Manufacturing method of electronic device and the electronic device

By reinforcing the solder connection structure with thermosetting resin, the impact resistance of electronic devices is improved, addressing breakage issues at the semiconductor chip-solder bump interface and enhancing manufacturing efficiency.

JP2024145229AActive Publication Date: 2024-10-15SENJU METAL IND CO LTD

Patent Information

Application Number
JP2023057491
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-15
Estimated Expiration
2043-03-31

AI Technical Summary

Technical Problem

Existing electronic device manufacturing methods using low-temperature solder bumps lack sufficient impact resistance, particularly at the interface between the semiconductor chip and the solder bumps, leading to breakage during drops.

Method used

Reinforce the solder connection structure between the semiconductor chip and low-temperature solder bumps with thermosetting resin by applying thermosetting flux or solder paste to form resin reinforcing portions on the chip and board, ensuring a specific resin height and width ratio, and omitting the mold underfill material process.

Benefits of technology

Enhances the impact resistance of electronic devices by reducing damage to the solder joints, improving manufacturing efficiency, and avoiding issues associated with mold underfill materials.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024145229000001_ABST
    Figure 2024145229000001_ABST
Patent Text Reader

Abstract

To provide a manufacturing method of an electronic device having an excellent impact resistance.SOLUTION: A manufacturing method of an electronic device of the present invention, contains: a solder bump formation step of forming a solder bump by bonding an upper part of a solder ball formed by a low melting point solder while contacting at least one upper fixing material of a thermosetting property flux and a thermosetting property solder paste to an electrode part of a lower surface of a semiconductor chip; and a mounting step of bonding the lower part of the solder bump to be bonded to the semiconductor chip against the electrode part of the upper surface of a mounting substrate. In the solder bump formation step, a resin hardening material of a flux residue in the upper fixing material becomes a state of being held to the lower surface of the semiconductor chip and the upper part of the solder bump.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a manufacturing method of an electronic device and to an electronic device. [Background technology]

[0002] Various soldering methods have been developed for use in the manufacturing process of electronic devices. Known examples of this type of technology include the technology described in Patent Document 1. Patent Document 1 describes a method in which a first bond is applied to the solder bumps of an electronic component with bumps, the component is aligned with and mounted on electrodes on a substrate, and then a second bond is filled into the entire space between the electronic component with bumps and the substrate using a dispenser (see, for example, Figures 1 and 2 of Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2000-031187 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, as a result of investigations by the present inventors, it has become clear that the method for manufacturing an electronic device described in Patent Document 1 leaves room for improvement in terms of the impact resistance of the electronic device. [Means for solving the problem]

[0005] It is generally known that when low-temperature solder having a low melting point is used for soldering, the impact resistance of the electronic device when dropped is low. Therefore, as in the solder connection method of Patent Document 1 mentioned above, reinforcing the lower part of the low-temperature solder bump and the upper surface of the mounting board with a thermosetting resin was considered, but it was not possible to sufficiently increase the impact resistance. The inventors observed breakage points when an electronic device using low-temperature solder bumps was dropped, and found many breakage points between the bottom surface of the semiconductor chip and the lower part of the low-temperature solder bumps. As a result of further intensive research based on this knowledge, the inventors discovered that the impact resistance of electronic devices using low-temperature solder can be improved by reinforcing with resin the solder connection structure between the electrode portion on the underside of the semiconductor chip and the lower portion of the low-temperature solder bump, which led to the completion of the present invention.

