Mask formation method, substrate processing method, and substrate inspection method

By incorporating alignment and correction steps in laser processing, the method addresses precision issues in mask formation on substrates, resulting in high-quality masks for precise etching and improved device performance.

JP2024156258APending Publication Date: 2024-11-06DISCO CORP
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2023070570
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-24
Publication Date
2024-11-06

Smart Images

  • Figure 2024156258000001_ABST
    Figure 2024156258000001_ABST
Patent Text Reader

Abstract

To form a high-quality mask.SOLUTION: There is provided a mask formation method for forming, on a reverse side of a substrate having a pattern provided on the surface side, a mask having an opening corresponding to the pattern, the method including: a coating step for coating the reverse side the substrate with a protective film; an alignment step for detecting the position of the pattern; and a mask formation step for removing the protective film at a position corresponding to the pattern so as to form the mask having the opening. In the mask formation step, a test pattern is formed on the protective film, the position of the test pattern is detected, the position of the pattern is detected, an amount of a deviation between the detected position of the test pattern and the detected position of the pattern is calculated as a test deviation amount, a correction amount is calculated on the basis of the test deviation amount, and the position where the protective film is to be removed is corrected on the basis of the correction amount and the protective film is removed, whereby the opening is formed in the protective film and the mask is formed.SELECTED DRAWING: Figure 11
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method of forming a mask for processing a substrate, a method of processing a substrate, and a method of inspecting a substrate. [Background technology]

[0002] In the device chip manufacturing process, a wafer is used in which devices are formed in multiple areas partitioned by multiple streets (planned division lines) arranged in a grid pattern. By dividing this wafer along the streets, chips equipped with devices (device chips) are obtained. The device chips are incorporated into various electronic devices such as mobile phones and personal computers.

[0003] To divide a substrate such as a wafer, a cutting device that cuts the substrate with an annular cutting blade, a laser processing device that performs laser processing on the substrate, etc. In recent years, development of a process called plasma dicing, in which the substrate is divided by performing plasma etching on the substrate, has also been progressing.

[0004] In plasma dicing, a protective film (resist film) is first formed on the front or back surface of the substrate, and then a mask with openings is formed on the substrate by patterning the protective film so that patterns such as streets are exposed. Then, etching gas in a plasma state is supplied to the wafer through the mask. This applies plasma etching to the wafer along the pattern (streets), and the wafer is divided into multiple device chips.

[0005] In addition, in the manufacturing process of device chips including MEMS devices, a pattern of a plurality of structures and the like is formed on the front side of a substrate. A processing method is known in which the rear side of the substrate is covered with a protective film, the protective film is removed from the rear side of the substrate in an area corresponding to the pattern to form an opening, a mask for etching is formed, and etching is performed through the formed mask to form a hole along the pattern (structure) (see Patent Document 1).

[0006] A mask formed for plasma etching or the like is formed, for example, by patterning a photoresist along a pattern of a street or a structure, etc. However, when forming a mask from photoresist, processes such as coating, exposing, and developing the photoresist are time-consuming and expensive equipment such as an exposure device is required.

[0007] Therefore, in order to simplify the mask formation process and reduce costs, a method of forming a mask using a laser processing device has been proposed. For example, a method is known in which a protective film is formed on a wafer, and then the protective film is partially removed along a pattern by irradiating it with a laser beam to form a mask that exposes the area to be processed (see Patent Document 2). Using this method, a mask can be formed more easily and at lower cost than when using a photoresist. [Prior art documents] [Patent documents]

[0008] [Patent Document 1] JP 2016-18869 A [Patent Document 2] JP 2016-207737 A Summary of the Invention [Problem to be solved by the invention]

[0009] In the above-mentioned processing method, when the protective film is partially removed at a predetermined position to form an etching mask, the protective film needs to be irradiated with a laser beam with high accuracy. However, the state of the optical system may change during the irradiation of the protective film with the laser beam, causing deviations in the position and size of the irradiated area of ​​the laser beam, resulting in a decrease in the irradiation accuracy of the laser beam.

[0010] When a protective film is irradiated with a laser beam with reduced irradiation accuracy, the position and size of the area exposed from the mask on the substrate will not match the area planned for etching, resulting in a low-quality mask, which will result in etching not being performed as planned, leading to poor characteristics of the final device.

[0011] The method of processing the protective film to form a mask may be performed by means other than a laser beam. For example, a mask is formed by cutting a predetermined area of ​​the protective film with an annular cutting blade to partially remove the protective film. Even in this case, the position and size of the area of ​​the substrate exposed from the mask may not match the area planned for etching, resulting in a low-quality mask.

[0012] The present invention has been made in consideration of such problems, and aims to provide a mask forming method for forming a high-quality mask, a substrate processing method using a high-quality mask, and an inspection method for inspecting a substrate, such as a substrate having a hole formed therein. [Means for solving the problem]

[0013] According to one aspect of the present invention, there is provided a method for forming a mask having an opening on a back side of a substrate having a pattern on its front side, the method including: a covering step of covering the back side of the substrate with a protective film; an alignment step of imaging the pattern provided on the front side of the substrate and detecting the position of the pattern; and a mask forming step of forming the mask having the opening by removing the protective film at a position corresponding to the pattern, the mask forming step including a test processing step of removing the protective film in a region corresponding to the pattern on the front side of the substrate and forming a test pattern in the protective film; and imaging the test pattern formed in the protective film in the test processing step, The present invention provides a method for forming a mask, comprising: a test pattern position detection step for detecting a position of the test pattern; a pattern position detection step for imaging the pattern provided on the front surface side of the substrate and detecting the position of the pattern; a correction amount calculation step for calculating a deviation amount between the position of the test pattern detected in the test pattern position detection step and the position of the pattern detected in the pattern position detection step as a test deviation amount and calculating a correction amount based on the test deviation amount; and a main processing step for correcting a position at which the protective film is to be removed based on the correction amount calculated in the correction amount calculation step, thereby removing the protective film, and forming the opening in the protective film to form the mask.

[0014] Preferably, in the alignment step and the pattern position detection step, light having a wavelength that passes through the substrate is used as illumination light to image the pattern provided on the front side of the substrate from the back side.

[0015] Also, preferably, in the test processing step, the protective film is removed only in a part of the region corresponding to the pattern on the front surface side of the substrate, to form the test pattern on the protective film.

[0016] More preferably, in the test processing step and the main processing step, the protective film is irradiated with a laser beam using a laser irradiation unit including a laser oscillator that emits a laser beam, an fθ lens that focuses the laser beam, and a scanning unit that scans the laser beam emitted by the laser oscillator and focused by the fθ lens, to remove the protective film, and in the main processing step, the scanning unit is controlled by referring to the correction amount.

[0017] According to another aspect of the present invention, there is provided a method for processing a substrate, the method comprising: a covering step of covering the rear side of the substrate with a protective film; an alignment step of imaging the pattern provided on the front side of the substrate to detect the position of the pattern; a mask forming step of forming a mask by removing the protective film at a position corresponding to the pattern and forming an opening in the protective film; and an etching step of etching the substrate through the mask to form a hole on the rear side of the substrate according to the pattern, the mask forming step including a test processing step of removing the protective film in a region corresponding to the pattern on the front side of the substrate and forming a test pattern in the protective film; a pattern position detection step of imaging the test pattern formed on the protective film and detecting a position of the test pattern, a pattern position detection step of imaging the pattern provided on the front side of the substrate and detecting a position of the pattern, a correction amount calculation step of calculating a deviation amount between the position of the test pattern detected in the test pattern position detection step and the position of the pattern detected in the pattern position detection step as a test deviation amount and calculating a correction amount based on the test deviation amount, and a main processing step of correcting a position at which the protective film is to be removed based on the correction amount calculated in the correction amount calculation step, thereby removing the protective film, and forming the opening in the protective film to form the mask.

[0018] According to yet another aspect of the present invention, after the etching step, the method includes a hole formation position detection step of imaging the hole formed on the back surface of the substrate and detecting the position of the hole, a processing deviation amount calculation step of calculating the amount of deviation between the position of the pattern detected in the pattern position detection step and the position of the hole detected in the hole formation position detection step as a processing deviation amount, and an acceptability determination step of determining whether the processing deviation amount calculated in the processing deviation amount calculation step falls within an allowable range. Effect of the Invention

[0019] In a method for forming a mask and a method for processing a substrate according to an embodiment of the present invention, a test pattern is formed by removing a protective film in an area corresponding to the pattern, and a correction amount is calculated based on the amount of misalignment between the test pattern and the pattern. The calculated correction amount can be used when forming an opening at a predetermined position in the protective film. As a result, a high-quality mask in which an opening is formed at a predetermined position with high accuracy is formed on the substrate.

[0020] By using a high-quality mask to process a substrate, holes can be formed in the substrate with high precision. This results in devices that are constructed using the pattern having good characteristics. Furthermore, when the misalignment between the hole formed in the substrate and the pattern provided on the front side of the substrate is evaluated as the amount of processing misalignment, the amount of processing misalignment is extremely small.

