Metal plate resistor and method of manufacturing metal plate resistor

The metal plate resistor design with slits and a through hole improves resin flow, enabling high-quality miniaturization and precise resistance values by addressing the challenges of injection molding in smaller resistors.

JP2024148907APending Publication Date: 2024-10-18KOA CORP
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023062481
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-07
Publication Date
2024-10-18

AI Technical Summary

Technical Problem

The miniaturization of metal plate resistors is hindered by the challenges of injection molding as they become smaller, making it difficult to achieve desired dimensions and quality.

Method used

A metal plate resistor design featuring a plate-shaped resistor with slits and a through hole, paired with a molded body that includes thick portions and electrodes formed by metal plating, allowing for improved resin flow during injection molding.

Benefits of technology

Enables the production of high-quality, miniaturized metal plate resistors with precise resistance values and stable dimensions through enhanced resin fluidity and reduced deformation during molding.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024148907000001_ABST
    Figure 2024148907000001_ABST
Patent Text Reader

Abstract

To provide a metal plate resistor that is for realizing a miniaturization, and a method of manufacturing the same.SOLUTION: A metal plate resistor 1 comprises: a plate-like resistor 6 that is made of a metal material; a pair of electrodes 3A and 3B that is provided to both end parts 6a and 6b of the resistor 6; and a mold body 4 that covers the resistor 6. The resistor 6 includes: a first slit 10A that extends in a width direction from one side surface 6c of the resistor 6 and is formed on the one electrode 3B side; a second slit 10B that extends in the width direction from the other side surface 6d of the resistor 6 and is formed on the other electrode 3A side; and a penetration hole 11 that is arranged between the first slit and the second slit.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a metal plate resistor and a method for making the same. [Background technology]

[0002] It is known to use a current detection resistor to monitor the current for controlling the charge / discharge current of a secondary battery. The current detection resistor is incorporated in the path of the current to be monitored, and is used in a configuration in which the voltage generated across the resistor by the current is detected, and the current is detected from a known resistance value. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japanese Patent Application Publication No. 6-020802 Summary of the Invention [Problem to be solved by the invention]

[0004] There is a type of resistor called a metal plate resistor, which is made by injection molding a thermoplastic resin (LPC) coated on a metal plate. In recent years, there has been a demand for smaller resistors as electronic devices become smaller. However, when manufacturing metal plate resistors, the difficulty of injection molding increases as the metal plate resistor becomes smaller. Therefore, it is difficult to realize the miniaturization of metal plate resistors.

[0005] It is therefore an object of the present invention to provide a metal plate resistor that can achieve miniaturization and a method for manufacturing the metal plate resistor. [Means for solving the problem]

[0006] In one embodiment, a metal plate resistor is provided, comprising a plate-shaped resistor made of a metal material, a pair of electrodes provided at both ends of the resistor, and a molded body covering the resistor. The resistor has a first slit formed on one electrode side extending in the width direction from one side surface of the resistor, a second slit formed on the other electrode side extending in the width direction from the other side surface of the resistor, and a through hole disposed between the first slit and the second slit.

[0007] In one embodiment, the molded body has a gate mark formed on the side of the resistor opposite to the side on which the first slit or the second slit is formed. In one embodiment, the resistor has a plate shape extending straight in its longitudinal direction, and the molded body has an upper thick portion arranged above the resistor and a lower thick portion arranged below the resistor, and the upper thick portion has a thickness the same as or thicker than the lower thick portion. In one embodiment, the pair of electrodes are formed by metal plating covering both ends of the resistor, and each of the pair of electrodes has a lower surface portion that is at the same height as the lower surface of the molded body or lower than the lower surface of the molded body.

