Thermoelectric conversion module and heat flow sensor
The use of Fe3Si in thermoelectric conversion modules addresses the high cost and material scarcity issues, enabling efficient power generation from room temperature to 400K.
Patent Information
- Application Number
- JP2023069438
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-20
- Publication Date
- 2024-10-31
- Estimated Expiration
- 2043-04-20
AI Technical Summary
Current thermoelectric conversion modules utilizing the anomalous Nernst effect face challenges due to high manufacturing costs and the need for rare materials, while those suitable for room temperature to 400K are not economically viable.
A thermoelectric conversion module using Fe3Si as the abnormal Nernst effect material, with a maximum absolute value of the abnormal Nernst coefficient of 2.0μV/K and standard deviation of 0.15μV/K or less in the range of 320K to 400K, allowing for efficient power generation in this temperature range.
The module provides an inexpensive solution suitable for room temperature to 400K, offering stable and efficient power generation characteristics.
Smart Images

Figure 2024155054000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a thermoelectric conversion module and a heat flow sensor. [Background technology]
[0002] Thermoelectric conversion modules are being actively developed to utilize unused thermal energy. Well-known thermoelectric conversion modules use the Seebeck effect, which can generate voltage from a temperature gradient.
[0003] In the Seebeck effect, a voltage is generated in the same direction as the temperature gradient, so thermoelectric conversion modules using the Seebeck effect have a complex three-dimensional structure with π-type structures as their building blocks. For this reason, it is difficult to make thermoelectric conversion modules using the Seebeck effect large-area or film-like. In addition, thermoelectric conversion modules using the Seebeck effect use rare materials, which poses the issue of high manufacturing costs. There are also issues from the viewpoint of toxicity.
[0004] In recent years, thermoelectric conversion modules using anomalous Nernst effect materials that generate electromotive force due to the anomalous Nernst effect have been proposed in addition to thermoelectric conversion modules that utilize the Seebeck effect. The anomalous Nernst effect is a phenomenon in which, when a temperature difference occurs due to a heat flow in a magnetic material, a voltage is generated in a direction perpendicular to both the magnetization direction and the temperature gradient.
[0005] The anomalous Nernst effect generates a voltage in a direction perpendicular to the temperature gradient. Therefore, a thermoelectric conversion module utilizing the anomalous Nernst effect has the advantage that it can be deployed along the heat source and can be easily made into a large area and a film.
[0006] For example, Patent Document 1 describes a thermoelectric conversion module that utilizes the anomalous Nernst effect, which has the composition formula Fe 3A first substance having a stoichiometric composition represented by X, wherein X is a typical element or a transition element, a second substance having an off-stoichiometric composition in which the composition ratio of Fe to X is deviated from that of the first substance, a third substance in which a part of the Fe sites of the first substance or a part of the Fe sites of the second substance is substituted with a typical metal element or a transition element other than X, and the composition formula is Fe 3 M1 1-x M2 x (0 < x < 1), wherein M1 and M2 are different typical elements from each other, or a fourth substance, or a fifth substance in which a part of the Fe sites of the first substance is substituted with a transition element other than X and a part of the sites of X is substituted with a typical metal element other than X. The first substance, the second substance, the third substance, the fourth substance, and the fifth substance exhibit an anomalous Nernst effect, and a thermoelectric conversion element is disclosed.
Prior Art Documents
Patent Documents
[0007]
Patent Document 1
Summary of the Invention
Problems to be Solved by the Invention
[0008] Currently, as a thermoelectric conversion module utilizing the anomalous Nernst effect, a thermoelectric conversion module using inexpensive materials is required. In addition, a thermoelectric conversion module suitable for use in a temperature range from room temperature to 400 K or less is required.
