Nanofibers containing lipid nanoparticles and method for manufacturing the same
Lipid nanoparticle-containing nanofibers with polyvinyl alcohol resin and liposomes address the stability and delivery challenges of existing formulations, achieving uniformity, mucoadhesion, and sustained drug release in the gastrointestinal tract.
Patent Information
- Application Number
- JP2024048905
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-28
- Filing Date
- 2024-03-26
- Publication Date
- 2024-10-11
AI Technical Summary
Existing nanofiber formulations struggle to stably incorporate liposomes, which are easily degraded by gastric acid or have difficulty penetrating the gastrointestinal wall, limiting their effectiveness in drug delivery systems.
The development of lipid nanoparticle-containing nanofibers using a polyvinyl alcohol resin as a base material, with lipid nanoparticles like liposomes, encapsulating drugs, and a specific mass ratio of polyvinyl alcohol to lipid constituents, produced through electrospinning, maintains the stability and mucoadhesive properties of the nanofibers.
The nanofibers achieve uniform fiber diameter, high mucoadhesive properties, and stable lipid nanoparticle retention, enhancing drug delivery by maintaining the liposome structure and improving retention in the gastrointestinal tract, allowing for sustained drug release.
Smart Images

Figure 2024144298000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a lipid nanoparticle-containing nanofiber capable of stably retaining lipid nanoparticles and delivering a drug, and a method for producing the same. [Background technology]
[0002] In the design of various formulations, including oral and transdermal formulations, mucoadhesive formulations that are formulated to adhere to mucous membranes such as gastrointestinal epithelial cells and skin are being considered as a method of drug release control to increase the bioavailability of drugs.
[0003] For example, Patent Document 1 proposes drug-containing ultrafine fibers prepared by dispersing a drug in a spinnable substrate such as polyurethane resin, polyvinyl alcohol, or gelatin and spinning the dispersed drug into the substrate, and a laminate of the drug-containing ultrafine fibers. In this case, a drug that is absorbed transdermally is used as the drug, and the film-like laminate is used as a transdermal absorption preparation.
[0004] Patent Document 2 proposes drug-containing nanofibers using a poorly soluble drug in an amorphous state, and a nanofiber nonwoven fabric thereof. It discloses that by containing a poorly soluble drug in an amorphous state, the drug dissolution rate was excellent.
[0005] On the other hand, for drugs that are easily decomposed by gastric acid, such as peptide drugs and nucleic acid drugs, or drugs that are difficult to penetrate the gastrointestinal wall or introduce into cells by themselves, preparations that use liposomes as carriers for DDS (drug delivery system) (liposome preparations) are known (e.g., Patent Document 3). [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2014-55119 A [Patent Document 2] Patent Publication No. 2021-88552 [Patent Document 3] Japanese Patent Application Publication No. 5-194191 Summary of the Invention [Problem to be solved by the invention]
[0007] The drug-containing nanofibers proposed in Patent Documents 1 and 2 are both nanofiber preparations obtained by preparing a spinning solution containing a drug in a solution that serves as the base material of the nanofiber, and then spinning the solution to produce drug-containing nanofibers and nonwoven fabrics of the nanofibers.
[0008] In the nanofiber laminate proposed in Patent Document 1, a transdermal absorption enhancer is contained in the nanofibers together with a drug in order to increase transdermal absorbability.
[0009] The nanofiber laminate proposed in Patent Document 2 is an orally administered agent that enhances the dissolution rate of a poorly soluble drug, and uses an amorphous drug.
[0010] By converting liposomal DDS reagents, which can improve the membrane permeability of polymeric drugs such as proteins and extend the release duration of water-soluble drugs, into nanofibers, it is expected that the proportion of drugs that can reach the target can be increased.
[0011] However, liposomes are easily disrupted by external stimuli, and therefore it is considered difficult to produce nanofibers using a spinning process. At present, there are no nanofibers containing liposome formulations as pharmaceutical agents.
[0012] The present invention has been made in consideration of the above circumstances, and an object of the present invention is to provide a nanofiber preparation in the form of a liposome or lipid nanoparticle, for a drug that is easily decomposed by gastric acid, etc., or a drug that is difficult to permeate the gastrointestinal wall or to be introduced into cells by itself. [Means for solving the problem]
[0013] The lipid nanoparticle-containing nanofiber of the present invention has the following aspects. [1] A lipid nanoparticle-containing nanofiber comprising a water-soluble resin including a polyvinyl alcohol-based resin and lipid nanoparticles. [2] The lipid nanoparticle-containing nanofiber according to claim 1, wherein the content of the polyvinyl alcohol-based resin in the water-soluble resin is 50% by weight or more. [3] The lipid nanoparticle-containing nanofiber according to the above aspect [1] or [2], wherein the lipid nanoparticle is a liposome.
[0014] [4] The lipid nanoparticle-containing nanofiber according to any one of the above aspects [1] to [3], further comprising a drug, the drug being retained within the lipid nanoparticle. [5] The lipid nanoparticle-containing nanofiber according to the above aspect [3], further comprising a drug, the drug being encapsulated within the liposome.
[0015] [6] The lipid nanoparticle-containing nanofiber according to any one of the above aspects [1] to [5], wherein the lipid nanoparticles are composed of phospholipids or cationic lipids. [7] The lipid nanoparticle-containing nanofiber according to any one of the aspects [1] to [6], wherein the lipid nanoparticle has a hydrophilic polymer modifying group.
[0016] [8] The lipid nanoparticle-containing nanofiber according to any one of the aspects [1] to [7], wherein the content ratio of the polyvinyl alcohol resin to the lipid constituting the lipid nanoparticles is 99.5:0.5 to 60:40 by mass ratio. [9] The lipid nanoparticle-containing nanofiber according to any one of the above aspects [1] to [8], wherein the polyvinyl alcohol-based resin has a degree of saponification of 80 to 94 mol %.
[10] The lipid nanoparticle-containing nanofiber according to any one of the above aspects [1] to [9], wherein the lipid nanoparticles have an average particle size of 10 to 1,000 nm.
[0017] The present invention also includes a lipid nanoparticle-containing nanofiber nonwoven fabric formed by laminating the lipid nanoparticle-containing nanofibers according to any one of the above aspects [1] to
[10] . The present invention also encompasses a mucoadhesive preparation comprising the nanofiber nonwoven fabric of the present invention.
[0018] Another aspect of the present invention is a method for producing nanofibers containing lipid nanoparticles, which includes a step of electrospinning a mixed solution of an aqueous solution containing a polyvinyl alcohol-based resin and a solution containing lipid nanoparticles and a drug.
[0019] In this specification, the lipid nanoparticle refers to a nanoparticle having an internal space (internal phase) surrounded by a lipid membrane, and is a concept that includes liposomes. Liposomes are lipid nanoparticles that have a bilayer composed, in particular, of phospholipid membranes. Effect of the Invention
[0020] According to the present invention, a nanofiber having a uniform fiber diameter and high mucoadhesiveness is obtained, and the lipid nanoparticles contained therein stably maintain their nanoparticle structure, so that the nanofiber can stably maintain and deliver drugs as a nanofiber for mucoadhesive formulations. [Brief description of the drawings]
[0021] [Figure 1A] 1 is a scanning electron microscope (SEM) photograph of LNP-NFS1 obtained in the evaluation of nanofiber uniformity performed in the examples. [Figure 1B] 1 is a scanning electron microscope (SEM) photograph of LNP-NFS2 obtained in the evaluation of nanofiber uniformity performed in the examples. [Diagram 2] 1 is a graph showing the results of a liposome retention test carried out in an example. [Diagram 3]Fluorescence micrographs showing the results of a liposome distribution evaluation test conducted in the examples, where (A) is an image of F-PVA, (B) is an image of Nile Red, and (C) is a composite image of (A) and (B). [Figure 4] Fluorescence micrographs showing the results of a liposome distribution evaluation test conducted in the examples, where (A) is an image of F-PVA, (B) is an image of Nile Red, and (C) is a composite image of (A) and (B). [Diagram 5] 1 is a graph showing the results of a test of liposome behavior in the digestive tract performed in an example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0022] The present invention will be described in detail below, but these are merely examples of preferred embodiments. In this specification, "mass" is synonymous with "weight".
