Method for preparing siloxane based polymeric liquid material and materials made therefrom

The acetic anhydride-based method for grafting organofunctional trialkoxysilanes onto hyPAS cores addresses the limitations of existing hyPAS production, achieving controlled core-shell structures with improved stability and functionalization for diverse applications.

JP2024156765AInactive Publication Date: 2024-11-06EIDGENISSISCHE MATERIALPRUFUNGS- UND FORSCHUNGSANSTALT EMPA
View PDF 13 Cites 0 Cited by

Patent Information

Application Number
JP2024121097
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2018-06-04
Filing Date
2024-07-26
Publication Date
2024-11-06
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Current methods for preparing hyperbranched polyalkoxysiloxanes (hyPAS) are limited by safety risks, corrosiveness of reagents, and lack of control over core-shell functionalization, leading to heterogeneous mixtures and inefficient production of core-shell structures.

Method used

A method involving the use of acetic anhydride chemistry to selectively graft organofunctional trialkoxysilanes onto a hyperbranched polysiloxane core, allowing for controlled formation of a functionalized siloxane shell in a core-shell structure, with steps conducted in a single reaction vessel and precise control over reactant ratios and conditions.

Benefits of technology

This approach yields polymeric liquid materials with a well-defined core-shell structure, enabling precise control over molecular weight and functionalization, resulting in stable, solvent-free materials suitable for various applications.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024156765000036
    Figure 2024156765000036
  • Figure 2024156765000037
    Figure 2024156765000037
  • Figure 2024156765000038
    Figure 2024156765000038
Patent Text Reader

Abstract

To provide a method for preparing a polymeric liquid material formed of molecular building blocks of core-shell type architecture, and materials made therefrom.SOLUTION: The present invention provides a polymeric liquid material formed of molecular building blocks of core-shell type architecture, wherein each building block consists of a hyperbranched polysiloxane core and a functional siloxane shell peripherally attached the core, the material comprising bridging oxygen moieties (Si-O-Si), hydrolysable alkoxy moieties (Si-O-R) and organofunctional moieties (R'-Si-) and ((R1-Si-R2) and less than 0.5 mass% of hydroxy moieties (Si-OH).SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates generally to methods for preparing polymeric liquid materials formed from core-shell structured molecular building blocks, and materials made therefrom. [Background technology]

[0002] With the progress of the nano era, science is targeting novel preparation methods that allow improved control of chemical building block units, thus relating atoms to the nanoscale. The creation of these new functional materials by design bridges the boundary areas from molecules to nanomaterials and from polymers to materials science. Figure 1 shows a rough classification in terms of size of molecular and nanoscale building blocks. Molecular building blocks (MBBs) are typically composed of tens to thousands of atoms and have a size of up to a few nanometers. Depending on their chemical nature and compactness, they are often liquid under ambient conditions. This is a clearly different characteristic from nanomaterials, which are solid at room temperature and composed of thousands to millions of atoms. As shown in the figure, there is no clear boundary between these material classes, with some overlap around 1 nm.

[0003] According to IUPAC, nanotechnology deals with novel materials with dimensions in the size range of approximately 1 nm to 100 nm, with structures, properties and interactions that are completely different from macroscopic materials. The so-called bottom-up approach, where molecular precursors are used to create nanoscale building blocks (NBBs), such as nanoparticles, by chemical reactions, offers the greatest flexibility to control new functionality and final material properties. In this particular technological field, the assembly of NBBs usually starts with atomic or small molecular precursors. Typical examples include: - polymeric nanoparticles prepared from organic monomers by emulsion polymerization; - precious metal nano-objects obtained by chemical reduction from the corresponding salt precursors in solution, -(Semi)metal oxide nanoparticles or "colloidal sols" synthesized from the corresponding (semi)metal salts or small molecule organometallic precursors such as alkoxides, acetylacetonates, etc.