[0008] In one embodiment, a method for manufacturing a metal plate resistor is provided, the method including the steps of: preparing a long resistor material made of a metal material; forming a first slit extending from one side of the resistor material, a second slit extending from the other side of the resistor material, and a through hole disposed between the first slit and the second slit; forming a molded body that covers a portion of the resistor material and fills the first slit, the second slit, and the through hole; cutting the resistor material so that a portion of the resistor material is exposed from the molded body; and forming electrodes by metal plating that covers both ends of the resistor material exposed from the molded body. Effect of the Invention

[0009] By forming a through hole in the resistor (resistor material), the fluidity of the resin poured into the space (space of the mold) in which the molded body that covers a part of the resistor (resistor material) is formed can be improved. Therefore, a high-quality metal plate resistor can be manufactured with high accuracy by injection molding. As a result, the miniaturization of the metal plate resistor can be realized. [Brief description of the drawings]

[0010] [Figure 1] FIG. 2 illustrates an embodiment of a metal plate resistor. [Diagram 2] FIG. 2(a) is a cross-sectional view taken along line AA in FIG. 1, FIG. 2(b) is an enlarged cross-sectional view of an electrode, and FIGS. 2(c) and 2(d) are views showing other embodiments of a molded body. [Diagram 3] FIG. 1 is a flow chart showing a process for manufacturing a resistor. [Figure 4] FIG. 1 illustrates one embodiment of a resistor material. [Diagram 5] FIG. 2 is a diagram showing a resistor material before and after pressing. [Figure 6] 1A to 1C are diagrams showing a process of forming a mold body. [Figure 7] FIG. 7(a) is a diagram showing a molded body formed by pouring resin into a space in a mold through a gate, and FIG. 7(b) is a side view of the resistor in FIG. 7(a). [Figure 8] 8(a) to 8(c) are diagrams showing the change over time of the resin poured into the space. [Figure 9] FIG. 9(a) is a diagram showing how a long resistor material is cut, and FIG. 9(b) is a diagram showing the cut resistor. [Figure 10] FIG. 13 illustrates another embodiment of a resistor. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Hereinafter, embodiments of the present invention will be described with reference to the drawings. In the drawings described below, the same or corresponding components are denoted by the same reference numerals, and duplicated descriptions will be omitted. In the multiple embodiments described below, the configuration of one embodiment that is not particularly described is the same as the other embodiments, so duplicated descriptions will be omitted.

[0012] FIG. 1 is a diagram showing an embodiment of a metal plate resistor. The metal plate resistor 1 is, for example, a surface-mount resistor mounted on a printed circuit board. Hereinafter, the metal plate resistor 1 may be simply referred to as resistor 1. As shown in FIG. 1, the resistor 1 includes a plate-shaped resistive element 6 made of a metal material (for example, an alloy such as a copper-manganese alloy, a copper-nickel alloy, or a nickel-chromium alloy), a pair of electrodes 3A, 3B provided on both ends 6a, 6b of the resistive element 6, and a molded body 4 made of a thermoplastic resin that covers the resistive element 6. In this embodiment, the nominal dimensions of the resistor 1 are 3.2 mm in the longitudinal direction, 1.6 mm in the width direction, and 0.6 mm in thickness. For example, the molded body 4 may be made of a thermosetting resin.

[0013] The resistor 6 has a plate shape that extends linearly in its longitudinal direction. The longitudinal direction of the resistor 6 is perpendicular to the width direction of the resistor 6. The resistor 6 has a first slit 10A extending in the width direction from one side surface 6c, a second slit 10B extending in the width direction from the other side surface 6d, and a through hole 11 disposed between the first slit 10A and the second slit 10B.

[0014] 1, the first slit 10A is formed on the side of one electrode 3B, and the second slit 10B is formed on the side of the other electrode 3A. In one embodiment, the first slit 10A may be formed on the side of the electrode 3A, and the second slit 10B may be formed on the side of the electrode 3B.

[0015] The first slit 10A and the second slit 10B restrict the flow path of the current passing through the resistive body 6. Thus, by forming the first slit 10A and the second slit 10B, the resistance value of the resistor 1 can be adjusted. The size of the first slit 10A and the second slit 10B may be determined based on the desired resistance value.

[0016] Through hole 11 is formed in the center of resistor 6, and first slit 10A and second slit 10B are disposed on both sides of through hole 11. Therefore, first slit 10A, second slit 10B, and through hole 11 are arranged in the longitudinal direction in the order of first slit 10A, through hole 11, and second slit 10B from the electrode 3B side.

