Touch roller, take-up device and laminate film

The touch roller with convex portions addresses the challenge of air bubbles in solvent-free lamination by ensuring uniform pressure across plain areas, improving laminate film appearance through enhanced bubble removal.

JP2024153161AInactive Publication Date: 2024-10-29TOPPAN HOLDINGS INC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023066881
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-17
Publication Date
2024-10-29
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Solvent-free lamination processes face challenges in removing air bubbles due to the high viscosity of the adhesive, leading to poor appearance in areas without printed patterns, as conventional touch rollers struggle to follow the level difference between printed and plain areas.

Method used

A touch roller with convex portions on its surface that protrude from other areas, designed to press against the plain areas of laminate films, ensuring uniform pressure and effective bubble removal, combined with a winding device that uses this roller to improve laminate film quality.

Benefits of technology

The convex touch roller effectively reduces air bubbles in plain areas, enhancing the appearance of laminate films laminated with solvent-free adhesives by promoting uniform pressure and adherence to the take-up roll.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024153161000001_ABST
    Figure 2024153161000001_ABST
Patent Text Reader

Abstract

To provide a touch roller, a take-up device and a laminate film that can improve poor external appearance of the laminate film which is laminated with a solventless adhesive.SOLUTION: A touch roller 5 is configured to press a laminate film 2 against a take-up roll 4 in a take-up device 1 for conveying the laminate film 2 in a length direction D and taking it up around the take-up roll 4, the laminate film having: a first film 21; a print part 22 formed on a part of the first film 21; a second film 24 arranged on the side of the print part 22 of the first film 21, and a solventless adhesive layer 23 arranged between the first film 21 and second film 24. Then a roller surface 51 which comes into contact with the laminate film 2 has a projection part 52 protruding more than other regions. The projection part 52 is provided on at least a part of a plain contact surface 54 brought into contact with a whole-area plain region 26 of the laminate film 2 where the print part 22 is not formed in the whole area in the length direction D.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a touch roller, a winding device, and a laminate film. [Background technology]

[0002] Packaging for everyday items such as food and cosmetics, as well as industrial items, is diverse, and there are many types of print patterns, which change daily. However, in many cases, the entire surface is not printed, and plain areas are often used to create transparent areas. In the lamination process, the laminate film is wound around a winding roll, but in such a lamination process, the plain areas may float after being wound around the winding roll, and since no pressure is applied to the areas, lamination may be defective. Therefore, the quality of the laminate film is generally improved by pressing the laminate film wound around the winding roll with a touch roller. General touch rollers are often made of flat rubber or iron, and Patent Document 1 shows a touch roller with grooves formed on the surface. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Japanese Utility Model Application Publication No. 62-063248 Summary of the Invention [Problem to be solved by the invention]

[0004] In recent years, solventless lamination, which uses solventless adhesives to laminate, has become common in order to be environmentally friendly. However, because solventless adhesives have high viscosity, air bubbles contained in the adhesive are difficult to remove during the lamination process, and these air bubbles can cause poor appearance.

[0005] In such solventless lamination, the removal of air bubbles can be promoted by using a touch roller. However, with a general touch roller, it is difficult to make it conform to the step between the printed part and the plain part, so it is difficult to remove air bubbles from the plain part. Even with the touch roller described in Patent Document 1, it is difficult to make it conform to the step between the printed part and the plain part, so it is difficult to remove air bubbles from the plain part. For this reason, it does not lead to improvement of poor appearance in the plain part.

[0006] The present disclosure has been made to solve such problems, and aims to provide a touch roller, a winding device, and a laminate film that can improve the poor appearance of a laminate film laminated with a solvent-free adhesive. [Means for solving the problem]

[0007] The present disclosure provides the following [1] to [8].