[0009]
Means for Solving the Problems
[0010] In order to solve the above problems, the present invention proposes the following means. <1> The thermoelectric conversion module according to the first aspect of the present invention comprises Fe 3 The present invention comprises an anomalous Nernst effect material containing Si, and when a magnetic field having a magnetic flux density of 2 T is applied, the maximum absolute value of the anomalous Nernst coefficient of the anomalous Nernst effect material is 2.0 μV / K or more in the range of 320 K to 400 K, The standard deviation of the absolute value of the anomalous Nernst coefficient is 0.15 μV / K or less in the temperature range of 320K to 400K. <2> A second aspect of the present invention is the thermoelectric conversion module of the first aspect, wherein the anomalous Nernst effect material is Fe 3 It may be a polycrystalline body of Si. <3> A third aspect of the present invention is the thermoelectric conversion module of the second aspect, wherein the polycrystalline body is Fe 3 Si D0 3 The structure may be <4> A heat flow sensor according to a fourth aspect of the present invention includes the thermoelectric conversion module according to the first to third aspects. Effect of the Invention
[0011] According to the above-described aspects of the present invention, it is possible to provide a thermoelectric conversion module and a heat flow sensor that are inexpensive and suitable for use in a temperature range from room temperature to 400K or less. [Brief description of the drawings]
[0012] [Figure 1] 1 is a schematic diagram illustrating a configuration of a thermoelectric conversion module according to a first embodiment. [Diagram 2] FIG. 1 is a schematic diagram showing the crystal structure of Fe3Si. [Diagram 3] FIG. 5 is a schematic diagram showing the configuration of a thermoelectric conversion module according to a second embodiment. [Figure 4] FIG. 11 is a plan view showing the configuration of a thermoelectric conversion module according to a third embodiment. [Diagram 5] FIG. 13 is a schematic diagram showing the configuration of a thermoelectric conversion module according to a fourth embodiment. [Figure 6] 1 is an XRD spectrum of an anomalous Nernst effect material of an embodiment. [Figure 7]FIG. 11 is a diagram showing the relationship between the temperature and the anomalous Nernst coefficient of the anomalous Nernst effect material of the embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] [First embodiment] Hereinafter, a thermoelectric conversion module 100 according to an embodiment of the present invention will be described with reference to the drawings. FIG. 1 is a schematic diagram showing the configuration of a thermoelectric conversion module 100 according to a first embodiment. As shown in FIG. 1, the thermoelectric conversion module 100 is made of Fe 3 The device comprises an anomalous Nernst effect material 1 containing Si, a first electrode 11, a second electrode 12, and a magnetic field application means 20. Each part will be described below.
[0014] (Anomalous Nernst effect material) In this embodiment, the anomalous Nernst effect material 1 is Fe 3 In this specification, the anomalous Nernst effect material has an anomalous Nernst coefficient S ANE This refers to materials with an absolute value of 1.0 μV / K or more. Anomalous Nernst effect material 1 is Fe 3 It may contain components other than Si, for example, Fe3Ga, Fe 3 Al, etc.
[0015] "The maximum absolute value of the anomalous Nernst coefficient of the anomalous Nernst effect material when a magnetic field with a magnetic flux density of 2 T is applied is 2.0 μV / K or more in the temperature range of 320 K to 400 K." In this embodiment, the maximum absolute value of the anomalous Nernst coefficient of the anomalous Nernst effect material 1 when a magnetic field with a magnetic flux density of 2T is applied is 2.0 μV / K or more in the range of 320K to 400K. Since the maximum absolute value of the anomalous Nernst coefficient of the anomalous Nernst effect material 1 when a magnetic field with a magnetic flux density of 2T is applied is 2.0 μV / K or more in the range of 320K to 400K, the thermoelectric conversion module 100 of the present disclosure can efficiently generate power in a temperature range from room temperature (e.g., 20°C) to 400K. It is preferable that the maximum absolute value of the anomalous Nernst coefficient of the anomalous Nernst effect material when a magnetic field with a magnetic flux density of 2T is applied is 2.0 μV / K or more in the range of 320K to 400K. The maximum absolute value of the anomalous Nernst coefficient of the anomalous Nernst effect material 1 is not particularly limited, but may be, for example, 50 μV / K or less. When using a thermoelectric power generation device or heat flow sensor in the range of 400 K or less, they are often used at temperatures above room temperature, including low-temperature parts such as heat sinks, and the temperature of the power generation device or sensor is often 320 K or higher, which is between room temperature and the higher temperature.
