Sheet dispenser
A tabletop sheet dispenser using microfiber cellulose composite resin addresses installation and aesthetic challenges of wall-mounted dispensers by providing a harmonious, durable, and space-efficient solution with a unique color and texture.
Patent Information
- Application Number
- JP2023066260
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-14
- Publication Date
- 2024-10-25
AI Technical Summary
Existing sheet dispensers, particularly those installed on walls, are bulky and limit installation options, making them unsuitable for kitchens and spaces with limited space, and are often monochromatic, failing to harmonize with other furnishings, with resin-based dispensers risking damage from drops.
A tabletop sheet dispenser made of microfiber cellulose composite resin, featuring a hexahedral design with stacked sheets and a pedestal, incorporating microfiber cellulose spots for color variation and enhanced strength, using a resin and microfiber cellulose blend with a white pigment for aesthetic harmony and durability.
The dispenser provides a light brown, stone-like appearance that harmonizes with surroundings, offers improved strength to resist drops, and reduces resin usage, ensuring compatibility with various interior designs while maintaining structural integrity.
Smart Images

Figure 2024152210000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a sheet dispenser that stores a stack of folded sheets such as paper towels and dispenses them one by one from a dispenser opening, and more particularly to a tabletop sheet dispenser. [Background technology]
[0002] Many dispensers for paper or nonwoven fabric sheets, sometimes called paper towels such as kitchen paper and cleaning wipes, are installed by suitable means with the back of the main body that stores the stack facing a wall, and the paper towel is pulled out from an outlet provided at the bottom for use (Patent Documents 1 to 3, etc.), although some are also known as freestanding or tabletop types (Patent Documents 4 to 6, etc.).
[0003] Dispensers of the type that are installed on a wall via the back of the main body, as shown in Patent Documents 1 to 3, are relatively large and have limited installation methods, and are therefore unsuitable for use in restaurants, delicatessens, supermarket kitchens, or ordinary homes, where it is difficult to secure installation space or locations. In such locations, the stationary types shown in References 4 to 6 are more suitable.
[0004] Many of these dispensers are made of resin because it is easy to process. Resin is not only easy to process, but some have excellent transparency, making it suitable as a material for dispensers. On the other hand, many dispensers made of resin are monochromatic, and many people have the impression that they do not match with other furnishings in terms of color. There is also a risk of them breaking if they are accidentally dropped from a table. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Japanese Patent Application Publication No. 06-144448 [Patent Document 2] JP 2006-204404 A [Patent Document 3] JP 2001-87161 A [Patent Document 4] JP 2007-153439 A [Patent Document 5] JP 2010-76811 A [Patent Document 6] JP 2013-135772 A Summary of the Invention [Problem to be solved by the invention]
[0006] Therefore, the main object of the present invention is to provide a tabletop sheet dispenser that can be suitably used in places with limited space, such as the kitchens of restaurants, delicatessens, and supermarkets, and in homes, that has an amber color that harmonizes with other furnishings when placed together with them, and that is strong. [Means for solving the problem]
[0007] The aspects of the present invention that solve the above problems are as follows.
[0008] (First aspect) A sheet dispenser for storing a stack of substantially rectangular parallelepiped sheets, the stack being made by stacking a plurality of rectangular sheets folded in half in a staggered manner such that the edges of the folded pieces are positioned on the inner fold surfaces of adjacent sheets, the stack comprising: The sheet dispenser comprises: The plate is made of a microfiber cellulose composite resin having a resin and microfiber cellulose having an average fiber diameter of 1 to 19 μm, and spots made of the microfiber cellulose are formed on the plate. A sheet dispenser characterized by:
[0009] (Second aspect) The device has a case body for storing a stack of substantially rectangular parallelepiped sheets, the stack being formed by stacking a plurality of rectangular sheets folded in half in a staggered manner with the edges of the folded pieces positioned on the inner folds of the adjacent sheets, a base portion for making the case body a tabletop type, and an outlet provided in the case body for pulling out the sheets, The case body and / or the base portion are The plate is made of a microfiber cellulose composite resin having a resin and microfiber cellulose having an average fiber diameter of 1 to 19 μm, and spots made of the microfiber cellulose are formed on the plate. A sheet dispenser characterized by:
[0010] The color of cellulose fibers changes to some extent depending on the length of the fiber diameter. The reason for the color change is not precisely known, but is probably due to the relationship between the transmittance and refractive index of the light irradiated to the fiber. In this embodiment, since the average fiber diameter of the microfiber cellulose is within the above range, it is considered that the composite resin will exhibit an amber color. In addition, the microfiber cellulose contained in the composite resin is in a state where each is appropriately dispersed by the kneading process, but some of them aggregate together to form aggregates. These aggregates are visually recognized as spots. Furthermore, the inventors have confirmed that the dispenser of this embodiment is stronger when formed from a composite resin having resin and microfiber cellulose than when formed from only resin.
[0011] (Third aspect) The plate is formed of a microfiber cellulose composite resin having the resin, the microfiber cellulose, and a white pigment, and is opaque. A sheet dispenser according to the first or second embodiment.
[0012] By including a white pigment in the microfiber cellulose composite resin, the spots scattered on the surface of the plate-like portion forming the dispenser of this embodiment and the white color of the white pigment combine to give the dispenser a stone-like texture. In addition, although microfiber cellulose has the property of agglomerating, when the white pigment is included, the white pigment enters the gaps formed between the microfiber cellulose, suppressing the aggregation of the microfiber cellulose. As a result, the microfiber cellulose remains appropriately dispersed in the composite resin, improving the strength of the composite resin. Note that, even if the aggregation of the microfiber cellulose is suppressed, it does not mean that aggregation does not occur at all.
[0013] (Fourth aspect) The area per unit area of the plate is 0.1 mm 2 The number of spots exceeding this limit is 10 to 12,000 per 100 cm of board. 2 This is what happens: The sheet dispenser according to the first or second embodiment.
[0014] Generally, cellulose fibers can be defibrated into pulp, microfiber cellulose, and cellulose nanofibers depending on the degree of defibration, but the spots with an average diameter in the range of this embodiment are formed mainly due to the inclusion of microfiber cellulose. Furthermore, if the spots have an area in the above range, they can be easily recognized visually, and the appearance will be different from the monotonous colors that are common in conventional dispensers, making them easier to harmonize with other furnishings.
[0015] (Fifth aspect) The microfibrous cellulose has a modified microfibrous cellulose in which all or a part of the hydroxyl groups are replaced with carbamate groups. The sheet dispenser according to the first or second embodiment.
[0016] The modified microfiber cellulose substituted with carbamate groups has fewer hydrogen bond points than unmodified microfiber cellulose, so the microfiber cellulose is less likely to aggregate due to hydrogen bonds, and the composite resin has improved strength.
[0017] (Sixth aspect) The thickness of the plate is 1 to 5 mm. A sheet dispenser according to the first or second embodiment.
[0018] (Seventh aspect) The microfiber cellulose composite resin has a flexural modulus of 1.0 to 3.0 GPa. A sheet dispenser according to the first or second embodiment.
[0019] If the flexural modulus is within the above range, the dispenser will be less likely to be damaged even if dropped from a table or subjected to other external forces.
[0020] (Eighth aspect) The microfiber cellulose has a lignin content of 1% or less in the raw pulp. A sheet dispenser according to the first or second embodiment.
[0021] Since the lignin content is within the above range, there is an advantage that the color does not fade easily even when used for a long period of time.
[0022] (Ninth aspect) The microfiber cellulose composite resin has a blending ratio of microfiber cellulose in the microfiber cellulose composite resin of 1 to 20% by mass. A sheet dispenser according to the first or second embodiment.
[0023] When the blending ratio is within the above range, the microfiber cellulose is appropriately dispersed in the resin, and the number of spots on the composite resin surface is also appropriate. Effect of the Invention
[0024] According to the present invention, a sheet dispenser having an amber colored appearance and improved resin strength is obtained. [Brief description of the drawings]
[0025] [Figure 1] 1 is a perspective view of a sheet dispenser according to the present invention; [Diagram 2] FIG. 2 is a front view of the sheet dispenser according to the present invention. [Diagram 3] FIG. 3 is a schematic diagram of a cross section taken along line AA in FIG. 2. [Figure 4] FIG. 1 is a schematic cross-sectional view showing another example of a sheet dispenser according to the present invention. [Diagram 5] FIG. 11 is a schematic cross-sectional view showing another example of the sheet dispenser according to the present invention when it is open. [Figure 6] FIG. 11 is a schematic cross-sectional view showing another example of a sheet dispenser according to the present invention. [Figure 7] FIG. 2 is a perspective view showing a pressing member according to the present invention. [Figure 8] FIG. 11 is a perspective view showing another example of a pressing member according to the present invention. [Figure 9] FIG. 2 is another perspective view of the sheet dispenser according to the present invention. [Figure 10] FIG. 13 is a perspective view of another embodiment of a sheet dispenser according to the present invention. [Figure 11] 1A and 1B are diagrams showing examples of a base part of a sheet dispenser according to the present invention. [Figure 12] FIG. 2 is a perspective view of another embodiment of a sheet dispenser according to the present invention. [Figure 13] FIG. 11 is a front view of another embodiment of a sheet dispenser according to the present invention. [Figure 14] FIG. 14 is a schematic diagram of the A'-A' cross section of FIG. [Figure 15] FIG. 11 is a schematic cross-sectional view showing still another embodiment of the sheet dispenser according to the present invention. [Figure 16] FIG. 1 is a diagram of a sheet dispenser according to the present invention. [Figure 17] FIG. 13 is a front view of a sheet dispenser according to a third embodiment. [Figure 18] This is a cross-sectional view taken along line II-II. [Figure 19] 19 is a cross-sectional view showing only the case main body of FIG. 18. [Figure 20] FIG. 2 is a front view of the case body of the embodiment. [Figure 21] FIG. 2 is a top view of the seat support of the present embodiment. [Figure 22] FIG. 19 is a cross-sectional view showing only the lid body of FIG. 18. [Figure 23] FIG. 2 is a front view of a case main body according to the first embodiment. [Figure 24] FIG. 2 is a diagram of spots formed on the surface of a sheet dispenser according to the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0026] The sheet dispenser of the present invention is a sheet dispenser that stores inside a stack of sheets having an approximately rectangular hexahedral shape, which is formed by stacking multiple folded square sheets in a staggered manner with the edges of the folded pieces positioned on the inner fold of the adjacent sheets, and is characterized in that the sheet dispenser is formed from a plate of a microfiber cellulose composite resin containing resin and microfiber cellulose having an average fiber diameter of 1 to 19 μm, and spots 41 made of the microfiber cellulose are formed on the plate.
[0027] Here, the resin contained in the microfiber cellulose composite resin refers to the resin pellets and resin powder described later, but is mainly the resin pellets. The resin pellets are intended solely for adjusting the blending ratio of the resin contained in the microfiber cellulose composite resin, and the resin powder is intended solely for suppressing the aggregation of the microfiber cellulose, which has the property of aggregating. Since both the resin pellets and the resin powder melt due to the heat applied during the kneading process, it is difficult to isolate each of them from the microfiber cellulose composite resin that has been formed once. In addition, the resin pellets and the resin powder may be different substances from each other, or may be the same substance. If the resin pellets and the resin powder are different substances from each other, the resin component Y2 derived from the resin powder may be visually recognized as a streaky pattern in the microfiber cellulose composite resin in which the resin component Y1 derived from the resin pellets is dominant, and the dispenser may have aesthetic appeal.
[0028] (Microfiber Cellulose) The microfiber cellulose, which is the raw material of the microfiber cellulose composite resin, will be described in detail below. When the cellulose raw material (hereinafter also referred to as "raw material pulp") is defibrated (refined), it becomes fine fibers with a fiber diameter shorter than that of the raw material pulp. The diameter of the fine fibers can be adjusted to cellulose fibers with an average fiber width of 19 μm or less, for example, depending on the degree of defibration. Among them, those with an average fiber diameter of 1 to 19 μm can be distinguished as microfiber cellulose and cellulose nanofibers that have been defibrated with an average fiber diameter shorter than that. Since cellulose nanofibers have a relatively small average fiber diameter and a large aspect ratio, they tend to form a dense three-dimensional network structure with many hydrogen bond points per unit cellulose fiber. However, when kneaded with a resin to form a composite resin, a significant improvement in strength cannot be expected. In addition, in the washing process performed for the purpose of removing unreacted remaining urea, etc. after the carbamate reaction described below, if the fiber to be washed is cellulose nanofiber, the dehydration is very poor. In contrast, since microfiber cellulose has a relatively large average fiber diameter, the three-dimensional network structure formed is less dense than that of cellulose nanofiber, but a significant improvement in strength can be expected when it is used as a composite resin. In addition, microfiber cellulose is easier to modify with carbamate groups (carbamate formation) than cellulose nanofiber, which is also a fine fiber, from the viewpoint of dehydration. Furthermore, since microfiber cellulose has a relatively large average fiber diameter, it is possible to visually confirm that it contains microfiber cellulose even when it is used as a composite resin. Therefore, the present invention is a method of suitably selecting microfiber cellulose from among the cellulose fibers obtained by defibration, and by providing this, it is possible to obtain an appearance that harmonizes with other furnishings and an effect of excellent strength.
