Adhesive tape

Incorporating fibrillated long fibers into the adhesive layer of natural rubber-based adhesives addresses the issue of holding power loss during processing, maintaining adhesion and durability.

JP2024156534APending Publication Date: 2024-11-06SEKISUI CHEMICAL CO LTD

Patent Information

Application Number
JP2023071079
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-24
Publication Date
2024-11-06

AI Technical Summary

Technical Problem

Adhesives containing natural rubber deteriorate during processing steps involving heat and shearing, leading to a significant decrease in holding power, particularly in hot-melt pressure-sensitive adhesives.

Method used

Incorporating fibrillated long fibers, such as acrylic modified polytetrafluoroethylene (PTFE) fibers, into the adhesive layer containing natural rubber to enhance molecular crosslinking and maintain holding power.

Benefits of technology

The adhesive tape maintains its holding power by preventing deterioration due to heat and shearing, ensuring effective adhesion and durability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024156534000001
    Figure 2024156534000001
Patent Text Reader

Abstract

To provide an adhesive tape with an adhesive layer that includes a rubber component containing natural rubber, capable of preventing a decrease in holding power during processing steps involving heat or shear.SOLUTION: An adhesive tape includes an adhesive layer that contains a rubber component containing natural rubber and fibrillated long fibers.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an adhesive tape having an adhesive layer containing natural rubber. [Background technology]

[0002] Since their appearance, pressure sensitive adhesives containing natural rubber have dominated pressure sensitive adhesives to this day, and are used in almost all applications, including packaging tapes, electrical insulating tapes, tapes for transporting electronic components, masking tapes, surface protection tapes, double-sided tapes, and medical tapes. This is because they exhibit excellent adhesion to a variety of adherends and can be supplied at low cost. In addition, from the viewpoint of reducing environmental impact, their demand has been increasing in recent years. As a pressure sensitive adhesive sheet having a pressure sensitive adhesive layer composed of a pressure sensitive adhesive containing natural rubber, for example, the pressure sensitive adhesive sheet for electrical equipment described in Patent Document 1 is known as a prior art. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2020-50711 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, due to the molecular structure, adhesives containing natural rubber are easily deteriorated during processing steps involving heat and shear, resulting in a significant decrease in holding power. In particular, when the adhesive containing natural rubber is a hot melt adhesive, the adhesive containing natural rubber is produced through processing steps involving heat and shear, resulting in a significant decrease in holding power of the adhesive. Therefore, an object of the present invention is to provide an adhesive tape which has an adhesive layer containing a rubber component including natural rubber and which is capable of suppressing a decrease in holding power due to processing steps involving heat and shear. [Means for solving the problem]

[0005] As a result of extensive investigations, the present inventors have found that the above problems can be solved by adding fibrillated long fibers to an adhesive component containing natural rubber, and have thus completed the present invention. [1] An adhesive tape having an adhesive layer containing a rubber component including natural rubber and fibrillated long fibers. [2] The adhesive tape according to the above [1], wherein the fibrillated long fibers are acrylic-modified polytetrafluoroethylene (PTFE) fibers. [3] The pressure-sensitive adhesive tape according to [1] or [2] above, wherein the fiber length of the fibrillated long fibers is 1 μm or more. [4] The pressure-sensitive adhesive tape according to any one of the above [1] to [3], wherein the average fiber diameter of the fibrillated long fibers is 500 nm or less. [5] The pressure-sensitive adhesive tape according to any one of the above [1] to [5], further comprising a substrate provided on one surface of the pressure-sensitive adhesive layer, the substrate being a paper substrate. [6] The pressure-sensitive adhesive tape according to any one of the above [1] to [5], wherein the molecular weight of the natural rubber is 400,000 daltons or more. [7] The pressure-sensitive adhesive tape according to any one of the above [1] to [6], wherein the pressure-sensitive adhesive layer has a gel fraction of 15% or more. [8] The pressure-sensitive adhesive tape according to any one of the above [1] to [7], wherein the pressure-sensitive adhesive layer is formed from a rubber-based pressure-sensitive adhesive containing a rubber component and fibrillated long fibers, and the rubber-based pressure-sensitive adhesive has a Mooney viscosity of 50 or more and 100 or less. [9] The adhesive tape according to any one of the above [1] to [8], having a bio content of 15% or more.

