Surface material and manufacturing method thereof
The manufacturing method for surface materials forms the binder layer on the inner side of the fabric, addressing the issue of unintended binder diffusion and ensuring high-quality prints by preventing binder layer components from being present on the main surface, thus achieving clear and intact print designs.
Patent Information
- Application Number
- JP2023070418
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-21
- Publication Date
- 2024-10-31
AI Technical Summary
Existing methods for manufacturing surface materials with binder layers result in unintended diffusion of binder liquid into the fabric, leading to poor print quality due to the presence of binder layer components on the wrong surface, which can cause poor color development and faded areas in prints.
A manufacturing method where the binder liquid is applied to the opposite main surface of the fabric with a solvent or dispersion medium, ensuring the binder layer is formed on the inner side, and the print is applied without binder layer components on the main surface, preventing unintended diffusion and controlling the position of the binder layer accurately.
This method ensures a surface material with an intended print on the main surface, preventing poor color development and faded areas, while maintaining the integrity of the print design.
Smart Images

Figure 2024155581000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a surfacing material and a method for its manufacture. [Background technology]
[0002] Conventionally, a surface material comprising a fabric and a layer of binder that bonds the constituent fibers has been used as a surface material that can be used to form the interior of an automobile or the like. As such a surface material, the applicant of the present application has proposed a surface material in which the ends of the fibers exposed on the main surface of the surface material that are present inside the fabric are fixed mainly by a layer of binder that is present inside the fabric, as described in JP 2021-98922 A (Patent Document 1). By having this configuration, the surface material described in Patent Document 1 is a surface material in which fibers are less likely to fall off from the main surface.
[0003] In the method for manufacturing a surface material according to Patent Document 1, a binder liquid is applied from one main surface of a fabric, and then a binder solvent and / or dispersion medium is applied from the same main surface, causing the binder liquid (more precisely, a composition that constitutes a binder layer contained in the binder liquid) to move from one main surface of the fabric to the other main surface. Then, the solvent and / or dispersion medium are removed, forming a binder layer on the inner side of one main surface of the fabric.
[0004] In recent years, the interior design of automobiles and other vehicles has also been required to have color, pattern, and other design features, and surface materials with partial prints on their main surfaces are in demand. For example, surface materials disclosed in JP 2015-104848 A (Patent Document 2) and JP 2016-147466 A (Patent Document 3) are known as such surface materials. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Patent Publication No. 2021-98922 [Patent Document 2] JP 2015-104848 A [Patent Document 3] JP 2016-147466 A Summary of the Invention [Problem to be solved by the invention]
[0006] However, in the conventional manufacturing method for a surface material as disclosed in Patent Document 1, a composition constituting a binder layer contained in the binder liquid was sometimes unintentionally present on the main surface of the fabric of the surface material opposite to the side to which the binder liquid was applied.
[0007] The reasons for this phenomenon are thought to be as follows: In the conventional manufacturing method for a surface material, the binder liquid is diluted by a solvent and / or a dispersion medium applied to move the binder liquid. The diluted binder liquid then unintentionally diffuses into the fabric. As a result, it was thought that the composition constituting the binder layer contained in the binder liquid would be unintentionally present on the main surface of the fabric opposite to the side to which the binder liquid was applied. Therefore, it was thought that it would be difficult to provide a surface material having a binder layer in a desired state by highly controlling the location of the composition constituting the binder layer contained in the binder liquid in the manufacturing method for a surface material according to the conventional technology.
[0008] In particular, the phenomenon of the diluted binder liquid unintentionally diffusing into the fabric was likely to occur when a solvent and / or dispersion medium containing additives such as a thickener or an antifoaming agent was used.
[0009] Furthermore, when a print was applied to the main surface of the fabric prepared in this manner opposite to the side to which the binder liquid was applied, the print sometimes had poor color development due to the print containing unnecessary components (compositions that make up the binder layer). As a result, it may not be possible to provide a surface with the intended print on the major surface. [Means for solving the problem]
[0010] The first invention is a surface material comprising a fabric, a print partially present on one main surface of the fabric, and a binder layer, the binder layer is present on the inner side of the other main surface of the fabric, The print does not contain the composition that constitutes the binder layer. Surface material." The second invention includes the steps of: (Step 1) preparing a fabric; (Step 2) preparing a printing liquid containing a composition constituting a print and a solvent and / or a dispersion medium for said composition; (Step 3) applying a printing liquid partially to one main surface of the fabric; (Step 4) removing the solvent and / or dispersion medium from the fabric to which the printing liquid has been partially applied, thereby forming a print partially on the one main surface of the fabric; (Step 5) preparing a binder liquid containing a binder and a solvent and / or a dispersion medium for the binder; (Step 6) applying the binder liquid to the other main surface of the fabric; (Step 7) applying a solvent and / or a dispersion medium for the binder to the other main surface of the fabric; (Step 8) removing the binder solvent and / or dispersion medium from the fabric; "A method for manufacturing a surface material, comprising the steps of: Effect of the Invention
[0011] As a result of investigations, the applicant has come to provide a surfacing material comprising "a fabric, a print partially present on one main surface of the fabric, and a binder layer, wherein the binder layer is present on the inner side of the other main surface of the fabric," in which the print does not contain a composition that constitutes the binder layer.
[0012] That is, in the surface material according to the first invention, the print is present on the main surface of the fabric without containing the composition that constitutes the binder layer, and therefore the problem of poor color development caused by the print containing unnecessary components (the composition that constitutes the binder layer) is prevented.
[0013] From the above, the present invention can provide a surface material having a desired print on the main surface of the fabric.
[0014] Furthermore, the method for producing a surface material according to the second invention is characterized in that a binder liquid is applied to one main surface of a fabric having a partial print on the other main surface, and then a solvent and / or dispersion medium for the binder is applied from the other main surface side, thereby moving the binder liquid already applied (more precisely, a composition that constitutes the binder layer contained in the binder liquid) from the other main surface side of the fabric to one main surface side, thereby producing the surface material.
[0015] As a result of investigations, the applicant of the present application has come to provide a surface material according to the first invention by adopting this manufacturing method.
[0016] In addition, it was found that the manufacturing method has the secondary effect of preventing the binder liquid diluted with the binder solvent and / or dispersion medium from unintentionally diffusing into the fabric. Therefore, the manufacturing method can provide the surface material according to the first invention by highly controlling the location of the composition constituting the binder layer contained in the binder liquid. Furthermore, it can provide a surface material having no binder layer on both main surfaces.
