Wiring substrate, light-emitting device, and manufacturing methods thereof

JP2024154216APending Publication Date: 2024-10-30NICHIA CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023067931
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-18
Publication Date
2024-10-30

AI Technical Summary

Benefits of technology

【0009】 本開示の実施形態によれば、放熱板等との熱結合性の向上を図る配線基板、その配線基板を用いる発光装置及びそれらの製造方法を提供することができる。

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024154216000001_ABST
    Figure 2024154216000001_ABST
Patent Text Reader

Abstract

To provide a wiring substrate that allows improvement of a thermal bonding property with a heat sink, and to provide a light-emitting device using the wiring substrate and manufacturing methods of the wiring substrate and the light-emitting device.SOLUTION: A wiring substrate 1 includes an insulative base body 10 having a first surface 10A and a second surface 10B on an opposite side to the first surface 10A and including a groove part 14 provided on the second surface 10B side and a through hole 18 connecting a bottom surface 14B of the groove part 14 of the second surface 10B with the first surface 10A; a metal member 40 disposed on the bottom surface 14B side of the groove part 14 and the through hole 18, spaced apart from an opening 14A of the groove part 14; and an insulating member 50 which is disposed so as to close the opening 14A of the groove part 14.SELECTED DRAWING: Figure 2A
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a wiring board, a light emitting device, and a method for manufacturing the same. [Background technology]

[0002] Conventionally, active metal brazing materials have been used for vias and wiring in ceramic substrates with high thermal conductivity, such as Si3N4 substrates. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 5693940 [Patent Document 2] Patent No. 6541530 Summary of the Invention [Problem to be solved by the invention]

[0004] An object of the embodiments of the present disclosure is to provide a wiring board that improves thermal coupling with a heat sink or the like, a light emitting device that uses the wiring board, and methods for manufacturing the same. [Means for solving the problem]

[0005] The wiring board disclosed in the embodiment has a first surface and a second surface opposite to the first surface, and has an insulating base material having a groove portion provided on the second surface side and a through hole connecting a bottom surface of the groove portion of the second surface and the first surface, a metal member arranged on the bottom surface side of the groove portion and in the through hole away from the opening of the groove portion, and an insulating member arranged to cover the opening of the groove portion.

[0006] Moreover, the light emitting device disclosed in the embodiment includes a wiring board disclosed in the embodiment, and a light emitting element having an element electrode arranged on the side of the first surface of the wiring board, and the metal member of the wiring board is electrically connected to the element electrode.

[0007] Furthermore, a method for manufacturing a wiring board disclosed in an embodiment includes preparing a substrate having a first surface and a second surface opposite to the first surface, a through hole penetrating the substrate to connect the first surface and the second surface, and a groove portion connected to the through hole and located on the second surface; arranging a conductive paste containing at least a metal powder, an active metal powder, and an organic solvent in the groove portion and the through hole; firing the conductive paste to obtain a metal member; and arranging an insulating member to cover an opening of the groove portion.

[0008] Furthermore, the manufacturing method of the light emitting device disclosed in the embodiment includes preparing a wiring board manufactured by the manufacturing method of the wiring board disclosed in the embodiment, and arranging a light emitting element having an element electrode on the wiring board, and in arranging the light emitting element, electrically connecting the metal member of the wiring board and the element electrode. Effect of the Invention

[0009] According to the embodiments of the present disclosure, it is possible to provide a wiring board that improves thermal coupling with a heat sink or the like, a light emitting device that uses the wiring board, and methods for manufacturing the same. [Brief description of the drawings]

[0010] [Figure 1A] 1 is a plan view illustrating an outline of a wiring board according to an embodiment; [Figure 1B] 1 is a bottom view illustrating an outline of a wiring board according to an embodiment; [Figure 2A] FIG. 1B is a cross-sectional view taken along line IIA-IIA in FIG. 1A. [Figure 2B] FIG. 1B is a cross-sectional view taken along line IIB-IIB in FIG. 1A. [Figure 2C] 3 is an enlarged cross-sectional view illustrating an outline of an interface between a metal member and a base material in a wiring board according to an embodiment. FIG. [Diagram 3] 4 is a flowchart illustrating a method for manufacturing a wiring board according to an embodiment. [Figure 4A]3 is a cross-sectional view illustrating an outline of a base material before processing in a method for manufacturing a wiring board according to an embodiment; [Figure 4B] 4 is a cross-sectional view illustrating an outline of a base material in which a groove portion is formed in the method for manufacturing a wiring board according to the embodiment. FIG. [Figure 4C] 4 is a cross-sectional view illustrating an outline of a base material in which a through hole is formed in the method for manufacturing a wiring board according to the embodiment. FIG. [Figure 4D] 4 is a cross-sectional view illustrating an outline of a base material on which a conductive paste is disposed in the method for manufacturing a wiring board according to the embodiment; FIG. [Figure 4E] 4 is a cross-sectional view illustrating an outline of a base material obtained by firing a conductive paste in a method for manufacturing a wiring board according to an embodiment. FIG. [Figure 4F] 10 is a cross-sectional view illustrating an outline of a base material in which an opening of a groove is formed on a curved surface in a method for manufacturing a wiring board according to an embodiment. FIG. [Figure 4G] 1 is a cross-sectional view illustrating an outline of a base material having an insulating member disposed in a groove in a method for manufacturing a wiring board according to an embodiment; [Figure 4H] 4 is a cross-sectional view illustrating an outline of a base material after polishing an insulating member in a method for manufacturing a wiring board according to an embodiment. FIG. [Figure 5A] 11 is a cross-sectional view illustrating an outline of a modified example of the wiring board. [Figure 5B] 13 is a cross-sectional view illustrating an outline of a base material obtained by firing a conductive paste in a manufacturing method of a modified example of a wiring board. FIG. [Figure 6] 1 is a cross-sectional view illustrating an outline of an application example of a wiring board. [Figure 7] 1 is a plan view illustrating an outline of a light emitting device according to an embodiment. [Figure 8] 8 is a cross-sectional view taken along line VIII-VIII in FIG. 7. [Figure 9] 4 is a flowchart illustrating a method for manufacturing a light emitting device according to an embodiment. [Figure 10A] 4 is a cross-sectional view illustrating an outline of a prepared wiring substrate in the manufacturing method of the light emitting device according to the embodiment. FIG. [Figure 10B]4 is a cross-sectional view illustrating an outline of a state in which a light emitting element is arranged on a wiring substrate in a manufacturing method for a light emitting device according to an embodiment. FIG. [Figure 10C] 4 is a cross-sectional view illustrating an outline of a state in which a heat sink is bonded to a wiring substrate in a manufacturing method for a light emitting device according to an embodiment. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0011] Hereinafter, an embodiment according to the present disclosure will be described with reference to the drawings. However, the embodiment described below is for embodying the technical idea according to the present disclosure, and the invention is not limited to the following unless otherwise specified. The contents described in one embodiment can be applied to other embodiments and modified examples. In addition, the drawings are schematic diagrams of the embodiments, and in order to clarify the description, the scale, interval, positional relationship, etc. of each member may be exaggerated, or some of the members may be omitted. The directions shown in each figure indicate the relative positions between the components, and are not intended to indicate absolute positions. In addition, the same names and symbols indicate, in principle, the same or homogeneous members, and detailed descriptions are omitted as appropriate. In addition, in the embodiments, "covering" is not limited to direct contact, but also includes indirect covering, for example, via other members. In addition, "disposing" is not limited to direct contact, but also includes indirect disposing, for example, via other members.