[10] The adhesive tape according to any one of the above [1] to [9], having an SP adhesive strength of 4 N / 24 mm or more.

[11] The pressure-sensitive adhesive tape according to any one of the above [1] to

[10] , which has a ball tack value of 8 or more. Effect of the Invention

[0006] According to the present invention, it is possible to provide a pressure-sensitive adhesive tape that includes a pressure-sensitive adhesive layer containing a rubber component including natural rubber and that can suppress a decrease in holding power due to processing steps involving heat or shear. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0007] [Adhesive tape] The pressure-sensitive adhesive tape of the present invention includes a pressure-sensitive adhesive layer containing a rubber component including natural rubber and fibrillated long fibers, which can prevent the holding power of the pressure-sensitive adhesive tape from decreasing due to processing steps involving heat and shear when producing the pressure-sensitive adhesive tape.

[0008] (Adhesive layer) The adhesive layer in the adhesive tape of the present invention contains a rubber component containing natural rubber and fibrillated long fibers. As described below, the adhesive layer is preferably formed from an adhesive containing a rubber component, fibrillated long fibers, and other components that are appropriately blended as necessary.

[0009] The rubber component contained in the adhesive layer of the adhesive tape of the present invention includes natural rubber. Natural rubber is obtained by coagulating latex extracted from Hevea Brasiliensis (Hevea genus, Hevea family, Hevea) which is mainly cultivated in various places such as Southeast Asia, the west coast of equatorial Africa, and the Amazon basin in Brazil. Examples of natural rubber include smoked sheet (RSS), pale crepe, blanket crepe, and hevea crumb. Among these, smoked sheet (RSS) is preferred.

[0010] From the viewpoint of the bio-ratio of the pressure-sensitive adhesive tape, the content of natural rubber in the pressure-sensitive adhesive layer is preferably 20 parts by mass or more, more preferably 35 parts by mass or more, and even more preferably 50 parts by mass, relative to 100 parts by mass of the total rubber components. The upper limit of the range of the content of natural rubber in the pressure-sensitive adhesive layer is not particularly limited, but is, for example, 100 parts by mass, preferably 90 parts by mass, more preferably 80 parts by mass, and even more preferably 70 parts by mass, relative to 100 parts by mass of the total rubber components.

[0011] From the viewpoint of the adhesive properties of the adhesive layer, the molecular weight of the natural rubber in the adhesive layer is preferably 400,000 Daltons or more, more preferably 600,000 Daltons or more, and even more preferably 800,000 Daltons or more. The upper limit of the range of the molecular weight of the natural rubber in the adhesive layer is not particularly limited, but is usually 1.4 million Daltons. The molecular weight of the natural rubber in the adhesive layer can be measured by the method described in the Examples below.

[0012] From the viewpoint of the bio-ratio of the adhesive tape, the rubber component preferably contains only natural rubber. However, from the viewpoint of the adhesive properties of the adhesive layer, the rubber component may contain a rubber component other than natural rubber. The rubber component other than natural rubber is, for example, a block copolymer. The block copolymer is a rubber other than natural rubber, and is preferably a synthetic rubber. Since the block copolymer is easily plasticized and flowed by heat, the adhesive constituting the adhesive layer can be a hot melt type adhesive by including the rubber component in the block copolymer. Examples of the block copolymer include styrene-isoprene-styrene block copolymer (SIS), styrene-butadiene-styrene block copolymer (SBS), and styrene-ethylene-butylene-styrene block copolymer (SEBS). These block copolymers can be used alone or in combination of two or more. From the viewpoint of the holding power of the adhesive tape, among these block copolymers, styrene-isoprene-styrene block copolymer (SIS) is preferred.

[0013] From the viewpoint of the bio-ratio of the pressure-sensitive adhesive tape, the content of the block copolymer in the pressure-sensitive adhesive layer is preferably 80 parts by mass or less, more preferably 65 parts by mass or less, and even more preferably 50 parts by mass or less, based on 100 parts by mass of the total rubber components. Also, from the viewpoint of the adhesive properties of the pressure-sensitive adhesive layer, the content of the block copolymer in the pressure-sensitive adhesive layer is preferably 10 parts by mass or more, more preferably 20 parts by mass or more, and even more preferably 30 parts by mass or more, based on 100 parts by mass of the total rubber components.