[0017] According to the method for producing a surface material of the present invention, printing can be performed on the main surface of the fabric where the composition constituting the binder layer contained in the binder liquid is not present. Therefore, it is possible to prevent the occurrence of a problem in which the print liquid is repelled due to the presence of the composition constituting the binder layer contained in the binder liquid on the main surface of the fabric, and the print is not well placed on the main surface. As a result, it is possible to prevent the occurrence of faint spots in the print and provide a surface material with the intended print on the main surface. [Brief description of the drawings]
[0018] [Figure 1] FIG. 1 is a schematic cross-sectional view of a surface material according to the present invention. [Diagram 2] FIG. 2 is a schematic cross-sectional view showing the state of a binder layer included in the surface material. [Diagram 3] 1A to 1C are schematic cross-sectional views showing a manufacturing process of a surface material according to the present invention. [Figure 4] 1A to 1C are schematic cross-sectional views showing a manufacturing process for a surface material according to the prior art. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0019] In the present invention, various configurations, such as the following configurations, can be appropriately selected. Note that, unless otherwise specified, the various measurements described in the present invention are performed under normal pressure, at a temperature of 20°C, and at a humidity of 65 RH%. Furthermore, unless otherwise specified, the various measurement results described in the present invention are measured to a value one digit smaller than the desired value, and the desired value is calculated by rounding off the value. As a specific example, when the desired value is to the first decimal place, the value is measured to the second decimal place, and the obtained value to the first decimal place is rounded off to calculate the value to the first decimal place, and this value is the desired value. Furthermore, each upper limit value and each lower limit value exemplified in the present invention can be combined arbitrarily.
[0020] The surface material of the present invention will be described with reference to Fig. 1, which is a schematic cross-sectional view of the surface material of the present invention cut in the thickness direction. The surface material (100) of the present invention comprises a fabric (10), a print (11, hereinafter sometimes abbreviated as print) partially present on one main surface of the fabric (the right main surface on the paper) and exposed on the one main surface, and a binder layer (13) composed of a resin-containing composition. The binder layer (13) is present on the inner side (the right main surface on the paper) of the other main surface of the fabric (10) (the left main surface on the paper) of the other main surface.
[0021] Here, the fabric (10) is a member that mainly plays a role in forming the framework of the surface material (100). The print (11) mainly plays a role in imparting design, such as color and pattern, to the surface material (100) and improving the feel of the main surface on which the print (11) is present. The binder layer (13) also plays a role in bonding and integrating the constituent fibers of the fabric (10) to prevent the shape of the fabric (10) from being unintentionally deformed, and to increase the rigidity of the fabric (10) and improve various physical properties. In addition, it plays a role in fixing the ends of the fibers exposed on the main surface of the surface material that are present inside the fabric (10) inside the fabric, making it difficult for the fibers to fall off from the main surface of the surface material (100).
[0022] The fabric (10) in the present invention is, for example, a sheet-like fiber assembly such as a fiber web, a nonwoven fabric, or a woven or knitted fabric. The surface material (100) of the present invention is flexible and has excellent heat moldability because it contains the fabric (10). Note that a surface material (100) including a fabric (10, particularly a nonwoven fabric) in which all of the constituent fibers are randomly entangled is more flexible and has better heat moldability, and is therefore preferred.
[0023] The fabric (10) may be constructed by laminating a plurality of these sheet-like fiber assemblies, or may be a fabric (10) having a single layer structure. However, by employing a fabric (10) having a single layer structure, it is possible to provide a fabric (10) that is less susceptible to delamination, and it is preferable to provide a surface material (100) that has excellent moldability when manufacturing an interior material by making the types and blending ratios of the constituent fibers on both main surfaces of the fabric (10) the same and making the conformability to a molding die on both main surfaces of the fabric (10) uniform.
[0024] The single-layer structure here means that the fabric (10) is not constructed by laminating multiple sheet-like fiber assemblies prepared individually. If layers can be easily peeled off from the fabric (10), or if the types and blending ratios of the constituent fibers on one main surface and the other main surface of the fabric (10) are not the same, it can be determined that the fabric (10) does not have a single-layer structure.
[0025] The fibers constituting the fabric (10) may be, for example, polyolefin resins (e.g., polyethylene, polypropylene, polymethylpentene, polyolefin resins having a structure in which a portion of the hydrocarbon is substituted with a cyano group or a halogen such as fluorine or chlorine), styrene resins, polyvinyl alcohol resins, polyether resins (e.g., polyether ether ketone, polyacetal, modified polyphenylene ether, aromatic polyether ketone, etc.), polyester resins (e.g., polyethylene terephthalate, polytrimethylene terephthalate, polybutylene terephthalate, polyethylene naphthalate, polybutylene naphthalate, polycarbonate, polyarylate, wholly aromatic polyester resins, etc.), polyimide resins, polya It can be constructed using known resins such as amidoimide resins, polyamide resins (e.g., aromatic polyamide resins, aromatic polyetheramide resins, nylon resins, etc.), resins having nitrile groups (e.g., polyacrylonitrile, etc.), urethane resins, epoxy resins, polysulfone resins (e.g., polysulfone, polyethersulfone, etc.), fluorine resins (e.g., polytetrafluoroethylene, polyvinylidene fluoride, etc.), cellulose resins, polybenzimidazole resins, acrylic resins (e.g., polyacrylonitrile resins copolymerized with acrylic esters or methacrylic esters, modacrylic resins copolymerized with acrylonitrile and vinyl chloride or vinylidene chloride, acrylic styrene resins, etc.).
[0026] These resins may be either linear polymers or branched polymers, may be block copolymers or random copolymers, and may have any three-dimensional structure or may have crystallinity, without any particular limitations. Furthermore, the constituent fibers may contain a plurality of resins.
[0027] In addition, when flame retardancy is required for the surface material (100), it is preferable that the constituent fibers of the fabric (10) contain a flame retardant resin. Examples of such flame retardant resins include modacrylic resins, vinylidene resins, polyvinyl chloride resins, polyvinylidene fluoride resins, novoloid resins, polychlar resins, polyester resins copolymerized with phosphorus compounds, acrylic resins copolymerized with halogen-containing monomers, aramid resins, and resins kneaded with halogen-based, phosphorus-based, or metal compound-based flame retardants.
[0028] The constituent fibers can be obtained by known methods such as melt spinning, dry spinning, wet spinning, direct spinning (melt blowing, spunbonding, electrostatic spinning, etc.), a method of extracting fibers having a small fiber diameter by removing one or more resin components from composite fibers, and a method of beating fibers to obtain split fibers.
[0029] The constituent fibers may be made of one type of resin or a plurality of types of resin. Fibers made of a plurality of types of resin may be generally called composite fibers, such as core-sheath type, sea-island type, side-by-side type, orange type, bimetal type, and the like.
[0030] The constituent fibers may include irregular cross-section fibers other than the roughly circular and elliptical fibers. The irregular cross-section fibers may have a fiber cross section of a hollow shape, a polygonal shape such as a triangular shape, an alphabetic shape such as a Y-shape, an irregular shape, a multi-lobed shape, a symbolic shape such as an asterisk shape, or a shape in which a plurality of these shapes are combined.