[0023] The lipid nanoparticle-containing nanofiber of the present invention is a nanofiber having lipid nanoparticles contained therein, the nanofiber having a base material made of a water-soluble resin mainly composed of a polyvinyl alcohol-based resin.
[0024] [Water-soluble resin] First, the water-soluble resin that is the base material of the nanofibers and the polyvinyl alcohol-based resin (hereinafter also referred to as "PVA-based resin") that is the main component of the water-soluble resin will be described.
[0025] 1.PVA resin
[0026] The PVA resin of the present invention is a resin obtained by saponifying a polyvinyl ester polymer obtained by polymerizing a vinyl ester monomer, and is composed of vinyl alcohol structural units corresponding to the degree of saponification and vinyl ester structural units remaining unsaponified.
[0027] The saponification degree of the PVA resin used in the present invention is preferably 80 to 94 mol%, more preferably 82 to 92 mol%, further preferably 84 to 90 mol%, and particularly preferably 85 to 89 mol%. When the saponification degree of the PVA resin is within the preferred range, the effects of the present invention tend to be easily obtained. In the present invention, the saponification degree of the PVA resin is a value determined by a method in accordance with JIS K 6726, and is an average saponification degree determined as an average value.
[0028] The average degree of polymerization of the PVA resin used in the present invention is preferably 200-4,000, more preferably 1,000-3,500, further preferably 1,500-3,000, and particularly preferably 2,000-2,800. When the average degree of polymerization of the PVA-based resin is 200 or more, the strength of the nanofiber tends to be good and the stability during use tends to be improved, and when the average degree of polymerization is 4,000 or less, the aqueous solution has an appropriate viscosity and nanofibers tend to be easily formed. In the present invention, the average degree of polymerization of the PVA resin is determined by a method in accordance with JIS K 6726.
[0029] The PVA resin can be obtained, for example, by saponifying a polyvinyl ester polymer obtained by polymerizing a vinyl ester monomer. Examples of such vinyl ester monomers include vinyl formate, vinyl acetate, vinyl propionate, vinyl valerate, vinyl butyrate, vinyl isobutyrate, vinyl pivalate, vinyl caprate, vinyl laurate, vinyl stearate, vinyl benzoate, and vinyl versatate, with vinyl acetate being preferred for practical purposes.
[0030] In addition, a monomer having copolymerizability with the vinyl ester monomer can be copolymerized to the extent that the effect of the present invention is not impaired. Examples of such copolymerization monomers include olefins such as ethylene, propylene, isobutylene, α-octene, α-dodecene, and α-octadecene; hydroxyl-containing α-olefins such as 3-buten-1-ol, 4-penten-1-ol, 5-hexen-1-ol, and 3,4-dihydroxy-1-butene, and derivatives thereof such as acylated products; unsaturated acids and salts thereof such as acrylic acid, methacrylic acid, crotonic acid, maleic acid, maleic anhydride, itaconic acid, and undecylenic acid; nitriles such as acrylonitrile and methacrylonitrile; amides such as diacetone acrylamide, acrylamide, and methacrylamide; ethylene sulfonic acid, allyl sulfonic acid, and methallyl sulfonic acid. olefin sulfonic acids and their salts; vinyl compounds such as alkyl vinyl ethers, dimethylallyl vinyl ketone, N-vinylpyrrolidone, vinyl chloride, vinyl ethylene carbonate, 2,2-dialkyl-4-vinyl-1,3-dioxolane, and glycerin monoallyl ether; substituted vinyl acetates such as isopropenyl acetate and 1-methoxyvinyl acetate; hydroxymethylvinylidene diacetates such as vinylidene chloride, 1,4-diacetoxy-2-butene, 1,4-dihydroxy-2-butene, vinylene carbonate, 1,3-diacetoxy-2-methylenepropane, 1,3-dipropionyloxy-2-methylenepropane, and 1,3-dibutyronyloxy-2-methylenepropane;Reaction products of 3-chloro-2-hydroxypropyltrimethylammonium chloride, 3-chloroethyltrimethylammonium chloride, 3-chloropropyltrimethylammonium chloride, etc. with polyvinyl alcohol resin, or N-acrylamidotrimethylammonium chloride, N-acrylamidoethyltrimethylammonium chloride, N-acrylamidopropyltrimethylammonium chloride, 2-acryloxyethyltrimethylammonium chloride, N-methyldimethylaminoacrylamide, allyltrimethylammonium chloride, meth Compounds having a cationic group such as allyltrimethylammonium chloride, dimethylallylamine, dimethylmethacrylamine, dimethyldiallylammonium chloride, diethyldiallylammonium chloride, ethyldiallylamine, and methyldiallylamine; hydroxymethylvinylidene diacetates such as 3,4-diacetoxy-1-butene, vinyl ethylene carbonate, glycerin monoallyl ether, 1,3-diacetoxy-2-methylenepropane, 1,3-dipropionyloxy-2-methylenepropane, and 1,3-dibutyronyloxy-2-methylenepropane; The content of such copolymerizable monomers may be preferably 10 mol % or less, more preferably 5 mol % or less, based on the total amount of the polymer.
[0031] In the present invention, it is preferable to use unmodified PVA as the PVA-based resin. Unmodified PVA is a vinyl alcohol polymer having vinyl alcohol structural units corresponding to the degree of saponification obtained by polymerizing and saponifying a vinyl ester monomer, and vinyl ester structural units in the unsaponified portion.
[0032] Two or more PVA-based resins can be used in combination. When using them in combination, PVA-based resins with different saponification degrees, average polymerization degrees, and block properties, or modified PVA-based resins can be used in combination.
[0033] PVA-based resins become gel-like when in contact with water, enabling them to exhibit adhesion to mucous membranes.
[0034] 2. Other water-soluble resins In addition to the PVA-based resins mentioned above, the water-soluble resins that make up the nanofiber substrate may include starch derivatives such as polyethylene glycol starch, oxidized starch, and cation-modified starch; natural proteins such as gelatin and casein; cellulose derivatives such as methylcellulose, ethylcellulose, hydroxyethylcellulose, and carboxymethylcellulose (CMC); natural polymeric polysaccharides such as sodium alginate and pectinic acid; water-soluble resins such as polyvinylpyrrolidone and poly(meth)acrylates; latexes such as styrene-butadiene rubber (SBR) latex and nitrile rubber (NBR) latex; and emulsions such as vinyl acetate resin emulsions, ethylene-vinyl acetate copolymer emulsions, (meth)acrylic ester resin emulsions, vinyl chloride resin emulsions, and urethane resin emulsions. In this specification, (meth)acrylic means acrylic or methacrylic.
[0035] The content ratio of the PVA-based resin in the water-soluble resin of the present invention is 50% by weight or more, and preferably 60% by weight or more, 70% by weight or more, 80% by weight or more, 92% by weight or more, 93% by weight or more, 94% by weight or more, or 95% by weight or more, based on the total amount of the water-soluble resin. By ensuring that the content of the PVA-based resin is within the above range, nanofibers with a uniform fiber diameter are easily obtained, and nanofibers in which lipid nanoparticles have good dispersibility are easily obtained.
[0036] [Lipid nanoparticles] The lipid nanoparticles referred to in this specification refer to nanoparticles having an internal space (internal phase) surrounded by a lipid membrane, and are a concept that includes liposomes. The lipids constituting the lipid membrane include neutral lipids and cationic lipids. The neutral lipids include phospholipids, aminolipids, sphingolipids, cholesterol, or derivatives thereof. Among these, phospholipids, or a mixture of phospholipids and cholesterol, or derivatives thereof, are particularly preferably used.
[0037] Among lipid nanoparticles, lipid nanoparticles having a lipid bilayer membrane composed of phospholipids are particularly called liposomes, and a complex of a liposome made of cationic lipid and a nucleic acid is particularly called a lipoplex.
[0038] Whether it is lipid nanoparticles or liposomes, drugs can be encapsulated in the internal phase, and they can act as drug carriers.
[0039] Examples of phospholipids include natural or synthetic phospholipids such as phosphatidylcholine, phosphatidylethanolamine, phosphatidylserine, phosphatidic acid, phosphatidylglycerol, phosphatidylinositol, lysophosphatidylcholine, sphingomyelin, egg yolk lecithin, soybean lecithin, and hydrogenated phospholipids.