[0004] More recently, researchers have targeted the controlled bottom-up synthesis of novel functional materials at the molecular level by precisely controlling the structure formation steps at the interface between small molecules and the nanoscale or even macroscale. For example, in the case of metal-organic frameworks (MOFs), molecular interactions are specifically selected and designed to combine organic precursors with metal / metal oxide precursors such that macroscopically large crystalline compounds with molecular-level control are obtained. Clearly, the molecular design approach gives access to an unprecedented variety of material properties. Similar concepts pursued in colloidal and polymer chemistry are at the forefront of materials science today.

[0005] In the state of the art, the introduction of specific chemical functionality into both MBBs or NBBs is achieved by either introducing functionalized species throughout the building block or by selectively grafting them onto the surface of the core block. In nanotechnology, the term core-shell describes nano-objects in which the core is covered with a layer of a second (often functionalized) compound. In molecular and polymer science, the term core-shell is not well established, but considering the high similarity, the term "core-shell" is extended here to MBBs and hyperbranched siloxane polymer science.

[0006] Among the classical representatives of highly compact dendritic MBBs, star polymers are a subclass of polymeric materials in which dendritic arms made with a given polymer chemistry emanate from a nucleus to which they are grafted. US Pat. No. 5,399,433 describes such star polymers, in which the peripheral polymer arms are functionalized with anionic or cationic groups attached by silane chemistry to improve the surfactant properties, but the main component is non-silicon-based. Furthermore, US Pat. No. 5,399,433 details two-arm and four-arm core-spacer-end group materials. The compounds described therein are linked by hydrosilylation chemistry and contain different molecular structures, namely i) a bisphenol-A organic core, a dimethylsiloxane spacer and organic groups (epoxy, methylstyrene, cyclopentadienyl) ends, ii) a tetrakis(dimethylsilyl)-siloxane core, a dicyclopentadiene spacer (or end), followed by a second tetramethyldisiloxane spacer and an epoxy or unsaturated end. US Pat. No. 5,399,433 describes a similar class of materials based on polyaromatic organic cores with three-fold and six-fold symmetry, siloxane spacer arms, and reactive organic end groups. US Pat. No. 5,499,433 proposes pure siloxane star polymer compounds without the use of "non-silicon" organic components. In the current state of the art, silane and siloxane-containing star polymers are generally obtained by successive molecular coupling reactions, each of which extends the shell by one building block unit. Coupling is most commonly achieved by hydrosilylation chemistry, producing low- to medium-molecular-weight polymers with well-defined compositions and sizes in the angstrom to nanometer range.

[0007] In contrast, organic / inorganic hybrid materials and NBBs can be obtained by different preparation techniques. For example, sol-gel techniques work in solution, starting from a colloidal suspension of molecular or oligomeric precursors, resulting in the spontaneous formation of nanoparticle building blocks. On the other hand, sols can be prepared in-situ from the olation and condensation reactions of oligomeric polyhydroxymetallic acids (e.g., silicic acid oligomers in the case of silica) through the control of solvent, pH, etc. They are used as classical NBBs to create porous metal oxide and hybrid materials. A more widely adapted route to metal oxide sols is from metal alkoxides such as TEOS, TMOS, Al or Ti isopropoxides in the respective parent alcohols and water as reactants. In a first step, hydrolysis of the alkoxy groups generates M-OH species, which then condense to form amorphous metal oxide NBBs or sols. Given the nature of the reversible interactions between the condensation of M-OH and the hydrolysis of MOM bonds, the morphology of the resulting materials is difficult to control, but is strongly influenced by the pH, precursor concentration, and solvent system. The preparation of colloidal sols using hydrolysis methods is a compromise between avoiding gelation, achieving a high degree of branching, and reducing the amount of volatile monomer fraction. Low molecular weight branched siloxane compounds are obtained by acid-catalyzed hydrolysis in neat (solvent-free) as described in US Pat. No. 5,399,633.