[0031] When the fabric (10) contains heat-fusible fibers as constituent fibers, the fibers are heat-fused together to impart strength and shape stability to the fabric (10), and to suppress the occurrence of scraping and unintended fluffing, which is preferable. Such heat-fusible fibers may be fully heat-fusible fibers, or may be partially heat-fusible fibers such as the above-mentioned composite fibers. For example, low-melting-point polyolefin resins and low-melting-point polyester resins can be used as components that exhibit heat-fusibility in the heat-fusible fibers.
[0032] When the fabric (10) contains a crimpable fiber, the stretchability is increased and the conformability to the mold is excellent, which is preferable. As such a crimpable fiber, for example, a fiber in which a latent crimp fiber has expressed crimp or a fiber to which mechanical crimp has been imparted can be used.
[0033] The constituent fibers of the fabric 10 may be made by kneading a pigment into the fibers, or may be dyed original fibers (such as black original fibers).
[0034] First, a fiber web can be prepared by, for example, a dry method in which the above-mentioned fibers are fed into a carding device or an air-laying device to entangle the fibers, a wet method in which the fibers are dispersed in a solvent and laid into a sheet to entangle the fibers, or a direct spinning method (a method in which fibers are spun and collected using a melt-blowing method, a spunbonding method, an electrostatic spinning method, or a method in which a spinning solution and a gas flow are discharged in parallel to spin the fibers (e.g., the method disclosed in JP-A-2009-287138)).
[0035] The constituent fibers of the prepared fiber web are then entangled and / or integrated to prepare a nonwoven fabric. Examples of methods for entangling and / or integrating the constituent fibers include a method of entangling the fibers with a needle or a water stream, and a method of bonding and integrating the constituent fibers with heat-fusible fibers by subjecting the fiber web to a heat treatment, for example.
[0036] The heat treatment method can be appropriately selected, and examples of the method that can be used include heating or heating and pressurizing with a roll, heating by subjecting the material to a heater such as an oven dryer, a far-infrared heater, a dry heat dryer, or a hot air dryer, and heating the resin contained therein by irradiating the material with infrared rays without pressure.
[0037] When the fabric 10 is a woven or knitted fabric, the woven or knitted fabric can be prepared using the fibers prepared as described above.
[0038] In addition to fiber webs, fabrics such as woven fabrics and knitted fabrics may also be subjected to the above-mentioned method of entangling and / or integrating constituent fibers.
[0039] The fineness of the constituent fibers of the fabric (10) is not particularly limited, but may be 0.1 dtex or more, 0.5 dtex or more, or 1.0 dtex or more so as to improve appearance retention, and may be 100 dtex or less, 50 dtex or less, 30 dtex or less, or 10 dtex or less so as to be able to prepare a surface material (100) with excellent moldability.
[0040] The fiber length of the constituent fibers of the fabric (10) is not particularly limited, but may be 20 mm or more, 25 mm or more, or 30 mm or more so as to improve appearance retention. On the other hand, if the fiber length exceeds 110 mm, fiber clumps tend to form during preparation of the fabric (10), which may make it difficult to prepare a surface material (100) with excellent moldability. Therefore, the fiber length is preferably 110 mm or less, and may be 80 mm or less. The "fiber length" refers to a value measured in accordance with JIS L1015 (2010), 8.4.1c) direct method (C method).
[0041] The various configurations of the fabric (10), such as thickness and basis weight, are not particularly limited and may be adjusted as appropriate.
[0042] The thickness of the fabric (10) may be 500 to 50,000 μm, 1000 to 3000 μm, or 1100 to 1900 μm. In the present invention, the thickness of the fabric (10) refers to the length between the end points (A in FIG. 2) and the end point (B in FIG. 2) of a line segment (shown as X in FIG. 2) calculated in the section (Method for confirming the presence of the binder layer) described later.
[0043] The fabric (10) has a basis weight of, for example, 50 to 500 g / m 2 and can be 80 to 300 g / m 2 and 100 to 250 g / m 2 In the present invention, the basis weight is the weight per square meter on the surface (principal surface) having the widest area of the object to be measured. 2 This refers to the mass per unit.
[0044] The composition constituting the binder layer is a resin that serves to bond and integrate the constituent fibers of the fabric (10) together, and may be, for example, a polyolefin resin (such as modified polyolefin), an ethylene-vinyl alcohol copolymer, an ethylene-acrylate copolymer such as an ethylene-ethyl acrylate copolymer, various rubbers and their derivatives (such as styrene-butadiene rubber (SBR), fluororubber, urethane rubber, ethylene-propylene-diene rubber (EPDM)), cellulose derivatives (such as carboxymethyl cellulose (CMC), hydroxyethyl cellulose, hydroxypropyl cellulose, etc.), etc. ), polyvinyl alcohol (PVA), polyvinyl butyral (PVB), polyvinylpyrrolidone (PVP), polyurethane, epoxy resin, polyvinylidene fluoride (PVdF), vinylidene fluoride-hexafluoropropylene copolymer (PVdF-HFP), acrylic resin (for example, polyacrylonitrile resin copolymerized with acrylic acid ester or methacrylic acid ester, modacrylic resin copolymerized with acrylonitrile and vinyl chloride or vinylidene chloride, versatate vinyl ester copolymerized acrylic resin, etc.) are included as essential components. When an acrylic resin is used as the resin constituting the binder layer, it is preferable because it can provide a surface material (100) that has excellent conformability to the molding die because it is moderately softened during thermoforming.
[0045] In addition, the binder layer may contain, in addition to the resin, additives such as flame retardants, fragrances, pigments, antibacterial agents, antifungal materials, photocatalyst particles, inorganic particles such as silica, hollow particles such as particles that foam when heated or already-foamed particles, emulsifiers, dispersants, and surfactants (e.g., fluorine-based water- and oil-repellents).
[0046] The basis weight of the binder layer contained in the fabric (10) is appropriately selected so as to provide a surface material (100) that satisfies the configuration of the present invention. Specifically, the basis weight is 2 g / m 2 It can be 200 g / m or more. 2 and can be less than 100 g / m 2 and 50 g / m 2 It can be the following:
[0047] The surface material (100) according to the present invention has a binder layer (13) inside the fabric (10), and is characterized by the state of the binder layer (13). That is, the binder layer (13) is present on the inner side (the right main surface side on the paper) of the other main surface of the fabric (10) (the left main surface on the paper).
[0048] In this case, the constituent fibers exposed on at least one of the main surfaces of the fabric (10) have ends present inside the fabric (10) that are fixed mainly by the binder layer (13) present inside the fabric (10) so that they are unlikely to fall off from the main surface, and the portions exposed to the main surface are not fixed by the binder layer (13), so that it is easy to provide a surface material (100) with a main surface that has a brushed feel and excellent touch, and the binder layer (13) is preferably present on the inner side (the left main surface on the paper) of one of the main surfaces of the fabric (10) (the right main surface on the paper). In other words, it is preferable that the binder layer (13) is not present on both main surfaces of the surface material (100).
[0049] The state of the binder layer (13) present in the fabric (10) can be confirmed by the following measurement method.