[0016] "The standard deviation of the absolute value of the anomalous Nernst coefficient measured at temperature intervals of 2 to 3 K in the temperature range of 320 K to 400 K when a magnetic field with a magnetic flux density of 2 T is less than 0.15 μV / K." In this embodiment, the standard deviation of the absolute values of the anomalous Nernst coefficient of the anomalous Nernst effect material 1 when a magnetic field with a magnetic flux density of 2 T is applied in a temperature range of 320 K to 400 K is 0.15 μV / K or less. It is preferable to determine the standard deviation of the absolute values of the anomalous Nernst coefficient from the absolute values of the anomalous Nernst coefficient obtained by measuring at temperature intervals of 2 to 3 K in the temperature range of 320 K to 400 K. Since the standard deviation of the absolute values of the anomalous Nernst coefficient is 0.15 μV / K or less in the temperature range of 320 K to 400 K, the thermoelectric conversion module 100 of the present disclosure can reduce the influence of temperature changes and generate electricity stably. When a magnetic field with a magnetic flux density of 2 T is applied and the temperature range is 320 K to 400 K, the standard deviation of the absolute value of the anomalous Nernst coefficient measured at temperature intervals of 2 to 3 K is preferably 0.10 μV / K or less, and more preferably 0.06 μV / K or less.
[0017] "Anomalous Nernst coefficient S ANE " Anomalous Nernst coefficient S ANE is expressed by the following formula (1). yy means the longitudinal resistance. α in Equation (1) yx means the transverse thermoelectric coefficient. σ in Eq. (1) yx means the Hall conductivity. S in formula (1) SE means the Seebeck coefficient.
[0018] Transverse thermoelectric coefficient α yx is expressed by the following formula (2). Here, ∂σ in the following formula (2) yx / ∂ε is the value at the Fermi level. k in the following equation (2) B is the Boltzmann constant. In the following formula (2), ε means energy, and in the following formula (2), e means elementary charge. In the following formula (2), T means the absolute temperature (K) of the measurement sample.
[0019] S ANE =ρ yy α yx -σ yx ρ yy S SE (1) α yx =-(π 2 / 3)·{(k B 2 T) / e}(∂σ yx / ∂ε) (2)
[0020] "Method for measuring the anomalous Nernst coefficient" The anomalous Nernst coefficient S of the anomalous Nernst effect material 1 mentioned above ANESpecifically, is measured as follows: A sample is cut into a flat plate (length L: 8 mm, width W: 1.5 mm, thickness t: 1 mm). One end of the cut sample is heated with a heater, and the other end is brought into contact with a heat sink, creating a temperature difference along the side L of the sample. A uniform temperature gradient is applied to the rectangular sample, and the temperature difference ΔT (K) is measured at two points separated by L_temp (mm). A magnetic field is applied in a direction perpendicular to this temperature difference, and the voltage (V) generated at two points separated by a distance W (mm) in a direction perpendicular to both the temperature difference and the magnetic field is measured. Anomalous Nernst coefficient S ANE is calculated from the obtained voltage (V) and other information using the following formula (3).
[0021] S ANE =(V / ΔT)×(L_temp / W)···(3)
[0022] "Fe 3 Si.” Anomalous Nernst effect material 1 is Fe 3 Polycrystalline Si or Fe 3 The anomalous Nernst effect material 1 is preferably a single crystal of Fe. 3 It is more preferable that the material is a polycrystalline body of Si. 3 Polycrystalline Si or Fe 3 Whether or not the material is a single crystal of Si can be determined by X-ray diffraction. The anomalous Nernst effect material 1 has an anomalous Nernst coefficient S ANE As long as the maximum absolute value of is 2.0μV / K or more, other components may be contained. The temperature of 320K to 400K is the temperature of the sample. A Celnox thermometer is placed in two places on the sample, one close to the heater and one close to the heat sink, and heat is applied from the heater in a step function manner to introduce a temperature gradient into the sample. The average temperature of the two places is the average value over time until the temperature gradient is relaxed.
