Method for constructing front edge protective layer for windmill blade

By installing wind turbine blades horizontally with the leading edge facing downward and supporting them from multiple positions, the method addresses deflection and cost issues in thermal spraying, ensuring precise and cost-effective construction of protective layers on large blades.

JP2024149045AInactive Publication Date: 2024-10-18MITSUBISHI HEAVY IND LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023062707
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-07
Publication Date
2024-10-18
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The increasing size of wind turbine blades due to larger generators complicates thermal spraying, leading to deflection issues and increased manufacturing costs, particularly for blades over 100 m in length.

Method used

A method for constructing a leading edge protective layer on wind turbine blades involves installing the blade horizontally with the leading edge facing downward and supporting it from multiple positions, followed by thermal spraying to minimize deflection and improve positional accuracy.

Benefits of technology

This approach reduces deflection and manufacturing costs by ensuring precise thermal spraying without the need for large-scale equipment, even for large blades, maintaining high precision and strength at the leading edge.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024149045000001_ABST
    Figure 2024149045000001_ABST
Patent Text Reader

Abstract

To provide a method for constructing a front edge protective layer for a windmill blade that can reduce flexure of a windmill blade at the time of thermal spraying as much as possible and can support the windmill blade without increasing the size relatively.SOLUTION: A method for constructing a front edge protective layer for a windmill blade 5 in which a protective layer 30 is provided in a tip 12 in a blade length direction L1 of a windmill blade body 5a formed of FRP and on a side of a front edge 16 includes: a posture setting step of setting an installation posture of the windmill blade body 5a so that the blade length direction L1 becomes substantially horizontal and the side of the front edge 16 is oriented downward; a support step of supporting a plurality of positions in the blade length direction L1 of the side of the front edge 16 with a support base 32; and a thermal spraying step of performing thermal spraying to the side of the front edge 16.SELECTED DRAWING: Figure 5
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a method for applying a leading edge protective layer to a wind turbine blade provided with a protective layer. [Background technology]

[0002] As the wind turbine rotor rotates, the wind turbine blades collide with foreign objects in the air (e.g., raindrops, dust, etc.) and are eroded, causing erosion on the leading edge of the wind turbine blade. To protect the wind turbine blades from this erosion, it is known to form an erosion-resistant protective layer on the leading edge of the wind turbine blade (see Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent Publication No. 2022-175830 Summary of the Invention [Problem to be solved by the invention]

[0004] As wind turbine generators become larger with an increase in power generation, the blade length of the wind turbine increases, making handling during thermal spraying difficult. In particular, in large wind turbines of the 100m class, the deflection of the wind turbine blades when supported increases, which may reduce the positional accuracy of thermal spraying. In addition, as the wind turbine blades become larger, the device that supports them also becomes larger, which is a problem in that manufacturing costs increase.

[0005] The present disclosure has been made in consideration of the above circumstances, and aims to provide a method for applying a leading edge protective layer to a wind turbine blade, which can minimize deflection of the wind turbine blade during thermal spraying and can support the wind turbine blade without increasing its size. [Means for solving the problem]

[0006] A leading edge protective layer construction method for a wind turbine blade according to one embodiment of the present disclosure is a leading edge protective layer construction method for a wind turbine blade in which a protective layer is provided at the tip and leading edge in the blade span direction of a wind turbine blade body formed of FRP, and includes an attitude setting step of setting an installation attitude of the wind turbine blade body so that the blade span direction is approximately horizontal and the leading edge faces downward, a supporting step of supporting multiple positions of the leading edge in the blade span direction, and a thermal spraying step of thermally spraying the leading edge portion. Effect of the Invention

[0007] The deflection of the wind turbine blade during thermal spraying can be minimized. Also, the wind turbine blade can be supported without increasing its size. [Brief description of the drawings]

