Method of manufacturing optical device structures
The method of substrate rotation and controlled etching with selective chemistries addresses the inefficiencies of traditional manufacturing processes for blazed optical devices, reducing time and cost while maintaining precision.
Patent Information
- Application Number
- JP2024062558
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2020-08-13
- Filing Date
- 2024-04-09
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2041-07-28
AI Technical Summary
Manufacturing blazed optical devices requires multiple lithographic patterning and angled etching steps, increasing time and cost.
A method involving substrate rotation and controlled etching using patterned resist structures with selective etch chemistries to form blazed optical devices without multiple lithographic and angled etching steps.
Reduces manufacturing time and cost by eliminating the need for multiple patterning and angled etching steps while maintaining high precision in optical device structure formation.
Smart Images

Figure 2024146941000001_ABST
Abstract
Description
[Technical field]
[0001]
[0001] 1. Field of the Invention
[0001] Embodiments of the present invention relate generally to optical devices for augmented reality, virtual reality, and mixed reality. In particular, embodiments described herein provide for forming a blazed optical device structure. [Background technology]
[0002]
[0002] Virtual reality is generally considered to be a computer-generated simulated environment in which a user has an apparent physical presence. Virtual reality experiences are generated in 3D and can be viewed using a head-mounted display (HMD), such as glasses or other wearable display devices with near-eye display panels, such as lenses, to display the virtual reality that replaces the real environment.
[0003]
[0003] Augmented reality, however, allows for an experience where the user can still see the surrounding environment through the display lenses of the glasses or other HMD device, and can also see images of virtual objects that are generated for the display and appear as part of the environment. Augmented reality can include any type of input, such as voice input or haptic input, as well as virtual images, graphics, and videos that enhance or augment the environment experienced by the user. Because augmented reality is a new technology, there are many challenges and design constraints.
[0004]
[0004] One such challenge is to display a virtual image overlaid on the surrounding environment. Optical devices, including waveguide couplers such as augmented reality waveguide couplers, and flat optical devices such as metasurfaces, are used to help overlay multiple images. The generated light propagates through the optical device until it exits the optical device and is overlaid on the surrounding environment. The optical device may require a structure with a blazed angle relative to the surface of the optical device substrate. Conventionally, multiple lithographic patterning and angled etching steps are required to fabricate a blazed optical device using one or more angled etching tools. The multiple lithographic patterning and angled etching steps increase manufacturing time and increase costs.
[0005]
[0005] Therefore, there is a need in the art for improved methods of forming optical devices, including blazed optical devices, using angled etching tools. Summary of the Invention
[0006] In one embodiment, a method is provided. The method includes positioning a substrate at a first rotation angle φ1 in a path of a beam. The beam is configured to be surface projected onto the substrate at a beam angle θ relative to a surface normal of the substrate. A patterned resist is formed on the substrate. In this case, the patterned resist includes two or more resist structures and one or more gaps. Each of the resist structures has a width, and each of the gaps has a linewidth defined by the adjacent resist structures. The method includes etching the substrate positioned at the first rotation angle φ1 with the beam, rotating the substrate to a second rotation angle φ2, and etching a sidewall of the resist structure directed toward the beam. Thereby, the width of the resist structure is reduced and the linewidth of the gap is increased. The method further includes rotating the substrate to the first rotation angle φ1, etching the substrate at the first rotation angle φ1 with the beam, and forming two or more optical device structures in the substrate. Forming the optical device structure includes repeating rotating the substrate to a second rotation angle φ2, etching sidewalls of the resist structure with the beam, rotating the substrate to a first rotation angle φ1, and etching the substrate with the beam until the resist structure is removed or the linewidth of the gap has a predetermined linewidth.
[0007]
[0007] In another embodiment, a method is provided. The method includes positioning a substrate in a path of a beam at a first rotation angle φ1. The beam is configured to be surface projected onto the substrate at a beam angle θ relative to a surface normal of the substrate. A device layer is formed on the substrate, and a patterned resist is formed on the device layer. The patterned resist includes two or more resist structures and one or more gaps. Each of the resist structures has a width, and each of the gaps has a linewidth defined by the adjacent resist structures. The method includes etching the device layer with the beam while the substrate is positioned at the first rotation angle φ1, rotating the substrate to a second rotation angle φ2, and etching a sidewall of the resist structure directed toward the beam. The width of the resist structures is thereby reduced and the linewidth of the gap is increased. The method further includes rotating the substrate to a first rotation angle φ1, etching the device layer at the first rotation angle φ1 with the beam, and forming two or more optical device structures in the device layer. Forming the optical device structures includes repeating rotating the substrate to a second rotation angle φ2, etching sidewalls of the resist structures with the beam, rotating the substrate to the first rotation angle φ1, and etching the device layer with the beam until the resist structures are removed or the linewidth of the gap has a predetermined linewidth.