[0023] "D0 3 structure" Anomalous Nernst effect material 1 is Fe 3If Si, then Fe 3 Si is D0 as shown in Fig. 2 3 It is preferable that the anomalous Nernst effect material 1 has a structure of D0 3 Due to the structure, the thermoelectric conversion module 100 of this embodiment exhibits superior power generation characteristics in the range from room temperature to 400 K. 3 The unit cell of the structure has eight body-centered cubic (bcc) subcells. In each subcell, a corner point is occupied by an Fe atom (Fe(II)), and each Fe(II) is shared by the eight adjacent subcells. Four of the eight subcells have four Fe atoms (Fe(I)) at their body centers, and the remaining four subcells have four Si atoms at their body centers. For example, D0 3 Structure of Fe 3 The lattice constant a of Si is 5.65 Å. 3 The lattice constant of Si can be measured by XRD.
[0024] The thickness of the anomalous Nernst effect material 1 is preferably 1.0 mm or more. By making the thickness 1.0 mm or more, the amount of generated current increases in the temperature range from room temperature to 400K or less.
[0025] (1st electrode 11) In the thermoelectric conversion module 100, the first electrode 11 is electrically connected to the anomalous Nernst effect material 1. The material of the first electrode is not particularly limited as long as it has electrical conductivity. For example, the material of the first electrode may be metals such as Au, Ag, Cu, and Al.
[0026] (2nd electrode 12) In the thermoelectric conversion module 100, the second electrode 12 is electrically connected to the anomalous Nernst effect material 1. The material of the second electrode is not particularly limited as long as it has electrical conductivity. For example, the material of the second electrode may be metals such as Au, Ag, Cu, and Al.
[0027] There is no particular limitation on the arrangement of the first electrode 11 and the second electrode 12. However, if there is a difference in temperature between the first electrode 11 and the second electrode 12, the Seebeck effect will be superimposed in addition to the anomalous Nernst effect, so for the heat flow sensor, it is preferable that the first electrode 11 and the second electrode 12 are arranged so that they are the same distance from the heat source.
[0028] (Magnetic field applying means 20) The magnetic field application means 20 is not particularly limited as long as it can apply a magnetic field in a direction perpendicular to the direction in which the temperature difference occurs and the direction in which the electromotive force is generated (the direction connecting the electrodes 11 and 12). Examples of the magnetic field application means 20 include a permanent magnet and an electromagnet.
[0029] (Thermoelectric Conversion Using Thermoelectric Conversion Module 100) 1, the thermoelectric conversion module 100 of this embodiment has a rectangular parallelepiped anomalous Nernst effect material 1 extending in one direction (Y direction in this embodiment), has a thickness of 0.1 μm or more in the thickness direction (Z direction in this embodiment), and is magnetized in the +X direction. A magnetic field is applied by a magnetic field application means 20. A known method can be used for applying the magnetic field.
[0030] When a heat flow Q flows in a direction (+Z direction in this embodiment) perpendicular to the direction of magnetization M (+X direction) through the anomalous Nernst effect material 1 of this embodiment, a temperature difference ΔT occurs in the +Z direction.
[0031] As a result, in the anomalous Nernst effect material 1, an electromotive force is generated in a direction (Y direction in this embodiment) perpendicular to both the direction of the heat flow Q (+Z direction) and the direction of the magnetization M (+X direction) due to the anomalous Nernst effect. As a result, the anomalous Nernst effect material 1 of this embodiment is capable of performing thermoelectric conversion.