[0017] The pair of electrodes 3A, 3B are formed by metal plating covering both ends 6a, 6b of the resistor 6. For example, each of the electrodes 3A, 3B has a copper-plated lower layer and a tin-plated upper layer. In order to suppress costs while ensuring solder wettability, the tin-plated upper layer has a predetermined thickness. The electrodes 3A, 3B have the same structure. For example, a middle layer plated with another metal (for example, nickel) may be provided between the copper-plated lower layer and the tin-plated upper layer.

[0018] Fig. 2(a) is a cross-sectional view taken along line AA in Fig. 1, Fig. 2(b) is an enlarged cross-sectional view of an electrode, and Fig. 2(c) and Fig. 2(d) are views showing other embodiments of a molded body. As shown in Fig. 2(a), the electrode 3A (and the electrode 3B) has an upper surface portion 3A-2 (and an upper surface portion 3B-2) arranged above the resistor 6, and a lower surface portion 3A-1 (and a lower surface portion 3B-1) arranged below the resistor 6.

[0019] The molded body 4 has an upper thick portion 4a arranged above the resistor 6 (i.e., on the side of the upper surface 6e of the resistor 6) and a lower thick portion 4b arranged below the resistor 6 (i.e., on the side of the lower surface 6f of the resistor 6). The upper surface portion 3A-2 of the electrode 3A is in close contact with the upper thick portion 4a of the molded body 4, and the lower surface portion 3A-1 is in close contact with the lower thick portion 4b. The upper surface portion 3B-2 of the electrode 3B is in close contact with the upper thick portion 4a of the molded body 4, and the lower surface portion 3B-1 is in close contact with the lower thick portion 4b.

[0020] The lower surface portion 3A-1 (and the lower surface portion 3B-1) is disposed at the same height as the lower surface of the molded body 4 (more specifically, the lower surface of the lower thick portion 4b) or below the lower surface of the molded body 4. In the embodiment shown in FIGS. 2(a) and 2(b), the entire lower surface portion 3A-1 (and the lower surface portion 3B-1) is disposed below the lower surface of the molded body 4, but in one embodiment, a part of the lower surface portion 3A-1 (and the lower surface portion 3B-1) may be disposed below the lower surface of the molded body 4.

[0021] 2(b), the electrode 3A has a riding portion 3A-1a formed on its lower surface portion 3A-1 that rides on the molded body 4. Similarly, the electrode 3B has a riding portion 3B-1a formed on its lower surface portion 3B-1 that rides on the molded body 4. By forming the riding portion 3A-1a (and the riding portion 3B-1a) in this manner, peeling of the molded body 4 from the resistor 6 can be prevented.

[0022] In the embodiment shown in Figures 2(c) and 2(d), the resistor 1 has a lower surface portion 3A-1 (and a lower surface portion 3B-1) arranged at the same height as the lower surface of the molded body 4, and an electrode 3A (and an electrode 3B) having a raised portion 3A-1a (and a raised portion 3B-1a) formed on the lower surface portion 3A-1 (and the lower surface portion 3B-1).

[0023] In the embodiment shown in Fig. 2(c), the molded body 4 has a step portion 50A formed on its lower surface, and the riding portion 3A-1a rides up on the step portion 50A. In the embodiment shown in Fig. 2(d), the molded body 4 has a chamfered portion 50B formed on its lower surface, and the riding portion 3A-1a rides up on the chamfered portion 50B.

[0024] Although not shown, the step portion 50A (or the chamfered portion 50B) is also formed on the side of the riding portion 3B-1a. Therefore, the riding portion 3B-1a is also riding on the step portion 50A (or the chamfered portion 50B).

[0025] With the configuration shown in Figures 2(c) and 2(d), the lower surface portion 3A-1 (and the lower surface portion 3B-1) is positioned at the same height as the lower surface of the molded body 4, and the electrode 3A (and the electrode 3B) has a riding portion 3A-1a (and the riding portion 3B-1a) formed on the lower surface portion 3A-1 (and the lower surface portion 3B-1).