[0021] Therefore, one aspect of the present invention provides a mask forming method for forming a high quality mask, a substrate processing method using a high quality mask, and an inspection method for inspecting a substrate, such as a substrate having a hole formed therein. [Brief description of the drawings]

[0022] [Figure 1] FIG. 1(A) is a perspective view that typically shows a substrate, and FIG. 2(B) is a perspective view that typically shows an enlarged portion of the surface of the substrate. [Diagram 2]FIG. 2A is a cross-sectional view that typically shows a substrate, and FIG. 2B is a cross-sectional view that typically shows a substrate on which a protective film has been formed. [Diagram 3] FIG. 2 is a partially sectional front view showing a film forming apparatus; [Figure 4] FIG. 1 is a perspective view showing a schematic diagram of a laser processing apparatus. [Diagram 5] 10A and 10B are cross-sectional views each showing a schematic state in which a protective film is laser-processed. [Figure 6] FIG. 6(A) is a cross-sectional view showing a schematic diagram of a substrate on which a protective film has been laser-processed to form a mask having an opening, and FIG. 6(B) is a cross-sectional view showing a schematic diagram of a substrate on which a hole has been formed by etching. [Figure 7] FIG. 7(A) is a plan view showing a schematic view of the back side of a substrate having a protective film formed on the back side, and FIG. 7(B) is a cross-sectional view showing a schematic view of the substrate before test processing of the protective film is performed. [Figure 8] FIG. 8(A) is a plan view showing a schematic view of the back surface side of a substrate when a test pattern is formed on a protective film, and FIG. 8(B) is a cross-sectional view showing a schematic view of the substrate and the protective film on which the test pattern is formed. [Figure 9] 2 is a cross-sectional view illustrating a substrate placed on a chuck table. FIG. [Figure 10] FIG. 2 is a cross-sectional view showing a schematic diagram of a substrate to be imaged. [Figure 11] Figure 11(A) is a plan view showing a schematic example of an image obtained by imaging the back side of a substrate with a test pattern formed on a protective film, Figure 11(B) is a plan view showing a schematic example of an image obtained by imaging the front side of the substrate, and Figure 11(C) is a plan view showing a schematic example of the positional relationship between the test pattern formed on the protective film and a pattern provided on the substrate. [Figure 12] 1 is a partially cross-sectional front view showing a schematic view of a plasma processing apparatus; [Figure 13] 1 is a cross-sectional view illustrating a substrate being plasma etched; [Figure 14]FIG. 14(A) is a plan view showing a schematic representation of the positional relationship between a pattern provided on a substrate and a hole formed in the substrate, and FIG. 14(B) is a cross-sectional view showing a schematic representation of the hole formed in the substrate. [Figure 15] FIG. 15(A) is a flowchart showing the flow of each step performed in a substrate processing method, and FIG. 15(B) is a flowchart showing the flow of each step performed in a mask formation step. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0023] Hereinafter, an embodiment according to one aspect of the present invention will be described with reference to the accompanying drawings. First, a configuration example of a substrate on which a mask is formed by the mask forming method according to the embodiment and a substrate processed using a mask by the substrate processing method according to the embodiment will be described. Fig. 1(A) is a perspective view showing a substrate 1 as a schematic diagram.

[0024] The substrate 1 is a plate-like member having a pair of surfaces. For example, the substrate 1 is a disk-like wafer made of a semiconductor material such as single crystal silicon, and includes a front surface (first surface) 1a and a back surface (second surface) 1b that are generally parallel to each other. The substrate 1 is divided into a plurality of rectangular regions by a plurality of streets (planned division lines) 3 that are arranged and set in a lattice pattern so as to intersect with each other.

[0025] However, there are no limitations on the material, shape, structure, size, etc. of the substrate 1. For example, the substrate 1 may be a wafer (substrate) made of a semiconductor other than silicon (GaAs, InP, GaN, SiC, etc.), sapphire, glass, ceramics, resin, metal, etc.

[0026] Devices 5 such as ICs (Integrated Circuits), LSIs (Large Scale Integration), LEDs (Light Emitting Diodes), MEMS (Micro Electro Mechanical Systems) devices, etc. are formed on the front surface 1a side of the multiple regions partitioned by the streets 3. By dividing the substrate 1 along the streets 3, multiple chips (device chips) each including a device 5 are manufactured. There are no limitations on the type, number, shape, structure, size, arrangement, etc. of the devices 5.

[0027] The substrate 1 is processed along the streets 3, and a dividing groove extending from the front surface 1a to the back surface 1b is formed in the substrate 1. When the substrate 1 is divided, for example, a mask (a patterned protective film) having an opening is formed on the front surface 1a or the back surface 1b of the substrate 1. The opening of the mask overlaps with the streets 3, and the substrate 1 is processed by etching or the like in the area exposed from the mask, thereby forming a dividing groove in the substrate 1.

[0028] 1(B) is a perspective view showing an enlarged schematic view of the surface 1a side of the substrate 1, and FIG. 2(A) is a cross-sectional view showing the substrate 1. On the surface 1a side of the substrate 1, countless various patterns 7, such as elements of specific shapes, wiring, circuits, electrodes, etc., included in the device 5, are formed. In other words, the device 5 is composed of various patterns 7. In each figure, a representative example of the pattern 7 is shown typically, but the shape, thickness, size, function, etc. of the pattern 7 are not particularly limited, and the number, arrangement, type, and number of types of each pattern 7 are also not limited.

[0029] In addition to the specific pattern 7, various structures are formed on the surface 1a of the substrate 1. In Fig. 2(A) and other figures, these structures are collectively expressed as one layer 9, but the layer 9 is not a single layer formed of a single material, but a layer formed by combining multiple layers having a specific planar shape. The layer 9 can also be called a functional layer.

[0030] In the device 5, a hole reaching a specific pattern 7 is formed from the rear surface 1b side of the substrate 1. When forming the hole in the substrate 1, a mask having an opening is formed on the rear surface 1b of the substrate 1. The opening of the mask is formed, for example, in an area overlapping with the pattern 7. Then, the substrate 1 is processed, such as by etching, in the area exposed from the mask, thereby forming the hole in the substrate 1.

[0031] Hereinafter, the substrate processing method according to this embodiment will be described taking as an example a case where a hole overlapping with a pattern 7 is formed in the substrate 1. Fig. 15(A) is a flowchart showing the flow of each step performed in the substrate processing method according to this embodiment.

[0032] In this substrate processing method, first, the back surface 1b side of the substrate 1 is covered with a protective film that will be the material of the mask (covering step S10). After that, the protective film is processed to form a mask having openings in predetermined regions on the substrate 1 (mask forming step S30), and the substrate 1 is processed using the mask (etching step S40). The substrate processing method described below includes a method of forming a mask used in processing. First, various devices used in the substrate processing method according to this embodiment will be described.

[0033] First, a film forming apparatus in which the coating step S10 is performed will be described. Fig. 3 is a partial cross-sectional front view that shows a schematic view of a film forming apparatus 2 that forms a protective film (resist film) that serves as a mask material on a substrate 1. The film forming apparatus 2 supplies a liquid resin that serves as a material for the protective film to the substrate 1, thereby forming a protective film 11 that covers the surface of the substrate 1.

[0034] The film forming apparatus 2 includes a cover 4 that houses each of the components of the film forming apparatus 2. The cover 4 is formed in a hollow cylindrical shape, and the inside of the cover 4 corresponds to a processing space 6 in which the protective film 11 is formed.

[0035] The cover 4 houses a spinner table 8 that holds the substrate 1. The upper surface of the spinner table 8 is a flat surface roughly parallel to the horizontal plane, and constitutes a holding surface 8a that holds the substrate 1. The holding surface 8a is connected to a suction source (not shown) such as an ejector via a flow path (not shown), a valve (not shown), and the like formed inside the spinner table 8. When the suction force (negative pressure) of the suction source is applied to the holding surface 8a with the substrate 1 placed on the holding surface 8a, the substrate 1 is sucked and held by the spinner table 8.

[0036] A cylindrical rotating shaft 10 is connected to the spinner table 8. The rotating shaft 10 is inserted into an opening 4a provided in the bottom wall of the cover 4. The upper end side of the rotating shaft 10 is fixed to the center of the lower surface side of the spinner table 8 in the processing space 6, and the lower end side of the rotating shaft 10 is disposed outside the cover 4.

[0037] The lower end of the rotating shaft 10 is connected to a motor 14 via a rotary joint 12. When the motor 14 is driven, the power of the motor 14 is transmitted to the spinner table 8 via the rotary joint 12 and the rotating shaft 10, causing the spinner table 8 to rotate around a rotation axis that is roughly parallel to the vertical direction.

[0038] The cover 4 also contains a protective film material supply unit 20 that supplies a protective film material 18, which is the raw material of the protective film 11. For example, the protective film material 18 is a liquid resin produced by dissolving a solute in a solvent. Specifically, water is used as the solvent, and a water-soluble resin is used as the solute.

[0039] Specific examples of water-soluble resins include polyvinyl alcohol (PVA), polyvinylpyrrolidone (PVP), polyethylene glycol (PEG), polyethylene oxide (PEO), hydroxypropyl cellulose, methyl cellulose, ethyl cellulose, polyacrylic acid, poly-N-vinyl acetamide, polystyrene sulfonic acid, special nylon, phenolic resin, methylol melamine resin, polyglycerin, etc.

[0040] The protective film material supply unit 20 includes an L-shaped arm 22. A supply nozzle 24 that supplies protective film material 18 toward the holding surface 8a of the spinner table 8 is attached to the tip end (one end) of the arm 22. The arm 22 is inserted into an opening 4b provided in the bottom wall of the cover 4, and a base end (the other end) of the arm 22 is disposed outside the cover 4.

[0041] A motor 26 is connected to the base end of the arm 22. When the motor 26 is driven, the arm 22 rotates about a rotation axis that is approximately parallel to the vertical direction, and the supply nozzle 24 pivots about the rotation axis of the arm 22. This allows the supply nozzle 24 to be positioned at a position where it overlaps the holding surface 8a (supply position) and a position where it does not overlap the holding surface 8a (retracted position).

[0042] A protective film material supply source 28 is connected to the arm 22, which supplies the protective film material 18 to the arm 22. The protective film material 18 supplied from the protective film material supply source 28 to the arm 22 is supplied to the supply nozzle 24 via a flow path (not shown) provided inside the arm 22, and is dropped from the supply nozzle 24 onto the substrate 1 held by the spinner table 8.

[0043] Substrate 1 is placed on spinner table 8 with front surface 1a facing holding surface 8a, substrate 1 is held by suction on spinner table 8, and protective film material 18 is dropped onto rear surface 1b of substrate 1 while rotating spinner table 8, whereby rear surface 1b of substrate 1 is coated with protective film material 18. That is, spin coating is performed.

[0044] The excess protective film material 18 supplied to the rear surface 1b of the substrate 1 advances outward from the outer edge of the substrate 1, drops through the processing space 6, and reaches the bottom wall of the cover 4. An opening 4c is provided in the bottom wall of the cover 4, and a drain pipe 30 is connected to the opening 4c. The protective film material 18 that has reached the bottom wall of the cover 4 is discharged from the drain pipe 30 to the outside of the processing space 6. Then, the dripping of the protective film material 18 from the supply nozzle 24 is stopped, and the protective film material 18 is dried on the rear surface 1b of the substrate 1, whereby the rear surface 1b of the substrate 1 is covered with the protective film 11.

[0045] Next, a description will be given of a laser processing apparatus in which the mask forming step S30 and the like are performed. Fig. 4 is a perspective view showing a schematic view of the laser processing apparatus 32. The laser processing apparatus 32 includes a base 34 that supports each of the components.