[0050] (How to check the binder layer) 1. Take a sample (shape: square or rectangular) from the measurement object (for example, the surface material (100)). 2. Prepare a staining solution capable of staining the binder contained in the measurement target (for example, Kayastain Q (manufactured by Nippon Kayaku Co., Ltd.)). 3. The binder contained in the sample is stained using a staining solution. 4. After dyeing, the sample is cut in the thickness direction, and inkjet printing glossy paper is placed on both main surfaces of the cut sample. The sample is then sandwiched between glass plates in the thickness direction from both sides of the inkjet printing glossy paper (pressure applied to the sample by the glass plates in the thickness direction: 20 g / cm 2) and then photograph the cross section of the cut sample under this condition using an optical microscope at 30x magnification. The photograph is taken so that the entire thickness direction of the cross section of the dyed sample fits within the vertical range of the optical microscope photograph. The photograph is also taken so that the area of a square, with one side being a line segment indicating the length of the sample in the thickness direction, fits within the optical microscope photograph. When there is a portion where the binder is present continuously across the horizontal direction (direction perpendicular to the thickness direction of the sample cross section) of the aforementioned square range in the optical microscope photograph, the surface material (100) having a portion where the binder composed of a composition containing the resin is present continuously is determined to be a surface material (100) having a binder layer (13).
[0051] As a result of checking the optical microscope photographs, When the binder layer (13) is not present on the other main surface of the fabric (10) (the left main surface on the paper), and the binder layer (13) is present on the inner side of the other main surface of the fabric (10) (the left main surface on the paper) (the right main surface side of the other main surface on the paper), It can be seen that a binder layer (13) is present on the inner side of the other main surface of the fabric (10).
[0052] In addition, the results of checking the optical microscope images showed that No binder layer (13) is present on the other main surface (the left main surface on the paper) of the fabric (10), and a binder layer (13) is present on the inner side (the right main surface on the paper) of the other main surface (the left main surface on the paper) of the fabric (10), and When a binder layer (13) is present on the inner side (the left main surface side on the paper) of one of the main surfaces (the right main surface on the paper) of the fabric (10), It can be seen that a layer of binder (13) is present between the two major surfaces of the fabric (10).
[0053] The number of binder layers (13) in the fabric (10) can be adjusted as appropriate and may be multiple, but it is preferred that the fabric (10) have only one binder layer (13) so that the surface material (100) of the present invention can be easily provided.
[0054] The thickness of the binder layer (13) can be adjusted as appropriate, but in the surface material (100) of the present invention, it is thinner than the thickness of the fabric (10) shown in the optical microscope photograph described above. As an example, it can be thinner than the thickness of the fabric (10), and can be 200 to 1000 μm, or 300 to 500 μm.
[0055] The thickness of the binder layer (13) can be determined by the following method, which will be mainly explained with reference to Fig. 2. In Fig. 2, the glossy paper for inkjet printing and the glass plate are omitted and not shown.
[0056] (Method of measuring binder layer thickness) 1. A line segment is drawn on the optical microscope photograph, connecting the two main surfaces of the fabric (10) in the above-mentioned optical microscope photograph at the shortest distance. The end point of the line segment on one main surface of the fabric (10) (the tangency between one main surface and the line segment) is defined as end point (A), and the end point of the line segment on the other main surface of the fabric (10) (the tangency between the other main surface and the line segment) is defined as end point (B). The length between end points (A) and (B) of the line segment is defined as the thickness of the fabric (10) (unit: μm). In the figure, the thickness of the fabric (10) is illustrated as X. 2. On the optical microscope photograph, the outline of one main surface of a binder layer (13) and the intersection point (a) of the line segment, and the outline of the other main surface of the binder layer (13) and the intersection point (b) of the line segment are drawn. Then, the length between the intersection points (a) and (b) of the line segment is calculated and used as the thickness of the binder layer (13) of the line segment. Note that the thickness of the binder layer (13) is illustrated as W in the drawing. 3. Draw five lines on the optical microscope photograph that are parallel to the first line drawn and connect the two main surfaces of the fabric (10) shown in the optical microscope photograph described above. Next, in the same manner as described above, draw the end points (A) and (B) and the intersection points (a) and (b) for each line segment. Then, find the length between the intersection points (a) and (b) for each line segment. 4. The average value of the lengths between the intersection points (a) and (b) of the five line segments obtained in the above manner is calculated, and the calculated value is regarded as the thickness (unit: μm) of the binder layer (13).
[0057] The percentage of the thickness of the binder layer (13) in the thickness of the fabric (10) can be adjusted as appropriate, and can be in the range of 5% to 80%, 10% to 60%, or 20% to 30%. This percentage can be found by calculating the percentage of the thickness (W) of the binder layer (13) in the thickness (X) of the fabric (10).
[0058] It is possible to appropriately adjust the extent to which the binder layer (13) exists inside the main surface of the fabric (10). The state of the binder layer (13) can be confirmed by the following method.
[0059] (Method of confirming the existence of binder layers) 1. Determine the length (X) between end point (A) and end point (B) of the line segment drawn as described above, the length between end point (A) and intersection point (a) of the line segment (shown as Y in the figure, meaning the depth from one main surface to where the binder layer (13) exists), and the length between end point (B) and intersection point (b) of the line segment (shown as Z in the figure, meaning the depth from the other main surface to where the binder layer (13) exists). 2. Calculate the value of 100×Y / X and the value of 100×Z / X (unit: %). 3. Draw five lines on the optical microscope photograph that are parallel to the first line drawn and connect both main surfaces of the fabric (10) shown in the optical microscope photograph. Next, in the same manner as described above, draw the end points (A) and (B) and the intersection points (a) and (b) for each line. Then, measure the lengths X, Y, and Z for each line segment and calculate the values of 100×Y / X and 100×Z / X, respectively. 4. By calculating the average value (unit: %) of the values of 100×Y / X for each of the five line segments obtained as described above, it can be determined that a binder layer (13) is present in a range equal to or greater than the average value (unit: %) from one main surface in the thickness direction of the fabric (10). 5. Similarly, by calculating the average value (unit: %) of the values of 100×Z / X for each of the five line segments obtained as described above, it can be determined that a binder layer (13) is present in a range equal to or greater than the average value (unit: %) from the other main surface in the thickness direction of the fabric (10).
[0060] In a surface material (100) that satisfies the configuration of the present invention, the average value of 100×Z / X (or the average value of 100×Z / X and the average value of 100×Y / X) is greater than 0%. The average value can be adjusted as appropriate so long as it satisfies the configuration of the present invention, and the average value of 100×Z / X or the average value of 100×Y / X can be 5% or more, 7% or more, 10% or more, or 15% or more. The upper limit of each average value can be adjusted as appropriate, and can be 73% or less, 70% or less, or 60% or less.
[0061] The surface material (100) according to the present invention can satisfy the following requirements. ·X and W are greater than 0, and the average of 100×Z / X is greater than 0. The sum of the average value of 100×Y / X and the average value of 100×Z / X is less than 100%. Since the surface material (100) of the present invention has the above-mentioned configuration, the ends of the fibers exposed on the main surface of the surface material (100) that exist inside the fabric (10) are fixed mainly by the binder layer (13) that exists inside the fabric (10), and therefore the fibers of the surface material (100) are unlikely to fall off from the main surface.