[0012] [Wiring board] A wiring board 1 according to an embodiment will be described with reference to Figs. 1A to 2C. Fig. 1A is a plan view illustrating an outline of the wiring board 1. Fig. 1B is a bottom view illustrating an outline of the wiring board 1. Fig. 2A is a cross-sectional view taken along line IIA-IIA in Fig. 1A. Fig. 2B is a cross-sectional view taken along line IIB-IIB in Fig. 1A. Fig. 2C is a cross-sectional view illustrating an enlarged outline of the interface between a metal member and a substrate.

[0013] The wiring board 1 has a first surface 10A and a second surface 10B opposite to the first surface 10A, and has an insulating base material 10 having a groove 14 provided on the second surface 10B and a through hole 18 connecting a bottom surface 14B of the groove 14 on the second surface 10B to the first surface 10A, a metal member 40 arranged on the bottom surface 14B side of the groove 14 and in the through hole 18 away from the opening 14A of the groove 14, and an insulating member 50 arranged so as to close the opening 14A of the groove 14. Each component of the wiring board 1 will be described below.

[0014] (base material) The substrate 10 is a plate-like member that serves as the base of the wiring board 1. The substrate 10 has a first surface 10A and a second surface 10B that is the opposite side of the first surface 10A, a groove 14 provided on the second surface 10B, and a through hole 18 that connects a bottom surface 14B of the groove 14 to the first surface 10A. The shape of the substrate 10 in a plan view is, for example, rectangular, and is not particularly limited. The thickness of the substrate 10 can be, for example, 0.2 mm or more and 2 mm or less, preferably 0.4 mm or more and 1.5 mm or less.

[0015] The substrate 10 is preferably insulating and has excellent heat dissipation properties. The substrate 10 may be made of ceramics, and is preferably a fired ceramic. By making the substrate 10 of fired ceramics, the wiring board 1 can improve the machining accuracy of the grooves 14 and the through holes 18. The substrate 10 may be made of ceramics containing at least one of silicon nitride, aluminum nitride, boron nitride, magnesium oxide, and aluminum oxide, and preferably contains silicon nitride or aluminum nitride. The substrate 10 is preferably made of nitride ceramics such as silicon nitride, aluminum nitride, and boron nitride, but may be made of oxide ceramics such as aluminum oxide, silicon oxide, calcium oxide, and magnesium oxide. The substrate 10 may also be made of beryllium oxide, silicon carbide, mullite, borosilicate glass, or the like.

[0016] (Groove) The groove portion 14 is a groove that is provided on the second surface 10B, recessed from the second surface 10B, and in which a metal member 40 is embedded. As described later, the metal member 40 embedded in the groove portion 14 constitutes embedded wiring 42, and one embedded wiring 42 is disposed in one groove portion 14.

[0017] The depth of the bottom surface 14B of the groove 14 from the second surface 10B can be 1 / 8 or more and 7 / 8 or less, preferably 1 / 4 or more and 3 / 4 or less, and particularly preferably 3 / 8 or more and 5 / 8 or less, relative to the thickness of the substrate 10. The depth of the bottom surface 14B of the groove 14 from the second surface 10B can be 30 μm or more and 80 μm or less, preferably 50 μm or more and 60 μm or less. By setting the depth to 30 μm or more, the wiring board 1 can separate the embedded metal member 40 from the second surface 10B, and by setting the depth to 80 μm or less, the strength of the substrate 10 can be maintained at the position of the bottom surface 14B. The depth of the groove 14 is the distance between the deepest position of the bottom surface 14B and the second surface 10B in the cross section in the width direction. The width direction of the groove 14 is the horizontal direction of the plate-shaped substrate 10 and is perpendicular to the extension direction of the embedded wiring 42.

[0018] Here, the description will be given assuming that the bottom surface 14B is a flat surface, but in the case where the through holes 18 are formed, the description will be given assuming that the portion excluding the through holes 18 is a flat surface. However, the bottom surface 14B may not be a flat surface but a curved surface. The width W2 of the bottom surface 14B can be, for example, 15 μm or more and 500 μm or less. Note that the width W2 of the bottom surface 14B refers to the width at the bottom surface 14B, but the bottom surface 14B may be roughened by processing or the like, or the bottom surface 14B may be a curved surface, and the width of the groove portion 14 may be a length measured at a position about 5 μm or more and 10 μm or less away from the bottom surface 14B, or at a position 1 / 2 the depth of the groove portion 14 from the second surface 10B in the depth direction.

[0019] The groove 14 is continuous with the second surface 10B via a curved surface CS that expands toward the opening 14A. The curved surface CS may be, for example, an arc shape with a radius of 0.1 μm to 20 μm, preferably 0.5 μm to 10 μm, in a cross section in the width direction. The width W1 of the opening 14A of the groove 14 is wider than the width W2 of the bottom surface 14B. Note that the width W1 of the opening 14A refers to the width at the second surface 10B, but the bottom surface 14B may be roughened by processing or the like, or the bottom surface 14B may be a curved surface, and the length measured at a position 1 / 10 of the depth of the groove 14 in the depth direction from the second surface 10B may be the width of the groove 14.

[0020] (Through hole) The through hole 18 is a hole connecting the bottom surface 14B of the groove portion 14 of the second surface 10B and the first surface 10A. Here, the through hole 18 is circular in plan view and has the same diameter from the bottom surface 14B to the first surface 10A. The diameter of the through hole 18 can be, for example, 50 μm to 500 μm, preferably 100 μm to 300 μm. The diameter of the through hole 18 may be tapered so that it is larger on the first surface 10A side and smaller on the bottom surface 14B side, or vice versa. The shape of the through hole 18 in plan view is not limited to a circle, and may be, for example, a polygonal shape including a rectangle, or an elliptical shape.

[0021] (Metal parts) Metal member 40 is a member that will become an electrode material or a wiring material in wiring board 1. Metal member 40 is disposed away from opening 14A of groove 14 on the bottom surface 14B side of groove 14 and in through hole 18.

[0022] The metal member 40 has pads 45 to which circuit components such as electronic components are connected, terminals 46 to which external wiring is connected, and at least two wiring layers connecting the pads 45 with each other and between the pads 45 and the terminals 46. One of the two wiring layers is a buried wiring 42 buried in the wiring board 1, and the other is an exposed wiring 41 exposed from the wiring board 1. The exposed wiring 41 and the buried wiring 42 are connected by via wiring 43 arranged in the through hole 18. The pads 45 and the terminals 46 are electrically connected to the metal member 40 arranged in the through hole 18. In the drawings, the exposed wiring 41 is omitted except for a part. The terminals 46 are arranged together in a certain area, and the illustration of individual terminals such as power lines and signal lines is omitted.