[0046] An X-axis direction moving table 46 is provided above the base 34. The lower side of the bottom plate of the X-axis direction moving table 46 is slidably attached to a pair of X-axis guide rails 48. An X-axis linear scale 48a is provided near the X-axis guide rails 48.

[0047] A reading head (not shown) is provided on the underside of the X-axis direction moving table 46. The reading head is used to detect the scale of the X-axis linear scale 48a, thereby calculating the position (coordinate) of the X-axis direction moving table 46 in the X-axis direction and the amount of movement in the X-axis direction.

[0048] A nut portion (not shown) is provided on the lower surface side of the bottom plate of the X-axis direction moving table 46, and a screw shaft 50 arranged approximately parallel to the X-axis direction is rotatably connected to this nut portion via balls (not shown). A motor 52 is connected to one end of the screw shaft 50.

[0049] When the motor 52 is operated, the screw shaft 50 rotates, and the X-axis direction moving table 46 moves along the X-axis direction. The pair of X-axis guide rails 48, the screw shaft 50, the motor 52, etc. constitute an X-axis direction moving mechanism 54.

[0050] The pair of X-axis guide rails 48 are fixed onto the Y-axis moving table 36. The Y-axis moving table 36 is slidably mounted on the pair of Y-axis guide rails 38 fixed to the upper surface of the base 34.

[0051] A Y-axis linear scale 38a used for detecting the position in the Y-axis direction of the Y-axis moving table 36 is provided near the Y-axis guide rail 38. A nut portion (not shown) is provided on the lower surface side of the Y-axis moving table 36.

[0052] A screw shaft 40 arranged substantially parallel to the Y-axis guide rail 38 is rotatably connected to the nut portion via balls (not shown). A motor 42 is connected to one end of the screw shaft 40. The Y-axis guide rail 38, the screw shaft 40, the motor 42, etc. constitute a Y-axis direction movement mechanism 44.

[0053] A chuck table 56 is supported on the X-axis direction moving table 46. When the X-axis direction moving mechanism 54 is operated, the chuck table 56 can be moved along the X-axis direction. When the Y-axis direction moving mechanism 44 is operated, the chuck table 56 can be moved along the Y-axis direction.

[0054] Next, the X-axis direction moving table 46 and the chuck table 56 will be described in detail with reference to Fig. 9. Fig. 9 includes a side view that shows a schematic representation of the X-axis direction moving table 46 and a partial cross-sectional side view that shows a schematic representation of the chuck table 56. However, in Fig. 9, hatching that should be applied to the cross section has been omitted for ease of explanation.

[0055] The chuck table 56 has a disk-shaped holding member 56a. The upper and lower surfaces of the holding member 56a are flat and parallel to each other. The holding member 56a is made of a transparent material that transmits visible light and infrared light (e.g., near-infrared light). The holding member 56a is made of, for example, quartz glass, borosilicate glass, or soda glass, but may also be made of calcium fluoride, lithium fluoride, or magnesium fluoride.

[0056] Suction paths (not shown) are formed inside the holding member 56a, and are connected to a plurality of suction ports (not shown) formed on the upper surface of the holding member 56a. A suction source (not shown), such as an ejector, is also connected to the suction paths. When the substrate 1 is placed on the holding member 56a and the suction source is operated, negative pressure acts on the substrate 1 through the suction paths and the suction ports, and the substrate 1 is sucked and held on the chuck table 56. Therefore, the upper surface of the holding member 56a functions as a holding surface.

[0057] In the suction passages and openings formed in the holding member 56a, a part of the light incident on the holding member 56a is scattered or reflected. Therefore, the holding member 56a is not completely transparent when viewed from the top or bottom, and may have light-shielding or opaque parts. However, a predetermined area of ​​the holding member 56a excluding these suction passages is transparent from the top to the bottom.

[0058] The X-axis direction moving table 46 includes a rectangular bottom plate 46a. The lower (-Z direction) side of the bottom plate 46a is slidably attached to a pair of X-axis guide rails 48. In addition, the lower end of a rectangular side plate 46b is connected to the front end (+X direction) of the bottom plate 46a.

[0059] A front end of a rectangular top plate 46c similar to the bottom plate 46a is connected to an upper end of the side plate 46b. The bottom plate 46a and the top plate 46c are arranged to overlap in the Z-axis direction, and the bottom plate 46a, the side plate 46b, and the top plate 46c form a space 46d that is open on both the rear (-X direction) side and the Y-axis direction.

[0060] A frame 56b of the chuck table 56 is supported on the upper surface side of the top plate 46c so as to be rotatable about a rotation axis that is substantially parallel to the Z-axis direction. A side surface of the frame 56b located above the top plate 46c functions as a pulley portion.

[0061] A rotary drive source 58 such as a motor is provided on the outer side surface of the side plate 46b. A pulley 58a is provided on the rotary shaft of the rotary drive source 58. A belt 60 is looped around the pulley 58a and the frame body 56b.

[0062] When the rotary drive source 58 is operated, the frame 56b rotates around a rotation axis that is approximately parallel to the Z-axis direction. By controlling the rotation of the pulley 58a, the chuck table 56 rotates around the rotation axis by an arbitrary angle.

[0063] A lower imaging unit 64 is fixed to the upper surface of the base 34 via a support arm 63 (see FIG. 4) whose longitudinal portion is disposed along the X-axis direction. A ball screw type lifting unit 62 that raises and lowers the support arm 63 is connected to the base end side of the support arm 63, and the lower imaging unit 64 is fixed to the tip of the support arm 63. When the lifting unit 62 is operated, the lower imaging unit 64 can be raised and lowered.

[0064] The lower imaging unit 64 is a so-called microscope camera unit. For example, the lower imaging unit 64 is composed of two cameras, a low-magnification camera and a high-magnification camera. However, the lower imaging unit 64 may be composed of one camera. The camera constituting the lower imaging unit 64 has a predetermined optical system such as a condenser lens, and an imaging element such as a CCD (Charge-Coupled Device) image sensor or a CMOS (Complementary Metal-Oxide-Semiconductor) image sensor (neither is shown).

[0065] When the X-axis direction moving mechanism 54 is operated to move the X-axis direction moving table 46, the lower imaging unit 64 is inserted into the space 46d of the X-axis direction moving table 46. The lower imaging unit 64 is provided below the chuck table 56. In addition, the optical axis of each condenser lens is disposed approximately perpendicular to the lower surface of the holding member 56a.

[0066] When imaging the substrate 1 with the lower imaging unit 64, the X-axis direction moving table 46 is moved to place the lower imaging unit 64 in the space 46d. Then, the substrate 1 is sucked and held on the chuck table 56 and an image of the substrate 1 is taken from below via the holding member 56a, whereby an image of the underside of the substrate 1 can be obtained. By operating the X-axis direction moving mechanism 54 and the Y-axis direction moving mechanism 44, the imaging area of ​​the substrate 1 can be changed.

[0067] A column 66 is provided at a position adjacent to the lifting unit 62 in the -Y direction so as to protrude upward from the upper surface of the base 34. The column 66 is provided with a casing 68 having a longitudinal portion approximately parallel to the X-axis direction.

[0068] At least a part of a laser irradiation unit (processing unit) 70 is provided in the casing 68. The laser irradiation unit 70 has a head portion 72 provided at the tip of the casing 68, and can irradiate a pulsed laser beam L having a wavelength (e.g., 355 nm) that is absorbed by the substrate 1 from the head portion 72.

[0069] Fig. 5 shows a schematic diagram of the simplest example of the optical system of the laser irradiation unit 70. The laser irradiation unit 70 has a laser oscillator 84 that emits a laser beam, an fθ lens (condenser lens) 88 that focuses the laser beam, and a mirror 86. The laser beam emitted from the laser oscillator 84 is reflected by the mirror 86, focused by the fθ lens 88, and irradiated downward from the head part 72. In Fig. 4, the laser beam L irradiated downward from the head part 72 is indicated by a dashed arrow.

[0070] The mirror 86 is connected to a drive source (not shown) that changes the direction, and the direction is controlled. Changing the direction of the mirror 86 changes the traveling direction of the laser beam emitted from the laser oscillator 84 and reflected by the mirror 86. This changes the position of the focusing point of the laser beam that is irradiated via the fθ lens 88 to the substrate 1 that is sucked and held on the chuck table 56. The direction-variable mirror 86 can function as a scanning unit (galvano scanner) that scans the laser beam emitted by the laser oscillator 84 and focused by the fθ lens 88.

[0071] An upper imaging unit 74 is provided at a position adjacent to the head portion 72 at the tip of the casing 68. The upper imaging unit 74 captures an image of the upper surface side of the substrate 1 held by suction on the chuck table 56. The camera included in the upper imaging unit 74 is configured similarly to the camera of the lower imaging unit 64.

[0072] A housing (not shown) is provided on the base 34, and a touch panel display 76 is provided on the front (+X direction) side of the housing, which serves as both an input section (i.e., an input interface) for the worker to input instructions and a display section for displaying information to the worker.

[0073] The touch panel display 76 displays, for example, captured images captured by the upper imaging unit 74 and the lower imaging unit 64. In addition, the touch panel display 76 may display a processed image created by performing image processing on the captured image.

[0074] The laser processing apparatus 32 includes a controller (control unit) 80 that controls each of the components. The controller 80 is configured by a computer including, for example, a processing device such as a CPU (Central Processing Unit), a main storage device such as a DRAM (Dynamic Random Access Memory), and an auxiliary storage device such as an HDD, SSD, or flash memory. The function of the controller is realized by operating the processing device and the like according to software stored in the auxiliary storage device.

[0075] Furthermore, various information is registered in the auxiliary memory device (memory device 82) of the controller 80, such as information on processing conditions for processing various workpieces, and images of the substrate 1 captured by the lower imaging unit 64 and the upper imaging unit 74.

[0076] Next, a plasma processing apparatus used in the etching step S40 for forming holes in the substrate 1 will be described. Fig. 12 is a partial cross-sectional front view showing a plasma processing apparatus 92. The plasma processing apparatus 92 includes a chamber 94 in which the substrate 1 is housed. The chamber 94 is made of a conductive material such as metal, and is grounded. The inside of the chamber 94 corresponds to a processing space 96 in which the plasma processing on the substrate 1 is carried out.

