Joining body

A bonded body with a titanium-based bonding layer and silicon nitride ceramic layer addresses silver migration issues, ensuring strong adhesion between ceramic and metal layers without silver, thus preventing short circuits.

JP2024146454AInactive Publication Date: 2024-10-15NHK SPRING CO LTD

Patent Information

Application Number
JP2023059355
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Conventional brazing materials containing silver can cause migration, leading to short circuits in bonded bodies used in semiconductor devices.

Method used

A bonded body comprising a ceramic layer, a metal layer made of copper, and a bonding layer containing titanium and an amphoteric metal element, such as tin or zinc, where titanium is primarily on the ceramic side and the amphoteric metal is primarily on the metal side, with the ceramic layer formed using silicon nitride.

Benefits of technology

The solution effectively bonds ceramic substrates and metal materials without using silver, suppressing migration and enhancing adhesion, thereby preventing short circuits.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024146454000001_ABST
    Figure 2024146454000001_ABST
Patent Text Reader

Abstract

To provide a joining body capable of firmly joining a ceramic substrate and a metal material without using silver.SOLUTION: A joining body of the invention includes: a ceramics layer; a metal layer composed of copper; and a joining layer that joints the ceramics layer and the metal layer and includes titanium and tin as a component.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a joint. [Background technology]

[0002] Conventionally, a bonded body in which a ceramic substrate having heat resistance and insulating properties and a conductive metal are bonded to each other has been known as a circuit board used in a semiconductor device or the like (see, for example, Patent Document 1). Patent Document 1 discloses a bonded body in which a copper plate is bonded to the surface of a ceramic substrate by a brazing material containing silver. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 3211856 Summary of the Invention [Problem to be solved by the invention]

[0004] However, brazing materials containing silver have the risk of causing migration due to the silver, which may result in a short circuit.

[0005] The present invention has been made in view of the above, and an object of the present invention is to provide a bonded body capable of firmly bonding a ceramic substrate and a metal material without using silver. [Means for solving the problem]

[0006] In order to solve the above-mentioned problems and achieve the object, the joined body of the present invention is characterized by comprising a ceramic layer, a metal layer made of copper, and a joining layer joining the ceramic layer and the metal layer, the joining layer containing titanium and an amphoteric metal element as components.

[0007] In addition, the joined body of the present invention is characterized in that, in the joining layer, the titanium is mainly present on the ceramic layer side, and the amphoteric metal element is mainly present on the metal layer side.

[0008] In addition, the joined body according to the present invention is characterized in that, in the above-mentioned invention, the ceramic layer is formed using silicon nitride.

[0009] In addition, the joined body according to the present invention is characterized in that, in the above-mentioned invention, the amphoteric metal element is tin.

[0010] The bonded body according to the present invention is characterized in that, in the above-mentioned invention, it forms a part of a component constituting a circuit board used in a power module. Effect of the Invention

[0011] According to the present invention, it is possible to firmly bond a ceramic substrate and a metal material without using silver. [Brief description of the drawings]

[0012] [Figure 1] FIG. 1 is a diagram showing a structure of a bonded body according to an embodiment of the present invention. [Diagram 2] FIG. 2 is a diagram illustrating a bonding method for a bonded body according to one embodiment of the present invention. [Diagram 3] FIG. 3 is a SEM (Scanning Electron Microscope) image showing a cross section of a part of a bonded body according to one embodiment of the present invention, in which a metal layer and a ceramic layer are bonded with titanium foil and tin foil. [Figure 4] FIG. 4 is a secondary electron image showing a cross section of a part of a bonded body according to one embodiment of the present invention, in which a metal layer and a ceramic layer are bonded with titanium foil and tin foil. [Diagram 5]FIG. 5 is a backscattered electron image showing a cross section of a part of a bonded body according to one embodiment of the present invention, in which a metal layer and a ceramic layer are bonded with a titanium foil and a tin foil. [Figure 6] FIG. 6 is a diagram showing element mapping of copper (Cu) in the secondary electron image shown in FIG. [Figure 7] FIG. 7 is a diagram showing element mapping of tin (Sn) in the secondary electron image shown in FIG. [Figure 8] FIG. 8 is a diagram showing element mapping of titanium (Ti) in the secondary electron image shown in FIG. [Figure 9] FIG. 9 is a diagram showing elemental mapping of silicon (Si) in the secondary electron image shown in FIG. [Figure 10] FIG. 10 is a diagram showing elemental mapping of nitrogen (N) in the secondary electron image shown in FIG. [Figure 11] FIG. 11 is a SEM (Scanning Electron Microscope) image showing a cross section of a portion of a bonded body according to one embodiment of the present invention, in which a metal layer and a ceramic layer are bonded together with titanium foil and zinc foil. [Figure 12] FIG. 12 is a secondary electron image showing a cross section of a part of a bonded body according to one embodiment of the present invention, in which a metal layer and a ceramic layer are bonded with titanium foil and zinc foil. [Figure 13] FIG. 13 is a backscattered electron image showing a cross section of a part of a bonded body according to one embodiment of the present invention, in which a metal layer and a ceramic layer are bonded together with titanium foil and zinc foil. [Figure 14] FIG. 14 is a diagram showing element mapping of copper (Cu) in the secondary electron image shown in FIG. [Figure 15] FIG. 15 is a diagram showing element mapping of zinc (Zn) in the secondary electron image shown in FIG. [Figure 16] FIG. 16 is a diagram showing element mapping of titanium (Ti) in the secondary electron image shown in FIG. [Figure 17]FIG. 17 is a diagram showing elemental mapping of silicon (Si) in the secondary electron image shown in FIG. [Figure 18] FIG. 18 is a diagram showing element mapping of nitrogen (N) in the secondary electron image shown in FIG. [Figure 19] FIG. 19 is a diagram illustrating the bondability of the bonded bodies according to Examples 1 to 7 depending on the bonding temperature. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] Hereinafter, an embodiment of the present invention (hereinafter, referred to as "embodiment") will be described with reference to the attached drawings. Note that the drawings are schematic, and the relationship between the thickness and width of each part, the thickness ratio of each part, etc. may differ from the actual ones, and the drawings may include parts with different dimensional relationships and ratios.