[0008]
[0008] In yet another embodiment, a method is provided. The method includes positioning a substrate at a first rotation angle φ1 in a path of a beam. The beam is configured to be surface projected onto the substrate at a beam angle θ relative to a surface normal of the substrate. A patterned resist is formed on the substrate. The patterned resist then includes two or more resist structures and one or more gaps. Each of the resist structures has a width, and each of the gaps has a linewidth defined by the adjacent resist structures. The substrate is etched by a beam generated by a substrate etching chemistry, and the resist structures are etched by a beam generated by a resist etching chemistry different from the substrate etching chemistry. The method further includes etching the substrate positioned at the first rotation angle φ1 with a beam generated by the substrate etching chemistry, rotating the substrate to a second rotation angle φ2, and etching a sidewall of the resist structure with the beam at the beam angle θ. The beam generated by the resist etching chemistry etches a sidewall of the resist structure directed toward the beam. Thereby, the width of the resist structure is decreased and the line width of the gap is increased. The method further includes rotating the substrate to a first rotation angle φ1, etching the substrate at the first rotation angle φ1 with a beam generated by the substrate etching chemistry, and forming two or more optical devices in the substrate. Forming the optical device structures includes repeating rotating the substrate to a second rotation angle φ2, etching the sidewalls of the resist structure with a beam generated by the resist etching chemistry, rotating the substrate to the first rotation angle φ1, and etching the substrate with a beam generated by the substrate etching chemistry until the resist structure is removed or the line width of the gap has a predetermined line width.
[0009]
[0009] In order that the above-mentioned features of the present disclosure may be understood in detail, a more particular description of the present disclosure briefly summarized above will be made by reference to embodiments, some of which are illustrated in the accompanying drawings. It should be noted, however, that the accompanying drawings only illustrate exemplary embodiments and therefore should not be considered as limiting the scope thereof, which may allow other equally effective embodiments. [Brief description of the drawings]
[0010] [Figure 1A]
[0010] FIG. 1 is a perspective front view of an optical device according to several embodiments described herein. [Figure 1B]
[0011] 1B and 1C are schematic cross-sectional views of device structures according to embodiments described herein. [Figure 1C] 1B and 1C are schematic cross-sectional views of device structures according to embodiments described herein. [Diagram 2]
[0012] FIG. 1 is a schematic side view of a tilted etching system in accordance with multiple embodiments described herein. [Diagram 3]
[0013] 1 is a schematic cross-sectional view of a tilted etching system according to multiple embodiments described herein. [Figure 4]
[0014] FIG. 2 is a flow diagram of a method for forming a plurality of blazed device structures of an optical device structure according to embodiments described herein. [Figure 5A]
[0015] 5A-5E are schematic cross-sectional views of a portion of a substrate during a method for forming multiple blazed device structures according to multiple embodiments described herein. [Figure 5B] 5A-5E are schematic cross-sectional views of a portion of a substrate during a method for forming multiple blazed device structures according to multiple embodiments described herein. [Figure 5C]5A-5E are schematic cross-sectional views of a portion of a substrate during a method for forming multiple blazed device structures according to multiple embodiments described herein. [Figure 5D] 5A-5E are schematic cross-sectional views of a portion of a substrate during a method for forming multiple blazed device structures according to multiple embodiments described herein. [Figure 5E] 5A-5E are schematic cross-sectional views of a portion of a substrate during a method for forming multiple blazed device structures according to multiple embodiments described herein. [Figure 5F]
[0016] 5F-5J are schematic top-down views of a portion of a substrate during a method for forming multiple blazed device structures according to embodiments described herein. [Figure 5G] 5F-5J are schematic top-down views of a portion of a substrate during a method for forming multiple blazed device structures according to embodiments described herein. [Figure 5H] 5F-5J are schematic top-down views of a portion of a substrate during a method for forming multiple blazed device structures according to embodiments described herein. [Figure 5I] 5F-5J are schematic top-down views of a portion of a substrate during a method for forming multiple blazed device structures according to embodiments described herein. [Figure 5J] 5F-5J are schematic top-down views of a portion of a substrate during a method for forming multiple blazed device structures according to embodiments described herein. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011]
[0017] For ease of understanding, wherever possible, the same reference numerals have been used to designate identical elements common to the figures. It is contemplated that elements and features of one embodiment may be beneficially incorporated in other embodiments without further description.
[0012]
[0018] FIELD OF THE DISCLOSURE
[0002] Embodiments of the present invention generally relate to optical devices for augmented reality, virtual reality, and mixed reality. In particular, embodiments described herein provide a method for forming a blazed optical device structure that utilizes rotation of a substrate having an optical device structure formed thereon and the ability to adjust the etch rate of a patterned resist disposed on the substrate and one of the device layer or the substrate to form the optical device structure without multiple lithographic patterning and angled etching steps.