[0040] Examples of phosphatidylcholine include soybean phosphatidylcholine, egg yolk phosphatidylcholine, dilauroylphosphatidylcholine, dimyristoylphosphatidylcholine, dipalmitoylphosphatidylcholine, dioleoylphosphatidylcholine, and distearoylphosphatidylcholine. Examples of the phosphatidylethanolamine include dioleoylphosphatidylethanolamine, dilauroylphosphatidylethanolamine, dimyristoylphosphatidylethanolamine, dipalmitoylphosphatidylethanolamine, and distearoylphosphatidylethanolamine. Examples of phosphatidylserine include dilauroylphosphatidylserine, dimyristoylphosphatidylserine, dipalmitoylphosphatidylserine, and distearoylphosphatidylserine. Phosphatidic acids include dimyristoyl phosphatidic acid, dipalmitoyl phosphatidic acid, and dioleoyl phosphatidic acid. Examples of phosphatidylglycerol include dilauroylphosphatidylglycerol, dimyristoylphosphatidylglycerol, dipalmitoylphosphatidylglycerol, and distearoylphosphatidylglycerol. Examples of phosphatidylinositol include dilauroylphosphatidylinositol, dimyristoylphosphatidylinositol, dipalmitoylphosphatidylinositol, and distearoylphosphatidylinositol. Phosphatidylcholine is preferred, and distearoylphosphatidylcholine is particularly preferred, from the viewpoint of forming stable liposomes, since the phase transition temperature at which the lipid bilayer structure of the liposome is formed and destroyed is relatively high (room temperature or higher).
[0041] The above-mentioned phospholipids may be modified to form phospholipid derivatives. The modifying group of the phospholipid derivative may be a hydrophilic polymer, such as polyethylene glycols, polyglycerins, polypropylene glycols (PEGs), polyvinyl alcohol, styrene-maleic anhydride alternating copolymers, polyvinylpyrrolidone, and synthetic polyamino acids, which may be used alone or in combination of two or more. Among these, polyethylene glycol-modified phospholipids, which are modified with polyethylene glycols, are preferred from the viewpoint of being less susceptible to the effects of interaction with mucus (mucin) in the digestive tract and increasing mucosal permeability.
[0042] The molecular weight of the polyethylene glycols is not particularly limited, but is preferably 500-10,000, more preferably 1,000-5,000, and further preferably 1,200-3,000. Examples of polyethylene glycols used for modification include 1,2-distearoyl-3-phosphatidylethanolamine-polyethylene glycols such as 1,2-distearoyl-3-phosphatidylethanolamine-PEG2000, 1,2-distearoyl-3-phosphatidylethanolamine-PEG5000, and distearoylglycerol-PEG2000 manufactured by Nippon Oil & Fats Corporation; 1,2-distearoyl-sn-glycero-3-phosphoethanolamine-N-[methoxy(polyethylene glycol)-2000]; and 1,2-distearoyl-sn-glycero-3-phosphoethanolamine-N-[methoxy(polyethylene glycol)-2000]. Examples of suitable phosphoethanolamines include 1.2-dipalmitoyl-sn-glycero-3-phosphoethanolamine-N-[methoxy(polyethylene glycol)-5000], 1.2-dipalmitoyl-sn-glycero-3-phosphoethanolamine-N-[methoxy(polyethylene glycol)-2000], 1.2-dipalmitoyl-sn-glycero-3-phosphoethanolamine-N-[methoxy(polyethylene glycol)-5000], and 1.2-dimyristoyl-sn-glycero-3-phosphoethanolamine-N-[methoxy(polyethylene glycol)-2000]. Particularly from the viewpoint of mucosal permeability, 1,2-distearoyl-sn-glycero-3-phosphoethanolamine-N-[methoxy(polyethylene glycol)-2000] is preferred.
[0043] Cationic lipid refers to lipids that have a net positive charge. Cationic lipids can bind negatively charged RNA to lipid matrices through electrostatic interactions. In general, cationic lipids have a lipophilic moiety such as a sterol, an acyl chain, a diacyl chain or more acyl chains, and the head group of the lipid typically carries a positive charge. In certain embodiments, cationic lipids have a net positive charge only at a certain pH, particularly an acidic pH, but at a different, preferably higher pH such as physiological pH, they preferably do not have a net positive charge, preferably have no charge, i.e., are neutral. For the purposes of this disclosure, such "cationically ionizable" lipids are included in the term "cationic lipid" unless the context is inconsistent. Examples of cationic lipids include N,N-dimethyl-2,3-dioleyloxypropylamine (DODMA), 1,2-di-O-octadecenyl-3-trimethylammoniumpropane (DOTMA), 3-(N-(N',N'-dimethylaminoethane)carbamoyl)cholesterol (DC-Chol), dimethyldioctadecylammonium (DDAB); 1,2-dioleoyl-3-trimethylammoniumpropane (DOTAP); 1,2-dioleoyl-3-dimethylammoniumpropane (DODAP); 1,2-diacyloxy-3-dimethylammoniumpropane (DODAP); 1,2-Dialkyloxy-3-dimethylammonium propane; Dioctadecyldimethylammonium chloride (DODAC), 1,2-distearyloxy-N,N-dimethyl-3-aminopropane (DSDMA), 2,3-di(tetradecoxy)propyl-(2-hydroxyethyl)dimethylazanium (DMRIE), 1,2-dimyristoyl-sn-glycero-3-ethylphosphocholine (DMEPC), l,2-dimyristoyl-3-trimethylammonium propane (DMTAP), 1,2-dioleyloxy Dipropyl-3-dimethylhydroxyethylammonium bromide (DORIE), 2,3-dioleoyloxy-N-[2(sperminecarboxamido)ethyl]-N,N-dimethyl-l-propanamide trifluoroacetate (DOSPA), 1,2-dilinoleyloxy-N,N-dimethylaminopropane (DLinDMA), 1,2-dilinolenyloxy-N,N-dimethylaminopropane (DLenDMA), dioctadecylamidoglycylspermine (DOGS), 3-dimethylamino-2-(cholest-5-ene-3-beta)-1,2 ... -oxybutane-4-oxy)-1-(cis,cis-9,12-octadecadienooxy)propane (CLinDMA), 2-[5'-(cholest-5-ene-3-beta-oxy)-3'-oxapentoxy)-3-dimethyl-1-(cis,cis-9',12'-octadecadienooxy)propane (CpLinDMA), N,N-dimethyl-3,4-dioleyloxybenzylamine (DMOBA), 1,2-N,N'-dioleylcarbamyl-3-dimethylaminopropane (DOcarbDAP), 2,3-dilinoleoyloxy-N,N-Dimethylpropylamine (DLinDAP), 1,2-N,N'-Dilinoleylcarbamyl-3-dimethylaminopropane (DLincarbDAP), 1,2-Dilinoleoylcarbamyl-3-dimethylaminopropane (DLinCDAP), 2,2-Dilinoleyl-4-dimethylaminomethyl-[1,3]-dioxolane (DLin-K-DMA), 2,2-Dilinoleyl-4-dimethylaminoethyl-[1,3]-dioxolane (DLin-K-XTC2-DMA), 2,2-Dilinoleyl-4-(2-dimethylaminoethyl)-[1,3] -dioxolane (DLin-KC2-DMA), heptatriaconta-6,9,28,31-tetraen-19-yl-4-(dimethylamino)butanoate (DLin-MC3-DMA), N-(2-hydroxyethyl)-N,N-dimethyl-2,3-bis(tetradecyloxy)-1-propanaminium bromide (DMRIE), (±)-N-(3-aminopropyl)-N,N-dimethyl-2,3-bis(cis-9-tetradecenyloxy)-1-propanaminium bromide (GAP-DMORIE), (±)-N-(3-aminopropyl)-N, N-Dimethyl-2,3-bis(dodecyloxy)-1-propanaminium bromide (GAP-DLRIE), (±)-N-(3-aminopropyl)-N,N-dimethyl-2,3-bis(tetradecyloxy)-1-propanaminium bromide (GAP-DMRIE), N-(2-aminoethyl)-N,N-dimethyl-2,3-bis(tetradecyloxy)-1-propanaminium bromide (βAE-DMRIE), N-(4-carboxybenzyl)-N,N-dimethyl-2,3-bis(oleoyloxy)propan-1-aminium (DOBAQ), 2 -({8-[(3β)-cholest-5-en-3-yloxy]octyl}oxy)-N,N-dimethyl-3-[(9Z,12Z)-octadeca-9,12-dien-1-yloxy]propan-1-amine (octyl-CLinDMA), 1,2-dimyristoyl-3-dimethylammonium propane (DMDAP), 1,2-dipalmitoyl-3-dimethylammonium propane (DPDAP), N1-[2-((1S)-1-[(3-aminopropyl)amino]-4-[di(3-aminopropyl)amino]butylcarboxamido)ethyl]-3,4-Di[oleyloxy]-benzamide (MVL5), 1,2-dioleoyl-sn-glycero-3-ethylphosphocholine (DOEPC), 2,3-bis(dodecyloxy)-N-(2-hydroxyethyl)-N,N-dimethylpropan-1-ammonium bromide (DLRIE), N-(2-aminoethyl)-N,N-dimethyl-2,3-bis(tetradecyloxy)propan-1-ammonium bromide (DLRIE), bromide (DMORIE), di((Z)-non-2-en-1-yl) 8,8'-((((2(dimethylamino)ethyl)thio)carbonyl)azanediyl) dioctanoate (ATX), N,N-dimethyl-2,3-bis(dodecyloxy)propan-1-amine (DLDMA), N,N-dimethyl-2,3-bis(tetradecyloxy)propan-1-amine (DMDMA), di((Z)- Non-2-en-1-yl)-9-((4-(dimethylaminobutanoyl)oxy)heptadecanedioate (L319), N-dodecyl-3-((2-dodecylcarbamoyl-ethyl)-{2-[(2-dodecylcarbamoyl-ethyl)-2-{(2-dodecylcarbamoyl-ethyl)-[2-(2-dodecylcarbamoyl-ethylamino)ethyl]-amino}-ethylamino)propionamide (Lipidoid 98N12-5), 1-[2-[bis(2-hydroxydodecyl)amino]ethyl-[2-[4-[2-[bis(2hydroxydodecyl)amino]ethyl]piperazin-1-yl]ethyl]amino]dodecan-2-ol (Lipidoid C12-200). DODMA, DOTMA, DOTAP, DODAC, and DOSPA are preferred.