[0029] The microfiber cellulose has an average fiber width of, for example, 1 to 19 μm, preferably 5 to 17 μm, and more preferably 10 to 15 μm. When the average fiber width of the microfiber cellulose is less than 1 μm, it is no different from cellulose nanofiber, and there is a risk that the effect of improving the strength of the resin (particularly the bending modulus) is not sufficiently obtained. In addition, the defibration time is long, and a large amount of energy is required. Furthermore, dehydration is deteriorated. When the dehydration is deteriorated, a large amount of energy is required for drying, and the large amount of energy may deteriorate the microfiber cellulose and reduce its strength. On the other hand, when the average fiber width of the microfiber cellulose is more than 19 μm, it is no different from pulp, and the reinforcing effect is insufficient, and when it is used as a sheet dispenser, the impression given by the color and pattern of the appearance may not be as expected.
[0030] As the raw material pulp for microfiber cellulose, one or more types can be selected and used from, for example, wood pulp made from broadleaf trees, coniferous trees, etc., non-wood pulp made from straw, bagasse, cotton, hemp, bast fiber, etc., and waste paper pulp (DIP) made from recycled waste paper, broke paper, etc. The above various raw materials may be in the form of a pulverized material (powdered material) called, for example, cellulose-based powder.
[0031] However, in order to prevent impurities from being mixed in as much as possible, it is preferable to use wood pulp as the raw material pulp. As the wood pulp, for example, one or more types may be selected from chemical pulps such as hardwood kraft pulp (LKP) and softwood kraft pulp (NKP), and mechanical pulp (TMP), etc.
[0032] The hardwood kraft pulp may be bleached hardwood kraft pulp, unbleached hardwood kraft pulp, or semi-bleached hardwood kraft pulp. Similarly, the softwood kraft pulp may be bleached softwood kraft pulp, unbleached softwood kraft pulp, or semi-bleached softwood kraft pulp.
[0033] As the mechanical pulp, for example, one or more types can be selected and used from stone ground pulp (SGP), pressed stone ground pulp (PGW), refiner ground pulp (RGP), chemi-ground pulp (CGP), thermo-ground pulp (TGP), ground pulp (GP), thermo-mechanical pulp (TMP), chemi-thermomechanical pulp (CTMP), refiner mechanical pulp (RMP), bleached thermo-mechanical pulp (BTMP), etc.
[0034] For the microfiber cellulose, it is preferable to use a pulp having a lignin content of 1.0% or less, and more preferably 0.8% or less, as the raw material pulp. When a carbamate-treated microfiber cellulose is used, for example, the cellulose fiber is heat-treated so that the substitution rate of the carbamate group is 2.0 mmol / g or more, and coloring is likely to proceed. However, if the lignin content of the raw material pulp is within the above range, coloring caused by lignin can be suppressed, and coloring when the microfiber cellulose is made into a composite resin can also be suppressed. In addition, when the cellulose raw material is carbamate-treated, carbamate-treatment also occurs for the lignin coexisting with the cellulose. Thereafter, when the cellulose is washed, the carbamate-treated lignin flows out and is removed, and as a result, the carbamate-treatment rate of the cellulose remaining in the fiber may decrease. If the lignin contained in the microfiber cellulose solid is at the above content, the amount of carbamate-treated products that flow out and do not contribute to fiber reinforcement can be suppressed, and the effect of excellent strength when made into a composite resin is achieved. Furthermore, if the lignin content of the raw pulp exceeds 1.0%, the surface of the sheet dispenser of this embodiment may fade or yellow over the long term.
[0035] The lignin content is a value measured in accordance with the Lignin Content Test Method (JAPAN TAPPI No. 61 (2000)).
[0036] From the viewpoint of preventing discoloration, the kappa number of the raw material pulp is preferably 2 or less, and more preferably 1 or less.
[0037] The kappa number is a value measured in accordance with the kappa number test method (JIS-P-8211 (2011)).
[0038] The lignin content and the kappa number can be adjusted, for example, by the selection of the raw pulp, cooking, bleaching, and the like.
[0039] In this embodiment, the whiteness of the raw pulp is preferably 50% or more, more preferably 80% or more, and particularly preferably 82% or more. If the whiteness of the raw pulp itself is less than 50%, the whiteness of the composite resin itself will be low.
[0040] The whiteness value is a value measured in accordance with JIS-P-8148:2001.
[0041] The raw material pulp can be defibrated by beating the raw material pulp using, for example, a homogenizer such as a beater, a high-pressure homogenizer, or a high-pressure homogenizer, a stone mill-type friction machine such as a grinder or a grinding machine, a single-shaft kneader, a multi-shaft kneader, a kneader refiner, a jet mill, etc. However, it is preferable to use a refiner or a jet mill.
[0042] The average fiber length of the microfibrous cellulose (average length of single fibers) is preferably 1.0 mm or less, more preferably 0.1 to 1.0 mm, more preferably 0.2 to 0.8 mm, and particularly preferably 0.3 to 0.6 mm. Microfibrous cellulose with an average fiber length of more than 1.0 mm is likely to aggregate and may not be sufficiently dispersed. On the other hand, if the average fiber length is 0.1 mm or more, a three-dimensional network between the fibers is easily formed, which has the advantage of improving dispersibility.
[0043] The average fiber length of the cellulose raw material that is the raw material for the microfiber cellulose is preferably 5.00 mm or less, preferably 0.50 to 5.00 mm, more preferably 1.00 to 3.00 mm, and particularly preferably 1.50 to 2.50 mm. If the average fiber length exceeds 5.00 mm, there is a risk of being disadvantageous in terms of production costs during defibration. On the other hand, if the average fiber length of the cellulose raw material is 0.50 mm or more, there is a possibility that an excellent reinforcing effect of the resin can be obtained.
[0044] The average fiber length of the microfibrous cellulose can be adjusted as desired by, for example, selecting the raw pulp, pre-treating, defibrating, and the like.
[0045] The fine A ratio of the microfiber cellulose is preferably 5% or more and 80% or less, more preferably 10% or more and 70% or less, and particularly preferably 15% or more and 60% or less. When the fine ratio is 5% or more, the proportion of homogeneous fibers is high, and the composite resin is less likely to break down. However, when the fine ratio exceeds 80%, the strength may be insufficient. In addition, when the fine ratio exceeds 80%, it is thought that some fibers are too low molecular weight, and these fibers are prone to generate oligosaccharides and monosaccharides that cause coloring when exposed to heat.
[0046] In addition, the fine A ratio of the microfiber cellulose is preferably within the above range, and the fine B ratio of the microfiber cellulose is preferably 15 to 50%, more preferably 16 to 40%. When the fine B ratio is within the above range, the strength of the composite resin is further increased.
[0047] The above is the fineness ratio of the microfiber cellulose, but it is more preferable if the fine A ratio of the cellulose raw material that is the raw material for the microfiber cellulose is also within a specified range. Specifically, the fine A ratio of the cellulose raw material that is the raw material for the microfiber cellulose is preferably 1% or more, more preferably 3 to 20%, and particularly preferably 5 to 18%. If the fine A ratio of the cellulose raw material before defibration is within the above range, it is considered that even if the microfiber cellulose is defibrated so that the fine A ratio is 30% or more, the damage to the fibers is small and the reinforcing effect of the resin is improved.
[0048] The fine A ratio can be adjusted by pretreatment such as enzyme treatment. However, especially when enzyme treatment is performed, the fiber itself may become tattered, and the reinforcing effect of the resin may decrease. Therefore, from this viewpoint, the amount of enzyme added is preferably 2% by mass or less, more preferably 1% by mass or less, and particularly preferably 0.5% by mass or less. Also, not performing enzyme treatment (addition amount 0% by mass) is also an option.
[0049] In this embodiment, "fine A rate" refers to the percentage of the total mass of pulp fibers with a fiber width of 75 μm or less and a fiber length of 0.2 mm or less to the total mass of pulp fibers. "Fine B rate" refers to the percentage of the total mass of pulp fibers with a fiber width of 10 μm or less and a fiber length of 0.2 mm or more to the total mass of pulp fibers.
[0050] The aspect ratio of the microfibrous cellulose is preferably 5 to 1000, more preferably 10 to 200, and even more preferably 20 to 100. If the aspect ratio is less than 5, a three-dimensional network cannot be sufficiently constructed, and even if the average fiber length is 0.1 mm or more, the reinforcing effect may be insufficient. On the other hand, if the aspect ratio exceeds 1000, the entanglement of the microfibrous cellulose becomes high, and dispersion in the resin may be insufficient.
[0051] The fibrillation rate of the microfibrous cellulose is preferably 0.1 to 3.0%, more preferably 0.3 to 2.8%, and particularly preferably 0.5 to 2.5%. If the fibrillation rate exceeds 3.0%, the contact area with water becomes too large, so that even if the microfibrous cellulose is defibrated to a range in which the average fiber width remains at 1 μm or more, dehydration may become difficult. On the other hand, if the fibrillation rate is less than 1.0%, there may be few hydrogen bonds between fibrils, making it impossible to form a strong three-dimensional network.
[0052] In this embodiment, the fibrillation rate refers to a value obtained by disintegrating cellulose fibers in accordance with JIS-P-8220:2012 "Pulp - Disintegration method" and measuring the resulting disintegrated pulp using a fiber analyzer "FS5" manufactured by Valmet Co., Ltd. The average fiber length and fine A rate of cellulose fibers can also be measured using a fiber analyzer "FS5" manufactured by Valmet Co., Ltd.
[0053] The crystallinity of the microfiber cellulose is preferably 50% or more, more preferably 55% or more, and particularly preferably 60% or more. If the crystallinity is less than 50%, the strength of the fiber itself decreases, and there is a risk that the strength of the resin cannot be improved. On the other hand, the crystallinity of the microfiber cellulose is preferably 95% or less, more preferably 90% or less, and particularly preferably 85% or less. If the crystallinity is more than 95%, the proportion of strong hydrogen bonds formed within the molecule increases, the fiber itself becomes easily rigid and aggregated, and dispersibility in the resin becomes poor.
[0054] The crystallinity of the microfibrous cellulose can be adjusted as desired, for example, by selecting the raw pulp, pre-treating it, and refining it.
[0055] The pulp viscosity of the microfiber cellulose is preferably 2 cps or more, more preferably 4 cps or more. If the pulp viscosity of the microfiber cellulose is less than 2 cps, it may be difficult to suppress the aggregation of the microfiber cellulose.
[0056] The freeness of the microfiber cellulose is preferably 500 ml or less, more preferably 300 ml or less, and particularly preferably 100 ml or less. If the freeness of the microfiber cellulose exceeds 500 ml, the effect of improving the strength of the resin may not be sufficiently obtained.
[0057] The zeta potential of the microfibrous cellulose is preferably -150 to 20 mV, more preferably -100 to 0 mV, and particularly preferably -80 to -10 mV. If the zeta potential is less than -150 mV, the compatibility with the resin may be significantly reduced, resulting in insufficient reinforcing effect. On the other hand, if the zeta potential is more than 20 mV, the dispersion stability may be reduced.
[0058] The water retention of the microfiber cellulose is preferably 80 to 400%, more preferably 90 to 350%, and particularly preferably 100 to 300%. If the water retention is less than 80%, the microfiber cellulose is no different from the raw material pulp, and the reinforcing effect of the composite resin due to the inclusion of the microfiber cellulose may be insufficient. On the other hand, if the water retention exceeds 400%, the dehydration tends to be poor, and it is difficult to obtain a homogeneous composite resin. On the other hand, if the water retention of the microfiber cellulose is within the above range, it is easy to dehydrate and the fibers are less likely to be damaged, which contributes to improving the strength of the composite resin. The water retention of the microfiber cellulose can be further reduced by substituting the hydroxyl group of the fiber with a carbamate group, and the dehydration and drying properties can be improved.
[0059] The water retention of the microfiber cellulose can be adjusted as desired by, for example, selecting the raw pulp, pre-treating it, defibrating it, and the like.
[0060] Microfiber cellulose does not require any particular modification treatment, but in order to improve water repellency and dispersibility, all or part of the hydroxyl groups of cellulose fibers may be substituted with carbamate groups to obtain modified microfiber cellulose. The timing of substituting the hydroxyl groups of microfiber cellulose with carbamate groups is not particularly limited. For example, a carbamate reaction may be carried out on a cellulose raw material before defibration to obtain microfiber cellulose having carbamate groups, or a carbamate reaction may be carried out on microfiber cellulose (cellulose raw material defibrated) to obtain microfiber cellulose having carbamate groups.
