Part for timepiece movement
Austenitic steels with selectively hardened outer surfaces using nitrogen and carbon diffusion address magnetic susceptibility and corrosion issues, enhancing pivot pin durability and performance.
Patent Information
- Application Number
- JP2024126512
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2013-01-17
- Filing Date
- 2024-08-02
- Publication Date
- 2024-10-11
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing pivot pins for mechanical watch movements are susceptible to magnetic fields, prone to corrosion, and lack sufficient hardness and wear resistance, which can disrupt watch operation and reduce longevity.
Austenitic steels or alloys are used for pivot pins, with a hardened outer surface achieved through selective diffusion of nitrogen and/or carbon atoms to a predetermined depth, maintaining the pin's core integrity and improving corrosion resistance and hardness.
The solution provides non-magnetic pivot pins with enhanced hardness, wear resistance, and corrosion resistance, ensuring reliable watch operation without magnetic interference and material delamination.
Smart Images

Figure 2024144687000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to components for clock movements, in particular for mechanical clock movements. More specifically, the present invention relates to non-magnetic pivot pins for a non-magnetic balance shaft, pallet shaft and escapement pinion. Regarding. [Background technology]
[0002] The manufacture of pivot pins for watches requires the use of a number of different working surfaces (shoulders, protrusions, tenons, etc.) The pin is then cut into a hardenable steel bar using a bar turning process. At least one hardening operation to improve the hardness and one or more hardening operations to improve the roughness The pin is then subjected to a heat treatment process that includes multiple tempering operations. This is followed by rolling the tenons, which consists of grinding the tenons to the desired dimensions. The rolling process also improves the hardness and roughness of the tenons. It should be noted that this is not even achievable for materials with a hardness below 600HV.
[0003] Pivot pins conventionally used in mechanical watch movements, such as balance pins, can be machined from bar stock. They are made from steel grades that are generally treated with lead and manganese sulfides to improve machinability. This type of steel, called 20AP, is a martensitic carbon steel containing 100% Cr. Known types of steels are typically used.
[0004] This type of material has the advantage of being easy to machine, especially for bar turning. This has the advantage that, after hardening and tempering, it is extremely advantageous for making pivot pins for watches. These steels have excellent mechanical properties, especially after heat treatment, excellent wear resistance and hardness. Typically, the tenon hardness of a pin made of 20AP steel is 700H after heat treatment and rolling. It can exceed V.
[0005] This type of material offers sufficient mechanical properties for the horological applications described above, but This material is magnetic and is used in particular to make a balance spring which cooperates with a ferromagnetic material. The use of this material for this purpose has the drawback that the operation of the watch may be interrupted after being exposed to a magnetic field. This phenomenon is well known to those skilled in the art and is described, for example, in It should also be noted that these martensitic steels are also sensitive to corrosion. do.
[0006] Austenite, which has the property of being non-magnetic, i.e. paramagnetic, diamagnetic or antiferromagnetic Attempts have been made to overcome these drawbacks by using stainless steels. However, these austenitic stainless steels have a crystalline structure, which is Stainless steels cannot be hardened or do not meet the requirements for making pivot pins for watches. This means that the appropriate hardness and therefore wear resistance cannot be achieved. One means of hardening is by cold working, but this hardening operation does not achieve hardnesses above 500 HV. Therefore, parts that require high resistance to wear due to friction and where the risk of deformation is almost zero For tenons where there is no risk of deformation or deformation, it is not necessary to use this type of steel. However, there are limitations.
[0007] Another approach aimed at overcoming these shortcomings is the use of diamond-like carbon ( This involves depositing a hardened layer of material, such as DLC, onto the pivot pin. A significant risk of delamination was observed, which could result in the movement of the watch causing the watch to malfunction. This is unsatisfactory as the formation of debris has been observed which can disrupt operation.