[0044] Cholesterol derivatives include, for example, cholestanol, cholestanone, cholestenone, coprostanol, cholesteryl-2'-hydroxyethyl ether, cholesteryl-4'-hydroxybutyl ether, tocopherol and derivatives thereof, and mixtures thereof. By including other hydrophobic moieties, such as cholesterol, in the lipid membrane of the lipid nanoparticles, the stability of the lipid nanoparticles can be enhanced, and the efficiency of drug delivery can be increased.
[0045] The lipid nanoparticles used in the present invention can be formed by using known methods such as, but not limited to, the hydration method, ultrasonic treatment method, ethanol injection method, ether injection method, reverse phase evaporation method, surfactant method, freeze-thaw method, etc. For example, in the case of the hydration method, lipids can be dissolved in an organic solvent, the organic solvent is evaporated to obtain a lipid membrane, and then the membrane is hydrated with an aqueous solvent. Examples of the organic solvent include ethanol, chloroform, ether, hexane, cyclohexane, toluene, and dichloromethane.
[0046] The lipid nanoparticles may be freeze-dried. The lipid nanoparticles can be made into a powder by freeze-drying. By using powdered lipid nanoparticles, the content of lipid nanoparticles in the spinning solution can be increased, and the amount of lipid nanoparticles contained in the nanofibers can be increased.
[0047] Freeze-drying methods include a method in which lipid nanoparticles are cooled and frozen, and then the frozen lipid nanoparticles are placed under vacuum to sublimate and remove water, followed by drying, and spray freeze-drying. During freeze-drying, a freeze-drying protective agent may be added as necessary, such as mannitol, trehalose, sucrose, lactose, cyclodextrin, dextran, etc.
[0048] The average particle size of the lipid nanoparticles is preferably from 10 to 1000 nm, more preferably from 10 to 500 nm, and even more preferably from 10 to 200 nm. An average particle size of 1,000 nm or less is preferable because it ensures good dispersibility of the lipid nanoparticles in the mixed liquid during nanofiber production, and an average particle size of 10 nm or more makes it possible to contain the required amount of even a polymeric drug. The particle size in the present invention is measured using a ZETASIZER Nano ZS (MALVERN INSTRUMENT) based on the principle of dynamic light scattering.
[0049] The size of the lipid nanoparticles contained in the nanofibers preferably varies little. Specifically, the polydispersity index, which is an index of the degree of polydispersity of the particle size distribution, is preferably 0.5 or less, more preferably 0.3 or less, and particularly preferably 0.2 or less. The polydispersity index in the present invention is measured using a ZETASIZER Nano ZS (MALVERN INSTRUMENT) based on the dynamic light scattering method.
[0050] The lipid nanoparticles of the present invention may contain other additives, such as lipid additives and excipients.
[0051] [Drugs] The drug contained in the lipid nanoparticle-containing nanofiber of the present invention is mainly a drug encapsulated in the lipid nanoparticle. In the case where the lipid membrane is a bilayer like a liposome, the drug may be contained in the lipid membrane, but is preferably encapsulated in the internal phase of the lipid nanoparticle.
[0052] Methods for encapsulating drugs in the internal phase of lipid nanoparticles include, but are not limited to, a method in which a drug is mixed and hydrated in a lipid nanoparticle-containing solution and then heated and kneaded, a remote loading method (pH gradient method), a lipid film method (vortex method), a reverse phase evaporation method, a surfactant removal method, a freeze-thaw method, etc., and any known method can be appropriately selected. When the drug is a negatively charged RNA, it is preferably combined with a liposome formed from a cationic lipid, and when the drug is an uncharged high molecular weight drug or low molecular weight drug, it is preferably combined with a liposome formed from a phospholipid. The drug encapsulated in the internal phase of the lipid nanoparticle is released from the nanofiber as lipid nanoparticles after administration. When the nanofiber is a mucoadhesive formulation, the lipid nanoparticles released from the nanofiber penetrate the mucosa, and then the lipid bilayer structure is disrupted in the mucus on the mucosa, releasing the encapsulated drug.
[0053] The drugs used in the present invention are suitable for lipid nanoparticle formulations and mucoadhesive formulations, i.e. drugs that are easily decomposed by gastric acid or the like, poorly membrane-permeable drugs, water-soluble drugs, polymer drugs, etc. Specific examples of the polymeric drugs include peptide drugs, protein drugs, and other polymeric drugs, nucleic acid drugs, etc. Examples of the polymeric drugs include oxytocin, desmopressin, leuprolide, goserelin, octreotide, peptides, proteins, fusion proteins, antigens, growth factors, cytokines, interferons, hormones, blood coagulation and fibrinolysis factors, enzymes, conjugated proteins, protein vaccines, antibody-like proteins, cells, and nucleic acids. Examples of nucleic acid medicines include vaccines, decoy nucleic acids, antisense nucleic acids, siRNAs, miRNAs, ribozymes, and aptamers.
[0054] The content ratio of lipid nanoparticles and drug varies depending on the physical properties of the drug, but the phospholipid:drug (mass ratio) is preferably 99.9:0.1 to 50:50, more preferably 99.5:0.5 to 75:25, and even more preferably 99:1 to 80:20. By setting the ratio within the above range, it is easy to encapsulate the drug within the lipid bilayer structure.
[0055] [Nanofibers containing lipid nanoparticles] The lipid nanoparticle-containing nanofiber of the present invention can be obtained by spinning a material containing the lipid nanoparticles and a water-soluble resin that is a nanofiber substrate.
[0056] The diameter (fiber diameter) of the lipid nanoparticle-containing nanofiber is preferably 1 nm to 10 μm, more preferably 1 to 2000 nm, particularly preferably 5 to 1000 nm, and further preferably 10 to 700 nm. If the fiber diameter of the nanofiber is too large, the liquid tends to drip during spinning and the nanofibers tend to aggregate, whereas if the fiber diameter of the nanofiber is too small, the strength and handleability tend to decrease. The fiber diameter of the nanofibers is measured using an electron microscope.