[0008] [Figure 1] 1 is a schematic configuration diagram showing a wind power generation device using a wind turbine blade according to an embodiment of the present disclosure. [Diagram 2] FIG. 2 is a plan view showing a wind turbine blade. [Diagram 3] FIG. 3 is a front view of the wind turbine blade of FIG. 2. [Figure 4] FIG. 4 is a cross-sectional view of the wind turbine blade shown in FIGS. 2 and 3. [Diagram 5] FIG. 11 is a front view showing an installed state of the wind turbine blade when a protective layer is formed. [Figure 6] FIG. 6 is a cross-sectional view of the support position of FIG. 5. [Figure 7] FIG. 4 is a partially enlarged front view showing the area in which a protective layer is formed on the tip of a wind turbine blade. [Figure 8] 5A to 5C are partially enlarged front views showing the order of forming protective layers. [Figure 9] FIG. 4 is a partially enlarged cross-sectional view showing the direction in which a protective layer is formed in the chord direction. [Figure 10] FIG. 2 is a cross-sectional view of an end portion in the chord direction of a protective layer formed on the blade surface of a wind turbine blade. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Hereinafter, an embodiment according to the present disclosure will be described with reference to the drawings. As shown in FIG. 1, the wind turbine generator 1 has a tower 3 erected on an installation surface B, a nacelle 6 installed at the upper end of the tower 3, and a rotor head 4 mounted on the nacelle 6 so as to be rotatable around a substantially horizontal axis.

[0010] A number of (e.g., three) wind turbine blades 5 are attached to the rotor head 4 in a radial manner around the rotation axis. This allows the force of the wind hitting the wind turbine blades 5 from the direction of the rotation axis of the rotor head 4 to be converted into power that rotates the rotor head 4 around the rotation axis. The obtained power is converted into electric power by a generator (not shown) and supplied to the outside.

[0011] As shown in Fig. 2, the wind turbine blade 5 includes a blade root portion 10 attached to the rotor head 4, a blade tip portion (tip portion) 12 located farthest from the rotor head 4, and an airfoil portion 14 extending between the blade root portion 10 and the blade tip portion 12. In Fig. 2, the blade span direction L1 is the horizontal direction.

[0012] The wind turbine blade 5 has a leading edge 16 and a trailing edge 18 from the blade root 10 to the blade tip 12. The outer shape of the wind turbine blade 5 is determined by a ventral side surface 20 which is a pressure surface (positive pressure surface) and a suction side surface 22 which is a negative pressure surface facing the ventral side surface 20. The wind turbine blade 5 is made of FRP (Fiber-Reinforced Plastic). Examples of FRP that can be used include carbon fiber reinforced plastic (CFRP) and glass fiber reinforced plastic (GFRP). The entire length of the wind turbine blade 5 from the blade root 10 to the blade tip 12 is in the 100 m class, for example, 80 m or more and 150 m or less. A 200 m class wind turbine blade may be used as the wind turbine blade 5 of this embodiment.

[0013] 3, the wind turbine blade 5 is provided with a pre-bend PB that is bent in advance on the blade tip 12 side. The amount of bending of the pre-bend PB is determined in advance assuming that the wind turbine blade 5 receives wind pressure during operation. Therefore, the pre-bend PB is bent so that the ventral side surface 20 that receives wind pressure is concave and the suction side surface 22 is convex.

[0014] As shown in Fig. 2, a protective layer 30 is formed on the wind turbine blade main body 5a in a predetermined region (leading edge portion) including the blade tip portion 12 and leading edge 16 of the wind turbine blade 5. The formation range of the protective layer 30 is indicated by a thick line in Fig. 2. The formation range of the protective layer 30 in the blade length direction L1 is 20 m to 40 m, preferably about 30 m, from the tip 12a of the blade tip portion 12. Note that the formation range of the protective layer 30 is not limited to this, and for example, in a region where the peripheral speed exceeds 90 m / s, it is set to a range of about 1 / 3 of the total length from the tip of the wind turbine blade 5. The protective layer 30 is made of a material having excellent wear resistance, such as a cermet or a Co (cobalt)-based alloy, etc. The protective layer 30 is formed, for example, by HVOF (High Velocity Oxy-Fuel) thermal spraying.

[0015] Figure 4 shows a cross section of a wind turbine blade 5. In the figure, the horizontal direction indicates the chord direction (cord direction) C1. If the total length of the wind turbine blade 5 is R, (a) is the cross section at a position of 0.9R, and (b) is the cross section at a position of 0.7R.

[0016] The chord length c in the cross section of Figure 4(a) is about 1 m. When the maximum blade thickness is t, the blade thickness ratio t / c is 18%. The chord length c in the cross section of Figure 4(b) is approximately 2 m, and the thickness ratio t / c is 25%.