[0013]
[0019] In one embodiment, a method includes positioning a substrate at a first rotation angle φ1 in a path of the beam, the beam configured to be projected onto a surface of the substrate at a beam angle θ relative to a surface normal of the substrate. The substrate has a patterned resist formed thereon. The patterned resist includes two or more resist structures. Each of the resist structures has a width and one or more gaps. Each of the gaps is defined by an adjacent resist structure and has a linewidth defined by the adjacent resist structure. The substrate positioned at the first rotation angle φ1 is etched with the beam. The substrate is rotated to a second rotation angle φ2 and sidewalls of the resist structures are etched with the beam at the beam angle θ. Thereby, the width of the resist structures is reduced and the linewidth of the gap is increased. The substrate is rotated to the first rotation angle φ1 and the substrate is etched with the beam at the first rotation angle φ1. Two or more optical device structures are formed in the substrate. Forming the optical device structure includes repeating rotating the substrate to a second rotation angle φ2, etching sidewalls of the resist structure with the beam, rotating the substrate to a first rotation angle φ1, and etching the substrate with the beam until the resist structure is removed or the linewidth of the gap has a predetermined linewidth.
[0014]
[0020] FIG. 1A shows a perspective front view of an optical device 100. It should be understood that the optical device 100 described below is an exemplary optical device. In one embodiment that may be combined with other embodiments described herein, the optical device 100 is a waveguide coupler, such as an augmented reality waveguide coupler. In another embodiment that may be combined with other embodiments described herein, the optical device 100 is a planar optical device, such as a metasurface. The optical device 100 includes a plurality of device structures 102 disposed in (as shown in FIG. 1B) or on (as shown in FIG. 1C) a substrate 101. As shown in FIG. 1C, the device structures 102 are formed in a device layer 114 formed on the substrate 101. The device structures 102 may be nanostructures having nano-sized dimensions, such as submicron dimensions, e.g., critical dimensions less than 1 μm. In one embodiment that may be combined with other embodiments described herein, the regions of the device structure 102 correspond to one or more gratings 104, such as the first grating 104a, the second grating 104b, and the third grating 104c. In one embodiment that may be combined with other embodiments described herein, the optical device 100 is a waveguide coupler that includes at least the first grating 104a corresponding to an input coupling grating and the third grating 104c corresponding to an output coupling grating. A waveguide coupler according to an embodiment that may be combined with other embodiments described herein may include the second grating 104b corresponding to an intermediate grating.
[0015]
[0021] 1B and 1C are schematic cross-sectional views of a number of device structures 102. In an embodiment that may be combined with other embodiments described herein, the device structure 102 is a blazed optical device 106 of a flat optical device, such as a metasurface. The method 400 described herein forms the blazed optical device 106. In another embodiment that may be combined with other embodiments described herein, the device structure 102 is a blazed optical device structure 106 of a waveguide coupler, such as an augmented reality waveguide coupler. A waveguide coupler according to an embodiment that may be combined with other embodiments described herein may include a blazed optical device structure 106 in at least one of the diffraction gratings 104. Each of the blazed device structures 106 includes a blazed surface 108, a sidewall 112, a depth h, and a linewidth d. The blazed surface 108 has a number of steps 110. In one embodiment, which may be combined with other embodiments described herein, the blazed surface 108 includes at least 16 steps 110, such as more than 32 steps 110, such as 64 steps 110. The blazed surface 108 has a blaze angle γ. The blaze angle γ is the angle between the blazed surface 108 and a surface parallel line p of the substrate 101, and is the angle between the surface normal of the substrate 101 and a facet normal f of the blazed surface 108. The depth h corresponds to the height of the sidewalls 112, and the line width d corresponds to the distance between the sidewalls 112 of adjacent blazed structures 106.
[0016]
[0022] In one embodiment that may be combined with other embodiments described herein, the blaze angles γ of two or more blazed device structures 106 are different. In another embodiment that may be combined with other embodiments described herein, the blaze angles γ of two or more blazed device structures 106 are the same. In one embodiment that may be combined with other embodiments described herein, the depths h of two or more blazed device structures 106 are different. In another embodiment that may be combined with other embodiments described herein, the depths h of two or more blazed device structures 106 are the same. In one embodiment that may be combined with other embodiments described herein, the line widths d of two or more blazed device structures 106 are different. In another embodiment that may be combined with other embodiments described herein, the line widths d of two or more blazed device structures 106 are the same.
[0017]
[0023] The substrate 101 may also be selected to transmit an appropriate amount of light at a desired wavelength or wavelength range, such as one or more wavelengths from about 100 to about 3000 nanometers. In some non-limiting embodiments, the substrate 101 is configured to transmit about 50% to about 100% or more of the IR to UV region of the light spectrum. The substrate 101 may be formed from any suitable material, provided that the substrate 101 can adequately transmit light at a desired wavelength or wavelength range and can serve as a suitable support for the blazed device structures 106 described herein (when the blazed device structures 106 are formed in the device layer 114). The substrate selection may include, but is not limited to, substrates of any suitable material, such as amorphous dielectrics, non-amorphous dielectrics, crystalline dielectrics, silicon oxides, polymers, and combinations thereof. In some embodiments, which may be combined with other embodiments described herein, the substrate 101 comprises a transparent material. Suitable examples may include oxides, sulfides, phosphides, tellurides, or combinations thereof. In one embodiment, the substrate 101 comprises silicon (Si), silicon dioxide (SiO2), germanium (Ge), silicon germanium (SiGe), sapphire, and a high-index transparent material such as a high refractive index glass.