[0014] The rubber component may contain rubber components other than natural rubber and block copolymers, as long as the effects of the present invention are not impaired. Examples of rubber components other than natural rubber and block copolymers include styrene-butadiene rubber (SBR), polyisobutylene rubber, liquid rubber, etc. The content of rubber components other than natural rubber and block copolymers is preferably 0 parts by mass or more and 10 parts by mass or less, more preferably 0 parts by mass or more and 5 parts by mass or less, even more preferably 0 parts by mass or more and 2 parts by mass or less, and even more preferably 0 parts by mass, based on 100 parts by mass of the total rubber component.

[0015] (Fibrillated long fibers) The fibrillated long fibers are long fibers having fine naps due to fluff. Examples of the fibrillated long fibers include fibrillated acrylic-modified polytetrafluoroethylene (PTFE) fibers, fibrillated polyethylene fibers, fibrillated acrylic fibers, fibrillated aramid fibers, and fibrillated cellulose fibers. From the viewpoint of suppressing the decrease in the retention force due to the processing step involving heat or shear, among these fibrillated long fibers, fibrillated acrylic-modified polytetrafluoroethylene (PTFE) fibers and fibrillated cellulose fibers are preferred, and fibrillated acrylic-modified polytetrafluoroethylene (PTFE) fibers are more preferred. For example, the long fibers can be fibrillated by beating. In addition, the fibrillated long fibers may be formed from the fibrillating agent by the shear force when a rubber composition containing a rubber component and a fibrillating agent having fibril forming ability is kneaded.

[0016] <Fiber length> The fiber length of the fibrillated long fibers in the pressure-sensitive adhesive layer is preferably 1 μm or more. When the fiber length of the fibrillated long fibers is 1 μm or more, the fibrillated long fibers crosslink the molecules of the rubber component that are broken down during the processing step involving heat or shear, thereby improving the holding power of the pressure-sensitive adhesive tape. From this viewpoint, the fiber length of the fibrillated long fibers is more preferably 1.5 μm or more, and even more preferably 2 μm or more. The upper limit of the range of the fiber length of the fibrillated long fibers is not particularly limited, but is usually equal to or less than the thickness of the paste. The fiber length of the fibrillated long fibers can be measured by the method described in the Examples below.

[0017] <Average fiber diameter> The average fiber diameter of the fibrillated long fibers in the pressure-sensitive adhesive layer is preferably 500 nm or less. When the average fiber diameter of the fibrillated long fibers is 500 nm or less, the fibrillated long fibers crosslink the molecules of the rubber component that are broken down during the processing step involving heat or shear, thereby improving the holding power of the pressure-sensitive adhesive tape. From this viewpoint, the average fiber diameter of the fibrillated long fibers is more preferably 450 nm or less, and even more preferably 400 nm or less. The lower limit of the range of the fiber length of the fibrillated long fibers is not particularly limited, but is usually 10 nm. The average fiber diameter of the fibrillated long fibers can be measured by the method described in the Examples below.

[0018] <Content> From the viewpoint of the holding power of the adhesive tape, the content of the fibrillated long fibers in the adhesive layer is preferably 0.05 parts by mass or more and 20 parts by mass or less, more preferably 0.1 parts by mass or more and 15 parts by mass or less, even more preferably 0.5 parts by mass or more and 10 parts by mass or less, and still more preferably 1.0 parts by mass or more and 5 parts by mass or less, per 100 parts by mass of the rubber component in the adhesive layer.

[0019] The fibrillated long fibers in the pressure-sensitive adhesive layer of the pressure-sensitive adhesive tape of the present invention may be formed by kneading a fibrillating agent having fibril-forming ability with a rubber component or the like, and bonding the resins together by an external action such as shear force to make the fibrillating agent fibrous. Examples of the fibrillating agent include the Metablen A series, represented by "Metablen A3000", "Metablen A3700" and "Metablen A3800" manufactured by Mitsubishi Chemical Corporation.

