Manufacturing method of electrode and electrode rolling device
By applying oil to the rolling rolls facing the unformed portion of the electrode sheet, the method prevents damage and wear, ensuring smooth rolling without interference.
Patent Information
- Application Number
- JP2023070057
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-21
- Publication Date
- 2024-10-31
- Estimated Expiration
- 2043-04-21
AI Technical Summary
Damage occurs to the unformed portion of an electrode sheet during the rolling process due to contact with rolling rolls, which can be caused by foreign objects or surface wear.
Supplying oil to the portion of the rolling rolls that faces the unformed portion of the electrode sheet to reduce friction and prevent damage.
Prevents the unformed portion of the electrode sheet from being caught and damaged by the rolling rolls, reducing wear and tear on the rolls.
Smart Images

Figure 2024155385000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing an electrode and an electrode rolling apparatus. [Background technology]
[0002] JP 2014-29806 A discloses an electrode manufacturing apparatus. The apparatus manufactures a belt-shaped electrode sheet. The manufactured belt-shaped electrode sheet has an uncoated region that is not coated with active material and extends in the longitudinal direction with a predetermined width at at least one end in the width direction of the electrode roll, and a coating section that continuously coats the remaining part in the width direction with active material in the longitudinal direction to form an active material layer. In the apparatus, an insulating material that becomes an insulating layer is applied in the longitudinal direction to an insulating region of a predetermined width set in advance along the boundary between the uncoated region and the coated region at least either before or after coating the active material on the electrode roll. In the electrode manufacturing apparatus, it is disclosed that the active material layer is formed and then roll-pressed. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2014-29806 A Summary of the Invention [Problem to be solved by the invention]
[0004] Incidentally, when the electrode sheet is pressed by the rolling rolls, damage may occur in the unformed portions. [Means for solving the problem]
[0005] The method for manufacturing an electrode disclosed herein includes a step of preparing an electrode sheet on which an active material layer containing an electrode active material is formed, except for an unformed portion set at at least one end in a width direction perpendicular to the longitudinal direction of a strip-shaped current collector foil, and a rolling step of rolling the active material layer by passing the electrode sheet between a pair of rolling rolls. In the rolling step, oil is supplied to at least a portion of the pair of rolling rolls facing the unformed portion. By supplying oil to at least a portion of the pair of rolling rolls facing the unformed portion, damage to the unformed portion is suppressed.
[0006] The electrode rolling device disclosed here is a device for rolling an electrode sheet including an electrode active material layer continuously applied along the longitudinal direction of a strip-shaped current collector foil and containing an electrode active material, and an unformed portion where the electrode active material layer is not disposed at at least one end in the width direction perpendicular to the longitudinal direction of the current collector foil. Here, the electrode rolling device includes a conveying device for feeding the electrode sheet along a predetermined conveying path, a pair of rolling rolls arranged on the conveying path along which the electrode sheet is conveyed, and an oil supplying mechanism for supplying oil to the surface of the rolling rolls in an area of the rolling rolls that sandwiches the unformed portion of the electrode sheet. In this case, too, the supply of oil to at least a portion of the pair of rolling rolls that faces the unformed portion suppresses damage to the unformed portion. [Brief description of the drawings]
[0007] [Figure 1] FIG. 1 is a front view showing a schematic diagram of an electrode rolling device 10. As shown in FIG. [Diagram 2] FIG. 2 is a side view that diagrammatically illustrates the rolling process carried out by the electrode rolling device 10. As shown in FIG. [Diagram 3] FIG. 3 is a graph showing the tendency of the amount of wear on the surfaces of the rolls 11 and 12. As shown in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] The disclosure herein is explained below. Unless otherwise specified, the disclosure herein is not intended to limit the invention described in the claims of this application. Each drawing is drawn diagrammatically and does not necessarily reflect the actual product. In addition, the same reference numerals are appropriately used for members and parts that perform the same function, and duplicated explanations are omitted. In this specification, a notation such as "X to Y" indicating a numerical range means "X or more and Y or less" unless otherwise specified.