[0032] (Method of manufacturing anomalous Nernst effect material 1) Anomalous Nernst effect material 1 is Fe 3 The manufacturing method of the anomalous Nernst effect material 1 will be described using a polycrystalline silicon as an example. 3The polycrystalline silicon can be produced, for example, by the following method. Fe and Si are arc-melted in a mono-arc furnace in an appropriate ratio, and cooled to obtain a D0 3 Fe with structure 3 The above-mentioned method can be used to produce polycrystalline Fe. 3 In the silicon polycrystalline body, the maximum absolute value of the anomalous Nernst coefficient of the anomalous Nernst effect material when a magnetic field of magnetic flux density 2 T is applied is 2.0 μV / K or more in the range of 320 K to 400 K, and the standard deviation of the absolute value of the anomalous Nernst coefficient of the anomalous Nernst effect material 1 when a magnetic field of magnetic flux density 2 T is applied is 0.15 μV / K or less. Therefore, when used in a temperature range from room temperature to 400 K or less, the thermoelectric conversion module of the present disclosure exhibits stable and excellent power generation characteristics.
[0033] The above describes the thermoelectric conversion module 100 according to the first embodiment. Since the anomalous Nernst effect material 1 in the thermoelectric conversion module 100 contains Fe and Si, the thermoelectric conversion module 100 is inexpensive and suitable for use in a temperature range from room temperature to 400 K or less.
[0034] Although the thermoelectric conversion module 100 includes the magnetic field application means 20, the thermoelectric conversion module 100 does not necessarily need to include the magnetic field application means 20.
[0035] Second Embodiment Next, a thermoelectric conversion module 100A according to the second embodiment will be described. Fig. 3 is a schematic diagram of the thermoelectric conversion module 100A.
[0036] As shown in FIG. 3, the thermoelectric conversion module 100A includes a substrate 30 and a power generating body 40 disposed on the substrate 30. As shown in FIG.
[0037] (Substrate 30) The substrate 30 has a first surface 30a on which the power generating body 40 is disposed, and a second surface 30b opposite to the first surface 30a. For example, the second surface 30b receives heat from a heat source (not shown). The material of the substrate 30 is not particularly limited. The material of the substrate 30 is preferably one having a high thermal conductivity. Examples of the material of the substrate 30 include AlN, Al 2 O 3 , MgO, BN, etc.
[0038] (1st electrode 11A) In the thermoelectric conversion module 100A, the first electrode 11A is electrically connected to one end of the power generation body 40. The material of the first electrode is not particularly limited as long as it has electrical conductivity. For example, the material of the first electrode may be metals such as Au, Ag, Cu, and Al.
[0039] (2nd electrode 12A) In the thermoelectric conversion module 100A, the second electrode 12A is electrically connected to the other end of the power generation body 40. The material of the second electrode is not particularly limited as long as it has electrical conductivity. For example, the material of the second electrode may be a metal such as Au, Ag, Cu, or Al.
[0040] (Power Generator 40) The power generating body 40 has one or more first anomalous Nernst effect materials 41 and one or more second anomalous Nernst effect materials 42. The first anomalous Nernst effect materials 41 and the second anomalous Nernst effect materials 42 may be the same as the anomalous Nernst effect material 1 described above.
[0041] One or more first anomalous Nernst effect materials 41 and one or more second anomalous Nernst effect materials 42 extend in one direction (here, the Y direction) within the plane of the first surface 30a and are arranged alternately in another direction (here, the X direction) that intersects with this one direction (orthogonal in the second embodiment).
[0042] The first anomalous Nernst effect material 41 has a first connection portion 41a protruding from one end (end on the +Y side) in one direction (Y direction) toward one side (-X side) in the other direction (X direction). On the other hand, the second anomalous Nernst effect material 42 has a second connection portion 42a protruding from the other end (end on the -Y side) in the one direction (Y direction) toward one side (-X side) in the other direction (X direction).