[0008] [1] A winding device that transports a long laminate film having a first film, a printed portion formed on a portion of the first film, a second film arranged on the side of the printed portion of the first film, and a solvent-free adhesive layer arranged between the first film and the second film in a longitudinal direction of the laminate film and winds it up onto a winding roll, the touch roller pressing the laminate film against the winding roll, wherein the roller surface that contacts the laminate film has a convex portion that protrudes more than other areas, and the convex portion is provided on at least a portion of the plain contact surface that contacts the entire plain area of ​​the laminate film where the printed portion is not formed over the entire longitudinal area of ​​the touch roller.

[0009] In this touch roller, the roller surface that contacts the laminate film has a protruding portion that protrudes from other regions, and this protruding portion is provided on at least a part of the plain contact surface that contacts the entire plain region of the laminate film, which has no printed portion formed over the entire longitudinal area. Therefore, the protruding portion penetrates into the entire plain region, increasing the pressure that presses the entire plain region against the winding roll, facilitating the removal of air bubbles from the entire plain region. This makes it possible to improve the appearance defects of the laminate film laminated with a solventless adhesive.

[0010] [2] The touch roller according to [1], wherein the convex portions are provided over the entire circumferential area of ​​the touch roller. In this touch roller, the convex portions are provided over the entire circumferential area of ​​the touch roller, which further promotes the removal of air bubbles from the entire plain area.

[0011] [3] The touch roller according to [1] or [2], wherein the convex portions extend in the circumferential direction of the touch roller. In this touch roller, the convex portions extend in the circumferential direction of the touch roller, which makes it possible to easily provide the convex portions and efficiently remove air bubbles from the entire plain region.

[0012] [4] The touch roller according to any one of [1] to [3], wherein the protruding height of the convex portions on the roller surface is from 1 μm to 2 mm. In this touch roller, since the protruding height of the convex portions on the roller surface is from 1 μm to 2 mm, air bubbles can be effectively removed from the entire plain region and the convex portions can be easily provided.

[0013] [5] The touch roller according to any one of [1] to [4], wherein the convex portions have elasticity. In this touch roller, the convex portions have elasticity, so that the convex portions are easily deformed to conform to the step between the entire plain area and the printed area, and are easily pressed against the winding roll.

[0014] [6] The touch roller according to any one of [1] to [5], wherein the protrusions have a durometer hardness, measured in accordance with JIS K6253, of 30 or more and 80 or less. In this touch roller, the protrusions have a durometer hardness of 30 or more and 80 or less, which makes it easier for the protrusions to press the entire plain region against the winding roll while suppressing deterioration of the protrusions.

[0015] [7] A winding device comprising: a conveying device that conveys a long laminate film having a first film, a printed portion formed on a portion of the first film, a second film arranged on the printed portion side of the first film, and a solventless adhesive layer arranged between the first film and the second film in a longitudinal direction of the laminate film, a winding roll on which the laminate film is wound, and the touch roller according to any one of claims 1 to 6 that presses the laminate film against the winding roll. Since this winding device is provided with the above-mentioned touch roller, it is possible to improve poor appearance of the laminate film laminated with a solventless adhesive.

[0016] [8] A long laminate film having a first film, a printed portion formed on a portion of the first film, a second film disposed on the side of the printed portion of the first film, and a solventless adhesive layer disposed between the first film and the second film, the laminate film having a plain region in which the printed portion is not formed over the entire length of the laminate film, and an air bubble area ratio in the plain region is 0% or more and 1.8% or less. This laminate film is laminated with a solventless adhesive, and has a plain region in which the printed portion is not formed over the entire length of the laminate film, but the air bubble area ratio in the plain region is 0% or more and 1.8% or less, so that the appearance defect can be improved. Effect of the Invention

[0017] According to the present disclosure, it is possible to improve the poor appearance of a laminate film laminated with a solvent-free adhesive. [Brief description of the drawings]

[0018] [Figure 1] FIG. 1 is a schematic cross-sectional view showing one embodiment of a winding device according to the present disclosure. [Diagram 2] FIG. 2 is a schematic plan view showing one embodiment of the laminate film of the present disclosure. [Diagram 3] FIG. 3 is a schematic cross-sectional view taken along line III-III shown in FIG. [Figure 4] FIG. 4 is a schematic plan view showing the relationship between the laminate film and the touch roller shown in FIG. [Diagram 5] FIG. 5 is a schematic plan view showing a part of a modified touch roller. [Figure 6] FIG. 6 is a schematic plan view showing a part of a modified touch roller. [Figure 7] FIG. 7 is a schematic development of the roller surface of a modified touch roller. [Figure 8] FIG. 8 is a schematic development of the roller surface of a touch roller according to a modified example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] Hereinafter, embodiments of the present disclosure will be described in detail with reference to the drawings. In the following description, the same or corresponding elements are denoted by the same reference numerals, and duplicated description will be omitted.