[0014] (Embodiment) 1 is a diagram showing the configuration of a bonded body according to one embodiment of the present invention. The bonded body 1 is used, for example, as a circuit board in a semiconductor device or the like. The bonded body 1 includes a metal layer 11 formed using a metal material, a ceramic layer 12 formed using a ceramic, and a bonding layer 13 provided between the metal layer 11 and the ceramic layer 12 to bond them together, forming a three-layer structure (metal layer / ceramic layer / metal layer) in which the ceramic layer 12 is located between the two metal layers 11. The bonded body 1 is used, for example, in a circuit board for a power module, that is, the bonded body 1 forms a part of a component constituting the circuit board for the power module.

[0015] The metal layer 11 has, for example, a plate shape. The metal layer 11 is formed using, for example, copper (Cu). In this embodiment, an example in which the metal layer 11 is formed using copper will be described.

[0016] The ceramic layer 12 has, for example, a plate shape and is formed using, for example, ceramics containing an oxide such as alumina, or ceramics containing a nitride such as aluminum nitride or silicon nitride.

[0017] The bonding layer 13 is made of foil-shaped titanium (Ti) (hereinafter also referred to as titanium foil) and foil-shaped tin (Sn) (hereinafter also referred to as tin foil), and forms a titanium active layer on the ceramic layer 12 side. Note that instead of tin foil, a foil-shaped amphoteric metal element, for example, foil-shaped zinc (Zn) may be used.

[0018] Next, a method for joining a joined body according to the present embodiment will be described with reference to Fig. 2. Fig. 2 is a diagram for explaining a method for joining a joined body according to an embodiment of the present invention. Fig. 2 shows a configuration of one side (lower side in Fig. 1) of the joining between a metal layer 11 and a ceramic layer 12 in a joined body 1. The other side is joined in the same manner.

[0019] First, titanium foil 13a and tin foil 13b are disposed on the surface of metal layer 11 (see FIG. 2(a)). Here, for example, titanium foil 13a has a thickness of 5 μm, and tin foil 13b has a thickness of 50 μm. FIG. 2(a) shows an example in which titanium foil 13a is placed on the surface of metal layer 11, and tin foil 13b is placed on titanium foil 13a, but this is not limiting and the order of the overlapping foils may be reversed. The titanium foil 13a and tin foil 13b form bonding layer 13.

[0020] After a titanium foil 13a and a tin foil 13b are disposed on the surface of the metal layer 11, the ceramic layer 12 is placed on the side of the metal layer 11 where the bonding layer 13 is disposed, and bonded (see FIG. 2(b)). At this time, the bonding conditions are set to, for example, a bonding temperature of 800°C to 950°C and a surface pressure of 20 MPa. A load is applied in a direction in which the metal layer 11 and the ceramic layer 12 approach each other.

[0021] The bonded body according to the present embodiment is produced by placing titanium foil 13a and tin foil 13b on the copper material constituting metal layer 11, and then sandwiching and bonding titanium foil 13a and tin foil 13b between the ceramic material and copper material constituting ceramic layer 12. Therefore, the bonded body according to the present embodiment can be produced by a simple process compared to the conventional case in which a brazing material is applied or a brazing material is disposed by screen printing.