[0057] The content of lipid nanoparticles contained in the lipid nanoparticle-containing nanofiber of the present invention is preferably 0.1 to 50% by weight, more preferably 0.5 to 45% by weight, even more preferably 1.0 to 40% by weight, and particularly preferably 5 to 35% by weight, based on the total weight of the nanofiber.
[0058] The content ratio of the PVA resin and the lipid membrane (phospholipid) of the lipid nanoparticle in the lipid nanoparticle-containing nanofiber of the present invention is preferably such that the PVA resin:phospholipid (mass ratio) is in the range of 99.5:0.5 to 60:40, more preferably 99:1 to 55:45, and even more preferably 98:2 to 50:50.
[0059] When the drug is negatively charged RNA, the N / P ratio, which is the ratio of amino groups to phosphate groups, is preferably 0.01-30, more preferably 0.5-20, and even more preferably 5-10. If the N / P ratio is too small, the RNA content in the lipid nanoparticles tends to decrease, which is undesirable, whereas if the N / P ratio is too large, it is undesirable from the viewpoint of cytotoxicity.
[0060] [Method for producing nanofibers] The lipid nanoparticle-containing nanofibers of the present invention can be obtained by using a mixed liquid containing a PVA-based resin and lipid nanoparticles as a raw material (spinning solution) and applying this mixed liquid to an electrospinning method (electrostatic spinning method) or a melt-blowing method. The lipid nanoparticle-containing nanofiber of the present invention has excellent stability of the lipid nanoparticles because the lipid nanoparticles are located within the fiber.
[0061] The mixture used as the spinning solution may be prepared by mixing the PVA-based resin, lipid nanoparticles, and drug in a solvent, or each may be prepared as a separate solution and then the solutions may be mixed together, or a solution of two of the PVA-based resin, lipid nanoparticles, and drug and a solution containing the remaining component may be prepared and then the respective solutions may be mixed together. Among these, it is preferable to prepare a mixture of lipid nanoparticles and a drug (drug-containing lipid nanoparticle solution) in advance, and mix this drug-containing lipid nanoparticle solution with a PVA-based resin solution in which a PVA-based resin is dissolved. According to this method, lipid nanoparticles containing a drug are easily obtained, and nanofibers containing the drug in the form of lipid nanoparticles containing the drug are easily obtained.
[0062] 1. Lipid nanoparticle-containing solution Examples of the solvent used in the preparation of the lipid nanoparticle-containing liquid include organic solvents such as alcohols (methanol, ethanol, butanol, hexafluoro-2-propanol, etc.), esters (methyl acetate, ethyl acetate, etc.), DMSO (dimethyl sulfoxide), chloroform, dichloromethane, etc., and water, etc., and water is preferred from the viewpoint of reducing the environmental load. The solvent containing water may contain other solvents (the organic solvents exemplified above, such as methanol, ethanol, methyl acetate, ethyl acetate, DMSO, etc.). From the viewpoint of spinning, it is preferable to adjust the viscosity of the lipid nanoparticle-containing liquid at 25° C. to 1 to 10,000 mPa·s. In this specification, the viscosity of the solution is measured by a Brookfield viscometer (hereinafter the same applies).
[0063] 2. PVA resin solution As the solvent for the PVA-based resin solution, a solvent such as that used for the lipid nanoparticle-containing liquid can be used, and water is preferred. The viscosity of the PVA-based resin solution at 25° C. is more preferably from 10 to 5000 mPa·s, and particularly preferably from 100 to 3000 mPa·s.
[0064] The PVA-based resin solution may contain an alkali metal salt or an alkaline earth metal salt. Examples of the alkali metal salt include potassium salts and sodium salts of organic and inorganic acids. Examples of the organic acid include acetic acid, propionic acid, butyric acid, lauric acid, stearic acid, oleic acid, and behenic acid. Examples of the inorganic acid include sulfuric acid, sulfurous acid, carbonic acid, and phosphoric acid. Examples of the alkaline earth metal salt include calcium salts and magnesium salts of organic and inorganic acids. Examples of the organic acid include acetic acid, propionic acid, butyric acid, lauric acid, stearic acid, oleic acid, and behenic acid. Examples of the inorganic acid include sulfuric acid, sulfurous acid, carbonic acid, and phosphoric acid.
[0065] 3. Spinning solution The concentration of the PVA resin in the spinning solution is preferably from 1 to 40% by weight, more preferably from 2 to 30% by weight, and further preferably from 5 to 20% by weight. By setting the PVA-based resin concentration within the above range, the mixture has a suitable viscosity, so that the fiber diameter of the obtained nanofibers becomes uniform, and nanoparticles are easily dispersed uniformly in the nanofibers, which is preferable.
[0066] The concentration of the lipid nanoparticles in the spinning solution is preferably 0.5 to 50% by weight, more preferably 1 to 40% by weight, and even more preferably 1.5 to 35% by weight.
[0067] In addition to the drug-containing lipid nanoparticles, PVA-based resin, and the solvent used in preparing these solutions, the spinning solution may contain, as appropriate, well-known additives such as plasticizers, lubricants, pigment dispersants, thickeners, anti-sticking agents, flow improvers, surfactants, defoamers, release agents, penetrating agents, dyes, pigments, fluorescent brightening agents, ultraviolet absorbers, antioxidants, preservatives, anti-mold agents, paper strength agents, and crosslinking agents.
[0068] The viscosity of the spinning solution at 25° C. is preferably adjusted to be in the range of 1 to 10,000 mPa·s, more preferably 10 to 5,000 mPa·s, and particularly preferably 100 to 3,000 mPa·s. If the viscosity is 1 mPa s or higher, fiber formation during spinning of the nanofibers tends to be good, whereas if the viscosity is 10,000 mPa s or lower, aggregation sites (beads) do not form in the nanofibers when they are made into nanofibers, and the fiber diameter of the nanofibers is stable, which is preferable.
[0069] 4. Spinning method The spinning solution prepared as described above is spun to obtain nanofibers containing lipid nanoparticles. Examples of the nanofiber spinning method include electrospinning using a spinning nozzle, electrospinning not using a spinning nozzle, melt blowing, etc. The electrospinning using a spinning nozzle is preferred.
[0070] [Nanofiber nonwoven fabric] The lipid nanoparticle-containing nanofiber nonwoven fabric of the present invention is a sheet-like product in which lipid nanoparticle-containing nanofibers are randomly laid and layered. The randomly layered nanofibers are appropriately entangled to form a nonwoven fabric.
[0071] The thickness of the lipid nanoparticle-containing nanofiber nonwoven fabric according to the present invention is preferably 0.1 to 500 μm, more preferably 0.3 to 300 μm, and even more preferably 0.5 to 100 μm. The basis weight of the obtained nanofiber nonwoven fabric is appropriately set depending on the application, but is preferably 0.1 to 40 g / m 2 , more preferably 0.5 to 20 g / m 2 , and more preferably 1 to 10 g / m 2 It is.
[0072] [Application] The lipid nanoparticle-containing nanofibers and nanofiber nonwoven fabrics using the same may be formulated in combination with an appropriate excipient. For example, they may be encapsulated in a capsule or the like to mask odors and tastes or to deliver the nanofibers to a desired site. They may also be used alone as a formulation. In particular, the nanofiber nonwoven fabrics may be used as mucoadhesive formulations.
[0073] The formulations are for oral administration and transdermal administration. In particular, the nanofiber nonwoven fabric can be used as an oral agent, a patch, or a tape. EXAMPLES
[0074] The present invention will be described in more detail below with reference to examples and comparative examples. However, the present invention is not limited to the following examples as long as it does not depart from the gist of the present invention.
[0075] [Ingredients used] 1.Water-soluble resin Polyvinyl alcohol resin (PVA) manufactured by Mitsubishi Chemical Corporation [unmodified PVA resin, saponification degree 88 mol%, average polymerization degree 2400] was added to distilled water and stirred at a temperature of 80°C to obtain an aqueous PVA resin solution (5.5 wt%) for use.
[0076] 2. Constituent materials of lipid nanoparticles (1) Phospholipids "COATSOME MC-8080" is a distearoylphosphatidylcholine (DSPC) manufactured by NOF Corporation (2) Cholesterol (CHOL) Cholesterol from Sigma-Aldrich (3) Phospholipid modifying agents "DSPE-020CN" (DSPE-PEG), 1.2-distearoyl-sn-glycero-3-phosphoethanolamine-N-[methoxy(polyethylene glycol)-2000 from Yuka Sangyo Co., Ltd.