[0009] Fig. 1 is a front view showing a schematic diagram of an electrode rolling apparatus 10. Fig. 2 is a side view showing a schematic diagram of a rolling process performed by the electrode rolling apparatus 10. Fig. 2 is a schematic diagram showing the pair of rolls 11, 12 as viewed from the side (the left side in Fig. 1) from which an electrode sheet 100 rolled by the pair of rolls 11, 12 exits. The electrode rolling apparatus 10 embodies the electrode manufacturing method disclosed herein.
[0010] The method for producing an electrode disclosed herein includes a step of preparing an electrode sheet 100 and a rolling step of rolling an active material layer. In the method for producing an electrode, the electrode sheet 100 is rolled, as shown in Fig. 2.
[0011] <Electrode sheet 100> The electrode sheet 100 is prepared in a step of preparing an electrode sheet 100. The electrode sheet 100 has an active material layer 103 containing an electrode active material formed thereon, except for an unformed portion 102 set at at least one end in the width direction perpendicular to the longitudinal direction of the strip-shaped current collecting foil. Such an electrode sheet 100 can be used as an electrode sheet for an electricity storage device, such as a positive electrode sheet or a negative electrode sheet for a lithium ion secondary battery.
[0012] Here, the term "electrode sheet" refers to an electrode sheet used in an electricity storage device, regardless of whether it is a positive electrode sheet or a negative electrode sheet. The term "electricity storage device" refers to a device capable of charging and discharging. The electricity storage device includes batteries generally called lithium ion batteries and lithium secondary batteries, as well as lithium polymer batteries and lithium ion capacitors. The secondary battery generally refers to a battery capable of repeated charging and discharging with the movement of charge carriers between the positive and negative electrodes. The electricity storage device may use an electrolyte or a solid electrolyte. For example, the secondary battery may be a secondary battery using a so-called liquid electrolyte, or a so-called all-solid-state battery using a solid electrolyte.
[0013] Here, the positive electrode sheet is a positive electrode current collector foil (e.g., aluminum foil) having a predetermined width and thickness, on both sides of which a positive electrode active material layer containing a positive electrode active material is formed, except for an unformed portion set at a certain width at one end of the width direction. For example, in a lithium ion secondary battery, the positive electrode active material is a material that can release lithium ions during charging and absorb lithium ions during discharging, such as a lithium transition metal composite material. In general, various positive electrode active materials have been proposed other than lithium transition metal composite materials, and are not particularly limited.
[0014] Here, the negative electrode sheet is a negative electrode current collector foil (copper foil in this case) of a predetermined width and thickness, on both sides of which a negative electrode active material layer containing a negative electrode active material is formed, except for an unformed portion set at a certain width on one edge in the width direction. In a lithium ion secondary battery, for example, the negative electrode active material is a material that can absorb lithium ions during charging, such as natural graphite, and release the lithium ions absorbed during charging during discharging. In general, various negative electrode active materials have been proposed other than natural graphite, and there is no particular limitation.
[0015] In the embodiment shown in FIG. 2, the electrode sheet 100 has an active material layer 103 provided in the middle of the width direction of a substrate made of a strip-shaped metal foil. The active material layer 103 is a layer containing active material particles, and is applied to a predetermined width of the middle of the width direction of the substrate at a predetermined thickness (basis weight) and is in a dried state. After the compression process, the electrode sheet 100 is cut at the middle of the width direction to obtain two electrode sheets. In the two obtained electrode sheets, the active material layer is formed in a portion excluding an unformed portion 102 set at one end of the width direction. The configuration of the electrode sheet 100 is not limited to the embodiment shown in FIG. 2.
[0016] For example, in this embodiment, protective layers 104 containing inorganic filler are provided on both ends in the width direction of the active material layer 103. The protective layers 104 may be provided on both ends in the width direction of the active material layer 103 in a coating process. The protective layers 104 may be formed by coating a paste material containing electrically insulating particles such as alumina. The protective layer 104 is a layer that protects the active material layer 103.
[0017] The protective layer 104 is provided, for example, when the electrode sheet 100 is a positive electrode sheet. The protective layer 104 is disposed so as to face the end of the negative electrode sheet. The end of the negative electrode sheet is cut in the manufacturing process of the negative electrode sheet, and therefore, burrs may be generated or metal foreign matter may be attached. The protective layer 104 prevents the end of the negative electrode sheet or the metal foreign matter from contacting the positive electrode current collector. For this reason, it is desirable that the protective layer 104 is not easily broken through even when burrs are generated on the end of the negative electrode sheet or when there is a metal foreign matter.