[0062] In addition, ·X and W are greater than 0, and the average of 100×Y / X is greater than 0. With this configuration, the constituent fibers exposed on the main surface of the fabric (10) are not fixed by the binder layer (13), and therefore the fibers are less likely to fall off from the main surface, and a surface material (100) can be provided that has a brushed feel and an excellent feel on the main surface.
[0063] The physical properties of the surface material (100), such as the basis weight and thickness, can be appropriately adjusted so as to achieve the object of the present invention. For example, the basis weight is 140 to 300 g / m 2 and 150 to 260 g / m 2 and 160 to 250 g / m 2 In addition, the thickness can be 500 to 50,000 μm, 1,000 to 3,000 μm, or 1,100 to 1,900 μm.
[0064] The surface material (100) of the present invention has a print (11) partially exposed on one main surface of the fabric (10). The print (11) can be composed of at least one of the resins listed as being contained in the composition constituting the binder layer (13) described above.
[0065] When the resin contained in the print (11) is the same as the resin contained in the composition constituting the binder layer (13), the physical properties of the print (11) and the binder layer (13) become similar, which is preferable because it makes the conformability to the molding die uniform and provides a surface material (100) with excellent moldability when producing an interior material.
[0066] Furthermore, when the resin contained in the print (11) is different from the resin contained in the composition constituting the binder layer (13), it is possible to realize a surface material (100) having both the print (11) capable of imparting design to the surface material (100) and the binder layer (13) capable of preventing fibers from falling off from the main surface of the surface material (100) in an embodiment having an optimal resin. As a result, it is possible to provide a surface material (100) that has the intended print (11) on the main surface and is less likely to cause fibers to fall off from the main surface, which is preferable.
[0067] The resin contained in the print (11) and the resin contained in the composition constituting the binder layer (13) can be confirmed by using various analytical instruments such as an FT-IR device or a thermal analyzer, or by understanding the manufacturing process of the surface material (100).
[0068] The print (11) may contain additives such as flame retardants, fragrances, pigments, antibacterial agents, antifungal materials, photocatalyst particles, inorganic particles such as silica, hollow particles such as particles that foam when heated or already-foamed particles, emulsifiers, dispersants, surfactants (e.g., fluorine-based water- and oil-repellent agents), etc.
[0069] The print (11) may be provided partially on at least one of the main surfaces of the fabric, and the form of the print may be appropriately selected. For example, the print may be provided on a portion of the main surface so as to form a pattern such as a line, dot, or irregular shape. By providing the print (11) partially on at least one of the main surfaces of the fabric, a surface material (100) rich in design, such as having a pattern, can be provided.
[0070] The print (11) on the surface material (100) may be of one type or of multiple types. Note that, as long as the print (11) is partially provided on at least one of the main surfaces of the surface material (100), the print (11) may be present on the other main surface of the surface material (100).
[0071] The mass of the print (11) on one of the main surfaces of the fabric (10) is appropriately selected, but if the mass is too large, the moldability of the surface material (100) may be deteriorated. Therefore, the mass of the print (11) is set to 50 g / m 2 It is preferable that the thickness is less than 30 g / m 2 The lower limit can be selected appropriately, but is preferably 1 g / m 2 It can be more than 5g / m 2 It can be more than 10g / m 2 It can be more than that.
[0072] In the surface material (100) of the present invention, the print (11) is present on the main surface of the fabric (10) without containing the composition that constitutes the binder layer (13). The print (11) not containing the composition that constitutes the binder layer (13) here means that the composition that constitutes the binder layer (13) is not mixed into the print (11).
[0073] Whether or not the print (11) contains the composition that constitutes the binder layer (13) can be confirmed by the following method.
[0074] (1) From the print (11) present on the main surface of the surface material (100), a part of the print (11) is taken as a sample (print sample) from the part of the print (11) that is exposed and is the furthest from the main surface. Then, using various analytical instruments such as an FT-IR device and a thermal analyzer, the type of composition that constitutes the taken print sample is clarified. (2) A portion of the binder layer (13) provided in the surface material (100) is collected as a sample (binder sample), and the type of composition constituting the collected binder sample is clarified using various analytical instruments such as an FT-IR device or a thermal analyzer. (3) comparing the type of composition constituting the print sample (e.g., the type of resin and the presence or absence of a pigment) with the type of composition constituting the binder sample (e.g., the type of resin and the presence or absence of a pigment); If the print sample does not contain all of the components that make up the binder sample, It is determined that "the print (11) does not contain the composition that constitutes the binder layer (13)." on the other hand, If the print sample contains all the components that make up the binder sample, It is determined that "the print (11) contains a composition that constitutes a binder layer (13)."
[0075] The fabric (10) having the binder layer (13) according to the present invention may be used as a surface material (100) by itself, but may also be a surface material (100) formed by laminating other components such as other fabrics, porous bodies, films, foams, etc. In this case, it is preferable to laminate the components so that the main surface of the fabric (10) having the print (11) is exposed.
[0076] Next, the manufacturing method of the surface material (100) of the present invention will be described with reference to Fig. 3, which is a schematic cross-sectional view showing the manufacturing process. Note that the explanation and annotation of numbers in the figures will be omitted for the same configurations.
[0077] The manufacturing method of the surface material (100) according to the present invention can be appropriately selected. As an example, (Step 1) preparing a fabric; (Step 2) preparing a printing liquid containing a composition constituting a print and a solvent and / or a dispersion medium for said composition; (Step 3) applying a printing liquid partially to one main surface of the fabric; (Step 4) removing the solvent and / or dispersion medium of the print from the fabric to which the printing liquid has been partially applied, thereby forming a print partially on the one main surface of the fabric; (Step 5) preparing a binder liquid containing a binder and a solvent and / or a dispersion medium for the binder; (Step 6) applying the binder liquid to the other main surface of the fabric; (Step 7) applying a solvent and / or a dispersion medium for the binder to the other main surface of the fabric; (Step 8) removing the binder solvent and / or dispersion medium from the fabric; The method for producing a surface material may include the steps of:
[0078] Step (1) will now be described.
[0079] As shown in Fig. 3(1), a sheet-like fabric such as a fiber web, a nonwoven fabric, a woven fabric, a knitted fabric, etc. is prepared as the fabric (10) as shown in Fig. 3(1). The fineness and length of the constituent fibers of the fabric (10), and the thickness and basis weight of the fabric (10) can be appropriately adjusted.
[0080] Step (2) will now be described.
[0081] A printing liquid containing a composition constituting a print and a solvent and / or a dispersion medium for the composition is prepared. The composition constituting the print contained in the printing liquid can be appropriately adjusted, and may contain additives such as resins, flame retardants, fragrances, antibacterial agents, antifungal materials, photocatalyst particles, inorganic particles such as silica, hollow particles such as particles that foam when heated or already foamed particles, emulsifiers, dispersants, surfactants, thickeners, defoamers, and pigments.