[0077] An opening 94a for transporting the substrate 1 is provided in a side wall of the chamber 94. A gate (opening / closing door) 98 for opening and closing the opening 94a is provided outside the opening 94a. A moving mechanism (not shown) such as an air cylinder is connected to the gate 98, and the moving mechanism raises and lowers the gate 98 along the side wall of the chamber 94.

[0078] By lowering the gate 98 to expose the opening 94a, the substrate 1 can be carried into the processing space 96 through the opening 94a, or the substrate 1 can be carried out from the processing space 96 through the opening 94a. In addition, by raising the gate 98 to close the opening 94a, the processing space 96 is sealed.

[0079] An opening 94b that connects the inside and outside of the chamber 94 is provided in the bottom wall of the chamber 94. The opening 94b is connected to an exhaust device 102 such as a vacuum pump via piping 100. When the exhaust device 102 is operated with the processing space 96 sealed, the processing space 96 is exhausted and reduced in pressure.

[0080] A chuck table 104 for holding the substrate 1 is provided in the processing space 96. The upper surface of the chuck table 104 is a flat surface that is approximately parallel to the horizontal plane, and constitutes a holding surface 104a for holding the substrate 1.

[0081] An electrostatic chuck that holds the substrate 1 by electrical force can be used as the chuck table 104. For example, the chuck table 104 is made of a dielectric material such as ceramics, and a disk-shaped electrode 106 is provided inside the chuck table 104. The electrode 106 is disposed approximately parallel to the holding surface 104a, and is connected to a high-frequency power source 110 via a matching unit 108.

[0082] A cooling path (not shown) through which a cooling liquid such as water flows may be provided inside the chuck table 104. The chuck table 104 is cooled by causing the cooling liquid to flow through the cooling path and circulating inside the chuck table 104.

[0083] A gas ejection head 112 is provided above the chuck table 104. The gas ejection head 112 is made of a conductive material such as metal, and is inserted into an opening 94c provided in the upper wall of the chamber 94. An annular bearing 114 made of an insulating material is provided between the chamber 94 and the gas ejection head 112. The bearing 114 is provided so as to surround the gas ejection head 112, and insulates the chamber 94 from the gas ejection head 112.

[0084] The gas ejection head 112 is connected to a high-frequency power supply 118 via a matching device 116. In addition, a lifting mechanism (not shown) that raises and lowers the gas ejection head 112 in the vertical direction is connected to the gas ejection head 112. By raising and lowering the gas ejection head 112 with the lifting mechanism, the distance between the chuck table 104 and the gas ejection head 112 is adjusted.

[0085] A gas diffusion space 112a to which gas for plasma processing is supplied is provided inside the gas ejection head 112. A plurality of gas supply paths 112b connecting the processing space 96 and the gas diffusion space 112a are provided on the lower surface side of the gas ejection head 112. A pair of gas supply paths 112c, 112d are provided on the upper surface side of the gas ejection head 112. The gas supply path 112c is connected to a gas supply source 122a via a pipe 120a, and the gas supply path 112d is connected to a gas supply source 122b via a pipe 120b.

[0086] The gas supply source 122a supplies a gas for plasma processing to the gas diffusion space 112a through the pipe 120a and the gas supply path 22c. Similarly, the gas supply source 122b supplies a gas for plasma processing to the gas diffusion space 112a through the pipe 120b and the gas supply path 112d. Then, the two types of gas are mixed in the gas diffusion space 112a. Note that, although FIG. 12 illustrates a form in which gas is supplied to the gas ejection head 112 from two gas supply sources 122a and 122b, the number of gas supply sources connected to the gas ejection head 112 may be one or three or more.

[0087] When performing plasma processing (plasma etching) on ​​the substrate 1 using the plasma processing apparatus 92, first, the gate 98 is lowered to expose the opening 94a. Then, the substrate 1 is carried into the processing space 96 through the opening 94a by a transport mechanism (not shown) and placed on the holding surface 104a of the chuck table 104. Note that, when carrying in the substrate 1, it is preferable to raise the gas ejection head 112 and widen the gap between the chuck table 104 and the gas ejection head 112.

[0088] Next, the gate 98 rises to close the opening 94a, and the processing space 96 is sealed. Then, a predetermined voltage is applied to the electrode 106 by the high frequency power supply 110. This generates dielectric polarization on the holding surface 104a side of the chuck table 104, and an electrostatic adsorption force acts between the holding surface 104a and the substrate 1. As a result, the substrate 1 is adsorbed and held by the holding surface 104a.

[0089] Furthermore, the height of the gas ejection head 112 is adjusted so that the chuck table 104 and the gas ejection head 112 are disposed at a distance suitable for plasma processing. Furthermore, the exhaust device 102 is operated to exhaust the processing space 96 and reduce the pressure.

[0090] Next, gas for plasma processing is supplied from gas supply source 122a and / or gas supply source 122b to gas diffusion space 112a. Also, high frequency power is applied to gas ejection head 112 by high frequency power source 118. As a result, the gas in gas diffusion space 112a is turned into plasma, and the gas in the plasma state is supplied and dispersed into processing space 96 via multiple gas supply paths 112b. Then, the gas in the plasma state is supplied to substrate 1 on chuck table 104, and a predetermined plasma processing is performed on substrate 1.

[0091] Next, a substrate processing method according to this embodiment, which is carried out using the apparatus described above, will be described. In the substrate processing method according to this embodiment, holes are formed on the back surface 1b of the substrate 1, which has a pattern 7 on its front surface 1a, along with the pattern 7. In particular, a mask having openings formed along the pattern 7 on the back surface 1b of the substrate 1 is disposed, and the substrate 1 is etched from the back surface 1b through the openings of the mask, forming holes in predetermined positions of the substrate 1. Each step will be described in detail below.

[0092] First, a coating step S10 is performed to coat the back surface 1b side of the substrate 1 with a protective film 11 (see FIG. 2(B)) which is a mask material. FIG. 3 includes a cross-sectional view showing the substrate 1 when the coating step S10 is performed.

[0093] In the coating step S10, the protective film 11 may be formed on the substrate 1 using the above-mentioned film forming apparatus 2. Specifically, the substrate 1 is first placed on the spinner table 8 so that the back surface 1b side is exposed upward and the front surface 1a side faces the holding surface 8a. In this state, when the suction force (negative pressure) of the suction source is applied to the holding surface 8a, the substrate 1 is sucked and held by the spinner table 8.

[0094] Next, the supply nozzle 24 is rotated and positioned directly above the center of the substrate 1. Then, while the spinner table 8 is rotated by the motor 14, the liquid protective film material 18 is dropped from the supply nozzle 24 and supplied to the rear surface 1b of the substrate 1. As a result, the protective film material 18 supplied to the center of the substrate 1 spreads radially toward the outer edge side of the substrate 1 due to centrifugal force, covering the entire rear surface 1b of the substrate 1. The thickness of the protective film material 18 covering the substrate 1 can be controlled by adjusting the rotation speed of the spinner table 8 and the supply amount of the protective film material 18.

[0095] Thereafter, the supply of protective film material 18 from supply nozzle 24 to substrate 1 is stopped, and rotation of spinner table 8 is maintained for a certain period of time. This causes protective film material 18 to dry, forming protective film 11 that covers rear surface 1b of substrate 1. After protective film material 18 has dried, a baking process or the like may be performed to harden protective film material 18, if necessary.

[0096] As described above, in the covering step S10, the protective film 11 is formed on the substrate 1, and the rear surface 1b of the substrate 1 is covered with the protective film 11. Fig. 2(B) is a cross-sectional view that shows a schematic diagram of the substrate 1 whose rear surface 1b side is covered with the protective film 11. However, the material and the formation method of the protective film 11 can be changed as appropriate.

[0097] Next, in order to form a mask by forming an opening in the protective film 11 at a position corresponding to the pattern 7, an alignment step S20 is performed in which the pattern 7 provided on the front surface 1a side of the substrate 1 is imaged to detect the position of the pattern 7. Thereafter, a mask formation step S30 is performed in which the protective film 11 is removed at a position corresponding to the pattern 7 to form an opening in the protective film 11, thereby forming a mask. The alignment step S20 and the mask formation step S30 are performed by a laser processing device 32 shown in FIG. 4 etc.

[0098] First, the substrate 1 is placed on the chuck table 56 so that the back surface 1b side is exposed upward and the front surface 1a side faces the upper surface of the holding member 56a. In this state, when the suction force (negative pressure) of the suction source is applied to the upper surface of the holding member 56a, the substrate 1 is sucked and held by the chuck table 56.

[0099] Next, the X-axis direction moving mechanism 54 and the Y-axis direction moving mechanism 44 are operated to position the chuck table 56 above the lower imaging unit 64. Then, the lower surface (front surface 1a) of the substrate 1 is imaged by the lower imaging unit 64 through the holding member 56a to obtain an image. Then, the pattern 7 shown in the image is detected, and the position of the pattern 7 is identified. The area overlapping with this pattern 7 is the position of the substrate 1 to be processed, and by identifying the position of the pattern 7, the position of the substrate 1 to be processed is identified.

[0100] It is preferable that the position of the pattern 7 based on the captured image is specified mainly by the function of the controller 80. For example, the controller 80 performs a predetermined image processing on the captured image and specifies the position of the outer edge of the pattern 7, the center position (center of gravity position) of the pattern 7, and the like, thereby specifying the position of the pattern 7.

[0101] Also, the lower imaging unit 64 may be used to image the entire surface 1a of the substrate 1 and identify the positions of all the patterns 7. Alternatively, the position of the substrate 1 to be processed may be identified based on the positions of some of the patterns 7 on the surface 1a of the substrate 1 and information on the arrangement of the patterns 7 on the surface 1a of the substrate 1.

[0102] The position of the pattern 7 may be specified by using the upper imaging unit 74. In this case, the chuck table 56 that suction-holds the substrate 1 is positioned below the upper imaging unit 74. Then, the upper imaging unit 74 images the front surface 1a side through the substrate 1 from the back surface 1b side to obtain an image. Then, the position to be processed is specified based on the position of the pattern 7 shown in the obtained image.

[0103] When the upper imaging unit 74 images the front surface 1a side through the substrate 1, a camera equipped with a sensor (image pickup element) capable of detecting light (e.g., infrared light) passing through the substrate 1 is used for the upper imaging unit 74. Then, in the alignment step S20, it is preferable to image the pattern 7 provided on the front surface 1a side of the substrate 1 from the back surface 1b side using light of a wavelength passing through the substrate 1 as illumination light.