[0018] An inorganic filler may be used for the electrically insulating particles contained in the protective layer 104. In addition to alumina, examples of the inorganic filler that may be used include boehmite, silica, mica, and hydrous magnesium silicate. Boehmite is less expensive than alumina, so the manufacturing cost of the secondary battery can be kept low. In addition to boehmite, examples of the inexpensive inorganic filler that may be used include silica and hydrous magnesium silicate.
[0019] 1, in the rolling step, the electrode sheet 100 is passed between a pair of rolling rolls 11 and 12 to roll out the active material layer 103. By rolling the active material layer 103, the electrode sheet 100 including the active material layer 103 is adjusted to an appropriate thickness.
[0020] Incidentally, the present inventor has found that when the electrode sheet 100 is sandwiched and rolled between the rolling rolls 11 and 12, an event occurs in which the unformed portion 102 breaks. The present inventor believes that when a foreign object is attached to either the rolling rolls 11 and 12 or the unformed portion 102, the unformed portion 102 gets caught by the rolling rolls 11 and 12 and is damaged.
[0021] FIG. 3 is a graph showing the tendency of the wear amount of the surface of the rolling rolls 11, 12. FIG. 3 shows the relationship between the position in the width direction of the rolling rolls 11, 12 and the wear amount of the surface of the rolling rolls 11, 12. The surfaces of the rolling rolls 11, 12 are worn due to long-term use. FIG. 3 shows the wear amount of the portion where the unformed portion 102, the protective layer 104, and the active material layer 103 contact from the left at the end of one side in the width direction of the electrode sheet 100. Here, the region A in FIG. 3 is approximately the portion where the unformed portion 102 of the electrode sheet 100 contacts. The region B in FIG. 3 is approximately the portion where the protective layer 104 formed on the edge of the active material layer 103 of the electrode sheet 100 contacts. The region C in FIG. 3 is approximately the portion where the active material layer 103 of the electrode sheet 100 contacts.
[0022] As shown in FIG. 3, the surfaces of the rolling rolls 11 and 12 are worn down with use. At this time, the portion C with which the active material layer 103 contacts is most likely to wear down, followed by the portion B with which the protective layer 104 contacts. The portion A with which the unformed portion 102 contacts tends to be less susceptible to wear. As a result, with use, the rolling rolls 11 and 12 experience a difference in the amount of wear between the portion C with which the active material layer 103 contacts and the portion A with which the unformed portion 102 contacts. For this reason, a step is generated on the surfaces of the rolling rolls 11 and 12 between the portion A with which the unformed portion 102 contacts and the portion C with which the active material layer 103 contacts.
[0023] In the example shown in FIG. 3, the protective layer 104 is provided on the edge of the active material layer 103 of the electrode sheet 100. In this case, as shown in FIG. 3, almost no wear is observed at the end of the portion A of the rolling rolls 11 and 12 where the unformed portion 102 comes into contact. In contrast, wear is observed toward the edge of the protective layer 104. Furthermore, in the portion facing the protective layer 104, wear is large in the vicinity S1 of the edge of the protective layer 104, and wear is also large toward the edge of the active material layer 103. Wear is observed to be significantly larger in the portion C where the active material layer 103 comes into contact than in the portion A where the unformed portion 102 comes into contact and the portion B where the protective layer 104 comes into contact.
[0024] In the example shown in Fig. 3, a step S3 of about 35 µm occurs due to the difference in the amount of wear between part C where active material layer 103 contacts and part A where unformed portion 102 contacts. If such a step S3 occurs in rolling rolls 11, 12, it can cause unformed portion 102 of electrode sheet 100 to get caught. Unformed portion 102 is formed of a thin metal foil. For this reason, if an end of unformed portion 102 gets caught on rolling rolls 11, 12, it can cause damage to unformed portion 102, such as breaking of unformed portion 102 starting from the caught portion.
[0025] In the electrode manufacturing method proposed here, as shown in FIG. 2, oil 30 is supplied to at least the portion of the pair of rolling rolls 11, 12 facing the unformed portion 102 in the rolling step.