[0020] <Take-up device> FIG. 1 is a schematic cross-sectional view showing one embodiment of a winding device of the present disclosure. The winding device 1 shown in FIG. 1 is a device for winding a long laminate film 2. The winding device 1 includes a conveying device 3 that conveys the laminate film 2 in the longitudinal direction D of the laminate film 2, a winding roll 4 on which the laminate film 2 is wound, and a touch roller 5 that presses the laminate film 2 against the winding roll 4. The conveying device 3 is, for example, composed of a pair of rollers that sandwich the laminate film 2, a driving device that rotates the rollers, and a driving device that rotates the winding roll 4. The winding roll 4 is a rotatable columnar or cylindrical member, and is configured to rotate to wind the laminate film 2. The touch roller 5 is a rotatable columnar or cylindrical member, and is configured to press the laminate film 2 against the winding roll 4 while rotating.

[0021] <Lamination film> FIG. 2 is a schematic plan view showing one embodiment of the laminate film of the present disclosure. FIG. 3 is a schematic cross-sectional view taken along line III-III shown in FIG. 2. As shown in FIGS. 2 and 3, the laminate film 2 is a laminate having a first film 21, a printed portion 22 formed on a portion of the first film 21, a second film 24 disposed on the printed portion 22 side of the first film 21, and a solvent-free adhesive layer 23 disposed between the first film 21 and the second film 24. That is, the laminate film 2 is a laminate in which the second film 24 is laminated to the printed portion 22 side of the first film 21, on which the printed portion 22 is formed on a portion of the first film 21, by a solvent-free adhesive that becomes the solvent-free adhesive layer 23. The region in which the printed portion 22 is not formed is called a plain portion 25.

[0022] As the first film 21, for example, a film for general packaging such as polyethylene terephthalate, polypropylene, polyamide, etc. may be used. The first film 21 may be provided with a barrier layer having water vapor barrier properties or oxygen barrier properties for the purpose of extending the expiration date of food, etc. Examples of such a barrier layer include vacuum deposition, polyvinyl alcohol, polyvinylidene chloride (PVDC), etc. As the first film 21, for example, a film manufactured and sold as a barrier film may be suitably used. Examples of such a barrier film include films with a processed barrier layer such as GL-AE and GL-ARH manufactured by Toppan Printing Co., Ltd.

[0023] The printed portion 22 is an ink layer formed by one or more inks. The printed portion 22 can be processed using ink materials used for general-purpose food packaging. For example, Riogran manufactured by Toyo Ink Mfg. Co., Ltd., Bellcolor manufactured by Sakata Inx Corporation, etc. can be used as the printed portion 22. The height of the printed portion 22 relative to the first film 21 is, for example, 0.5 μm or more and 10 μm or less. The height of the printed portion 22 relative to the first film 21 is the step between the first film 21 and the printed portion 22, that is, the step between the plain portion 25 and the printed portion 22.

[0024] The solvent-free adhesive layer 23 is a cured product of a solvent-free adhesive. That is, the solvent-free adhesive layer 23 is a cured product of a solvent-free adhesive that laminates the second film 24 to the first film 21. The solvent-free adhesive is an adhesive that does not contain an organic solvent. The fact that the adhesive layer is formed using a solvent-free adhesive rather than a solvent-based adhesive can be analyzed, for example, by Fourier transform infrared spectroscopy. Examples of the solvent-free adhesive include an adhesive that contains a polyisocyanate component and a polyol component and does not contain an organic solvent or water. The polyisocyanate component and the polyol component are each prepared in advance in appropriate amounts, and then mixed at the time of use.