[0104] Here, the position where the opening is to be formed in the protective film 11 is specified by the alignment step S20. For example, when it is planned to etch the substrate 1 to form a hole in a region overlapping with the pattern 7, the protective film 11 is irradiated with the laser beam L as described below so that an opening is formed in the region of the protective film 11 overlapping with the pattern 7 based on the position of the pattern 7.

[0105] However, the position where the hole in the substrate 1 is formed and the position where the opening in the protective film 11 is formed are not limited to this. For example, the position where the hole in the substrate 1 is planned to be formed does not have to completely overlap with the pattern 7, and a hole larger or smaller than the pattern 7 in a plan view may be planned to be formed, or a hole may be planned to be formed at a position shifted from the pattern 7. The planar shape of the pattern 7 and the planar shape of the opening formed in the protective film 11 do not necessarily match.

[0106] In either case, in alignment step S20, the position where the opening in protective film 11 is to be formed, i.e., the position where laser processing of protective film 11 is performed, is identified based on the position of pattern 7. In this manner, the position of pattern 7 is identified in alignment step S20 in order to form holes in substrate 1 at positions corresponding to pattern 7, and to form openings in protective film 11 at positions corresponding to pattern 7. This makes it possible to form holes in substrate 1 that correspond to pattern 7.

[0107] In the laser processing device 32, next, a mask forming step S30 is performed. In the mask forming step S30, the substrate 1 is moved below the head portion 72 of the laser irradiation unit 70. Then, while changing the orientation of the mirror 86 to switch the focusing position of the laser beam L, the laser beam L is focused at a predetermined position of the protective film 11, and the protective film 11 is laser processed. In other words, the laser beam L is scanned by the scanning unit at each predetermined processing location of the protective film 11.

[0108] 5 is a cross-sectional view showing a schematic diagram of the substrate 1 at the start of the mask formation step S30. In the mask formation step S30, the mask is formed by removing the protective film 11 at a position corresponding to the pattern 7 to form an opening in the protective film 11. In particular, the laser irradiation unit 70 is used to focus the laser beam L at a position where the opening in the protective film 11 is to be formed, and the protective film 11 at that position is removed. An example of processing conditions for performing the laser processing is shown below.

[0109] Laser beam wavelength: 365nm Average output: 0.7W Pulse repetition frequency: 200kHz Scanning speed of the focal point: 200mm / s

[0110] 6(A) is a cross-sectional view showing a schematic view of the substrate 1 at the completion of the mask formation step S30. When the protective film 11 is removed at a position corresponding to the pattern 7 to form an opening 15, a mask 13 is formed on the back surface 1b side of the substrate 1. Here, the mask 13 has a function of protecting an area that is not to be etched from an etchant when etching is performed on the substrate 1 as described later. In other words, the mask 13 is a patterned resist film.

[0111] In the substrate processing method according to this embodiment, next, an etching step S40 is performed in which the substrate 1 is etched through the mask 13 to form holes along the pattern 7 on the rear surface 1b side of the substrate 1. Here, the holes along the pattern 7 refer to holes whose positions and shapes are determined based on the position, shape, etc. of the pattern 7. The etching step S40 is performed using a plasma processing apparatus 92 shown in FIG.

[0112] Fig. 13 is a partial cross-sectional front view showing the substrate 1 in the etching step S40. The pattern 7 of the substrate 1 and the opening 15 of the mask 13 are omitted in Fig. 13. In the etching step S40, an etchant is supplied to the rear surface 1b side of the substrate 1 by the plasma processing device 92, and the substrate 1 is processed from the rear surface 1b side, and holes are formed in the substrate 1.

[0113] Specifically, first, the substrate 1 is held by the chuck table 104 so that the back surface 1b side of the substrate 1 on which the mask 13 is formed is exposed upward and the opposite front surface 1a side faces the holding surface 104a. Further, an etching gas is supplied to the gas diffusion space 112a (see FIG. 12) of the gas ejection head 112, and high frequency power is applied to the gas ejection head 112.

[0114] As a result, the gas in the gas diffusion space 112a is turned into plasma, and plasma-state gas 124 (etchant gas) containing ions and radicals is generated. Then, the plasma-state gas 124 is supplied to the rear surface 1b side of the substrate 1, whereby the substrate 1 exposed through the openings 15 of the mask 13 is etched.

[0115] For example, when the substrate 1 is a silicon wafer, a fluorine-based gas (CF4, SF6, etc.) is supplied from the gas supply source 122a, and an inert gas (He, Ar, etc.) is supplied from the gas supply source 122b, and these gases are mixed in the gas diffusion space 112a.

[0116] Then, high frequency power is applied to the gas ejection head 112. This causes the gas supplied to the gas diffusion space 112a to turn into plasma, and the gas 124 in the plasma state is supplied to the front surface 1a side of the substrate 1. As a result, the gas 124 enters the opening 15 of the mask 13 and acts on the back surface 1b side of the substrate 1 exposed inside the opening 15. This causes plasma etching to be performed on the region of the substrate 1 corresponding to the pattern 7, and a hole is formed. FIG. 6(B) is a cross-sectional view showing a schematic diagram of the substrate 1 in which a hole 17 along the pattern 7 has been formed.

[0117] Then, as the supply of gas 124 continues, the plasma etching progresses and the hole deepens, until the hole reaches pattern 7 on the front surface 1a side of substrate 1. In the etching step S40, the hole may be formed by the Bosch process. In this case, the process of etching substrate 1 by sequentially performing a protective film formation step, an anisotropic etching step, and an isotropic etching step is repeated, so that hole 17 reaches front surface 1a of substrate 1.

[0118] In the protective film forming step, the inner surface of the hole is covered with a protective film by supplying plasmatized gas to the back surface 1b side (mask 13 side) of the substrate 1. Specifically, gas for forming the protective film is supplied to the gas diffusion space 112a (see FIG. 12) of the gas ejection head 112, and high frequency power is applied to the gas ejection head 112. As a result, the gas in a plasma state is supplied to the back surface 1b side of the substrate 1.

[0119] When gas is supplied to the substrate 1, ions and radicals contained in the gas enter the holes and are deposited on the inner walls of the holes as well. As a result, a protective film is formed on the inner walls of the holes, and the holes are covered with the protective film.

[0120] For example, in the gas diffusion space 112a (see FIG. 12), a gas containing C4F8 supplied from a gas supply source 122a and an Ar gas supplied from a gas supply source 122b are mixed and turned into plasma. Then, CF radicals contained in the gas are deposited on the inner wall of the hole, and an insulating protective film containing fluorocarbon is formed on the inner wall of the hole. For example, the gas supply time is set to 6 seconds or more and 8 seconds or less, and a protective film having a thickness of 10 nm or less is formed.

[0121] Next, an anisotropic etching step is performed. In the anisotropic etching step, a plasma gas is supplied to the back surface 1b side (mask 13 side) of the substrate 1, whereby the protective film covering the bottom of the hole is anisotropically plasma etched, and the protective film is removed. Specifically, an etching gas is supplied to the gas diffusion space 112a (see FIG. 12) of the gas ejection head 112. For example, a fluorine-based gas (CF4, SF6, etc.) supplied from the gas supply source 122a and an inert gas (He, Ar, etc.) supplied from the gas supply source 122b are mixed in the gas diffusion space 112a.

[0122] Then, high frequency power is applied to the electrode 106 and the gas ejection head 112 (see FIG. 12). This causes the gas in the gas diffusion space 112a to be converted into plasma and accelerated toward the chuck table 104, subjecting the protective film to anisotropic plasma etching. When the anisotropic plasma etching is continued for a certain period of time (e.g., about 3 seconds), the portion of the protective film covering the bottom of the hole is removed, exposing the bottom of the hole.

[0123] Next, an isotropic etching step is performed. In the isotropic etching step, a plasma gas is supplied to the back surface 1b side (mask 13 side) of the substrate 1, so that the bottom of the hole is isotropically plasma etched. Specifically, an etching gas is supplied to the gas diffusion space 112a (see FIG. 12) of the gas ejection head 112. For example, a fluorine-based gas (CF4, SF6, etc.) supplied from the gas supply source 122a and an inert gas (He, Ar, etc.) supplied from the gas supply source 122b are mixed in the gas diffusion space 112a.

[0124] Then, high-frequency power is applied to the gas ejection head 112 (see FIG. 12). This causes the gas supplied to the gas diffusion space 112a to become plasma, and the gas in the plasma state is supplied to the rear surface 1b side of the substrate 1 for a certain period of time (for example, 5 seconds or more and 7 seconds or less). Note that in the isotropic etching step, high-frequency power is not applied to the electrode 106 (see FIG. 12). Therefore, isotropic plasma etching is performed on the substrate 1. As a result, the bottom of the hole and its vicinity are removed, making the hole deeper.

[0125] Thereafter, the above-mentioned protective film forming step, anisotropic etching step, and isotropic etching step are repeated until the hole reaches the pattern 7 on the front surface 1a side of the substrate 1. When the hole reaches the pattern 7 on the front surface 1a side of the substrate 1, the etching step S40 is completed.

[0126] When the etching step S40 is completed, the mask 13 is removed. For example, the mask 13 is subjected to an ashing process, thereby removing the mask from the substrate 1. When the mask 13 is made of a water-soluble resin, the mask 13 can be easily removed by supplying pure water or the like to the mask 13.

[0127] In the substrate processing method described above, when the protective film 11 is partially removed at a predetermined position to form the etching mask 13, it is necessary to irradiate the protective film 11 with the laser beam L with high accuracy. However, while the protective film 11 is irradiated with the laser beam L, the state of the optical system may change due to an increase in the environmental temperature, etc., causing deviations in the position and size of the irradiated region of the laser beam, thereby decreasing the irradiation accuracy of the laser beam L.

[0128] When the protective film 11 is irradiated with a laser beam L with reduced irradiation accuracy, the position and size of the area of ​​the substrate 1 exposed from the mask 13 will not match the area planned for etching, resulting in low quality mask 13. As a result, etching will not be performed as planned, leading to poor characteristics of the device 5 that is finally formed.