[0026] By supplying the oil 30 to at least the portion of the pair of rolling rolls 11, 12 facing the unformed portion 102, the unformed portion 102 becomes slippery even when the unformed portion 102 comes into contact with the pair of rolling rolls 11, 12. Therefore, even if a foreign object is attached to either the rolling rolls 11, 12 or the unformed portion 102, or if a step occurs on the surface of the rolling rolls 11, 12 due to wear, the unformed portion 102 of the electrode sheet 100 is unlikely to get caught by the rolling rolls 11, 12, and the unformed portion 102 is unlikely to be damaged.
[0027] For example, as shown in FIG. 3, the oil 30 may be supplied to the portion A where the unformed portion 102 comes into contact. In addition, when the electrode sheet 100 has a protective layer 104, the oil 30 may be supplied so as to cover the portion B where the protective layer 104 comes into contact. It is preferable that the oil 30 does not remain on the active material layer 103. For this reason, it is preferable that the oil 30 is not supplied so as to cover the portion C where the active material layer 103 comes into contact. Note that if the oil 30 is volatile and does not remain over time, there is no problem even if the oil adheres to the active material layer 103. In this case, a part of the oil 30 may be applied to the active material layer 103.
[0028] For example, when the width of the unformed portion 102 of the electrode sheet 100 is taken as 100%, the oil 30 is preferably supplied to the region of the rolling rolls 11 and 12 facing the unformed portion 102 of the electrode sheet 100 at a width of 80 to 120%. Also, for example, as shown in Fig. 3, when the electrode sheet 100 has a protective layer 104, when the combined width T1 of the unformed portion 102 and the protective layer 104 is taken as 100%, the width T2 to which the oil 30 is applied is set at a width of 80 to 120%, and the oil 30 is preferably supplied to the region of the rolling rolls 11 and 12 facing the unformed portion 102 and the protective layer 104 of the electrode sheet 100. For example, if the width T1 of the unformed portion 102 (including the protective layer 104) of the electrode sheet 100 is 35 mm, then, as shown in FIG. 2, oil 30 may be supplied to both ends of the width direction of the portion through which the electrode sheet 100 passes, with a width of 30 mm or more and 40 mm or less.
[0029] Although it is not necessarily necessary to supply the oil 30 to all areas facing the unformed portions 102 of the electrode sheet 100, according to the knowledge of the present inventor, it is preferable to supply the oil 30 to a portion facing the end of the electrode sheet 100 on the side where the unformed portions 102 are formed. By supplying the oil 30 to a portion facing the end of the electrode sheet 100 on the side where the unformed portions 102 are formed, the end of the unformed portions 102 of the electrode sheet 100 is less likely to get caught by the rolling rolls 11, 12, and damage to the unformed portions 102 of the electrode sheet 100 caused by the end of the unformed portions 102 of the electrode sheet 100 getting caught by the rolling rolls 11, 12 can be suppressed.
[0030] According to the findings of the present inventors, for example, the oil 30 may be supplied to both ends in the width direction of the pair of rolling rolls, particularly the part corresponding to the electrode sheet 100. In the rolling process, the oil 30 may be applied to both ends in the width direction of the pair of rolling rolls through which the electrode sheet 100 passes, with a width of 30 mm to 40 mm. In this case, the oil 30 is applied to the rolling rolls 11 and 12 with a sufficient width for the end of the unformed portion 102 of the electrode sheet 100. Therefore, even if the end of the unformed portion 102 of the electrode sheet 100 comes into contact with the rolling rolls 11 and 12, it is unlikely to be caught by the rolling rolls 11 and 12, and the unformed portion 102 is unlikely to be damaged.
[0031] In the rolling process, oil may be supplied to the circumferential side surfaces of the rolling rolls 11 and 12 downstream in the conveying direction of the electrode sheet 100. In this case, the oil 30 becomes familiar with the surfaces of the rolling rolls 11 and 12 after being supplied thereto and before reaching the portion of the electrode sheet 100 to be rolled, so that unevenness of the oil 30 is suppressed to a small extent.
[0032] As shown in Fig. 2, the electrode sheet 100 may be provided with a protective layer 104 containing an inorganic filler on the edge of the active material layer 103. In this case, the oil 30 may be supplied to at least a part of the region of the rolling rolls 11, 12 that faces the protective layer 104. This makes the protective layer 104 and the unformed portion 102 slip easily on the surfaces of the rolling rolls 11, 12 and less likely to get caught by the rolling rolls 11, 12. Therefore, even if a step occurs on the surface of the rolling rolls 11, 12 due to the protective layer 104 or a foreign matter adheres to the part, the unformed portion 102 is less likely to be damaged.
