Cork member, and manufacturing method therefor

By using cellulose nanofibers to bind cork grains, the cork member achieves low carbon dioxide emissions and retains functional properties, addressing the environmental impact of traditional cork products.

JP2024147411APending Publication Date: 2024-10-16UCHIYAMA MFG
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2023060402
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-03
Publication Date
2024-10-16

AI Technical Summary

Technical Problem

There is a need for products with low carbon dioxide emissions during their life cycles, particularly in the context of environmental conservation, as naturally derived products are increasingly sought after, and existing cork members do not adequately address this issue.

Method used

A cork member is manufactured by binding cork grains together using cellulose nanofibers as a binder, and the manufacturing process involves mixing cork grains with a cellulose nanofiber dispersion and evaporating the liquid dispersion medium.

Benefits of technology

This approach results in a cork member with significantly reduced carbon dioxide emissions throughout its life cycle, while maintaining desirable properties such as heat insulation and sound absorption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024147411000001_ABST
    Figure 2024147411000001_ABST
Patent Text Reader

Abstract

To provide a cork member in which a discharge amount of carbon dioxide in a life cycle is low.SOLUTION: A cork member is formed by binding cork particles to each other via a binder. The binder is a cellulose nanofiber.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a cork component and a method for producing the same. [Background technology]

[0002] Cork tissue, which is the bark of the cork oak, has various properties such as elasticity, heat insulation, waterproofness, breathability, and sound absorption. Therefore, cork particles, which are crushed cork bark, are compressed and molded together with an adhesive, bonded together with the adhesive, and heated as necessary to evaporate the solvent in the adhesive, and used as cork components in various forms according to the purpose. For example, a wooden flooring material having a layer of a mixture of cellulose-based dry fine powder and cork powder and a plate-shaped member made of resin or the like is known (see, for example, Patent Document 1).

[0003] On the other hand, various water-based adhesives have been studied from the viewpoint of reducing the environmental load. Also, cellulose nanofiber (hereinafter, also referred to as "CNF") is known as a type of naturally derived adhesive component. Known water-based adhesives containing CNF include an easily peelable adhesive composition in which CNF and other additives are dispersed in water, and a water-based resin adhesive and a water-based adhesive composition containing CNF (see, for example, Patent Document 2 and Patent Document 3). [Prior art documents] [Patent documents]

[0004] [Patent Document 1] Japanese Patent Application Publication No. 60-210406 [Patent Document 2] JP 2017-025130 A [Patent Document 3] JP 2014-132072 A Summary of the Invention [Problem to be solved by the invention]

[0005] In recent years, natural products have been in demand from the perspective of environmental conservation. In addition, carbon dioxide (CO 2 ) emissions, and there is a demand for products with low carbon dioxide emissions over their life cycle.

[0006] One aspect of the present invention aims to provide a cork component that has low carbon dioxide emissions over its life cycle. [Means for solving the problem]

[0007] In order to solve the above problems, a cork material according to one embodiment of the present invention is a cork material in which cork particles are bound to each other via a binder, and the binder is cellulose nanofiber.

[0008] In addition, in order to solve the above problems, a method for manufacturing a cork part according to one embodiment of the present invention includes a step of mixing cork particles with a cellulose nanofiber dispersion, and a step of evaporating the dispersion medium of the cellulose nanofiber dispersion from the resulting mixture. Effect of the Invention

[0009] According to one aspect of the present invention, a cork member having low carbon dioxide emissions over its life cycle can be provided. [Brief description of the drawings]

[0010] [Figure 1] FIG. 2 is a photograph showing the entire cork member of Example 1. [Diagram 2] FIG. 2 is an enlarged photograph of a portion of the surface of the cork member of Example 1. [Diagram 3] FIG. 13 is a photograph showing the entire cork member of Example 2. [Figure 4] FIG. 11 is an enlarged photograph of a portion of the surface of the cork member of Example 2. [Diagram 5] FIG. 2 is a scanning microscope photograph of the boundary between cork particles in a cross section of the cork member of Example 1. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] [Cork parts] The cork member is made of cork particles bonded together with a binder. The cork member is a bonded body of such cork particles, and can have various shapes and can be used for various purposes.