[0008] The preparation of chemically modified colloidal sols with controlled core-shell type structures, e.g., TEOS-based NBBs with a shell made with a second functional silane, is complicated by the fact that the hydrolysis and condensation kinetics of different silanes (TEOS vs. functional silanes) can differ significantly, resulting in poor surface selectivity of the deposits, as shown diagrammatically in Figure 2. This is especially true for the cohydrolysis of two different silane compounds, where there is a clear preference to form a heterogeneous mixture of "silane A" and "silane B" particles rather than homogeneous, statistically mixed, pure phase hybrid "AB" particles.

[0009] To improve the deposition selectivity of functional shells on NBBs, slowing down the reaction rate is often the only option. US Pat. No. 6,399,433 describes the functionalization of commercially available "Ludox" silica particles and similar colloids with shells made of functional organosilanes in dilute aqueous solutions, with slow dosing of functional silanes and at pH 4 (the reaction mixture is left to react for 24 hours at room temperature), where the hydrolysis / condensation rate is very slow. A more rapid alternative is emulsion-based radical polymerization chemistry. US Pat. No. 6,399,433 describes composite nanoparticles and their preparation, in which polymer core particles obtained by emulsion polymerization are coated with a layer of organosilane compounds by appropriate condensation chemistry. US Pat. No. 6,399,433 describes the reverse case, i.e., a PDMS-like core prepared as an emulsion, coated with a polyacrylate shell made by radical emulsion polymerization mediated by the use of a silane coupling agent with acrylate functionality. US Pat. No. 6,399,433 describes another very similar PDMS core / organic poly-(alkenyl aromatic) shell hybrid NBB material.

[0010] In the world of silicon-based MBBs, hyperbranched polyalkoxysiloxanes (hyPAS) are one of the most promising candidates offering both functionality and size control in one and the same molecule. hyPAS are small molecular building blocks with typical molecular weights ranging from 500 to 50,000 g / mol, spanning the size range from a few angstroms to single digit nanometers. Compared to the "sol-gel" hydrolytic route mentioned above, hyPAS are most commonly prepared by "non-hydrolytic" methods. This means that the condensation reactions used to join small molecule precursors to form larger polymeric MBBs can be controlled by stoichiometric addition of reactants, and thus can be started, stopped, and restarted at any given time. Furthermore, the synthesis can be carried out "neat", i.e., in the absence of additional solvents such as water or alcohol. Due to the nearly spherical and compact nature of hyPAS, they exhibit lower melt viscosities and much higher solubility than their linear polymer analogues. The classical preparation "non-hydrolytic" synthetic route for single-component hyPAS is as follows: 1) Condensation of the hydroxide obtained by reaction of alkoxysilanes with alkali hydroxides (silanol route) 2) Condensation of chlorides with alkoxysilanes (chloride route) 3) Condensation of a single alkoxysilane with itself by ether elimination 4) Condensation of acetoxy-functional alkoxysilanes with themselves by elimination of the corresponding acetate ester (acetoxy route) 5) Condensation of alkoxysilanes by reaction with acetic anhydride in the presence of a suitable catalyst with elimination of the acetate ester (anhydride route).

[0011] Method 1) is not very practical since it requires quantitative amounts of strong caustic hydroxide and the corresponding recovery and disposal of waste materials. Method 2) is described in US Pat. No. 5,399,633, in which the preparation of hyperbranched polysiloxanes proceeds by heterocondensation of chlorosilanes and alkoxysilanes with elimination of alkyl halides. The reaction is catalyzed by Ti-, V-, Zr-containing organometallic compounds. The highly corrosive nature of the chlorosilane reagents limits their commercialization.

[0012] Method 3) entails significant safety hazards in industrial environments due to the formation of dialkyl ethers with very low boiling points and very high flammability. Moreover, the homocondensation of such alkoxides is not self-terminating by consumption of a stoichiometrically limited second species such as chlorosilanes, hydroxysilanes, or acetoxysilanes, and must therefore be stopped by thermal quenching at any point without precise information on the progress of the reaction, making product control much more difficult.