[0023] Here, the pad portion 45, the terminal portion 46, and the exposed wiring 41 are arranged with a substantially uniform thickness on the first surface 10A of the wiring board 1. The thickness of the pad portion 45, the terminal portion 46, and the exposed wiring 41 from the first surface 10A can be, for example, 5 μm or more and 100 μm or less, and is preferably 10 μm or more and 50 μm or less.

[0024] The buried wiring 42 is disposed on the bottom surface 14B side of the groove 14. The metal member 40 disposed in the groove 14 has a curved surface at least at the interface with the insulating member 50. Here, the buried wiring 42 has a thickness from the bottom surface 14B thinner on the center side in the width direction of the groove 14. The thickness of the buried wiring 42 from the bottom surface 14B at the center in the width direction of the groove 14 can be, for example, 1 μm or more and 200 μm or less, and is preferably 5 μm or more and 100 μm or less.

[0025] The via wiring 43 is disposed so as to fill the through hole 18. Here, the via wiring 43 has a cylindrical shape. The diameter of the via wiring 43 can be, for example, 50 μm or more and 500 μm or less, and preferably 100 μm or more and 300 μm or less.

[0026] The shape of the pad portion 45 in plan view is, for example, rectangular. Some of the pad portions 45 have a through hole 18 arranged at the center of each pad portion 45 in plan view, and are connected to the buried wiring 42 through a via wiring 43. The buried wiring 42 is connected to the exposed wiring 41 through another via wiring 43, and the exposed wiring 41 is connected to the terminal portion 46.

[0027] The metal member 40 is mainly composed of metal and contains at least one of Cu, Cr, Ni, Ag, Al, Zn, Sn, and an Ag-Cu alloy. The metal member 40 preferably further contains active metal elements such as Ti, Ce, Zr, and Mg.

[0028] The metal member 40 preferably has a metal compound layer 60 at the interface with the base material 10, and is disposed on the base material 10 via the metal compound layer 60. That is, the pad portion 45, the terminal portion 46, the exposed wiring 41, the buried wiring 42, and the via wiring 43 are preferably disposed on the base material 10 via the metal compound layer 60. By having the metal member 40 have the metal compound layer 60 at the interface with the base material 10, the bond between the metal member 40 and the base material 10 can be strengthened.

[0029] As illustrated in Fig. 2C, the metal compound layer 60 is a layer containing a large amount of compounds 61 between the active metal element contained in the metal member 40 and nonmetallic inorganic elements such as N and O contained in the base material 10. The compounds 61 are, for example, TiN or TiO2. Note that although the metal compound layer 60 is not shown in Fig. 2C and other figures, in the present disclosure, the metal member 40 is disposed on the base material 10 via the metal compound layer 60.

[0030] (Insulating material) The insulating member 50 is a member that covers and insulates the metal member 40 so that the metal member 40 is not exposed from the second surface 10B. The insulating member 50 is disposed in the groove 14, and it is preferable that the surface of the insulating member 50 and the second surface 10B are flush flat surfaces. It is preferable that the insulating member 50 has a curved surface that faces the curved surface CS of the groove 14. This makes it possible to increase the distance between the metal member 40 and the second surface 10B along the interface between the insulating member 50 and the base material 10, thereby improving the insulation properties.

[0031] The insulating member 50 may be made of ceramics or resin. The material of the insulating member 50 is preferably one that is insulating and has high thermal conductivity, such as cement or glass containing BN or the like, thermosetting resins such as epoxy resin, silicone resin, phenol resin, polyimide resin, polyurethane resin, melamine resin, and urea resin, and thermoplastic resins such as polyvinylpyrrolidone resin, polyvinyl alcohol resin, polyethylene glycol resin, and polyamide resin.

[0032] In wiring board 1 having the above-mentioned configuration, one of the two wiring layers is embedded on second surface 10B and insulated by insulating member 50, and second surface 10B is made flat. This allows wiring board 1 to be bonded to a heat sink or the like via a conductive bonding member, improving thermal bonding and increasing heat dissipation.

[0033] [Method of manufacturing wiring board] Next, a method S1 for manufacturing a wiring board according to an embodiment will be described with reference to the drawings. FIG. 3 is a flow chart illustrating the method S1 for manufacturing a wiring board. FIG. 4A is a cross-sectional view illustrating an outline of the base material 10 before processing. FIG. 4B is a cross-sectional view illustrating an outline of the base material 10 in which the groove portion 14 is formed. FIG. 4C is a cross-sectional view illustrating an outline of the base material 10 in which the through-hole 18 is formed. FIG. 4D is a cross-sectional view illustrating an outline of the base material 10 in which the conductive paste 80 is disposed. FIG. 4E is a cross-sectional view illustrating an outline of the base material 10 in which the conductive paste 80 is fired. FIG. 4F is a cross-sectional view illustrating an outline of the base material 10 in which the opening 14A of the groove portion 14 is formed on the curved surface CS. FIG. 4G is a cross-sectional view illustrating an outline of the base material 10 in which the insulating member 50 is disposed in the groove portion 14. FIG. 4H is a cross-sectional view illustrating an outline of the base material 10 in which the insulating member 50 is polished.

[0034] The method for manufacturing a wiring board S1 includes preparing a base material 10 having a first surface 10A and a second surface 10B opposite to the first surface 10A, a through hole 18 penetrating the base material 10 so as to connect the first surface 10A and the second surface 10B, and a groove portion 14 connected to the through hole 18 and located on the second surface 10B, disposing a conductive paste 80 containing at least a metal powder, an active metal powder, and an organic solvent in the groove portion 14 and the through hole 18, sintering the conductive paste 80 to obtain a metal member 40, and disposing an insulating member 50 so as to close an opening 14A of the groove portion 14. The method for manufacturing a wiring board S1 further includes, after obtaining the metal member 40 S30 and before disposing the insulating member 50 S50, widening the opening 14A of the groove portion 14 S40.

[0035] That is, the method S1 for manufacturing a wiring board includes preparing a base material 10 (S10), arranging a conductive paste 80 (S20), obtaining a metal member 40 (S30), widening an opening 14A of a groove portion 14 (S40), and arranging an insulating member (S50). Each component of the method S1 for manufacturing a wiring board will be described below.

[0036] (Preparing the substrate) In preparing a substrate S10 (hereinafter referred to as step S10), a substrate 10 is prepared having a first surface 10A and a second surface 10B opposite the first surface 10A, a through hole 18 penetrating to connect the first surface 10A and the second surface 10B, and a groove portion 14 connected to the through hole 18 and located on the second surface 10B.

[0037] The substrate 10 to be prepared is preferably a fired ceramic containing silicon nitride or aluminum nitride. The second surface 10B is preferably smoothed so that the arithmetic mean roughness Ra as defined in JIS B0601 is 0.01 μm or more and 1.5 μm or less. The smoothing can be performed by polishing, for example. By smoothing the second surface 10B, it is possible to improve the adhesion when the wiring board is joined to an external heat sink or the like.

[0038] The fired ceramic substrate 10P is a plate-shaped member. The through holes 18 are formed to the depth of the bottom surfaces 14B of the grooves 14, so that the through holes 18 and the grooves 14 penetrate the ceramic substrate 10P. Either the through holes 18 or the grooves 14 may be formed first. Here, the through holes 18 are formed after the grooves 14 are formed.