[0077] 3. Model drugs Fluorescein isothiocyanate-dextran (FD-4) [Mw: 3000-5000] manufactured by Sigma-Aldrich
[0078] 4. Labeling substance (1) Fluorescent labeling substance for PVA-based resin Fluorescein isothiocyanate isomer type I (FITC) from Sigma-Aldrich (2) Fluorescent labeling substance for liposomes (2-1) Nile Red manufactured by Tokyo Chemical Industry Co., Ltd. (2-2) Indocyanine Green (ICG) manufactured by MP Biomedicals
[0079] 5.Other (1) Liposomal freeze-drying protection agent Hydroxypropyl-β-cyclodextrin (HPβCD) manufactured by Junsei Chemical Co., Ltd. was used.
[0080] [Preparation of liposomes] 1. PEGylated liposomes (LNP1) The phospholipids DSPC and CHOL were dissolved in chloroform to concentrations of 28.05 mg / mL and 1.934 mg / mL, respectively, and the solvent was removed under reduced pressure in a 40°C water bath using a rotary evaporator (Tokyo Rikakiki N-1110) to prepare a thin film. This thin film was dried under reduced pressure overnight or more, and then hydrated with distilled water in a water bath at 60°C, and then extruded using an extruder (AVESTIN's LiposoFast TM The liposomes were passed 41 times through a filter having a pore size of 100 nm (Nucleporo Track-Etoch Membrane, manufactured by Whatman) at a pressure of 300 kPa to 400 kPa using a pressure adjuster (Mitsubishi Microwave Oven) (Mitsubishi Microwave Oven). Liposomes 1 (LNP1) were obtained by passing the liposomes 41 times through a filter having a pore size of 100 nm (Nucleporo Track-Etoch Membrane, manufactured by Whatman) at a pressure of 300 kPa to 400 kPa using a pressure adjuster (Mitsubishi Microwave Oven). The liposome 1 was added to an aqueous solution of DSPE-PEG, which is a phospholipid modifying agent, so that the mass ratio of DSPC:DSPE-PEG was 1:2.2. The mixture was incubated at 60° C. for 1 hour to obtain a PEG-modified liposome 1 (PEG-LNP1). Characteristics of PEG-modified liposome 1 (PEG-LNP1): particle size 109.4 nm, polydispersity index 0.183.
[0081] 2. PEGylated liposomes (LNP2) A 21.3 mg / mL HPβCD aqueous solution was used as a freeze-drying protection agent. This HPβCD aqueous solution was mixed with the PEG-modified liposome 1 prepared above (PEG-LNP1 (DSPC+DSPE-PEG):HPβCD = 20.3:21.3 (mass ratio)) and pre-frozen at -100°C using a cooling trap device (Tokyo Rika Kikai UT-4000). Then, using a freeze dryer (Tokyo Rika Kikai FDU-2200), it was freeze-dried at 10 Pa or less for 48 hours, and the freeze-dried product of PEG-modified liposome 1 was named PEG-modified liposome 2 (PEG-LNP2). The properties of PEG-modified liposome 2 (lyophilized product) are as follows. The particle size and polydispersity index were almost the same as those before lyophilization, and it was confirmed that no denaturation of the PEG-modified liposome was observed due to lyophilization. Average particle size 106.0nm, polydispersity index 0.131.
[0082] [Preparation of drug-containing lipid nanoparticles and freeze-dried products thereof] The phospholipids DSPC and CHOL were dissolved in chloroform to concentrations of 28.05 mg / mL and 1.934 mg / mL, respectively, and the solvent was removed under reduced pressure in a 40°C water bath using a rotary evaporator (Tokyo Rikakiki N-1110) to prepare a thin film. This was mixed with a 16 mg / mL aqueous solution of FD-4 used as a model drug (FD-4:DSPC=1:1.75 (mass ratio)) and treated with an extruder to obtain drug-containing liposome 1. The obtained solution of drug-containing liposome 1 was mixed with a PEGylated solution to adjust the concentration to 12.62 mg / mL (DSPC:DSPE-PEG=1:2.2 (mass ratio) in the mixture). Incubation at 60° C. for 1 hour in this state yielded lipid nanoparticles in which a drug was encapsulated in PEG-modified LNP1 (drug-containing PEG-LNP1).
[0083] The prepared drug-loaded PEG-LNP1 was mixed with 21.3 mg / mL of a freeze-drying solution (aqueous HPβCD solution) (phospholipid:HPβCD = 1.9:1 (mass ratio)) and pre-frozen at -100°C using a cooling trap device (Tokyo Rika Kikai UT-4000).Then, using a freeze-dryer (Tokyo Rika Kikai FDU-2200), the mixture was freeze-dried at 10 Pa or less for 48 hours to obtain a freeze-dried product of drug-loaded PEG-LNP1.
[0084] [Production of lipid nanoparticle-containing nanofiber nonwoven fabric (LNP-NFS)] 1. Liposome-containing nonwoven fabric No. 1 and 2: The PEG-LNP1 and PEG-LNP2 prepared above were added to the aqueous PVA resin solution in the mixing ratios shown in Table 1, and then the mixture was stirred to obtain a liposome-containing PVA solution (spinning solution). Using a syringe pump (Yutaka Electronics Manufacturing Co., Ltd.) and a high voltage generator (HVU-30P100 manufactured by MEC Co., Ltd.), the liposome-containing PVA solution was filled into a plastic 5 mL syringe and placed in the syringe pump. Nanofiberization was carried out for 10 hours with the nozzle diameter set to 22 G, the voltage between the electrodes set to 11 kV, the distance from the nozzle tip to the collection plate set to 12 cm, and the discharge rate of the liposome-containing PVA solution set to 0.5 ml / hour, forming a nonwoven fabric on the collection plate to produce liposome-containing nanofiber nonwoven fabrics (LNP-NFS1, LNP-NFS2).
[0085] [Table 1]
[0086] 2. Drug-containing liposome-containing nanofiber nonwoven fabric (drug-containing LNP-NFS) A nanofiber nonwoven fabric containing liposomes was produced in the same manner as above, except that a freeze-dried drug-containing PEG-LNP was used instead of PEG-LNP. The resulting nanofiber nonwoven fabric is called drug-containing LNP-NFS3. The composition of the spinning solution used for drug-containing LNP-NFS3 is shown in Table 2 below.
[0087] [Table 2]
[0088] [Evaluation method and evaluation] 1. Uniformity of nanofibers containing lipid nanoparticles The morphology of the lipid nanoparticle-containing nanofiber nonwoven fabrics (LNP-NFS) No. 1 and No. 2 prepared above was observed with a SEM (JCM-7000, manufactured by JEOL Ltd.) to evaluate the uniformity of the lipid nanoparticle-containing nanofibers. A carbon double-sided tape for SEM (Nissin EM Cat. No. 7321) was attached to the sample stage, and the nanofiber sample was attached on top of it. After that, platinum coating was applied using an ion coating device (JEOL DII-29010SCTR SmartCoater), and observation was performed using a scanning electron microscope (SEM) in a vacuum state under an accelerating voltage of 15 kV-20 kV. The SEM photographs of nanofiber nonwoven fabrics No. 1 and No. 2 are shown in Figure 1A and Figure 1B, respectively.
[0089] It was confirmed that the nanofiber nonwoven fabric (LNP-NFS) No. 1 containing PEG-LNP1 was a uniform nanofiber without any aggregates (beads).The nanofiber nonwoven fabric (LNP-NFS) No. 2 yielded fibers with a uniform fiber diameter for the most part, but some aggregates (beads) were observed.
[0090] 2. Structural stability of lipid nanoparticles The nanofiber nonwoven fabrics (LNP-NFS) No. 1 and 2 were mixed with 8 g of distilled water (9.9 g) to redisperse the PEG-LNPs contained in the nanofiber nonwoven fabrics in water. The particle size and polydispersity index of the redispersed lipid nanoparticles were measured using a ZETASIZER Nano. For reference, the average particle size and polydispersity index measured for PEG-LNP1 and its freeze-dried product used in preparing the spinning dosing solution are also shown in Table 3.
