformed, the connected state is maintained by the restoring force of the protrusion 151 and the recess 152. The connecting portion 150 can have a snap-fit ​​type or other fitting structure in addition to the press-fit type. It is preferable to sandwich a buffer material 132 between the two parts. The buffer material 132 compressed by being sandwiched between the two parts acts as a spring by elastic deformation, and can prevent the connection between the two parts from loosening.

[0149] From the viewpoint of ensuring the holding surface pressure against the honeycomb heater element, the Young's modulus of the buffer material 132 is preferably at least 0.05 MPa, more preferably at least 0.06 MPa, and even more preferably at least 0.1 MPa. From the viewpoint of ensuring a deformation allowance for obtaining a sufficient buffer effect, the Young's modulus of the buffer material 132 is preferably at most 0.3 MPa, more preferably at most 0.25 MPa, and even more preferably at most 0.2 MPa. Therefore, the range of the Young's modulus of the buffer material 132 can be, for example, at least 0.05 MPa and not more than 0.3 MPa.

[0150] The method for measuring the Young's modulus of the buffer material 132 is as described in the description of the buffer material 127 .

[0151] The materials constituting the cushioning material 132 are as described in the description of the cushioning material 127, including the preferred embodiment.

[0152] In the heater element assembly in Figures 5A and 5B, the components represented by the same symbols as those in Figures 4A and 4B are the same as those described with respect to the heater element assembly in Figures 4A and 4B, so their explanations will be omitted.

[0153] (3. Heater element manufacturing method) Next, a method for producing the heater element according to the present invention will be described by way of example. The method for manufacturing the honeycomb structure that constitutes the heater element includes a molding step and a firing step. In the forming step, a clay containing ceramic raw materials including BaCO3 powder, TiO2 powder, and powder of a rare earth nitrate or hydroxide is formed to produce a honeycomb formed body having a relative density of 60% or more. The ceramic raw material can be obtained by dry mixing each powder so as to obtain a desired composition. The clay can be obtained by adding a dispersion medium, a binder, a plasticizer, and a dispersant to a ceramic raw material and kneading the mixture. The clay may contain additives such as a sifter, a metal oxide, a property improver, and a conductive powder, as necessary. The blending amount of components other than the ceramic raw materials is not particularly limited as long as the blending amount is such that the relative density of the honeycomb formed body is 60% or more.

[0154] In this specification, the "relative density of the honeycomb formed body" means the ratio of the density of the honeycomb formed body to the true density of the entire ceramic raw material. Specifically, it can be calculated by the following formula. Relative density of honeycomb formed body (%) = Density of honeycomb formed body (g / cm 3 ) / True density of ceramic raw material (g / cm 3 ) x 100 The density of the honeycomb molded body can be measured by the Archimedes method using pure water as a medium. The true density of the entire ceramic raw material is calculated by multiplying the total mass (g) of each raw material by the total actual volume (cm 3 ) can be calculated by dividing it by

[0155] The dispersion medium may be water or a mixed solvent of water and an organic solvent such as alcohol, with water being particularly preferred.

[0156] Examples of the binder include organic binders such as methyl cellulose, hydroxypropoxyl cellulose, hydroxyethyl cellulose, carboxymethyl cellulose, and polyvinyl alcohol. In particular, it is preferable to use methyl cellulose and hydroxypropoxyl cellulose in combination. The binder may be used alone or in combination of two or more kinds, but it is preferable that the binder does not contain an alkali metal element.

[0157] Examples of the plasticizer include polyoxyalkylene alkyl ethers, polycarboxylic acid polymers, and alkyl phosphate esters.

[0158] The dispersant may be a surfactant such as polyoxyalkylene alkyl ether, ethylene glycol, dextrin, fatty acid soap, polyalcohol, etc. The dispersant may be used alone or in combination of two or more kinds.

[0159] The honeycomb formed body can be produced by extruding a clay. In the extrusion molding, a die having a desired overall shape, cell shape, partition wall thickness, cell density, etc. can be used.

[0160] The lower limit of the relative density of the honeycomb molded body obtained by extrusion molding is preferably 60% or more, and more preferably 65% ​​or more. By controlling the relative density of the honeycomb molded body within such a range, it is possible to densify the honeycomb molded body and reduce the electrical resistance at room temperature. The upper limit of the relative density of the honeycomb molded body is not particularly limited, but is generally 80% or less, and preferably 75% or less.

[0161] The honeycomb molded body can be dried before the firing step. The drying method is not particularly limited, and for example, a conventionally known drying method such as hot air drying, microwave drying, dielectric drying, reduced pressure drying, vacuum drying, freeze drying, etc. Among these, a drying method that combines hot air drying with microwave drying or dielectric drying is preferred because it can quickly and uniformly dry the entire molded body.