[0018]
[0024] In some embodiments, which may be combined with other embodiments described herein, the device layer 114 may be any material, including, but not limited to, silicon oxycarbide (SiOC), titanium dioxide (TiO2), silicon dioxide (SiO2), vanadium(IV) oxide (VO x), aluminum oxide (Al2O3), aluminum doped zinc oxide (AZO), indium tin oxide (ITO), tin dioxide (SnO2), zinc oxide (ZnO), tantalum pentoxide (Ta2O5), silicon nitride (Si3N4), zirconium dioxide (ZrO2), niobium oxide (Nb2O5), cadmium stannate (Cd2SnO4), or silicon carbonitride (SiCN) containing materials. In some embodiments that may be combined with other embodiments described herein, the material of the device layer 114 may have a refractive index between about 1.5 and about 2.65. In other embodiments that may be combined with other embodiments described herein, the material of the device layer 114 may have a refractive index between about 3.5 and about 4.0.
[0019]
[0025] 2 is a schematic side view of an angled etching system 200. It should be understood that the angled etching system 200 described below is an exemplary angled etching system, and that other angled etching systems may be used or modified to fabricate optical devices 100 having blazed device structures 106 according to embodiments of the present disclosure.
[0020]
[0026] The tilted etching system 200 includes an ion beam chamber 202. A power source 204, a first gas source 206, and a second gas source are coupled to the ion beam chamber 202. In one embodiment, which may be combined with other embodiments described herein, the power source 204 is a radio frequency (RF) power source. The first gas source 206 is in fluid communication with an interior space 205 of the ion beam chamber 202. The first gas source 206 is an inert gas source that supplies an inert gas, such as argon, hydrogen, or helium, to the ion beam chamber 202. The second gas source 208 is in fluid communication with the interior space 205 of the ion beam chamber 202. The second gas source 208 is a process gas source that supplies a process gas to the ion beam chamber 202. The process gas includes, but is not limited to, one or more of a chlorine-containing gas, a fluorine-containing gas, a bromine-containing gas, an oxygen-containing gas, a silicon-containing gas, a nitrogen-containing gas, a hydrogen-containing gas, and the like. In embodiments of the method 400 described herein, which may be combined with other embodiments described herein, more than one process gas may be utilized.
[0021]
[0027] The first process gas may have a substrate etch chemistry that is selective to the resist material. The etch selectivity of the first process gas having the substrate etch chemistry provides a substrate material to resist material (described below) selectivity of about 5:1 or greater. The etch selectivity of the first process gas having the device material etch chemistry provides a device material to resist material selectivity of about 5:1 or greater. In one embodiment, which may be combined with other embodiments described herein, the substrate etch chemistry includes a chlorine-containing gas, a fluorine-containing gas, or a combination thereof. In another embodiment, which may be combined with other embodiments described herein, the device material etch chemistry includes a chlorine-containing gas, a fluorine-containing gas, or a combination thereof.
[0022]
[0028] The second process gas may have a resist etch chemistry that is selective to the substrate material or the device material. The etch selectivity of the second process gas having the resist material etch chemistry provides a resist material to substrate material selectivity of about 10:1 or more, or a resist material to device material selectivity of about 10:1 or more. In one embodiment that may be combined with other embodiments described herein, the resist etch chemistry includes oxygen gas (O2) and carbon tetrafluoride (CF4). In another embodiment that may be combined with other embodiments described herein, the resist etch chemistry includes argon gas (Ar), nitrogen gas (N2), and hydrogen gas (H2). In yet another embodiment that may be combined with other embodiments described herein, the resist etch chemistry includes nitrogen gas (N2) and hydrogen gas (H2).
[0023]
[0029] In operation, a plasma is generated in the ion beam chamber 202 by applying RF power via a power source 204 to an inert gas and a process gas provided to an interior volume 205 of the ion beam chamber 202 to generate a plasma. Ions of the plasma of the inert gas and the process gas are extracted through an aperture 210 in an extraction plate 212 to generate an ion beam 216. The aperture 210 of the ion beam chamber 202 is operable to direct the ion beam 216 at an angle α with respect to a reference plane 218 oriented perpendicular (i.e., surface normal) to the substrate 101. The ion beam 216 includes, but is not limited to, a spot beam, a ribbon beam, or a full substrate sized beam. The generated ion beam 216 includes one of a substrate etch chemistry, a device material etch chemistry, or a resist etch chemistry depending on the process gas utilized.
[0024]
[0030] The substrate 101 is held on a platen 214 coupled to a first actuator 219. The first actuator 219, which may be a linear actuator, a rotary actuator, a stepper motor, or the like, is configured to move the platen 214 in a scanning motion along the y-direction and / or the z-direction. In an embodiment, which may be combined with other embodiments described herein, the first actuator 219 is further configured to tilt the platen 214 such that the substrate 101 is positioned at a tilt angle β relative to the x-axis of the ion beam chamber 202. The angle α and the tilt angle β result in a beam angle θ relative to a reference plane 218 that is normal to the substrate 101. A second actuator 220 may also be coupled to the platen 214 and rotates the substrate 101 about the x-axis of the platen 214.