[0026] 2(a), the thickness D1 of the upper thick portion 4a (i.e., the distance between the upper surface of the resistor 6 and the upper surface of the molded body 4) is greater than the thickness D2 of the lower thick portion 4b (i.e., the distance between the lower surface of the resistor 6 and the lower surface of the molded body 4). In other words, the upper thick portion 4a has a greater thickness than the lower thick portion 4b.

[0027] It is preferable that the thickness of the lower thick portion 4b is always constant even if the thickness of the resistor 6 is changed according to the desired resistance value. In other words, it is preferable that, as the molded body 4, even if the thickness of the resistor 6 is changed, only the thickness of the upper thick portion 4a changes. With this configuration, even if the thickness of the resistor 6 is changed according to the desired resistance value, the resistor 1 can be stably mounted without changing the height and the shape of the lower surface (mounting surface) of the resistor 1. In one embodiment, the upper thick portion 4a may have the same thickness as the lower thick portion 4b.

[0028] FIG. 3 is a flow chart showing a manufacturing process of a resistor. FIG. 4 is a diagram showing an embodiment of a resistor material. As shown in step S101 of FIG. 3 and in FIG. 4, a long resistor material made of a metal material is prepared. The resistor material constitutes a resistor 6. In the embodiment shown in FIG. 4, the long resistor material is wound around a bobbin 8 as a winding frame. There are various types of resistor materials having various thicknesses, and a resistor material having an optimal thickness is appropriately determined according to a desired resistance value.

[0029] In this embodiment, a resistor material having a thickness of 0.12 to 0.3 mm is appropriately selected and used. The width dimension of the resistor material is 1.4 mm. If the thickness is thinner than 0.12 mm, the rigidity of the resistor 6 is low, and the resistor will deform during injection molding regardless of whether or not there is a slit. If the thickness is thicker than 0.3 mm, it is difficult to form the slits and through holes.

[0030] Fig. 5 is a diagram showing the resistor material before and after press processing. As shown in Fig. 5, the resistor material before press processing is a long flat plate. As shown in step S102 of Fig. 3 and Fig. 5, a pattern press processing is performed on the resistor material to form positioning holes 12, through holes 11, and slits 10A and 10B in the resistor material.

[0031] More specifically, a punching machine (not shown) is used to punch the resistor material from its lower surface to its upper surface (i.e., from the lower surface 6f to the upper surface 6e of the resistor 6) to form the positioning hole 12, the through hole 11, and the slits 10A and 10B. For example, at least one or all of the through hole 11 and the slits 10A and 10B may be formed by laser processing.

[0032] The positioning hole 12 is used to precisely position the through hole 11, the slits 10A and 10B, and the molded body 4, and is formed first. After step S102 in Fig. 3, laser processing is performed on the surface of the resistor material (i.e., the upper surface 6e and the lower surface 6f of the resistor 6) to finely adjust the resistance value (see step S103). For example, in step S103, the resistance value may be finely adjusted by surface processing such as a grinder or sandblasting.

[0033] Fig. 6 is a diagram showing the process of forming a molded body. Fig. 7(a) is a diagram showing a molded body formed by pouring resin into a space in a mold through a gate, and Fig. 7(b) is a diagram showing the resistor in Fig. 7(a) as seen from the side.

[0034] First, resistor material is fed into a metal mold ML for forming the molded body 4 (see FIG. 6). In order to perform injection molding for multiple pieces at the same time, the metal mold ML shown in FIG. 6 is a cassette type with multiple pieces arranged therein, and is incorporated into a lower die (not shown). The metal mold ML is attachable to the lower die and removable from the lower die. There are multiple metal molds ML corresponding to different thicknesses of the resistor 6. Therefore, the most suitable metal mold ML is selected appropriately depending on the thickness of the resistor 6 and incorporated into the lower die.

[0035] When an upper die (not shown) is attached to the lower die in which the metal mold ML is incorporated, a space SP (i.e., a cavity meaning a recess in the metal mold into which resin flows) is formed in the portion of the resistor 6 where the molded body 4 is formed (see FIG. 7(a)). In this embodiment, since multiple injection moldings are performed simultaneously, the metal mold ML has multiple spaces SP, but the number of spaces SP is not limited to this embodiment.