[0008] To overcome the shortcomings of austenitic stainless steels, yet another approach, namely, nitrogen Surface hardening of the pivot pin by annealing, carburizing or carbonitriding has been proposed. In this treatment, nitrogen and / or carbon react with the chromium in the steel to form chromium nitrides and / or chromium carbides. The formation of chromium causes localized wear of the chromium matrix, resulting in corrosion resistance. is known to significantly decrease, which makes desirable clock applications difficult. [Prior art documents] [Non-patent literature]
[0009] [Non-Patent Document 1] Bulletin Annuel Suisse de Chromometrie, Volume 1, Pages 52-74 Summary of the Invention [Problem to be solved by the invention]
[0010] The object of the present invention is to limit the susceptibility to magnetic fields and to improve the resistance required in the watch industry. A pivot pin capable of achieving improved hardness to meet wear and impact resistance requirements. What is proposed is to overcome all or part of the above mentioned drawbacks.
[0011] It is also an object of the present invention to provide a non-magnetic pivot pin having improved corrosion resistance. do.
[0012] It is yet another object of the present invention to provide a non-magnetic pivot pin which is simple and economical to manufacture. It is. [Means for solving the problem]
[0013] The present invention therefore relates to a metallic pivot pin for a clock movement, said pivot pin having an end At least one tenon is provided on at least one of the portions, and the metal is adapted to be in contact with the magnetic field of the pivot pin. To limit susceptibility, austenitic steel, austenitic cobalt alloy or austenitic a nickel alloy having a nickel-nickel base, and at least an outer surface of the at least one tenon The surface is characterized by being hardened to a predetermined depth relative to the center of the pin.
[0014] As a result, the surface area or the entire pin is hardened, i.e. the center of the pin remains almost unchanged By selectively hardening portions of the pin in this way, the pivot pin is In addition to having good corrosion resistance while still maintaining a consistent overall roughness, The advantages of this type include low susceptibility to cracking and hardness in the principal stress region. The use of austenitic steels has the advantage that they can be largely machined. .
[0015] According to other advantageous features of the invention: - the predetermined depth is between 5 and 40% of the total diameter d of the tenon, typically between 5 and 35 microns; The hardened outer surface contains diffused atoms of at least one chemical element, The other chemical element is a non-metal, preferably nitrogen and / or carbon; -The hardened outer surface has a hardness of over 1000HV.
[0016] Furthermore, the invention relates to a clock movement, said movement being any of the above-mentioned variants. In particular, these pivot pins include the balance pin, the pallet pin, and and / or an escapement pinion.
[0017] Finally, the invention relates to a method for manufacturing a pivot pin, comprising the following steps: a) Austenitic steel, austenitic edge, to limit susceptibility to magnetic fields At least one end of the alloy or austenitic nickel alloy substrate is forming a pivot pin including a tenon; b) To harden the pivot pin while maintaining a high roughness in the main stressed areas, Diffusing atoms to a predetermined depth on at least an outer surface of the at least one pivot. Step 1:
[0018] As a result, by diffusing atoms into steel or cobalt or nickel alloys, The entire surface area or tenon is hardened without the need to deposit a second material on top of the tenon. The hardening takes place within the material of the pivot pin, which according to the invention is advantageously a hardening agent deposited on the pin. This prevents any subsequent delamination that may occur in the layers.
[0019] Furthermore, the present invention aims to diffuse carbon and / or nitrogen atoms into the interstitial sites of the alloy. Thermochemical treatment does not, in principle, form carbon and / or nitrogen which could impair the corrosion resistance of the pivot pin. stomach.
[0020] According to other advantageous features of the invention: - the given depth means 5-40% of the total diameter d of the tenon; The atoms are at least one chemical element, preferably a non-metal, such as nitrogen and / or carbon. Includes; - step b) consists of a thermochemical diffusion treatment; - step b) consists of ion implantation and diffusion treatments; - The tenons are rolled or ground after step b).
[0021] Further characteristics and advantages are set forth in the following description, given by way of non-limiting illustration with reference to the accompanying drawings, in which: It will become clearer from the light. [Brief description of the drawings]
[0022] [Figure 1] FIG. 1 is a diagram of a pivot pin according to the present invention. [Diagram 2] FIG. 2 is a partial cross-sectional view of a tenon of a balance according to the invention after a diffusion treatment operation and before a rolling or grinding operation. [Diagram 3] FIG. 3 is a partial cross-sectional view similar to FIG. 2, showing the tenon after the diffusion treatment operation and before the rolling or grinding operation. [Figure 4] FIG. 4 is a graph showing the hardness profile from the surface to the center of a tenon of a balance post according to the present invention after diffusion treatment and before rolling or polishing treatment. [Diagram 5] FIG. 5 is a graph showing the hardness profile from the surface to the center of a tenon of a balance post according to the present invention after a diffusion treatment and after a rolling or polishing treatment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0023] The present invention relates to components for a clock movement, in particular a mechanical clock movement. This invention relates to a non-magnetic pivot pin for a
[0024] The invention will now be described with reference to its application to a non-magnetic balance shaft 1 as a pivot pin. For example, the wheel set of a watch, typically the escapement pinion or anchor, Other types of clock pivot pins, such as a clock bar, may also be envisaged.