[0129] Therefore, in the substrate processing method according to the present embodiment, when forming the mask 13 by forming the opening 15 in the protective film 11, the protective film 11 is test-processed, the result of the test processing is evaluated to determine a correction amount, and the processing position of the protective film 11 is corrected based on the correction amount to form the opening 15. That is, in the mask formation step S30, the test processing is performed, and the mask 13 is formed by actually processing the protective film 11 using the result of the test processing.

[0130] Each step of the mask formation step S30 in the substrate processing method according to this embodiment will be described in detail below. Fig. 7(A) includes a plan view showing a schematic view of the back surface 1b side of the substrate 1 at the start of the mask formation step S30. Fig. 7(B) includes a cross-sectional view showing a schematic view of the substrate 1 at the start of the mask formation step S30.

[0131] Fig. 7(B) shows one pattern 7 formed on the front surface 1a side of the substrate 1 and its surrounding area. Fig. 7(B) omits layer 9, which is a structure other than pattern 7 on the front surface 1a side of the substrate 1. As shown in Fig. 7(B), at this point in time, openings 15 and the like have not been formed in protective film 11 covering the back surface 1b side of the substrate 1.

[0132] 15B is a flow chart showing the flow of each step of the mask formation step S30. Each step of the mask formation step S30 will be described in order. First, in the mask formation step S30, the protective film 11 is removed from an area corresponding to the pattern 7 on the front surface 1a of the substrate 1, and a test processing step S31 is performed to form a test pattern on the protective film 11.

[0133] The position of pattern 7 is specified by performing alignment step S20, and at this point, the region where opening 15 is to be formed in mask formation step S30, i.e., the position where protective film 11 is to be removed, is specified. Below, an example will be described in which protective film 11 is removed in a region that overlaps pattern 7 exactly to form opening 15 in mask 13.

[0134] Fig. 7(A) is a plan view showing a schematic view of the rear surface 1b side of the substrate 1, and Fig. 7(A) shows an area 19 where the opening 15 is to be formed. However, the area 19 is not limited to overlapping the pattern 7 exactly. In Fig. 7(A), the area 19 is represented by a dashed line. Position A in Fig. 7(A) corresponds to position A in Fig. 7(B), and position A' in Fig. 7(A) corresponds to position A' in Fig. 7(B).

[0135] In the test processing step S31, for example, the protective film 11 is removed in the region 19 where the protective film 11 is scheduled to be removed or in a region inside the region 19, and a test pattern 21 is formed on the protective film 11. The test pattern 21 may be formed by the laser processing device 32 under the same conditions as those for forming the opening 15 in the protective film 11 as described above, except that the irradiation position of the laser beam L is different. That is, in the test processing step S31, the protective film 11 is irradiated with the laser beam L using the laser irradiation unit 70 to remove the protective film 11.

[0136] Figure 8(A) is a plan view showing a schematic view of the back surface 1b side of a substrate 1 on which a test pattern 21 is formed on a protective film 11 in an area inside region 19, and Figure 8(B) is a cross-sectional view showing a schematic view of the substrate 1 on which a test pattern 21 is formed.

[0137] In particular, in the test processing step S31, it is preferable to remove the protective film 11 only from a part or the entirety of the region 19 corresponding to the pattern 7 on the front surface 1a side of the substrate 1, and form the test pattern 21 on the protective film 11. In this case, the formation of the test pattern 21 does not affect the quality of the mask 13, since the test pattern 21 is removed from the protective film 11 when the main processing step S35 is performed as described below.

[0138] Explaining from another perspective, when the test pattern 21 is formed inside the region 19 of the protective film 11, the test pattern 21 can be formed by utilizing the protective film 11 that is lost as the opening 15 when the mask 13 is finally formed, as described below. Therefore, the protective film 11 in the region required for the mask 13 is not lost in the formation of the test pattern 21. As described below, the formed test pattern 21 can be used to evaluate the irradiation accuracy of the laser beam L.

[0139] After the test processing step S31, a test pattern position detection step S32 is performed in which the test pattern 21 formed on the protective film 11 in the test processing step S31 is imaged and the position of the test pattern 21 is detected.

[0140] The test pattern 21 formed on the protective film 11 is imaged by the lower imaging unit 64 of the laser processing device 32. When the lower imaging unit 64 images the substrate 1 from the lower surface (front surface 1a) side, the chuck table 56 is moved above the lower imaging unit 64 as shown in Fig. 9. Then, the back surface 1b side is imaged through the substrate 1 from the front surface 1a side to obtain an image showing the test pattern 21. In this case, an imaging element capable of receiving light of a wavelength that passes through the substrate 1 is used for the imaging camera provided in the lower imaging unit 64.

[0141] However, when imaging is performed by the lower imaging unit 64, there are cases where the test pattern 21 is hidden by the pattern 7 and does not appear in the captured image. Therefore, imaging of the test pattern 21 formed on the protective film 11 may be performed by the upper imaging unit 74 of the laser processing device 32. Fig. 10 is a cross-sectional view that shows a schematic view of the substrate 1 imaged from the top surface (rear surface 1b) side by the upper imaging unit 74. When the substrate 1 is imaged by the upper imaging unit 74, the test pattern 21 formed on the protective film 11 is imaged.

[0142] Fig. 11(A) is a plan view showing a schematic example of a captured image showing the back surface 1b side of the substrate 1. The captured image shown in Fig. 11(A) is, for example, an image obtained when the substrate 1 is imaged by the upper imaging unit 74. Fig. 11(A) shows a test pattern 21a formed on the protective film 11. Then, in a test pattern position detection step S32, the position of the test pattern 21a is identified from the captured image showing the test pattern 21a.

[0143] For example, the controller 80 of the laser processing device 32 detects the test pattern 21a from the captured image and specifies its position. More specifically, among the pixels constituting the captured image, a region of pixels belonging to the test pattern 21a is detected, and the position of the center of gravity of a plane figure having the same shape and size as the region is specified as the position of the test pattern 21a. However, the method of specifying the position of the test pattern 21a is not limited to this. The specified position of the test pattern 21a may be recorded in the storage device 82.

[0144] In the mask formation step S30, a pattern position detection step S33 is performed in which a pattern provided on the front surface 1a side of the substrate 1 is imaged and the position of the pattern is detected. The pattern position detection step S33 is performed in the same manner as the test pattern position detection step S32. That is, the pattern position detection step S33 is performed, for example, by the upper imaging unit 74 or the lower imaging unit 64 of the laser processing device 32. Then, an image showing the pattern 7a of the substrate 1 is obtained.

[0145] 9, when the lower imaging unit 64 images the substrate 1 from the lower surface (surface 1a) side, the chuck table 56 is moved above the lower imaging unit 64. Then, the surface 1a side of the substrate 1 is imaged, and an image showing the pattern 7a is obtained.

[0146] When the upper imaging unit 74 images the substrate 1 from the top surface (rear surface 1b) side, the chuck table 56 is moved below the upper imaging unit 74 as shown in Fig. 10. Then, the front surface 1a side is imaged through the substrate 1 from the rear surface 1b side to obtain an image showing the pattern 7a. In this case, an imaging element capable of receiving light of a wavelength that passes through the substrate 1 is used for the imaging camera provided in the upper imaging unit 74. Then, in the pattern position detection step S33, it is preferable to image the pattern 7a provided on the front surface 1a side of the substrate 1 from the rear surface 1b side using light of a wavelength that passes through the substrate 1 as illumination light.

[0147] Fig. 11(B) is a plan view showing an example of a captured image showing the front surface 1a side of the substrate 1. The captured image shown in Fig. 11(B) is, for example, an image obtained when the substrate 1 is imaged by the lower imaging unit 64. The captured image shown in Fig. 11(B) shows a pattern 7a. Then, in a pattern position detection step S33, the position of the pattern 7a is identified from the captured image showing the pattern 7a.

[0148] For example, the controller 80 of the laser processing device 32 detects the pattern 7a from the captured image and identifies its position. The position of the pattern 7a is identified in the same manner as the method for identifying the position of the test pattern 21a described above. The identified position of the pattern 7a may be recorded in the storage device 82.

[0149] Here, the test pattern 21a whose position is detected in the test pattern position detection step S32 may be formed in the protective film 11 at a position corresponding to the pattern 7a whose position is detected in the pattern position detection step S33. In other words, the test pattern 21a is formed in the protective film 11 in a region 19 where the opening 15 of the mask 13 used to form the hole 17 in the substrate 1 along the pattern 7a whose position is detected in the pattern position detection step S33 is to be formed.

[0150] Furthermore, the test patterns 21a do not need to be formed in all of the regions 19 of the protective film 11 where the openings 15 of the mask 13 are formed. It is sufficient that the test patterns 21a are formed in the protective film 11 in a number and positions that are sufficient to evaluate the irradiation accuracy of the laser beam L. Furthermore, in the test pattern position detection step S32, it is not necessary to detect the positions of all of the test patterns 21a formed in the protective film 11. It is sufficient that the positions of the test patterns 21a are detected in a number that is sufficient to evaluate the irradiation accuracy of the laser beam L.

[0151] Further, the test pattern position detection step S32 and the pattern position detection step S33 may be performed either first or simultaneously. For example, immediately after acquiring an image showing the pattern 7a using the upper imaging unit 74 or the lower imaging unit 64, an image showing the test pattern 21a overlapping the pattern 7a is acquired without moving the chuck table 56.

[0152] In this case, after the first imaging, the second imaging can be performed simply by adjusting the focus by raising and lowering the upper imaging unit 74 or the lower imaging unit 64 along the Z-axis direction, etc. Therefore, the area captured in the two captured images is the same, and the irradiation accuracy of the laser beam L can be intuitively and easily evaluated by directly comparing the two images.

[0153] Furthermore, when the test pattern position detection step S32 and the pattern position detection step S33 are performed simultaneously in this manner, the movement of the chuck table 56 is minimized, so that the time required for the mask formation step S30 may be relatively short.

[0154] If a captured image showing the pattern 7 has been acquired in the alignment step S20, the captured image acquired in the alignment step S20 may be used in the pattern position detection step S33 to detect the position of the pattern 7. In this case, the detection of the position of the pattern 7 may be performed immediately after the captured image showing the pattern 7 has been acquired in the alignment step S20.

[0155] In other words, the pattern position detection step S33 may be performed simultaneously with the alignment step S20. In other words, some steps of the mask formation step S30 may be performed simultaneously with the alignment step S20.