[0025] As the second film 24, for example, a polyamide film, a PET (polyethylene terephthalate) film, an ethylene vinyl alcohol film, an aluminum-deposited CPP (non-oriented polypropylene) film, or the like can be used.

[0026] The laminate film 2 has an entire plain region 26 in which no printed portion 22 is formed across the entire length in the longitudinal direction D. In other words, the entire plain region 26 is a region that has the same width and extends in the longitudinal direction D, and is a region in which no printed portion 22 is formed. The laminate film 2 shown in FIG. 2 has two entire plain regions 26.

[0027] In the entire plain region 26, air bubbles are difficult to remove due to the step between the plain part 25 and the printed part 22, but the air bubble area ratio is set to 0% or more and 1.8% or less by pressing the laminate film 2 against the winding roll 4 by the touch roller 5. In this case, the air bubble area ratio in the entire plain region 26 is preferably 0% or more and 1.5% or less.

[0028] When air bubbles are present in the adhesive layer, when the laminate is observed from the lamination direction (when the laminate is viewed in plan) with an optical microscope, a difference in brightness occurs between the air bubble portion and the portion where no air bubbles are present. Therefore, in this embodiment, for each measurement target area of ​​the laminate film 2, which is a laminate, an area where the brightness is higher than a predetermined threshold is extracted, and the area ratio of the extracted area to the entire measurement target area is calculated, and this calculation result is taken as the air bubble area ratio. The smaller the air bubble area ratio value, the smaller the amount of air bubbles.

[0029] Specifically, an image of the laminate film 2 taken from the lamination direction using a transmitted light source of an optical microscope (e.g., Keyence Microscope VHX-7000) is binarized, and the ratio of the number of pixels occupied by the air bubble portion taken as dark contrast to the total number of pixels of the image is calculated. A known method can be used to set a threshold value during binarization, and for example, Otsu's binarization method can be used. The laminate film 2 of this embodiment has one adhesive layer (solventless adhesive layer 23), but when the laminate film 2 has multiple adhesive layers, the image can be taken by focusing on the adhesive layer to be observed.

[0030] <Touch roller> FIG. 4 is a schematic plan view showing the relationship between the laminate film and the touch roller shown in FIG. 1. As shown in FIG. 1 and FIG. 4, the touch roller 5 has a roller surface 51 that contacts the laminate film 2 on its outer circumferential surface. The roller surface 51 is the outer circumferential surface of the touch roller 5. The roller surface 51 has a convex portion 52 that protrudes from other regions. The other region of the roller surface 51 other than the convex portion 52 is called the reference roller surface 53. In other words, the convex portion 52 is a portion that protrudes from the reference roller surface 53, and the convex portion 52 has a larger diameter than the reference roller surface 53. Here, the surface of the roller surface 51 that contacts the entire plain region 26 of the laminate film 2 is called the plain contact surface 54. The convex portion 52 is provided on at least a part of the plain contact surface 54.

[0031] The convex portions 52 may be provided on the entire plain contact surface 54, may be provided only on a part of the plain contact surface 54, or may be provided beyond the plain contact surface 54. The width of the convex portions 52 may be the same as the width of the plain contact surface 54, may be narrower than the width of the plain contact surface 54, or may be wider than the width of the entire plain region 26. In the touch roller 5 shown in FIG. 4, the width of the convex portions 52 is the same as the width of the plain contact surface 54, and the convex portions 52 are provided on the entire plain contact surface 54. FIGS. 5 and 6 are schematic plan views showing a part of a touch roller of a modified example. In the touch roller 5 shown in FIG. 5, the width of the convex portions 52 is narrower than the width of the plain contact surface 54, and the convex portions 52 are provided only on a part of the plain contact surface 54. In the touch roller 5 shown in FIG. 6, the width of the convex portions 52 is wider than the width of the plain contact surface 54, and the convex portions 52 are provided beyond the plain contact surface 54.