[0020] (tackifier resin) The pressure-sensitive adhesive layer may contain a tackifier resin from the viewpoint of improving adhesive strength. As the tackifier resin, a tackifier resin having low polymerization inhibition properties such as hydrogenated terpene resin, hydrogenated rosin, disproportionated rosin resin, petroleum resin, etc. is preferable. Among these, a hydrogenated type is preferable, since a tackifier resin having many double bonds inhibits a polymerization reaction, and among these, a hydrogenated petroleum resin is preferable. From the viewpoint of improving the cohesive strength and adhesive strength of the adhesive, the softening point of the tackifier resin may be about 95° C. or higher, but preferably includes one that is 120° C. or higher, and for example, one that is 95° C. or higher and lower than 120° C. may be used in combination with one that is 120° C. or higher and 150° C. or lower. The softening point may be measured by the ring and ball method specified in JIS K2207. The content of the tackifier resin in the adhesive layer is preferably 10 parts by mass or more and 200 parts by mass or less, more preferably 20 parts by mass or more and 150 parts by mass or less, and even more preferably 40 parts by mass or more and 130 parts by mass or less, relative to 100 parts by mass of the total rubber component.

[0021] (Softener) The pressure-sensitive adhesive layer may contain a softener. By containing a softener, the processability of the pressure-sensitive adhesive constituting the pressure-sensitive adhesive layer can be improved. Examples of the softening agent include polybutene, polyisobutylene, process oil, and naphthenic oil. The content of the softener in the adhesive layer is preferably 5 parts by mass or more and 100 parts by mass or less, more preferably 10 parts by mass or more and 50 parts by mass or less, and even more preferably 15 parts by mass or more and 30 parts by mass or less, based on 100 parts by mass of the total rubber component.

[0022] (fine particles) The pressure-sensitive adhesive layer may contain fine particles, which can improve the adhesive strength of the pressure-sensitive adhesive layer. Examples of the fine particles include inorganic hollow particles such as glass balloons, shirasu balloons, and fly ash balloons; organic hollow particles made of polymethyl methacrylate, acrylonitrile-vinylidene chloride copolymers, polystyrene, and phenolic resins; inorganic fine particles such as glass beads, silica beads, calcium carbonate, clay, carbon, titanium oxide, zinc oxide, and synthetic mica; and organic fine particles such as ethyl polyacrylate, polyurethane, polyethylene, and polypropylene. The content of the microparticles in the pressure-sensitive adhesive layer is preferably 10 parts by mass or more and 100 parts by mass or less, more preferably 20 parts by mass or more and 70 parts by mass or less, and even more preferably 30 parts by mass or more and 50 parts by mass or less, based on 100 parts by mass of the total rubber component.

[0023] (Anti-aging agent) The pressure-sensitive adhesive layer may contain an antioxidant, which can suppress deterioration of the pressure-sensitive adhesive layer due to oxidation. Examples of the antioxidant include phenol-based antioxidants, amine-based antioxidants, phosphorus-based antioxidants, and waxes. The content of the antioxidant in the pressure-sensitive adhesive layer is preferably 0.01 parts by mass or more and 50 parts by mass or less, more preferably 0.1 parts by mass or more and 20 parts by mass or less, and even more preferably 0.5 parts by mass or more and 10 parts by mass or less, relative to 100 parts by mass of the total rubber component.

[0024] (Crosslinking agent) The pressure-sensitive adhesive layer may contain a crosslinking agent, which can improve the cohesive strength of the pressure-sensitive adhesive layer. Examples of the crosslinking agent include sulfur, thiuram-based crosslinking agents, phenolic resin-based crosslinking agents, and isocyanate-based crosslinking agents. The content of the crosslinking agent in the pressure-sensitive adhesive layer is preferably 0.01 parts by mass or more and 50 parts by mass or less, more preferably 0.1 parts by mass or more and 20 parts by mass or less, and even more preferably 0.5 parts by mass or more and 10 parts by mass or less, relative to 100 parts by mass of the total rubber component.

[0025] (Other Ingredients) The pressure-sensitive adhesive layer may contain, in addition to the above-mentioned components, various additives that are conventionally used in pressure-sensitive adhesives, such as pigments, dyes, polymerization initiators, flame retardants, and thickeners.