[0025]
[0031] 3 is a schematic cross-sectional view of an angled etching system 300. It should be understood that the angled etching system 300 described below is an exemplary angled etching system, and that other angled etching systems may be used or modified to fabricate optical devices 100 having blazed device structures 106 according to embodiments of the present disclosure.
[0026]
[0032] The angled etching system 300 includes an electron beam chamber 302. A power supply 304, a first gas source 306, and a second gas source 308 are coupled to the electron beam chamber 302. The first gas source 306 and the second gas source 308 are in fluid communication with an interior space 305 of the electron beam chamber 302. For example, the first gas source 306 and the second gas source 308 may extend through the electrode 322, or the electrode 322 may include a plurality of apertures to function as a gas distribution showerhead. The first gas source 306 is an inert gas source that supplies an inert gas (as described above) to the electron beam chamber 302. The second gas source 308 is a process gas source (as described above) that supplies a process gas to the electron beam chamber 302. In embodiments of the method 400 described herein, which may be combined with other embodiments described herein, more than one process gas may be utilized. The two or more process gases include a substrate etch chemistry, a device material etch chemistry, and a resist etch chemistry as described herein.
[0027]
[0033] The substrate 101 is held on a platen 314 coupled to a first actuator 321. The first actuator 321, which may be a linear actuator, a rotary actuator, a stepper motor, etc., is configured to raise and lower the platen 314 within the electron beam chamber 302. A second actuator 320 may also be coupled to the platen 314 and rotates the substrate 101 about a vertical axis of the platen 314. The platen 314 includes an electrode 324 disposed therein. In one embodiment, the electrode 324 is a chucking device, such as an electrostatic chuck, for securing the substrate 101 to the electrode 324 during processing of the substrate 101. Power from the power supply 304 may be utilized to bias the electrode 324 to either chuck the substrate 101 to the electrode 324 or to affect the bombardment of electrons to the substrate 101.
[0028]
[0034] In operation, a plasma is generated within the electron beam chamber 302 by a variety of bulk and surface processes, for example by inductive coupling. Ions generated by an inductively coupled plasma are believed to be influenced by an electric field that encourages ions generated from the plasma of the inert gas and process gas to collide with the electrode 322. Other plasma generation processes, such as capacitively coupled configurations, hollow cathode configurations, DC electrode biasing, or electron beam plasma generation processes, may be utilized in accordance with embodiments described herein.
[0029]
[0035] Ion bombardment of the electrode 322 is believed to cause the electrode 322 to emit secondary electrons. Negatively charged energetic secondary electrons are emitted from the electrode 322. Thus, the electron beam 316 is accelerated from the electrode 322 at a beam angle θ with respect to a reference plane 318 oriented perpendicular (i.e., surface normal) to the substrate 101. The electron beam 316 includes, but is not limited to, a spot beam, a ribbon beam, or a full substrate sized beam. The generated electron beam 316 includes one of a substrate etch chemistry, a device material etch chemistry, or a resist etch chemistry, depending on the process gases utilized.
[0030]
[0036] As described herein, the ion beam 216 generated from the angled etching system 200 (e.g., an ion etching system) and the electron beam 316 generated from the angled etching system 300 (e.g., an electron beam etching system) are collectively described as the beam 516 (as shown in FIGS. 5A-5J). In that case, the beam 516 is one of an ion beam or an electron beam. In some embodiments of the method 400 that may be combined with other embodiments described herein, the beam 516 has one of a substrate etch chemistry, a device material etch chemistry, or a resist etch chemistry in the operations of the method 400 described herein. In some embodiments that may be combined with other embodiments described herein, at least the substrate etch chemistry and the resist etch chemistry are different. In other embodiments that may be combined with other embodiments described herein, at least the device material etch chemistry and the resist etch chemistry are different. As described herein, the ability to tune the etch rate of the resist material 506 and one of the device layer 114 or substrate 101, and rotation of the substrate 101 forms a blazed optical device structure without multiple lithographic patterning and etching steps.
[0031]
[0037] Figure 4 is a flow diagram of a method 400 for forming a plurality of blazed optical device structures 106 of an optical device structure 100, as shown in Figures 5A-5E and 5F-5J. Figures 5A-5E are schematic side views of a portion 501 of a substrate 101 during method 400. Figures 5F-5J are schematic top views of a portion 501 of a substrate 101 during method 400.
[0032]
[0038] For ease of explanation, the method 400 is described with reference to the angled etching system 200 of FIG. 2 and the angled etching system 300 of FIG. 3. However, it should be noted that angled etching systems other than the angled etching systems 200, 300 may also be utilized in conjunction with the method 400. In an embodiment that may be combined with other embodiments described herein, the portion 501 may correspond to a portion or an entire surface of a substrate 101 of a planar optical device having a plurality of blazed optical device structures 106 formed thereon. In another embodiment that may be combined with other embodiments described herein, the portion 501 may correspond to a portion or an entire surface of a substrate 101 of a waveguide coupler having a plurality of blazed optical device structures 106 formed thereon. The portion 501 may correspond to one or more diffraction gratings 104. Although Figures 5A-5E and 5F-5J depict etching substrate 101 such that blazed optical device structure 106 is disposed within the substrate, device layer 114 may be disposed on surface 103 (as described above) such that blazed optical device structure 106 is disposed within device layer 114.
