Paper container
A laminated structure with a deformable greaseproof paper layer and resin layers in paper containers addresses oil leakage issues by filling joint gaps, ensuring the container's integrity and appearance during microwave heating.
Patent Information
- Application Number
- JP2023062958
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-07
- Publication Date
- 2024-10-18
AI Technical Summary
Paper containers used for storing foods with a large amount of oil face issues with oil leakage and seepage, particularly at the joints, due to pinholes formed during thermal welding and heating in microwave ovens, which affect the aesthetic appearance and commercial value.
A laminated structure for paper containers comprising a base paper layer, a first resin layer, a greaseproof paper layer, and a second resin layer, where the greaseproof paper layer is thinner and deformable, allowing the molten resin to fill gaps at the joint, thereby preventing oil seepage.
The laminated structure effectively suppresses oil seepage at the joint between the body and bottom of the paper container, maintaining the integrity and appearance of the container even when heated in a microwave oven.
Smart Images

Figure 2024149218000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a paper container that is required to be oil-resistant. [Background technology]
[0002] In recent years, from the perspective of environmental conservation, there has been discussion about replacing plastic containers with paper containers. However, the paper containers must be guaranteed to have the same performance as the plastic containers.
[0003] Paper containers for storing foodstuffs that contain a large amount of oil (such as pasta fried in sauce) are required to be oil-resistant (Patent Document 1 and Patent Document 2).
[0004] In particular, food ingredients are now often heated in microwave ovens, making oil resistance more important.
[0005] The use of greaseproof paper can solve some of the problems associated with foodstuffs that contain large amounts of oil. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] JP 2006-056127 A [Patent Document 2] JP 2009-030192 A Summary of the Invention [Problem to be solved by the invention]
[0007] An example of a paper container has a circular bottom and a body part that stands upright from the bottom in an inverted truncated cone shape or a cylindrical shape. If necessary, the body part may have a flange or a lid on the upper edge.
[0008] The sector-shaped blank is rolled, one end is placed underneath and the other end is placed on top of it, and the ends are overlapped and joined (eg, heat welded) to form a body portion.
[0009] The periphery of the bottom is squeezed and the bottom is fitted into the body from below to form a paper container.
[0010] Pinholes may occur when the blank is deformed during container molding, and also when the joints are thermally welded.
[0011] When heating in a microwave oven, the temperature inside the container can exceed 100°C, which may cause pinholes to form due to moisture foaming or softening of the coating layer.
[0012] These pinholes cause oil bleeding. The inventors are currently investigating a method for solving this problem.
[0013] Similarly, oil seepage is generally likely to occur at the joint of the body and at the joint between the body and the base. Oil seepage significantly mars the aesthetic appearance of the container, and as a result, reduces the commercial value of the foodstuffs.
[0014] The present invention is intended to solve the above-mentioned problems, and has an object to provide a technology for suppressing seepage of contents, particularly at the joint between the body and bottom of a paper container. [Means for solving the problem]
[0015] The paper container of the present invention, which achieves the above object, includes a bottom and a body part standing upright from the bottom. The bottom has a laminated structure. The laminated structure has a base paper layer, a first resin layer provided adjacent to the base paper layer, an grease-resistant paper layer provided adjacent to the first resin layer, and a second resin layer provided adjacent to the grease-resistant paper layer.
[0016] As the first resin layer melts and flows, the grease-resistant paper layer deforms. As the grease-resistant paper layer deforms, the molten second resin layer flows to fill in the gap that occurs at the joint between the body and the base. This prevents the contents from seeping out.
[0017] In the above invention, the greaseproof paper layer is preferably thinner than the base paper layer.
[0018] This makes the grease-resistant paper layer more susceptible to deformation.
[0019] In the above invention, the grease-resistant paper layer preferably has a basis weight of 20 to 60 g / m2.
[0020] The basis weight of 20 to 60 g / m2 is thinner than commonly used greaseproof paper, which makes the greaseproof paper layer more susceptible to deformation.
[0021] In the above invention, preferably, at least one of the first resin layer and the second resin layer has an MFR of 3 or more.
[0022] This causes the molten resin to flow.
[0023] In the above invention, the base paper layer is preferably a general paper.
[0024] Regular paper is not oil-resistant and is inexpensive, which helps to reduce overall manufacturing costs.
[0025] In the above invention, the oil-resistant paper layer preferably contains an oil-resistant agent made of a C6 short-chain fluorine-based compound.