[0032] The protrusions 52 may extend in the circumferential direction R of the touch roller 5, or may extend in a direction inclined relative to the circumferential direction R of the touch roller 5. Figs. 7 and 8 are schematic developments of the roller surface of a touch roller of a modified example. In the touch roller 5 shown in Figs. 4 and 7, the protrusions 52 extend in the circumferential direction R of the touch roller 5. In the touch roller shown in Fig. 8, the protrusions 52 extend in a direction inclined relative to the circumferential direction R of the touch roller 5.

[0033] The protrusions 52 may be provided over the entire area of ​​the touch roller 5 in the circumferential direction R, or may be provided over only a part of the touch roller 5 in the circumferential direction R. The touch roller 5 shown in FIGS. 4 to 8 has the protrusions 52 provided over the entire area of ​​the touch roller 5 in the circumferential direction R.

[0034] The touch roller 5 may be, for example, iron formed into a roll, rubber wound around an iron core formed into a roll, or rubber formed into a roll. In addition to these, any rigid material such as ceramics may be used as long as it can be processed into a roll. The protrusions 52 may be formed directly when the touch roller 5 is manufactured, or may be formed by attaching a tape or the like to the reference roller surface 53 of the touch roller 5.

[0035] The protrusions 52 are preferably made of an elastic material such as rubber or fluororesin. Examples of the material for the rubber forming the protrusions 52 include general-purpose rubbers such as acrylonitrile butadiene rubber (NBR), silicone rubber, and urethane rubber. The protrusions 52 preferably have a durometer hardness of 30 or more and 80 or less, as measured in accordance with JIS K6253.

[0036] The protruding height H of the convex portions 52 on the roller surface 51 is preferably 1 μm or more and 2 mm or less, more preferably 10 μm or more and 1.5 mm or less, and even more preferably 50 μm or more and 1 mm or less. Furthermore, the protruding height H of the convex portions 52 on the roller surface 51 is preferably equal to or greater than the thickness of the printed portion 22 formed on the first film 21. This protruding height H is the protruding height of the convex portions 52 relative to the reference roller surface 53, and is the step between the reference roller surface 53 and the convex portions 52.

[0037] As described above, in the touch roller 5 according to this embodiment, the roller surface 51 that contacts the laminate film 2 has the convex portions 52 that protrude further than other regions, and these convex portions 52 are provided on at least a portion of the plain contact surface 54 that contacts the entire plain region 26 of the laminate film 2 in which no printed portion 22 is formed over the entire area in the longitudinal direction D. Therefore, the convex portions 52 penetrate into the entire plain region 26, increasing the pressure that presses the entire plain region 26 against the winding roll, facilitating the removal of air bubbles from the entire plain region 26. This makes it possible to improve the appearance defects of the laminate film 2 laminated with a solventless adhesive.

[0038] Furthermore, in this touch roller 5, the protrusions 52 are provided over the entire area of ​​the touch roller 5 in the circumferential direction R, which further promotes the removal of air bubbles from the entire plain area .

[0039] Furthermore, in this touch roller 5, the convex portions 52 extend in the circumferential direction R of the touch roller 5, which makes it possible to easily provide the convex portions 52 and efficiently remove air bubbles from the entire plain area 26.

[0040] In addition, in this touch roller 5, the protruding height H of the convex portions 52 on the roller surface 51 is 1 μm or more, preferably 10 μm or more, and more preferably 50 μm or more, so that the entire plain area 26 can be pressed against the winding roll to an extent that can improve poor appearance of the laminate film 2. On the other hand, the protruding height H of the convex portions 52 on the roller surface 51 is 2 mm or less, preferably 1.5 mm or less, and more preferably 1 mm or less, so that the convex portions 52 can be easily provided.

[0041] In addition, in this touch roller 5, since the convex portions 52 have elasticity, the convex portions 52 are easily deformed to conform to the steps between the entire plain area 26 and the printed area 22, making it easier to press the entire plain area 26 against the winding roll.