[0012] The cork particles are crushed cork. Various sizes of cork particles, ranging from hundreds of microns to tens of millimeters, are known. In the embodiment of the present invention, cork particles of an appropriate size are used depending on the application or desired properties of the cork member.

[0013] Examples of cork products include cork stoppers, coasters, cork boards, cork mats, and functional products. The functional products have a specific shape depending on the application to achieve the intended function. Examples of functional products include heat insulating products, sound absorbing products, and insulating products.

[0014] The binder that binds the cork particles together is cellulose nanofiber (CNF). CNF is a cellulose fiber with a nano-sized fiber width. The fiber diameter of CNF is, for example, several nm to several hundred nm (e.g., 4 to 500 nm), and the aspect ratio of CNF (ratio of average fiber length to average fiber diameter) is, for example, 100 or more. In this specification, "to" means a range with the numerical values ​​before and after it as boundary values.

[0015] The average fiber diameter and the average fiber length of the CNF may be the average values ​​of the fiber diameter and the fiber length of a plurality of fibers (e.g., 200 fibers) randomly selected using, for example, a transmission electron microscope. The fiber size of the CNF may be a value obtained by another measurement method or a catalog value, as long as it is shown that the CNF has a fiber width on the nano-order.

[0016] The CNF may be modified. Examples of modified cellulose include carboxymethylated cellulose, carboxylated cellulose, and cationically modified cellulose. The CNF may be substantially only unmodified cellulose nanofibers, may be a mixture of unmodified cellulose nanofibers and modified cellulose nanofibers, or may be substantially only modified cellulose nanofibers.

[0017] More specifically, in the cork component, the CNFs are interposed between the cork particles. The cork particles are closed-cell foams, and when the cork particles are bound together, the CNFs do not penetrate into the numerous voids present in the cork particles, but rather bond the surfaces of the cork particles together.

[0018] Since the CNFs are present at the boundaries between the cork particles, the cork component can be essentially constructed as an aggregate of cork particles. Therefore, from the viewpoint of forming the cork component, the CNF content in the cork component may be within a range capable of binding the cork particles together.

[0019] The cork member may be composed of only the cork particles and the CNF that binds them, or may further contain other components as long as the effects of this embodiment can be obtained. Examples of the other components include heat insulating particles and additives. The content of the other components in the coil member can be appropriately determined within a range in which both the effect of the present invention and the effect of the addition of the other components can be obtained.

[0020] The insulating particles are particles that have insulating properties, for example, particles that have many voids like cork particles and have insulating properties equal to or greater than those of cork particles. The insulating particles are preferably particles that are bound together by CNF like cork particles, and in a cork component that further contains such insulating particles, the cork particles and the insulating particles are preferably bound together by CNF.

[0021] Examples of the additives include flame retardants, surfactants, thickeners, moisturizing agents, dye deepening agents, preservatives, antifungal agents, degassing agents, antifoaming agents, and reduction inhibitors.

[0022] [Characteristics of cork materials] The cork member according to the embodiment of the present invention can exhibit various properties provided by the cork particles and CNF.

[0023] [Thermal insulation] From the viewpoint of applying the cork member to a heat insulating member, the thermal conductivity of the cork member is preferably 0.1 W / (m / K) or less, and more preferably 0.08 W / (m / K) or less. There is no lower limit for the thermal conductivity of the cork member, and it may be appropriately set within a range that is feasible for the cork member. The thermal conductivity of the cork member can be measured by a known method for measuring the thermal conductivity of the cork member, and can be adjusted by a known method for adjusting the thermal conductivity of the cork member.

[0024] The cork member according to the present embodiment is expected to exhibit other properties besides heat insulation, and to be applied to such specific uses. For example, the cork member is expected to exhibit sound absorption properties, and to be applied to sound absorption members. The sound absorption properties can be measured by a known technique capable of measuring the sound absorption properties of the cork member. The cork member according to the present embodiment is also expected to exhibit insulating properties, and to be applied to insulating members. The insulating properties can be measured by a known technique capable of measuring the insulating properties of the cork member, similar to the above-mentioned sound absorption properties.