[0013] Method 4) generally uses acetoxysilane, which is quite expensive. US Pat. No. 5,399,633 describes the preparation of lightly branched organosilane compounds by acetoxy derivatization starting from dimethylsiloxane prepolymers crosslinked with trifunctional silanes. The patent further describes the utility of the classical acetoxy route when only a few condensation bonds need to be made, i.e., when combining monomers with oligomeric / polymeric building blocks to make larger macromolecules. This can be done, for example, by refluxing silanol-terminated prepolymers with an alkoxy-terminated crosslinker in the presence of acetic acid at reflux at elevated temperatures, or directly with an acetoxy-terminated crosslinker (e.g., triacetoxysilane).

[0014] Method 5) was recently invented by Moeller et al. (e.g., Non-Patent Document 1) and is today the most advanced approach for preparing hyPAS in terms of scalability, process safety, and ease of implementation. It offers dramatically improved commercialization possibilities over 1) to 4) and the closest state of the art to the present invention, but at the same time it cannot address the selective "core-shell" problem of functionalizing hyPAS. As a result, Patent Document 12 is limited to the preparation of single-component hyPAS MBBs by the anhydride route. In the examples, the authors discuss the one-step preparation of pure silicate and titanate polyalkoxymetalates from their respective alkoxides, but in the central claim 1 others are also mentioned, specifically zirconates and hafnates. This same patent further describes in the Examples below the similar preparation of single-component organofunctional hyPAS prepared from organofunctional trialkoxysilanes, specifically methyltriethoxysilane (MTES) and heptadecafluoro-(1,1,2,2)-tetrahydrodecyltriethoxysilane. Organofunctional trialkoxysilanes are ideal precursors for introducing chemical functional groups due to the large selection of commercially available compounds and attractive prices. US Pat. No. 5,399,433 does not exclude the preparation of statistically mixed multicomponent hyPAS, which is the most obvious way to introduce specific organic chemical functionalities, but does not elaborate on the concept.

[0015] As an extension of Moeller's original work, US Pat. No. 5,399,633 deals with the chemical functionalization of silicate hyPAS prepared by Moeller's route 5) and their application as additives in coating formulations. Functional precursors are created by alcohol condensation of accessible alkoxy groups on the "Moeller type" hyPAS with hydroxyl-terminated polymers (preferred examples are polyalkylene oxides such as PEG, PPG, and polydimethylsiloxane (PDMS)) at temperatures in the range of 130°C. In this way, core-shell-like MBBs modified with PEG, PPG, PDMS, etc. are created, but without the full freedom to prepare the shell in a bottom-up manner with full control over the composition and shell substructure. The main difference with the present invention is in the mode of shell grafting by a single chemical bond formed to attach preformed linear polymer molecules to the hyPAS core. [Prior art documents] [Patent documents]

[0016] [Patent Document 1] DE 10 2008 063070 A1 [Patent Document 2] US Patent Application Publication No. 2004 / 0122186 [Patent Document 3] US Patent Application Publication No. 2007 / 19773 [Patent Document 4] US Patent Application Publication No. 2010 / 0305293 [Patent Document 5] European Patent Application Publication No. 1510520 [Patent Document 6] European Patent Application Publication No. 1978055 [Patent Document 7] European Patent Application Publication No. 1118632 [Patent Document 8] European Patent Application Publication No. 3059262 [Patent Document 9] US Patent Application Publication No. 2009 / 0215927 [Patent Document 10] European Patent Application Publication No. 0728793 [Patent Document 11] WO 00 / 40640 [Patent Document 12] International Publication No. 2004 / 058859 [Patent Document 13] International Publication No. 2004 / 058859 [Patent Document 14] International Publication No. 2014 / 187972 [Non-patent literature]