[0061] Having a carbamate group means that a carbamate group (an ester of carbamic acid) is introduced into the microfiber cellulose. The carbamate group can be represented by the following structural formula (Chemical Formula 1), and is, for example, represented by -O-CO-NH-, and examples thereof include -O-CO-NH2, -O-CONHR, and -O-CO-NR2.
[0062] [ka]
[0063] Here, n represents an integer of 1 or more. Each R is independently at least one of a saturated linear hydrocarbon group, a saturated branched hydrocarbon group, a saturated cyclic hydrocarbon group, an unsaturated linear hydrocarbon group, an unsaturated branched hydrocarbon group, an aromatic group, and a group derived therefrom.
[0064] Examples of the saturated linear hydrocarbon group include linear alkyl groups having 1 to 10 carbon atoms, such as a methyl group, an ethyl group, and a propyl group.
[0065] Examples of the saturated branched hydrocarbon group include branched alkyl groups having 3 to 10 carbon atoms, such as an isopropyl group, a sec-butyl group, an isobutyl group, and a tert-butyl group.
[0066] Examples of the saturated cyclic hydrocarbon group include cycloalkyl groups such as a cyclopentyl group, a cyclohexyl group, and a norbornyl group.
[0067] Examples of the unsaturated linear hydrocarbon group include linear alkenyl groups having 2 to 10 carbon atoms, such as ethenyl, propen-1-yl, and propen-3-yl, and linear alkynyl groups having 2 to 10 carbon atoms, such as ethynyl, propyn-1-yl, and propyn-3-yl.
[0068] Examples of the unsaturated branched hydrocarbon group include branched alkenyl groups having 3 to 10 carbon atoms, such as a propen-2-yl group, a buten-2-yl group, and a buten-3-yl group, and branched alkynyl groups having 4 to 10 carbon atoms, such as a butyn-3-yl group.
[0069] Examples of the aromatic group include a phenyl group, a tolyl group, a xylyl group, and a naphthyl group.
[0070] Examples of derivative groups include groups in which one or more hydrogen atoms in the above-mentioned saturated linear hydrocarbon groups, saturated branched hydrocarbon groups, saturated cyclic hydrocarbon groups, unsaturated linear hydrocarbon groups, unsaturated branched hydrocarbon groups, and aromatic groups are substituted with substituents (e.g., hydroxy groups, carboxy groups, halogen atoms, etc.).
[0071] In microfiber cellulose having a carbamate group (also called modified microfiber cellulose) (in which a carbamate group has been introduced), some or all of the highly polar hydroxyl groups are replaced with carbamate groups having relatively low polarity. Therefore, microfiber cellulose having a carbamate group has low hydrophilicity and high affinity with resins having low polarity. As a result, microfiber cellulose having a carbamate group has excellent uniform dispersion with similarly hydrophobic resins. In addition, a slurry of microfiber cellulose having a carbamate group has low viscosity and good handling properties.
[0072] The substitution rate of the carbamate group for the hydroxyl group of the microfiber cellulose is preferably 0.1 to 2.0 mmol / g, more preferably 0.2 to 1.8 mmol / g, and particularly preferably 0.3 to 1.6 mmol / g. When the substitution rate exceeds 2.0 mmol / g, the hydrogen bond between cellulose caused by the hydroxyl group of the cellulose is weakened (agglomeration relaxation effect), and in addition, the affinity with the resin is increased (affinity improvement effect) by the introduction of the carbamate group, which is more hydrophobic than the hydroxyl group, so that the resin and the microfiber cellulose are mutually entangled, and the microfiber cellulose is less likely to aggregate, and the role of resin reinforcement is surely fulfilled. On the other hand, when the substitution rate of the carbamate group is high, especially when it exceeds 2.0 mmol / g, the heat resistance of the composite resin is reduced. In this regard, when the cellulose fiber is subjected to heat, the detachment of the hydroxyl group usually occurs, and the molecular chain may become shorter starting from the point where the detachment occurs. And, when a part of the hydroxyl group is modified by carbamate conversion or the like, the detachment of the hydroxyl group occurs more easily. Therefore, if the substitution rate of the carbamate group is too high, the molecular chain becomes too short, the decomposition temperature drops, and the heat resistance is reduced. If the substitution rate of the carbamate group exceeds 2.0 mmol / g, the average fiber length of the pulp is shortened by carbamateizing the cellulose fiber, and as a result, the average fiber length of the microfiber cellulose tends to be less than 0.1 mm, and there is a risk that sufficient resin reinforcement effect will not be achieved. If the substitution rate exceeds 10.0 mmol / g, the cellulose fiber will not be able to maintain its fiber shape.
[0073] In this embodiment, the carbamate group substitution rate (mmol / g) refers to the amount of carbamate groups contained in 1 g of cellulose raw material having carbamate groups. The carbamate group substitution rate is calculated by measuring the N atoms present in the carbamate-treated pulp by the Kjeldahl method and calculating the carbamate rate per unit weight. Cellulose is a polymer with anhydroglucose as a structural unit, and has three hydroxyl groups per structural unit.
[0074] <Carbamate formation> Examples of methods for obtaining carbamate-treated microfibrous cellulose include a method in which a cellulose raw material is subjected to a carbamate reaction and then finely divided (fibrillated) to obtain carbamate-treated microfibrous cellulose, and a method in which the cellulose raw material is finely divided (fibrillated) and then subjected to a carbamate reaction to obtain carbamate-treated microfibrous cellulose. Here, the defibration of the cellulose raw material is explained first, and then the carbamate reaction (modification) is explained. However, either the defibration or the carbamate reaction may be carried out first. In particular, it is preferable to carry out the carbamate reaction first, and then defibration. This is because the cellulose raw material before defibration has a high dehydration efficiency, and the cellulose raw material is easily defibrated by the heating accompanying the carbamate reaction.
[0075] The process of carbamate-converting microfiber cellulose (which may be a cellulose raw material as mentioned above; the same applies below) can be mainly divided into, for example, a mixing process, a removal process, and a heat treatment. The mixing process and the removal process can be collectively referred to as a conditioning process for preparing a mixture to be subjected to a heat treatment. Carbamate-conversion also has the advantage that chemical modification can be performed without using an organic solvent.
[0076] In the mixing treatment, the microfiber cellulose or the like and urea or a derivative of urea (hereinafter simply referred to as "urea or the like") are mixed in a dispersion medium.
[0077] Examples of urea and urea derivatives that can be used include urea, thiourea, biuret, phenylurea, benzylurea, dimethylurea, diethylurea, tetramethylurea, and compounds in which the hydrogen atoms of urea are substituted with alkyl groups. These urea and urea derivatives can be used alone or in combination. However, it is preferable to use urea.
[0078] The upper limit of the mixture mass ratio of urea etc. to microfiber cellulose etc. (urea etc. / microfiber cellulose etc.) is preferably 20 / 100, more preferably 17 / 100, and even more preferably 15 / 100. On the other hand, the lower limit is preferably 3 / 100, more preferably 5 / 100, and even more preferably 7 / 100. By making the mixture mass ratio 3 / 100 or more, the efficiency of carbamate formation is improved. On the other hand, even if the mixture mass ratio exceeds 20 / 100, the carbamate formation is not further promoted.
[0079] The dispersion medium is usually water, although other dispersion media such as alcohols, ethers, and mixtures of water with other dispersion media may also be used.
[0080] In the mixing process, for example, microfibrous cellulose, etc. and urea, etc. may be added to water, microfibrous cellulose, etc. may be added to an aqueous solution of urea, etc., or urea, etc. may be added to a slurry containing microfibrous cellulose, etc. Furthermore, in order to mix uniformly, stirring may be performed after addition. Furthermore, the dispersion containing microfibrous cellulose, etc. and urea, etc. may contain other components. When the microfibrous cellulose, etc. is a sheet-shaped cellulose raw material, a method may be adopted in which the cellulose raw material is impregnated in a mixed liquid of urea, etc. and a dispersion medium and mixed. When the cellulose raw material is in a sheet shape, heat is easily transferred within the sheet, so that a lower heating temperature and a shorter heating time in the heat treatment can be expected.
[0081] In the removal treatment, the dispersion medium is removed from the dispersion liquid containing the microfibrous cellulose etc. and urea etc. obtained in the mixing treatment. By removing the dispersion medium, the urea etc. can be reacted efficiently in the subsequent heat treatment.
[0082] The dispersion medium is preferably removed by volatilizing it by heating, which makes it possible to efficiently remove only the dispersion medium while leaving behind the components such as urea.
[0083] When the dispersion medium is water, the lower limit of the heating temperature in the removal treatment is preferably 95°C, more preferably 100°C, and particularly preferably 105°C. By setting the heating temperature at 95°C or higher, the dispersion medium can be efficiently volatilized (removed). On the other hand, the upper limit of the heating temperature is preferably 140°C, more preferably 135°C, and particularly preferably 130°C. If the heating temperature exceeds 140°C, the dispersion medium and urea may react, and the urea may decompose independently.
[0084] The heating time in the removal treatment can be appropriately adjusted depending on the solid content concentration of the dispersion liquid, etc. Specifically, it is, for example, 6 to 24 hours.
[0085] In the heat treatment following the removal treatment, a mixture of the microfiber cellulose and urea is heat-treated. In this heat treatment, some or all of the hydroxyl groups of the microfiber cellulose react with urea and are replaced with carbamate groups. More specifically, when urea is heated, it is decomposed into isocyanic acid and ammonia as shown in the following reaction formula (1). Isocyanic acid is very reactive, and for example, carbamate groups are formed on the hydroxyl groups of cellulose as shown in the following reaction formula (2). NH2-CO-NH2→ HN=C=O + NH3…(1) Cell-OH + HN=C=O → Cell-O-CO-NH2 …(2)
[0086] The lower limit of the heating temperature in the heat treatment is the melting point of urea (about 134°C) or higher, more preferably 150°C, and particularly preferably 200°C. By setting the heating temperature at or above the melting point of urea, the urea becomes molten and easily comes into contact with the cellulose fibers, so that the carbamate formation is efficiently carried out. The upper limit of the heating temperature is preferably 300°C, more preferably 280°C, and particularly preferably 260°C. If the heating temperature exceeds 300°C, the microfiber cellulose etc. may decompose, and the reinforcing effect may become insufficient.
[0087] The lower limit of the heating time in the heat treatment is preferably 1 second, more preferably 5 seconds, and particularly preferably 10 seconds. By setting the heating time to 1 second or more, the carbamate reaction can be carried out reliably. On the other hand, the upper limit of the heating time is preferably 5 minutes, more preferably 3 minutes. If the heating time exceeds 5 minutes, it is not economical, and carbamate reaction can be carried out sufficiently in 5 minutes.
[0088] However, prolonged heating time leads to deterioration of cellulose fibers. Therefore, the pH conditions in the heat treatment are important. The pH is preferably 9 or more, more preferably 9 to 13, and particularly preferably 10 to 12, which is an alkaline condition. As a second best option, the pH is 7 or less, preferably 3 to 7, and particularly preferably 4 to 7, which is an acidic or neutral condition. Under neutral conditions of pH 7 to 8, the average fiber length of the cellulose fibers is shortened, and the reinforcing effect of the resin may be inferior. On the other hand, under alkaline conditions of pH 9 or more, the reactivity of the cellulose fibers is increased, the reaction with urea, etc. is promoted, and the carbamate reaction occurs efficiently, so that the average fiber length of the cellulose fibers can be sufficiently secured. On the other hand, under acidic conditions of pH 7 or less, the reaction of decomposing urea, etc. into isocyanic acid and ammonia proceeds, the reaction with cellulose fibers is promoted, and the carbamate reaction occurs efficiently, so that the average fiber length of the cellulose fibers can be sufficiently secured. However, if possible, it is preferable to perform the heat treatment under alkaline conditions. This is because acidic conditions may cause acid hydrolysis of cellulose to proceed.
[0089] The pH can be adjusted by adding an acidic compound (eg, acetic acid, citric acid, etc.) or an alkaline compound (eg, sodium hydroxide, calcium hydroxide, etc.) to the mixture.
[0090] As a heating device in the heat treatment, for example, a hot air dryer, a papermaking machine, a dry pulp machine, etc. can be used.
[0091] The mixture after the heat treatment may be washed. This washing may be performed with water or the like. By this washing, the unreacted remaining urea and the like can be removed.
[0092] (slurry) If necessary, the microfiber cellulose is dispersed in an aqueous medium to form a dispersion (slurry). The aqueous medium is particularly preferably entirely water, but an aqueous medium that is another liquid that is compatible with water can also be used. As the other liquid, lower alcohols having 3 or less carbon atoms can be used.