[0033]
[0039] In operation 401, as shown in Figures 5A and 5F, the substrate 101 is positioned at a first rotation angle φ1 as defined by the reference line 502 as shown in Figure 5F. In one embodiment, which may be combined with other embodiments described herein, the first rotation angle φ1 is 0 degrees as defined by the reference line 502. The substrate 101 or device layer 114 (not shown) includes a patterned resist 504 disposed thereon. The patterned resist 504 includes a resist material 506 patterned into a plurality of resist structures 508 disposed on the surface 103 of the substrate 101. The resist material 506 of the patterned resist 504 is selected based on a substrate etch chemistry (in embodiments in which the substrate 101 is etched to form the blazed optical device structure 106) or a device material etch chemistry (in embodiments in which the device material layer 114 is etched to form the blazed optical device structure 106). In one embodiment, the resist material 506 is a photosensitive material. Thereby, the patterned resist 504 may be patterned by a lithography process, such as photolithography or digital lithography, or by a laser ablation process to form a plurality of resist structures 508. In an embodiment, the resist material 506 is an imprintable material. Thereby, the patterned resist 504 may be patterned by a nanoimprint process to form a plurality of resist structures 508. In another embodiment that may be combined with other embodiments described herein, the resist material 506 is a hard mask material, and the patterned resist 504 may be patterned through one or more etching processes to form a plurality of resist structures 508. In yet another embodiment that may be combined with other embodiments described herein, the patterned resist 504 is an optical planarization layer.
[0034]
[0040] Each resist structure 508 includes a lower surface 509, a first sidewall 510, a second sidewall 512, and a top surface 514. Each resist structure 508 has a height 515 from the lower surface 509 to the top surface 514. Each resist structure 508 has a width 522 from the first sidewall 510 to the second sidewall 512 of the resist structure 508. A plurality of gaps 518 are defined by adjacent resist structures 508. Each of the gaps 518 has a linewidth 520 between the first sidewall 510 and the second sidewall 512 of the adjacent resist structure 508. The height 515, linewidth 520, and width 522 are selected to adjust the number and linewidth d of steps 110 of the blazed surface 108 of the plurality of blazed device structures 106. For example, increasing height 515 increases the number of repeat intervals that etch substrate 101 (or device layer 114 ) and resist structure 508 , thereby increasing the number of steps 110 .
[0035]
[0041] In operation 402, the substrate 101 is exposed to the beam 516 at a beam angle θ relative to a surface normal of the substrate 101. In one embodiment, which may be combined with other embodiments described herein, the beam angle θ is about 10 degrees to about 80 degrees relative to a surface normal of the substrate 101. The beam 516 has a substrate etch chemistry or a device etch chemistry that is selective to the resist material 506. That is, the exposed portions 517 of the substrate 101 or the exposed portions of the device layer 114 (not shown) are removed at a higher rate than the resist material 506. After the beam 516 etches the exposed portions of the substrate 101, in operation 402 (as shown in FIG. 5B ), a depth h of the exposed portions 517 corresponding to the blazed device structure 106 is formed.
[0036]
[0042] In operation 403, as shown in FIG. 5H, the substrate 101 is rotated to a second rotation angle φ2 defined by the reference line 502. In an embodiment that may be combined with other embodiments described herein, the platen 214, 314 holding the substrate 101 is rotated to a second rotation angle φ2. In another embodiment that may be combined with other embodiments described herein, the second rotation angle φ2 corresponds to 90 degrees relative to the reference line 502. The rotation of the substrate 101 is not limited to a rotation angle φ corresponding to 90 degrees, but may correspond to any predetermined angle φ. This rotation allows the beam 516 to contact the resist structure 508 due to a shadowing effect. In an embodiment that may be combined with other embodiments described herein, the beam 516 will remain at a beam angle θ with respect to the reference surface 218, 318 oriented perpendicular (i.e., surface normal) to the substrate 101 throughout the method 400. A constant beam angle may improve throughput. 5A, 5B, and 6A because there is no need to reset the beam angle θ. In one embodiment, which may be combined with other embodiments described herein, the method 400 described herein uses only one angled etching system 200, 300 and requires patterning the resist material 506 only once, providing mass production capabilities.
[0037]
[0043] In operation 404, the resist structure is exposed to the beam 516 at a beam angle θ. The beam 516 etches either the first sidewall 510 or the second sidewall 512, depending on which sidewall 510, 512 is exposed to the beam 516. In an embodiment, which may be combined with other embodiments described herein, the first sidewall 510 is exposed to the beam 516. The beam 516 has a chemistry that corresponds to the resist etch chemistry, such that the ions or electrons will substantially etch only the resist structure 508 during the resist etch process. The resist etch chemistry is selective to the substrate 101 or device layer 114. That is, the resist structure 508 is removed at a higher rate than the device layer 114 or substrate 101. After the beam 516 etches the resist structure 508, the width 522 of the resist structure 508 is reduced relative to the width shown in FIGS. 5A and 5B. The line width 520 between the first sidewall and the second sidewall is increased relative to the line width shown in Figures 5A and 5B.