[0006] According to one aspect of the present invention, there is provided the following manufacturing method for an electronic device and the electronic device. 1. A solder bump forming process in which an upper fixing material, which is at least one of a thermosetting flux and a thermosetting solder paste, is brought into contact with an electrode portion on the lower surface of a semiconductor chip, and an upper portion of a solder ball made of a low melting point solder is joined to the electrode portion to form a solder bump; a mounting process of joining lower portions of the solder bumps joined to the semiconductor chip to electrode portions on an upper surface of a mounting substrate, In the solder bump forming step, a cured resin of flux residue in the upper fixing material is held by the lower surface of the semiconductor chip and the upper portions of the solder bumps. 2. A method for manufacturing the electronic device according to claim 1, comprising the steps of: The mounting step includes: supplying at least one lower fixing material of a thermosetting flux and a thermosetting solder paste to the lower part of the solder bump joined to the semiconductor chip or to the electrode part on the upper surface of the mounting substrate; a lower portion of the solder bump is joined to the electrode portion on the upper portion of the mounting substrate; In the mounting step, a cured resin of flux residue in the lower fixing material is held on the upper surface of the mounting substrate and on the lower parts of the solder bumps. 3. A method for manufacturing the electronic device according to claim 2, comprising the steps of: After the mounting process, the height of the solder bumps in one cross section of the mounting substrate is HB The resin height of the lower resin reinforcement part made of the resin cured product of the flux residue in the lower fixing material is H E Then, H E / H B x 100, the resin height ratio is 10% or more. 4. A method for manufacturing the electronic device according to 2., After the mounting process, the radius of the solder bump is W B The resin width of the lower resin reinforcement part made of the resin cured product of the flux residue in the lower fixing material is W E Then, W E / W B x 100, the resin width ratio is 30% or more. 5. A method for manufacturing an electronic device according to any one of 1. to 4., A method for manufacturing an electronic device, which does not include a step of filling all of the gap between the mounting substrate and the semiconductor chip with a mold underfill material after the mounting step. 6. A method for manufacturing an electronic device according to any one of 1. to 5., A method for manufacturing an electronic device, comprising the steps of: (a) forming a solder bump on a substrate; (b) mounting the solder bump on the substrate; 7. A method for manufacturing an electronic device according to any one of 1. to 6., A method for manufacturing an electronic device, wherein the melting point of the solder ball made of the low melting point solder is 180°C or lower, when the solidus temperature is taken as the melting point. 8. A method for manufacturing an electronic device according to any one of 1. to 7., the thermosetting flux comprises a thermosetting resin and an activator; The method for manufacturing an electronic device, wherein the thermosetting solder paste comprises the thermosetting flux and solder powder. 9. A method for manufacturing an electronic device according to any one of 1. to 8., When the thermosetting flux or the thermosetting flux contained in the thermosetting solder paste is measured using a differential scanning calorimeter (DSC) based on a DSC curve measured at a temperature rise rate of 20°C / min in the range of 25°C to 250°C, A method for manufacturing an electronic device, wherein the heat generation peak temperature is from [T+10]°C to [T+50]°C, where T is the melting point of the solder ball made of the low melting point solder. 10. A mounting board; A semiconductor chip; a solder bump made of a low melting point solder for joining an electrode portion on the upper surface of the mounting substrate and an electrode portion on the lower surface of the semiconductor chip; an upper resin reinforcing portion held by a lower surface of the semiconductor chip and upper portions of the solder bumps, the upper resin reinforcing portion being made of a thermosetting flux or a resin cured product of flux residue of a thermosetting solder paste. 11. An electronic device according to claim 10, an electronic device comprising a lower resin reinforcing portion held by an upper surface of the mounting substrate and by lower portions of the solder bumps, the lower resin reinforcing portion being made of a thermosetting flux or a resin cured product of flux residue of a thermosetting solder paste. 12. An electronic device according to claim 11, In one cross section of the mounting board, the height of the solder bump is H B , the resin height of the lower resin reinforcement part is H E Then, H E / H B x 100 is 10% or more. 13. The electronic device according to claim 10 or 11, In one cross section of the mounting substrate, the radius of the solder bump is W B , the resin width of the lower resin reinforcement part is W E Then, W E / W B x 100, the resin width ratio of which is 30% or more. 14. The electronic device according to any one of 11 to 13, an air gap that is not filled with a mold underfill material is formed between the upper surface of the mounting substrate and the lower surface of the semiconductor chip; Effect of the Invention

[0007] According to the present invention, a method for manufacturing an electronic device having excellent impact resistance is provided. [Brief description of the drawings]

[0008] [Figure 1] 1A to 1C are cross-sectional views illustrating a process for manufacturing the semiconductor device according to the present embodiment. [Diagram 2] 1A to 1C are cross-sectional views illustrating a process for manufacturing the semiconductor device according to the present embodiment. [Diagram 3] 1 is a diagram illustrating an example of a semiconductor device according to an embodiment of the present invention; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In all drawings, similar components are given similar reference numerals and their explanations will be omitted as appropriate. Also, the drawings are schematic diagrams and do not correspond to the actual dimensional ratios. In the present embodiment, the directions of front, back, left, right, top and bottom are defined as shown in the drawings. However, this is defined for the sake of convenience in order to easily explain the relative relationships of the components. Therefore, it does not limit the directions during the manufacture or use of the product embodying the present invention.

[0010] An outline of the method for manufacturing the electronic device according to this embodiment will be described. The manufacturing method for an electronic device of this embodiment includes a solder bump formation process in which an upper part of a solder ball made of low melting point solder is joined to an electrode part on the underside of a semiconductor chip while contacting the upper fixing material, which is at least one of a thermosetting flux and a thermosetting solder paste, to form a solder bump, and a mounting process in which a lower part of the solder bump joined to the semiconductor chip is joined to an electrode part on the upper surface of a mounting substrate, and in the solder bump formation process, a resin cured product of the flux residue in the upper fixing material is held by the underside of the semiconductor chip and the upper part of the solder bump.

[0011] According to the findings of the present inventors, it has been found that the impact resistance of electronic devices can be improved by reinforcing with resin the lower surface of the semiconductor chip and the upper portions of the solder bumps in the low melting point solder joints.

[0012] Although the detailed mechanism is unclear, it is thought that the upper resin reinforcement part (resin reinforcement structure) held between the underside of the semiconductor chip and the upper part of the low-melting point solder bump absorbs external shocks, such as when dropped, thereby preventing damage to the low-temperature solder joints.

[0013] In one preferred embodiment, in addition to the upper part of the solder bump, the upper surface of the mounting board and the lower part of the low melting point solder bump can be reinforced with a lower resin part (resin reinforcement structure). This further improves the impact resistance of the electronic device. This is expected to extend the life of low temperature solder joints.

[0014] In one preferred embodiment, by reinforcing the upper part of the low melting point solder bump with resin, or by reinforcing both the upper part and the lower part of the low melting point solder bump with resin, it becomes possible to omit part or all of the filling and curing process of the mold underfill material. In addition, by eliminating the process of filling and curing the molded underfill material, it is possible to avoid problems that arise when using molded underfill material, such as poor curing, migration, and breaks due to expansion.