[0022] Next, an example of a bonding interface in a bonded body will be described with reference to FIGS. 3 is a scanning electron microscope (SEM) image showing a cross section of a part of a bonded body according to one embodiment of the present invention, in which a metal layer and a ceramic layer are bonded with titanium foil and zinc foil. In the example shown in FIG. 3, a cross section of a bonded body bonded at a bonding temperature of 850° C. and a surface pressure of 20 MPa is shown. Cu and the ceramic layer R CE The ceramic layer between CE On the side, titanium active layer R Ti is formed.

[0023] 4 to 10 show cross-sectional images of the bonded body observed with an Electron Probe Micro Analyzer (EPMA). In Fig. 4 to Fig. 10, there is a copper material layer made of copper on the top, a ceramic layer made of Si3N4 on the bottom, and a bonding layer made of titanium foil and tin foil between the copper material layer and the ceramic layer.

[0024] Fig. 4 is a secondary electron image showing a cross section of a part of a bonded body according to an embodiment of the present invention. Fig. 5 is a backscattered electron image showing a cross section of a part of a bonded body according to an embodiment of the present invention. The secondary electron image shown in Fig. 4 is an image that depends on the surface (cross-sectional) shape. In addition, the backscattered electron image shown in Fig. 5 shows the difference in composition.

[0025] 6 to 10 show element mapping of the secondary electron image shown in FIG. 4. Specifically, FIG. 6 shows element mapping of copper (Cu). FIG. 7 shows element mapping of tin (Sn). FIG. 8 shows element mapping of titanium (Ti). FIG. 9 shows element mapping of silicon (Si). FIG. 10 shows element mapping of nitrogen (N).

[0026] As can be seen from FIG. 6 to FIG. 10, copper is located at the top, and silicon and nitrogen are located at the bottom. Also, tin is located on the copper side as a bonding layer, and titanium is located mainly on the silicon side as a bonding layer (titanium active layer). That is, the bonded body forms layers in the order of Cu / Sn+Ti / Cu+Ti / Ti+Sn / SiN. At this time, titanium and tin hardly move to the region where copper and silicon exist, and in the region corresponding to the bonding layer 13, a part of titanium is mixed in the region where tin exists. Therefore, in the bonded body according to the present embodiment, it can be said that the components constituting the bonding layer remain in the layer and do not move to the outside (here, the copper material layer and the ceramic layer).

[0027] An example of a bonded body in which a metal layer and a ceramic layer are bonded with a titanium foil and a zinc foil will be described with reference to Figs. 11 to 18. Fig. 11 is a scanning electron microscope (SEM) image showing a cross section of a part of a bonded body according to one embodiment of the present invention, in which a metal layer and a ceramic layer are bonded with a titanium foil and a zinc foil. The example shown in Fig. 11 shows a cross section of a bonded body bonded at a bonding temperature of 850°C and a surface pressure of 20 MPa, and the copper layer R Cu and the ceramic layer R CE The ceramic layer between CE On the side, titanium active layer R Ti is formed.

[0028] Images of the cross section of the bonded body observed by an Electron Probe Micro Analyzer (EPMA) are shown in Figures 12 to 18. Figures 4 to 10 show a copper material layer made of copper on the top, a ceramic layer made of Si3N4 on the bottom, and a bonding layer formed of titanium foil and zinc foil between the copper material layer and the ceramic layer.

[0029] Fig. 12 is a secondary electron image showing a cross section of a part of a bonded body according to an embodiment of the present invention, in which a metal layer and a ceramic layer are bonded with titanium foil and zinc foil. Fig. 13 is a backscattered electron image showing a cross section of a part of a bonded body according to an embodiment of the present invention, in which a metal layer and a ceramic layer are bonded with titanium foil and zinc foil. The secondary electron image shown in Fig. 4 shows an image that depends on the surface (cross-sectional) shape. Also, the backscattered electron image shown in Fig. 5 shows the difference in composition.

[0030] 14 to 18 show element mapping of the secondary electron image shown in FIG. 12. Specifically, FIG. 14 shows element mapping of copper (Cu). FIG. 15 shows element mapping of zinc (Zn). FIG. 16 shows element mapping of titanium (Ti). FIG. 17 shows element mapping of silicon (Si). FIG. 18 shows element mapping of nitrogen (N).

[0031] As can be seen from Figures 14 to 18, copper is located at the top, and silicon and nitrogen are located at the bottom. Furthermore, zinc is located on the copper side as a bonding layer, and titanium is located mainly on the silicon side as a bonding layer (titanium active layer). That is, the bonded body forms layers in the order of Cu+Zn / Cu+Zn+Ti / Ti+Cu+Zn / SiN. At this time, zinc is dissolved in copper to form a Cu-Zn alloy (brass), but migration to the ceramic layer (SiN) is not observed.