[0017] [Non-Patent Document 1] Macromolecules 2006, 39, 1701~1708 Summary of the Invention [Problem to be solved by the invention]

[0018] The object of the present invention is to provide methods for producing improved hyPAS materials, the same and various applications thereof. [Means for solving the problem]

[0019] According to one aspect of the present invention (claim 1), there is provided a method for preparing a polymeric liquid material formed from molecular building blocks of core-shell type structure, each building block consisting of a hyperbranched polysiloxane core and a functional siloxane shell peripherally attached to said core, the method comprising the steps of: a) at least one silicon tetraalkoxide Si(OR)4, where R is an unbranched or branched alkyl group having up to 4 carbon atoms; and optionally: - one R''-organofunctional trialkoxysilane R''-Si(OR)3, and optionally an R,R-organofunctional dialkoxysilane R3-Si(OR)2-R4; or - a mixture of different R''-organofunctional trialkoxysilanes and, optionally, at least one R3,R4-organofunctional dialkoxysilane; A functional mixture of In the form of monomers or oligomers, in the presence of a catalyst, the desired DP コア charging a reaction vessel with a first stoichiometric amount of acetic anhydride selected according to b) heating the reaction mixture provided in step a) with stirring in a water-free inert atmosphere to reach a desired reaction temperature and distilling off the resulting acetate reaction product until the reaction and distillate flow ceases, thereby forming said hyperbranched polysiloxane core; c) - one R'-organofunctional trialkoxysilane R'-Si(OR)3 and optionally an R1,R2-organofunctional dialkoxysilane R1-Si(OR)2-R2, or - a mixture of different R'-organofunctional trialkoxysilanes and, optionally, at least one R1,R2-organofunctional dialkoxysilane, シェル and optionally in the presence of a catalyst, to the hot reaction mixture formed in step b) with continued stirring to initiate the selective accumulation of said functional siloxane shells onto the cores formed in step b), whereby additional acetate esters are formed and distilled, and the reaction is continued until the flow of distillate is again stopped; R' and R'' are independently selected substituents, each of which may be represented as LZ; -L is -C6H4-, -C6H4-CH2-, -CH2-CH2-C6H4-CH2- and -[(CH)2] n - a linker group selected from the group consisting of (n=0, 1, 2, 3, 4); -Z is:

[0020] [ka]

[0021] is a terminal functional group selected from R * -H, -CH3, -C2H5, -C3H8, -C4H 10 and -C6H5; or Z is -[(CH)2] m -CH3 (m = 0, 1, 2, ..., 11); and R1, R2, R3 and R4 are -CH3, -C2H5, -C6H5, -C6H, provided that the triplets (R', R1, R2) and (R'', R3, R4) are not identical. 11 , -CH=CH2, -CH2-CH2-Cl, and -C5H5; Process and; d) optionally building up an additional functional layer on the shell by repeating the addition and reaction protocol described in step c) at least once; e) optionally removing low molecular weight reaction products and / or residual starting materials in the reaction mixture by vacuum distillation by gradually reducing the pressure in the reaction vessel and maintaining the final pressure in the range of 5-250 mbar for 10-120 minutes; f) cooling and isolating the polymeric liquid material thus obtained; Steps a) to e) are carried out in one and the same reaction vessel.

[0022] As will become clearer below, the core may contain a limited content of organofunctional siloxane moieties in addition to the predominantly non-organofunctional siloxane component. The shell, by definition, is composed exclusively of organofunctional siloxane moieties. The provision that the triplets (R', R1, R2) and (R'', R3, R4) are not identical means that the composition of the shell and the composition of the core component with optional functionality are not identical.

[0023] In the above preparation methods, the amounts of reactants used in the various steps will be selected depending on the desired composition of the polymeric liquid material to be formed. In particular, the amounts of reactants are selected to meet the content limitations further defined below.