[0015] <Electronic device manufacturing method> Each step of the method for manufacturing an electronic device according to this embodiment will now be described in detail.

[0016] An example of a method for manufacturing an electronic device according to this embodiment includes at least a solder bump forming step and a mounting step. In the solder bump formation process, the solder balls are soldered to the electrodes of the semiconductor chip via the upper fixing material, while in the mounting process, the solder bumps are soldered to the electrodes of the mounting board via the lower fixing material or a commonly used flux other than the lower fixing material.

[0017] One example of such a mounting process is to supply at least one lower fixing material of thermosetting flux and thermosetting solder paste to the lower part of the solder bump joined to the semiconductor chip or to the electrode part on the upper surface of the mounting substrate, and then to join the lower part of the solder bump to the electrode part on the upper part of the mounting substrate. In such a mounting process, the cured resin of the flux residue in the lower fixing material is held by the upper surface of the mounting substrate and the lower part of the solder bump.

[0018] 1 and 2 are cross-sectional views that typically show an example of a manufacturing process for a semiconductor device according to this embodiment, where Fig. 1 corresponds to a solder bump formation process, and Fig. 2 corresponds to a mounting process. An example of a manufacturing process for a semiconductor device will now be described in detail with reference to FIGS. 1(a) to (c) and 2(a) to (c).

[0019] First, as shown in FIG. 1( a ), an upper fixing material 50 is supplied to the electrode portion 14 on the lower surface 12 of the semiconductor chip 10 . As a supplying method, any of the known supplying methods used for flux or paste can be used, for example, a printing method such as screen printing, a transfer method such as pin transfer, or a discharge method such as jet dispensing or dispensing. Moreover, the supply amount and supply position of the upper fixing material 50 can be designed appropriately.

[0020] Examples of the semiconductor chip 10 include a Mold Array Package (MAP), a Quad Flat Package (QFP), a Small Outline Package (SOP), a Chip Size Package (CSP), a Quad Flat Non-leaded Package (QFN), a Small Outline Non-leaded Package (SON), a Ball Grid Array (BGA), a Lead Flame BGA (LF-BGA), a Flip Chip BGA (FCBGA), a Molded Array Process BGA (MAPBGA), an Embedded Wafer-Level BGA (eWLB), a Fan-In type eWLB, and a Fan-Out type eWLB. In addition to the semiconductor chip 10, any electronic component that can be mounted on a PCB substrate by solder connection can be used without any particular limitation.

[0021] 1(b), the solder balls 20 are mounted on the electrodes 14 covered with the upper fixing material 50. Specifically, after aligning the solder balls 20 with the electrodes 14 on the lower surface 12 side of the semiconductor chip 10, the upper parts of the solder balls 20 are brought into contact with the electrodes 14 via the upper fixing material 50. As the mounting method, a known method can be used, for example, a ball transfer method or a mount method.

[0022] 1(c), the solder balls 20 are heated to a temperature equal to or higher than their melting point to solder the upper portions of the solder balls 20 to the electrode portions 14. Heating is started after the solder balls 20 and the electrode portions 14 are brought into contact with each other, or simultaneously with the contact of the two. As a heating method, reflow in a reflow furnace is preferred. 1(c) as the solder balls 20 melt due to the heat applied during solder bonding and a portion of the solder balls 20 bonds to the electrode portions 14. In the following processes, the solder balls 20 will be referred to as solder bumps 21.

[0023] When the solder balls 20 are joined, the flux action of the upper fixing material 50 reduces the oxide film on the upper surfaces of the solder balls 20, thereby making them in a good condition for solder joining.

[0024] 1(c), the flux residue contained in the upper fixing material 50 is cured by heating during bonding of the solder balls 20 to form a cured resin. This cured resin becomes the upper resin reinforcement part 51 (resin reinforcement structure). The upper resin reinforcement part 51 has a structure held by at least the lower surface 12 of the semiconductor chip 10 and the upper parts of the solder bumps 21. However, the upper resin reinforcement part 51 is configured not to cover the entire surface of the solder bumps 21, but to expose at least the lower parts of the solder bumps 21 (the connection parts with the electrodes 34 on the mounting board 30 side).

[0025] The solder balls 20 may be made of any low melting point solder material. As the low melting point solder material, for example, a eutectic solder in which a metal such as Bi or In is added to Sn to form an alloy can be used, and a SnBi-based solder alloy is preferable. The SnBi solder alloy may contain about 20 to 70 mass% Bi, and may contain one or more other elements such as Ag, Cu, Sb, and Ni, as necessary. The SnBi solder alloy may contain, for example, about 5 mass% or less of other elements. The remainder of the SnBi solder alloy, after Bi and other elements, is Sn. The upper limit of the melting point of the low melting point solder material is, for example, 180° C. or less, preferably 160° C. or less, more preferably 150° C. or less, and even more preferably 140° C. or less. On the other hand, the lower limit of the melting point of the low-melting-point solder material is not particularly limited, but may be, for example, 100° C. or higher. The melting point of the low melting point solder material is determined by the solidus temperature (℃) calculated based on the melting curve obtained by DSC in accordance with JIS Z3198-1:2014.