[0043] The first anomalous Nernst effect material 41 is electrically connected to one end (end on the +Y side) in one direction (Y direction) of the second anomalous Nernst effect material 42 via a first connection portion 41a. On the other hand, the second anomalous Nernst effect material 42 is electrically connected to the other end (end on the -Y side) of the first anomalous Nernst effect material 41 via a second connection portion 42a.
[0044] As a result, in the power generating body 40, the first anomalous Nernst effect material 41 and the second anomalous Nernst effect material 42 adjacent to each other are electrically connected in series, so that the power generating body 40 has a meandering shape.
[0045] The power generating body 40 and the first anomalous Nernst effect material 41 are arranged such that the direction of magnetization M1 (-X direction in the second embodiment) is opposite to the direction of magnetization M2 (+X direction in the second embodiment) of the second anomalous Nernst effect material 42. Furthermore, both the first anomalous Nernst effect material 41 and the second anomalous Nernst effect material 42 have anomalous Nernst coefficients with negative signs.
[0046] In the thermoelectric conversion module 100A, when a heat flow Q flows from the second surface 30b side of the substrate 30 toward the power generator 40, a temperature difference occurs in the power generator 40 in the direction of the heat flow, and a voltage V is generated in the power generator 40 due to the anomalous Nernst effect.
[0047] When the second surface 30b of the substrate 30 receives heat from the heat source, a heat flow Q flows in the +Z direction toward the power generator 40. At this time, in the first anomalous Nernst effect material 41, an electromotive force E1 is generated in a direction (+Y direction) perpendicular to both the direction of the magnetization M1 (-X direction) and the direction of the heat flow Q (+Z direction). On the other hand, in the second anomalous Nernst effect material 42, an electromotive force E2 is generated in a direction (-Y direction) perpendicular to both the direction of the magnetization M2 (+X direction) and the direction of the heat flow Q (+Z direction).
[0048] In the power generating body 40, the first anomalous Nernst effect material 41 and the second anomalous Nernst effect material 42 adjacent to each other are electrically connected in series. Therefore, the electromotive force E1 generated in the first anomalous Nernst effect material 41 and the electromotive force E2 generated in the second anomalous Nernst effect material 42 are added together, and the output voltage V can be increased.
[0049] In the thermoelectric conversion module 100A of the present embodiment, the temperature gradient, the magnetization direction, and the voltage direction are perpendicular to each other, so that it is possible to use the first anomalous Nernst effect material 41 and the second anomalous Nernst effect material 42 in thin sheet form.
[0050] Here, assuming that the length in the longitudinal direction (extension direction) of the first anomalous Nernst effect material 41 and the second anomalous Nernst effect material 42 is L1 and the thickness (height) is H1, when the temperature difference in the first anomalous Nernst effect material 41 and the second anomalous Nernst effect material 42 is constant, the voltage V generated by the anomalous Nernst effect is proportional to L1 / H1. In other words, the longer and thinner the first anomalous Nernst effect material 41 and the second anomalous Nernst effect material 42 are, the larger the obtained voltage V becomes.
[0051] Third Embodiment Next, a thermoelectric conversion module 100B according to a third embodiment will be described. Fig. 4 is a plan view of the thermoelectric conversion module 100B. The thermoelectric conversion module 100B includes a substrate 30 and a power generation body 40B disposed on the substrate 30.
[0052] (Power generating body 40B) The power generating body 40B has a plurality of anomalous Nernst effect materials 45 and wiring 50.
[0053] "Abnormal Nernst effect material 45" The anomalous Nernst effect material 45 may be made of the same material as the anomalous Nernst effect material 1. The anomalous Nernst effect materials 45 are arranged in parallel on the substrate 30 in a direction (X direction) perpendicular to the extension direction (Y direction) so that the directions of the magnetization M1A are the same (-X direction).