[0033] Here, the oil 30 to be supplied is preferably one that volatilizes and disappears over time and does not remain on the electrode sheet 100. For example, an isoparaffin-based hydrocarbon solvent or the like can be used. For example, a commercially available oil such as Aqua Chemical Co., Ltd.'s non-cleaning processing oil GS-5A or GS-7A can be used as the oil 30. The oil 30 to be supplied is preferably one that can keep the friction between the pair of rolling rolls 11, 12 and the electrode sheet 100 low and can volatilize and disappear over time. From this perspective, the oil 30 is not limited to the above. As the oil 30 to be supplied to the surfaces of the rolling rolls 11, 12, various oils having similar functions can be used in addition to the above isoparaffin-based hydrocarbon solvents.
[0034] Various methods can be considered for supplying the oil 30. The present inventors have considered applying the oil 30 to a predetermined area on the surface of the reduction rolls 11 and 12. In this case, it is easy to control the width and amount of the oil 30 to be supplied, and it is easy to supply an appropriate amount of oil 30 to an appropriate area.
[0035] The electrode rolling apparatus 10 shown in FIG. 1 embodies such an electrode manufacturing method. As shown in FIG. 1, the electrode rolling device 10 includes a transport device 40, a pair of rolling rolls 11 and 12, and an oil supply mechanism 14.
[0036] The conveying device 40 may be a device that conveys the strip-shaped electrode sheet 100 along a predetermined conveying path 40a. As shown in FIG. 1, the conveying device 40 may be a device that conveys the strip-shaped electrode sheet 100 along a predetermined conveying path 40a in a roll-to-roll manner. In this case, the strip-shaped electrode sheet 100 before rolling may be wound up on a roll 41 in advance and prepared. The conveying device 40 may send out the electrode sheet 100 from the roll 41 along the conveying path 40a, pass the electrode sheet 100 through a pair of rolling rolls 11 and 12, and then wind the rolled electrode sheet 100 on a roll 42.
[0037] <A pair of rolling rolls 11, 12> The pair of rolling rolls 11, 12 are disposed on the conveying path 40a along which the electrode sheet 100 is conveyed. The pair of rolling rolls 11, 12 may each be a cylindrical roll. As described above, the surfaces of the rolling rolls 11, 12 are worn with use, so that the rolling rolls 11, 12 may be replaceable members. The pair of rolling rolls 11, 12 may each be configured to rotate along the conveying direction of the conveying path 40a along which the electrode sheet 100 is conveyed. Although not shown, the pair of rolling rolls 11, 12 are incorporated in a press machine, and the distance between them is adjusted. The press machine applies a force P to the rotating shafts 11a, 12a of the pair of rolling rolls 11, 12 in the directions facing each other. As a result, the electrode sheet 100 passing through the pair of rolling rolls 11, 12 is rolled.
[0038] <Oil supply mechanism 14> The oil supply mechanism 14 is a mechanism that supplies oil to the surfaces of the rolling rolls 11, 12 in the regions of the rolling rolls 11, 12 that sandwich the unformed portion 102 of the electrode sheet 100. In this embodiment, as shown in FIG. 1, the oil supply mechanism 14 includes a mechanism 14A that supplies oil 30 to the outer circumferential surface of the rolling roll 11, and a mechanism 14B that supplies oil 30 to the outer circumferential surface of the rolling roll 12. In this embodiment, the oil supply mechanism 14 is configured as a mechanism that applies oil 30 to the surfaces of the rolling rolls 11, 12. The oil supply mechanisms 14A, 14B each include an application member 51 and a supply member 52.
[0039] <Coating member 51> Here, the application member 51 is a member that is brought into contact with each of the pair of rolling rolls 11, 12. The application member 51 is preferably a member that can be soaked with the oil 30, such as felt, sponge, or nonwoven fabric. In addition, since the application member 51 is pressed against the pair of rolling rolls 11, 12 with a required force, it is preferable to use a member that has good slip properties, abrasion resistance, and water retention (oil retention). In this embodiment, the application member 51 is attached to the tip of an arm 51a.