[0039] In step S10, the grooves 14 and the through holes 18 can be formed by laser processing. Here, the through holes 18 are formed so as to have the same diameter from the first surface 10A to the bottom surface 14B. The through holes 18 may be formed so as to have a smaller diameter from the first surface 10A to the bottom surface 14B, for example, by irradiating the first surface 10A with a CO2 laser.

[0040] (Placing conductive paste) In disposing a conductive paste (S20) (hereinafter referred to as step S20), a conductive paste 80 containing at least a metal powder, an active metal powder, and an organic solvent is disposed in the groove portion 14 and the through hole 18. The conductive paste 80 is further disposed on the first surface 10A. The conductive paste 80 is fired to become the metal member 40.

[0041] The metal powder is a powder containing at least one of Cu, Cr, Ni, Ag, Al, Zn, Sn, and Ag-Cu alloy. Among these, Ag-Cu alloy is preferable because it can be sintered at a relatively low temperature of 780°C to 850°C. In addition, Cu and Ag are preferable because they have high electrical conductivity. Here, the metal powder is mainly composed of Ag-Cu alloy with a mixing ratio of Ag and Cu of 72:28, which is close to Ag-Cu eutectic. The median diameter of the metal powder is preferably 1 μm to 50 μm. In addition to the Ag-Cu alloy, at least one of metal powders having a melting point higher than that of the Ag-Cu alloy, such as Cu, Cr, and Ni, may be included. As a result, when the Ag-Cu alloy is fired at a temperature of, for example, about 800° C. to 850° C., the metal powder having a melting point higher than the firing temperature is included, so that the metal powder does not melt. This makes it possible to suppress the volumetric shrinkage of the conductive paste 80 and to increase the thermal conductivity and electrical conductivity of the conductive paste 80.

[0042] The active metal powder is a powder containing an active metal element, and may be a powder containing at least one selected from TiH2, CeH2, ZrH2, and MgH2. Here, the active metal powder preferably contains TiH2 so as to react with the nitrogen contained in the base material 10 prepared in step S10.

[0043] The organic solvent is a solvent that acts as a binder for the metal powder and the activated metal powder, and can be, for example, a resin such as acrylic, epoxy, urethane, ethyl cellulose, silicone, phenol, polyimide, polyurethane, melamine, urea, etc. The viscosity of the conductive paste 80 can be adjusted by changing the type and amount of the organic solvent.

[0044] As an example, the metal powder contained in the conductive paste 80 is 60% to 90% by weight, the active metal powder is 1% to 10%, and the organic solvent is 5% to 30%. Preferably, the metal powder is 70% to 85%, and the active metal powder is 1% to 10%. The metal component including the metal powder and the active metal powder is preferably 90% or less by weight, and the organic solvent of the conductive paste 80 placed in the groove portion 14 is preferably 10% or more. By increasing the content ratio of the organic solvent, the volumetric shrinkage rate associated with drying during firing can be increased, and the surface of the metal member 40 after firing of the conductive paste 80 can be recessed.

[0045] The conductive paste 80 can be arranged by, for example, screen printing. The conductive paste 80A arranged on the first surface 10A side may be the same as the conductive paste 80B arranged on the second surface 10B side, but it is preferable that they are different. The conductive paste 80A arranged on the first surface 10A side preferably has a lower organic solvent content than the conductive paste 80B arranged on the second surface 10B side, and preferably has a smaller volume shrinkage rate associated with drying during firing. The conductive paste 80A arranged on the first surface 10A is preferably arranged so as to have a uniform thickness from the first surface 10A.

[0046] (Obtaining metal parts) In obtaining the metal member S30 (hereinafter referred to as step S30), the conductive paste 80 is fired to obtain the metal member 40. The firing temperature can be 780° C. or higher and 1100° C. or lower, and preferably 780° C. or higher and 850° C. or lower. The firing atmosphere is 10 -5 It is preferable to use a vacuum atmosphere of less than 1 Pa or an Ar atmosphere of 99.9% or more.

[0047] The conductive paste 80 placed in the groove portion 14 becomes the buried wiring 42 of the metal member 40, the conductive paste 80 placed in the through hole 18 becomes the via wiring 43, and the conductive paste 80 placed on the first surface 10A becomes the exposed wiring 41, the pad portion 45, and the terminal portion 46.

[0048] By baking the conductive paste 80, the organic solvent is decomposed, volatilized, and removed. By removing the organic solvent, the volume of the metal member 40 shrinks relative to the volume of the conductive paste 80. Due to this shrinkage, the metal member 40 is disposed away from the opening 14A of the groove portion 14 and on the bottom surface 14B side of the groove portion 14 and the through hole 18. That is, in the groove portion 14, the metal member 40 is disposed closer to the bottom surface 14B side, and the insulation property of the second surface 10B side can be improved. Also, due to this shrinkage, the surface of the metal member 40 on the second surface 10B side is curved so as to be recessed toward the first surface 10A side. That is, the metal member 40 is formed so that the surface on the second surface 10B side is a curved surface.

[0049] Furthermore, a metal compound layer containing a reaction product between the non-metallic elements contained in the base material 10 and the active metal elements contained in the metal member 40 is formed by the firing. That is, the metal member 40 has a metal compound layer that changes from the active metal powder at the interface between the base material 10 and the metal member 40. Here, the metal compound layer contains TiN that is a reaction product between the nitrogen contained in the base material 10 and TiH2 contained in the active metal powder of the conductive paste 80. By having a metal compound layer at the interface between the base material 10 and the metal member 40, the reliability of the joint can be improved.

[0050] (Widening the opening of the groove) In widening the opening of the groove portion S40 (hereinafter referred to as step S40), portions of the substrate 10 and the metal member 40 are removed to widen the opening 14A of the groove portion 14 so that the groove portion 14 is continuous with the second surface 10B via a curved surface CS that widens toward the opening 14A side. Here, portions of the substrate 10 and the metal member 40 are removed by blasting. The blasting process removes the end of the metal member 40 on the opening 14A side and removes the corners of the substrate 10 at the opening 14A, making it possible to form a rounded curved surface CS.

[0051] The curved surface CS can be formed, for example, in an arc shape in a cross section in the width direction. The metal member 40 is disposed on the bottom surface 14B side of the curved surface CS. Step S40 may be performed by polishing with a ceramic fiber brush, etching, laser processing, or the like.

[0052] (Install insulating materials) In arranging an insulating member S50 (hereinafter referred to as step S50), an insulating member 50 is arranged so as to cover the opening 14A of the groove portion 14. The insulating member 50 covers the metal member 40 exposed on the second surface 10B side, and the metal member 40 is insulated from the second surface 10B side.

[0053] It is preferable that the insulating member 50 is disposed in the groove 14 with a width wider than that of the metal member 40. In step S40, the width W1 of the opening 14A of the groove 14 is formed wider than the width W2 of the bottom surface 14B. Therefore, the insulating member 50 can be disposed so that its width is wider on the opening 14A side than on the bottom surface 14B side. This can improve the insulation properties.

[0054] The insulating member 50 can be arranged, for example, by applying the material of the insulating member 50 before curing or drying and solidifying it by heating or the like. The material of the insulating member 50 can be a resin such as ceramic cement containing BN or the like, an epoxy resin, or a silicone resin, or glass, etc. The insulating member 50 can be arranged by potting, spraying, inkjet printing, screen printing, etc.