[0093] The solid content of the slurry is preferably 0.1 to 10.0% by mass, more preferably 0.5 to 5.0% by mass. If the solid content is less than 0.1% by mass, excessive energy may be required for dehydration or drying. On the other hand, if the solid content is more than 10.0% by mass, the fluidity of the slurry itself may decrease, and when a dispersant is used, the slurry may not be mixed uniformly.
[0094] (Resin powder) Depending on the storage conditions, microfiber cellulose may aggregate with other fibers, and once aggregated, it takes time to disperse them again. In order to suppress the aggregation of microfiber cellulose and to facilitate redispersion, it is a good idea to mix resin powder with the microfiber cellulose. If microfiber cellulose and resin powder are mixed together to form a mixture, the microfiber cellulose will remain dispersed and stable, making it less likely to aggregate. In particular, when microfiber cellulose is dried, it is prone to aggregation, so mixing with resin powder can suppress aggregation. Examples of resin powder that can be used include polyolefin resin, epoxy resin, styrene-based elastomer resin such as polystyrene, acrylonitrile-styrene resin (AS resin), acrylonitrile-butadiene-styrene resin (ABS resin), etc., and it is particularly preferable to use polyolefin resin.
[0095] As the polyolefin component, for example, one or more types selected from polymers of alkenes such as ethylene, propylene, butadiene, isoprene, etc., can be used. However, it is preferable to use a polypropylene resin, which is a polymer of propylene.
[0096] As the resin powder, an acid-modified resin powder in which a part of the main chain or side chain of the resin powder is substituted (modified) with an acid group can be preferably used. In the acid-modified resin powder, the acid group is ionic bonded to a part or all of the carbamate group of the microfiber cellulose. This ionic bond improves the reinforcing effect of the resin.
[0097] As the acid-modified resin powder, for example, polyolefin resin, epoxy resin, styrene-based elastomer resin, etc., each of which is substituted with an acid group, i.e., acid-modified polyolefin resin, acid-modified epoxy resin, acid-modified styrene-based elastomer resin, etc., can be used. Among these, it is preferable to use an acid-modified polyolefin resin. The acid-modified polyolefin resin is a copolymer of an unsaturated carboxylic acid component and a polyolefin component.
[0098] As the unsaturated carboxylic acid component, for example, one or more selected from maleic anhydrides, phthalic anhydrides, itaconic anhydrides, citraconic anhydrides, citric anhydrides, etc. can be used. However, it is preferable to use maleic anhydrides, and it is suitable to use maleic anhydride-modified polypropylene resin.
[0099] The resin powder to be mixed with the microfiber cellulose may be a mixture of an acid-modified resin powder and a non-acid-modified resin powder, or the entire amount of the resin powder may be an acid-modified resin powder, or the entire amount of the resin powder may be a non-acid-modified resin powder. When the acid-modified resin powder and the non-acid-modified resin powder are mixed, the amount of the non-acid-modified resin powder mixed is preferably 0 to 200 parts by mass, more preferably 1 to 100 parts by mass, and particularly preferably 10 to 70 parts by mass, relative to 100 parts by mass of the acid-modified resin powder.
[0100] The ratio of the average particle diameter of the resin powder to the average fiber diameter of the microfiber cellulose to be mixed (average particle diameter of the resin powder (μm) / average fiber diameter of the microfiber cellulose (μm)) is preferably 12 to 200, more preferably 25 to 100. If the ratio is less than 12, the resin powder is too small relative to the microfiber cellulose, so that the fibers may come into contact with each other during the drying process, and the effect of preventing aggregation due to the presence of the resin powder may not be exhibited. If the ratio exceeds 200, the resin powder is too large relative to the microfiber cellulose, so that the resin powder cannot enter between the fibers during the drying process, and the effect of preventing aggregation due to the presence of the resin powder may not be exhibited. In the case of the microfiber cellulose of this embodiment, the average particle diameter of the resin powder is preferably 1 to 2000 μm, more preferably 10 to 1500 μm, and even more preferably 100 to 1000 μm. If it is within this range, aggregation of the dried microfiber cellulose can be suppressed, which is preferable.
[0101] The weight average molecular weight of the maleic anhydride modified polypropylene is, for example, 1,000 to 100,000, and preferably 3,000 to 50,000.
[0102] The acid value of the maleic anhydride modified polypropylene is preferably 0.5 mgKOH / g or more and 100 mgKOH / g or less, and more preferably 1 mgKOH / g or more and 50 mgKOH / g or less.
[0103] Furthermore, the MFR (melt flow rate) of the acid-modified resin powder is preferably 2000 g / 10 min (190° C. / 2.16 kg) or less, more preferably 1500 g / 10 min or less, and particularly preferably 500 g / 10 min or less. If the MFR exceeds 2000 g / 10 min, the dispersibility of the cellulose fibers may decrease.
[0104] The acid value is measured in accordance with JIS-K2501 by titration with potassium hydroxide, and the MFR is measured in accordance with JIS-K7210 by placing a load of 2.16 kg at 190°C and measuring the weight of the sample that flows out in 10 minutes.
[0105] The resin powder used for mixing to disperse the microfiber cellulose and the resin pellets mixed when kneading the microfiber cellulose have different average particle diameters, and it is preferable that the resin powder has an average particle diameter smaller than that of the resin pellets. The resin powder and the resin pellets may use the same resin compound or different resin compounds.
[0106] (White pigment) A sheet dispenser processed using only resin as a raw material without including microfiber cellulose has a transparent or bluish transparent color, and may give the impression of not harmonizing with other furnishings when installed in a room together with other furnishings. In addition, the microfiber cellulose composite resin processed into the board constituting the sheet dispenser is opaque, depending on the thickness of the board, and has a pulp-derived amber color. This color blends in with other furnishings, household goods, and walls, for example, and gives a harmonious impression. To make it even more harmonious, it is recommended to process the dispenser using a microfiber cellulose composite resin containing a white pigment. In other words, if the board is formed of a microfiber cellulose composite resin having resin, microfiber cellulose, and a white pigment and is opaque, the appearance of the microfiber cellulose composite resin will have a stone-like texture, and will blend in better with other furnishings, household goods, and walls.
[0107] Before the microfiber cellulose is composited with the resin pellets, the microfiber cellulose may be dried so that the moisture content falls within a predetermined range. However, during drying, the cellulose may irreversibly aggregate due to hydrogen bonding, and the reinforcing effect of the fiber may not be fully exhibited. Therefore, by including a white pigment together with the microfiber cellulose, there is an advantage that the hydrogen bonding between the cellulose fibers in the microfiber cellulose is physically inhibited. In addition, by including a white pigment in the microfiber cellulose composite resin, the resin can also be reinforced.
[0108] When a white pigment is used, it is easy to form a composite with a matrix such as a resin. In addition, since the white pigment is a general-purpose inorganic material, there is an advantage that there are few limitations on the use. Furthermore, a white pigment is particularly preferable for the following reasons. When a white pigment is used, it is easy to control the size and shape of the powder to a constant value. Therefore, there is an advantage that the size and shape can be adjusted to match the size and shape of the cellulose fibers so that the effect of entering the gaps and suppressing the aggregation of the cellulose fibers can be easily achieved, and the effect can be easily pinpointed. In addition, even if fibers of various sizes are present in the slurry, there is an advantage that the white pigment can enter the gaps and suppress the aggregation of the cellulose fibers during the process of the fibers aggregating during the removal of the aqueous medium.
[0109] The white pigment can be added to the microfiber cellulose composite resin that has been kneaded once, and then heated and melted again to mix homogeneously, and then processed into the shape of a dispenser. Alternatively, the white pigment can be fed to a kneader together with the resin and the microfiber cellulose to be kneaded to obtain a microfiber cellulose composite resin containing the white pigment, which can then be processed into the shape of a dispenser.
[0110] Examples of white pigments that can be used include kaolin, clay, engineered kaolin, delaminated clay, heavy calcium carbonate, light calcium carbonate, talc, titanium dioxide, barium sulfate, calcium sulfate, zinc oxide, silicic acid, silicate salts, colloidal silica, satin white, etc. In particular, the microfiber cellulose composite resin obtained by mixing titanium dioxide has a color that combines the white color derived from titanium dioxide with the amber color and spots 41 derived from microfiber cellulose, so that even if a sheet dispenser processed with the composite resin is installed indoors, it blends in well with the surroundings and is unlikely to feel out of place.
[0111] The amount of the white pigment per part by mass of the microfiber cellulose is preferably 2.0 parts by mass or less, more preferably 0.01 to 1.5 parts by mass, and even more preferably 0.1 to 1.0 part by mass. If the ratio of the white pigment per part by mass of the microfiber cellulose exceeds 2.0 parts by mass, the spots 41 derived from the microfiber cellulose may become difficult to see, and the whiteness may become too strong.
[0112] The average particle size of the white pigment is preferably 0.01 to 10 μm, more preferably 0.05 to 5 μm, and particularly preferably 0.1 to 1 μm. If the average particle size exceeds 10 μm, the white color exhibited may become uneven, which may cause problems in appearance. On the other hand, if the average particle size is less than 0.01 μm, the finely divided white pigment particles may aggregate with each other, resulting in poor dispersion of the white pigment, which may cause unevenness in the white color exhibited, which may cause problems in appearance.
[0113] In this specification, the average particle size of the white pigment is a median diameter calculated from a volume-based particle size distribution measured by removing only the resin from a white pigment masterbatch in a masterbatch state with a resin using hot xylene or the like, and measuring the removed powder as it is or in the form of an aqueous dispersion using a particle size distribution measuring device (for example, a laser diffraction / scattering particle size distribution measuring device manufactured by Horiba, Ltd.).
[0114] (Kneading) The kneading is performed by supplying a mixture containing microfiber cellulose and resin powder to a kneader. Here, in order to adjust the blending amount of microfiber cellulose contained in the microfiber cellulose composite resin finally produced, it is preferable to add and supply resin pellets in addition to the mixture and knead them. The resin pellets to be kneaded preferably have an average particle diameter of 1 to 10 mm, more preferably 2 to 5 mm. If the average particle diameter is less than 1 mm, the resin may melt before reaching the kneading shaft in the kneader and adhere to the wall surface, etc., and the adhered resin may hinder the supply of subsequent resin pellets, and may not be quantitatively kneaded. Furthermore, the thermal conductivity between the resin pellets is poor, and a lot of energy is consumed until the resin pellets are melted. If the average particle diameter exceeds 10 mm, problems such as poor thermal conductivity between the resin pellets, a lot of energy is consumed until the resin pellets are melted, it is difficult to supply to the kneader, heat conduction is biased, and it takes a long time to melt may occur. The above-mentioned white pigment can be supplied to the kneader together with the mixture and the resin pellets.
[0115] The temperature of the kneading treatment is equal to or higher than the glass transition point of the resin pellets, and varies depending on the type of resin pellets, but is preferably 100 to 220° C., more preferably 130 to 210° C., and particularly preferably 160 to 200° C. In the kneading treatment, in addition to melting the resin pellets, the resin powder contained in the microfibrous cellulose solid material also melts.
[0116] For the kneading process, one or more of kneaders having a single kneading shaft or a multi-screw kneading extruder having two or more kneading shafts can be selected and used. Among these, it is preferable to use a multi-screw kneader having two or more shafts. Two or more multi-screw kneaders having two or more shafts may be used in parallel or in series.
[0117] As the resin for the resin pellets, it is preferable to use at least one of a thermoplastic resin and a thermosetting resin.
[0118] As the thermoplastic resin, one or more types can be selected from polyolefins such as polypropylene (PP) and polyethylene (PE), polyester resins such as aliphatic polyester resin and aromatic polyester resin, polystyrene (styrene resin), polyacrylic resins such as methacrylate and acrylate, polyamide resin, polycarbonate resin, polyacetal resin, acrylonitrile-styrene resin (AS resin), acrylonitrile-butadiene-styrene resin (ABS resin), etc., and can be used.
[0119] However, it is preferable to use any one of polyolefin and polyester resin, acrylonitrile-styrene resin (AS resin), acrylonitrile-butadiene-styrene resin (ABS resin), and polystyrene resin. As the polyolefin, it is preferable to use polypropylene. Furthermore, as the polyester resin, examples of aliphatic polyester resins include polylactic acid, polycaprolactone, etc., and examples of aromatic polyester resins include polyethylene terephthalate, etc., but it is preferable to use a biodegradable polyester resin (also simply called "biodegradable resin").
[0120] Examples of the thermosetting resin that can be used include phenol resins, urea resins, melamine resins, furan resins, unsaturated polyesters, diallyl phthalate resins, vinyl ester resins, epoxy resins, urethane resins, silicone resins, thermosetting polyimide resins, etc. These resins can be used alone or in combination of two or more.