[0032] In the embodiment of the present invention described above, the copper material layer made of copper and the ceramic layer are joined by the joining layer formed of titanium foil and tin foil, so that the copper material layer and the ceramic layer can be joined in a joining mode in which the movement of components between the layers is suppressed. By suppressing the movement of components between the layers, the occurrence of migration like that of conventional silver is suppressed, and the adhesion of the joining layer to the copper material layer and the ceramic layer is increased. Therefore, according to this embodiment, the ceramic substrate and the copper material can be firmly joined without using silver.

[0033] In the embodiment of the present invention, an example has been described in which the bonded body 1 is constructed by sandwiching a ceramic layer between two metal layers. However, a configuration in which one metal layer 11 and a ceramic layer 12 are bonded by a bonding layer 13 may also be used, or a configuration in which n+1 (n>1) metal layers 11 and n ceramic layers 12 are alternately arranged and bonded. EXAMPLES

[0034] Examples of the bonded body according to the present invention will be described below, although the present invention is not limited to these examples.

[0035] Example 1 In Example 1, a bonded body was produced by bonding a copper plate and a silicon nitride plate at a bonding temperature of 800° C. The bonded body according to Example 1 has layers in the following order: Cu / Sn+Ti / Cu+Ti / Ti+Sn / SiN.

[0036] Example 2 In Example 2, a bonded body was produced in the same manner as in Example 1, except that the bonding temperature was set to 840° C. The bonded body according to Example 2 has layers in the following order: Cu / Sn+Ti / Cu+Ti / Ti+Sn / SiN.

[0037] Example 3 In Example 3, except that the amphoteric metal element was zinc (Zn), a bonded body was produced in the same manner as in Example 1. The bonded body according to Example 3 has layers in the following order: Cu+Zn / Cu+Zn+Ti / Cu+Zn / Ti / SiN.

[0038] Example 4 In Example 4, a bonded body was produced in the same manner as in Example 3, except that the bonding temperature was set to 800° C. The bonded body according to Example 4 has layers in the following order: Cu+Zn / Cu+Zn+Ti / Cu+Zn / Ti / SiN.

[0039] Example 5 In Example 5, a bonded body was produced in the same manner as in Example 3, except that the bonding temperature was 840° C. The bonded body according to Example 5 has layers in the following order: Cu+Zn / Cu+Zn+Ti / Ti+Cu+Zn / SiN.

[0040] Example 6 In Example 6, a bonded body was produced in the same manner as in Example 3, except that the bonding temperature was 930° C. The bonded body according to Example 6 has layers in the following order: Cu+Zn / Cu+Zn+Ti / Ti+Cu / SiN.

[0041] Example 7 In Example 7, a bonded body was produced in the same manner as in Example 1, except that the bonding temperature was set to 930° C. The bonded body according to Example 7 has layers in the order of Cu / Ti / SiN.

[0042] Fig. 19 is a diagram for explaining the bondability depending on the bonding temperature of the bonded bodies according to Examples 1 to 7 of the present invention. The bondability was evaluated by visual inspection, etc., using a SAT (Scanning Acoustic Tomograph: an ultrasonic flaw detector) and a SEM (Scanning Electron Microscope). As shown in Fig. 19, all of the bonded bodies according to Examples 1 to 7 showed good bondability.

[0043] Although the embodiments for carrying out the present invention have been described above, the present invention should not be limited to the above-described embodiments.

[0044] In this manner, the present invention may include various embodiments not described here, and various design modifications may be made without departing from the technical idea defined by the claims.

[0045] As described above, the bonded body according to the present invention is suitable for firmly bonding a ceramic substrate and a metal material without using silver. [Explanation of symbols]

[0046] 1 zygote 11 Metal layer 12 Ceramic layer 13 Bonding layer 13a Titanium foil 13b tin foil

Claims

1. A ceramic layer; A metal layer made of copper; a bonding layer for bonding the ceramic layer and the metal layer, the bonding layer including titanium and an amphoteric metal element as components; A bonded body comprising:

2. In the bonding layer, The titanium is mainly present on the ceramic layer side, the amphoteric metal element is mainly present on the metal layer side; 2. The bonded body according to claim 1 .

3. The ceramic layer is formed using silicon nitride.

2. The bonded body according to claim 1 .

4. The amphoteric metal element is tin.

4. The bonded body according to claim 1, wherein the bonded body is a bonded body having a thickness of 100 nm or less.

5. A part of a component constituting a circuit board used in a power module.

2. The bonded body according to claim 1 .

Citation Information

Patent Citations

  • Ceramic circuit board and its producing method

    JP2003283064A

  • Method for manufacturing joined body and method for producing substrate for power module

    JP2015209356A

  • Bonded body and dielectric circuit board

    JP2019085327A

  • Method and furnace for manufacturing metal ceramic base material

    JP2023007427A

  • Joining body, circuit substrate, semiconductor device, and method for manufacturing joining body

    WO2022024832A1

Cited By

  • Joined body and production method for joined body

    WO2025202754A1