[0055] It is preferable that the insulating member 50 is disposed so as to form a flat surface on the same plane as the second surface 10B. Here, the insulating member 50 is solidified or hardened so as to protrude from the second surface 10B, and the protruding insulating member 50 is polished so that the second surface 10B and the insulating member 50 form a flat surface on the same plane. By having the insulating member 50 and the second surface 10B form a flat surface, the wiring board 1 and an external heat sink or the like are brought into close contact with each other, suppressing the generation of an air layer, and improving the efficiency of heat transfer.

[0056] Moreover, it is preferable that the area of ​​the insulating member 50 on the second surface side of the wiring board 1 is as small as possible. By reducing the area of ​​the insulating member 50, the area of ​​the highly thermally conductive base material 10 facing an external heat sink or the like can be increased, thereby improving heat dissipation.

[0057] In the manufacturing method S1 for a wiring board including the above-mentioned configuration, a metal member 40 is disposed on the bottom surface 14B side of a groove 14 provided on the second surface 10B of the base material 10, and an insulating member 50 is disposed so as to close the groove 14, thereby making it possible to provide wiring insulated from the second surface 10B side without stacking a sheet or the like that is the material for the base material. Also, insulation can be improved by removing a part of the base material 10 and the metal member 40 and widening the opening 14A to form a curved surface.

[0058] In step S10, the grooves 14 may be formed by blasting, and the through holes 18 may be formed by laser processing. By forming the grooves 14 by blasting, the bottom surface 14B can be formed into a curved shape that is deeper toward the center of the grooves 14. This increases the area where the metal member 40 and the base material 10 face each other, and further improves heat dissipation and bonding. The grooves 14 and the through holes 18 may be formed by blasting, punching, etching, or the like.

[0059] [Modification of wiring board] Next, a modified example of the wiring board will be described below. Fig. 5A is a cross-sectional view illustrating an outline of a modified wiring board 1A.

[0060] The wiring board 1A of the modified example differs from the wiring board 1 in that the base material 10 has a recess 16 on the first surface 10A and a through hole 18 at the position of the recess 16. In the wiring board 1A of the modified example, the metal member 40 is disposed in the recess 16 rather than on the first surface 10A. By disposing the metal member 40 in the recess 16, the wiring board can be made thinner. In addition, it is preferable that the metal member 40 disposed in the recess 16 and the first surface 10A of the base material 10 form a flat surface on the same plane. This enables the wiring board to be made even thinner.

[0061] In the modified wiring board 1A, the pad portion 45, the terminal portion 46, and the exposed wiring 41 are disposed in the recessed portion 16. The depth of the recessed portion 16 from the first surface 10A can be, for example, 5 μm or more and 100 μm or less, and preferably 10 μm or more and 50 μm or less.

[0062] [Manufacturing method of modified wiring board] Next, a manufacturing method of a modified wiring board will be described. Fig. 5B is a cross-sectional view illustrating an outline of base material 10 after conductive paste 80 is baked in the manufacturing method of modified wiring board 1A.

[0063] The manufacturing method of the wiring board 1A of the modified example differs from manufacturing method S1 in that a base material to be prepared has a recess 16 on the first surface 10A, and conductive paste 80 is placed in the recess 16 instead of on the first surface 10A. The manufacturing method also includes polishing metal member 40 on the first surface 10A side.

[0064] In the manufacturing method of the wiring board 1A of the modified example, in the step S10 of preparing a base material, the first surface 10A further includes a recess 16, and a through hole 18 is provided at the position of the recess 16. The recess 16 is formed in an area of ​​the first surface 10A where the exposed wiring 41, the pad portion 45, and the terminal portion 46 are to be provided. The depth of the recess 16 can be, for example, 5 μm or more and 100 μm or less, and preferably 10 μm or more and 50 μm or less. The recess 16 can be formed by etching, blasting, or laser processing. The order of forming the through hole 18 and the recess 16 does not matter.

[0065] Then, in placing conductive paste S20, conductive paste 80 is placed in recess 16 formed together with groove 14 and through hole 18. Step S30 can be performed in the same manner as in manufacturing method S1.

[0066] The manufacturing method of the wiring board 1A of the modified example further includes polishing the metal member 40 after step S30 so that the first surface 10A of the base material 10 and the metal member 40 form a flush flat surface. Polishing the metal member may be performed at any stage after step S30. Here, steps S40 and S50 are performed first. Polishing can be performed with aluminum oxide, diamond, silicon carbide, or the like. Note that steps S40 and S50 can be performed in the same manner as in manufacturing method S1.

[0067] [Application examples of wiring boards] Next, an application example of the wiring board will be described below. Fig. 6 is a cross-sectional view illustrating an outline of an application example of the wiring board.

[0068] An application example of the wiring board is a device in which a heat sink 90 is bonded to the second surface 10B of the wiring board 1 via a bonding member 95. The surface of the heat sink 90 bonded to the second surface 10B is a flat surface. Here, the heat sink 90 is a plate-shaped member. The heat sink 90 may have irregularities on the surface other than the surface bonded to the wiring board 1, for example, to increase the surface area. The material of the heat sink 90 may be a metal such as copper or aluminum.

[0069] The bonding member 95 is a member that bonds or adheres the wiring board 1 and the heat sink 90. ​​The bonding member 95 fills the gap between the wiring board 1 and the heat sink 90, thereby expelling air and improving the efficiency of heat transfer. Since the second surface 10B side of the wiring board 1 is insulated, a conductive bonding member 95 made of hardened solder, brazing material, paste containing Ag, or the like can be used, thereby improving heat dissipation.

[0070] In addition, in the application example of the wiring board, a modified wiring board 1A can be used in place of the wiring board 1. The modified wiring board 1A has a configuration similar to that of the wiring board 1 on the second surface 10B side, and like the wiring board 1, the heat sink 90 is bonded via a bonding member 95, thereby improving heat dissipation.

[0071] [Light emitting device] Next, a light emitting device 100 according to an embodiment will be described with reference to the drawings. Fig. 7 is a plan view illustrating an outline of the light emitting device 100. Fig. 8 is a cross-sectional view taken along line VIII-VIII in Fig. 7.

[0072] The light emitting device 100 is a device that combines an application example of a wiring board with light emitting elements 20, and the on / off and brightness of each light emitting element 20 can be controlled from outside via the terminal portion 46. Here, 15 light emitting elements 20 are aligned and arranged on the first surface 10A side. There is no particular limit to the number of light emitting elements 20.

[0073] The light emitting device 100 includes a wiring board 1 and a light emitting element 20 having an element electrode 21 arranged on a first surface 10A side of the wiring board 1, and a metal member 40 of the wiring board 1 is electrically connected to the element electrode 21. Here, a light-transmitting member 30 is arranged on an upper surface of the light emitting element 20. Each component of the light emitting device 100 will be described below.

[0074] (wiring board) The light emitting element 20 is disposed on the wiring board 1 with the first surface 10A facing up. The pad portion 45 of the metal member 40 has a size and shape that allows the element electrode 21 of the light emitting element 20 to be disposed thereon. As in the application example of the wiring board described above, the wiring board 1 has a heat sink 90 bonded to the second surface 10B side via a bonding member 95.