[0042] In addition, in this touch roller 5, since the protrusions 52 have a durometer hardness of 30 or more, deterioration of the protrusions 52 can be suppressed. On the other hand, since the protrusions 52 have a durometer hardness of 80 or more, the protrusions 52 are easily deformed to conform to the step between the entire plain area 26 and the printed area 22, and the entire plain area 26 is easily pressed against the winding roll 4.

[0043] The winding device 1 according to this embodiment includes the above-mentioned touch roller 5, and therefore can improve appearance defects of the laminate film 2 laminated with a solventless adhesive.

[0044] The laminate film 2 of this embodiment is laminated with a solvent-free adhesive and has a plain area 26 in which no printed portion 22 is formed across the entire longitudinal direction D of the laminate film 2. However, since the air bubble area ratio in the plain area 26 is 0% or more and 1.8% or less, and preferably 0% or more and 1.5% or less, the appearance defect can be improved.

[0045] The above describes the embodiments of the present disclosure, but the present disclosure is not limited to the above embodiments, and may be modified or applied to other things without changing the gist of the claims. EXAMPLES

[0046] The present disclosure will be described in more detail with reference to the following examples, but the present disclosure is not limited to these examples.

[0047] (Preparation of Laminate Film) A printed film was produced by forming a printed area on the barrier film "GL-ARH" (manufactured by Toppan Printing Co., Ltd.) so that a blank area was formed over the entire length of the barrier film. Bellcolor White, manufactured by Sakata Inx Corporation, was used as the ink for forming the printed area. The printed film and nylon film "ONMB 15μm" were bonded together at 2g / m using a solvent-free adhesive "A248B / A246A" (manufactured by Mitsui Chemicals, Inc.). 2 The winding device was set to a processing speed of 150 m / min and a touch roller pressure of 0.2 MPa.

[0048] (Appearance evaluation) The produced laminate film was wound up on a winding device, and the appearance of the laminate film was visually observed and judged as follows. A: No noticeable large bubbles B: Large, noticeable bubbles

[0049] (Air bubble area ratio measurement) After the prepared laminate film was wound up on a winding device, the bubble area ratio in the entire plain area was measured. In measuring the bubble area ratio, an optical microscope was used to focus on the entire plain area of ​​the laminate film 2, and an area with a brightness higher than a predetermined threshold was extracted, and the area ratio of the extracted area to the entire measurement target area was calculated, and this calculation result was taken as the bubble area ratio. Specifically, an image taken of the laminate film from the stacking direction using a transmitted light source of an optical microscope (Keyence Corporation Microscope VHX-7000) was binarized, and the ratio of the number of pixels occupied by the bubble part taken as a dark contrast to the total number of pixels of the image was calculated. Then, this calculation result was taken as the bubble area ratio.

[0050] Example 1 In producing the laminate film, a printed portion was formed on the barrier film so that the height of the printed portion on the printed film was 2 μm.

[0051] The touch roller of Example 1 was produced by wrapping a fluororesin tape with a thickness of 0.2 mm over the entire plain contact surface of the iron core touch roller, which comes into contact with the entire plain region. In the touch roller of Example 1, the fluororesin tape formed convex portions with a protruding height of 0.2 mm on the plain contact surface. Thereafter, an appearance evaluation and a bubble area ratio measurement were carried out. The results are shown in Table 1.

[0052] Example 2 In producing the laminate film, a printed portion was formed on the barrier film so that the height of the printed portion on the printed film was 2 μm.

[0053] The touch roller of Example 2 was produced by cutting the portion of the outer peripheral surface of a rubber roll having a durometer hardness of 70 other than the plain contact surface that contacts the entire plain region. In the touch roller of Example 2, a convex portion with a protruding height of 1 mm was formed on the plain contact surface by the cutting process. Thereafter, an appearance evaluation and a measurement of the air bubble area ratio were performed. The results are shown in Table 1.

[0054] Example 3 In producing the laminate film, a printed portion was formed on the barrier film so that the height of the printed portion on the printed film was 0.7 μm.