[0038]
[0044] As shown in FIG. 5C, a first step of the plurality of steps 110 is formed. The plurality of steps 110 form the blazed surface 108 shown in FIG. 1B and FIG. 1C. The blaze angle γ is the angle between the blazed surface 108 and the surface parallel line p of the substrate 101. The blaze angle γ may be achieved by increasing or decreasing the etching rate of the beam 516. Adjustment of the blaze angle γ may be achieved by etching at different rates, such that the depth h, line width 520, and width 522 are predetermined values corresponding to different numbers of steps 110 formed on the blazed surface 108. Thus, the blaze angle γ may be adjusted such that the blazed device structure 106, such as the blazed device structure 106 of the diffraction grating 104, may modulate the light propagating through the optical device 100 as desired.
[0039]
[0045] In operation 405, operations 401-404 are repeated until a predetermined number of steps 110 (as shown in FIG. 1B and FIG. 1C) are formed on the optical device 100. In one embodiment, which may be combined with other embodiments described herein, the substrate 101 is rotated to a first rotation angle φ1 and the substrate 101 or device layer 114 is etched using the beam 516 until the resist structures 508 are removed or the line width 520 of the gap 518 has a predetermined line width. As shown in FIG. 5I, the platen 214, 314 on which the substrate 101 is positioned is rotated to a first rotation angle φ1. As shown in FIG. 5, the depth h of the exposed portion 517 corresponding to the blazed device structure 106 increases with respect to the depth h shown in FIG. 5A-5C. As shown in FIG. 5J, the platen 214, 314 on which the substrate 101 is positioned is rotated to a second rotation angle φ2 defined by the reference line 502. After the beam 516 etches the resist structures 508, the width 522 of the resist structures 508 decreases relative to the width shown in Figures 5A-5D. The line width 520 between the first sidewall 510 and the second sidewall 512 increases relative to the line width 520 shown in Figures 5A-5D. In optional operation 406, the remaining resist material 506 disposed on the device layer 114 or substrate 101 is removed. Although only four resist structures 508 and three gaps 518 are shown, the entire patterned resist 504 may be etched. A desired number of blazed device structures 106 are thereby formed according to a predetermined design of the optical device 100.
[0040]
[0046] In summary, a method for forming an optical device structure is described herein. The method utilizes the rotation of a substrate having a blazed optical device structure formed thereon and the ability to adjust the etch rate of a patterned resist disposed on the substrate and one of the device layer or the substrate to form an optical device structure without multiple lithography patterning and tilted etching steps. If the beam angle is constant, throughput can be improved because there is no need to reset the beam angle θ. Only one tilted etching system can be used and the resist material needs to be patterned only once, which can provide mass production capabilities.
[0041]
[0047] While the forgoing is directed to multiple embodiments of the disclosure, other and further embodiments of the disclosure may be devised without departing from the basic scope thereof, the scope of which is defined by the following claims.
Claims
1. A first rotation angle φ is introduced into the path of the beam. 1 wherein the beam is configured to be projected onto a surface of the substrate at a beam angle θ relative to a surface normal of the substrate, the substrate having a patterned resist formed thereon, the patterned resist comprising: two or more resist structures, each of the resist structures having a width; and positioning a substrate including one or more gaps, each of the gaps being defined by adjacent resist structures and having a linewidth defined by the adjacent resist structures; The beam is rotated by the first rotation angle φ 1 Etching the substrate positioned at The substrate is rotated at a second rotation angle φ 2 and etching sidewalls of the resist structures directed toward the beam, the sidewalls being etched such that the width of the resist structures decreases and the linewidth of the gap increases; The substrate is rotated at the first rotation angle φ 1 and rotate the beam by the first rotation angle φ 1 Etching the substrate at forming two or more optical device structures in the substrate, the forming of the optical device structures comprising: The substrate is rotated at the second rotation angle φ until the resist structure is removed or the line width of the gap has a predetermined line width. 2 to 30°; etching the sidewalls of the resist structure with the beam; and rotating the substrate at the first rotation angle φ 1 and repeating rotating the substrate to a position adjacent the substrate and etching the substrate with the beam to form two or more optical device structures.
2. The first rotation angle φ 12. The method of claim 1, wherein etching the substrate at comprises generating the beam with a substrate etch chemistry that etches the substrate at a higher rate than the patterned resist.
3. 10. The method of claim 1, wherein etching the sidewalls of the resist structure comprises generating the beam with a resist etch chemistry that etches the patterned resist at a higher rate than the substrate.
4. The first rotation angle φ 1 The method of claim 1 , wherein: is 0 degrees.
5. The second rotation angle φ 2 The method of claim 1 , wherein is 90 degrees.
6. The method of claim 1 , wherein the beam angle θ is from about 10 degrees to about 80 degrees.
7. The method of claim 1 , wherein the resist structure comprises a photodefinable material, an imprintable material, an optical planarization material, or a hard mask material.