[0075] (Light emitting element) The light emitting element 20 is a member that emits light when power is supplied. As an example, the light emitting element 20 has a rectangular shape. The light emitting element 20 includes a semiconductor laminate, in which a light-transmitting substrate such as sapphire or gallium nitride is disposed on the upper surface side of the semiconductor laminate, and a pair of element electrodes 21 is disposed on the lower surface side. As the semiconductor laminate, any composition can be used depending on the desired emission wavelength. For example, a nitride semiconductor (In x Al y Ga 1-x-yN, 0≦X, 0≦Y, X+Y≦1), GaP, or GaAlAs or AlInGaP capable of emitting red light can be used. The size and shape of the light emitting element 20 can be appropriately selected depending on the purpose of use.

[0076] The pair of element electrodes 21 are, for example, rectangular and exposed on the lower surface of the light emitting element 20. The element electrodes 21 can be made of, for example, a single layer or a laminated film of a metal such as gold, platinum, palladium, rhodium, nickel, tungsten, molybdenum, chromium, titanium, or an alloy thereof.

[0077] Here, the element electrode 21 is electrically connected to the pad portion 45 of the metal member 40 via the conductive member 70. The conductive member 70 may be a metal such as gold or solder, or a hardened conductive paste material that is a mixture of powdered metal and a resin binder.

[0078] (Translucent member) The light-transmitting member 30 is a member that protects the upper surface of the light-emitting element 20 and is located on the light extraction surface of the light-emitting device 100. Here, the light-transmitting member 30 is rectangular, as an example, and has the same size and shape as the light-emitting element 20 in a planar view. The light-transmitting member 30 may have a shape and size that encompasses the light-emitting element 20 in a planar view.

[0079] The light-transmitting member 30 is made of a light-transmitting resin material, and may be, for example, an epoxy resin, a silicone resin, or a resin obtained by mixing these. The light-transmitting member 30 may contain a phosphor, and for example, by containing a phosphor that absorbs blue light from the light-emitting element 20 and emits yellow light, the light-emitting device 100 can emit white light. The light-transmitting member 30 may also contain a plurality of types of phosphors, and for example, by containing a phosphor that absorbs blue light from the light-emitting element 20 and emits green light and a phosphor that emits red light, the light-emitting device 100 can emit white light.

[0080] The light-transmitting member 30 may further include a light-emitting material such as a phosphor or quantum dots. Examples of such phosphors include yttrium-aluminum (gallium-doped) garnet activated with cerium, nitrogen-containing calcium aluminosilicate (strontium) activated with europium, potassium fluorosilicate activated with manganese, and β-sialon phosphors. Specific examples of phosphors include yttrium-aluminum garnet phosphors (e.g., (Y,Gd)3(Al,Ga)5O 12 :Ce), lutetium aluminum garnet phosphors (e.g., Lu3(Al,Ga)5O 12 :Ce), terbium aluminum garnet phosphors (e.g., Tb3(Al,Ga)5O 12 :Ce), CCA phosphors (e.g., Ca 10 (PO4)6Cl2:Eu), SAE phosphors (e.g., Sr4Al 14 O 25 :Eu), chlorosilicate phosphors (e.g., Ca8MgSi4O 16 Cl2:Eu), silicate phosphors (e.g., (Ba,Sr,Ca,Mg)2SiO4:Eu), β-sialon phosphors (e.g., (Si,Al)3(O,N)4:Eu) or α-sialon phosphors (e.g., Ca(Si,Al) 12 (O,N) 16 :Eu) and other oxynitride phosphors, LSN phosphors (e.g., (La,Y)3Si6N 11 :Ce), BSESN phosphors (e.g., (Ba,Sr)2Si5N8:Eu), SLA phosphors (e.g., SrLiAl3N4:Eu), CASN phosphors (e.g., CaAlSiN3:Eu) or SCASN phosphors (e.g., (Sr,Ca)AlSiN3:Eu), nitride phosphors such as KSF phosphors (e.g., K2SiF6:Mn), KSAF phosphors (e.g., K2(Si 1-x Al x )F 6-x: Mn, where x satisfies 0 < x < 1), or fluoride-based phosphors such as MGF-based phosphors (e.g., 3.5MgO·0.5MgF2·GeO2:Mn), etc. Examples of quantum dots include quantum dots having a perovskite structure (e.g., (Cs,FA,MA)(Pb,Sn)(F,Cl,Br,I)3, where FA represents formamidinium and MA represents methylammonium), II-VI group quantum dots (e.g., CdSe), III-V group quantum dots (e.g., InP), quantum dots having a chalcopyrite structure (e.g., (Ag,Cu)(In,Ga)(S,Se)2), etc.

[0081] The light-emitting device 100 may include a covering member that covers the side surfaces of the light-emitting element 20 and the light-transmissive member 30 on the upper surface of the wiring substrate 1. The covering member is a member that protects the upper surface of the wiring substrate 1, the light-emitting element 20, and the light-transmissive member 30, and is disposed with the upper surface of the light-transmissive member 30 exposed.

[0082] The covering member can be formed of a resin having light reflectivity, light transmissivity, light-shielding property, etc., a resin containing a light-reflective substance in these resins, etc. The covering member preferably has at least one of light reflectivity and light-shielding property. Examples of the resin include resins containing one or more of silicone resin, modified silicone resin, epoxy resin, modified epoxy resin, acrylic resin, or hybrid resin. Examples of the light-reflective substance include titanium oxide, silicon oxide, zirconium oxide, potassium titanate, aluminum oxide, aluminum nitride, boron nitride, mullite, etc. The covering member may contain a phosphor, a diffusing material, a coloring agent, etc.

[0083] The light emitting device 100 having the above-mentioned configuration includes a wiring board 1 on whose upper surface the light emitting element 20 is arranged and on whose lower surface the heat sink 90 is joined. One of the element electrodes 21 is connected to the buried wiring 42 from the pad portion 45 on the upper surface through the via wiring 43, and is connected to the exposed wiring 41 that returns to the upper surface through another via wiring 43 and leads to the terminal portion 46. This allows the light emitting device 100 to arrange the terminal portion 46 connected to the external wiring on the first surface 10A, thereby increasing the degree of freedom in arranging the light emitting element 20. In addition, the lower surface of the wiring board 1 is insulated from the buried wiring 42 and is formed flat, and can be joined to the flat surface of the heat sink 90 by a conductive joining member 95. This allows the light emitting device 100 to increase the thermal bonding between the wiring board 1 and the heat sink 90, thereby improving the heat dissipation.

[0084] [Manufacturing method of light emitting device] Next, a method S100 for manufacturing a light emitting device according to an embodiment will be described with reference to the drawings. Fig. 9 is a flow chart illustrating the method S100 for manufacturing a light emitting device. Fig. 10A is a cross-sectional view illustrating an outline of a prepared wiring board 1. Fig. 10B is a cross-sectional view illustrating an outline of a state in which a light emitting element 20 is arranged on the wiring board 1. Fig. 10C is a cross-sectional view illustrating an outline of a state in which a heat sink 90 is bonded to the wiring board 1.