[0025] Referring to FIG. 1, a balance head 1 according to the present invention is illustrated, which has different diameters. The structure includes a plurality of portions 2, the portions 2 being typically disposed between two end portions defining a tenon 3. Each of these tenons defines a recessed shoulder 2a and a protruding portion 2b. It is configured to pivot on a bearing within an opening in the ruby.
[0026] Limiting Tenshin 1's sensitivity to magnetism induced by objects it comes into contact with on a daily basis It is important to avoid adversely affecting the operation of the clock in which it is incorporated.
[0027] Surprisingly, the present invention overcomes both problems simultaneously without compromise and provides additional advantages. Therefore, the metal 4 of the base 1 is austenitic and preferably stainless steel. This advantageously limits the susceptibility of the balance to magnetic fields. One outer surface 5 (Figs. 2 and 3) is hardened to a given depth relative to the rest of the stele, This advantageously provides excellent adhesion while maintaining a high degree of roughness on the outer surface. It can provide hardness.
[0028] In fact, according to the present invention, it is possible to obtain a hardness of more than 1000 HV on the outer surface of the tenon 3. The above values are based on the presence of at least 16.5% Cr and 10% Ni (DIN X2Cr NiMo17-12-2+Su+Cu) with the addition of sulfur and manganese sulfide, Obtained from 6L chromium-nickel austenitic stainless steel. Of course, the composition ratio If it provides paramagnetic, diamagnetic or antiferromagnetic properties and good machinability, other stainless steels Steel may also be envisaged.
[0029] It has been experienced that a hardening depth of 5 to 40% of the total diameter d of tenon 3 is sufficient for application to tenons. For example, when the radius d / 2 is 50 μm, the The hardening depth is preferably about 15 μm. Of course, depending on the application, it may be 5 to 80% of the total diameter d. It is possible to provide different cure depths.
[0030] Preferably according to the invention, the hardened outer surface 5 of the pivot 3 is treated with nitrogen and / or carbon. It contains at least one diffused atom of a nonmetallic material. In fact, as explained below, in Steel 4 Through interstitial saturation of atoms in the lattice, the surface can be etched without the need to deposit a second material on top of the pin 3. The area 5 hardens. In fact, the hardening takes place within the material 4 of the tenon 3, which is advantageous according to the invention. This prevents any subsequent delamination during use.
[0031] Thus, at least one surface area 5 is hardened, i.e. the center of the tenon 3 and / or the pin. The remaining part of the material is either almost unchanged without significantly changing the mechanical properties of the material 1, or As a result of such selective modification of the tenon 3, good corrosion resistance is obtained. Low susceptibility to magnetic fields, in the main stress areas, while maintaining strength and fatigue resistance The advantages of hardness and high roughness can be combined.
[0032] The present invention also relates to a method for producing a bar as described above. The method of the present invention advantageously comprises: It includes the following steps: a) To limit the susceptibility of the balance to magnetic fields, the base material is made of austenitic steel, Step 1 to form a tenon 3; b) at least the outer surface 5 of the tenon 3 in order to harden the tenon in the main area where stress is applied; Diffusing atoms to a predetermined depth in the
[0033] According to a first preferred embodiment, the necessary dimensions and final surface finish of the tenon 3 are achieved. In order to achieve this, the tenon 3 is rolled or ground after step b). It has improved wear resistance and impact resistance compared to pins that have only had the tenon hardened. You get a pin that
[0034] The results shown in Figures 4 and 5 were based on the Tenshin, which had been subjected to the diffusion treatment of step b) on all surfaces. From the graph, the surface of the pin including the surface of tenon 3 is approximately 1300HV (curve A, Figure 4). Contrary to expectations, the surface layer 5a (the dark layer in FIG. 2) The rolling operation which removed a part of the tenon 3 also removed the hardest part of the surface layer 5 of the tenon 3, and Nevertheless, the surface hardness of tenon 3 (curve B, Fig. 5) remains advantageously above 1000 HV. This provides tenon 3 with satisfactory wear resistance properties for the relevant application. You will also understand.
