Dye-sensitized solar cell

By setting the cell gap to 10-15 μm with spacers in the sealing material, the dye-sensitized solar cells achieve enhanced reliability and durability by preventing electrolyte leakage and optimizing power generation.

JP2024151863APending Publication Date: 2024-10-25TOPPAN HOLDINGS INC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023065613
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-13
Publication Date
2024-10-25

AI Technical Summary

Technical Problem

Dye-sensitized solar cells face challenges in achieving high reliability due to potential electrolyte leakage through the sealing material, which can be exacerbated by changes in cell size and environmental conditions.

Method used

The cell gap between the first and second substrates is defined to be between 10 μm to 15 μm, with a sealing material that includes spacers to maintain a stable gap and prevent electrolyte leakage, while optimizing power generation area.

Benefits of technology

This configuration enhances the reliability and durability of the solar cells by reducing liquid leakage and maintaining a stable cell gap, thereby improving power generation performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024151863000001_ABST
    Figure 2024151863000001_ABST
Patent Text Reader

Abstract

To provide a highly reliable dye-sensitized solar cell.SOLUTION: A dye-sensitized solar cell comprised: an electrode formed on a first substrate; an electron transport layer formed on the electrode; a light absorbing layer formed on the electron transport layer and including an electron collector and a dye; a counter electrode formed on a second substrate disposed opposite the first substrate; a catalyst layer formed on the counter electrode; electrolyte filled in between the light absorbing layer and the catalyst layer; and a sealing material which bonds the first substrate and the second substrate while sealing the electrolyte. The distance between the first substrate and the second substrate is 10 μm to 15 μm.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to dye-sensitized solar cells. [Background technology]

[0002] Solar cells are expected to be used as power sources and energy harvesting elements for IoT (Internet of Things) devices. Solar cells are broadly classified into silicon-based solar cells, compound-based solar cells, and organic solar cells. Among organic solar cells, dye-sensitized solar cells (DSCs) are known. Dye-sensitized solar cells generate electricity through an oxidation-reduction reaction using a dye for absorbing light and an electrolyte. The electrolyte used in dye-sensitized solar cells includes solid-type electrolytes and liquid-type electrolytes. The liquid-type electrolyte may be injected, for example, using the ODF (One Drop Filling) method. The dye-sensitized solar cell cell containing the injected electrolyte is sealed with a sealant. In recent years, high reliability is required for dye-sensitized solar cells. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2016-018897 A Summary of the Invention [Problem to be solved by the invention]

[0004] An object of the present disclosure is to provide a dye-sensitized solar cell having high reliability. [Means for solving the problem]

[0005] A dye-sensitized solar cell according to one embodiment includes an electrode formed on a first substrate, an electron transport layer formed on the electrode, a light absorbing layer formed on the electron transport layer and containing an electron collector and a dye, a counter electrode formed on a second substrate disposed opposite the first substrate, a catalyst layer formed on the counter electrode, an electrolyte filled between the light absorbing layer and the catalyst layer, and a sealant for bonding the first substrate and the second substrate together while sealing the electrolyte. The distance between the first substrate and the second substrate is 10 μm to 15 μm. Effect of the Invention

[0006] According to the present disclosure, it is possible to provide a highly reliable dye-sensitized solar cell. [Brief description of the drawings]

[0007] [Figure 1] FIG. 1 is a cross-sectional view showing an example of the configuration of a dye-sensitized solar cell according to an embodiment. [Diagram 2] FIG. 2 is a diagram for explaining the power generation principle of a dye-sensitized solar cell. [Diagram 3] FIG. 3 shows the correlation between adhesive layer thickness and adhesive strength. [Figure 4A] FIG. 4A shows the results of an experiment measuring the peel strength of dye-sensitized solar cells fabricated with cell gaps of 10 μm, 15 μm, and 20 μm and various seal widths of the sealing material. [Figure 4B] FIG. 4B is a bar graph showing a comparison of the peel strength for each cell gap. [Diagram 5] FIG. 5 is a graph showing comparative results of 85° C. / 85% RH reliability tests for dye-sensitized solar cells with a cell gap of 20 μm, dye-sensitized solar cells with a cell gap of 15 μm, and dye-sensitized solar cells with a cell gap of 10 μm. [Figure 6A] FIG. 6A is a diagram showing a manufacturing process of a dye-sensitized solar cell. [Figure 6B] FIG. 6B is a diagram showing the manufacturing process of a dye-sensitized solar cell. [Figure 6C]FIG. 6C is a diagram showing a manufacturing process of a dye-sensitized solar cell. [Figure 6D] FIG. 6D is a diagram showing the manufacturing process of a dye-sensitized solar cell. [Figure 6E] FIG. 6E is a diagram showing a manufacturing process of a dye-sensitized solar cell. [Figure 7] FIG. 7 is a diagram showing a modified example in which a columnar spacer is used as the spacer. [Figure 8] FIG. 8 is a diagram showing a modified example in which a columnar spacer is used as the spacer. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0008] Hereinafter, an embodiment will be described with reference to the drawings. Fig. 1 is a cross-sectional view showing an example of the configuration of a dye-sensitized solar cell according to an embodiment.