[0082] The type of solvent or dispersion medium can be selected as appropriate, for example, water, but it is preferable to use a dispersion medium in which the printing composition can be dispersed but in which the fabric (10) is not dissolved, so that the printing liquid can be applied appropriately to the fabric (10).
[0083] The concentration of the components constituting the print contained in the printing liquid and the viscosity of the printing liquid are appropriately adjusted so as to provide the surface material (100) according to the present invention.
[0084] Step (3) will now be described.
[0085] The method of partially applying the printing liquid to one of the main surfaces of the fabric (10) can be appropriately selected. The printing liquid prepared as described above can be applied to one of the main surfaces of the fabric (10) either directly or in a foamed state, using a gravure roller or the like to partially apply the printing liquid to the main surface of the fabric to form a pattern, or the printing liquid can be applied by printing. In addition to applying one type of printing liquid, multiple types of printing liquids may be applied. In addition, when multiple types of printing liquids are applied, the application mode of each printing liquid (type of composition constituting each print, pattern, etc.) may be different.
[0086] Step (4) will now be described.
[0087] The solvent and / or dispersion medium of the print is removed from the fabric (10) to which the print liquid has been partially applied. The method for removing the solvent or dispersion medium in this process can be appropriately selected, but for example, the solvent or dispersion medium can be evaporated and removed by heating in a heater such as an oven dryer, far-infrared heater, dry heat dryer, or hot air dryer, or by leaving the material to stand at room temperature or in a reduced pressure atmosphere. The heating temperature for removing the solvent or dispersion medium is a temperature at which the solvent or dispersion medium can volatilize, and the upper limit of the heating temperature is adjusted so that the components of the fabric (10) and the composition of the print (11) are not unintentionally denatured.
[0088] This process makes it possible to prepare a fabric (10) formed in such a manner that the print (11) is partially exposed on one of the main surfaces of the fabric (the main surface on the side where the printing liquid is applied; in FIG. 3(2), this is the main surface on the right side of the paper), as shown in FIG. 3(2).
[0089] Step (5) will now be described.
[0090] A binder liquid containing a binder and a solvent and / or a dispersion medium for the binder is prepared. The type of the solvent or dispersion medium can be appropriately selected, for example, water, but it is preferable to use a dispersion medium in which the binder can be dispersed and in which the fabric (10) and the print (11) are not dissolved, so that the binder liquid can be applied to the fabric (10). The composition constituting the binder layer (13) contained in the binder liquid can be appropriately adjusted, and may contain additives such as resins, flame retardants, fragrances, pigments, antibacterial agents, antifungal materials, photocatalyst particles, inorganic particles such as silica, hollow particles such as particles that foam when heated or already foamed particles, emulsifiers, dispersants, surfactants, thickeners, and defoamers.
[0091] The concentration of the composition constituting the binder layer (13) contained in the binder liquid and the viscosity of the binder liquid are appropriately adjusted so as to provide the surface material (100) according to the present invention.
[0092] Step (6) will now be described.
[0093] As shown in FIG. 3(3), the binder liquid is applied (12) to the other main surface of the fabric (10) (the main surface opposite the side on which the print is applied; in FIG. 3(3), the main surface on the left side of the page).
[0094] The method for applying the binder liquid can be selected appropriately, and examples of the method that can be used include a method of spraying or applying the binder liquid directly or in a foamed state to the other main surface of the fabric (10) using a spray or an impregnated roll, or a method of immersing the other main surface of the fabric (10) in the binder liquid. The amount of binder liquid applied to the other main surface of the fabric (10) is appropriately adjusted so as to provide the surfacing material (100) of the present invention. The number of times that the binder liquid (12) is applied to the other main surface of the fabric (10) may be one or more times.
[0095] Step (7) will now be described.
[0096] A binder solvent and / or dispersion medium is applied to the other main surface of the fabric (10) (the main surface to which the binder liquid has been applied, the left main surface on the paper in FIG. 3(3)).
[0097] In this process of the present invention, the binder liquid (12 in FIG. 3(3)) present on the other main surface is moved from that other main surface to the inside of the fabric by the binder solvent and / or dispersion medium (hereinafter, sometimes referred to as a solvent-containing liquid or a dispersion medium-containing liquid) that is subsequently applied, thereby making it possible to eliminate the presence of the binder liquid on that other main surface.
[0098] The solvent-containing liquid and / or dispersion medium-containing liquid may contain a thickener, an antifoaming agent, etc. The amount of the solvent-containing liquid and / or the dispersion medium-containing liquid applied to the other main surface of the fabric (10) is appropriately adjusted so as to provide the surfacing material (100) according to the present invention. The solvent-containing liquid and / or the dispersion medium-containing liquid may be applied to the other main surface of the fabric (10) once or multiple times.
[0099] Adjusting the amount of the solvent-containing liquid and / or dispersion medium-containing liquid applied to a small amount makes it easier to realize a surface material (100) in which the binder layer (13) is present in a shallow portion on the inner side from the other main surface of the fabric (10) (the left main surface on the paper in FIG. 3(4)). Adjusting the amount of the solvent-containing liquid and / or dispersion medium-containing liquid applied to a large amount makes it easier to realize a surface material (100) in which the binder layer (13) is present in a deep portion on the inner side from the other main surface of the fabric (10) (the left main surface on the paper in FIG. 3(4)). In other words, by adjusting the amount of the solvent-containing liquid and / or dispersion medium-containing liquid applied to the other main surface of the fabric (10), the presence state of the binder layer (13) in the fabric (10) can be adjusted.
[0100] In the conventional method for manufacturing the surface material (100), the binder liquid diluted with the solvent and / or dispersion medium applied to move the binder liquid unintentionally diffuses into the fabric (10). Therefore, even if the amount of the solvent-containing liquid and / or dispersion medium-containing liquid applied to the other main surface of the fabric (10) is adjusted, it is difficult to adjust the state of the binder layer (13) in the fabric (10).
[0101] As a result, it may not be possible to provide a surface with the intended print on the major surface.
[0102] On the other hand, it has been found that the manufacturing method of the surfacing material (100) according to the present invention can prevent the binder liquid diluted with a solvent and / or a dispersion medium from unintentionally diffusing into the fabric (10). As a result, it is easy to adjust the state of the binder layer (13) in the fabric (10).
[0103] In order to efficiently exert the above-mentioned effects, it is preferable to apply a solvent-containing liquid and / or a dispersion medium-containing liquid to the other main surface of the fabric (10) before the binder liquid (12) applied to the other main surface of the fabric (10) dries.
[0104] Furthermore, in the surface material (100) of the present invention produced by the method for producing the surface material (100) of the present invention, a composition constituting the binder layer (13) may be present on one main surface of the fabric (10). By employing the method for producing the surface material (100) of the present invention, even if the composition constituting the binder layer (13) is present on that main surface, the surface material (100) can be produced by controlling the amount of the composition present to be small.