[0040] <Supply member 52> The supply member 52 is a member that supplies the oil 30 to the application member 51. The supply member 52 is attached, for example, along the arm 51a, and may be configured as a pipe that supplies the oil 30 to the application member 51. As shown in FIG. 1, the oil supply mechanism 14 may include a tank 53, a pump 54, and a check valve 55, which may be connected to each other by a pipe 56. The oil may be supplied from the tank 53 to the supply member 52 through the pipe 56 by the pump 54, and the oil 30 may be further supplied from the supply member 52 to the application member 51. The check valve 55 is a device that prevents the oil 30 from flowing back.
[0041] 1, the oil supply mechanism 14 includes application members 51 that contact the pair of rolls 11, 12, respectively, and a supply member 52 that supplies oil to the application members 51. This allows oil 30 to be continuously supplied to the surfaces of the pair of rolls 11, 12 through the application members 51.
[0042] The oil supply mechanism 14 may include a spring mechanism 61 that biases the application member 51 toward each of the pair of rolling rolls. For example, the angle of the arm 51a may be variable, and the spring mechanism 61 may be configured to press the application member 51 attached to the tip of the arm 51a toward the surfaces of the pair of rolling rolls 11, 12. By providing a spring mechanism that biases the application member 51 toward each of the pair of rolling rolls 11, 12, the application member 51 is pressed against the surfaces of the rolling rolls 11, 12 with a stable strength. For this reason, oil can be stably supplied to the surfaces of the rolling rolls 11, 12. In addition, since the oil 30 is stably supplied to the surfaces of the rolling rolls 11, 12, damage to the unformed portion 102 caused by the electrode sheet 100 getting caught on the rolling rolls 11, 12 is prevented. The specific structure of the spring mechanism 61 may have various configurations. For example, a spring (not shown) that generates an elastic reaction force so that the arm 51a is inclined toward the surfaces of the pair of rolls 11 and 12 may be incorporated in the angle adjustment mechanism of the arm.
[0043] The oil supply mechanism 14 is configured such that, in the circumferential direction of the rolling rolls 11, 12, the applicator 51 is pressed against the surface of the rolling rolls 11, 12 against the side peripheral surface downstream in the conveying direction of the electrode sheet 100. Here, the side peripheral surface downstream of the rolling rolls 11, 12 in the conveying direction of the electrode sheet 100 means the side peripheral surface of the half portion downstream in the conveying direction of the electrode sheet 100 when the rolling rolls 11, 12 are divided in half by a straight line connecting the rotation center of the rolling rolls 11, 12 and the part on the circumference where the electrode sheet 100 is sandwiched by the rolling rolls 11, 12. Since the application member 51 is pressed against the surfaces of the rolling rolls 11, 12 on the side peripheral surface downstream in the conveying direction of the electrode sheet 100, the oil 30 becomes familiar with the surfaces of the rolling rolls 11, 12 from when the oil 30 is supplied to the surfaces of the rolling rolls 11, 12 until it reaches the portion of the electrode sheet 100 being rolled, thereby minimizing unevenness in the oil 30.
[0044] In this way, the electrode rolling device 10 includes an oil supply mechanism 14 that supplies oil 30 to the surfaces of the rolling rolls 11, 12 in the regions of the rolling rolls 11, 12 that sandwich the unformed portions 102 of the electrode sheet 100. Since the oil 30 is supplied to the surfaces of the rolling rolls 11, 12 in the regions of the rolling rolls 11, 12 that sandwich the unformed portions 102 of the electrode sheet 100, even if a foreign object is attached to either the rolling rolls 11, 12 or the unformed portions 102, or if a step occurs on the surfaces of the rolling rolls 11, 12 due to wear, the unformed portions 102 of the electrode sheet 100 are unlikely to get caught by the rolling rolls 11, 12, and the unformed portions 102 are unlikely to be damaged.