[0054] "Wiring 50" In the thermoelectric conversion module 100B, one end of the wiring 50 is electrically connected to one end side (-Y side) of the anomalous Nernst effect material 45, and the other end is electrically connected to the other end side (+Y side) of another adjacent anomalous Nernst effect material 45. This electrically connects the anomalous Nernst effect materials 45 in series. The material of the wiring 50 is not particularly limited as long as it has conductivity. For example, the material of the wiring 50 may be metal such as Au, Ag, Cu, or Al.
[0055] The heat flow Q flows from the substrate 30 side to the power generating body 40B side (flows in the +Z direction). The thermoelectric conversion module 100B can be manufactured more easily than the thermoelectric conversion module 100A because the adjacent anomalous Nernst effect materials 45 are connected via the wiring 50.
[0056] [Fourth embodiment] Next, a thermoelectric conversion module 100C according to a fourth embodiment will be described. Fig. 5 is a schematic diagram showing the configuration of the thermoelectric conversion module 100C.
[0057] 5, the thermoelectric conversion module 100C includes a substantially cylindrical hollow member 31 and a long sheet-like anomalous Nernst effect material 32 spirally wound around the outer circumferential surface of the hollow member 31. The anomalous Nernst effect material 32 may be the same as the anomalous Nernst effect material 1. The anomalous Nernst effect material 32 is magnetized in a direction parallel to the axial direction (X direction) of the hollow member 31.
[0058] In the thermoelectric conversion module 100C, when the inside of the hollow member 31 is hotter than the outside, the heat flow P flows from the inside to the outside of the hollow member 31, and a temperature gradient (temperature difference) occurs from the inside to the outside of the hollow member 31. This generates a voltage V in the anomalous Nernst effect material 32. In this embodiment, an electromotive force is generated along the longitudinal direction of the anomalous Nernst effect material 32 (the direction perpendicular to both the magnetization direction and the heat flow direction).
[0059] In the thermoelectric conversion module 100C of this embodiment, the temperature gradient, the magnetization direction, and the voltage direction are perpendicular to each other, so that it is possible to use a thin sheet-like anomalous Nernst effect material 32.
[0060] As shown in formula (4), the electromotive force generated by the anomalous Nernst effect increases as the length of the anomalous Nernst effect material increases. Therefore, in the thermoelectric conversion module 100C of this embodiment, by employing the long sheet-like anomalous Nernst effect material 32 wound in a spiral shape around the outer circumferential surface of the hollow member 31 described above, the length of the anomalous Nernst effect material can be increased, and a further increase in the voltage V can be expected.
[0061] The present invention is not limited to the configurations of the above-described embodiments, and various modifications can be made without departing from the spirit of the present invention. For example, the above-mentioned thermoelectric conversion modules 100, 100A, 100B, and 100C can be applied to various devices. For example, by providing the thermoelectric conversion modules 100, 100A, 100B, and 100C in a heat flow sensor, it is possible to determine whether the thermal insulation performance of a building is good or bad.
[0062] In addition, by installing thermoelectric conversion modules 100, 100A, 100B, and 100C in an exhaust device of a motorcycle or the like, electricity can be generated by utilizing the heat (waste heat) of the exhaust gas, and the thermoelectric conversion modules 100, 100A, 100B, and 100C can be effectively used as auxiliary power sources.
[0063] Furthermore, the thermoelectric conversion modules 100, 100A, 100B, and 100C of the present embodiment can be provided with not only the function as the thermoelectric conversion element described above, but also the function of temperature modulation (particularly cooling) by supplying electric power, like a Peltier element. EXAMPLES
[0064] The effects of the present invention will be more clearly understood by the following examples. Note that the present invention is not limited to the following examples, and can be modified as appropriate without departing from the spirit and scope of the present invention.