[0105] However, in order to provide a surface material (100) with an even better feel, it is preferable to adjust the amount of the solvent-containing liquid and / or dispersion medium-containing liquid applied to one main surface of the fabric (10) so that a binder layer (13) formed by removing the solvent and / or dispersion medium from the binder liquid (12) is formed on the inner side of one main surface of the fabric (10) (the right main surface on the page in Figure 3 (4)).
[0106] Step (8) will now be described. The solvent and / or dispersion medium contained in the fabric prepared as described above is removed.
[0107] The method for removing the solvent or dispersion medium can be appropriately selected, but for example, the solvent or dispersion medium can be evaporated and removed by heating in a heater such as an oven dryer, far-infrared heater, dry heat dryer, or hot air dryer, or by leaving the material to stand at room temperature or under reduced pressure, etc. The heating temperature when removing the solvent or dispersion medium is a temperature at which the solvent or dispersion medium can volatilize, and the upper limit of the heating temperature is adjusted so that the components of the fabric (10) and the functions of the resin constituting the binder are not unintentionally reduced.
[0108] In addition, in the case where the composition is provided with particles that expand when heated, the particles may be expanded in this step.
[0109] Through the above-mentioned steps, a binder layer (13) formed by removing the solvent and / or dispersion medium from the binder liquid (12) can be formed at least on the inner side of the other main surface of the fabric (10) (the left main surface on the page in FIG. 3(4)). FIG. 3(4) illustrates a surface material (100) having no binder layer (13) on both main surfaces as an example of the surface material (100) of the present invention. As a result, a surface material (100) satisfying the configuration of the present invention shown in FIG. 3(4) can be prepared.
[0110] Whether or not the print (11) contains the composition constituting the binder layer (13) may be determined by checking the manufacturing process of the surface material (100). In other words, when the surface material (100) is prepared by applying a printing liquid to the main surface on which the binder liquid, the composition constituting the binder layer (13), or the binder layer (13) is present, the composition constituting the binder layer (13) is unintentionally mixed into the print (11) present on the prepared surface material (100). As a result, the print (11) contains the composition constituting the binder layer (13).
[0111] In contrast, in the method for producing a surface material (100) according to the present invention, a binder liquid is applied to a fabric (10) having a print (11) to produce the surface material (100). Therefore, even if the binder liquid is applied to the print (11) present on the surface of the surface material (100), the binder liquid can be prevented from unintentionally diffusing into the fabric (10), and the composition constituting the binder layer (13) is not unintentionally mixed into the print (11). Therefore, the method for producing a surface material (100) according to the present invention can provide a surface material (100) having a print (11) on the main surface of the fabric (10) that does not contain the composition constituting the binder layer (13). As a result, a surface material (100) can be provided in which the problem of poor color development in the print (11) caused by the print (11) not containing the composition constituting the binder layer (13) is prevented.
[0112] The applicant of the present application has investigated a method for applying a binder liquid (12 in FIG. 4(2)) to one of the main surfaces (the left main surface on the page) of a fabric (10 in FIG. 4(1)) before a print is applied, as shown in FIG. 4, which is a schematic cross-sectional view showing the manufacturing process of the surface material according to Patent Document 1, and then applying a solvent-containing liquid and / or a dispersion medium-containing liquid to the one of the main surfaces (the main surface on the side to which the binder liquid has been applied, the left main surface on the page in FIG. 4).
[0113] As a result of the investigation, it was found that the binder liquid, diluted with the solvent and / or dispersion medium applied to move the binder liquid, unintentionally diffuses into the fabric (10) by capillary action. Therefore, as shown in Figure 4 (3), the composition constituting the binder layer (13) was unintentionally present on the main surface (the main surface on the right side of the paper) on which the print was to be applied.
[0114] When printing liquid is applied to such a main surface to partially form a print (14 in FIG. 4(4)), the print (14) is present on the main surface of the fabric while containing the composition constituting the binder layer (13) that is unintentionally present on the main surface (FIG. 4(4)). As a result, a problem occurs in which the color of the print (14) is poor, and it is sometimes impossible to provide a surface material (100) with the intended print (14) on its main surface.
[0115] Furthermore, when printing liquid is applied to a main surface on which the composition constituting the binder layer (13) is present, the presence of the composition causes the printing liquid to be repelled from the main surface, resulting in problems such as the print (14) not adhering properly, and in some cases making it impossible to provide a surface material with the intended print (14) on the main surface.
[0116] In contrast to the above-mentioned conventional manufacturing methods, the manufacturing method of the present invention can prepare a surface material (100) having a print (11) that does not contain a composition constituting the binder layer (13). The surface material (100) is laminated with a separately prepared substrate and subjected to a molding process to prepare an interior material. Alternatively, the surface material (100) may be subjected to various secondary processes, such as a process of processing the surface material (100) by punching it into a specific shape according to the application or mode of use, or a process of adjusting various physical properties such as thickness and surface smoothness by reliant press processing, and the surface material (100) that has undergone the secondary process may be subjected to a molding process to prepare an interior material. EXAMPLES
[0117] The present invention will be specifically described below with reference to examples, but the scope of the present invention is not limited thereto.
[0118] (Fabric Preparation) A fiber web was formed by opening 100% dyed polyester fibers (fineness: 1.3 dtex, fiber length: 51 mm) with a carding machine. Then, the fibers were carded from one side with a needle density of 800 / cm. 2 Then, the fabric is subjected to a needle punching process at 150°C. This process produces a single-layer nonwoven fabric (basis weight: 180 g / m 2 A film having a thickness of 1300 μm was prepared.
[0119] (Preparation of binder liquid) A binder liquid (binder dispersion) was prepared by mixing the following ingredients. Thickener (solid content: 0.41 parts by weight) 27 parts by weight Defoamer (solid concentration: 0.16 parts by weight) 0.4 parts by weight Acrylic styrene resin emulsion (Tg of acrylic styrene resin: -5°C, solid content: 15.75 parts by mass) 35 parts by mass 1 part 25% ammonia water ·Water...36.6 parts by mass
[0120] (Preparation of Dispersion Medium-Containing Liquid) A dispersion medium-containing liquid was prepared by mixing the following ingredients. Thickener (solid content: 0.41 parts by weight) 19.5 parts by weight Defoamer (solid concentration: 0.16 parts by weight) 0.4 parts by weight 1 part 25% ammonia water ·Water...79.1 parts by mass The dispersion medium-containing liquid did not contain any binder component.