[0162] The firing step involves holding the material at 1150-1250° C., then increasing the temperature to a maximum temperature of 1360-1430° C. at a rate of 20-600° C. / hour, and holding the temperature for 0.5-10 hours. By holding the honeycomb formed body at a maximum temperature of 1360 to 1430° C. for 0.5 to 10 hours, it is possible to obtain a honeycomb structure mainly composed of BaTiO3-based crystal grains in which part of Ba has been substituted with a rare earth element. Moreover, by maintaining the temperature at 1150 to 1250°C, Ba2TiO4 crystal particles generated during the firing process are easily removed, so that the honeycomb structure portion can be densified. Furthermore, by setting the heating rate from 1150-1250°C to the maximum temperature of 1360-1430°C at 20-600°C / hour, 1.0-10.0 mass% of Ba6Ti 17 O 40 Crystal grains can be generated in the honeycomb structure.

[0163] The holding time at 1150 to 1250° C. is not particularly limited, but is preferably 0.5 to 10 hours. By setting the holding time in this range, Ba2TiO4 crystal particles formed during the firing process can be stably and easily removed.

[0164] The firing step preferably includes holding the mixture at 900 to 950° C. for 0.5 to 5 hours during heating. Holding the mixture at 900 to 950° C. for 0.5 to 5 hours allows BaCO3 to efficiently decompose, making it easier to obtain a honeycomb structure having a predetermined composition.

[0165] A degreasing step may be carried out before the firing step to remove the binder. The degreasing step is preferably carried out in an air atmosphere in order to completely decompose the organic components. Moreover, it is preferable that the firing step be performed in an air atmosphere from the viewpoints of controlling electrical characteristics and reducing manufacturing costs. The firing furnace used in the firing step and the degreasing step is not particularly limited, but an electric furnace, a gas furnace, or the like can be used.

[0166] A pair of electrode layers (first electrode layer 102a and second electrode layer 102b) are bonded to the honeycomb structure portion thus obtained, thereby manufacturing a heater element. The first electrode layer 102a and the second electrode layer 102b can be formed on the first end face 101a and the second end face 101b of the honeycomb structure portion by a metal deposition method such as sputtering, vapor deposition, electrolytic deposition, and chemical deposition. The first electrode layer 102a and the second electrode layer 102b can also be formed by applying an electrode paste to the first end face 101a and the second end face 101b of the honeycomb structure portion and then baking it. They can also be formed by thermal spraying. The first electrode layer 102a and the second electrode layer 102b may be composed of a single layer, but may also be composed of multiple electrode layers with different compositions. When the first electrode layer 102a and the second electrode layer 102b are formed on the end faces by the above method, if the thickness of the electrode layer is set not to be excessively large, the cells can be prevented from being blocked.

[0167] The method of forming the first electrode layer 102a and the second electrode layer 102b is not limited, but includes baking of electrode paste, dry plating such as sputtering and vapor deposition, wet plating such as electrolytic deposition and chemical deposition, and bonding of metal or alloy plates. Each method has a suitable thickness range. In baking of electrode paste, the thickness can be about 5 to 30 μm, in dry plating such as sputtering and vapor deposition, the thickness can be about 100 to 1000 nm, in thermal spraying, the thickness can be about 10 to 100 μm, and in wet plating such as electrolytic deposition and chemical deposition, the thickness can be about 5 to 30 μm. In addition, in bonding of metal or alloy plates, the thickness of the electrode layer can be about 5 to 100 μm.

[0168] Next, the first terminal 109a is connected to the outer surface of the first electrode layer 102a, and the second terminal 109b is connected to the outer surface of the second electrode layer 102b. As described above, the two can be connected by welding, brazing, mechanical contact, or the like. Alternatively, the first terminal 109a (second terminal 109b) may be connected by simultaneously baking the electrode paste for forming the first electrode layer 102a (second electrode layer 102b).

[0169] Next, if necessary, the current-carrying parts 105a and 105b are connected to the first terminal 109a and the second terminal 109b, respectively. As described above, the connection between the two can be made by welding, brazing, mechanical contact, or the like.

[0170] Next, a first functional material-containing layer 107a that covers a part of the outer surface of the first electrode layer 102a, and a second functional material-containing layer 107b that covers a part of the outer surface of the second electrode layer 102b are formed. In a preferred embodiment, a third functional material-containing layer 111a that covers a part of the outer surface of the first terminal 109a, and a fourth functional material-containing layer 111b that covers a part of the outer surface of the second terminal 109b are further formed. In a more preferred embodiment, a fifth functional material-containing layer 113 that covers a part or the entire surface of the partition wall 106 that forms the flow path inside the cell 104 is further formed.

[0171] The first functional material-containing layer 107a, the second functional material-containing layer 107b, the third functional material-containing layer 111a, the fourth functional material-containing layer 111b, and the fifth functional material-containing layer 113 may be formed individually or simultaneously. These functional material-containing layers can be formed simultaneously, for example, by the following process. The heater element before the formation of the functional material-containing layer is immersed in a slurry containing a functional material such as a moisture absorbent, a binder, and a dispersion medium for a predetermined time, and excess slurry on the outer peripheral surface of the honeycomb structure part is removed by blowing and wiping. After that, the slurry is dried to form these functional material-containing layers. The drying can be performed while heating the heater element to a temperature of, for example, about 120 to 600°C. A series of processes of immersion, slurry removal, and drying may be performed only once, but by repeating the process multiple times, a functional material-containing layer of a desired thickness can be provided on the surface of the electrode layer, etc.