[0024] In this context, the term "functional admixture" is used to refer to the amount of at least one organofunctional trialkoxysilane and optionally dialkoxysilane added in step a). Such admixture may provide specific functional properties to the core.

[0025] Advantageous embodiments are defined in the dependent claims and in the following description and examples. According to one embodiment (claim 2), the functional admixture is zero, in other words the core is composed essentially only of non-organofunctional siloxane moieties.

[0026] According to a further embodiment (claim 3), R is methyl or ethyl. According to another embodiment (claim 4), the reaction temperature in steps b) to e) is in the range of 70°C to 170°C, preferably in the range of 100°C to 150°C, most preferably in the range of 120°C to 140°C, and the pressure during steps b) to d) is in the range of 0.1 bar to 2 bar, preferably in the range of 0.5 bar to 1.4 bar, most preferably in the range of 0.9 bar to 1.2 bar.

[0027] According to yet another embodiment (claim 5), the silicon tetraalkoxide Si(OR)4 is tetraethoxysilane (TEOS) or tetramethoxysilane (TMOS), or a mixture of their monomers and oligomers.

[0028] According to a further embodiment (claim 6), the acetate reaction product is removed from the system via a distillation column comprising a number of theoretical plates, such that the lower boiling reaction products are separated from the higher boiling residual reactants in solution, whereby the latter are continuously fed back into the reaction mixture.

[0029] According to yet a further embodiment (claim 7), the catalyst is selected from the group of Ti(OR'')4, or Zn(II) alkanolates Zn(OR'')2, with R''=-CH2CH3, -CH(CH3)2, -CH2CH2CH3, -C(CH3)3, -CH2CH2CH2CH3, or the catalyst is Ti(O-Si(CH3)3)4 and the amount of catalyst is 0.01-1.5% on a molar basis of the total alkoxysilane precursor used in the core growth step.

[0030] According to yet another embodiment (claim 8), R' is: i) R' = -CH 5、 -CH=CH2, ii) R'=LZ, L is -CH2- and Z=[(CH)2] p -CH3 (p=0, 1, 2, 4, 6, 8, 10, 12, 14), iii) R'=LZ, L=-CH2CH2CH2-(n-propyl) and Z=-Br, -Cl, -I, -SH, -OH, -NH2, -NH-(BOC), -NH-(FMOC), -(2-oxiranyl), -methoxy-(2-oxiranyl), -N3, -SO3R, -PO3R2, -acrylate, -methacrylate, -ethacrylate, -propacrylate, -butacrylate; or iv) R'=LZ, L=CH2 and Z=vinyl, -acrylate, -methacrylate, -ethacrylate, -propacrylate, -butacrylate; is selected from the group R1 and R2 are the same and are selected from the group consisting of -CH3, -C6H5, and -CH=CH2, where R1=-CH3 and R2=-CH=CH2.

[0031] According to a further aspect (claim 9) there is provided a polymeric liquid material prepared by the method of the invention carried out without functional admixtures, the material being formed from molecular building blocks of core-shell type structure, each building block consisting of a hyperbranched polysiloxane core and a functional siloxane shell attached to the core at its periphery, the material comprises less than 0.5 weight percent hydroxy moieties (Si—OH); The core has a degree of polymerization (DP) in the range of 1.3-2.7, especially in the range of 1.5-2.5. コア having The shell is formed from R'-substituted siloxane moieties and, optionally, R1-, R2-substituted siloxane moieties and has a degree of polymerization DP in the range of 0.3 to 2.5, in particular in the range of 1.0 to 2.3. シェル having The molar ratio of total silicon to free hydrolyzable alkoxy in the material is 1:1.25 to 1:2.75; The material has a viscosity in the range of 10 to 100,000 cP; The core is composed of a non-organofunctional siloxane moiety, the non-organofunctional siloxane moiety being -General formula

[0032] [ka]