[0091] [Table 3]
[0092] It was confirmed that the lipid nanoparticles extracted from the nanofiber nonwoven fabric, regardless of whether they were frozen or not, maintained the average particle size of the lipid nanoparticles before the spinning solution was prepared, and the polydispersity index was also maintained at 0.5 or less (0.2 or less). In particular, in the case of LNP-NFS2, despite the high liposome content of 60% or more, it was confirmed that the average liposome particle size was 150 nm or less, and aggregation was suppressed. It is thought that the polyvinyl alcohol resin used as the water-soluble resin acts as a dispersion stabilizer.
[0093] 3. Mucoadhesiveness evaluation The results were evaluated using the flow-through method (Eliyahu, S., Aharon, A. & Bianco-Peled, H. Acrylated chitosan nanoparticles with enhanced mucoadhesion. Polymers (Basel). 10, 1-17 (2018).)). A nanofiber nonwoven fabric (drug-containing LNP-NFS3) made using drug-containing liposomes (drug-containing PEG-LNP1) was placed on a porcine stomach tissue slice, and the amount of drug dissolved was quantified by dropping the second solution for dissolution test (manufactured by Nacalai Tesque, Inc.) onto the slice to mimic mucus clearance. As a comparative example for reference, the amount of drug dissolved was also quantified when a suspension of drug-containing PEG-LNP1 was used.
[0094] As the porcine stomach tissue (middle part, mucosa part, DARD Co., Ltd.), a square piece of stomach tissue cut into 1.5 cm on each side was used. This stomach tissue piece was attached to the inside of a 50 mL centrifuge tube with a through hole at the bottom using double-sided tape. 200 μL (20 mM) of a liposome suspension encapsulating FD-4 or 16 mg of liposome-containing nanofibers was added to the stomach piece, and incubated for 10 minutes in a dark place at 37°C (small thermo-hygrostat, Yamato Scientific) equipped with a humidifier. The centrifuge tube was tilted 45 degrees from the horizontal, and a peristaltic pump (Masterflex TM L / S, Cole Parmer) and solvent-resistant tubing (Masterflex TM Chem-Durance TM Bio L / S TM Using a precision pump tubing (inner diameter x outer diameter: 0.8 x 4.1 mm), the second solution for the dissolution test was dripped at a rate of 2 mL / min. After the start of dripping, the eluate was collected at 0.25, 0.5, 1, 2, 3, 4, 5, and 10 minutes, and the fluorescence intensity of FD-4 was measured.
[0095] The results are shown in Figure 2. In Figure 2, the horizontal axis indicates the time elapsed after the start of the dissolution test, and the vertical axis indicates the drug concentration in the eluate collected at each time. The black bars indicate the drug concentration in the drug-containing PEG-LNP suspension (comparative example), and the white bars indicate the drug concentration in the drug-containing LNP-NFS3.
[0096] As shown in Figure 2, in the suspension of non-nanofiberized drug-loaded PEG-LNP1, the drug concentration in the eluate was extremely high 0.25 minutes after the start of dripping the eluate, and then dropped significantly. This means that in the case of non-nanofiberized drug-loaded PEG-LNP, most of the liposomes were washed away within 0.25 minutes after reaching the mucosa. On the other hand, in the case of the nanofiber sheet of drug-loaded PEG-LNP1 (LNP-NFS3), the drug concentration of the eluate 0.25 minutes after the start of dripping was less than one-tenth that of the liposome suspension, and the drug concentration of the eluate remained almost constant from 1.5 to 10 minutes. This confirmed that the drug-loaded PEG-LNP was released continuously by the nanofiber adhering to the mucosa.
[0097] 4. Ribosome distribution in nanofiber nonwoven fabric As described below, the PVA resin and liposomes were fluorescently labeled, and fluorescently labeled nanofibers and nanofiber nonwoven fabrics were produced.
[0098] (1) Preparation of fluorescently labeled polyvinyl alcohol (F-PVA) 300 mg of PVA was added to 8 mL of DMSO and 50 μL of pyridine, and dissolved at 100° C. After dissolution, 50 mg of FITC and 20 mg of dibutyltin dilaurate were added and reacted at 100° C. for 2 hours. 50 mL of anhydrous butanol was added to the reaction solution to cause precipitation, and the solution was centrifuged at 3500 rpm for 5 minutes. The above operation of adding butanol and centrifuging was repeated five times to remove unreacted FITC, and the solution was dried under reduced pressure overnight. After drying, the solution was dissolved in distilled water at 80° C. and pre-frozen at -100° C. Then, a freeze dryer (Tokyo Rika Kikai FDU-2200) was used to freeze-dry the solution at 10 Pa or less for 48 hours to obtain fluorescently labeled polyvinyl alcohol (F-PVA).
[0099] (2) Preparation of fluorescently labeled liposomes Fluorescently labeled liposomes were prepared by encapsulating Nile Red in the lipid membrane of liposome 1 as follows. Nile red was added to DSPC 28.05 mg / mL and CHOL 1.934 mg / mL to a concentration of 0.064 mg / mL (DSPC:CHOL:Nile red = 14.5:1.0:0.03 (mass ratio)), dissolved in chloroform, and the solvent was removed under reduced pressure in a water bath at 40 °C using a rotary evaporator (Tokyo Rikakiki N-1110) to prepare a thin film. After drying under reduced pressure overnight or more, the thin film was hydrated using distilled water in a water bath at 60 °C and then extruded with an extruder (AVESTIN LiposoFast TM The liposomes were passed 41 times through a filter with a pore size of 100 nm (Whatman Nucleporo Track-Etoch Membrane) at a pressure of 300 kPa to 400 kPa using a MicroFiber Filter (MicroFiber Filter -Pneumatic) to obtain fluorescently labeled liposome 1 (F-LNP1) containing Nile red.
[0100] The fluorescently labeled liposome (F-LNP1) prepared above was mixed with an aqueous DSPE-PEG solution at a concentration of 12.62 mg / mL (DSPE:DSPE-PEG = 1:2.2 (mass ratio)) and incubated at 60°C for 1 hour to obtain a fluorescently labeled PEG-modified liposome (F-PEG-LNP1). This fluorescently labeled PEG-modified liposome (F-PEG-LNP1) was pre-frozen at -100°C. It was then freeze-dried for 48 hours at 10 Pa or less using a freeze-dryer (Tokyo Rikakikai FDU-2200) to obtain a freeze-dried product of the fluorescently labeled PEG-modified liposome.
[0101] (3) Preparation of fluorescently labeled nonwoven fabric A 5.5% aqueous solution (fluorescently labeled PVA-based resin aqueous solution) containing F-PVA and PVA in a ratio (mass ratio) of 1:9 was prepared. Spinning solutions No. 3 and No. 4 were prepared using the freeze-dried fluorescently labeled liposome (F-PEG-LNP1) in the same mixing ratio as LNP-NFS1 or LNP-NFS2. Using this spinning solution, nanofibers were produced in the same manner as LNP-NFS No. 1, and fluorescently labeled nanofiber nonwoven fabrics No. 3 and No. 4 (F-LNP-NFS3, F-LNP-NFS4) were produced on the collection plate.
[0102] (4) Measurement of liposome distribution in nanofiber nonwoven fabric The fluorescently labeled nanofiber nonwoven fabric (F-LNP-NFS) prepared above was placed on a glass slide, and a cover glass was placed on top and secured with cellophane tape to prepare a sample for measurement. Observation was performed by CLSM (Carl Zeiss LSM 700). Photographs of fluorescently labeled lipid nanoparticle-containing nanofiber nonwoven fabrics No. 3 and No. 4 are shown in Figures 3 and 4, respectively. The observation of the fluorescent label of the PVA resin and the fluorescent label of the liposomes (Nile Red) were performed under the following conditions. In Figures 3 and 4, A is a photograph of the fluorescent label of the PVA resin, B is a photograph of Nile Red, and C is a composite of photographs A and B.
[0103] Observation of fluorescent labels on PVA-based resins EGFP 488nm Gain 750 Pinhole 68.3 Laser Intensity 10.0
[0104] Observation of liposome label (Nile Red) Rhoda 555nm Gain 730 Pinhole 68.3 Laser Intensity 10.0
[0105] In both Figures 3 and 4, the nanofiber state could be observed in Photograph B, which was an image of Nile Red. This confirmed that lipid nanoparticles were contained in the nanofibers and were uniformly distributed within the nanofibers.