[0172] Although an organic binder may be used as the binder, it is preferable to use an inorganic binder because there is a concern that the binder may emit smoke due to heat, and the components in the smoke may flow into the vehicle interior and deteriorate the vehicle interior environment. The suitable types of inorganic binders are as described above.

[0173] The dispersion medium can be water, an organic solvent (e.g., toluene, xylene, ethanol, n-butanol, ethyl acetate, butyl acetate, terpineol, dihydroterpineol, texanol, ethylene glycol monobutyl ether acetate, diethylene glycol monoethyl ether acetate, diethylene glycol monoethyl ether, diethylene glycol monobutyl ether acetate, diethylene glycol monobutyl ether), or a mixture thereof.

[0174] (4. Air Conditioning System) According to one embodiment of the present invention, there is provided an air conditioning system including the above-mentioned heater element, which can be used to improve the interior space of various vehicles such as automobiles, as well as buildings such as houses, offices, factories, stores, warehouses, and freezers, and vehicles such as ships and airplanes.

[0175] (4-1. First air conditioning system 1000) FIG. 6 is a schematic diagram showing the configuration of a first air conditioning system 1000 according to one embodiment of the present invention. The first air conditioning system 1000 is At least one heater element 100; A power source 200 such as a battery for applying a voltage to the heater element 100; An inlet pipe 400 that communicates between an interior space such as a vehicle cabin and an inlet end face of the heater element 100; An outlet pipe 500 having a first passage 500a that connects the outlet end face of the heater element 100 to the room; A fan 600 for drawing air from inside the room through an inlet pipe 400 to an inlet end face of the heater element 100; Equipped with.

[0176] In the air conditioning system shown in Fig. 6, the heater element 100 is arranged such that the inlet end face is the first end face 101a and the outlet end face is the second end face 101b. However, the heater element 100 can also be arranged such that the inlet end face is the second end face 101b and the outlet end face is the first end face 101a. There may be only one heater element 100, but multiple heater elements 100 may be arranged in series or parallel.

[0177] In addition to the first path 500a, the outflow pipe 500 may have a second path 500b that connects the outlet end face of the heater element 100 to the outside of the vehicle or the like. The outflow pipe 500 may also have a switching valve 300 that can switch the flow of air passing through the outflow pipe 500 between the first path 500a and the second path 500b.

[0178] The first air conditioning system 1000 is A first mode in which the voltage applied from the power source 200 is turned off, the switching valve 300 is switched so that the air flowing through the outflow pipe 500 passes through the first path 500a, and the ventilator 600 is turned on; A second mode in which the applied voltage from the power source 200 is turned on, the switching valve 300 is switched so that the air flowing through the outflow pipe 500 passes through the second path 500b, and the ventilator 600 is turned on; The vehicle may have the following operating modes:

[0179] The first air conditioning system 1000 can include a control unit 900 capable of switching between the first mode and the second mode. The control unit 900 may be configured to alternately execute the first mode and the second mode, for example. By repeating the switching between the first mode and the second mode in a constant cycle, it becomes possible to stably discharge the components to be removed, such as water vapor, from inside the vehicle to the outside.

[0180] In the first mode, the components to be removed from the air are removed. Specifically, air from the room flows in from the inlet end face of the heater element 100 through the inlet pipe 400, passes through the heater element 100, and then flows out from the outlet end face of the heater element 100. The components to be removed from the air from the room are captured by a functional material such as a dehumidifier while passing through the heater element 100, and are removed. The air from which the components to be removed have been removed and flows out from the outlet end face of the heater element 100 is returned to the room through the first path 500a of the outlet pipe 500. The air may be supplied to another air conditioning system (e.g., HVAC in a vehicle).

[0181] In the second mode, the functional material such as a dehumidifier is regenerated. Specifically, air from the room flows into the inlet end face of the heater element 100 through the inlet pipe 400, passes through the heater element 100, and then flows out from the outlet end face of the heater element 100. The heater element 100 generates heat when energized, which heats the functional material supported on the heater element 100, causing the components to be removed that have been captured by the functional material to leave the functional material or react.

[0182] In order to promote the release of the components to be removed captured in the functional material, it is preferable to heat the functional material to a temperature equal to or higher than the release temperature depending on the type of functional material. When a moisture absorbent is used as the functional material, it is preferable to heat at least a part of the moisture absorbent, preferably the whole, to 70 to 150°C, more preferably to 80 to 140°C, and even more preferably to 90 to 130°C. In addition, it is preferable to perform the second mode for a time until the functional material is sufficiently regenerated. Although it depends on the type of functional material, for example, when a moisture absorbent is used as the functional material, in the second mode, the functional material is preferably heated to the above temperature range for 1 to 10 minutes, more preferably for 2 to 8 minutes, and even more preferably for 3 to 6 minutes.