[0025] In addition, since the cork member according to the present embodiment can be manufactured using CNF as an adhesive, it can be manufactured without using organic solvents, as described below. 2 The emissions are sufficiently low and the life cycle carbon dioxide emissions (LC-CO 2 It is expected that cork materials with lower LC-CO emissions will be provided than conventional cork materials. 2 The amount of emissions can be calculated using the following formula: <expression> Mass of each material (kg) x Emission coefficient of each material (kg-CO 2 / kg)

[0026] [Method of manufacturing cork member] The cork part of this embodiment can be manufactured by a method including a mixing step of mixing cork particles with a CNF dispersion, and an evaporation step of evaporating the dispersion medium of the CNF dispersion from the resulting mixture.

[0027] [Mixing process] In the mixing step, the cork particles may be commercially available products, or may be cork material that has been crushed and classified as necessary.

[0028] The CNF dispersion is composed of CNF as a dispersoid and a dispersion medium. The CNF dispersion may be a commercially available product or a prepared product. The CNF dispersion may be prepared, for example, by suspending natural cellulose in water and treating it with a high-pressure homogenizer or grinder to pulverize it.

[0029] The dispersion medium may be any liquid capable of dispersing CNF well. Examples of the dispersion medium include water, organic solvents, and mixed solutions thereof. From the viewpoint of reducing the burden on the environment, it is preferable to use an aqueous dispersion of CNF for the CNF dispersion, that is, the dispersion medium is water. Also, from the viewpoint of reducing the burden on the environment, it is preferable that the CNF dispersion is a dispersion consisting of only CNF and water and does not contain additives. The content of CNF in the CNF dispersion may be an amount capable of functioning as an adhesive for cork particles, for example, 1% by mass or more.

[0030] [Evaporation process] In the evaporation step, the dispersion medium can be removed from the mixture by heating, but is not limited thereto. The evaporation step may be a step of drying the mixture, and for example, when the dispersion medium is water, it can be performed by a method such as spray drying, freeze drying, or vacuum drying. When the dispersion medium is a mixed solution of water and an organic solvent, the evaporation step can be performed by a method such as drying using a drum dryer or spray drying using a spray dryer.

[0031] The temperature of the evaporation step can be appropriately determined depending on the method of the evaporation step. When heating is used, the temperature of the evaporation step should be determined within a range in which the cork particles and CNF are not denatured by heat.

[0032] [Other processes] The manufacturing method of the present embodiment may further include other steps in addition to the steps described above, as long as the effects of the present invention are obtained. For example, the manufacturing method may further include a compression step of compressing the mixture. The compression step is suitable from the viewpoint of obtaining a cork member having a specific shape by molding.

[0033] It is preferred from the viewpoint of obtaining a molded cork part that the compression step is carried out simultaneously with the evaporation step, i.e. the dispersion medium is evaporated from the mixture while the mixture is compressed. Such a step can be carried out by placing the mixture in a mold having a shape corresponding to the specific shape and heating it while compressing it in the mold.

[0034] 〔summary〕 A first aspect of the present invention is a cork component formed by bonding cork particles to each other via a binder, the binder being cellulose nanofiber. According to the first aspect, it is possible to provide a cork component with low carbon dioxide emissions over its life cycle.

[0035] The second aspect of the present invention is the same as the first aspect, except that the cellulose nanofibers are interposed between the cork particles. The second aspect is even more effective in terms of fully exhibiting the properties of cork in the cork member.

[0036] A third aspect of the present invention is a method for producing a cork part, comprising the steps of mixing cork particles with a cellulose nanofiber dispersion and evaporating the dispersion medium of the cellulose nanofiber dispersion from the resulting mixture. According to the third aspect, it is possible to provide a cork part with low carbon dioxide emissions over its life cycle.

[0037] A fourth aspect of the present invention is the third aspect, in which an aqueous dispersion of cellulose nanofibers is used as the cellulose nanofiber dispersion. The fourth aspect is even more effective from the viewpoint of reducing the environmental burden caused by the production of cork members.

[0038] A fifth aspect of the present invention is the method according to the third or fourth aspect, further comprising a step of compressing the mixture, and evaporating the dispersion medium from the mixture while compressing the mixture. The fifth aspect is even more effective in terms of obtaining a cork member molded into a desired shape.