[0026] The adhesive constituting the adhesive layer in the adhesive tape of the present invention is preferably a hot melt adhesive. By forming the adhesive layer from a hot melt adhesive, it is not necessary to use a solvent in the adhesive layer, and therefore the environmental load can be further reduced. In addition, since the pressure-sensitive adhesive layer is formed without using a solvent, it is preferable that the pressure-sensitive adhesive layer does not substantially contain a solvent. Note that, "substantially not containing a solvent" means that the amount of residual solvent in the pressure-sensitive adhesive layer is less than 100 ppm by mass, but the lower the amount of residual solvent, the better, preferably less than 10 ppm by mass, more preferably 3 ppm by mass or less, and particularly preferably 0 ppm by mass.

[0027] <Gel fraction> The gel fraction of the pressure-sensitive adhesive layer in the pressure-sensitive adhesive tape of the present invention is preferably 15% or more. When the gel fraction of the pressure-sensitive adhesive layer is 15% or more, the holding power of the pressure-sensitive adhesive tape can be further improved. From this viewpoint, the gel fraction of the pressure-sensitive adhesive layer is more preferably 20% or more, even more preferably 25% or more, and even more preferably 30% or more. The upper limit of the range of the gel fraction of the pressure-sensitive adhesive layer is not particularly limited, but is usually 80%. The gel fraction of the pressure-sensitive adhesive layer can be measured by the method described in the Examples below. The gel fraction of the pressure-sensitive adhesive layer can be adjusted by the type and content of the rubber in the rubber component of the pressure-sensitive adhesive layer, and the type, average fiber diameter, fiber length and content of the fibrillated long fiber. The fibrillated long fiber has the effect of promoting crosslinking of the pressure-sensitive adhesive layer and increasing the gel fraction of the pressure-sensitive adhesive layer, just like the cross-linking agent. <Thickness> The thickness of the adhesive layer is not particularly limited, but may be, for example, about 5 μm to 200 μm, and preferably 10 μm to 100 μm. When the thickness of the adhesive layer is within this range, the resulting adhesive tape can exhibit sufficient adhesive strength.

[0028] <Mooney viscosity> The Mooney viscosity of the rubber-based adhesive which constitutes the adhesive layer in the adhesive tape of the present invention and contains a rubber component and fibrillated long fibers is preferably 50 or more and 100 or less. If the Mooney viscosity of the rubber-based adhesive is 50 or more, it is possible to prevent adhesion between the rubber-based adhesives and improve the handleability, and if it is 100 or less, it is possible to improve the kneadability of the rubber-based adhesive. From this viewpoint, the Mooney viscosity of the rubber-based adhesive is more preferably 60 or more and 90 or less, and even more preferably 70 or more and 85 or less. The Mooney viscosity of the rubber-based adhesive can be measured by the method described in the Examples below. The Mooney viscosity of the rubber-based adhesive can be adjusted by the type and content of rubber in the rubber component of the rubber-based adhesive.

[0029] (base material) The pressure-sensitive adhesive tape of the present invention may further comprise a substrate provided on one side of the pressure-sensitive adhesive layer. Examples of the substrate material include paper such as kraft paper, Japanese paper, crepe paper, fine paper, coated paper, synthetic paper, etc.; cloth such as cotton cloth, staple cloth, acetate cloth, glass cloth, polyester cloth, etc.; nonwoven fabric such as polyester nonwoven fabric, rayon nonwoven fabric, etc.; cellophane film, polyvinyl chloride film, polypropylene film, polyethylene film, polyester film, acetate film, etc.; metal foil such as aluminum foil, copper foil, etc.; polyurethane foam, polyethylene foam, vinyl chloride foam, chloroprene foam, natural rubber foam, butyl rubber foam, etc. Among these, the substrate material is preferably paper, more preferably kraft paper.

[0030] The thickness of the substrate is not particularly limited, but is preferably from 40 μm to 400 μm, more preferably from 60 μm to 300 μm, and further preferably from 80 μm to 200 μm.

[0031] When a paper substrate such as craft paper is used as the substrate material, a filler layer may be formed on at least one side of the paper substrate. The filler layer may be provided on the surface of the substrate on which the adhesive layer is provided, but is preferably provided on the surface opposite to the surface on which the adhesive layer is provided. Then, a release layer, which will be described later, may be formed on the filler layer provided on the opposite surface. The filler layer may be formed of a polyolefin layer or the like. Examples of polyolefin resins constituting the filler layer include polyethylene-based resins and polypropylene-based resins, with polyethylene-based resins being more preferred. The filler layer may be formed by laminating a resin such as a polyolefin resin on the surface of the substrate by lamination or the like. The thickness of the filling layer is not particularly limited, but is preferably from 1 μm to 20 μm, and more preferably from 3 μm to 15 μm.