[0121] (Preparation of printing liquid) A printing liquid was prepared in the following proportions. Acrylic acid ester resin emulsion (Tg of acrylic acid ester resin: -40°C, solid content of acrylic acid ester resin emulsion: 50% by mass): 20 parts by mass Thickener (solid content: 1.5% by weight): 25 parts by weight Defoamer (solid content: 14% by weight): 0.5 parts by weight Silicone resin emulsion (solid content: 33.8% by weight): 3 parts by weight Black pigment (solid content: 3.8% by weight): 0.1 parts by weight 25% ammonia water: 1 part by weight ·Water: 50.4 parts by mass
[0122] Comparative Example 1 A binder liquid was applied to the entire surface of one of the main surfaces of the single-layer nonwoven fabric using a cylinder at a rate of 280 g / m. 2 Next, a cylinder was used to apply 400 g / m of the dispersion medium-containing liquid to the entire main surface on the side where the binder liquid was applied. 2 Granted. Then, the fabric was dried in a tenter dryer at 160°C, whereby the constituent fibers were bonded and fixed together by the acrylic styrene resin contained in the binder liquid, and the dispersion medium was removed. The fabric was then cooled by dissipating heat, resulting in a fabric (basis weight: 225 g / m2) with an acrylic styrene resin layer (binder layer) on the inner side of one of the main surfaces (average value of 100×Z / X: 17%, average value of 100×Y / X: 0%), as shown in Figure 4(3). 2 A film having a thickness of 1300 μm was prepared. In the thus prepared fabric having a binder layer, the composition constituting the binder layer was not present on the main surface on which the binder liquid and the dispersion medium-containing liquid were applied, whereas the composition constituting the binder layer was present on the main surface opposite to the side on which the binder liquid and the dispersion medium-containing liquid were applied. Next, the printing liquid was applied partially to the main surface of the fabric having a binder layer inside, on the side opposite to the side to which the binder liquid and the dispersion medium-containing liquid were applied, using a cylinder. Thereafter, the fabric was dried using a dryer at a temperature of 160°C, resulting in a surface material (basis weight: 245 g / m2) having a print (a print consisting of a grained print pattern) derived from the printing liquid partially exposed over the entire main surface. 2 , thickness: 1300 μm,) was prepared. In the surface thus prepared, the print contained a composition that constituted a layer of binder.
[0123] Example 1 The printing liquid was applied partially onto one of the main surfaces of the single-layered nonwoven fabric, which was the fabric, using the cylinder used in Comparative Example 1. Thereafter, the fabric was dried using a dryer at a temperature of 160°C, resulting in a fabric (basis weight: 200 g / m2) with a print (a print consisting of a grained print pattern) derived from the printing liquid partially exposed over the entire main surface. 2 A film having a thickness of 1300 μm was prepared. Then, 280 ml / m of binder liquid was applied to the entire main surface of the fabric with the print opposite the main surface on which the print was present, using a cylinder. 2 Next, a cylinder was used to apply 400 ml / m of the dispersion medium-containing liquid to the entire main surface on the side where the binder liquid was applied. 2 Granted. Then, the fabric was dried in a tenter dryer at 160°C, whereby the constituent fibers were bonded and fixed together by the acrylic styrene resin contained in the binder liquid, and the dispersion medium was removed. The fabric was then cooled by dissipating heat, resulting in a fabric (basis weight: 245 g / m2) with an acrylic styrene resin layer (binder layer) on the inner side of one main surface (average value of 100×Y / X: 15%) and on the inner side of the other main surface (average value of 100×Z / X: 17%), as shown in Figure 3(4). 2 A film having a thickness of 1300 μm was prepared. In the thus prepared fabric having a binder layer therein, the composition constituting the binder layer was not present on either of the main surfaces. Also, in the surface material prepared, the print did not contain any composition that constitutes the binder layer.
[0124] (Method of evaluating print appearance and color, and the evaluation results) The main surface of the surface material on which the print was present was visually inspected to evaluate the color and state of the print. As a result of the confirmation, the color of the print on the surface material prepared in Example 1 was black, whereas the color of the print on the surface material prepared in Comparative Example 1 was gray. The reason for this was thought to be that the print on the surface material prepared in Comparative Example 1 contained a composition that constitutes a binder layer.
[0125] In addition, in the surface material prepared in Comparative Example 1, there were faint areas in the print. The reason for this was thought to be that the printing liquid was applied to the main surface where the composition constituting the binder layer was present, and the printing liquid was repelled. In contrast, in the surface material prepared in Example 1, there were no faint areas in the print. The reason for this was thought to be that the printing liquid was applied to the main surface where the composition constituting the binder layer was not present.
[0126] From the above results, it was found that the surface material satisfying the constitution of the present invention was a surface material that prevented the occurrence of poor color development of the print.In addition, the surface material satisfying the constitution of the present invention was a surface material that prevented the occurrence of the problem that the print does not adhere well to the main surface due to the presence of the composition that constitutes the binder layer. [Industrial Applicability]
[0127] The surface material of the present invention is a surface material that can be used to prepare various interior materials, particularly interior materials such as vehicle ceilings, pillar garnishes, doors, instrument panels, steering wheels, shift levers, console boxes, tonneau covers, luggage floors, and luggage sides. [Explanation of symbols]
[0128] 100: Surface material 10:Fabric 11: Print that does not contain a composition that constitutes a binder layer 12: Applied binder liquid 13: Binder layer 14: Print containing a composition constituting a binder layer W: The thickness of the binder layer at the line segment connecting the two main surfaces of the fabric constituting the surface material at the shortest distance X: Thickness of the fabric that constitutes the surface material Y: Depth from one main surface to where the binder layer exists Z: The depth from the other main surface to where the binder layer exists A: The end point of one of the main surfaces of the fabric in the line segment that connects the two main surfaces of the fabric constituting the surface material at the shortest distance (the point of contact between one of the main surfaces and the line segment) B: The end point of the line segment that connects the two principal surfaces of the fabric constituting the surface material at the shortest distance on the other principal surface side of the fabric (the point of contact between the other principal surface and the line segment) a: Intersection of the contour of one main surface of the binder layer and the line segment b: Intersection of the line segment with the contour of the other main surface of the binder layer
Claims
1. A surface material comprising a fabric, a print partially present on one main surface of the fabric, and a layer of a binder, the binder layer is present on the inner side of the other main surface of the fabric, The print does not contain the composition that constitutes the binder layer. Surface material.
2. (Step 1) preparing a fabric; (Step 2) preparing a printing liquid containing a composition constituting a print and a solvent and / or a dispersion medium for said composition; (Step 3) applying a printing liquid partially to one main surface of the fabric; (Step 4) removing the solvent and / or dispersion medium from the fabric to which the printing liquid has been partially applied, thereby forming a print partially on the one main surface of the fabric; (Step 5) preparing a binder liquid containing a binder and a solvent and / or a dispersion medium for the binder; (Step 6) applying the binder liquid to the other main surface of the fabric; (Step 7) applying a solvent and / or a dispersion medium for the binder to the other main surface of the fabric; (Step 8) removing the binder solvent and / or dispersion medium from the fabric; A method for manufacturing a surface material comprising the steps of:
Citation Information
Patent Citations
Skin material
JP2015104848A
Skin material for vehicle interior
JP2016147466A
Surface material and method for manufacturing the same
JP2021098922A