[0065] (Preparation of anomalous Nernst effect material of the embodiment) An appropriate ratio of Fe and Si was placed in a mono-arc furnace (step 1). Next, a rotary pump and a turbo molecular pump were used to evacuate the furnace to an ultimate pressure of 0.2 Pa. Then, Ar purging was performed three times, and the furnace was filled with argon gas up to 0.08 MPa. After filling with argon gas, an arc discharge was started (step 2). After the arc discharge started, an arc discharge was performed under a condition of 4 amperes to melt the metal, and the molten state was maintained for 10 to 15 seconds (step 3). After waiting about 1 minute until the temperature reached room temperature, the obtained metal material was turned over (step 4). The process from step 2 to step 4 was repeated 6-7 times to produce an anomalous Nernst effect material.
[0066] (XRD) XRD was measured using a Rigaku Smart Lab X-ray diffractometer, with the samples ground into powder and then loaded into a sample holder.
[0067] (Anomalous Nernst coefficient) The anomalous Nernst coefficient was calculated as follows. A flat sample (approximately L=8mm, W=1.5mm, t=1mm) for evaluation was cut out from the anomalous Nernst effect material. One end of the sample was heated with a heater, and the other end was brought into contact with a heat sink, creating a temperature difference along the edge L of the sample. Thermocouples were placed at two points separated by L_temp on the sample to measure the temperature difference ΔT. A magnetic field with a magnetic flux density of 2T was applied in a direction perpendicular to this temperature difference and perpendicular to the surface of the flat sample. The voltage V generated at two points separated by a distance W was measured in a direction perpendicular to both the temperature difference and the magnetic field. The anomalous Nernst coefficient was calculated from the voltage when a magnetic field with a magnetic flux density of 2T was applied, based on the above formula (3).
[0068] The XRD diffraction peaks are shown in Figure 6. As a result of the XRD measurement, the anomalous Nernst effect material obtained above was found to be composed of Fe 3 It is a polycrystalline silicon, and its crystal structure is D0 3 It was also confirmed that Fe 3 The lattice constant of Si was 5.65 Å.
[0069] The measurement results of the anomalous Nernst coefficient of the anomalous Nernst effect material obtained above are shown in FIG. 7. The horizontal axis of FIG. 7 is temperature (K), and the vertical axis is anomalous Nernst coefficient (μV / K). As shown in FIG. 7, the anomalous Nernst effect material of the embodiment has a maximum absolute value of the anomalous Nernst coefficient of 2.0μV / K or more at 320K to 400K (in this embodiment, the absolute value of the anomalous Nernst coefficient is 2.0μV / K or more at 320K to 400K), and when the anomalous Nernst coefficient was measured at a temperature interval of 2 to 3K in the temperature range of 320K to 400K, the standard deviation of the absolute value of the anomalous Nernst coefficient was 0.05μV / K. Therefore, it was confirmed that the thermoelectric conversion module using the anomalous Nernst effect material of the embodiment exhibits stable and excellent power generation performance in the range of room temperature to 400K. [Explanation of symbols]
[0070] 1 anomalous Nernst effect material, 11 first electrode, 12 second electrode, 20 magnetic field application means, 100 thermoelectric conversion module
Claims
1. Fe 3 The anomalous Nernst effect material contains Si, the maximum absolute value of the anomalous Nernst coefficient of the anomalous Nernst effect material when a magnetic field having a magnetic flux density of 2 T is applied is 2.0 μV / K or more in the range of 320 K to 400 K; A thermoelectric conversion module, wherein the standard deviation of the absolute value of the anomalous Nernst coefficient is 0.15 μV / K or less in a temperature range of 320K to 400K.
2. The anomalous Nernst effect material is Fe 3 The thermoelectric conversion module according to claim 1 , which is a polycrystalline body of Si.
3. The polycrystalline body is D0 3 The thermoelectric conversion module according to claim 2 , having a structure.
4. A heat flow sensor comprising the thermoelectric conversion module according to any one of claims 1 to 3.
Citation Information
Patent Citations
Magnetic thermoelectric element and power generation method
JP2018078147A
Spin-orbit torque device
US20220158084A1
Thermoelectric conversion element and thermoelectric conversion device
WO2020218613A1
Thermoelectric conversion element
WO2023013704A1