[0032] The adhesive tape may have a release agent layer on the surface of the substrate opposite to the surface on which the adhesive layer is provided. The release agent layer may be directly laminated on the substrate, but is preferably laminated on the substrate via the above-mentioned sealing layer. By providing the release agent layer, when the adhesive tape is wound into a roll to form a roll, the adhesive layer comes into contact with the release agent layer, so that the adhesive tape can be easily unwound from the roll. The release agent layer may be formed from a known release agent such as a silicone-based release agent or a long-chain alkyl-based release agent.

[0033] When the substrate is a paper substrate and is a multi-layer substrate having a sealing layer as described above, the substrate has a basis weight of 10 g / m 2 More than 150g / m 2 It is preferable that the thickness is less than 40 g / m 2 More than 100g / m 2 It is more preferable that:

[0034] (Bio rate) The bio ratio (content of carbon derived from living organisms) of the pressure-sensitive adhesive tape of the present invention is preferably 15% or more. When the bio ratio of the pressure-sensitive adhesive tape of the present invention is 15% or more, petroleum resources can be saved in the production of the pressure-sensitive adhesive tape, and carbon dioxide emissions associated with the production of the pressure-sensitive adhesive tape can be suppressed, thereby reducing the environmental load. From this viewpoint, the bio ratio of the pressure-sensitive adhesive tape of the present invention is more preferably 20% or more, and even more preferably 25% or more. The upper limit of the range of the bio ratio of the pressure-sensitive adhesive tape of the present invention is not particularly limited, but is preferably 100%. The bio ratio of the pressure-sensitive adhesive tape can be measured by the method described in the Examples below. The bio ratio of the pressure-sensitive adhesive tape can be adjusted by the proportion of natural rubber in the pressure-sensitive adhesive layer and the type and content of fibrillated long fibers.

[0035] (SP adhesive strength) The SP adhesive strength of the adhesive tape of the present invention is preferably 4 N / 24 mm or more. When the SP adhesive strength of the adhesive tape is 4 N / 24 mm or more, the holding power of the adhesive tape is sufficiently prevented from decreasing due to a processing step involving heat or shear. From this viewpoint, the SP adhesive strength of the adhesive tape of the present invention is more preferably 5 N / 24 mm or more, and even more preferably 6 N / 24 mm or more. The upper limit of the range of the SP adhesive strength of the adhesive tape of the present invention is not particularly limited, but is usually 50 N / 24 mm. The SP adhesive strength of the adhesive tape can be measured by the method described in the Examples below. The SP adhesive strength of the adhesive tape can be adjusted by the type, average fiber diameter, fiber length and content of the fibrillated long fiber.

[0036] (Ball tack value) The ball tack value of the pressure-sensitive adhesive tape of the present invention is preferably 8 or more. When the pressure-sensitive adhesive tape has a ball tack value of 8 or more, the pressure-sensitive adhesive tape can immediately exhibit practical adhesive strength when applied to an adherend. From this viewpoint, the ball tack value of the pressure-sensitive adhesive tape of the present invention is more preferably 9 or more, even more preferably 10 or more, and even more preferably 11 or more. The upper limit of the range of the ball tack value of the pressure-sensitive adhesive tape of the present invention is not particularly limited, but is usually 30. The ball tack value of the pressure-sensitive adhesive tape can be measured by the method described in the Examples below. The ball tack value of the pressure-sensitive adhesive tape can be adjusted by the type, average fiber diameter, fiber length and content of the fibrillated long fiber.

[0037] (Method of manufacturing adhesive tape) The adhesive tape of the present invention can be produced by, for example, melt-mixing adhesive components such as natural rubber or other rubber components, fibrillating agent or fibrillated long fibers, and adhesive components such as tackifier resin, fine particles, softener, and antioxidant as necessary at high temperature to obtain an adhesive, and then coating the obtained root adhesive on the surface of a support. This method has the advantages of not requiring a drying step because it does not contain a solvent, being fast in coating speed, and not causing a risk of explosion or fire. The temperature during melt mixing is not particularly limited, but may be, for example, 130 to 180°C, and preferably 150 to 170°C. For example, a pressurized high-speed kneader or an extruder type mixer is used for melt mixing of the adhesive components, but when a fibrillating agent is used to form fibrillated long fibers, a mixer that can apply sufficient shear is preferably used. When a fibrillating agent is used, fibrillated long fibers can be formed by the fibrillating agent during mixing. For example, a slit die coater or a roll coater is used for coating, but is not particularly limited. The adhesive tape of the present invention contains natural rubber, and the fibrillated long fibers suppress the loss of holding power of the adhesive tape caused by deterioration of the natural rubber due to melt mixing at high temperatures.