[0085] The manufacturing method S100 of the light emitting device includes preparing a wiring board manufactured by the manufacturing method S1 of the wiring board S1, S110, and arranging a light emitting element on the wiring board, S120. In arranging the light emitting element on the wiring board, S120, the metal member 40 of the wiring board 1 and the element electrode 21 are electrically connected. Here, the manufacturing method S100 of the light emitting device further includes joining a heat sink 90, S130, after arranging the light emitting element, S120. Each component of the manufacturing method S100 of the light emitting device will be described below.

[0086] (Prepare the wiring board) In preparing a wiring board S110 (hereinafter referred to as step S110), a wiring board 1 manufactured by a wiring board manufacturing method S1 is prepared. In the wiring board 1, the first surface 10A side on which the light emitting elements 20 are arranged is set as the upper surface, and pad portions 45 of the metal member 40 are formed according to the size and arrangement of the light emitting elements 20, the interval between a pair of element electrodes 21, and the like.

[0087] (Placing light-emitting elements) In arranging the light emitting elements S120 (hereinafter referred to as step S120), the light emitting elements 20 are arranged with the element electrodes 21 facing the wiring board 1. The light emitting elements 20 can be arranged in rows and columns on the wiring board 1. The element electrodes 21 are fixed to and electrically connected to the pad portions 45 of the metal member 40 by the conductive members 70. The connection by the conductive members 70 may be made by arranging bumps of gold, solder, or the like on the element electrodes 21 or the pad portions 45 and applying pressure and heat, or may be made by applying a conductive paste material and curing it.

[0088] The light-transmitting member 30 is disposed in advance on the upper surface of the light-emitting element 20. The light-transmitting member 30 can be disposed by applying the material of the uncured light-transmitting member 30 by, for example, potting, spraying, inkjet printing, printing, or the like, and then curing the material. The light-transmitting member 30 may be a sheet-like or plate-like member disposed on the upper surface of the light-emitting element 20 via a light-transmitting adhesive, or the light-emitting element 20 on which the light-transmitting member 30 has not been disposed in advance may be disposed on the wiring board 1, and then the light-transmitting member 30 may be disposed on the upper surface of the light-emitting element 20.

[0089] (Joining the heat sink) In joining a heat sink S130 (hereinafter referred to as step S130), a heat sink 90 is joined to the second surface 10B of the wiring board 1 on which the light emitting element 20 is arranged via a joining member 95. It is preferable that the surface of the heat sink 90 that is joined to the wiring board 1 is flat.

[0090] Step S130 can be performed by applying uncured bonding member 95, which is a paste-like solder or brazing material, a paste containing powdered Ag, or the like, to one or both of wiring board 1 and heat sink 90, and heating while applying pressure. Since second surface 10B side of wiring board 1 is insulated, conductive bonding member 95 can be used.

[0091] The manufacturing method S100 of the light emitting device may further include disposing a covering member after step S120 and before or after step S130. The covering member can be disposed, for example, by discharging an uncured resin material from a dispenser nozzle, applying it, and then curing it. The upper surface of the covering member is preferably formed so as to be flush with the upper surface of the light-transmitting member 30. In disposing the covering member, the covering member may further be polished, or the covering member and the light-transmitting member 30 may be polished.

[0092] In the manufacturing method S100 for a light emitting device having the above-mentioned configuration, by arranging the light emitting element 20 on the wiring board 1 with improved thermal coupling with the heat sink 90, a light emitting device 100 with high heat dissipation properties can be manufactured.

[0093] The present disclosure includes the following embodiments: [Section 1] an insulating base material having a first surface and a second surface opposite to the first surface, a groove provided on the second surface side, and a through hole connecting a bottom surface of the groove on the second surface and the first surface; a metal member disposed on a bottom surface side of the groove portion and in the through hole away from an opening of the groove portion; an insulating member disposed so as to close the opening of the groove. [Section 2] 2. The wiring board according to item 1, wherein the insulating member is disposed in the groove, and a surface of the insulating member and the second surface are flush with each other. [Section 3] 3. The wiring board according to item 1 or 2, wherein the metal member disposed in the groove has a curved surface. [Section 4] The groove is continuous with the second surface via a curved surface that widens toward the opening side, 4. The wiring board according to claim 1, wherein the insulating member is disposed in the groove with a width greater than that of the metal member. [Section 5] 5. The wiring board according to any one of items 1 to 4, wherein the base material has a recess on the first surface, and the through hole is provided at the position of the recess. [Section 6] the wiring board has pads arranged on the first surface at positions to which circuit components are connected, and terminals arranged at positions to which external wiring is connected, 6. The wiring board according to claim 1, wherein the pad portion and the terminal portion are electrically connected to the metal member disposed in the through hole. [Section 7] 7. The wiring board according to claim 1, wherein the insulating member is made of a ceramic or a resin. [Section 8] 8. The wiring board according to claim 1, wherein the substrate is made of a ceramic material. [Section 9] 9. The wiring board according to any one of items 1 to 8, wherein the base material includes at least one of silicon nitride, aluminum nitride, boron nitride, magnesium oxide, and aluminum oxide. [Section 10] 10. The wiring board according to claim 1, wherein the metal member includes at least one of Cu, Cr, Ni, Ag, Al, Zn, Sn, and an Ag-Cu alloy. [Section 11] 11. The wiring board according to claim 1, wherein the metal member has a metal compound layer at an interface between the base material and the metal member. [Section 12] A wiring board according to any one of items 1 to 11, a light-emitting element having an element electrode, the light-emitting element being disposed on the first surface side of the wiring substrate; The metal member of the wiring board is electrically connected to the element electrode. [Section 13] preparing a substrate having a first surface and a second surface opposite to the first surface, a through hole penetrating the first surface and connecting the first surface and the second surface, and a groove portion connected to the through hole and located on the second surface; Placing a conductive paste containing at least a metal powder, an active metal powder, and an organic solvent in the groove and the through hole; Firing the conductive paste to obtain a metal member; and arranging an insulating member so as to cover the opening of the groove. [Section 14] Item 14. The method for manufacturing a wiring board according to item 13, wherein, in disposing the conductive paste, the metal powder contained in the conductive paste is, by weight percentage, 60% or more and 90% or less, the active metal powder is, by weight percentage, 1% or more and 10% or less, and the organic solvent is, by weight percentage, 5% or more and 30% or less. [Section 15] Item 15. The method for manufacturing a wiring board according to item 13 or 14, wherein, in obtaining the metal member, the metal member is disposed on a bottom side of the groove and in the through hole away from an opening of the groove. [Section 16] 16. The method for manufacturing a wiring board according to any one of items 13 to 15, wherein in obtaining the metal member, the metal member is formed to have a curved surface. [Section 17] After obtaining the metal member, the method further includes removing a portion of the base material and the metal member to widen an opening of the groove portion so that the groove portion is continuous with the second surface via a curved surface that widens toward the opening side, Item 17. The method for manufacturing a wiring board according to any one of items 13 to 16, wherein, in arranging the insulating member, the insulating member is arranged in the groove with a width wider than that of the metal member. [Section 18] Item 18. The method for manufacturing a wiring board according to item 17, wherein the opening of the groove is widened by removing a part of the base material and the metal member by blasting. [Section 19] Item 19. The method for producing a wiring board according to any one of items 13 to 18, wherein the metal member is obtained by forming a metal compound layer at an interface between the substrate and the metal member, the metal compound layer being different from the active metal powder. [Section 20] 20. The method for manufacturing a wiring board according to any one of items 13 to 19, wherein in preparing the base material, the first surface further comprises a recess, and the through hole is provided at a position of the recess. [Section 21] 21. The method for manufacturing a wiring board according to any one of items 13 to 20, wherein in preparing the base material, the grooves and the through holes are formed by laser processing. [Section 22] 21. The method for manufacturing a wiring board according to any one of items 13 to 20, wherein in preparing the base material, the grooves are formed by blast processing, and the through holes are formed by laser processing. [Section 23] 23. The method for producing a wiring board according to any one of items 13 to 22, wherein the firing temperature in obtaining the metal member is 780° C. or higher and 1100° C. or lower. [Section 24] In obtaining the metal member, the firing atmosphere is 10 -5 24. The method for manufacturing a wiring board according to any one of items 13 to 23, wherein the atmosphere is a vacuum of 0.1 Pa or less or an Ar atmosphere of 99.9% or more. [Section 25] Item 21. The method for manufacturing a wiring board according to item 20, further comprising polishing the metal member after obtaining the metal member so that the first surface of the base material and the metal member form a flat surface on the same plane. [Section 26] Preparing a wiring board manufactured by the wiring board manufacturing method according to any one of items 13 to 25; and disposing a light emitting element having an element electrode on the wiring substrate; In the method for manufacturing a light emitting device, the metal member of the wiring board and the element electrode are electrically connected in arranging the light emitting element. [Explanation of symbols]