[0121] The resin pellets may contain an inorganic filler, preferably at a ratio that does not interfere with thermal recycling. Examples of the inorganic filler include simple substances of metal elements in Groups I to VIII of the periodic table, such as Fe, Na, K, Cu, Mg, Ca, Zn, Ba, Al, Ti, and silicon, as well as oxides, hydroxides, carbonates, sulfates, silicates, and sulfites, and various clay minerals made of these compounds.
[0122] Specific examples include barium sulfate, calcium sulfate, magnesium sulfate, sodium sulfate, calcium sulfite, zinc oxide, silica, heavy calcium carbonate, light calcium carbonate, aluminum borate, alumina, iron oxide, calcium titanate, aluminum hydroxide, magnesium hydroxide, calcium hydroxide, sodium hydroxide, magnesium carbonate, calcium silicate, clay wollastonite, glass beads, glass powder, silica sand, silica stone, quartz powder, diatomaceous earth, white carbon, glass fiber, etc. A plurality of these inorganic fillers may be contained. Also, it may be one contained in waste paper pulp.
[0123] The blending ratio of the resin pellets to the microfiber cellulose is preferably 5.0 to 9.0 parts by mass, more preferably 5.5 to 8.5 parts by mass, and even more preferably 6.0 to 8.0 parts by mass, per part by mass of the microfiber cellulose. If the blending ratio is within the above range, the strength of the microfiber cellulose composite resin, particularly the bending strength and tensile modulus of elasticity, can be significantly improved, and the color inherent to the microfiber cellulose appears in the composite resin, making it harmonize with the interior.
[0124] The blending ratio of the microfiber cellulose and the resin contained in the finally obtained microfiber cellulose composite resin is usually the same as the blending ratio of the microfiber cellulose and the resin (resin powder and resin pellets).
[0125] In addition, the microfiber cellulose composite resin has improved strength due to the microfiber cellulose being dispersed in the resin, and the contribution to the improvement of strength is largely due to the physical properties of the microfiber cellulose rather than the physical properties of the resin itself. In other words, for the types of resin powders and resin pellets shown above, the resin strength can be expected to be improved by kneading at least the microfiber cellulose to form a composite resin.
[0126] Solubility parameters (cal / cm) of microfiber cellulose and resin 3 ) 1 / 2 The difference in (SP value) can be expressed as SP value difference=SPMFC value-SPPOL value, where SPMFC value of microfiber cellulose and SPPOL value of resin are used. The difference in SP value is preferably 10 to 0.1, more preferably 8 to 0.5, and particularly preferably 5 to 1. If the difference in SP value exceeds 10, microfiber cellulose may not disperse in the resin, and the reinforcing effect may not be obtained. On the other hand, if the difference in SP value is less than 0.1, microfiber cellulose dissolves in the resin, does not function as a filler, and the reinforcing effect cannot be obtained. In this regard, the smaller the difference between the SPPOL value of the resin (solvent) and the SPMFC value of the microfiber cellulose (solute), the greater the reinforcing effect.
[0127] The solubility parameter (cal / cm 3 ) 1 / 2 The SP value is a measure of the intermolecular force acting between a solvent and a solute, and the closer the SP values of the solvent and solute are, the greater the solubility.
[0128] (α-Olefin Copolymer) The microfiber cellulose composite resin of this embodiment may contain an α-olefin copolymer as appropriate. An α-olefin copolymer is a polymer in which an α-olefin (an olefin having a carbon-carbon double bond at the end) is copolymerized with a monomer such as ethylene or propylene, and contains an α-olefin with a long side chain. The microfiber cellulose composite resin containing this α-olefin copolymer has a polymer chain that is difficult to align, and is not crystallized or rigidified, so that unlike polyethylene or polypropylene, it can impart flexibility to the composite resin and improve the bending modulus.
[0129] Examples of α-olefins include linear units such as propylene, 1-butene, 1-pentene, 1-hexene, 4-methyl-1-pentene, 1-octene, 1-decene, 1-dodecene, 1-tetradecene, 1-hexadecene, 1-octadecene, and 1-eicosene, and cyclic units such as cyclopentene, cycloheptene, norbornene, 5-methyl-2-norbornene, tetracyclododecene, and 2-methyl-1,4,5,8-dimethano-1,2,3,4,4a,5,8,8a-octahydronaphthalene.
[0130] When the microfiber cellulose composite resin contains an α-olefin copolymer, the blending ratio of the α-olefin copolymer is preferably 15% by mass or less, more preferably 1 to 13% by mass, and particularly preferably 3 to 10% by mass, based on the total amount of the composite resin. If the blending ratio exceeds 15% by mass, the flexibility is excessively imparted, so that even if the compatibility with the fiber is high, the reinforcing effect of the fiber cannot be fully exerted, resulting in insufficient rigidity.
[0131] (Molding process) The microfiber cellulose composite resin, which is a kneaded product produced by kneading, can be molded into a desired shape after being kneaded again as necessary. The size, thickness, shape, etc. of this molded product are not particularly limited, and can be, for example, a sheet, pellet, powder, fiber, etc. The white pigment may be mixed when the microfiber cellulose composite resin produced by kneading is kneaded again.
[0132] The temperature during the molding process is equal to or higher than the glass transition point of the resin, and differs depending on the type of resin, but is, for example, 90 to 260°C, and preferably 100 to 240°C.
[0133] The kneaded material can be molded by, for example, mold molding, injection molding, extrusion molding, hollow molding, foam molding, etc. The kneaded material can also be spun into fibers and mixed with the above-mentioned plant materials to form a mat or board. The mixed fibers can be simultaneously deposited by air laying, for example.
[0134] As the apparatus for molding the kneaded product, for example, one or more types may be selected from an injection molding machine, a blow molding machine, a hollow molding machine, a blow molding machine, a compression molding machine, an extrusion molding machine, a vacuum molding machine, a pressure molding machine, etc., and may be used.
[0135] The above molding can be carried out following kneading, or the kneaded mixture can be cooled once and then chipped using a crusher or the like, and the chips can then be fed into a molding machine such as an extrusion molding machine or an injection molding machine.
[0136] Each part of the dispenser of this embodiment can be made of a microfiber cellulose composite resin. The microfiber cellulose composite resin is molded into the shape of each part by the above-mentioned molding machine. Each part is mainly plate-shaped, and spots 41 can be seen with the naked eye on the surface. The spots 41 are formed by agglomerates of microfiber cellulose aggregated by hydrogen bonding or entanglement, and are brown or black in color. The shapes of the spots 41 are different from each other. This is because the microfiber cellulose aggregates are aggregated to different sizes. Among the agglomerates scattered in the microfiber cellulose composite resin, those on the surface can be confirmed as spots 41.
[0137] If a composite resin containing cellulose fibers and resin is to be manufactured, it would seem that instead of microfiber cellulose, cellulose nanofibers, which have a shorter average fiber diameter than microfiber cellulose, or pulp, which has a longer average fiber diameter, could be used as the cellulose fibers. However, in a composite resin made of cellulose nanofiber and resin, the average fiber diameter of the cellulose nanofiber is relatively short, so that the spots 41 are difficult to see with the naked eye when processed into each part of the dispenser, and the cellulose nanofiber has a lighter amber color than the microfiber cellulose, and is transparent or nearly white-transparent, which may make it difficult to harmonize with other interior goods.
[0138] Furthermore, in a composite resin made of pulp and resin, no spots 41 visible to the naked eye are seen, and the color of the pulp is strongly expressed, resulting in an appearance different from that of the embodiments of the present invention, and there is a risk that the strength reinforcing effect will not be achieved.
[0139] However, this does not exclude the microfiber cellulose composite resin of the embodiment that does not contain either or both of cellulose nanofiber and pulp, and even a microfiber cellulose composite resin that contains either or both of cellulose nanofiber and pulp can be used in the dispenser of this embodiment as long as it has an appearance that harmonizes with other interior goods.
[0140] If the microfiber cellulose composite resin contains microfiber cellulose, the microfiber cellulose composite resin will have an amber-colored appearance and will have a stronger strength than the resin itself. In particular, the blending ratio of microfiber cellulose in the microfiber cellulose composite resin is preferably 1 to 20 mass%, more preferably 3 to 18 mass%, and even more preferably 5 to 15 mass%. With this blending ratio, the dispenser will have a bright amber color in appearance, giving an impression of harmony with other furnishings, and also improving the strength reinforcing effect.
[0141] In addition, while conventional dispensers are made of resin, the dispenser of the present invention has all or part of each part constituting the dispenser made of microfiber cellulose composite resin, and since the microfiber cellulose composite resin itself has high strength, the thickness of each part can be made thinner than that of conventional dispensers. Furthermore, since the dispenser of the present invention replaces part of the resin with microfiber cellulose, the amount of resin used can be reduced by preferably 1 to 15%, more preferably 3 to 12%, compared to conventional dispensers made only of resin, and is environmentally friendly.
[0142] The appearance of spots 41 formed on a plate made of microfiber cellulose composite resin is shown in Fig. 24. The spots 41 formed on a plate made of microfiber cellulose composite resin need only be visible to the naked eye, and the area of the spots 41 is not strictly limited. In addition, the area of the spots 41 per unit area of the plate is 0.1 mm 2 The number of the spots 41 that are 0.1 mm or more in area is not limited. 2 The number of spots 41 is preferably 10 to 12,000 per 100 cm of the plate. 2 , more preferably 20-6000 pieces / 100cm 2 , and more preferably 50 to 3000 pieces / 100 cm 2 Exists. Area 0.1mm 2 10 spots above 41 / 100cm board 2 If the number of spots is more than 12,000, the spots 41 are easily visible on the white resin dispenser, and the design is excellent. 2 If it is below this value, the spots 41 will be moderately noticeable against the white background, and the appearance will give a good impression.
[0143] Microfiber cellulose generally has a tendency to aggregate. This is because, microscopically, many hydroxyl groups on the surface of the cellulose fibers of the microfiber cellulose are hydrogen-bonded with hydroxyl groups of other microfiber cellulose, or aggregated by intermolecular forces acting between the microfiber cellulose. When trying to produce a microfiber cellulose composite resin with excellent strength, it is important to knead the microfiber cellulose with the resin in a state where it is as dispersed as possible. In this regard, the degree of dispersion of the microfiber cellulose is affected by the balance between the size of the microfiber cellulose and the size of the resin, the affinity between the microfiber cellulose and the resin, for example, the combination and blending ratio of the microfiber cellulose, the resin, and the white pigment, such as the fact that they are mutually hydrophobic, as well as by thoroughly mixing the mixture of the microfiber cellulose and the resin. On the other hand, cellulose nanofibers have a shorter average fiber diameter than microfiber cellulose, and therefore have a larger number of hydroxyl groups per unit surface area of the cellulose fibers. This means that cellulose nanofibers have more hydrogen bond points, and therefore cellulose nanofibers are more likely to aggregate by hydrogen bonding with each other. Therefore, even if cellulose nanofibers are mixed with resin, they are not as easily dispersed as microfiber cellulose, and even if they are made into a composite resin, localized unevenness in strength and color is likely to occur. Also, cellulose nanofiber aggregates formed by aggregating cellulose nanofibers have a smaller average diameter than microfiber cellulose aggregates, and are difficult to visually recognize as spots 41 with the naked eye when made into a composite resin.
[0144] The area per unit area of the plate is 0.1 mm 2 Number of spots 41 or more (number / 100cm board) 2 ) can be measured in accordance with JIS-P-8146. The area of each spot (41) is not particularly limited, but the upper limit is 2.0 mm 2 In this case, each spot is recognized as a dot rather than a pattern, and no regularity is seen in the scattering of the spots 41 as a whole on the board, which is aesthetically pleasing.
[0145] The density of the spots 41 can be adjusted by changing the blending ratio of the microfiber cellulose contained in the microfiber cellulose composite resin forming the dispenser.
[0146] The microfiber cellulose composite resin forming the dispenser of the present invention has a higher strength than a resin that is not composited. For example, when the resin is polypropylene, the bending modulus of the microfiber cellulose composite resin is 1.1 to 1.7 times higher than that of a resin that is not composited.
[0147] Furthermore, the flexural modulus of the microfiber cellulose composite resin forming the dispenser of the present invention is preferably 1.0 to 3.0 GPa, more preferably 1.5 to 2.8 GPa, if the resin is polypropylene.
[0148] The flexural modulus was measured at 23°C in accordance with JIS-K7171:2008.
[0149] (First embodiment) Next, an embodiment of a dispenser X1 of the present invention will be described in detail below with reference to FIGS.
[0150] The dispenser according to the present invention is a stationary, tabletop sheet dispenser X1 in which a case body 10 for storing a sheet stack 1 is supported at a predetermined height by a base portion 20 and used by placing it on a kitchen counter, a washbasin, a hand-washing area counter, a work counter, a floor, etc.