[0036] The resistor material is fed into the mold ML so that the first slit 10A, the second slit 10B, and the through hole 11 are all contained within one space SP. The upper mold (not shown) is used in common even if the thickness of the resistor 6 changes. Therefore, even if the thickness of the resistor 6 changes, the thickness of the lower thick portion can be kept constant. In this embodiment, the thickness of the lower thick portion is 0.1 mm.

[0037] After the resistor material is fed into the mold ML, the resin constituting the molded body 4 is poured into the space SP through the gate GT (see FIG. 7(a)) to form the molded body 4 (see step S104 in FIG. 3). The molded body 4 fills the first slits 10A, the second slits 10B, and the through-holes 11.

[0038] The gate GT is a communication passage for introducing resin into the space SP. By performing injection molding of the molded body 4 through the gate GT, a gate mark 20 is formed on the side of the molded body 4 (see FIG. 7(b)). After injection molding, the molded body 4 is connected to the gate portion (resin filled in the gate GT), so it needs to be separated from the gate portion. The gate mark 20 is a cut mark that is created when the molded body 4 is separated from the gate portion.

[0039] As shown in Figures 7(a) and 7(b), the molded body 4 has a side 4c arranged on the side of side 6c of the resistor 6, a side 4d arranged on the side of side 6d of the resistor 6, and a gate mark 20 formed on the side 4d.

[0040] More specifically, the gate mark 20 is formed on the side of the resistor 6 opposite to the side on which the first slit 10A or the second slit 10B is formed. In this embodiment, the gate mark 20 is formed on the side 4d arranged on the side of the side 6d opposite to the side 6c on which the first slit 10A is formed. In one embodiment, the gate mark 20 may be formed on the side 4c arranged on the side of the side 6c opposite to the side 6d on which the second slit 10B is formed.

[0041] In this manner, when mold body 4 is formed into resistor body 6, gate mark 20 is disposed so as to be adjacent to second slit 10B (or first slit 10A) in the longitudinal direction of resistor 1.

[0042] Moreover, the gate mark 20 is disposed on the electrode 3B (or electrode 3A) side in the longitudinal direction (substantially the same position as the first slit 10A (or the second slit 10B)). With this arrangement, it is possible to prevent the resistor 6 from being deformed due to the resin being poured into the space SP through the gate GT.

[0043] When pressurized resin is poured into the space SP through the gate GT, stress is generated in the resistor 6, i.e., the resistor material, by the poured resin. In this embodiment, the gate GT is disposed on the opposite side of the first slit 10A (or the second slit 10B). More specifically, the gate GT is disposed on the opposite side of the first slit 10A (or the second slit 10B) formed in the side surface 6c (or the side surface 6d) of the resistor 6, and on the electrode 3B (or electrode 3A) side in the longitudinal direction (substantially the same position as the first slit 10A (or the second slit 10B)).

[0044] In this state, when resin is poured from the opposite side of the first slit 10A (or the second slit 10B) through the gate GT, it is possible to prevent the resin poured into the first slit 10A (or the second slit 10B) from directly colliding with the first slit 10A (or the second slit 10B), thereby preventing deformation of the resistor 6 due to stress generated in the resistor 6.

[0045] On the other hand, when the gate GT is arranged on the same side as the first slit 10A (or the second slit 10B), more specifically, when the gate GT is arranged on the same side as the first slit 10A (or the second slit 10B) formed in the side surface 6c (or the side surface 6d) of the resistor 6 and on the electrode 3B (or the electrode 3A) side (approximately the same position as the first slit 10A (or the second slit 10B) in the longitudinal direction), when resin is poured from the first slit 10A (or the second slit 10B) side through the gate GT, the resin collides with the corner of the side surface 6c (or the side surface 6d) of the resistor 6 and the side surface of the slit, and is pushed downward and may be significantly deformed. Therefore, the resistor 6 may be deformed due to the stress generated in the resistor 6.