[0183] In the second mode, air from the room flows out from the outlet end face of the heater element 100 while carrying with it the components to be removed that have been separated from the functional material while passing through the heater element 100. The air containing the components to be removed that flows out from the outlet end face of the heater element 100 passes through the second path 500b of the outlet piping 500 and is discharged to the outside of the room.

[0184] The voltage applied to the heater element 100 can be switched on and off by, for example, electrically connecting the power source 200 and a pair of terminals 109a, 109b of the heater element 100 with an electric wire 810 and operating a power switch 910 provided in the middle of the wire. The control unit 900 can operate the power switch 910.

[0185] The ventilator 600 can be switched on and off by, for example, electrically connecting the control unit 900 and the ventilator 600 via an electric wire 820 or wirelessly and operating a switch (not shown) of the ventilator 600 by the control unit 900. The ventilator 600 can also be configured so that the amount of ventilation can be changed by the control unit 900.

[0186] The switching of the switching valve 300 can be performed, for example, by electrically connecting the control unit 900 and the switching valve 300 via an electric wire 830 or wirelessly, and operating a switch (not shown) of the switching valve 300 by the control unit 900.

[0187] The switching valve 300 is not particularly limited as long as it is a valve that is electrically driven and has the function of switching the flow path, and examples of the switching valve 300 include a solenoid valve and an electric valve. In one embodiment, the switching valve 300 includes an opening / closing door 312 supported by a rotating shaft 310, and an actuator 314 such as a motor that rotates the rotating shaft 310. The actuator 314 is configured to be controllable by the control unit 900.

[0188] From the viewpoint of stably ensuring the above-mentioned functions, it is desirable that the heater element 100 of the first air conditioning system 1000 is disposed at a position close to the room. Therefore, from the viewpoint of preventing electric shock, etc., it is preferable that the driving voltage is 60V or less. Since the honeycomb structure part used in the heater element 100 has low electrical resistance at room temperature, it is possible to heat the honeycomb structure part at this low driving voltage. The lower limit of the driving voltage is not particularly limited, but is preferably 10V or more. If the driving voltage is less than 10V, the current during heating of the honeycomb structure part becomes large, so it is necessary to make the electric wire 810 thicker. Therefore, the driving voltage of the first air conditioning system 1000 can be, for example, 10V or more and 60V or less.

[0189] In the embodiment shown in Fig. 6, the fan 600 is installed upstream of the heater element 100. More specifically, the fan 600 is installed in the middle of the inlet pipe 400 that communicates between the heater element 100 and the room, and the air that has passed through the fan 600 flows into the heater element 100 so as to be forced therethrough. Alternatively, the fan 600 may be installed downstream of the heater element 100. In this case, the fan 600 can be installed, for example, in the middle of the outlet pipe 500, and the air that has passed through the inlet pipe 400 flows into the heater element 100 so as to be sucked therein. EXAMPLES

[0190] [1. Specifications of honeycomb structure] A honeycomb structure having the following specifications was prepared. -The cross section and end face shape of the honeycomb structure perpendicular to the flow path direction: Square (curvature radius 6mm or more) -Cell opening shape perpendicular to the flow path direction: Square with chamfered corners Partition thickness: 0.100mm - Thickness of outer wall: 0.3mm Cell density: 80 cells / cm 2 Cell pitch: 1.11mm Cell aperture ratio: 0.797 -Size of cross section perpendicular to the direction of flow of honeycomb structure: 90mm x 90mm Length of the honeycomb structure in the direction of flow: 12 mm Volume resistivity of the material that composes the outer wall and partition at 25°C: 15 Ω cm - Curie point of the material that composes the outer wall and partition: 120℃ Material for the outer wall and partition: Barium titanate -Density of material constituting outer wall and bulkhead: 5750kg / m 3 -Specific heat of the material that composes the outer wall and partition: 550J / kg / K

[0191] [2. Characteristics of the functional material (moisture absorbent) used] A commercially available amorphous aluminum silicate was prepared as a moisture absorbent. 5 g of the amorphous aluminum silicate, which had been dried at 180°C for more than 2 hours, was left in a thermohygrostat at room temperature (25°C) and a relative humidity of 50% for one hour. From the increased mass of the amorphous aluminum silicate taken out of the thermohygrostat, the mass (g) of water that could be adsorbed per 1 g of dried mass was calculated, and found to be 15 g / g.

[0192] After drying at 180℃ for 2 hours or more, 5g of amorphous aluminum silicate was placed in a thermohygrostat with a relative humidity of 50% and the mass change when left for one hour at various temperatures was investigated. From this, the temperature range where the mass (g) of water that can be adsorbed per 1g of dry mass is 5g / g or more was determined to be 10℃ to 25℃.