[0009] The dye-sensitized solar cell 1 according to one embodiment may include a plurality of dye-sensitized solar cell units. In Fig. 1, two units are shown. The number of units is not limited to two.

[0010] As shown in FIG. 1, each unit is formed between a first substrate 11 and a second substrate 12. The first substrate 11 is a transparent substrate such as a glass substrate. The first substrate 11 is used as an anode substrate. The second substrate 12 is disposed so as to face the first substrate 11. The second substrate 12 is a transparent substrate such as a glass substrate like the first substrate 11. The second substrate 12 is used as a cathode substrate.

[0011] An electrode 13 is formed at the position of each unit on the first substrate 11. The electrodes 13 are spaced apart such that there is no influence of leakage current between adjacent electrodes. The electrodes 13 are formed of a transparent conductive oxide (TCO) film such as indium tin oxide (ITO) or fluorine doped tin oxide (FTO). The electrodes 13 are used as anode electrodes. Although not shown in FIG. 1, the electrodes 13 of each unit are led out to the outside of the dye-sensitized solar cell 1. Terminals are formed on the led out electrodes 13. Wiring is led out from the terminals. This wiring is connected to one end of a load not shown.

[0012] A counter electrode 14 is formed at the position of each unit on the second substrate 12. The counter electrodes 14 are spaced apart such that there is no influence of, for example, leakage current between adjacent electrodes. Like the electrode 13, the counter electrode 14 is formed of a transparent conductive oxide film (TCO) such as indium tin oxide (ITO) or fluorine-doped tin oxide (FTO). The counter electrode 14 is used as a cathode electrode. Although not shown in FIG. 1, the counter electrode 14 of each unit is led out to the outside of the dye-sensitized solar cell 1. A terminal is formed on the led out counter electrode 14. Wiring is led out from the terminal. This wiring is connected to one end of a load (not shown).

[0013] An electron transport layer 15 is formed on each electrode 13. The electron transport layer 15 is made of titanium oxide (TiO x The electron transport layer 15 is made of a metal oxide film such as TCO, which has a higher resistance than metal. The electron transport layer 15 can be provided to suppress loss due to the electrode 13 made of TCO, which has a higher resistance than metal. In addition, the formation of the electron transport layer 15 improves the adhesion of the light absorbing layer 16, which is further formed on the electron transport layer 15.

[0014] A light absorbing layer 16 is formed on each of the electron transport layers 15. The light absorbing layer 16 is a layer formed by adsorbing a dye to an electron collector. The electron collector is, for example, a porous oxide semiconductor, such as titanium oxide (TiO 2) is an aggregate. The dye is, for example, a ruthenium (Ru) dye (RU) (such as N719 dye). The electron collector is not limited to titanium oxide, but may be, for example, zinc oxide, tin oxide, tungsten oxide, niobium oxide, indium oxide, or a complex thereof. The dye is not limited to N719 dye. For example, N3 dye and BlackDye may be used as ruthenium-based dyes, and D149, xanthene, PVK, merocyanine, oxazine, or the like may be used as pure organic dyes.

[0015] A catalyst layer 17 is formed on each of the counter electrodes 14. The catalyst layer 17 is, for example, a platinum layer, a carbon layer, or the like.