[0026] The upper fastening material 50 is at least one of a thermosetting flux and a thermosetting solder paste. The thermosetting flux and the thermosetting solder paste may be any one that has a fluxing effect and forms a resin reinforcement structure by the resin cured product of the flux residue. The flux action means a reducing action to remove the oxide film formed on the solder surface, and an action to lower the surface tension of the solder and promote wettability.

[0027] The semiconductor chip 10 with the solder bumps 21 shown in FIG. 2(a) obtained in the above-mentioned solder bump formation step and a mounting substrate 30 are prepared.

[0028] The mounting board 30 may be a printed circuit board (PCB board) or a flexible printed circuit board. The use of the mounting board 30 is not particularly limited.

[0029] Next, a lower fixing material 60 is supplied to either the semiconductor chip 10 side or the mounting substrate 30 side. When supplied to the semiconductor chip 10 side, the lower fixing material 60 is supplied to the lower parts of the solder bumps 21 joined to the semiconductor chip 10, as shown in FIG. 2(b1). Alternatively, when the lower fixing material 60 is supplied to the mounting substrate 30 side, the lower fixing material 60 is supplied to the electrode portion 34 on the upper surface 32 of the mounting substrate 30 as shown in FIG. 2(b2).

[0030] Here, the mounting substrate 30 may have, on the upper surface 32, electrode portions 35 for connecting to electrical components other than the semiconductor chip 10, in addition to the electrode portions 34 for connecting to the solder bumps 21 of the semiconductor chip 10. When supplied to such a mounting substrate 30, the lower fixing material 60 is supplied only to the electrode portions 34 corresponding to the solder bumps 21. Moreover, the mounting substrate 30 has a mounting area on an upper surface 32 for mounting one or more semiconductor chips 10. Each mounting area has an arrangement pattern of a plurality of electrode portions 34 corresponding to the arrangement pattern of the plurality of electrode portions 14 of the semiconductor chip 10.

[0031] The lower fixing material 60 can be supplied by any of the methods exemplified for supplying the upper fixing material 50. However, when supplying the lower fixing material 60 to the lower parts of the solder bumps 21, a dipping method may be used in addition to the above-mentioned examples. Moreover, the supply amount and supply position of the lower fixing material 60 can be designed as appropriate.

[0032] 2(c), the lower part of the solder bump 21 covered with the lower fixing material 60 is brought into contact with the electrode part 34 on the upper surface 32 of the mounting substrate 30, or the lower part of the solder bump 21 is brought into contact with the electrode part 34 covered with the lower fixing material 60 on the upper surface 32 of the mounting substrate 30. Then, after or simultaneously with the contact, heating is performed to solder-join the lower part of the solder bump 21 and the electrode part 34. As a heating method, reflow in which heating is performed in a reflow furnace is preferable.

[0033] Here, due to the flux action of the lower fixing material 60, the oxide film on the lower surface of the solder bump 21 is reduced, etc., so that the lower surface is in a good condition for soldering. 2(c), the flux residue contained in the lower fixing material 60 is cured by heating the solder bumps 21 to form a cured resin. This cured resin becomes the lower resin reinforcement portion 61 (resin reinforcement structure). The lower resin reinforcement portion 61 has a structure that is held at least by the lower portions of the solder bumps 21 and the upper surface 32 of the mounting substrate 30.

[0034] By the above steps, an electronic device 1 is obtained, which has an upper resin reinforcing portion 51 and a lower resin reinforcing portion 61 that respectively reinforce the upper and lower portions of the solder bumps 21. A cross-sectional view showing a schematic view of a portion of the obtained electronic device 1 is shown in FIG.

[0035] In another embodiment, the method for manufacturing an electronic device may not include a step of filling all of the gap between the mounting substrate 30 and the semiconductor chip 10 with a mold underfill material after the mounting step (e.g., after FIG. 2(c)). Here, the gap means a fillable space between the lower surface 12 of the semiconductor chip 10 and the upper surface 32 of the mounting substrate 30, excluding the solder bumps 21, the upper resin reinforcement portion 51, and in some cases, the lower resin reinforcement portion 61 and the electrode portion 34. The fillable space may be partially filled with the mold underfill material, but it is preferable that the entirety of the fillable space is not filled with the mold underfill material.

[0036] In another embodiment, the method for manufacturing an electronic device may not include a cleaning step for cleaning away flux residues after at least one of the solder bump forming step and the mounting step, thereby improving the manufacturing efficiency of the method for manufacturing an electronic device.

[0037] In another embodiment, the mounting process may use a known flux such as a water-soluble flux instead of the lower fixing material 60. As a result, the electronic device 1 in Fig. 2(c) may have only the upper resin reinforcing portion 51 formed on the upper portion of the solder bump 21, and may not have the lower resin reinforcing portion 61 formed below it.

[0038] In another embodiment, it is possible to control the structure of the lower resin reinforcing portion 61 formed in FIG. 2(c) by adjusting the supply amount of the lower fixing material 60, etc.

[0039] In a cross-sectional view of the resulting electronic device 1 in a specified substrate thickness direction, the upper resin reinforcement portion 51 and the lower resin reinforcement portion 61 formed on the same solder bump 21 may have a structure separated from each other, or may have a structure in which at least a portion of the lower resin reinforcement portion 61 is joined to the upper resin reinforcement portion 51, or may have a structure in which the lower resin reinforcement portion 61 covers the entire surface of the upper resin reinforcement portion 51.