[0045] Although the electrode rolling device 10 has been described, the electrode rolling device 10 is not limited to the above. For example, the oil supply mechanism 14 has been described as being configured so that the application member 51 is pressed against the surfaces of the rolling rolls 11 and 12. The oil supply mechanism 14 is not limited to such a configuration. Although not shown, a method of supplying oil to the surfaces of the rolling rolls 11 and 12 may be, for example, dripping a predetermined amount of oil at predetermined positions on the surfaces of the rolling rolls 11 and 12. Alternatively, the oil may be sprayed at predetermined positions on the surfaces of the rolling rolls 11 and 12. Alternatively, after dripping or spraying the oil, the oil may be spread to a predetermined width by pressing a wiper against the surfaces of the rolling rolls 11 and 12 to which the oil has been supplied.
[0046] The invention disclosed herein has been described in various ways. Unless otherwise specified, the embodiments described herein do not limit the present invention. Furthermore, the embodiments of the invention disclosed herein can be modified in various ways, and each component or each process described herein can be omitted or combined as appropriate, unless a particular problem occurs.
[0047] As described above, this specification includes the disclosures set forth in the following sections.
[0048] Section 1: preparing an electrode sheet on which an active material layer containing an electrode active material is formed, except for an unformed portion set at at least one end portion in a width direction perpendicular to a longitudinal direction of a strip-shaped current collecting foil; a rolling step of rolling the active material layer by passing the electrode sheet between a pair of rolling rolls; Including, In the rolling step, oil is supplied to at least a portion of the pair of rolling rolls facing the unformed portion. A method for manufacturing an electrode.
[0049] Section 2: Item 2. The manufacturing method according to item 1, wherein in the rolling step, oil is supplied to a region of the rolling roll facing the unformed portion of the electrode sheet in a width of 80 to 120% of the width of the unformed portion of the electrode sheet.
[0050] Section 3: Item 3. The manufacturing method according to item 1 or 2, wherein in the rolling step, the oil is supplied to both ends of the pair of rolling rolls in the width direction of a portion through which the electrode sheet passes, with a width of 30 mm to 40 mm.
[0051] Section 4: 4. The manufacturing method according to any one of items 1 to 3, wherein in the rolling step, the oil is supplied to a downstream side peripheral surface of the rolling roll in a circumferential direction of the rolling roll in a conveying direction of the electrode sheet.
[0052] Section 5: 5. The method according to claim 1, wherein the electrode sheet has a protective layer containing an inorganic filler provided on an edge of the active material layer, and the oil is supplied to at least a portion of an area facing the protective layer.
[0053] Item 6: Item 6. The manufacturing method according to item 5, wherein in the rolling step, oil is supplied to a region of the rolling roll that faces the unformed portion of the electrode sheet and the protective layer in a width of 80 to 120% when a combined width of the unformed portion of the electrode sheet and the protective layer is taken as 100%.
[0054] Section 7: Item 2. The manufacturing method according to item 1, wherein the oil is applied to the surface of the rolling roll.
[0055] Section 8: An electrode rolling device for rolling an electrode sheet comprising: an electrode active material layer continuously applied along a longitudinal direction of a strip-shaped current collector foil and containing an electrode active material; and an unformed portion in which the electrode active material layer is not disposed at at least one end portion in a width direction perpendicular to the longitudinal direction of the current collector foil, the electrode sheet comprising: a conveying device that conveys the electrode sheet along a predetermined conveying path; A pair of rolling rolls arranged in a transport path along which the electrode sheet is transported; an oil supply mechanism that supplies oil to a surface of the rolling roll in a region of the rolling roll that sandwiches the unformed portion of the electrode sheet; Equipped with Electrode rolling equipment.
[0056] Section 9: The oil supply mechanism includes an application member that is in contact with each of the pair of rolls, and a supply member for supplying oil to the application member; Item 9. The electrode rolling apparatus according to item 8, comprising:
[0057] Section 10: Item 10. The electrode rolling device according to item 9, wherein the oil supply mechanism includes a spring mechanism that biases the application member toward each of the pair of rolling rolls.