[0016] An electrolyte solution 18 is filled between the light absorbing layer 16 and the catalyst layer 17. As a solvent for the electrolyte solution 18, for example, acetonitrile, methoxyacetonitrile, ethylene carbonate, etc. can be used. As a solute for the electrolyte solution 18, for example, iodine (I 2 ), 1,2-dimethyl-3-n-propylimidazolium iodide (DMPImI), lithium iodide (LiI), 4-tert-butylpyridine (TBP), etc. can be used. As shown in FIG. 1, the electrolyte 18 is partitioned by a sealant 19. The sealant 19 bonds the first substrate 11 and the second substrate 12 together and prevents the electrolyte 18 from leaking out to the outside. The sealant 19 can be a resin with excellent solvent resistance, such as an acrylic resin or an olefin resin. Spacers 19a are mixed into the sealant 19. The spacers 19a are mixed in order to set the cell gap of the dye-sensitized solar cell 1, that is, the distance between the first substrate 11 and the second substrate 12 in the example of FIG. 1, to a desired value, which will be described later. The spacers 19a can be granular spacers such as resin beads. The spacers 19a can be, for example, silica particles. The spacers 19a can also be conductive particles. If the spacers 19a are made of conductive particles, a plurality of dye-sensitized solar cell units 1 can be connected in series or in parallel via the sealing material 19.

[0017] FIG. 2 is a diagram for explaining the power generation principle of the dye-sensitized solar cell 1. In the following example, the electron collector is titanium oxide (TiO 2 ), the dye is a ruthenium (Ru) dye, and the electrolyte 18 is an iodine (I) electrolyte.

[0018] First, when light is incident on the dye-sensitized solar cell 1, the light is absorbed by the dye 16a formed on the substrate. The dye 16a is excited by absorbing the light. The reaction formula is, for example, shown in the following formula (1). Ru → Ru + +e - (1) Electrons emitted from the excited dye 16a (e - ) is, for example, a porous titanium oxide (TiO 2 The electrons injected into the electron collector 16b move to the electrode 13, which is an anode electrode.

[0019] On the other hand, electrons (e - The dye 16a that has lost the ion exchange function reacts with, for example, iodide ions (I - ) in electrolyte 18. - ) is an electron (e - ) to dye 16a, triiodide ions (I 3 - The reaction formula is shown in the following formulas (2) and (3). Ru+e - →Ru (2) 3I - →I 3 - +2e - (3) The triiodide ion (I 3 - ) is transported from the cathode electrode 14 to the counter electrode 14 by electrons (e -At this time, a potential difference is generated between the counter electrode 14 and the electrode 13. If a load is connected between the counter electrode 14 and the electrode 13, the electrons that have moved to the electrode 13 will move through the load to the counter electrode 14. Then, the electrons that have reached the counter electrode 14 will be converted into triiodide ions (I 3 - ) is absorbed by the iodide ion (I 3 - ) is the iodide ion (I - ) The reaction formula is shown, for example, in the following formula (4). I 3 - +2e - →3I - (4) The above-mentioned redox reaction is repeated to generate electricity in the dye-sensitized solar cell 1. For such a redox reaction to occur, the energy level of the dye 16a in the excited state must be higher than the energy level of the electron collector 16b, and the energy level of the dye 16a in the ground state must be lower than the energy level of the electrolyte 18.

[0020] Here, depending on the usage environment of the dye-sensitized solar cell 1 or over a long period of use, leakage of the electrolyte solution 18 from the sealing material 19 of the dye-sensitized solar cell 1 may occur. The leakage occurs, for example, when the adhesion between the first substrate 11 or the second substrate 12 and the sealing material 19 decreases, causing a part of the sealing material 19 to peel off.

[0021] To prevent leakage, the seal width of the sealant 19 (the width in the direction perpendicular to the gap direction of the sealant 19, w in FIG. 1) s ) is effective. On the other hand, when considering reducing the cell size of the dye-sensitized solar cell 1, increasing the seal width of the sealant 19 leads to a decrease in the effective area for power generation of the dye-sensitized solar cell 1. Therefore, it is required to prevent liquid leakage while making the seal width of the sealant 19 as short as possible.

[0022] Here, there is a correlation between the thickness of the adhesive layer and the adhesive strength as shown in FIG. 3. Here, curve A in FIG. 3 is a curve that represents the relationship between the thickness of the adhesive layer and the adhesive strength when shear or tensile stress acts predominantly on the adhesive layer. Curve B in FIG. 3 is a curve that represents the relationship between the thickness of the adhesive layer and the adhesive strength when peel or impact stress acts predominantly on the adhesive layer. As shown by curve A, when shear or tensile stress is predominant, the peak of the adhesive strength tends to be on the side where the adhesive layer is thinner. On the other hand, as shown by curve B, when peel or impact stress is predominant, the peak of the adhesive strength tends to be on the side where the adhesive layer is thicker.