[0055] A fluororesin tape with a thickness of 0.2 mm was wound over the entire plain contact surface of the iron core touch roller, which contacts the entire plain region, to produce the touch roller of Example 3. In the touch roller of Example 3, the fluororesin tape formed convex portions with a protruding height of 0.2 mm on the plain contact surface. Thereafter, an appearance evaluation and a bubble area ratio measurement were performed. The results are shown in Table 1.

[0056] Example 4 In producing the laminate film, a printed portion was formed on the barrier film so that the height of the printed portion on the printed film was 8 μm.

[0057] A fluororesin tape with a thickness of 0.2 mm was wound over the entire plain contact surface of the iron core touch roller, which contacts the entire plain region, to produce the touch roller of Example 4. In the touch roller of Example 4, the fluororesin tape formed convex portions with a protruding height of 0.2 mm on the plain contact surface. Thereafter, an appearance evaluation and a measurement of the air bubble area ratio were performed. The results are shown in Table 1.

[0058] Comparative Example 1 In producing the laminate film, a printed portion was formed on the barrier film so that the height of the printed portion on the printed film was 2 μm.

[0059] A touch roller with an iron core was used as the touch roller of Comparative Example 1. Then, an appearance evaluation and a bubble area ratio measurement were performed. The results are shown in Table 1.

[0060] [Table 1]

[0061] As shown in Table 1, Comparative Example 1, in which the touch roller had no convex portions, was rated as B in appearance, and the bubble area ratio in the entire plain region was also high at 1.9%. In contrast, Examples 1 to 4, in which the touch roller had convex portions, all received an appearance rating of A, and the bubble area ratio in the entire plain region was also all lower than Comparative Example 1. [Explanation of symbols]

[0062] 1...winding device, 2...laminate film, 3...conveying device, 4...winding roll, 5...touch roller, 21...first film, 22...printed portion, 23...solvent-free adhesive layer, 24...second film, 25...plain portion, 26...entire plain area, 51...roller surface, 52...convex portion, 53...reference roller surface, 54...plain contact surface, D...longitudinal direction, R...circumferential direction.

Claims

1. A winding device that transports a long laminate film having a first film, a printed portion formed on a portion of the first film, a second film disposed on the printed portion side of the first film, and a solventless adhesive layer disposed between the first film and the second film in a longitudinal direction of the laminate film and winds it up around a winding roll, comprising: a touch roller that presses the laminate film against the winding roll, The roller surface that comes into contact with the laminate film has a protrusion that protrudes from other areas, The convex portion is provided on at least a part of a plain contact surface that contacts an entire plain area of ​​the laminate film in which the printed portion is not formed over the entire area in the longitudinal direction. Touch roller.

2. The convex portion is provided over the entire circumferential area of ​​the touch roller. The touch roller according to claim 1.

3. The protrusion extends in the circumferential direction of the touch roller. The touch roller according to claim 1.

4. The protruding height of the convex portion on the roller surface is 1 μm or more and 2 mm or less. The touch roller according to claim 1.

5. The protrusion has elasticity. The touch roller according to claim 1.

6. The convex portion has a durometer hardness of 30 or more and 80 or less, as measured in accordance with JIS K6253. The touch roller according to claim 1.

7. a conveying device that conveys a long laminate film in a longitudinal direction of the laminate film, the long laminate film having a first film, a printed portion formed on a portion of the first film, a second film disposed on the printed portion side of the first film, and a solvent-free adhesive layer disposed between the first film and the second film; a winding roll on which the laminate film is wound; The touch roller according to any one of claims 1 to 6, which presses the laminate film against the winding roll. Winding device.

8. A long laminate film having a first film, a printed portion formed on a portion of the first film, a second film disposed on the printed portion side of the first film, and a solvent-free adhesive layer disposed between the first film and the second film, The laminate film has a plain area in the longitudinal direction in which the printed portion is not formed, The air bubble area ratio in the entire plain region is 0% or more and 1.8% or less. Laminating film.

Citation Information

Patent Citations

  • Winder touch roller

    JP1987063248U