[0046] 8(a) to 8(c) are diagrams showing the change over time of the resin poured into the space. As shown in Fig. 8(a) to 8(c), by pouring the resin through the gate GT from the electrode 3B (or electrode 3A) side, i.e., from the edge of the space SP, the resin fills the entire space SP without leaving any gaps, and the first slit 10A, the second slit 10B, and the through hole 11 are filled with the resin.

[0047] The resistor 1 is manufactured by injection molding. More specifically, the resistor 1 is manufactured by coating the resin (more specifically, thermoplastic resin or thermosetting resin) constituting the molded body 4 onto the resistor material (i.e., metal material) constituting the resistor 6. Generally, in the process of filling the cavity with resin, due to the fluidity of the resin, the resin may not be filled sufficiently, resulting in a void (underfill). This phenomenon is called a short shot. The problem of such short shots becomes more prominent as metal plate resistors become smaller.

[0048] According to this embodiment, the through holes 11 formed in the resistor 6 can improve the fluidity of the resin poured into the space SP in which the resistor 6 is disposed, and can suppress the occurrence of short shots. As a result, a high-quality resistor 1 can be manufactured with high accuracy by injection molding, and the miniaturization of the resistor 1 can be stably achieved.

[0049] In this embodiment, the through hole 11 is circular and has a hole diameter of 0.3 to 0.7 mmΦ. If the hole diameter is smaller than 0.3 mmΦ, it is difficult to form the through hole, and if the hole diameter is larger than 0.7 mmΦ, it is difficult to form the through hole because the position of the through hole is too close to the slit.

[0050] The first slit 10A and the second slit 10B formed in the resistor 6 can also achieve the same effect as the through hole 11. More specifically, the slits 10A and 10B formed in the resistor 6 can improve the fluidity of the resin, similar to the through hole 11, and can suppress the occurrence of short shots.

[0051] In this embodiment, the first slit 10A and the second slit 10B each have a depth (dimension in the width direction) of 0.3 to 0.9 mm and a width (dimension in the longitudinal direction) of 0.3 mm. If the depth is shallower than 0.3 mm, the effect of suppressing short shots is reduced. If the depth is deeper than 0.9 mm, the rigidity of the resistor 6 is reduced, and the resistor 6 is deformed during injection molding.

[0052] In this embodiment, the gate mark 20 is not disposed on the center side of the molded body 4 in the longitudinal direction of the resistor 1, but is disposed on the electrode 3B (or electrode 3A) side (see FIG. 7(b)). This arrangement also makes it possible to suppress the occurrence of short shots.

[0053] Furthermore, by forming the through hole 11 in the resistor 6, the upper thick portion 4a and the lower thick portion 4b of the molded body 4 are connected to each other through the through hole 11, improving the adhesion between them (see FIG. 2(a)). The molded body 4 having such a strong structure can more reliably prevent peeling from the resistor 6.

[0054] In order to improve the adhesion of the molded body 4 to the resistor 6, it is important to determine the ratio of resin occupying the connection part (shaded part in FIG. 7(a)) between the upper thick part 4a and the lower thick part 4b. For example, the ratio of resin occupying the connection part is calculated by dividing the area of ​​the connection part by the area of ​​the horizontal cross section of the molded body 4 and expressing the result as a percentage. The size of the connection part is determined based on the size of the through hole 11 and the sizes of the slits 10A and 10B.

[0055] According to the results of prototype evaluation, the ratio of the resin occupying the connection portion is preferably 20% or more. Therefore, in one embodiment, the size of the through hole 11 and the sizes of the slits 10A and 10B are determined so that the ratio of the resin is 20% or more.

[0056] As shown in Figures 6 and 7(b), an ejector pin EJ is disposed in the space SP of the mold ML to remove the mold body 4 from the mold ML. The ejector pin EJ is movable in the vertical direction (see Figure 7(b)). By moving the ejector pin EJ upward (i.e., in the direction in which the ejector pin EJ is pressed against the mold body 4), the mold body 4 is pushed out of the mold ML. The mold body 4 is removed from the mold ML by being pushed out.