[0023] In the embodiment, a thickness of the adhesive layer that is resistant to both shear and peeling, i.e., a cell gap (SG in FIG. 1) corresponding to the distance between the first substrate 11 and the second substrate 12, is specified, and the dye-sensitized solar cell 1 is manufactured with such a cell gap. Here, in consideration of the power generation capacity of the dye-sensitized solar cell 1, the porous oxide semiconductor, for example, TiO 2 The particle size is generally about 10-20 nm. In consideration of the power generation capacity of the dye-sensitized solar cell 1, the film thickness of the light absorbing layer 16 needs to be about 10 μm, taking into account that the surface roughness (roughness factor (RF)) of the light absorbing layer 16 is about 1000. Therefore, it is desirable to specify the cell gap with a lower limit of 10 μm.

[0024] Fig. 4A shows the results of an experiment measuring the peel strength of dye-sensitized solar cells created by varying the seal width of the sealing material with a cell gap of 10 μm, 15 μm, and 20 μm. The dye-sensitized solar cell 1 used in the experiment is an empty cell that is not filled with electrolyte 18. Straight lines A, B, and C in Fig. 4A are approximate straight lines that represent the relationship between the seal width and the peel strength when the seal cell gap is 10 μm, 15 μm, and 20 μm, respectively.

[0025] As shown in Fig. 4A, the peel strength increases as the seal width of the sealant 19 increases. This is as described above. Furthermore, as shown in Fig. 4A, for the same seal width, the peel strength increases in the order of 10 μm, 15 μm, and 20 μm.

[0026] Figure 4B is a bar graph comparing peel strength for each cell gap. In Figure 4B, peel strength results for seal widths of 1.0 mm, 1.5 mm, and 2.0 mm are extracted from the approximation curves A, B, and C in Figure 4A, respectively. The peel strength ratio on the vertical axis of the bar graph in Figure 4B represents the ratio of each peel strength when the peel strength for a seal width of 1.0 mm and a cell gap of 20 μm is taken as 1. It can also be seen from Figure 4B that for the same seal width, the peel strength increases as the cell gap narrows. In particular, this tendency becomes stronger as the seal width increases.

[0027] FIG. 5 shows the results of a 85°C 85% RH reliability test comparing dye-sensitized solar cells with a cell gap of 20 μm, dye-sensitized solar cells with a cell gap of 15 μm, and dye-sensitized solar cells with a cell gap of 10 μm. In the test, dye-sensitized solar cells were prepared under different cell gap conditions with various seal widths, and the time until leakage occurred when each dye-sensitized solar cell was exposed to a temperature of 85°C and a relative humidity of 85% was measured. The vertical axis of FIG. 5 shows the ratio of the time until leakage to the time until leakage of a dye-sensitized solar cell with a seal width of 1.2-1.3 mm and a cell gap of 20 μm, which is set to 1. As shown in FIG. 5, the time until leakage of a dye-sensitized solar cell 1 with a cell gap of 15 μm is about twice as long as the time until leakage of a dye-sensitized solar cell 1 with a cell gap of 20 μm. Furthermore, as shown in Figure 5, the time until leakage of the dye-sensitized solar cell 1 with a cell gap of 10 μm is about 5 to 6 times longer than the time until leakage of the dye-sensitized solar cell 1 with a cell gap of 20 μm. In this way, the reliability of the dye-sensitized solar cell is improved by narrowing the cell gap.

[0028] For the above reasons, in this embodiment, the cell gap is set to 10 to 15 μm. By specifying the cell gap in this manner, the reliability of the dye-sensitized solar cell 1 can be improved.

[0029] Here, the narrowing of the cell gap relatively increases the shear stress in the sealing material 19. This makes it difficult for the sealing material 19 to deform against an external force caused by the balance between the increase and decrease of the electrolyte 18 when the electrolyte 18 is injected. As a result, the cell gap can be maintained at a desired value not only in the peripheral part of the dye-sensitized solar cell 1 but also in the center. In addition, the increase in shear stress eliminates local thinning of the sealing material 19 caused by the step of the wiring formed by the light absorption layer 16 and the like. This also improves durability against liquid leakage. Furthermore, the increase in shear stress reduces the breakage of the peripheral sealing material caused by the pressure difference between the inside and outside of the peripheral sealing material when the electrolyte 18 is injected by the ODF (One Drop Filling) method. As a result, a stable cell gap can be formed.

[0030] In addition, the current value of the dye-sensitized solar cell is determined by the carrier I - and I 3 - It is considered that the time required for the carriers to travel is the time required for the carriers to travel between the light absorbing layer 16 and the catalyst layer 17. By shortening the cell gap, the inter-electrode distance between the light absorbing layer 16 and the catalyst layer 17 is also shortened. By shortening the inter-electrode distance, the time required for the carriers to travel is shortened, leading to an increase in the current value. In this way, shortening the cell gap also contributes to improving the power generation performance.