[0193] After drying at 180°C for more than 2 hours, 5g of amorphous aluminum silicate was left for one hour in a thermo-hygrostat at room temperature (25°C) and a relative humidity of 50% to adsorb moisture. The amorphous aluminum silicate after adsorption was placed in a thermo-hygrostat at a relative humidity of 50% and the mass change when left for 0.1 hours at various temperatures was investigated. The lowest temperature at which the mass loss rate of the amorphous aluminum silicate after adsorption was 30% was determined as the moisture desorption temperature, which was 70°C.

[0194] [3. Manufacturing of heater element assembly] Heater element assemblies according to the following Examples and Comparative Examples were each produced in the number required for various analyses and tests.

[0195] <Example 1> A paste of aluminum powder mixed with a binder resin was applied to both end faces (first end face 101a and second end face 101b) of the honeycomb structure part and baked to bond a pair of electrode layers (first electrode layer 102a and second electrode layer 102b) by baking (volume resistivity at 25°C: 2.0 × 10 -7 Ω cm). The percentage (coverage rate) of the area of ​​the first end face 101a (second end face 101b) covered by the first electrode layer 102a (second electrode layer 102b) to the area of ​​the portion of the first end face 101a (second end face 101b) excluding the openings of the cells 104 (the partition wall portion and the outer peripheral wall portion) was calculated based on both areas and was 99%. The average thickness of the entire first electrode layer 102a (second electrode layer 102b), the average thickness of the portion other than the outer periphery, and the average thickness of the outer periphery were measured by the above-mentioned measuring method. The results are shown in Table 1. The conditions for the first electrode layer 102a and the second electrode layer 102b are the same.

[0196] Next, pure aluminum (A1050) (volume resistivity at 25°C: 2.0 × 10 -7 A first terminal 109a and a second terminal 109b, which are rectangular plates having planar dimensions of 100 mm × 4 mm and a thickness of 1 mm, were connected by soldering to the outer surfaces of the first electrode layer 102a and the second electrode layer 102b, respectively, only to the outer peripheries of the first end face 101a and the second end face 101b.

[0197] The ratio (coverage rate) of the area covered by first terminal 109a (second terminal 109b) to the area of ​​first end face 101a (second end face 101b) was calculated based on the areas of both, and was found to be 3%. The conditions for the first terminal 109a and the second terminal 109b are the same.

[0198] Next, amorphous aluminum silicate powder, silica powder, and a solvent (water) were mixed in a mass ratio of amorphous aluminum silicate:silica:solvent = 95:5:100 and stirred to prepare a moisture absorbent slurry. The obtained moisture absorbent slurry was applied to the outer surface of the first electrode layer 102a and the outer surface of the second electrode layer 102b by a brush coating method, and then dried in a dryer at 190°C for 2 hours to form the first functional material-containing layer 107a and the second functional material-containing layer 107b, thereby preparing a heater element. The first functional material-containing layer 107a and the second functional material-containing layer 107b were produced under the same conditions.

[0199] The ratio (coverage) of the area of ​​the outer surface of the first electrode layer 102a (second electrode layer 102b) covered by the first functional material-containing layer 107a (second functional material-containing layer 107b) to the area of ​​the portion of the outer surface of the first electrode layer 102a (second electrode layer 102b) to which the first terminal 109a (second terminal 109b) is not connected was calculated based on both areas and was 95% or more. The average thickness of the first functional material-containing layer 107a (second functional material-containing layer 107b) was measured by the above-mentioned measuring method and was 200 μm.

[0200] Using the procedure described above, electrical resistance measurements were performed at 12 points on each of the first functional material-containing layer 107a and the second functional material-containing layer 107b. The range of electrical resistance (minimum to maximum) was 3.0×10 6 ~4.0×10 6 It was Omega.

[0201] The heater element obtained by the above procedure was sandwiched from the first end face 101a side and the second end face 101b side by a frame 120 having a first frame portion 121 and a second frame portion 122 but no third frame portion 123, and a heater element assembly having the structure shown in Figures 3A and 3B was assembled. However, the outer peripheral shape of the first frame portion 121 and the second frame portion 122 was made to be approximately rectangular corresponding to the outer peripheral shape of the heater element. In addition, no cushioning material was used anywhere. The first frame portion 121 and the second frame portion 122 have a portion 126a that locally protrudes toward the inner periphery, and the protruding portion 126a forms at least a part of the portion that presses the first terminal 109a toward the first end face 101a. The first frame portion 121 and the second frame portion 122 were formed by injection molding or cutting processing from a base material. The first frame portion 121 and the second frame portion 122 were connected by a combination of bolts and nuts. The connection points were four points equally spaced in the circumferential direction of the flange portion 121b (flange portion 122b).