[0026] This provides the oil-resistant paper layer with oil resistance. Effect of the Invention
[0027] According to the paper container of the present invention, it is possible to prevent the contents from bleeding out at the joint between the body and the bottom, which is particularly suitable when the contents contain oil. [Brief description of the drawings]
[0028] [Figure 1] General structure of a typical paper container (overall) [Diagram 2] Schematic structure of a typical paper container (bottom) [Diagram 3] Cross-sectional view of the joint between the body and bottom of a typical paper container [Figure 4] Detailed composition of the paper used on the bottom (comparison example and preferred example) [Diagram 5] Detailed structure of the joint between the body and the bottom (comparison example and preferred example) [Figure 6] Operation at the joint between the body and the bottom (Comparative example and preferred example) [Figure 7] Simple example of grease-resistant paper DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0029] ~ Knowledge gained in the process of arriving at this invention ~ Fig. 1 shows a schematic configuration of a typical paper container. The paper container includes a bottom 10 and a body 20 standing upright from the bottom 10. A joint 11 is formed between the bottom 10 and the body 20, and a joint 21 is formed between the body portions 20 themselves.
[0030] The body 20 of the paper container is formed from a sector-shaped blank. The blank is rolled up, one end 22 is placed on the bottom and the other end 23 is placed on the top so that the joining surfaces face each other, and both ends 22, 23 are overlapped and joined at a predetermined joining width. In this way, the body 20 of the paper container is formed.
[0031] Fig. 2 shows the schematic structure of a typical bottom of a paper container. The bottom 10 of the paper container is circular. The periphery of the bottom body 12 is squeezed to form a joining surface 13. At that time, a plurality of wrinkles 14 are generated in the circumferential direction on the joining surface 13.
[0032] The paper container is formed by fitting the bottom 10 from below into the body 20. The bottom joint surface 13 comes into contact with the body lower part 24, and the body lower part 24 is folded back so that the bottom joint surface 13 is sandwiched between the folded back part 25.
[0033] The bottom portion 10 and the body portion 20 are joined together by pressing the joint portion 11 with a roller, thereby forming a paper container.
[0034] By the way, from experience, oil seepage is likely to occur at the joint 11 and the joint 21. Furthermore, oil seepage is particularly likely to occur at the joint 16 where the joint 11 and the joint 21 overlap.
[0035] Fig. 3 is a cross-sectional view of the location where joint 11 and joint 21 overlap. While the right-hand view of Fig. 1 is a vertical cross-section, Fig. 3 is a horizontal cross-section. Fig. 3 is a processed photograph of the cross-section.
[0036] At the joint 16, one end 26, 27 and the other end 28, 29 overlap and are then folded back to form folded back portions 27, 29, with the bottom joint surface portion 13 being sandwiched between the one end 26, 27 and the other end 28, 29.
[0037] The inventors produced a number of sample products, stored pasta fried in sauce in them, heated them in a microwave oven, and observed whether oil seeped through the joint 16. They noticed that there were differences in whether oil seeped through or not.
[0038] Further, upon further observation, it was noticed that oil seepage was prominent when the wrinkles 14 and the joints 16 overlapped. On the other hand, when the wrinkles 14 and the joints 16 did not overlap, oil seepage was rare, and even if it did occur, it was only a small amount.
[0039] ~Considerations in Comparative Examples~ Figures 4 to 6 show a comparison between the comparative example and the preferred example of the present application. Figure 4 is a detailed configuration diagram of papers 12, 13 used in bottom portion 10. Figure 5 is a detailed configuration diagram of joint portion 16. Figure 6 is an explanatory diagram of the operation when forming joint portion 16. In order to simplify the drawings, the illustration of folded portions 27, 29 is omitted in Figure 6.
[0040] In the comparative example, a paper is used in which a polyethylene resin adhesive layer 34 (equivalent to a thickness of 40 μm) is laminated to an oil-resistant paper layer 33 (manufactured by Nippon Paper Crecia Co., Ltd.) having a basis weight of 300 g / m2 (equivalent to a thickness of 500 μm). More specifically, the polyethylene resin adhesive layer 34 is a laminate of a high melting point layer (equivalent to a thickness of 20 μm) and a low melting point layer (equivalent to a thickness of 20 μm).
[0041] A step corresponding to the paper thickness occurs between the end faces of the drum wrapper 26 and the drum wrapper 28. Furthermore, the squeeze wrinkles 14 are located near the step.
[0042] In action 1, roller compression begins from the right side of the figure. The adhesive layer of the body paper 26 and the adhesive layer of the bottom paper 13 are bonded. In action 2, molten resin flows into the vicinity of the step as the compression proceeds. When the roller passes near the end face of the body paper 28, the thickness of the layer makes it highly rigid, and a large reaction force acts. In action 3, the body paper 28 and bottom paper 13 are bonded. Molten resin flows into the vicinity of the step.