[0094] 1. Wiring board 1A Wiring board (modified version) 10 Base material 10A 1st side 10B 2nd side 14 Groove 14A aperture 14B Bottom 16 Recess 18 Through hole 20 Light emitting element 21 Element electrode 30 Translucent material 40 Metallic parts 41 Exposed wiring 42 Buried wiring 43 Via wiring 45 Pad section 46 Terminal section 50 Insulating material 60 Metal compound layer 61 compounds 70 Conductive materials 80 Conductive Paste 90 Heat sink 95 Joint Materials 100 Light emitting device

Claims

1. an insulating base material having a first surface and a second surface opposite to the first surface, a groove provided on the second surface side, and a through hole connecting a bottom surface of the groove in the second surface and the first surface; a metal member disposed on a bottom surface side of the groove portion and in the through hole away from an opening of the groove portion; an insulating member disposed so as to close the opening of the groove.

2. 2 . The wiring board according to claim 1 , wherein the insulating member is disposed in the groove, and a surface of the insulating member and the second surface are flush with each other.

3. The wiring board according to claim 1 , wherein the metal member disposed in the groove has a curved surface.

4. The groove is continuous with the second surface via a curved surface that widens toward the opening side, The wiring board according to claim 1 , wherein the insulating member is disposed in the groove with a width greater than that of the metal member.

5. The wiring board according to claim 1 , wherein the base material has a recess on the first surface, and the through hole is provided at the position of the recess.

6. the wiring board has pads arranged on the first surface at positions to which circuit components are connected, and terminals arranged at positions to which external wiring is connected, The wiring board according to claim 1 , wherein the pad portion and the terminal portion are electrically connected to the metal member disposed in the through hole.

7. 2. The wiring board according to claim 1, wherein the insulating member is made of a ceramic or resin material.

8. The wiring board according to claim 1 , wherein the base material is made of ceramics.

9. The wiring board according to claim 1 , wherein the base material contains at least one of silicon nitride, aluminum nitride, boron nitride, magnesium oxide, and aluminum oxide.

10. 2. The wiring board according to claim 1, wherein the metal member includes at least one of Cu, Cr, Ni, Ag, Al, Zn, Sn, and an Ag--Cu alloy.

11. The wiring board according to claim 1 , wherein the metal member has a metal compound layer at an interface between the base material and the metal member.

12. A wiring board according to any one of claims 1 to 11, a light-emitting element having an element electrode, the light-emitting element being disposed on the first surface side of the wiring substrate; The metal member of the wiring board is electrically connected to the element electrode.

13. preparing a substrate having a first surface and a second surface opposite to the first surface, a through hole penetrating the first surface and connecting the first surface and the second surface, and a groove portion connected to the through hole and located on the second surface; Placing a conductive paste containing at least a metal powder, an active metal powder, and an organic solvent in the groove and the through hole; Firing the conductive paste to obtain a metal member; and arranging an insulating member so as to cover the opening of the groove.

14. 14. The method for manufacturing a wiring board according to claim 13, wherein, in disposing the conductive paste, the metal powder contained in the conductive paste is, by weight percentage, 60% or more and 90% or less, the active metal powder is, by weight percentage, 1% or more and 10% or less, and the organic solvent is, by weight percentage, 5% or more and 30% or less.

15. The method for manufacturing a wiring board according to claim 13 , wherein in obtaining the metal member, the metal member is disposed on a bottom side of the groove and in the through hole away from an opening of the groove.

16. The method for manufacturing a wiring board according to claim 13, wherein in obtaining the metal member, the metal member is formed to have a curved surface.

17. After obtaining the metal member, the method further includes removing a portion of the base material and the metal member to widen an opening of the groove portion so that the groove portion is continuous with the second surface via a curved surface that widens toward the opening side, The method for manufacturing a wiring board according to claim 13 , wherein the insulating member is disposed in the groove with a width greater than that of the metal member.

18. The method for manufacturing a wiring board according to claim 17, wherein the widening of the opening of the groove comprises removing a part of the base material and the metal member by blasting.

19. The method for producing a wiring board according to claim 13, wherein the metal member is obtained by forming a metal compound layer made of the active metal powder at the interface between the base material and the metal member.

20. The method for manufacturing a wiring board according to claim 13 , wherein in preparing the base material, the first surface further comprises a recess, and the through hole is provided at a position of the recess.

21. The method for manufacturing a wiring board according to claim 13 , wherein in preparing the base material, the groove and the through hole are formed by laser processing.

22. The method for manufacturing a wiring board according to claim 13 , wherein in preparing the base material, the grooves are formed by blast processing, and the through holes are formed by laser processing.

23. The method for manufacturing a wiring board according to claim 13, wherein the firing temperature in obtaining the metal member is 780° C. or more and 1100° C. or less.

24. In obtaining the metal member, the firing atmosphere is 10 -5 14. The method for manufacturing a wiring board according to claim 13, wherein the atmosphere is a vacuum of 0.1 Pa or less or an Ar atmosphere of 99.9% or more.

25. The method for manufacturing a wiring board according to claim 20 , further comprising, after obtaining the metal member, polishing the metal member so that the first surface of the base material and the metal member form a flush, flat surface.

26. preparing a wiring board manufactured by the method for manufacturing a wiring board according to any one of claims 13 to 25; and disposing a light emitting element having an element electrode on the wiring substrate; In the method for manufacturing a light emitting device, the metal member of the wiring board and the element electrode are electrically connected in arranging the light emitting element.

Citation Information

Patent Citations

  • Device for mounting panel

    JP1981093940A