[0040] Furthermore, in a cross-sectional view of the resulting electronic device 1 in a specified substrate thickness direction, in the gap between the two most adjacent solder bumps 21, a portion of one lower resin reinforcement portion 61 may be joined to a portion of the other lower resin reinforcement portion 61, and one, the other, or both lower resin reinforcement portions 61 may fill some or all of the gap.

[0041] In at least one cross section of the electronic device 1 shown in FIG. 3 (or the mounting substrate 30 after the mounting process shown in FIG. 2(c)), the height of the solder bumps 21 is H B , the radius of the solder bump 21 is W B The resin height of the lower resin reinforcement portion 61 is H E , the resin width of the lower resin reinforcement portion 61 is H E It is defined as: The height of the solder bump 21 means the maximum value, and the radius of the solder bump 21 means half the maximum diameter. Also, the resin height and resin width of the lower resin reinforcing portion 61 mean the maximum values. The solder bumps 21 to be measured include solder bumps A located on the outermost periphery of the mounting area where the semiconductor chip 10 is mounted, and also solder bumps A located on the outermost periphery of the mounting area where the adjacent solder bump distance is within the above W B The lower resin reinforcement portion 61 to be measured includes the solder bump B, which is four times or more larger than the adjacent solder bump distance 4×W. B The average values ​​of the measured values ​​of the solder bumps 21 and the lower resin reinforcement portions 61 to be measured are defined as the resin height ratio and the resin width ratio, respectively.

[0042] The above H E , H B Using this, the ratio of the resin height of the lower resin reinforcement portion 61 to the height of the solder bump 21, i.e., the resin height ratio (%), is calculated as H E / H B Calculated from x100. The lower limit of the resin height ratio (%) is, for example, 10% or more, preferably 20% or more, and more preferably 30% or more, which can further improve the impact resistance of the electronic device. The upper limit of the resin height ratio (%) is not particularly limited, but may be 100% or less, or may be 90% or less.

[0043] Also, the above W E , W B Using this, the ratio of the resin width of the lower resin reinforcement portion 61 to the radius of the solder bump 21, i.e., the resin width ratio (%), is calculated as W E / W B Calculated from x100. The lower limit of the resin width ratio (%) is, for example, 30% or more, preferably 50% or more, and more preferably 60% or more, which can further improve the impact resistance of the electronic device. The upper limit of the resin width ratio (%) is not particularly limited, but may be more than 100%, may be 100% or less, or may be 90% or less.

[0044] <<Thermosetting flux and thermosetting solder paste>> An example of a thermosetting flux that can be used includes a thermosetting resin and an activator. As an example of a thermosetting solder paste, one that further contains solder powder in addition to the components contained in the thermosetting flux can be used.

[0045] An example of the thermosetting resin is an epoxy resin. If necessary, a curing agent for a thermosetting resin or a curing catalyst for a thermosetting resin may be contained. Factors for adjusting the exothermic peak temperature described below to a desired range include, for example, the type of curing agent, the type of catalyst, or appropriate adjustment of the compounding ratio thereof.

[0046] Examples of the activator include organic acids, organic halogen compounds, and amine hydrohalides.

[0047] The thermosetting flux may contain, in addition to the above components, a base resin, a thixotropic agent, a solvent, and the like. The thermosetting flux may further contain additives other than those described above, such as colorants, antifoaming agents, surfactants, and matting agents, within the scope of the invention. These may be used alone or in combination of two or more.

[0048] The solder powder contained in the thermosetting solder paste is preferably made of the above-mentioned low melting point solder material. The average particle size (median diameter) of the solder powder is, for example, 5 μm to 45 μm, or preferably 10 μm to 35 μm. The content of the thermosetting flux in the thermosetting solder paste is, for example, 10% by mass to 80% by mass, and preferably 15% by mass to 70% by mass. In this specification, the symbol "to" indicates that the upper and lower limits are included, unless otherwise specified.

[0049] For the thermosetting flux or the thermosetting flux contained in the thermosetting solder paste, a differential scanning calorimeter (Hitachi High-Tech Science Corporation, DSC7020) is used to measure the exothermic peak temperature (°C) based on a DSC curve measured in the range of 25°C to 250°C at a heating rate of 20°C / min. For thermosetting solder paste as the subject of DSC measurement, it is sufficient to use the flux components obtained by excluding the solder powder from the thermosetting solder paste, or it is also possible to use a thermosetting flux extracted by centrifuging the thermosetting solder paste to remove the solder powder. In addition, it is preferable to draw a baseline on the obtained DSC curve, starting from a flat portion.

[0050] The above-mentioned exothermic peak temperature is, for example, from [T+10]°C to [T+50]°C, preferably from [T+15]°C to [T+45]°C, and more preferably from [T+20]°C to [T+40]°C. By setting the heat generation peak temperature to the above lower limit, soldering defects can be suppressed. Furthermore, by setting the heat generation peak temperature to the above upper limit, the flux residue contained in the upper fixing material 50 and the lower fixing material 60 can be appropriately cured by heating (reflow) during the above-mentioned soldering. Note that, although an after-cure may be performed after reflow if necessary, by setting the heat generation peak temperature to the above upper limit, such an after-cure is unnecessary, and productivity can be improved.