[0035] Advantageously, according to the invention, regardless of the embodiment, the method can be applied to bulk conditions. Thus, step b) involves the carburizing or nitriding of the plurality of balance shafts and / or the unfinished components of the plurality of balance shafts. Step b) may preferably consist of a thermochemical treatment such as by adding nitrogen and / or carbon It is clear that this can be achieved by interstitial diffusion of atoms of nonmetallic chemical elements into steel 4. Finally, advantageously, the compressive stress of the present method improves fatigue and impact resistance. I found out that...
[0036] Step b) may also consist of an ion implantation step and / or a thermal diffusion treatment. This embodiment has the advantage of being unlimited in the type of diffusing atoms, and of being capable of both interstitial and substitutional diffusion. The advantage of this method is that it allows both the injection and dispersion of the liquid.
[0037] Of course, the invention is not limited to the described embodiment, and various modifications and variations will become apparent to those skilled in the art. Various modifications and variations are possible. In particular, it is not essential for application to pivot pins such as those of clocks. However, the tenon 3 is entirely or almost entirely processed, i.e., 80% or more of the diameter d of the tenon 3 is processed. It is possible to envisage this.
[0038] According to the invention, the basic material for making the pivot pin is also at least cobalt. Austenitic cobalt alloys containing 39% Co, typically 39% Co, 19% C r, 15% Ni, 6% Mo, 1.5% Mn, 18% Fe and the balance consisting of additives. The alloy known as DIN K13C20N16Fe15D7, or at least Both are austenitic nickel alloys containing 33% nickel, typically 35% Ni , 20% Cr, 10% Mo, 33% Co and the balance being additives, MP3 It may be made of the alloy known as 5N®. [Explanation of symbols]
[0039] 1 Pivot pin, balance 2 parts 3 Tenon 4 metals, steel, materials 5. Tenon outer surface d Total diameter
Claims
1. 1. A metallic pivot pin for a clock movement, comprising: the pivot pin includes at least one tenon on at least one of its ends; The metal is austenitic to limit the susceptibility of the pivot pin to magnetic fields. steel, austenitic cobalt alloy or austenitic nickel alloy; and At least the outer surface (5) of the at least one tenon (3) is aligned with the center of the pivot pin. The nitrogen is introduced through carbon and / or nitrogen interstitial atoms to a predetermined depth. The hardened layer is hardened without forming chromium oxide and / or chromium carbide. , pivot pin.
2. 1. A method for manufacturing a metallic pivot pin for a timepiece movement, comprising the steps of: a) Austenitic steel, austenitic cobalt, etc., to limit susceptibility to magnetic fields. At least one of the pivot pins is made of a base material of a nickel alloy or an austenitic nickel alloy. forming said pivot pin with at least one tenon (3) at one end; b) at least one of the tenons (3) is hardened to harden the tenon (3); Diffusion of carbon and / or nitrogen atoms into interstitial sites at the outer surface to a predetermined depth. This step forms a hardened layer with negligible formation of chromium nitride and / or chromium carbide. P The method includes:
3. 1. A method for manufacturing a metallic pivot pin for a timepiece movement, comprising the steps of: a) At least 16.5% Cr and 10% Austenitic chromium-nickel stainless steel containing Ni, at least 39% Cobalt austenitic cobalt steels containing at least 33% nickel; At least one of the pivot pins is made of a metal substrate selected from the group including nickel-nickel steel. forming said pivot pin including at least one tenon (3) at an end thereof; b) at least one of the tenons (3) is hardened to harden the tenon (3); Chromium nitride is formed by diffusing atoms into interstitial positions at the outer surface to a predetermined depth. and / or forming a hardened layer that reduces the effect of corrosion resistance due to the formation of chromium carbide. The method includes:
Citation Information
Patent Citations
Surface treatment for metallic material
JP1996134700A
Metal part, gear device, power transmission device, and apparatus having the part and devices
JP2003214526A
High-temperature gas valve with corrosion-resistant protective layer