[0151] The sheet stack 1 targeted by the tabletop sheet dispenser X1 of the present invention (hereinafter, simply referred to as the dispenser X1) has a basis weight of 20 to 60 g / m 2A set of one or more rectangular sheets of approximately 100 mm in diameter are folded in half, stacked in a staggered manner with the edges of each folded piece positioned on the inner fold of the adjacent sheet above and below, and when the folded piece of the top or bottom one or more stacked pieces is pulled, the folded pieces of the adjacent sheets are pulled and pulled out due to friction specific to paper that the sheets have. This sheet stack 1 is generally produced by a folding machine called an interfolder, and is generally rectangular in shape, although there is some misalignment due to stacking. In the present invention, either the top or bottom surface of the stack of sheets 1 (hereinafter also referred to simply as a stack) from which the sheets are pulled out is referred to as the pull-out side 1A.
[0152] The dispenser X1 has a case body 10 composed of a front plate portion 11, a bottom plate portion 12, a back plate portion 13, a side plate portion 14, and a top plate portion 15, has a rectangular parallelepiped internal space 10A slightly larger than the size of the bundle 1, and has a roughly rectangular hexahedral box-like appearance. The dispenser X1 of the present invention is not limited to the appearance of the illustrated example, and may have any suitable design. However, from the viewpoint of space saving, the above-mentioned configuration of the case body 10 is desirable, and the following description will be based on the case body 10 in which the internal space composed of the above-mentioned plate portions is rectangular parallelepiped-shaped, and the appearance is roughly rectangular hexahedral-shaped.
[0153] In this form of dispenser X1, the case body 10 having the above-mentioned configuration is fixed to the base portion 20 at a predetermined height so that the front panel portion 11 constituting the front surface thereof is inclined forward, and accordingly the bottom panel portion 12 is inclined downward from the back panel portion side to the front panel portion side, so that the inner bottom surface 12A, which is the inner surface of the case body of the bottom panel portion 12, also inclines downward from the back panel side to the front panel side and is connected to the front panel portion 11.
[0154] The front plate 11 of the dispenser X1 in this embodiment has a width L1 of about 210 to 270 mm, a height L2 of about 70 to 140 mm, and is provided with a sheet outlet 16 in the center of the height direction, which opens in an elongated shape extending in the width direction. To take out a sheet, a part of the sheet exposed from the outlet 16 is picked up and pulled out downward, forward, or in a direction perpendicular to the front plate 11.
[0155] The back plate 13 of the case body 10 is positioned between the front plate 11 and the back plate 13 at an appropriate interval so that the stack 1 of sheets can be interposed therebetween, and the interval is about 80 to 150 mm in consideration of the thickness (height) of the commercially available stack 1. In the illustrated example, since the case body 10 has a rectangular parallelepiped shape, the back plate 13 is parallel to the front plate 11, i.e., inclined, but the back plate 13 does not necessarily have to be inclined, and for example, the back plate 13 may be inclined vertically or closer to vertical than the front plate 11. In addition, the dispenser X1 may be hinged to the bottom plate 12 or the side plate 14 via the hinge portion 19, and the back plate 13 may be a lid that can be opened and closed, so that the stack 1 can be placed in the case body by opening the back plate 13, as shown in particular in FIGS. 1 to 3. As shown in Fig. 4 and Fig. 5, the cover 15X may be integrated with the top plate 15 and a part 14A of the side plate 14, and a hinge 19 may be provided on the other part 14B of the side plate 14 to open and close freely. The hinge 19 for opening and closing the back plate 13 and the cover 15X may be achieved by a known technique such as a hinge, and is not particularly limited in the present invention. The dispenser X1 of this embodiment may be open on the back side without providing the back plate 13, as shown in Fig. 6.
[0156] On the other hand, the top plate 15 of the case body 10 is positioned with an appropriate gap between it and the bottom plate 12 so that the stack of sheets 1 can be interposed. In the illustrated example, the top plate inner surface 15A and the inner bottom surface 12A are parallel to each other, and the distance between them is slightly longer than the length between the folded edges 1B and 1C of the stack 1, so that when the stack is contained within the case body, the top plate inner surface 15A restricts the movement of the stack 1 toward the top plate. In this way, the free movement of the stack 1 in the vertical direction is restricted, making it more difficult for the stack 1 to collapse or fall over unintentionally within the case body.
[0157] On the other hand, the side plate portions 14 are located between the sides of the front plate portion 11 and the back plate portion 13, and are arranged at a predetermined interval to regulate the movement of the stack 1 stored inside the case body in the width direction, thereby contributing to smooth removal of sheets from the removal opening 16 and protecting the stack 1 from dirt such as dirty liquids, dust, and dirt. The side plate portions 14 may be arranged integrally with the side edges of the front plate portion 11 and the back plate portion 13 as shown in Fig. 1, or may be composed of two members 14A, 14B as shown in Fig. 4. However, the side plate portions 14 may be appropriately configured in consideration of the design and the like, as long as an internal space 10A capable of storing the stack 1 can be secured.
[0158] On the other hand, the dispenser X1 of this embodiment includes a pressing member 30 having a placing portion 31 on which a surface 1B of the bundle 1 stored in the case main body 10A where the folded edges are arranged is placed, and a pressing portion 32 that presses the back side surface 1D of the bundle 1 placed on the placing portion 31. The placing portion 31 may have any shape and configuration that allows the bundle 1 having a rectangular hexahedral shape to be stably placed, for example, a flat plate shape, a rod shape, or the like, and is arranged so as to extend in a direction from the front plate side toward the back plate side on the inner bottom surface 12A of the case main body 10A. The pressing portion 32 is formed, for example, so as to stand from the edge 31E of the back plate side of the placing portion 31 that extends in a direction from the front plate side toward the back plate side, or in the vicinity thereof, and is formed so as to be able to contact the back side surface 1D of the bundle 1 placed on the placing portion 31. The shape of the pressing portion 32 is not limited, but examples thereof include a flat plate shape, a rod shape, and the like. The pressing portion 32 is fixed to the placement portion 31. The pressing member 30 in the dispenser X1 shown in FIG. 1 has a shape shown in FIG. 7, and the placement portion 31 is composed of two elongated flat plates extending in a direction from the front plate portion side toward the back plate portion side along each side plate portion 14, 14 inside the case body 10A, and the pressing portion 32 is a flat plate of a rectangular parallelepiped shape having approximately the same size as or slightly larger than the back side surface 1D of the bundle 1, which is adhered to the back plate portion side edge 31E of the two elongated flat plates so as to stand from this edge 31E, and is configured such that the center portion is hollowed out and it contacts only the peripheral portion of the back side surface 1D of the bundle 1 placed on the placement portion 31. The pressing member is not limited to the shape shown in FIG. 7, and may have only one placement portion 31 as shown in FIG. 8. The shape of the pressing member 30 in this embodiment is not necessarily limited, but as shown in the example, a preferred example is one formed by assembling or bending a flat plate into an approximately L-shape or an approximately T-shape when viewed from the side, as this has a simple structure and is easy to manufacture.
[0159] On the other hand, the pressing member 30 is arranged by being placed on the inner bottom surface 12A of the case body 10A via the placement portion 31, and is movable in the front-rear direction (the direction connecting the front plate portion and the back plate portion in the figure) within the case body 10A. In the illustrated dispenser X1, the pressing member 30 is placed on the inner bottom surface 12A of the case body 10A via the placement portion 31, and both the inner bottom surface and the inner bottom surface side of the placement portion 31 are smooth, so that the friction between the inner bottom surface 12A and the placement portion 31 is small, and when the bundle 1 is placed on the placement portion 31 and the weight of the pressing member 30 itself, the inclination of the inner bottom surface 12A allows the pressing member 30 to slide toward the front plate portion. In addition, through holes 11B, 11B through which the placement portion 31 passes are formed near the connection portion of the front plate portion 11 with the inner bottom surface 12A, and the placement portion 31 of the pressing member 30 can move on the inner bottom surface so as to protrude outside the case body through the through holes 11B, 11B. As a result, in the dispenser X1, the pressing member 30 moves in the front-rear direction within the case body 10A, and in particular, the distance between the pressing portion 32 and the front plate inner surface 11A changes. Therefore, in the dispenser X1, when the stack 1 is placed on the placement portion 31 so as to be positioned between the pressing portion 32 of the pressing member 30 and the front plate inner surface 11A, as the thickness of the stack decreases with the drawing of the sheets from the take-out opening 16, the pressing member 30 moves on the inner bottom surface 12A and the placement portion 31 protrudes from inside the case body through the through hole 11B. At this time, the pressing state of the pressing portion 32 against the rear side surface 1D of the stack 1 is maintained by the movement of the pressing member 30. The shape of the through holes 11B, 11B is not limited, but is set to a size that does not allow the sheets to pass through easily. Of course, the shape of the through holes 11B corresponds to the shape of the placement portion 31.
[0160] In the dispenser X1 of this embodiment, the pressing member 30 on which the bundle 1 is placed moves in the case body 10A as the thickness of the bundle 1 decreases, and the pressing member 32 always presses the back side surface 1D of the bundle 1 due to the movement. That is, the bundle 1 is moderately sandwiched between the pressing member 32 and the front plate inner surface 11A. Furthermore, since the bundle 1 is not placed directly on the inner bottom surface 12A but is placed on the placing member 31 of the pressing member 30, the ease of movement of the placing member 31 relative to the inner bottom surface 12A can be easily adjusted, and the bundle 1 can always be effectively moved toward the front plate as the thickness of the bundle 1 decreases. Since the bundle 1 is moved in this way, it becomes possible to smoothly take out the bundle 1 from the take-out opening 16. Furthermore, since the pressing member 32 and the placing member 31 are integral, the pressing member 32 does not fall down in the case body 10A. Although not shown, the pressing member 30 may be provided with rollers or the like on the placement portion 31 so that the pressing member 30 can move smoothly on the inner bottom surface 12A by mechanical means.
[0161] 9, the protruding length of the placement portion 31 protruding from the through holes 11B, 11B formed in the front panel 11 of the dispenser X1 increases as the thickness of the stack inside the case body 10A from which the sheets have been pulled out decreases. Therefore, by making the protruding length of the placement portion 31 protruding from the front panel 11 visible and confirming it from the outside, it is possible to confirm the time to replenish the stack 1 even if the case body 10 is made of an opaque material so that the stack cannot be seen from the outside. Note that a mark for confirming replenishment may be attached to an appropriate position of the placement portion 31.
[0162] Here, in order to allow the pressing member 30 to move smoothly on the inner bottom surface 12A toward the front plate portion, the inner bottom surface 12A and the inner bottom surface of the placement portion 31 may be smoothed or coated with a lubricant. Also, guide rails or the like may be provided to improve the ease of sliding. The weight of the pressing member 30 is not particularly limited, but if it is too light, its effect as a pressing member is small, and if it is too heavy, the contact pressure between the drawer side surface 1A of the stack 1 and the front plate portion inner surface 11A becomes too high, making it difficult to draw out the sheets. The preferable weight is 30 to 80 g.
[0163] Furthermore, if the pressing portion 32 is hollowed out in the center as shown in Figures 7 and 8 so that it contacts only the peripheral edge of the rear side surface 1D of the stack 1, the load at the center will be reduced when the sheets are pulled out from the outlet 16, allowing the sheets to be pulled out smoothly, which is desirable (the hollowed out portion is indicated by the symbol 33 in the figures).
[0164] Here, the preferred inclination of the front plate 11 is such that when the dispenser X1 is placed on a horizontal surface, the inclination angle ∠A of the front plate 11 is 30 to 70 degrees with respect to the horizontal surface. The inclination angle ∠B of the placement portion 31 is preferably 20 to 60 degrees. If the inclination angle ∠A of the front plate 11 is less than 30 degrees, it is difficult to grasp the sheet and the hand is likely to touch the placement surface such as a workbench, making it difficult to effectively pull out the sheet. If it exceeds 70 degrees, it is difficult for the pull-out side surface 1A of the stack 1 to lean against the inner surface of the front plate. If the inclination angle ∠B of the placement portion 31 is 20 degrees or more, the pressing member 30 is likely to move smoothly on the inner bottom surface toward the front plate as the sheet is pulled out from the take-out opening 16. Note that the "inclination" and "angle" according to the present invention are based on the dispenser X1 being placed on a horizontal surface.