[0051] <Electronic equipment> FIG. 2 is a cross-sectional view that illustrates an example of the electronic device 1 of the present embodiment. The electronic device 1 of this embodiment includes a mounting substrate 30, a semiconductor chip 10, and solder bumps made of low-melting-point solder that join electrode portions 34 on an upper surface 32 of the mounting substrate 30 and electrode portions 14 on a lower surface 12 of the semiconductor chip 10. Such an electronic device 1 includes an upper resin reinforcing portion 51 that is held on the lower surface 12 of the semiconductor chip 10 and on the upper portions of the solder bumps 21. This upper resin reinforcing portion 51 is made of a thermosetting flux or a resin cured product of flux residue of a thermosetting solder paste.

[0052] In addition, it is preferable that the electronic device 1 in another embodiment further includes a lower resin reinforcing portion 61 held by the upper surface 32 of the mounting substrate 30 and the lower portions of the solder bumps 21. This lower resin reinforcing portion 61 is made of a resin cured product of a thermosetting flux or a flux residue of a thermosetting solder paste.

[0053] Furthermore, in another embodiment of the electronic device 1, a gap that is not filled with the mold underfill material may be formed between the upper surface 32 of the mounting substrate 30 and the lower surface 12 of the semiconductor chip 10.

[0054] Although the embodiments of the present invention have been described above, these are merely examples of the present invention, and various configurations other than those described above can be adopted. Furthermore, the present invention is not limited to the above-described embodiments, and modifications and improvements within the scope of the present invention are included in the present invention. EXAMPLES

[0055] The present invention will be described in detail below with reference to examples, but the present invention is not limited to the descriptions of these examples.

[0056] <Electronic device manufacturing> [Example 1] As outlined in FIGS. 1-2, the electronic device 1 was manufactured according to the following specific procedures. The following thermosetting flux (upper fixing material 50) was applied to each of the multiple electrode parts 14 on the lower surface 12 of the CSP (semiconductor chip 10) (FIG. 1(a)). Then, solder balls 20 (SnBi-based solder alloy, melting point: about 139°C, diameter: about 300 μm) were mounted on each of the positions corresponding to the multiple electrode parts 14 (FIG. 1(b)). Then, reflow was performed at a peak temperature of about 190°C to bond the solder bumps 21 and the electrode parts 14 (FIG. 1(c)). At this time, the flux residue of the thermosetting flux hardened to form the upper resin reinforcement part 51 (solder bump formation process). In the semiconductor chip 10 with the solder bumps 21 shown in FIG. 2(a) obtained by the above, the upper resin reinforcement part 51 was formed so as to cover a part of the lower surface 12 of the semiconductor chip 10 and a part of the upper part of the solder bumps 21, but the lower part of the solder bumps 21 was exposed. Next, the following thermosetting solder paste was applied to a plurality of electrode parts 34 of the following PCB board (mounting board 30) (FIG. 2(b2)), and then the lower parts of the solder bumps 21 of the semiconductor chip 10 were brought into contact with the electrode parts 34 on the upper surface 32 of the mounting board 30, and reflow was performed at a peak temperature of about 190° C. to bond the solder bumps 21 and the electrode parts 34 (FIG. 2(c)). At this time, the flux residue of the thermosetting solder paste hardened to form a lower resin reinforcing part 61 (mounting process). The lower resin reinforcing part 61 was in a state in which it covered at least a part of the upper surface 32 of the mounting board 30 and a part of the lower parts of the solder bumps 21. As a result of the above, an electronic device 1, the outline of which is shown in FIG.

[0057] (material) Semiconductor chips CSP (Chip Size Package) Package size: 12 x 12 x 1.1 mm Pitch: 0.5mm Ball Size: Diameter 0.3mm Bump: 192 pieces Mounting board PCB Board Board size: 174 x 140 x 0.8 mm Material: FR-4 (MCL-E-67 Hitachi Chemical) Land:NSMD

[0058] ·Thermosetting flux The epoxy resin, amine-based hardener, and activator were mixed in a specific ratio to prepare a thermosetting flux. The peak exothermic temperature of the thermosetting flux was about 170°C. The exothermic peak temperature was determined from the DSC curve obtained by measuring the DSC curve of the thermosetting flux at a temperature rise rate of 20°C / min in the range of 25°C to 250°C using a differential scanning calorimeter (DSC7020, manufactured by Hitachi High-Tech Science Corporation). The DSC curve used was the one in which the baseline was drawn, with the flat portion as the initial portion. ·Thermosetting solder paste The above thermosetting flux was mixed with solder powder of a low melting point solder material (SnBi-based solder alloy, melting point: about 139° C., average particle size: about 20 μm) so that the content of the thermosetting flux was 60 mass %, to obtain a thermosetting solder paste.