[0043] The grease-resistant paper layer 33 of the comparative example is relatively thick and its shape does not change much when the resin melts. The shape of the wrinkles 14 is almost maintained. Resin accumulates in the space formed by the wrinkles 14. As a result, the resin cannot fill the step. Unbonded areas occur near the end faces of the body paper 28.
[0044] The unjoined portion extends downward from the periphery of the bottom body 12 along the end face of the body paper 28 to the lower end of the joining surface portion 13, and forms an intrusion path in the unjoined portion. Oil intrudes from the intrusion path (outward path) and reaches the lowermost end (turn-back point) of the body paper 26.
[0045] Similarly, an intrusion path (return path) is formed along the end surface of the body wrap 29. Oil seeps out from the back surface of the bottom body 12 through the intrusion path (return path).
[0046] In addition, oil remains liquid even when heated to over 100℃ in a microwave oven, so it easily penetrates into the penetration path. As a result, oil seepage is likely to occur.
[0047] Since the oil seepage is caused by the formation of an infiltration path, it is difficult to suppress the oil seepage even if the oil-resistant paper layer 33 is improved.
[0048] ~Configuration and operation of the preferred embodiment of the present application~ In a preferred embodiment, a paper is used in which a polyethylene resin lamination layer 32 (equivalent to a thickness of 20 μm) is laminated onto a base paper layer 31 (manufactured by Nippon Paper Industries Co., Ltd.) having a basis weight of 220 g / m2 (equivalent to a thickness of 350 μm), an oil-resistant paper layer 33 (manufactured by Tenma Tokushu Paper Co., Ltd.) having a basis weight of 40 g / m2 (equivalent to a thickness of 65 μm), and a polyethylene resin adhesive layer 34 (equivalent to a thickness of 40 μm). More specifically, the polyethylene resin adhesive layer 34 is a laminate of a high melting point layer (equivalent to a thickness of 20 μm) and a low melting point layer (equivalent to a thickness of 20 μm).
[0049] A step corresponding to the paper thickness occurs between the end faces of the drum wrapper 26 and the drum wrapper 28. Furthermore, the squeeze wrinkles 14 are located near the step.
[0050] In action 1, the roller starts pressing from the right side in the figure. The adhesive layer of the body paper 26 and the adhesive layer of the bottom paper 13 are bonded. In action 2, the melted resin flows into the area near the step as the pressure is applied. When the roller passes near the end face of the body paper 28, the thickness of the layer makes the material highly rigid, and a large reaction force acts.
[0051] In operation 3, the body paper 28 and the bottom paper 13 are bonded together. The molten polyethylene resin lamination layer 32 flows into the area near the step.
[0052] Meanwhile, the base paper layer 31 is relatively thick and has rigidity, while the preferred example grease-resistant paper layer 33 is relatively thin and its shape is easily changed as the resin melts and flows. As a result, when pressed, the base paper layer 31 maintains a shape close to the wrinkles 14, while the wrinkles of the grease-resistant paper layer 33 are smoothed out.
[0053] The polyethylene-based resin adhesive layer 34 melts as the grease-resistant paper layer 33 deforms, and moves to fill in the steps. The occurrence of unbonded areas near the end faces of the body paper 28 is suppressed.
[0054] As a result, oil seepage caused by the formation of an infiltration path is suppressed.
[0055] ~Effects Summary~ As explained in the comparison between the comparative example and the preferred example of the present application, oil seepage occurs on the rear surface of the bottom body 12 in the comparative example of the present application, whereas oil seepage on the rear surface of the bottom body 12 is suppressed in the preferred example of the present application.
[0056] In fact, when pasta fried in sauce was placed in a container and heated in a microwave (500W for 4 minutes), no oil seepage occurred in any of the test cases.
[0057] On the other hand, the oil-resistant paper layer 33 of the preferred example of the present application is characterized by being thinner than the oil-resistant paper layer 33 of the comparative example of the present application. As a result, it is necessary to consider oil seepage in the lamination direction, particularly when the oil-resistant paper layer 33 of the preferred example of the present application is torn.
[0058] In contrast, the polyethylene resin lamination layer 32 and the polyethylene resin adhesive layer 34 act as double reinforcement, so that even if the preferred example oil-resistant paper layer 33 of the present application is torn, oil seepage in the stacking direction (oil seepage into the base paper layer 31) can be suppressed.
[0059] As a result, ordinary paper (or coated paper) can be used for the base paper layer 31. In other words, oil-resistant processing is not required. Ordinary paper is cheaper than oil-resistant paper, and manufacturing costs can be reduced.