[0165] On the other hand, it is preferable that the take-out opening 16 is arranged so that the folded pieces of the sheets constituting the stack 1 are located near the take-out opening when the stack 1 is placed on the placement section. Although not necessarily required, as shown in FIG. 3, if an extension 17 is provided at the upper and lower edges of the take-out opening 16, which extends forward (outward) from the inner surface of the front plate 11 via a continuously smooth arc surface 17R or a curved surface, the sheets can be pulled out more smoothly along the arc surface 17R. If an extension 17 is provided, it is sufficient that it extends about 10 mm from the outer surface of the front plate. Furthermore, if a recessed missing portion 18 that is rectangularly missing downward is formed in the center of the width direction of the take-out opening 16, the center of the exposed portion of the sheets can be easily picked up. The shape of the recessed missing portion 18 is not limited to this rectangle, and may be, for example, a semicircle, a semiellipse, or the like.
[0166] Here, the case body 10 can be formed from a microfiber cellulose composite resin or the following materials. As the material, a suitable material can be selected from synthetic resin materials such as acrylic resin, AS resin, urea resin, ABS resin, polypropylene resin, etc.
[0167] As described above, the dispenser X1 allows the time to replenish the bundle 1 to be confirmed by the protrusion of the mounting portion 31 even if the case body 10 is made of an opaque material, but of course the case body 10 may be made all or partly transparent to be visible. By making the case body 10 transparent in this way, the state of the bundle 1 inside the case body can be better understood, and the appropriate time to replenish the bundle 1 can be confirmed. For example, if the top plate portion 15 and the side plate portions 14, 14 are made transparent, the state of the bundle 1 inside the case body 10 can be easily understood. However, the dispenser of this embodiment has the advantage that the time to replenish can be confirmed by the protrusion of the mounting portion 31, regardless of the presence or absence of a transparent portion as described above, even if the case body is formed of an opaque material, particularly a microfiber cellulose composite resin, from which the bundle inside cannot be seen in consideration of design.
[0168] When the case body 10 according to the embodiment of the present invention is made of a microfiber cellulose composite resin, each part constituting the case body 10 (front plate 11, bottom plate 12, back plate 13, lid 13, side plate 14, top plate 15, outlet 16, extension 17, placement portion 31, pressing portion 32, etc.) can be formed in a plate shape, and the thickness of the plate can be preferably 1 to 5 mm, more preferably 2 to 4 mm. In conventional tabletop sheet dispensers, the thickness of each part was thicker than that of the embodiment of the present invention. However, since the case body 10 according to the present invention is made of a microfiber cellulose composite resin and has high strength, it has sufficient strength even if the thickness of each part is made thinner than that of conventional products.
[0169] On the other hand, the base part 20 of the dispenser X1 of this embodiment is for supporting the case body 10 at a predetermined height while maintaining the inclination of the front panel part 11 and for allowing it to be placed on any surface such as a workbench. The shape of the base part 20 is not particularly limited. However, since the dispenser X1 is operated by grabbing a part of the exposed sheet from below the outlet 16, it is preferable that the base part 20 is shaped to support the case body 10 so that the height L4 of the outlet 16 is 90 to 140 mm when the dispenser is placed on the base part 20. If the height is 90 to 140 mm, a sufficient space can be secured below the outlet.
[0170] Also, the base 20 may be an integral structure with the case body 10 as shown in Figs. 1 and 4, or may be a separate body. For example, as shown in Figs. 10 and 11, if the base 20 is composed of two base side plates 21, 21 arranged in parallel with their lower edges as installation parts, a back plate 22 connecting the base side plates, and a support plate 23 on which the bottom plate part 12 of the case body 10 is placed, the front lower area of the case body 10 is widely opened, making it easier to pick up the sheet. In addition, in order to fix the case body 10 to the base 20, an appropriate fixing means such as an adhesive or a known locking structure can be used. In addition, when the front lower area is released in this way, the sheet exposed from the take-out opening 16 can be supported and lifted by the placement part protruding from the case body, making it easier to pick up.
[0171] The base 20 can be made of a microfiber cellulose composite resin or the following materials. The material can be selected appropriately from synthetic resin materials such as acrylic resin, AS resin, urea resin, ABS resin, polypropylene resin, etc. The lower surface of the base 20 may be provided with an appropriate anti-slip mechanism or fixing mechanism made of, for example, a rubber material or a magnet.
[0172] When the base portion 20 of the embodiment of the present invention is made of microfiber cellulose composite resin, each part constituting the base portion 20 (base side panel 21, back panel 22, support panel 23, etc.) can be formed in a plate shape, and the thickness of the plate can be preferably 3 to 5 mm, and more preferably 3 to 4 mm.
[0173] When a microfiber cellulose composite resin is used as a material for forming the case body 10 and / or the base 20, it may have resin, microfiber cellulose, and a white pigment, or may have resin and microfiber cellulose without a white pigment. In particular, a microfiber cellulose composite resin having resin, microfiber cellulose, and a white pigment is preferable because the color of the exterior blends in with the interior and has a stone-like texture, for example.
[0174] Fig. 16 shows a prototype of the dispenser X1 of the present invention. The case body 10 is made of a microfiber cellulose composite resin, and the base part 20 is made of a resin. Regardless of Fig. 16, the case body 10 may be made of a resin, the case body 10 may be made of a microfiber cellulose composite resin, or both the case body 10 and the base part 20 may be made of a microfiber cellulose composite resin.
[0175] The embodiment described above relates to the dispenser X1 in which the case body 10 is provided with the pressing member 30, but the dispenser X1' may be of another type in which the case body 10 does not have the pressing member 30.
[0176] FIG. 17 shows a prototype dispenser X1 of the first embodiment.
[0177] Second embodiment The dispenser X1' in which the case body 10 does not have the pressing member 30 has a similar form to the dispenser X1 described above, except for the absence of the pressing member 30. Below, the difference between the dispenser X1' in which the case body 10 does not have the pressing member 30 and the dispenser X1 in which the case body 10 is provided with the pressing member 30 will be described.
[0178] In the dispenser X1', the bundle 1 is placed on the inner bottom surface 12A. The orientation of the bundle 1 should be the same as that of the bundle 1 provided in the dispenser X1. The dispenser X1' does not need to have a through hole 11B. When one or a set of folded pieces at the top or bottom of the stack of the bundle 1 exposed from the outlet 16 is pulled out, the remaining bundle 1 shifts toward the front panel 11 by the thickness of the folded pieces. In addition, the dispenser X1' is lighter in weight because it does not have the pressing member 30. The dispenser X1' in which the case body 10 does not have the pressing member 30 can be in the form shown in Figures 12 to 15.
[0179] Third embodiment The sheet dispenser of the present invention may be a wall-mounted dispenser. A sheet dispenser X101 of a third embodiment will be described with reference to Figs. 17 to 23. Fig. 17 is a front view of the sheet dispenser of this embodiment, Fig. 18 is a cross-sectional view taken along line II-II, Fig. 19 is a side cross-sectional view of the case body, Fig. 20 is a front view of the case body, Fig. 21 is a top view of the sheet support, Fig. 22 is a front view of the sheet support, and Fig. 23 is a side cross-sectional view of the lid.
[0180] The sheet dispenser X101 is made of, for example, a resin or a microfiber cellulose composite resin, and is composed of a case body 101, a sheet support 102, and a lid 103. In the dispenser X101 of the third embodiment, each part forming the dispenser X101 is made of a plate. The plate may be formed of a resin or a microfiber cellulose composite resin. For example, the dispenser X101 may be formed entirely of a microfiber cellulose composite resin, the lid 103 may be formed of a microfiber cellulose composite resin, and the case body 101 and the sheet support 102 may each be formed of a resin, or the lid 103 and the sheet support 102 may be formed of a microfiber cellulose composite resin, and the case body 101 may each be formed of a resin.
[0181] The case body 101 has a top plate portion 110, a back plate portion 111, and a pair of left and right inner pieces 112, 112 extending forward at both side edges of the back plate portion 111 at a right angle to the back plate portion 111. A positioning hole 112A for fixing and positioning the sheet support 102 is formed in the lower part of the inner pieces 112, 112. The shape of the positioning hole 112A is not particularly limited. It may be a circular hole or a rectangular hole. In the illustrated example, a rectangular hole is used.
[0182] On the other hand, in the lower part of the inner pieces 112, 112, a locking long hole 112a corresponding to the positioning hole 112A is formed in addition to the positioning hole 112A in order to securely fix the sheet support 102. In this embodiment, two locking long holes 112a are formed in one inner piece so as to correspond to the positioning hole 112A. In the illustrated example, the locking long hole 112a is formed at a position spaced an appropriate distance above the positioning hole 112A. The shape of the locking long hole can also be changed as appropriate. Furthermore, in the lower part of the inner pieces 112, 112, a pair of lid body connecting circular holes 113A to which the lid body 103 is connected are formed in addition to the positioning holes etc. 112A for fixing the sheet support 102. In this embodiment, the lid body connecting circular hole 113A is formed in one inner piece so that the mounting position of the lid body 103 can be adjusted.
[0183] On the other hand, the sheet support 102 has a rear inclined surface 124 that slopes downward from the back plate side toward the front side, a front inclined surface 125 that slopes downward from the front plate side toward the rear side, and support side plates 126, 126 connecting the rear inclined surface 124 and the front inclined surface 125, and has a sheet take-out opening 120 between the lower edges of both the inclined surfaces 124, 125. Furthermore, the sheet support 102 of this embodiment has positioning protrusions 121 on the outer surfaces of the support side plates 126, 126, and this positioning protrusion 121 is fitted into the pair of positioning holes to be positioned at a predetermined position between the inner pieces. Furthermore, the sheet support 102 has a locking piece 122 separate from the positioning protrusion 121, and the positioning protrusion 121 is fitted into the positioning hole 112A, and the locking piece 122 is fitted into the locking long hole 112a, so that the sheet support 102 is fixed between the inner pieces 112, 112 of the case body 101. In this manner, the sheet support 102 is fixed to the inner pieces 112, 112 at the lower part of the case body 101, and constitutes the bottom of the dispenser X101. When the sheet support 102 is configured in this manner, due to the presence of the inclined surfaces 124, 125, during use, i.e., when sheets are drawn out one by one from the outlet 120, the lower edges of the lowermost sheet and the sheet above it are guided by the inclined surfaces 124, 125 to the outlet.
[0184] On the other hand, the sheet dispenser X101 of this embodiment has the upper edges of the rear inclined surface 124 and the front inclined surface 125, and further has a vertical surface 127 extending substantially vertically upward from the upper edges of the support side plates 126, 126, and this vertical surface 127 forms a square-shaped wall surface 127 that is open up and down. The sheet stack 1 is stored in the area surrounded by this square-shaped wall surface 127. This vertical surface 127 restricts the movement of the sheet stack 1 to the side, especially in the front-rear direction, so that when the sheet stack 1 is taken out from the outlet 120, it does not move unnecessarily inside the dispenser, and is one of the effects of stable take-out. In addition, the bent parts 124t, 125t between the inclined surfaces 124, 125 and the vertical surface 127 support the lower edge of the sheet stack 1 or its vicinity, and the accident of a large number of sheets being taken out at once during use, especially when the number of tissue sheets inside the dispenser is low, is significantly reduced. Furthermore, in the present embodiment, the inclined surfaces 124, 125 of the rear inclined surface 124 and the front inclined surface 125 are formed such that the steeply inclined surfaces 124A, 125A located on the upper side and the gently inclined surfaces 124B, 125B located on the lower side are continuous through the inclined curves 128, 128, as a preferred example. The angle between the steeply inclined surfaces 124A, 125A and the gently inclined surfaces 124B, 125B is preferably about 320 to 350 degrees. By forming the inclined surfaces 124, 125 of the front inclined surface 125 and the rear inclined surface 124 with two types of inclined surfaces in this way, the guide of the sheets is ensured to enable smooth drawing, while when the sheet stack 1 is taken out, several loose sheets on the lower side are supported by the other inclined curves 128, 128, and the accident of drawing out a large number of sheets at once during use, especially when the number of tissue sheets inside the dispenser is low, is further reduced.
[0185] On the other hand, the sheet support 102 has protrusions 129, 129 protruding inward from the support side plate 126. That is, the protrusions 129, 129 are located below the vertical surface 127. The protrusions 129, 129 are formed at this position to support the lower surface (the lower portion after use is started) of the stored sheet stack 1. In this embodiment, the protrusions 129, 129 are preferably shaped to extend downward from the top plate portion 110 side so that the protrusion length increases, and have convex portions 129t, 129t that protrude further inward at the lower end. With such a protrusion shape, the distance between the pair of protrusions protruding from the support side plate becomes narrower as it goes downward, so that the sheet stack 1 is supported in a curved state so that it is convex downward as it goes downward. This curvature makes the bottom sheet extremely easy to pick up from the take-out opening. In addition, it provides an appropriate resistance when the sheet stack is pulled out, allowing smooth pulling and effectively preventing the following sheets from being pulled out as a bundle. Furthermore, when the sheet stack 1 is stored, the load due to the weight of the sheet stack is reduced toward the bottom, so that the inclined surfaces 124, 125 guide the bottom sheet and the sheet above it more smoothly and reliably.