[0038] (Adhesive tape applications) The applications of the pressure-sensitive adhesive tape of the present invention are not particularly limited, but by using natural rubber, the pressure-sensitive adhesive tape of the present invention has low production costs, a good balance of adhesive properties, and excellent practicality at low temperatures, and is therefore suitable for packaging applications and office applications. EXAMPLES

[0039] The present invention will be described in more detail below using examples, but the present invention is not limited to these examples.

[0040] [Evaluation method]

[0041] In the examples and comparative examples, the pressure-sensitive adhesive tapes were evaluated by the following evaluation methods. (Molecular weight of natural rubber) The molecular weight of natural rubber was measured by GPC (Gel Permeation Chromatography) analysis, and the peak top molecular weight was taken as the molecular weight of natural rubber. Specifically, the GPC analysis was performed using an ACQUITY APC (Waters) as an apparatus and an ACQUITY APCXT125-XT45-XT45 (Waters, 3 μm, 4.6×150 mm) as a column, and polystyrene was used as a GPC standard substance when calculating the molecular weight, and tetrahydrofuran was used as the GPC measurement solvent. (Measurement conditions) Mobile phase: Tetrahydrofuran 1.0mL / min Sample concentration: 0.2% by mass Detector: Refractive index (RI) detector, photodiode array (PDA) detector GPC standard material: Polystyrene (Waters, molecular weight: 266-1,800,000) Column temperature: 40℃

[0042] (Fiber length and average fiber diameter of fibrillated long fibers) The cross section of the adhesive tape was photographed using a scanning electron microscope (SEM), the fiber lengths of 10 arbitrarily selected fibrillated long fibers were measured, and the maximum measured fiber length was taken as the fiber length of the fibrillated long fibers. The cross section of the adhesive tape was also photographed using a SEM, the average fiber diameter of 10 arbitrarily selected fibrillated long fibers was measured, and the measured average fiber diameter was taken as the average fiber diameter of the fibrillated long fibers.

[0043] (Mooney viscosity of rubber-based adhesive) The Mooney viscosity of rubber-based adhesives is specifically Mooney viscosity ML1+4 (100℃), and was measured according to the method specified in JIS K 6300. In "ML1+4", "M" stands for Mooney M, "L" stands for rotor shape L, and "(1+4)" stands for 1 minute of preheating time and 4 minutes of rotor rotation time. Also, "(100℃)" means that it was measured at 100℃.

[0044] (Gel fraction of adhesive layer) A test piece of the adhesive layer was taken, and the mass A (mg) of the test piece was precisely weighed. Next, toluene was added to the test piece so that the adhesive solid content concentration was 6% by mass, and the test piece was immersed in toluene and shaken for 24 hours, and then filtered through a 200-mesh wire net to collect the insoluble matter on the wire net, vacuum-dried, and the mass B (mg) of the insoluble matter was precisely weighed. From the obtained value, the gel fraction (% by mass) was calculated using the following formula. Gel fraction (mass%) = 100 × (B / A)

[0045] (Bio-ratio of adhesive tape) The bio content of the adhesive tape was measured in accordance with ASTM 6866.

[0046] (SP adhesive strength of adhesive tape) In accordance with JIS Z 0237, the SP adhesive strength of the adhesive tape was measured 2 hours after application (left at 23° C.).

[0047] (Ball tack value of adhesive tape) The ball tack value of the adhesive tape was measured and calculated using a ball tack tester (manufactured by Yasuda Seiki Seisakusho) in accordance with JIS Z 0237 under conditions of a temperature of 23° C. and a relative humidity of 50%.