[0106] 5. Liposome behavior in the digestive tract (1) Preparation of ICG-labeled LNP Lipid nanoparticles encapsulating the fluorescent reagent ICG were prepared as follows, and the behavior of the liposomes in the digestive tract was evaluated. DSPC was dissolved in chloroform to a concentration of 28.05 mg / mL, CHOL was dissolved in 1.934 mg / mL, and indocyanine green (ICG) was dissolved in chloroform to a concentration of 40 μg / mL. The solvent was removed under reduced pressure using a rotary evaporator (Tokyo Rikakiki N-1110) in a water bath at 40 °C to prepare a thin film. After drying under reduced pressure overnight or more, the thin film was hydrated using distilled water in a water bath at 60 °C and then extruded with an extruder (AVESTIN LiposoFast TM The mixture was passed 41 times through a filter having a pore size of 100 nm (Whatman Nucleporo Track-Etoch Membrane) at a pressure of 200 kPa to 300 kPa using a pressure adjuster (Mitsubishi Microwave Oven) (Mitsubishi Microwave Oven). ICG-labeled liposomes were obtained. The ICG-labeled liposomes were mixed with an aqueous DSPE-PEG solution to a concentration of 12.62 mg / mL (DSPC:DSPE-PEG=1:2.2 (mass ratio)) and incubated at 60° C. for 1 hour to prepare ICG-labeled PEG-modified liposomes. HPβCD was mixed with the ICG-labeled PEG-modified liposomes to a concentration of 21.3 mg / mL (phospholipids (DSPC+DSPE-PEG):HPβCD = 20.3:21.3 (mass ratio)) and pre-frozen at -100°C. Then, using a freeze dryer (Tokyo Rika Kikai FDU-2200), the mixture was freeze-dried at 10 Pa or less for 48 hours to obtain a freeze-dried product of ICG-labeled PEG-modified liposomes.
[0107] (2) Preparation of spinning solution and fabrication of nanofiber nonwoven fabric The frozen ICG-labeled PEG-modified liposomes prepared above were dissolved in 5 mL of PVA aqueous solution (5.5%) to obtain a spinning solution. The mixing ratio of PVA resin and PEG-modified liposomes in the spinning solution was the same as that of lipid nanoparticle-containing nanofiber nonwoven fabric (LNP-NFS) No. 1.
[0108] Using this spinning dope, nanofibers were produced in the same manner as for LNP-NFS No. 1, to obtain nanofiber nonwoven fabric No. 5.
[0109] (3) Measurement of pharmacokinetics in the gastrointestinal tract Male Wistar rats (Japan SLC, 8 weeks old) that had been fasted for 24 hours prior to administration were anesthetized with isoflurane inhalation and intragastrically administered a No. 9 gelatin capsule filled with 16 mg of the nanofiber nonwoven fabric prepared above using a mini capsule administering device (Natsume Seisakusho, administration needle: 1.8 x 100 mm, cup: 3.4 x 7 mm).
[0110] For comparison, a suspension of frozen ICG-labeled PEG-modified liposomes used to prepare the spinning solution was administered intragastrically using an oral probe attached to a 1 mL syringe (manufactured by Fuchigami Instruments, tip diameter: 2.3 mm, outer diameter: 1.2 × 80 mm).
[0111] Four hours after administration, the rats were euthanized by isoflurane hyperanesthesia, the small intestine was removed, and the ICG-derived fluorescence was observed using IVIS (IVIS Lumina2, Caliper Life Sciences) under the conditions described below.
[0112] The excised small intestine was divided into three sections (upper, middle, and lower), and the retention in the digestive tract was measured based on the fluorescence intensity (total radiant efficiency) ratio using Living Image Software. The measurement results for each section are shown in Figure 5. In Figure 5, the vertical axis represents the fluorescence intensity. In FIG. 5, the black bars represent the suspension of ICG-labeled PEG-modified liposomes (Comparative Example), and the white bars represent the measurement results of the lipid nanoparticle-containing nanofiber nonwoven fabric.
[0113] (4) Measurement conditions Ex filter: 745 nm Em filter: 820 nm Binning: Medium Exposure time: 1sec F / stop: 2
[0114] Total Radiant Efficiency[p / s] / [μW / cm 2 ]= Radiated brightness at the skin surface (photon / sec) / excitation light intensity (μW / cm 2 )
[0115] (5) Evaluation results The fluorescence intensity in the middle and lower parts of the small intestine was higher with the nanofiber nonwoven fabric than with the non-nanofiber liposome suspension. The total amount of detected fluorescence intensity was also higher with the liposome suspension. From the above results, it is considered that in the case of the non-nanofiberized liposome suspension, some of the liposomes had already reached the cecum due to clearance by the small intestinal mucus, and the amount of liposomes remaining in the small intestine was reduced.
[0116] On the other hand, in the case of the nanofiber nonwoven fabric using nanofibers containing lipid nanoparticles, the retention in the digestive tract was improved by nanofiberization, and it was confirmed that the liposomes remained in the digestive tract for a longer period 4 hours after administration. From this, it was confirmed that the nanofibers of the present invention have improved retention in the digestive tract and can efficiently deliver the drug in the liposome. [Industrial Applicability]
[0117] The lipid nanoparticle-containing nanofibers of the present invention have a uniform fiber diameter, high mucoadhesion, and are uniformly distributed in the nanofibers while maintaining the liposome structure. Therefore, a liposome preparation using a nanofiber nonwoven fabric with high mucoadhesion due to the water-soluble resin used as the nanofiber substrate can be delivered to a specific mucosa while maintaining the liposome structure, and after the lipid nanoparticles permeate through the mucosa, the drug encapsulated in the lipid nanoparticles can be released. Therefore, since the DDS formulation using the lipid nanoparticle-containing nanofiber of the present invention can remain in the digestive tract for a long period of time, it can be used as an oral agent, patch, or tape, reducing the frequency of administration.
Claims
1. A lipid nanoparticle-containing nanofiber comprising a water-soluble resin including a polyvinyl alcohol-based resin and lipid nanoparticles.
2. The lipid nanoparticle-containing nanofiber according to claim 1, wherein the content of the polyvinyl alcohol-based resin in the water-soluble resin is 50% by weight or more.
3. The lipid nanoparticle-containing nanofiber according to claim 1 , wherein the lipid nanoparticle is a liposome.
4. The lipid nanoparticle-containing nanofiber of claim 1 , further comprising a drug, the drug being retained within the lipid nanoparticle.
5. The lipid nanoparticle-containing nanofiber according to claim 3 , further comprising a drug, the drug being encapsulated within the liposome.
6. The lipid nanoparticle-containing nanofiber according to claim 1 , wherein the lipid nanoparticles are composed of phospholipids or cationic lipids.
7. The lipid nanoparticle-containing nanofiber according to claim 1 , wherein the lipid nanoparticle has a hydrophilic polymer modifying group.
8. The lipid nanoparticle-containing nanofiber according to claim 1, wherein the content ratio of the polyvinyl alcohol resin to the lipid constituting the lipid nanoparticle is 99.5:0.5 to 60:40 by mass ratio.
9. The lipid nanoparticle-containing nanofiber according to claim 1, wherein the polyvinyl alcohol resin has a degree of saponification of 80 to 94 mol%.
10. The lipid nanoparticle-containing nanofiber according to claim 1, wherein the average particle diameter of the lipid nanoparticles is 10 to 1000 nm.
11. A lipid nanoparticle-containing nanofiber nonwoven fabric comprising a layer of lipid nanoparticle-containing nanofibers according to any one of claims 1 to 10.
12. A mucoadhesive preparation comprising the nanofiber nonwoven fabric of claim 11.
13. A method for producing nanofibers containing lipid nanoparticles, comprising the step of electrospinning a mixture of an aqueous solution containing a polyvinyl alcohol-based resin and a solution containing lipid nanoparticles and a drug.
Citation Information
Patent Citations
Liposome pharmaceutical preparation
JP1993194191A
Drug-containing ultrafine fiber and utilization thereof
JP2014055119A
Drug-containing fiber, method for producing the same, and oral preparation composed of the fiber
JP2021088552A