[0202] Table 1 shows the following conditions for the commercially available resins used for the first frame portion 121 and the second frame portion 122. The conditions for the resins used for the first frame portion 121 and the second frame portion 122 are the same. R1: Resin type (Comparative Example 1 is made of metal) R2: Rockwell hardness (HRR and HRM) measured according to ASTM D785-2008 R15 R3: Thermal conductivity at 25°C measured in accordance with JIS R1611:2010 R4: Deflection temperature under load as specified in JIS K7191-1:2015 R5: Melting point R6: Volume resistivity at 25°C measured in accordance with JIS C2139:2008

[0203] For the obtained heater element assembly, the structural conditions of the holding portion 121a (122a) are shown in Table 1. The structural conditions of the holding portion 121a and the holding portion 122a are the same. S1: The ratio of the area of ​​the portion of the first end face 101a (second end face 101b) that receives pressure from the holding portion 121a (122a) to the entire area of ​​the first end face 101a (second end face 101b). S2: Range of width W of holding portion 121a (122a) (if there is a part that locally protrudes toward the inner circumference, that part is also considered as part of the range of the width of the holding portion) S3: The number of portions 126a (126b) of the holding portion 121a (122a) that locally protrude inward S4: When observed from the first end face 101a (second end face 101b) side, the ratio of the area of ​​the portion 126a (126b) of the holding portion 121a (122a) that locally protrudes inward (when there are multiple portions 126a (126b) that locally protrude inward, this refers to the total area of ​​those portions) to the area of ​​the first end face 101a (second end face 101b) S5: Whether or not only the portion 126a (126b) of the holding portion 121a (122a) that locally protrudes toward the inner periphery constitutes the holding portion 121a (122a) that applies pressure to at least a part of the outer periphery of the first end face 101a (second end face 101b). S6: The ratio of the area of ​​the portion of the outer surface of the first terminal 109a (second terminal 109b) that is pressed toward the first end face 101a (second end face 101b) by the portion 126a (126b) that locally protrudes inwardly of the holding portion 121a (122a)

[0204] <Examples 2, 3, 7, and 8> A heater element assembly was assembled under the same conditions as in Example 1, except that the commercially available resin used for the first frame 121 and the second frame 122 was changed to the conditions listed in Table 1. The conditions of the resin used for the first frame 121 and the second frame 122 were the same.

[0205] <Examples 4 to 6> A heater element assembly was assembled under the same conditions as in Example 1, except that a commercially available cushioning material having the type and Young's modulus shown in Table 1 was used and the sheet-like cushioning material was placed between the retaining portion 121a of the first frame portion 121 and the first end face 101a, and between the retaining portion 122a of the second frame portion 122 and the second end face 101b, under the conditions shown in Table 1. In the table, the thickness displacement rate of the compressed cushioning material in the compression direction was calculated using the following formula: Displacement rate (%) = (1 - thickness of cushioning material after compression / thickness of cushioning material before compression) x 100.

[0206] <Examples 9, 10, 13, and 14> A heater element assembly was assembled under the same conditions as in Example 1, except that the structural conditions of the holding portion 121a (122a) were changed to those shown in Table 1. The structural conditions of the holding portion 121a and the holding portion 122a are the same.

[0207] <Example 11> A heater element assembly was assembled under the same conditions as in Example 1, except that the average thicknesses of the first electrode layer 102a and the second electrode layer 102b at their outer peripheries were changed to the values ​​shown in Table 1 using a handy roller.

[0208] <Example 12> A heater element assembly was assembled under the same conditions as in Example 1, except that a frame 120 having a third frame 123 in addition to the first frame 121 and the second frame 122 was used. However, the outer peripheral shapes of the first frame 121, the second frame 122, and the third frame 123 were approximately rectangular corresponding to the outer peripheral shape of the heater element. In addition, no cushioning material was used between the third frame 123 and the outer peripheral wall 103. The conditions of the resin used for the third frame 123 were the same as those for the first frame 121 and the second frame 122.

[0209] <Comparative Example 1> A heater element assembly was assembled under the same conditions as in Example 1, except that the material of the first frame portion 121 and the second frame portion 122 was changed to a metal (SUS304) having the properties shown in Table 1. The conditions of the first frame portion 121 and the second frame portion 122 are the same.

[0210] 4. Heater Element Assembly Characteristics <Water discharge performance> The frame was removed from the heater element assembly according to each of the examples and comparative examples obtained by the above procedure, and a sample of Φ25 mm (flow path length unchanged) was cut out from the heater element. The sample was inserted into a quartz glass tube with a wall thickness of 1 mm, an inner diameter of 25 mm, and a length of 26 mm, and then set in a HORIBA MEXA-6000FT. Nitrogen gas heated to 120°C was flowed through the flow path of the sample at 40 L / min for 1 hr to dry the sample, and then the introduction of nitrogen gas was stopped, and water vapor gas adjusted to 0.6% was introduced at 25°C and 50 L / min for 10 minutes, and then the introduction of water vapor gas was stopped and nitrogen gas heated to 120°C was introduced at 15 L / min for 10 minutes to measure the water discharge performance of the sample. Note that, for Example 12, the test was performed in a state where the sample was inserted into a polyether ether ketone resin tube with a wall thickness of 1 mm, an inner diameter of 25 mm, and a length of 26 mm instead of the quartz glass tube. For Comparative Example 1, instead of the quartz glass tube, the test was performed with the sample inserted into a metal tube made of SUS304 with a wall thickness of 1 mm, an inner diameter of 25 mm, and a length of 26 mm. The water discharge performance was evaluated based on the following criteria. 〇: Water discharge amount is 0.0353g / cm 3 Super, 0.0367g / cm 3 less than ◎: Water discharge amount is 0.0367g / cm 3 End ×: Water discharge amount is 0.0353g / cm 3 below