[0059] (Cross-section observation of electronic devices) In one cross section of the electronic device 1 shown in FIG. 3, the height of the solder bump 21 is H B , the radius of the solder bump 21 is W B The resin height of the lower resin reinforcement portion 61 is H E , the resin width of the lower resin reinforcement portion 61 is H E It is defined as: The height of the solder bump 21 means the maximum value, and the radius of the solder bump 21 means half the maximum diameter. Also, the resin height and resin width of the lower resin reinforcing portion 61 mean the maximum values. The above HE , H B Using this, the ratio of the resin height of the lower resin reinforcement portion 61 to the height of the solder bump 21, i.e., the resin height ratio (%), is calculated as H E / H B Calculate from W × 100. E , W B Using this, the ratio of the resin width of the lower resin reinforcement portion 61 to the radius of the solder bump 21, i.e., the resin width ratio (%), is calculated as W E / W B Calculated from x100. The solder bumps 21 to be measured include solder bumps A located on the outermost periphery of the mounting area where the semiconductor chip 10 is mounted, and also solder bumps A located on the outermost periphery of the mounting area where the adjacent solder bump distance is within the above W B The lower resin reinforcement portion 61 to be measured includes the lower resin reinforcement portion 61 formed on each of the solder bumps A and B, and includes the solder bump B, which has an adjacent solder bump distance of 4×W or more. B The average values ​​of the measured values ​​of the solder bumps 21 and the lower resin reinforcement portions 61 to be measured are defined as the resin height ratio and the resin width ratio. Here, the cross-sectional photographs of the electronic device 1 in Example 1 and Examples 2 and 3 described below, and Comparative Example 2, include 16 solder bumps 21, and the spacing between adjacent solder bumps 21 was basically the above-mentioned pitch (0.5 mm). However, with the left end as the base, the adjacent solder bump distances between the 5th and 6th, between the 8th and 9th, and between the 11th and 12th were 4×W. E That was all. In Example 1 and Examples 2-3 and Comparative Example 2 described below, eight points were used as measurement targets: the first and sixteenth solder bumps 21 classified as solder bump A, and the fifth, sixth, eighth, ninth, eleventh, and twelfth solder bumps 21 classified as solder bump B.

[0060] [Examples 2 to 3] In the above mounting process, the above thermosetting solder paste was applied so that the resin height ratio and resin width ratio of the lower resin reinforcing portion 61 had the values ​​in Table 1. Except for this, the electronic device 1 was obtained in the same manner as in Example 1.

[0061] [Example 4] In the above mounting process, the electronic device 1 was obtained in the same manner as in Example 1, except that a commercially available water-soluble flux was applied instead of the above thermosetting solder paste. However, in the electronic device 1 of Example 4, the upper resin reinforcing part 51 was formed, but the lower resin reinforcing part 61 was not formed.

[0062] [Comparative Example 1] Except for using a commercially available water-soluble flux instead of the thermosetting flux in the solder bump forming process and applying a commercially available water-soluble flux instead of the thermosetting solder paste in the mounting process, an electronic device 1 was obtained in the same manner as in Example 1. However, in the electronic device 1 of Comparative Example 1, the upper resin reinforcing portion 51 and the lower resin reinforcing portion 61 were not formed.

[0063] [Comparative Example 2] An electronic device 1 was obtained in the same manner as in Example 1, except that in the above solder bump formation process, a commercially available water-soluble flux was used instead of the thermosetting flux, and in the above mounting process, the above thermosetting solder paste was applied so that the resin height ratio and resin width ratio of the lower resin reinforcing portion 61 were the values ​​shown in Table 1. However, in the electronic device 1 of Comparative Example 2, the upper resin reinforcing portion 51 was not formed, but the lower resin reinforcing portion 61 was formed.

[0064] [Table 1]

[0065] The electronic devices manufactured as described above were evaluated for the following items.

[0066] <Drop impact test> Using an impact tester (HDST-230, manufactured by Shin-Ei Technology Co., Ltd.) that generates a JEDEC standard "impact waveform of 1500G, 0.5ms," a drop impact test was repeatedly performed on the electronic device obtained above, applying the standard impact.

[0067] (Average number of falls) A system capable of measuring the resistance value of the electronic device obtained above was constructed by connecting multiple electronic devices (daisy chain). 1. Before the above-mentioned <drop impact test>, the initial resistance value (R0) was measured. 2. Next, the resistance value was measured each time the above-mentioned <Drop Impact Test> was performed. At this time, the resistance value of the electronic device after the Xth drop was R X Here, X is the number of falls. 3.R X When / R0 was 1.5 or more, it was determined that a break had occurred in the connection between the semiconductor chip 10 and the mounting board 30 in the electronic device (because the part that started to break during the drop impact test loses continuity and resistance starts to increase). And, X, when this break occurred, was taken as the number of drops at the time of break. The above steps 1 to 3 were repeated eight times. The average number of drops at break was calculated, and this was taken as the average number of drops. The results are shown in Table 1.

[0068] (failure rate) The above-mentioned "drop impact test" was carried out on the electronic devices obtained above the average number of drops shown in Table 1. Thereafter, one of the cross sections of the electronic device (selecting a row in which the bumps had breaks) was observed, and the number of bumps with breaks was counted. In the cross section of the observed electronic device, the number of bumps with fractures was taken as N, and the total number of bumps was taken as P (16 in this case). The failure rate (%) was calculated based on the ratio of the number of fractured bumps to the total number of bumps in the row with fractures, that is, based on the formula: N / P x 100. The results are shown in Table 1.

[0069] (comprehensive evaluation) Based on the results of the above (average number of drops) and (failure rate), the shock resistance of the electronic devices was judged on a four-level scale, in the order of excellent, good, fair, and poor. The results are shown in Table 1.