[0156] After the test pattern position detection step S32 and the pattern position detection step S33 are performed, a correction amount calculation step S34 is performed. In the correction amount calculation step S34, the amount of deviation between the position of the test pattern 21 detected in the test pattern position detection step S32 and the position of the pattern 7 detected in the pattern position detection step S33 is calculated as a test deviation amount. Then, the correction amount is calculated based on the test deviation amount.

[0157] Fig. 11(C) is a plan view showing a schematic positional relationship between test pattern 21a formed on protective film 11 and pattern 7a provided on substrate 1. In particular, in plan view 27a shown in Fig. 11(C), the outer edge of test pattern 21a is represented by a dashed line, and the outer edge of pattern 7a is represented by a solid line. In plan view 27a, center (centre of gravity) 21b of test pattern 21a and center (centre of gravity) 7b of pattern 7a are each represented by a point.

[0158] For example, in test pattern position detection step S32, the position of center 21b of test pattern 21a is detected, and in pattern position detection step S33, the position of center 7b of pattern 7a is detected. Then, the test deviation amount is calculated from the relative positions of center 21b of test pattern 21a and center 7b of pattern 7a. For example, the test deviation amount and deviation direction are calculated from the difference in coordinates between center 21b and center 7b on the XY plane. In Fig. 11(C), the deviation 23 between the two is represented by an arrow.

[0159] Next, a correction amount is calculated based on the test deviation amount. This correction amount is used to correct the irradiation conditions of the laser beam L when the laser beam L is irradiated onto the protective film 11 in the main processing step S35 described later. For example, if the test pattern 21a is formed on the protective film 11 so that the center 21b of the test pattern 21a is expected to overlap with the center 7b of the pattern 7a, the amount of deviation 23 (test deviation amount) shown in FIG. 11(C) becomes the correction amount as it is.

[0160] However, the calculated correction amount is not limited to this. For example, in the test processing step S31, the center 21b of the test pattern 21a may not be formed on the protective film 11 so as to overlap with the center 7b of the pattern 7a. In other words, the test pattern 21a may be formed on the protective film 11 so as to shift the centers 21b and 7b of the pattern 7a.

[0161] In this case, the amount of correction can be determined by evaluating the deviation between the position where the test pattern 21a is planned to be formed and the position where the test pattern 21a is actually formed. In this case, the deviation between the position where the test pattern 21a is planned to be formed and the position where the test pattern 21a is actually formed can be evaluated by defining the positional relationship between the test pattern 21a and the pattern 7a.

[0162] For example, the planned positional relationship between the position where the test pattern 21a is planned to be formed and the position of the pattern 7a is compared with the actual positional relationship between the position where the test pattern 21a is actually formed and the position of the pattern 7a. If these two positional relationships match, that is, if the test deviation amount is the planned amount, it is found that there is no need to correct the irradiation conditions of the laser beam L, and the correction amount can be calculated as zero. If these two positional relationships do not match, the correction amount can be calculated from these deviations.

[0163] In any case, in the correction amount calculation step S34, the amount of deviation between the position of the test pattern 21a and the position of the pattern 7a is calculated as a test deviation amount, and the correction amount is calculated based on the test deviation amount. The calculation of the correction amount may be performed, for example, by a function of the controller (control unit) 80 of the laser processing device 32. In addition, the calculated correction amount, etc. may be registered in the storage device (storage unit) 82 of the controller 80.

[0164] Here, the correction amount is the amount of correction related to the irradiation position among the irradiation conditions of the laser beam L. However, the correction amount is not limited to this, and may be a correction amount related to an irradiation condition other than the irradiation position. In addition, when the calculated correction amount is the amount of correction related to the irradiation position, the direction of correction may be calculated together.

[0165] In the mask formation step S30, the position where the protective film 11 is removed is corrected based on the correction amount calculated in the correction amount calculation step S34, and then the main processing step S35 is performed to remove the protective film 11 and form an opening 15 in the protective film 11 to form a mask 13. Fig. 6(B) is a cross-sectional view that shows a schematic view of the main processing step S35 in the mask formation step S30.

[0166] In the main processing step S35, the laser irradiation unit 70 of the laser processing device 32 irradiates the protective film 11 with the laser beam L so that the openings 15 are formed over the entire area 19 (see FIGS. 7(A) and 7(B)) where the openings 15 are scheduled to be formed. At this time, the irradiation conditions during irradiation of the laser beam L performed in the test processing step S31 are corrected by the calculated correction amount to derive new irradiation conditions, and the protective film 11 is irradiated with the laser beam L under the derived new irradiation conditions. For example, in the main processing step S35, the scanning unit (galvano scanner) is controlled by referring to the calculated correction amount.

[0167] When the irradiation position of the laser beam L among the irradiation conditions is corrected by the calculated correction amount, and the laser beam L is irradiated onto the protective film 11 under the corrected irradiation conditions, the opening 15 is formed with high precision in the region 19 where the opening 15 is to be formed. That is, a high-quality mask 13 is formed. In particular, according to the substrate processing method of this embodiment, the protective film 11 itself on which the mask is to be formed can be used to perform test processing for condition correction immediately before the mask is formed, and therefore the condition correction can be performed with extremely high effectiveness.

[0168] Then, when test pattern 21 fits into area 19 where opening 15 is to be formed, protective film 11 is removed around test pattern 21, and test pattern 21 disappears after being taken into opening 15. Therefore, test pattern 21 does not remain on mask 13, and test pattern 21 does not affect processing of substrate 1 in etching step S40.

[0169] Furthermore, in the substrate processing method according to this embodiment, after the etching step S40 is performed, the accuracy of the processing may be evaluated by observing the hole 17 (see FIG. 6(B)) formed in the substrate 1. Then, the quality of the processing may be judged by evaluating the deviation between the position where the hole 17 is planned to be formed in the substrate 1 and the position where the hole 17 is actually formed in the etching step S40. Hereinafter, the substrate processing method according to this embodiment will be described, focusing on the configuration related to the judgment of the quality of the processing.

[0170] After the etching step S40, a hole formation position detection step S50 is performed in which the hole 17 formed in the rear surface 1b of the substrate 1 is imaged to detect the position of the hole 17. The hole formation position detection step S50 is performed, for example, by utilizing the upper imaging unit 74 or the lower imaging unit 64, similarly to the alignment step S20, the test pattern position detection step S32, and the pattern position detection step S33. In this case, after the etching step S40 is completed, the substrate 1 is returned to the laser processing device 32.

[0171] However, the substrate processing method according to the present embodiment is not limited to this, and the hole formation position detection step S50 may be performed by a device equipped with an imaging unit and different from the laser processing device 32. Below, an example will be described in which the subsequent steps are performed by the laser processing device 32.

[0172] In the hole formation position detection step S50, the substrate 1 is suction-held by the chuck table 56. Then, the chuck table 56 is positioned below the upper imaging unit 74 or above the lower imaging unit 64, and an image of the substrate 1 is captured. Then, the position of the hole 17 is identified based on the captured image.

[0173] For example, the controller 80 of the laser processing device 32 detects the hole 17 from the captured image and identifies its position. More specifically, among the pixels constituting the captured image, a region of pixels belonging to the hole 17 is detected, and the position of the center of gravity of a planar figure having the same shape and size as the region is identified as the position of the hole 17. However, the method of identifying the position of the hole 17 is not limited to this. The identified position of the hole 17 may be recorded in the storage device 82.

[0174] In particular, in the hole formation position detection step S50, it is preferable to capture an image in the vicinity of the pattern 7 whose position has been detected in the pattern position detection step S33. This is because the position of the hole 17 identified from the captured image obtained in the hole formation position detection step S50 is compared with the position of the pattern 7 in the vicinity thereof to determine whether the formation position of the hole 17 (machining deviation) is acceptable or not.

[0175] However, the substrate processing method according to this embodiment is not limited to this, and in the hole formation position detection step S50, imaging may not be performed in the vicinity of the pattern 7 whose position has been detected in the pattern position detection step S33. In this case, in order to determine whether the position of the hole 17 identified from the captured image is acceptable or not, an additional pattern position detection step S33 may be performed in which the pattern 7 formed on the substrate 1 in the vicinity of the hole 17 is imaged and its position is identified.

[0176] In other words, a separate pattern position detection step S33 may be performed before the processing deviation amount calculation step S60, in addition to the pattern position detection step S33 in the mask formation step S30. For example, the pattern position detection step S33 may be performed simultaneously with, immediately before, or immediately after the hole formation position detection step S50.

[0177] In this case, in the hole formation position detection step S50, the hole 17 to be the object of position detection can be selected regardless of the pattern 7 whose position was detected in the mask formation step S30, so that an operation of searching for a specific pattern 7 (hole 17) is not necessary, and the process is simplified. In other words, as long as the hole 17 and the pattern 7 to be the object of position detection are a pair that are closest to each other, the hole 17 and the pattern 7 to be the object of position detection can be arbitrarily selected.

[0178] Next, a processing deviation amount calculation step S60 is performed to calculate the amount of deviation between the position of the pattern 7 detected in the pattern position detection step S33 and the position of the hole 17 detected in the hole formation position detection step S50 as a processing deviation amount.

[0179] Fig. 14(A) is a plan view showing a schematic positional relationship between a hole 17a formed in a substrate 1 and a pattern 7c provided on the substrate 1. Fig. 14(B) is a cross-sectional view showing a schematic positional relationship of the substrate 1 with the hole 17a formed therein. In particular, in the plan view 27b shown in Fig. 14(A), the outer edge of the hole 17a and the outer edge of the pattern 7c are represented by solid lines. In addition, in the plan view 27b, the center (center of gravity) 17b of the hole 17a and the center (center of gravity) 7d of the pattern 7c are each represented by a point.

[0180] For example, in the machining deviation amount calculation step S60, the position of the center 17b of the hole 17a is detected, and in the pattern position detection step S33, the position of the center 7d of the pattern 7c is detected. Then, the machining deviation amount is calculated from the relative positions of the center 17b of the hole 17a and the center 7d of the pattern 7c. For example, the test deviation amount and the deviation direction are calculated from the difference in coordinates between the center 21b and the center 7b in the XY plane. In Fig. 14(A), the deviation 25 between the two is represented by an arrow.