[0211] <Bondability between the first electrode layer (second electrode layer) and the first terminal (second terminal)> The frame was removed from the heater element assembly, and the resulting heater element was placed sideways (the extension direction of the cell was horizontal) on the measurement table and fixed, and the joined terminal was pushed out from the vertical direction of the top surface, and the maximum stress at which a stress-displacement diagram was obtained when the terminal was pushed out was determined. The bonding strength between the first electrode layer and the first terminal, and the bonding strength between the second electrode layer and the second terminal were measured separately, and the average value was taken as the measured value. The measurement device used was a general universal testing machine (INSTRON6800). The bonding strength was evaluated based on the following criteria. 〇: Over 0.95MPa, under 1.05MPa ◎: 1.05MPa or more ×: 0.95MPa or less

[0212] <Heater element retention> A voltage of 13 V was applied between the first and second terminals of the heater element assemblies according to the examples and comparative examples obtained by the above procedure, and air (25°C) was passed through the flow path of the heater element assembly at a flow rate of 40 L / min while heating for 3 minutes, and it was confirmed that the heater element reached an average temperature of 120°C or higher. After stopping the current, air at 25°C was passed through the flow path of the heater element assembly at 750 L / min for 3 minutes to cool the heater element to an average temperature of 25°C or lower. Thereafter, a voltage of 13 V was applied again, and air (25°C) was passed through the flow path of the heater element assembly at a flow rate of 40 L / min to heat for 3 minutes, and it was investigated whether the heater element could reach an average temperature of 120°C or higher without being damaged or falling off the frame. The retention of the heater element to the frame was evaluated based on the following criteria. ○: The heater element did not break or fall off from the frame when reheated, and reached an average temperature of 120°C or higher. ×: The heater element was broken or fell off from the frame during reheating.

[0213] <Pressure loss> The pressure loss between both end faces of the flow passage of the heater element assembly according to each of the Examples and Comparative Examples obtained by the above procedure was measured when air (25°C) was flowed from one end face side at a flow rate of 750 L / min. The evaluation was based on the following criteria. ○: Pressure loss is over 58.2 Pa and less than 60 Pa ◎: Pressure loss is 58.2 Pa or less

[0214] From the above test results, it can be seen that the resin frame has a lower thermal conductivity than the metal frame, which reduces heat loss and improves water discharge performance. Also, from the results of the thermal test, it can be seen that the resin frame has a higher retention performance for the heater element than the metal frame, i.e., it has a higher protection performance for the heater element.

[0215] [Table 1-1]

[0216] [Table 1-2] [Explanation of symbols]

[0217] 100: Heater element 101a: First end surface 101b: Second end face 102a: First electrode layer 102b: Second electrode layer 103:Outer wall 103a:Aisle 103e: Outer surface 104: Cell 105a: Current carrying parts 105b: Current-carrying parts 105c: End 106: Bulkhead 107a: First functional material containing layer 107b: Second functional material containing layer 109a: First terminal 109b: Second terminal 111a: Third functional material containing layer 111b: Fourth functional material containing layer 113:Fifth functional material containing layer 120: Frame 121: First frame 121a: Holding part 121b: Flange part 122: Second frame part 122a: Holding part 122b: Flange part 123: Third frame 124: Fasteners 125: Recess 126a: A part that protrudes locally toward the inner circumference 126b: Part that protrudes locally toward the inner circumference 127: Cushioning material 131: Cushioning material 132: Cushioning material 150:Connection part 151: Convex 152: Recess 154: Division point 200: Power supply 300: Switching valve 310: Rotation axis 312: Opening and closing door 314: Actuator 400: Inlet pipe 500: Outlet pipe 500a: First route 500b: Secondary route 600: Ventilator 810:Electric wire 820: Electric wire 830: Electric wire 900: Control unit 910: Power switch 1000: First Air Conditioning System