[0017] 4, the protective layer 30 is formed from the ventral side surface 20 to the suction side surface 22 across the leading edge 16. The formation range of the protective layer 30 is determined in consideration of erosion of the wind turbine blade 5 by raindrops, etc.

[0018] Next, the process of forming the protective layer 30 will be described. As shown in Fig. 5, after the outer shape of the wind turbine blade main body 5a of the wind turbine blade 5 is formed, the wind turbine blade 5 is installed in a posture in which the blade length direction L1 is approximately horizontal and the leading edge 16 faces downward (posture setting process). That is, the wind turbine blade 5 is installed upright so that the blade chord direction C1 of the wind turbine blade main body 5a faces approximately vertically. At this time, the wind turbine blade 5 is supported from below by a plurality of supports 32 provided at predetermined intervals in the blade length direction L1 (support process).

[0019] 6 shows that the leading edge 16 side of the wind turbine blade 5 is supported by a plurality of support bases 32. Each support base 32 is provided on the as-formed installation surface BS. Note that the wind turbine blade 5 may be supported with the leading edge 16 side facing downward. For example, instead of the method of supporting the wind turbine blade 5 from below by the support bases 32 described above, the wind turbine blade 5 may be supported by holding and lifting the leading edge 16 facing downward by a hanging member such as a wire hung from above the wind turbine blade 5.

[0020] As shown in Figures 5 and 6, spraying is performed by the spraying section with the leading edge 16 facing downward. The spraying section accelerates the spraying material, which has been heated and melted or softened, in the form of droplets or particles by a carrier gas and sprays it onto the surface of the wind turbine blade body 5a.

[0021] 7 shows the sprayed area formed on the blade tip 12 of the wind turbine blade 5. As shown in the figure, a protective layer 30 is formed in a predetermined area (leading edge portion) on the leading edge 16 side of the wind turbine blade 5.

[0022] As shown in FIG. 8, the spraying is performed by reciprocating the sprayed part in the blade length direction L1 (the direction indicated by (1) in the figure) (first spraying step). This results in a multi-layered protective layer. The thickness is, for example, about 500 μm to 600 μm. The irradiation width of the sprayed part on the blade surface is, for example, about 10 mm.

[0023] After the above-mentioned first spraying process, the position of the sprayed portion is changed so that spraying is performed at an adjacent position adjacent to the chord direction C1 (the direction shown by (2) in the figure) (chord position changing process). Then, at this adjacent position, spraying is performed by reciprocating the sprayed portion in the chord direction C1 in the spanwise direction L1 (the direction shown by (1) in the figure) in the same manner as in the first spraying process (second spraying process). The first and second spraying processes are formed by scanning the sprayed portion so that it reciprocates in the spanwise direction L1. This is because the change in curvature of the blade surface is smaller in the spanwise direction L1 than in the chord direction C1.

[0024] As shown in Figure 9, the position change direction in the above-mentioned chord position changing process is a direction from one blade surface of the wind turbine blade 5 (e.g., the ventral side surface 20 or the suction side surface 22) through the leading edge 16 to the other blade surface (e.g., the suction side surface 22 or the ventral side surface 20), as indicated by the arrow in the figure.

[0025] 10 shows a cross section of an end 30a in the chord direction C1 of the protective layer 30 formed on the blade surface (ventral side surface 20 or suction side surface 22) of the wind turbine blade 5. As shown in the figure, the thickness of the end 30a of the protective layer 30 is formed to gradually decrease toward its edge (the right side in the figure). This is achieved by gradually shifting the sprayed portion in the chord direction C1 when spraying the end 30a of the protective layer 30 to laminate the protective layer 30 in the thickness direction (end spraying process).

[0026] The effects of the present embodiment described above are as follows. The wind turbine blade 5 has a greater strength at the leading edge 16 than at the trailing edge 18. Since multiple positions on the leading edge 16 side, which has greater strength, are supported from below, it is possible to minimize the deflection of the wind turbine blade body 5a. This improves the positional accuracy of the thermal spraying. Since thermal spraying is performed on the leading edge 16 side located below, thermal spraying can be performed by accessing the wind turbine blade body 5a from below. This eliminates the need for large-scale thermal spraying equipment, thereby reducing manufacturing costs.