[0058] Section 11: Item 10. The electrode rolling device according to item 9, wherein the oil supply mechanism is configured so that the application member is pressed against the surface of the rolling roll on a downstream side peripheral surface in a conveying direction of the electrode sheet in a circumferential direction of the rolling roll. [Explanation of symbols]
[0059] 10 Electrode rolling equipment 11,12 Rolling mill 11a, 12a Rotation axis 14 Oil supply mechanism 14A Mechanism for supplying oil 30 to the outer peripheral surface of the rolling roll 11 14B Mechanism for supplying oil 30 to the outer peripheral surface of the rolling roll 12 30 Oil 40 Transport device 40a Transport route 41 Rolls 42 rolls 51 Coating material 51a Arm 52 Supply Materials 53 Tank 54 Pump 55 Check valve 56 Piping 61 Spring mechanism 100 Electrode Sheet 102 Unformed part 103 Active material layer 104 Protective layer A: The part where the unformed part 102 comes into contact B: Part in contact with protective layer 104 C: A portion in contact with the active material layer 103 S1: Near the edge of the protective layer 104 S3 Step T1: The combined width of the unformed portion 102 and the protective layer 104 T2 Width where oil 30 is applied
Claims
1. preparing an electrode sheet on which an active material layer containing an electrode active material is formed, except for an unformed portion set at at least one end portion in a width direction perpendicular to a longitudinal direction of a strip-shaped current collecting foil; a rolling step of rolling the active material layer by passing the electrode sheet between a pair of rolling rolls; Including, In the rolling step, oil is supplied to at least a portion of the pair of rolling rolls facing the unformed portion. A method for manufacturing an electrode.
2. 2. The manufacturing method according to claim 1, wherein in the rolling step, oil is supplied to an area of the rolling roll facing the unformed portion of the electrode sheet in a width of 80 to 120% when the width of the unformed portion of the electrode sheet is 100%.
3. The manufacturing method according to claim 1 , wherein in the rolling step, the oil is supplied to both ends in a width direction of the pair of rolling rolls, the both ends being located at a portion through which the electrode sheet passes, with a width of 30 mm to 40 mm.
4. The manufacturing method according to claim 1 , wherein in the rolling step, the oil is supplied to a side peripheral surface of the rolling roll that is downstream in a conveying direction of the electrode sheet in the circumferential direction of the rolling roll.
5. The manufacturing method according to claim 1 , wherein the electrode sheet has a protective layer containing an inorganic filler provided on an edge of the active material layer, and the oil is supplied to at least a part of an area facing the protective layer.
6. 6. The manufacturing method according to claim 5, wherein in the rolling step, oil is supplied to an area of the rolling roll that faces the unformed portion of the electrode sheet and the protective layer in a width of 80 to 120% when the combined width of the unformed portion of the electrode sheet and the protective layer is taken as 100%.
7. The method according to claim 1 , wherein the oil is applied to the surface of the rolling roll.
8. An electrode rolling device for rolling an electrode sheet comprising: an electrode active material layer continuously applied along a longitudinal direction of a strip-shaped current collector foil and containing an electrode active material; and an unformed portion in which the electrode active material layer is not disposed at at least one end portion in a width direction perpendicular to the longitudinal direction of the current collector foil, the electrode sheet comprising: a conveying device that conveys the electrode sheet along a predetermined conveying path; A pair of rolling rolls arranged in a transport path along which the electrode sheet is transported; an oil supply mechanism that supplies oil to a surface of the rolling roll in a region of the rolling roll that sandwiches the unformed portion of the electrode sheet; Equipped with Electrode rolling equipment.
9. The oil supply mechanism includes an application member that is in contact with each of the pair of rolls, and a supply member for supplying oil to the application member; The electrode rolling apparatus according to claim 8 , further comprising:
10. 10. The electrode rolling apparatus according to claim 9, wherein the oil supply mechanism includes a spring mechanism that biases the applicator member toward each of the pair of rolls.
11. 10. The electrode rolling device according to claim 9, wherein the oil supply mechanism is configured such that the application member is pressed against a surface of the rolling roll on a side peripheral surface downstream in a conveying direction of the electrode sheet in a circumferential direction of the rolling roll.
Citation Information
Patent Citations
Pole piece calendering system and pole piece calendering process
CN112310338A
Coating device and method for preparing electrode plate
JP2008006396A
Method of manufacturing electrode plate for battery
JP2010080272A
Production apparatus of sheet for lithium ion secondary battery, production method of sheet for lithium ion secondary battery, and manufacturing method for lithium ion secondary battery
JP2015176842A
Method for manufacturing positive electrode plate, method for manufacturing nonaqueous electrolyte secondary battery, and nonaqueous electrolyte secondary battery
JP2018092707A
Cited By
Leveling mobile robot
KR1020250009728A