Claims

1. A heater element assembly comprising a heater element and a frame, The heater element is a honeycomb structure portion capable of generating heat by application of electricity, the honeycomb structure portion having an outer peripheral wall and partition walls disposed on an inner peripheral side of the outer peripheral wall, the partition walls defining a plurality of cells that form flow paths extending from a first end face to a second end face, the partition walls containing a material having PTC characteristics; a first electrode layer covering a part or the whole of a surface of the partition wall forming the first end face; a second electrode layer covering a part or the whole of a surface of the partition wall forming the second end face; a first terminal connected to an outer surface of the first electrode layer; and a second terminal connected to an outer surface of the second electrode layer; having The frame body is for clamping the heater element from the first end surface side and the second end surface side, a first frame portion made of resin and arranged on the first end surface side, the first frame portion having a flange portion arranged on the outer peripheral side of an outer peripheral contour of the first end surface, and a retaining portion arranged on the inner peripheral side of the outer peripheral contour of the first end surface and applying pressure to at least a part of an outer periphery of the first end surface; and a second frame portion made of resin and arranged on the second end surface side, the second frame portion having a flange portion arranged on the outer peripheral side of an outer peripheral contour of the second end surface, and a retaining portion arranged on the inner peripheral side of the outer peripheral contour of the second end surface and applying pressure to at least a part of an outer periphery of the second end surface; having Heater element assembly.

2. The heater element assembly according to claim 1, wherein the resin constituting the first frame portion and / or the second frame portion has a Rockwell hardness measured in accordance with ASTM D785-2008 R15 of 150 HRR or less and / or 120 HRM or less.

3. The heater element assembly according to claim 1 or 2, wherein the resin constituting the first frame portion and / or the second frame portion has a deflection temperature under load of 145°C or higher as measured in accordance with JIS K7191-1:2015.

4. 3. The heater element assembly according to claim 1, wherein the resin constituting the first frame and / or the second frame has a melting point of 250° C. or higher.

5. 3. The heater element assembly according to claim 1, wherein the resin constituting the first frame portion and / or the second frame portion has a thermal conductivity of 0.5 W / m / K or less at 25°C measured in accordance with JIS R1611:2010.

6. The resin constituting the first frame portion and / or the second frame portion has a volume resistivity of 1.0×10 at 25° C. measured in accordance with JIS C2139:2008. 16 3. The heater element assembly according to claim 1, wherein the resistance is Ω·cm or more.

7. 3. The heater element assembly according to claim 1 or 2, wherein the resin constituting the first frame portion and / or the second frame portion contains one or two types selected from polyether ether ketone (PEEK) and polybutylene terephthalate (PBT).

8. A ratio of an area of ​​the first end face to which pressure is applied by the holding portion of the first frame portion to an area of ​​the first end face is 10% or less, and / or a ratio of an area of ​​the second end face to which pressure is applied by the holding portion of the second frame portion to an area of ​​the second end face is 10% or less; A heater element assembly according to claim 1 or 2.

9. A ratio of an area of ​​the first end face to which pressure is applied by the holding portion of the first frame portion to an area of ​​the first end face is 2% or less, and / or a ratio of an area of ​​the second end face to which pressure is applied by the holding portion of the second frame portion to an area of ​​the second end face is 2% or less; A heater element assembly according to claim 1 or 2.

10. the holding portion of the first frame portion has a portion that presses the first terminal toward the first end surface, and / or the holding portion of the second frame portion has a portion that presses the second terminal toward the second end surface, A heater element assembly according to claim 1 or 2.

11. A cushioning material is interposed between the holding portion of the first frame portion and the first end surface, and / or A cushioning material is interposed between the holding portion of the second frame portion and the second end surface. A heater element assembly according to claim 1 or 2.

12. 3. The heater element assembly according to claim 1, wherein the frame has a third frame portion made of resin and surrounding an outer circumferential surface of the outer circumferential wall of the heater element.

13. The heater element assembly according to claim 12, wherein a buffer material is interposed between the third frame portion and the outer peripheral wall.

14. 3. The heater element assembly according to claim 1, wherein the first frame portion and the second frame portion are separated from each other and connected to each other by a fastener.

15. 3. The heater element assembly according to claim 1, wherein the first frame portion and the second frame portion are separated from each other and connected to each other by a fitting structure.

16. 3. The heater element assembly according to claim 1, wherein the first frame portion and the second frame portion are separated from each other and connected by an adhesive.

17. and / or, an average value of the thickness of the first electrode layer at an outer periphery of the first end surface and at a connection point with the first terminal is greater than an average value of the thickness of the first electrode layer at other portions. an average thickness of the second electrode layer at an outer circumferential portion of the second end face and at a connection portion between the second terminal and the second end face is greater than an average thickness of the second electrode layer at other portions; A heater element assembly according to claim 1 or 2.

18. and / or, the average thickness of the first electrode layer over the entire outer periphery of the first end surface is greater than the average thickness of the first electrode layer over the remaining portion. an average thickness of the second electrode layer over the entire outer periphery of the second end face is greater than an average thickness of the second electrode layer over the other portion; A heater element assembly according to claim 1 or 2.

Citation Information

Patent Citations

  • JP1974114130A

  • Air cleaning system for vehicle, and control method of the air cleaning system for vehicle

    JP2020104774A

  • Air purification device for vehicle

    JP2020111282A

  • Heating element for heating passenger compartment, method of use thereof, and heater for heating passenger compartment

    WO2020036067A1

Cited By

  • Vehicle air conditioning system