[0181] In the substrate processing method according to the present embodiment, next, a pass / fail judgment step S70 is carried out to judge whether or not the processing misalignment amount calculated in the processing misalignment amount calculation step S60 falls within an allowable range. The pass / fail judgment step S70 may be realized, for example, by a function of the controller (control unit) 80 of the laser processing device 32. The allowable range of the processing misalignment amount, which serves as a criterion for judgment, may be registered in advance in the storage device 82 of the controller 80.

[0182] In the pass / fail determination step S70, the controller 80 compares the machining deviation amount calculated in the machining deviation amount calculation step S60 with the allowable range stored in the storage device 82. If the calculated machining deviation amount falls within the allowable range, it is determined that the machining was performed appropriately. On the other hand, if the calculated machining deviation amount does not fall within the allowable range, it is determined that some machining abnormality has occurred.

[0183] Possible causes of processing abnormalities include mistaking the substrate 1, an abnormality in the mask 13, inappropriate implementation of the etching step S40, etc. However, in the substrate processing method according to the present embodiment, test processing is performed in advance so that the mask 13 is created with high quality, and the processing conditions are corrected to create the mask 13, so the possibility of an abnormality in the mask 13 is relatively low.

[0184] In any case, since the process needs to be checked by a manager of the processing method of the substrate 1, if it is determined that a processing abnormality has occurred, the controller 80 performs a warning operation. For example, the controller 80 displays the details of the processing abnormality that has occurred on the touch panel display 76 of the laser processing device 32, and notifies the manager of the warning. However, the method of notifying the warning is not limited to this.

[0185] As described above, in the substrate processing method (mask forming method) according to this embodiment, a test pattern is formed by removing the protective film in an area corresponding to the pattern, and a correction amount is calculated based on the amount of misalignment between the test pattern and the pattern. The calculated correction amount can be used when forming an opening at a predetermined position in the protective film. As a result, a high-quality mask in which an opening is formed at a predetermined position with high accuracy is formed on the substrate.

[0186] The present invention is not limited to the above embodiment, and can be modified in various ways. For example, in the above embodiment, as shown in Fig. 15(A) and Fig. 15(B), the substrate 1 is processed in the steps from the coating step S10 to the pass / fail determination step S70. However, one aspect of the present invention is not limited to this.

[0187] In the method for processing the substrate 1 according to one embodiment of the present invention, the steps from the coating step S10 to the etching step S40 can be implemented as a method for forming a mask on the substrate 1. According to this method for forming a mask, the mask 13 can be formed by forming the opening 15 in the protective film 11 with reference to the result of the test processing, so that the mask 13 can be formed with high quality.

[0188] In addition, in one aspect of the present invention, the steps of pattern position detection step S33, hole formation position detection step S50, processing deviation amount calculation step S60, and pass / fail determination step S70 in the processing method for the substrate 1 can be implemented as a method for inspecting the processed substrate. According to this substrate inspection method, it is possible to easily determine whether the processing performed on the substrate 1 is good or bad, that is, whether the processing deviation amount falls within the allowable range, based on the positional relationship between the hole 17 formed in the substrate 1 and the pattern 7 formed on the front surface 1a of the substrate 1.

[0189] Furthermore, for example, in the above embodiment, a case has been described where the laser processing device 32 is used in the mask formation step S30, but the substrate processing method (mask formation method) according to one aspect of the present invention is not limited to this.

[0190] For example, in the mask formation step S30, the protective film 11 may be partially removed by a cutting device (not shown) equipped with a cutting blade having an annular grinding wheel portion to form the opening 15. In addition, the test pattern 21 may also be formed in the protective film 11 by partially cutting the protective film 11.

[0191] Even in this case, by forming test pattern 21 on protective film 11 with a cutting blade, calculating the amount of correction based on the position where test pattern 21 is formed, and performing the main processing with reference to the amount of correction, a high-quality mask 13 in which openings 15 are formed with high accuracy can be obtained. Then, by using high-quality mask 13, substrate 1 can be processed (etched) with high quality.

[0192] The structures, methods, and the like according to the above-described embodiments can be modified as appropriate without departing from the scope of the object of the present invention. [Explanation of symbols]

[0193] 1 Board 1a surface 1b back side 3 Street 5 Devices Patterns 7, 7a, 7c 7b,7d center 9 layers 11 Protective film 13. Mask 15 Aperture 17,17a hole 17b center 19 areas 21,21a Test Pattern 21b center 23,25 Shift 27a,27b Plan view 2 Film deposition equipment 4 Cover 4a,4b opening 6 Processing Space 8 Spinner Table 8a Holding surface 10 Rotation axis 12 Rotary joint 14 Motor 18 Protective film material 20 Protective film supply unit 22 Arm 22c Gas supply line 24 Supply Nozzle 26 Motor 28 Protective film material supply source 30 Drainage tube 32 Laser processing equipment 34 Foundation 36 Y-axis moving table 38 Y-axis guide rail 38a Y-axis linear scale 40 Screw shaft 42 Motor 44 Y-axis direction movement mechanism 46 X-axis moving table 46a bottom plate 46b side plate 46c Top 46d space 48 X-axis guide rail 48a X-axis linear scale 50 Screw shaft 52 Motor 54 X-axis direction movement mechanism 56 Chuck Table 56a Retaining member 56b Frame 58 Rotational drive source 58a Pulley 60 Belt 62 Lifting unit 63 Support Arm 64 Lower imaging unit Column 66 68 Casing 70 Laser irradiation unit 72 Head section 74 Upper imaging unit 76 Touch panel display 80 Controller 82 Storage device 84 Laser Oscillator 86 Mirror 88 fθ lens 92 Plasma processing equipment 94 Chamber 94a,94b,94c opening 96 Processing Space Gate 98 100 Piping 102 Exhaust system 104 Chuck table 104a Retaining surface 106 Electrode 108 Matching box 110 High frequency power supply 112 Gas ejection head 112a Gas diffusion space 112b, 112c, 112d Gas supply line 114 Bearings 116 Matching box 118 High frequency power supply 120a, 120b Piping 122a, 122b Gas supply source 124 Gas

Claims

1. A method for forming a mask, comprising the steps of: forming a mask on a back surface of a substrate having a pattern on a front surface thereof, the mask having an opening corresponding to the pattern, the method comprising the steps of: a coating step of coating the back side of the substrate with a protective film; an alignment step of imaging the pattern provided on the front surface side of the substrate to detect the position of the pattern; a mask forming step of forming the mask having the opening by removing the protective film at a position corresponding to the pattern; The mask forming step includes: a test processing step of removing the protective film in an area corresponding to the pattern on the front surface side of the substrate to form a test pattern on the protective film; a test pattern position detection step of imaging the test pattern formed on the protective film in the test processing step and detecting a position of the test pattern; a pattern position detection step of imaging the pattern provided on the front surface side of the substrate and detecting the position of the pattern; a correction amount calculation step of calculating a deviation amount between the position of the test pattern detected in the test pattern position detection step and the position of the pattern detected in the pattern position detection step as a test deviation amount, and calculating a correction amount based on the test deviation amount; a main processing step of correcting a position where the protective film is to be removed based on the correction amount calculated in the correction amount calculation step, thereby removing the protective film, and forming the opening in the protective film to form the mask.

2. In the alignment step and the pattern position detection step, 2. The method for forming a mask according to claim 1, wherein the pattern provided on the front side of the substrate is imaged from the back side thereof using light having a wavelength that is transmitted through the substrate as illumination light.

3. 3. The method for forming a mask according to claim 1, wherein in the test processing step, the protective film is removed only in a portion of the region corresponding to the pattern on the front surface side of the substrate, to form the test pattern on the protective film.

4. In the test processing step and the main processing step, removing the protective film by irradiating the protective film with a laser beam using a laser irradiation unit including a laser oscillator that emits a laser beam, an fθ lens that collects the laser beam, and a scanning unit that scans the laser beam emitted by the laser oscillator and collected by the fθ lens; 3. The method for forming a mask according to claim 1, wherein in the main processing step, the scanning unit is controlled by referring to the correction amount.

5. A method for processing a substrate, the method comprising the steps of: forming holes on a back surface of a substrate having a pattern on a front surface thereof, the holes being aligned with the pattern; a coating step of coating the back side of the substrate with a protective film; an alignment step of imaging the pattern provided on the front surface side of the substrate to detect the position of the pattern; a mask forming step of forming a mask by removing the protective film at a position corresponding to the pattern and forming an opening in the protective film; and etching the substrate through the mask to form holes on the back side of the substrate according to the pattern. The mask forming step includes: a test processing step of removing the protective film in an area corresponding to the pattern on the front surface side of the substrate and forming a test pattern on the protective film; a test pattern position detection step of imaging the test pattern formed on the protective film in the test processing step and detecting a position of the test pattern; a pattern position detection step of imaging the pattern provided on the front surface side of the substrate and detecting the position of the pattern; a correction amount calculation step of calculating a deviation amount between the position of the test pattern detected in the test pattern position detection step and the position of the pattern detected in the pattern position detection step as a test deviation amount, and calculating a correction amount based on the test deviation amount; a main processing step of correcting a position where the protective film is to be removed based on the correction amount calculated in the correction amount calculation step, thereby removing the protective film, and forming the opening in the protective film to form the mask.

6. a hole formation position detection step of imaging the hole formed on the back surface of the substrate after the etching step and detecting the position of the hole; a processing deviation amount calculation step of calculating a deviation amount between the position of the pattern detected in the pattern position detection step and the position of the hole detected in the hole formation position detection step as a processing deviation amount; 6. The method for processing a substrate according to claim 5, further comprising a pass / fail judging step of judging whether or not the amount of processing deviation calculated in the amount of processing deviation calculation step falls within an allowable range.

7. 1. A method for inspecting a substrate having a pattern on a front side and holes formed on a back side along the pattern, comprising: a pattern position detection step of imaging the pattern formed on the front surface side of the substrate and detecting the position of the pattern; a hole formation position detection step of imaging the hole formed on the back surface side of the substrate and detecting the position of the hole; a processing deviation amount calculation step of calculating a deviation amount between the position of the pattern detected in the pattern position detection step and the position of the hole detected in the hole formation position detection step as a processing deviation amount; and a pass / fail judging step of judging whether or not the processing deviation amount calculated in the processing deviation amount calculating step falls within an allowable range.

Citation Information

Patent Citations

  • Processing method for wafer

    JP2016018869A

  • Division method

    JP2016207737A