[0057] 1, 2, and 7(b), the molded body 4 has an ejector mark 5 formed in its upper thick portion 4a. The ejector mark 5 is formed by contact of the ejector pin EJ with the molded body 4. The ejector mark 5 is formed in the center of the upper thick portion 4a of the molded body 4.

[0058] In this embodiment, the resistor 1 is a surface mount resistor, and is mainly mounted by reflow soldering. If the ejector marks 5 were formed on the lower thick portion 4b of the molded body 4, air (or gas generated from the solder paste) would be trapped in the ejector marks 5 by the flux during reflow, and the resistor 1 would be mounted tilted by the air (gas). By forming the ejector marks 5 on the upper thick portion 4a of the molded body 4, the resistor 1 is stably mounted without being affected by the ejector marks 5.

[0059] When surface mounting the resistor 1, the upper thick portion 4a of the molded body 4 is sucked by a nozzle and mounted. In this embodiment, the inside of the ejector mark 5 is a flat surface. Therefore, even if the upper thick portion 4a of the molded body 4 is sucked by a nozzle, there is no risk of air leaking through the ejector mark 5, and stable mounting is possible.

[0060] Fig. 9(a) is a diagram showing how a long resistor material is cut, and Fig. 9(b) is a diagram showing the cut resistor. As shown in step S105 of Fig. 3 and Fig. 9(a), after forming the molded body 4 (see step S104), the resistor material is cut using a press die PM (press processing) so that a part of the resistor material is exposed from the molded body 4.

[0061] The press die PM moves from the lower thick portion 4b to the upper thick portion 4a of the molded body 4 (see the direction of the arrow in FIG. 9(a)), and the resistor material is cut in this direction. By cutting the resistor material, a sag surface 40A is formed on the lower surface 6f of the resistor 6, and a burr surface 40B is formed on the upper surface 6e (see FIG. 9(b)). The sag surface 40A is a smooth cut surface formed on the lower surface 6f. The burr surface 40B is a sharp cut surface formed on the upper surface 6e and protrudes from the upper surface 6e.

[0062] If the burr surface 40B were formed on the lower surface 6f of the resistor element 6, the burr surface 40B would protrude from the lower surface 6f. In this way, if the burr surface 40B is on the mounting surface side, there is a risk that the resistor 1 will be mounted at an angle due to the burr surface 40B. In this embodiment, the burr surface 40A is formed on the lower surface 6f of the resistor element 6. Even if the burr surface 40A is on the mounting surface side, it does not adversely affect the mountability of the resistor 1.

[0063] As shown in step S106 of FIG. 3 and in FIG. 6, after cutting the resistor material (see step S105), electrodes 3A and 3B are formed by metal plating (e.g., electrolytic barrel plating) that covers both ends of the resistor material (i.e., both ends 6a and 6b of the resistor 6) (see step S106).

[0064] More specifically, both ends 6a, 6b of the resistor 6 are copper-plated, and then the copper-plated ends 6a, 6b are tin-plated. Thus, each of the electrodes 3A, 3B has a copper-plated lower layer and a tin-plated upper layer. In one embodiment, a middle layer plated with another metal (e.g., nickel) may be provided between the copper-plated lower layer and the tin-plated upper layer.

[0065] In this embodiment, the thickness of the copper plating is 0.1 to 0.2 mm, and the thickness of the tin plating is 0.003 to 0.012 mm. If the thickness of the copper plating is thinner than 0.1 mm, the lower surface portion 3A-1 (and the lower surface portion 3B-1) of the electrode cannot be disposed at the same height as the lower surface of the molded body 4 (more specifically, the lower surface of the lower thick portion 4b) or lower than the lower surface of the molded body 4. If the thickness of the copper plating is thicker than 0.2 mm, the thickness of the product will be too thick and will not comply with the dimensional standard.