[0031] Next, a method for manufacturing the dye-sensitized solar cell 1 will be described. Figures 6A to 6E are diagrams showing the manufacturing process of the dye-sensitized solar cell 1. In this embodiment, an anode substrate on which an anode electrode is formed and a cathode substrate on which a cathode electrode is formed are separately formed, and then the two are bonded together to manufacture the dye-sensitized solar cell 1.

[0032] First, a method for manufacturing the anode substrate will be described with reference to Figs. 6A to 6C. As shown in Fig. 6A, an electrode 13, an electron transport layer 15, and a light absorbing layer 16 are formed in sequence on a first substrate 11 such as a glass substrate. For example, a transparent conductive oxide film such as an ITO film and a titanium oxide (TiO x After the transparent conductive oxide film and the titanium oxide film are formed in sequence, the transparent conductive oxide film and the titanium oxide film are etched to match the shapes of the electrode 13 and the electron transport layer 15. Then, the light absorbing layer 16 is formed on the electron transport layer 15 of each unit. For this purpose, first, an electron collector, for example, TiO 2 The paste is formed on the electron transport layer 15 of each unit by a method such as screen printing. The TiO 2 The paste is fired at high temperatures of 300°C to 550°C for 60 to 240 minutes. 2 For example, TiO 2 The film is immersed in the dye solution at room temperature for about 16 to 48 hours, whereby the dye is deposited. As described above, the thickness of the anode electrode is the sum of the thicknesses of the electrode 13, the electron transport layer 15, and the light absorbing layer 16. In practice, the thickness of the anode electrode is almost equal to the thickness of the light absorbing layer 16. For example, TiO 2 When TiO is used, the thickness of the film after firing is set to about 10 μm. 2 The paste and application amount are set.

[0033] Next, as shown in FIG. 6B, a sealant 19 is applied by a method such as dispensing. Although not shown in FIG. 6B, when a plurality of dye-sensitized solar cells 1 are formed on the first substrate 11, a peripheral seal may be formed to surround the outermost dye-sensitized solar cell 1. Granular spacers with a particle size of 10-15 μm, for example, resin beads, are mixed into the sealant 19. The amount of the resin beads mixed in is, for example, about 1.25% by weight of the sealant 19, but is not limited thereto. This results in a cell gap of 10-15 μm after the substrates are bonded together.

[0034] In recent years, in order to reduce the cell size of the dye-sensitized solar cell 1, it has become necessary to form the encapsulant 19 small as well. Therefore, in order to form the encapsulant 19 to a desired size, it is necessary to measure the cross-sectional area of ​​each substrate. Based on the performance of a general drawing cross-section measurement device, the cross-sectional area S of the encapsulant 19 is 3000 μm 2 -30000μm 2 On the other hand, the seal width w s The minimum seal width w of the sealing material 19 must be equal to or greater than the width A of the wiring of the electrode 13 and the counter electrode 14 passing through the sealing material 19 plus the processing margin B. The processing margin is generally ±0.1 mm. smin The maximum seal width w of the sealing material 19 is the wiring width A+0.2 mm. smax is limited by the maximum cross-sectional area. For example, the maximum seal width w when the cell gap is 15 μm is smax is the maximum cross-sectional area S of the encapsulant 19 max / Cell gap SG + processing margin B = (30000 / 15) / 1000 + 0.2 = 2.2 mm.

[0035] Next, as shown in FIG. 6C, the electrolyte solution 18 is applied onto the light absorbing layer 16. In this embodiment, the electrolyte solution 18 is applied by dripping from above the first substrate 11. The amount of the electrolyte solution 18 to be dripped is, for example, 1 / (the volume V of the dye-sensitized solar cell 1). c )-(Volume of the sealing material 19 V s )-(anode electrode volume V e ) is calculated from the volume V c is (the distance D between the sealing materials 19) × (the length L of the sealing materials 19) s ) × (cell gap SG). Volume V of the sealing material 19 s is the cross-sectional area measurement result of the sealing material 19 × (seal width W s + Length of sealing material 19 L s Here, the cross-sectional area of ​​the sealing material 19 is calculated by converting the cross-sectional area of ​​the sealing material 19 measured in a diagonal direction into the perpendicular direction. The volume V of the anode electrode e is substantially the volume of the light absorbing layer 16 (the width w e )×(length of light absorbing layer 16 Le )×(film thickness d of the light absorbing layer 16)×(correction coefficient α). s are the width of the encapsulant, w s The length L of the light absorbing layer 16 is perpendicular to both the direction of the cell gap SG and the direction of the cell gap SG. e are the width w of the light absorbing layer 16, e The correction coefficient α is a coefficient for taking into consideration that the light absorbing layer 16 is an accumulation of porous oxide semiconductors.