[0048] (SP holding power of adhesive tape (slip)) The adhesive layer side was attached to a polished SUS plate so that the adhesion area was 24 mm × 24 mm, and left to stand for 30 minutes under conditions of 23 ° C × 50% RH. Then, a load of 1 kg was applied under conditions of 23 ° C, and the displacement after 24 hours from the application of the load of 1 kg was measured according to the holding strength measurement method of JIS Z 0237.

[0049] [Examples 1 to 3, Comparative Example 1] The adhesive components mixed according to the amounts shown in Table 1 were charged into a kneading-extrudability tester (manufactured by Toyo Seiki Seisakusho Co., Ltd., product name "Labo Plastomill (registered trademark)"). The adhesive components were melt-kneaded under the conditions shown in Table 1, extrusion-molded, and coated on craft paper to produce adhesive tapes of Examples and Comparative Examples. The evaluation results of the obtained adhesive tapes are shown in Table 1.

[0050] [Table 1]

[0051] The components in Table 1 are as follows. Natural rubber: Smoked sheet (RSS Grade 1), masticated and pelletized product Block copolymer: Styrene-isoprene-styrene block copolymer (SIS), manufactured by JSR Corporation, product name "SIS5506" Fibrillated long fiber (fibrillating agent): Acrylic modified polytetrafluoroethylene (PTFE), manufactured by Mitsubishi Chemical Corporation, product name "Metabrene A-3000" Tackifier resin: Petroleum resin, manufactured by Zeon Corporation, product name "Quinton A-100" Softener: Process oil, manufactured by JXTG Energy Corporation, product name "Kurisef Oil F220" Fine particles: Calcium carbonate, manufactured by Nitto Funka Kogyo Co., Ltd., product name "NS#100" Antioxidant: Phenol-based antioxidant (2,2'-methylenebis-(4-ethyl-6-t-butylphenol)), manufactured by Yoshitomi Pharmaceutical Co., Ltd., product name "Yoshinox 425"

[0052] The pressure-sensitive adhesive tapes of Examples 1 to 3 had high SP retention because they had a pressure-sensitive adhesive layer containing a rubber component including natural rubber and fibrillated long fibers, whereas the pressure-sensitive adhesive layer of the pressure-sensitive adhesive tape of Comparative Example 1 did not contain fibrillated long fibers and therefore had low SP retention.

Claims

1. An adhesive tape comprising an adhesive layer containing a rubber component including natural rubber and fibrillated long fibers.

2. 2. The pressure-sensitive adhesive tape according to claim 1, wherein the fibrillated long fibers are acrylic-modified polytetrafluoroethylene (PTFE) fibers.

3. 2. The pressure-sensitive adhesive tape according to claim 1, wherein the fibrillated long fibers have a fiber length of 1 μm or more.

4. 2. The pressure-sensitive adhesive tape according to claim 1, wherein the average fiber diameter of the fibrillated long fibers is 500 nm or less.

5. Further comprising a substrate provided on one surface of the pressure-sensitive adhesive layer, The adhesive tape according to claim 1 , wherein the substrate is a paper substrate.

6. 2. The pressure-sensitive adhesive tape according to claim 1, wherein the molecular weight of the natural rubber is 400,000 daltons or more.

7. The pressure-sensitive adhesive tape according to claim 1 , wherein the pressure-sensitive adhesive layer has a gel fraction of 15% or more.

8. 2. The adhesive tape according to claim 1, wherein the adhesive layer is formed from a rubber-based adhesive containing a rubber component and fibrillated long fibers, and the rubber-based adhesive has a Mooney viscosity of 50 or more and 100 or less.

9. 2. The pressure-sensitive adhesive tape according to claim 1, having a bio content of 15% or more.

10. 2. The adhesive tape according to claim 1, having an SP adhesive strength of 4 N / 24 mm or more.

11. 2. The pressure-sensitive adhesive tape according to claim 1, which has a ball tack value of 8 or more.

Citation Information

Patent Citations

  • Self-adhesive tape and its production

    JP1995224257A

  • Pressure-sensitive adhesive composition for kraft pressure-sensitive adhesive tape

    JP1995268298A

  • Heat-conductive pressure-sensitive adhesive composition, heat-conductive pressure-sensitive adhesive sheet and electronic element

    JP2011246590A

  • Press bonding paper for confidential post card

    JP2015189205A

  • Adhesive composition and adhesive sheet

    JP2020012031A

Cited By

  • Adhesive tape