8. The method of claim 1 , wherein the optical device structure includes at least 32 steps.
9. The method of claim 1 , wherein the beam is a ribbon beam, a spot beam, or a full substrate size beam.
10. The method of claim 1 , wherein the beam is an ion beam or an electron beam.
11. A first rotation angle φ is introduced into the path of the beam. 1 wherein the beam is configured to be projected onto a surface of the substrate at a beam angle θ relative to a surface normal of the substrate, the substrate having a device layer disposed thereon and a patterned resist formed on the device layer, the patterned resist comprising: two or more resist structures, each of the resist structures having a width; and positioning a substrate including one or more gaps, each of the gaps being defined by adjacent resist structures and having a linewidth defined by the adjacent resist structures; The substrate is rotated at the first rotation angle φ 1 etching the device layer with the beam while positioned at The substrate is rotated at a second rotation angle φ 2 and etching sidewalls of the resist structures directed toward the beam, the sidewalls being etched such that the width of the resist structures decreases and the linewidth of the gap increases; The substrate is rotated at the first rotation angle φ 1 and rotate the beam by the first rotation angle φ 1 etching the device layer at forming two or more optical device structures in the device layer, the forming of the optical device structures comprising: The substrate is rotated at the second rotation angle φ until the resist structure is removed or the line width of the gap has a predetermined line width. 2 rotating the substrate at a first rotation angle φ to a first position; etching the sidewalls of the resist structure with the beam; and rotating the substrate at a first rotation angle φ to a first position. 1 and repeating rotating the beam to a position at which the device layer is etched and etched with the beam to form two or more optical device structures.
12. 12. The method of claim 11, wherein etching the device layer comprises generating the beam with a device material etch chemistry that etches the device layer at a higher rate than the patterned resist.
13. 13. The method of claim 12, wherein an etch selectivity between the device material and the patterned resist is about 5:1 or greater.
14. 12. The method of claim 11, wherein etching the sidewalls of the resist structure comprises generating the beam with a resist etch chemistry that etches the patterned resist at a higher rate than the device layer.
15. 15. The method of claim 14, wherein an etch selectivity between the patterned resist and the device layer is about 10:1 or greater.
16. The first rotation angle φ 1 is 0 degrees, and the second rotation angle φ 2 The method of claim 11 , wherein is 90 degrees.
17. The method of claim 11 , wherein the beam is a ribbon beam, a spot beam, or a full substrate size beam.
18. The method of claim 11 , wherein the optical device structure includes at least 32 steps.
19. The device layers are made of silicon oxycarbide (SiOC), titanium dioxide (TiO 2 ), silicon dioxide (SiO 2 ), vanadium(IV) oxide (VO x ), aluminum oxide (Al 2 O 3 ), aluminum doped zinc oxide (AZO), indium tin oxide (ITO), tin dioxide (SnO 2 ), zinc oxide (ZnO), tantalum pentoxide (Ta 2 O 5 ), silicon nitride (Si 3 N 4 ), zirconium dioxide (ZrO 2 ), niobium oxide (Nb 2 O 5 ), cadmium stannate (Cd 2 SnO 4 12. The method of claim 11, further comprising one or more of: silicon carbonitride (SiCN)-containing materials.
20. A first rotation angle φ is introduced into the path of the beam. 1 wherein the beam is configured to be projected onto a surface of the substrate at a beam angle θ relative to a surface normal of the substrate, the substrate having a patterned resist formed thereon, the patterned resist comprising: two or more resist structures, each of the resist structures having a width; and one or more gaps, each of the gaps being defined by adjacent resist structures and having a linewidth defined by the adjacent resist structures; the substrate is etched by the beam generated by a substrate etching chemistry; positioning a substrate, the resist structure being etched by the beam generated by a resist etch chemistry different from the substrate etch chemistry; Using the beam generated by the substrate etch chemistry, the first rotation angle φ 1 Etching the substrate positioned at The substrate is rotated at a second rotation angle φ 2 and etching sidewalls of the resist features with the beam at the beam angle θ, wherein the beam produced by the resist etching chemistry etches the sidewalls of the resist features directed at the beam, etching the sidewalls such that the width of the resist features decreases and the linewidth of the gap increases; The substrate is rotated at the first rotation angle φ 1 and rotate the beam by the first rotation angle φ 1 Etching the substrate at forming two or more optical device structures in the substrate, the forming of the optical device structures comprising: The substrate is rotated at the second rotation angle φ until the resist structure is removed or the line width of the gap has a predetermined line width. 2to etch the sidewalls of the resist structure using the beam generated by the resist etching chemistry; and rotating the substrate at the first rotation angle φ. 1 and etching the substrate with the beam generated by the substrate etch chemistry, forming two or more optical device structures.
Citation Information
Patent Citations
Method for manufacturing step-type phase grating
CN102331594A
Production of diffraction grating plate
JP1997230121A
Production of diffraction optical device
JP2001074924A
Method for manufacturing diffraction optical element
JP2002350623A
Optical element equipped with binary blaze grating, metal mold for molding, and optical pickup unit