[0036] Next, a method for manufacturing a cathode substrate will be described with reference to Fig. 6D. As shown in Fig. 6D, a counter electrode 14 and a catalyst layer 17 are formed in sequence on a second substrate 12 such as a glass substrate. For example, a transparent conductive oxide film such as an ITO film and a platinum film are formed in sequence on the second substrate 12, and then the transparent conductive oxide film and the platinum film are etched to match the shapes of the counter electrode 14 and the catalyst layer 17. In this manner, a cathode substrate is manufactured.

[0037] After the anode substrate and the cathode substrate are manufactured, the anode substrate and the cathode substrate are bonded together with a sealant 19 interposed therebetween, as shown in FIG. 6E.

[0038] As described above, in the embodiment, a dye-sensitized solar cell having a cell gap specified based on reliability is obtained. A dye-sensitized solar cell having such a cell gap has high resistance to liquid leakage, etc. In addition, since the cell gap is changed without changing the seal width, high reliability is obtained, and the effective area can be increased because the seal width of the sealant 19 does not become larger than necessary.

[0039] [Variations] A modified example of the embodiment will be described. In the embodiment, the spacers for forming the cell gap are granular spacers such as resin beads. In contrast, the spacers may be any spacers capable of forming a desired cell gap. For example, as shown in FIG. 7, columnar spacers 19b having a height of 10 μm-15 μm may be used as the spacers. The columnar spacers 19b may be formed on the first substrate 11 prior to application of the sealing material 19 shown in FIG. 6B. The columnar spacers 19b may be formed on the second substrate 12.

[0040] Here, the columnar spacer 19b does not necessarily have to be formed at the position of the sealing material 19. The columnar spacer 19b may be formed at a position outside the sealing material 19 as shown in FIG.

[0041] The present invention is not limited to the above-mentioned embodiment, and various modifications can be made in the implementation stage without departing from the gist of the invention. In addition, the embodiments may be implemented in appropriate combination, and in that case, the combined effect can be obtained. Furthermore, the above-mentioned embodiment includes various inventions, and various inventions can be extracted by combinations selected from the multiple components disclosed. For example, if the problem can be solved and the effect can be obtained even if some components are deleted from all the components shown in the embodiment, the configuration from which the components are deleted can be extracted as an invention. [Explanation of symbols]

[0042] 1 dye-sensitized solar cell, 11 first substrate, 12 second substrate, 13 electrode, 14 counter electrode, 15 electron transport layer, 16 light absorption layer, 16a dye, 16b electron collector, 17 catalyst layer, 18 electrolyte, 19 sealing material, 19a, 19b spacers.

Claims

1. An electrode formed on a first substrate; an electron transport layer formed on the electrode; a light absorbing layer formed on the electron transport layer and including an electron collector and a dye; a counter electrode formed on a second substrate disposed opposite the first substrate; A catalyst layer formed on the counter electrode; an electrolyte filled between the light absorbing layer and the catalyst layer; a sealant that bonds the first substrate and the second substrate together while sealing the electrolytic solution; Equipped with The distance between the first substrate and the second substrate is 10 μm to 15 μm. Dye-sensitized solar cells.

2. The gap between the first substrate and the second substrate is set by a particulate spacer having a particle size of 10 μm to 15 μm mixed into the sealing material. The dye-sensitized solar cell according to claim 1 .

3. The distance between the first substrate and the second substrate is set by a columnar spacer having a height of 10 μm to 15 μm. The dye-sensitized solar cell according to claim 1 .

4. The columnar spacer is formed at a position separated from the sealing material. The dye-sensitized solar cell according to claim 3 .

5. The width of the sealing material that seals the electrolyte is equal to or greater than the sum of the width of the wiring passing through the sealing material and the processing margin of the sealing material. The dye-sensitized solar cell according to claim 1 .

Citation Information

Patent Citations

  • Method for forming photoelectrode base material layer used for dye-sensitized solar battery, base material for dye-sensitized solar batteries, method for manufacturing dye-sensitized solar battery, and dye-sensitized solar battery

    JP2016018897A