[0186] In addition, the upper surface of the protrusion in this embodiment is hemispherical. This allows the sheet to move smoothly to the outlet without getting caught when pulled out. However, it is preferable that the distance L1 between the protrusions 129, 129 and the rear inclined surface 124 and the front inclined surface 125 is 6 mm to 12 mm. If it is 6 mm or less, the distance to the outlet is too close, and the paper is likely to get caught on the protrusion when it is taken out, resulting in poor resistance to pulling out. If it is 12 mm or more, the gap between the outlet and the protrusion is too large, and the sheets are likely to fall in a stack when the number of remaining sheets is low.
[0187] On the other hand, the sheet support 102 of this embodiment has the outlet 120 located between the front inclined surface 125 and the rear inclined surface 124, and is configured with an elongated portion 120L extending parallel to the back plate portion and the front plate portion, and a recessed portion 120V that is continuous with the elongated portion at the center of the sheet support and recessed in an approximately trapezoidal shape toward the upper surface side. The shape of the recessed portion is not limited to an approximately trapezoidal shape, but this shape is preferable because it is easy to realize the effects of the present invention. The upper edge of either the front side or the rear side recessed portion is located on a vertical surface that continues to the inclined surface. It is preferable that the upper edge of the front side recessed portion is located on a vertical surface that continues to the front side inclined surface. The stacked surface of the sheet stack 1 placed on the sheet support 102 is exposed from the recessed portion. By forming the recessed portion in this way, the stacked surface of the sheet stack 1 can be touched, making it easier to pick up the first sheet when starting to use it. Furthermore, the side portions are not pressed down excessively, and this, combined with the aforementioned flexure, allows for smoother pull-out, and the risk of the drawers being pulled out in a bundle is significantly reduced.
[0188] On the other hand, the lid 103 has a top plate 130, a front plate 131, and outer pieces 132, 132 extending toward the rear side at right angles to the front plate 131 on both side edges of the front plate 131, and the bottom side is open. The height of the front plate 131 is slightly higher than the back plate 111 of the case body 101, and the space between the outer pieces 132, 132 is formed slightly wider than the space between the inner pieces 112, 112 of the case body 101. Furthermore, the lid 103 has protrusions 133, 133 formed on the lower part of the outer pieces 132, 132 and protruding toward the opposing lid side pieces, and these protrusions 133, 133 are rotatably fitted into the pair of lid connecting circular holes 113A of the case body 101 from the outer side of the inner pieces, so that the lid can be opened and closed with respect to the case body 101 around the protrusions. Furthermore, the center of the lower edge 131e of the front plate of the lid is curved toward the upper edge, making it easier to pick up a sheet from the opening and easier to touch the stacked surface of the sheet stack exposed from the recess, making it easier to pull out the first sheet. The uppermost position of this curved edge is located below the lower edge of the vertical surface of the sheet support, i.e., the boundary with the inclined surface. Therefore, the end surface is not exposed when viewed from the front, preventing water splashes, dust, etc. from adhering to the end surface, ensuring the hygiene of the following sheets that are not yet used. It also has excellent design.
[0189] On the other hand, in the sheet dispenser X101 of this embodiment, a rear guide rib 115 protruding toward the front side is formed on the surface of the back plate portion 111 facing the front plate portion 131, and a front guide rib 135 protruding toward the rear side is formed on the surface of the front plate portion 131 facing the back plate portion 111. In this embodiment, the rear guide ribs 115 are arranged so that there are two of them, one each at a position spaced a predetermined distance from each of the inner pieces 112, 112, and the front guide ribs 135 are also arranged so that there are two of them, one each at a position spaced a predetermined distance from each of the outer pieces 132, 132. However, the number of each guide rib is not limited to this. In addition, the rear guide rib 115 and the front guide rib 135 do not need to be formed at positions facing each other when the lid body 103 is closed. These guide ribs 115, 135 are configured so that their protruding length increases proportionally from the upper side of the case toward the sheet support 102 side, and due to the presence of these ribs, the load of the weight of the sheet bundle 1 on the upper surface of the sheet support 102 when the sheet bundle 1 is stored is reduced, and the guide of the bottom sheet and the sheet one sheet above it by the inclined surfaces 124, 125 becomes smoother and more reliable. Also, these guide ribs 115, 135 are characteristically configured so that their protruding tips protrude further inward of the dispenser than the vertical surfaces 127, 127, that is, toward the opposing front plate portion or back plate portion. By protruding in this manner, the weight of a part of the sheet bundle 1 between the guide ribs is less likely to be applied to a part of the sheet bundle 1 that has passed through the guide ribs 115, 135 and moved between the vertical surfaces 127, 127, and thus the smooth drawing mechanism of the sheet support described above and the function of preventing the sheets from being drawn out in a bundle are effectively exhibited. Here, the height of the guide ribs may be appropriately designed according to the amount of sheets to be piled up, that is, the amount of sheets to be stored. Generally, 1 to 30 cm is sufficient. EXAMPLES
[0190] A test piece was manufactured to be the plate that would form the dispenser, and the bending modulus and the presence or absence of spots were evaluated. The microfiber cellulose used had an average fiber diameter of 14 μm and an average fiber length of 0.38 mm. The microfiber cellulose was made from pulp with a lignin content of 0.1%.
[0191] (Test Examples 1 and 2) 46.4g of maleic anhydride modified polypropylene (MAPP) powder was added to 2650g of microfiber cellulose with a solid content concentration of 3.5% by mass to form a mixture, which was then dried in a dryer heated to 130°C and compressed with a compressor (TS-55, manufactured by Tosa Tech Co., Ltd.) to obtain a compressed solid (microfiber cellulose compressed solid) formed of resin and microfiber cellulose. The microfiber cellulose compressed solid was kneaded in a twin-screw kneader at 180°C and 200 rpm to obtain a microfiber cellulose composite resin master batch. The obtained microfiber cellulose composite resin master batch was dry-blended with polypropylene pellets and α-olefin copolymer (Tafmer DF640, manufactured by Mitsui Chemicals, Inc.) in a predetermined ratio, and then kneaded in a twin-screw kneader at 180°C and 200 rpm to obtain a microfiber cellulose composite resin. The microfiber cellulose composite resin was cut into cylindrical shapes with a diameter of 2 mm and a length of 2 mm using a pelleter, and then injection molded into rectangular specimens (length 59 mm, width 9.6 mm, thickness 3.8 mm) at 180°C. The blending ratios of polypropylene pellets, α-olefin copolymer, and microfiber cellulose were adjusted to be as shown in Table 1.
[0192] (Test Examples 3 to 6) Test Examples 3 to 6 were produced in the same manner as Test Example 1, except for the following points. A titanium oxide master batch as a white pigment and polypropylene pellets were added to the same compressed solid as Test Example 1, and kneaded in a twin-screw kneader under conditions of 180°C and 200 rpm to obtain a microfiber cellulose composite resin master batch. The blending ratios of the polypropylene pellets, α-olefin copolymer, microfiber cellulose, and titanium oxide master batch were adjusted to be as shown in Table 1.
[0193] (Test Examples 7 and 8) Polypropylene pellets, α-olefin copolymer, and titanium oxide master batch were dry blended in a specified ratio and kneaded in a twin-screw kneader at 180°C and 200 rpm to obtain a composite resin. The composite resin was cut into cylindrical shapes with a diameter of 2 mm and a length of 2 mm using a pelletizer, and injection molded into rectangular test pieces (length 59 mm, width 9.6 mm, thickness 3.8 mm) at 180°C. The blending ratio of polypropylene pellets and titanium oxide master batch was adjusted to be as shown in Table 1.
[0194] The presence or absence of spots was evaluated as follows. The area per unit area of the test piece is 0.1 mm 2 The number of spots exceeding 10 / 100cm 2 If it was above that, it was marked as "◎". Although spots can be confirmed on the test piece, the area per unit area is less than 0.1 mm 2 The number of spots exceeding 10 / 100cm 2 If it was less than this, it was marked as “O”. The test piece in which no spots were observed was marked "X".
[0195] The results are shown in Table 1. [Table 1] [Explanation of symbols]
[0196] X1...desktop sheet dispenser, X1'...desktop sheet dispenser, 1...sheet stack, 1A...drawer side of sheet stack, 1B...surface where the folded edges are lined up and that contacts the placement portion, 1C...surface where the folded edges are lined up and that does not contact the placement portion, 1D...rear side which is the opposite side to the drawer side of the sheet stack, 10...case body, 10A...internal space of the case body (or inside the case body), 11...front plate portion, 11A...inner surface of the front plate portion (surface where the drawer side of the stack abuts), 11B...through hole, 12...bottom Plate portion, 12A... inner bottom surface (inner surface of bottom plate portion), 13... back plate portion, lid portion, 14, 14A, 14B... side plate portion, 15... top plate portion, 15X... lid portion, 15A... inner surface of top plate portion, 16... outlet, 17... extension portion, 17R... arc surface of extension portion, 18... recessed portion, 19... hinge portion, 20... base portion, 21... base side plate, 22... rear plate, 23... support plate, 30... pressing material, 31... placement portion, 31E... edge of placement portion on back plate side, 32... pressing portion, 41... spots, L1... width of front plate portion, L2... height direction length of front plate portion, L3... extent of non-slip portion periphery, L4...height of outlet, ∠A...inclination angle of front plate, ∠B...inclination angle of placement surface, 101...case body, 102...sheet support, 103...lid, 110...top plate, 11...back plate, 112...inner piece, 112A...positioning hole, 112a...long hole for locking, 113A...circular hole for connecting lid, 115...rear guide rib, 115t...projecting end of rear guide rib, 120...outlet, 120L...elongated portion, 120V...recess, 120e...upper edge of recess, 121...positioning protrusion, 122...locking piece, 124... rear inclined surface, 125...front inclined surface, 124A, 125A...upper steep slope, 124B, 125B...lower gentle slope, 124t, 125t...bent portion, 126...support side panel, 127...vertical surface (vertical wall), 128...curve, 129...protrusion, 129t...lower convex portion of protrusion, 130...top panel, separation distance, 131...front panel, 131e...lower edge of front panel, 132...outer piece, 133...protrusion, 135...front guide rib, 135t...protruding end of front guide rib, X101...sheet dispenser.
Claims
1. A sheet dispenser for storing a stack of substantially rectangular parallelepiped sheets, the stack being made by stacking a plurality of rectangular sheets folded in half in a staggered manner such that the edges of the folded pieces are positioned on the inner fold surfaces of adjacent sheets, the stack comprising: The sheet dispenser comprises: The plate is made of a microfiber cellulose composite resin having a resin and microfiber cellulose having an average fiber diameter of 1 to 19 μm, and spots made of the microfiber cellulose are formed on the plate. A sheet dispenser characterized by:
2. The device has a case body for storing a stack of substantially rectangular parallelepiped sheets, the stack being formed by stacking a plurality of rectangular sheets folded in half in a staggered manner with the edges of the folded pieces positioned on the inner folds of the adjacent sheets, a base portion for making the case body a tabletop type, and an outlet provided in the case body for pulling out the sheets, The case body and / or the base portion are The plate is made of a microfiber cellulose composite resin having a resin and microfiber cellulose having an average fiber diameter of 1 to 19 μm, and spots made of the microfiber cellulose are formed on the plate. A sheet dispenser characterized by:
3. The plate is formed of a microfiber cellulose composite resin having the resin, the microfiber cellulose, and a white pigment, and is opaque.
3. A sheet dispenser according to claim 1 or 2.
4. The area per unit area of the plate is 0.1 mm 2 The number of spots exceeding this limit is 10 to 12,000 per 100 cm of board. 2 This is what happens:
3. A sheet dispenser according to claim 1 or 2.
5. The microfibrous cellulose has a modified microfibrous cellulose in which all or a part of the hydroxyl groups are replaced with carbamate groups.
3. A sheet dispenser according to claim 1 or 2.
6. The thickness of the plate is 1 to 5 mm.
3. A sheet dispenser according to claim 1 or 2.
7. The flexural modulus of the microfiber cellulose composite resin is 1.0 to 3.0 GPa; 3. A sheet dispenser according to claim 1 or 2.
8. The microfiber cellulose has a lignin content of 1% or less in the raw pulp.
2. The sheet dispenser of claim 1.
9. The microfiber cellulose composite resin has a blending ratio of microfiber cellulose in the microfiber cellulose composite resin of 1 to 20% by mass.
2. The sheet dispenser of claim 1.
Citation Information
Patent Citations
Paper towel dispenser and method of taking out paper towel sheet
JP1994144448A
Towel paper holder
JP2001087161A
Paper holder
JP2006204404A
Sheet feeding unit
JP2007153439A
Sanitary thin paper dispenser
JP2010076811A
Cited By
Sheet dispenser
WO2026004527A1