[0066] Fig. 10 is a diagram showing another embodiment of the resistor. In the embodiment shown in Fig. 10, the thickness D1 of the upper thick portion 4a is also greater than the thickness D2 of the lower thick portion 4b. Meanwhile, in this embodiment, the electrode 3A (and the electrode 3B) has not only the riding portion 3A-1a (and the riding portion 3B-1a) but also the riding portion 3A-2a (and the riding portion 3B-2a) formed on the upper surface portion 3A-2 (and the upper surface portion 3B-2) that rides on the molded body 4. With this configuration, it is possible to more reliably prevent the molded body 4 from peeling off from the resistor 6.

[0067] In one embodiment, the resistor 1 may include a lower surface portion 3A-1 (and a lower surface portion 3B-1) disposed at the same height as the lower surface of the molded body 4, and an electrode 3A (and an electrode 3B) having a raised portion 3A-1a (and a raised portion 3B-1a) formed on the lower surface portion 3A-1 (and a lower surface portion 3B-1). For example, the molded body 4 may have a step portion 50A or a chamfered portion 50B formed on its lower surface (see FIGS. 2(c) and 2(d)).

[0068] In one embodiment, the resistor 1 may include an upper surface portion 3A-2 (and an upper surface portion 3B-2) disposed at the same height as the upper surface of the molded body 4, and an electrode 3A (and an electrode 3B) having a riding portion 3A-2a (and a riding portion 3B-2a) formed on the upper surface portion 3A-1 (and an upper surface portion 3B-1). Although not shown, for example, the molded body 4 may have a step portion 50A or a chamfered portion 50B formed on its upper surface.

[0069] The above-described embodiments have been described for the purpose of enabling a person having ordinary skill in the art to practice the present invention. Various modifications of the above-described embodiments are naturally possible for a person skilled in the art, and the technical idea of ​​the present invention can be applied to other embodiments. Therefore, the present invention is not limited to the described embodiments, but is to be interpreted in the broadest scope according to the technical idea defined by the claims. [Explanation of symbols]

[0070] 1 metal plate resistor 3A,3B electrode 3A-1 Bottom part 3A-1a Riding section 3A-2 Top part 3A-2a Riding section 3B-1 Bottom part 3B-1a Riding section 3B-2 Top part 3B-2a Riding section 4 Molded body 4a Upper thick part 4b Lower thick part 5 Ejector marks 6 Resistors 6a, 6b both ends 6c,6d Side 6e Top 6f Bottom 8 Bobbin 10A First Slit 10B Second slit 11 Through hole 12 Positioning hole 20 Gate Remains 40A Droopy Face 40B Burr surface 50A stepped section 50B Chamfered part SP space GT Gate ML Mold PM Press Die

Claims

1. A plate-shaped resistor made of a metal material; A pair of electrodes provided at both ends of the resistor; A molded body covering the resistor, The resistor is a first slit formed on one electrode side and extending in a width direction from one side surface of the resistor; a second slit formed on the other electrode side, extending in a width direction from the other side surface of the resistor; a through hole disposed between the first slit and the second slit.

2. 2. The metal plate resistor according to claim 1, wherein the molded body has a gate mark formed on a side of the resistor element opposite to the side on which the first slit or the second slit is formed.

3. The resistor has a plate shape extending straight in its longitudinal direction, The mold body is An upper thick portion disposed above the resistor; a lower thick portion disposed below the resistor, 3. The metal plate resistor according to claim 1, wherein the upper thick portion has a thickness equal to or greater than that of the lower thick portion.

4. The pair of electrodes is formed by metal plating covering both ends of the resistor, The metal plate resistor according to claim 3 , wherein each of the pair of electrodes has a lower surface portion that is located at the same height as a lower surface of the molding body or lower than the lower surface of the molding body.

5. A step of preparing a long resistor material made of a metal material; forming a first slit extending from one side of the resistor material, a second slit extending from the other side of the resistor material, and a through hole disposed between the first slit and the second slit; forming a mold body that covers a portion of the resistor material and fills the first slit, the second slit, and the through hole; cutting the resistor material so that a portion of the resistor material is exposed from the mold body; and forming electrodes by metal plating to cover both ends of the resistor material exposed from the molded body.

Citation Information

Patent Citations

  • Bulk metal chip resistor

    JP1994020802A