[0027] Since the wind turbine blade main body 5a is installed vertically so that the chord direction C1 of the wind turbine blade main body 5a faces substantially vertically during thermal spraying, the section modulus of the wind turbine blade main body 5a becomes large and deflection can be minimized.

[0028] Even in the case of a large wind turbine blade 5 of 100 m class, which exceeds 80 m, the deflection of the wind turbine blade main body 5a is small, so the protective layer can be formed with high precision.

[0029] The wind turbine blade leading edge protective layer construction method described in each of the above-described embodiments can be understood, for example, as follows.

[0030] A leading edge protective layer construction method for a wind turbine blade according to a first aspect of the present disclosure is a leading edge protective layer construction method for a wind turbine blade (5) having a protective layer (30) provided at a tip portion (12) and a leading edge (16) in a blade length direction (L1) of a wind turbine blade body (5a) formed from FRP, and includes an attitude setting step of setting an installation attitude of the wind turbine blade body so that the blade length direction is approximately horizontal and the leading edge portion faces downward, a supporting step of supporting multiple positions of the leading edge portion in the blade length direction, and a thermal spraying step of thermally spraying the leading edge portion.

[0031] The leading edge of the wind turbine blade is thicker than the trailing edge, making it stronger. Since the leading edge, which has greater strength, is supported from below at multiple positions, it is possible to minimize the deflection of the wind turbine blade body. This improves the positional accuracy of the thermal spraying. Since thermal spraying is performed on the leading edge portion located below, the wind turbine blade body can be accessed from below for thermal spraying, which eliminates the need for large-scale thermal spraying equipment and reduces manufacturing costs.

[0032] In the wind turbine blade leading edge protective layer construction method according to a second aspect of the present disclosure, in the first aspect, the attitude setting step sets an installation attitude of the wind turbine blade main body so that a chord direction (C1) of the wind turbine blade main body is approximately vertical.

[0033] Since the wind turbine blade body is installed vertically so that the chord direction of the wind turbine blade body faces a substantially vertical direction, the section modulus of the wind turbine blade body becomes large and deflection can be minimized.

[0034] A wind turbine blade leading edge protective layer construction method according to a third aspect of the present disclosure is characterized in that in the first or second aspect, the dimension of the wind turbine blade body in the blade span direction is 80 m or more.

[0035] Even for large wind turbine blades exceeding 80m, the deflection of the wind turbine blade body is small, so the protective layer can be formed with high precision. [Explanation of symbols]

[0036] 1. Wind power generation equipment 3. Tower 4 Rotor Head 5 windmill blade 5a Wind turbine blade body 6. Nacelle 10 Wing root 12 Wing tip (tip) 12a Tip 14 Airfoil section 16 Leading Edge 18 Trailing edge 20 Ventral aspect 22 Dorsal aspect 30 protective layer 30a end 32 Support stand B Installation surface Installation surface when forming BS C1 chord direction L1 spanwise direction PB Pre-bend

Claims

1. A method for constructing a leading edge protective layer for a wind turbine blade, the method comprising the steps of: providing a protective layer at a leading edge portion of a wind turbine blade body formed of FRP in a blade span direction; an attitude setting step of setting an installation attitude of the wind turbine blade body so that the blade length direction is substantially horizontal and the leading edge portion faces downward; a supporting step of supporting the leading edge portion at a plurality of positions in the spanwise direction; a thermal spraying step of thermally spraying the leading edge portion; A method for constructing a leading edge protective layer for a wind turbine blade having the above structure.

2. The wind turbine blade leading edge protective layer construction method according to claim 1 , wherein the attitude setting step sets an installation attitude of the wind turbine blade main body so that a chord direction of the wind turbine blade main body is substantially vertical.

3. 3. The wind turbine blade leading edge protective layer construction method according to claim 1 or 2, wherein a dimension of the wind turbine blade body in the blade span direction is 80 m or more.

Citation Information

Patent Citations

  • Wind turbine rotational blade and wind turbine generating apparatus having the same

    JP2014148984A

  • Wind turbine blade and method for manufacturing the same

    JP2020084217A

  • Blade tip clamp arrangement

    US20150337799A1

  • Wind turbine blade repair method

    US20160046088A1

  • Blade structure and manufacturing method of blade structure

    JP2022175830A