[0039] According to the above-mentioned embodiment of the present invention, a cork member is provided that is essentially made of coil particles and CNF and has a simple structure, yet can exhibit various useful properties. The present invention is expected to contribute to reducing carbon dioxide emissions, and is expected to contribute to achieving, for example, Goal 13 of the Sustainable Development Goals (SDGs) advocated by the United Nations, "Take urgent action to combat climate change."

[0040] The present invention is not limited to the above-described embodiments, and various modifications are possible within the scope of the claims. Embodiments obtained by appropriately combining the technical means disclosed in the different embodiments are also included in the technical scope of the present invention. EXAMPLES

[0041] An embodiment of the present invention will now be described.

[0042] Example 1 The following components were placed in a bowl in the following amounts and mixed to obtain Mixture 1. CNF aqueous dispersion A is an aqueous dispersion manufactured by Daio Paper Corporation, and has a CNF content of 14% by mass. Cork grains (particle size 4mm~8mm) 20 parts by mass CNF aqueous dispersion A 80 parts by mass

[0043] Mixture 1 was supplied to the mold and heated while being compressed in the mold to evaporate the water inside the mold. In this way, a plate-shaped cork member 1 was produced. Photographs of cork member 1 are shown in Figures 1 and 2. Figure 1 shows a photograph of the entire cork member 1, and Figure 2 shows an enlarged photograph of a portion of the surface of cork member 1. As shown in Figures 1 and 2, cork particles are bonded to each other via CNF to form cork member 1.

[0044] Example 2 A plate-shaped cork member 2 was produced in the same manner as in Example 1, except that CNF aqueous dispersion B was used instead of CNF aqueous dispersion A. CNF aqueous dispersion B is an aqueous dispersion produced by Nippon Paper Industries Co., Ltd., and has a CNF content of 1 mass%. Photographs of the cork member 2 are shown in Figs. 3 and 4. Fig. 3 shows a photograph of the entire cork member 2, and Fig. 4 shows an enlarged photograph of a portion of the surface of the cork member 2. As shown in Figs. 3 and 4, the cork member 2 is also formed by cork particles being bonded to each other via CNF, similar to the cork member 1. Within the range shown in these photographs, no substantial difference is confirmed between the cork member 1 and the cork member 2.

[0045] 〔evaluation〕 <Cross-section microscopy> The joints between the cork particles in the cross section of the cork member 1 were observed with a scanning electron microscope (SEM). The micrograph is shown in Figure 5. As is clear from Figure 5, two cork particles, A and B, are adjacent to each other, and as indicated by the arrows in the figure, CNF is interposed between the two cork particles. In this way, it can be seen that the CNF bonds the cork particles together. In other words, It can be seen that there is a CNF layer between the cork particles, and that the cork particles are bonded together in a planar manner via the CNF.

[0046] <Thermal insulation> The thermal conductivity of each of the cork members 1 and 2 was measured using a steady-state thermal conductivity measuring device (manufactured by ULVAC Corporation). The thermal conductivity of the cork member 1 was 0.07 W / (m / K), and the thermal conductivity of the cork member 2 was 0.07 W / (m / K). [Industrial Applicability]

[0047] INDUSTRIAL APPLICABILITY The present invention can be utilized to provide functional members that have a lower environmental impact and are capable of exhibiting various properties.

Claims

1. 1. A cork member comprising cork particles bound to each other via a binder, the binder being cellulose nanofiber.

2. The cork member according to claim 1 , wherein the cellulose nanofibers are interposed between the cork particles.

3. A method for manufacturing a cork member, comprising the steps of: mixing cork particles with a cellulose nanofiber dispersion; and evaporating the dispersion medium of the cellulose nanofiber dispersion from the resulting mixture.

4. The method for manufacturing a cork member according to claim 3 , wherein the cellulose nanofiber dispersion is an aqueous dispersion of cellulose nanofibers.

5. The method for manufacturing a cork member according to claim 3 or 4, further comprising a step of compressing the mixture, and evaporating the dispersion medium from the mixture while compressing the mixture.

Citation Information

Patent Citations

  • Manufacture of particle board

    JP1983069031A

  • Porous wooden interior finish material

    JP1993052020A

  • Method for manufacturing woody board

    JP2018103482A

  • Thermoplastic elastomer cork composites

    JP2021533018A

  • Solid molded article and manufacturing method of solid molded article, and diaphragm and manufacturing method of diaphragm

    JP2022151571A