[0070] The electronic devices obtained by the manufacturing methods of Examples 1 to 4 showed superior shock resistance compared to Comparative Examples 1 and 2. [Explanation of symbols]

[0071] 1 Electronic equipment 10. Semiconductor Chips 12 Bottom side 14 Electrode section 20 Solder balls 21 Solder Bumps 30 Mounting Board 32 Top side 34, 35 Electrode part 50 Top fixing material 51 Upper resin reinforcement part 60 Lower fixing material 61 Lower resin reinforcement part

Claims

1. a solder bump forming process in which an upper fixing material, which is at least one of a thermosetting flux and a thermosetting solder paste, is brought into contact with an electrode portion on the lower surface of the semiconductor chip while an upper portion of a solder ball made of a low melting point solder is joined to the electrode portion to form a solder bump; a mounting process of joining lower portions of the solder bumps joined to the semiconductor chip to electrode portions on an upper surface of a mounting substrate, In the solder bump forming step, a resin cured product of flux residue in the upper fixing material is held by the lower surface of the semiconductor chip and by the upper portions of the solder bumps.

2. 2. A method for manufacturing an electronic device according to claim 1, comprising the steps of: The mounting step includes: supplying at least one lower fixing material of a thermosetting flux and a thermosetting solder paste to the lower part of the solder bump joined to the semiconductor chip or to the electrode part on the upper surface of the mounting substrate; a lower portion of the solder bump is joined to the electrode portion on the upper portion of the mounting substrate; In the mounting step, a cured resin of flux residue in the lower fixing material is held on the upper surface of the mounting substrate and on the lower parts of the solder bumps.

3. A method for manufacturing an electronic device according to claim 2, comprising the steps of: After the mounting process, the height of the solder bumps in one cross section of the mounting substrate is H B The resin height of the lower resin reinforcing portion made of the resin cured product of the flux residue in the lower fixing material is H E Then, H E / H B x 100), the resin height ratio is 10% or more.

4. A method for manufacturing an electronic device according to claim 2, comprising the steps of: After the mounting process, the radius of the solder bump is W B The resin width of the lower resin reinforcement part made of the resin cured product of the flux residue in the lower fixing material is W E Then, W E / W B x 100), the resin width ratio is 30% or more.

5. A method for manufacturing an electronic device according to claim 1 or 2, comprising the steps of: A method for manufacturing an electronic device, which does not include a step of filling all of the gap between the mounting substrate and the semiconductor chip with a mold underfill material after the mounting step.

6. A method for manufacturing an electronic device according to claim 1 or 2, comprising the steps of: A method for manufacturing an electronic device, comprising the steps of: (a) forming a solder bump on a substrate; (b) mounting the solder bump on the substrate;

7. A method for manufacturing an electronic device according to claim 1 or 2, comprising the steps of: A method for manufacturing an electronic device, wherein the melting point of the solder balls made of the low melting point solder is 180° C. or lower, when the solidus temperature is taken as the melting point.

8. A method for manufacturing an electronic device according to claim 1 or 2, comprising the steps of: the thermosetting flux comprises a thermosetting resin and an activator; The method for manufacturing an electronic device, wherein the thermosetting solder paste comprises the thermosetting flux and solder powder.

9. A method for manufacturing an electronic device according to claim 1 or 2, comprising the steps of: When the thermosetting flux or the thermosetting flux contained in the thermosetting solder paste is measured for an exothermic peak temperature (°C) based on a DSC curve measured at a temperature rise rate of 20°C / min in the range of 25°C to 250°C using a differential scanning calorimeter (DSC), A method for manufacturing an electronic device, wherein the heat generation peak temperature is from [T+10]°C to [T+50]°C, where T (°C) is the melting point of the solder ball made of the low melting point solder.

10. A mounting board; A semiconductor chip; a solder bump made of a low melting point solder for joining an electrode portion on the upper surface of the mounting substrate and an electrode portion on the lower surface of the semiconductor chip; an upper resin reinforcing portion held by a lower surface of the semiconductor chip and upper portions of the solder bumps, the upper resin reinforcing portion being made of a thermosetting flux or a resin cured product of flux residue of a thermosetting solder paste.

11. 11. The electronic device of claim 10, an electronic device comprising a lower resin reinforcing portion held by an upper surface of the mounting substrate and by lower portions of the solder bumps, the lower resin reinforcing portion being made of a thermosetting flux or a resin cured product of flux residue of a thermosetting solder paste.

12. 12. The electronic device of claim 11, In one cross section of the mounting substrate, the height of the solder bump is H B , the resin height of the lower resin reinforcement portion is H E Then, H E / H B x 100 is 10% or more.

13. 12. The electronic device of claim 11, In one cross section of the mounting substrate, the radius of the solder bump is W B , the resin width of the lower resin reinforcement part is W E Then, W E / W B x 100, the resin width ratio is 30% or more.

14. 12. An electronic device according to claim 10 or 11, an air gap that is not filled with a mold underfill material is formed between the upper surface of the mounting substrate and the lower surface of the semiconductor chip;

Citation Information

Patent Citations

  • Solder bump forming method, flip-chip mounting method and mounting structure

    JP2001284382A

  • Noncleaning flux corresponding to lead-free solder and solder composition containing the flux

    JP2002239785A

  • Electronic component mounting method

    JP2012069839A

  • Mounting method and mounting structure of electronic component

    JP2015115500A

  • Thermosetting flux composition, solder composition and method for manufacturing electronic substrate

    JP2018161673A

Cited By

  • Quantum semiconductor device and quantum computer

    WO2026140712A1