[0060] ~Detailed consideration~ The oil-resistant paper layer 33 of the preferred embodiment of the present invention is characterized by its thinness. In the above example, the basis weight is 40 g / m2. It is preferable that the basis weight is 20 to 60 g / m2. If the basis weight is less than 20 g / m2, the oil resistance function may not be maintained or the layer may be torn. If the basis weight is more than 60 g / m2, the shape deformation action due to the resin flow becomes insufficient.
[0061] The basis weight of 20 to 60 g / m2 roughly corresponds to a thickness of 30 to 100 μm. The density is 0.5 to 0.7 g / m3.
[0062] That is, the preferred grease-resistant paper layer 33 of the present application has appropriate tensile strength (based on JISP 8113) and appropriate tensile elongation (based on JISP 8113). The tensile strength is preferably 1.0 kN / m or more in both MD and CD. It is more preferably 3.0 kN / m or more in MD and 1.5 kN / m or more in CD. The tensile elongation is preferably 2.0% or more in both MD and CD.
[0063] Figure 7 shows a simple example of the suitability of the grease-resistant paper layer 33 of the present invention. The grease-resistant paper layer 33 is sandwiched between two cylindrical bodies, one above the other, and fixed in place. A rod of a certain weight is dropped from a certain height, and the displacement of the grease-resistant paper layer 33 is measured. If the displacement falls within a certain range, it is judged to be suitable. In the example shown in the figure, grease-resistant paper that encompasses the cross section of the cylinder is used.
[0064] Alternatively, a load cell may be provided at the upper end of the rod to measure the load required to press the grease-resistant paper layer 33 a specified amount (e.g., 5 mm). For example, when the basis weight was 30 g / m2, the average load for the five samples was 0.15 N. When the basis weight was 40 g / m2, the average load for the five samples was 0.19 N. When the basis weight was 50 g / m2, the average load for the five samples was 0.19 N.
[0065] In the case of the reference example with a basis weight of 170 g / m2, the average load of the five samples was 0.78 N, which is clearly different from the preferred range of the present application. In this way, the suitability of the grease-resistant paper layer 33 of the preferred example of the present application can be easily examined.
[0066] Therefore, a suitable grease-resistant paper layer 33 may be specified by an index other than basis weight.
[0067] The oil-resistant paper layer 33 preferably contains 0.3 wt % or more of an oil-resistant agent made of a C6-based short-chain fluorine-based compound, and has a kit value of 5 or more.
[0068] The polyethylene resin laminating layer 32 and the polyethylene resin adhesive layer 34 preferably have an MFR (Melt Flow Rate) of 3 to 20 cm3 / 10 min. If the MFR is less than 3, the oil-resistant paper layer 33 is less likely to deform due to the resin flow. As a result, the effects of the present invention cannot be fully obtained. If the MFR is more than 20, the film formation may become unstable.
[0069] The polyethylene resin laminating layer 32 and the polyethylene resin adhesive layer 34 have a density of 0.97 g / cm3 or less. [Explanation of symbols]
[0070] 10. Bottom of paper container 11 Joint between body and bottom 12 Bottom body 13 Joint surface part 14 Wrinkles 16: Joint where joint 11 and joint 21 overlap 20 Paper container body 21 Joint between the torsos 22 One end of the body 23 Other end of body 24 Lower torso 25 Folding part 26 One end 27 One end (folded part) 28 Other end 29 Other end (folded part) 31 Base paper layer 32 Polyethylene resin lamination layer 33 Grease-resistant paper layer 34 Polyethylene resin adhesive layer
Claims
1. A paper container including a bottom and a body part standing upright from the bottom, The bottom portion is made of a laminated structure, The laminate structure is A base paper layer; A first resin layer provided adjacent to the base paper layer; An oil-resistant paper layer provided adjacent to the first resin layer; A second resin layer provided adjacent to the oil-resistant paper layer. have A paper container characterized by:
2. The greaseproof paper layer is thinner than the base paper layer. A paper container characterized by:
3. The oil-resistant paper layer has a basis weight of 20 to 60 g / m2.
2. The paper container according to claim 1.
4. At least one of the first resin layer and the second resin layer has an MFR of 3 or more.
2. The paper container according to claim 1.
5. The base paper layer is a general paper 2. The paper container according to claim 1.
6. The oil-resistant paper layer contains an oil-resistant agent made of a C6-based short-chain fluorine-based compound.
2. The paper container according to claim 1.
Citation Information
Patent Citations
Packaging material for desiccant
JP2000334894A
Laminate material for paper-made container, and paper-made container using the same
JP2004352293A
Barrier cup
JP2006232363A
Water and oil resistant paper and method for producing the same
JP2009120996A
Oil resistant paper and packaging bag
JP2021004422A