[0033] The non-organofunctional end-linked siloxane moiety (Q 1 chemical species) and / or -General formula

[0034] [ka]

[0035] The non-organofunctional disiloxane portion (Q 2 chemical species) and / or -General formula

[0036] [ka]

[0037] The non-organofunctional trisiloxane portion (Q 3 chemical species) and / or -General formula

[0038] [ka]

[0039] The non-organofunctional tetraloxane moiety (Q 4 chemical species) Including, The shell: -General formula

[0040] [ka]

[0041] Monoorganofunctional end-linked siloxane moieties (T 1 chemical species) and / or -General formula

[0042] [ka]

[0043] The monoorganofunctional disiloxane moiety (T 2 chemical species) and / or -General formula

[0044] [ka]

[0045] Monoorganofunctional trisiloxane (T 3 chemical species) part, and, optionally, -General formula

[0046] [ka]

[0047] End-linked diorganofunctional siloxane (D 1 chemical species) part and / or -General formula

[0048] [ka]

[0049] Diorganofunctional disiloxane (D 2 Chemical species) portion, R, R', R1 and R2 are as defined in claim 1. According to one embodiment, the material has a viscosity in the range of 50 to 5,000 cP.

[0050] Advantageously (claim 10), the relative atomic ratio of T species to Q species ranges from 0.03:1 to 1:1, preferably from 0.03:1 to 0.75:1, most preferably from 0.05:1 to 0.5:1.

[0051] According to another aspect of the present invention (claim 11) there is provided a hydrolysis product obtained by reacting a polymeric liquid material according to the first aspect with a predetermined amount of water or a predetermined amount of a water-solvent mixture.

[0052] According to a further aspect, the polymeric liquid material according to the further aspect, or the corresponding hydrolysis product according to the second aspect, is used for various applications as defined in claims 12 and 13.

[0053] Surprisingly, it has been found that a functional shell can be selectively constructed onto an existing hyPAS core or nucleus by administering a single organofunctional silane compound or mixture comprising at least one organofunctional trialkoxysilane under identical reaction conditions using successive acetic anhydride reactions (i.e., method 5) described in the introduction).

[0054] The direct reaction products are: - is clearly polymeric in nature, with the typical size of its constituent core-shell MBBs being less than 2 nm; - depending on the reaction conditions selected, they show a statistical distribution of molecular weights with a variable content of unreacted monomers and small oligomers, the lower molecular species can be optionally removed by vacuum distillation and recycled. Individual building blocks typically contain 30-500 Si atoms; - having a significant content of hydrolyzable and reactively crosslinking alkoxy groups in both the core and the shell; -An essentially solvent-free liquid mixture of pure MBB having a viscosity in the range of 10 to 100,000 cP; -MBB is star polymer-like in terms of its molecular structure.

[0055] A clear distinction with other star polymers from the known state of the art can be made with regard to the hyperbranched nature of the core, which indicates a significant degree of cross-linking in the core, and more importantly, the nature of the shell with respect to its variable size (from end-capping to mainly linear polymer chains of variable length). コア =1.3~2.7) and shell (DP シェル = 0.3–2.5) is within the limited polymerization range of both substructures.

[0056] In the present invention, the term "core-shell" is adopted from nanomaterials science. Based on the apparent polymeric character of the reaction products encompassed by the present invention, the boundary region between the core and shell must be understood as a diffuse shell, rather than a sharp boundary with an abrupt change in composition. This diffuse shell layer structure, where the concentration of functional shell species varies over several bond lengths or angstroms, is a direct result of condensation chemistry, i.e., grafting of functional silane shells onto preformed hyPAS cores. Since the outer arms of the dendritic hyPAS cores are highly permeable to smaller silane monomers and oligomers, it is clear that the degree of shell grafting is highest at their periphery, but there is no sharp cut-off. Nevertheless, the term "core-shell" still applies, since grafting at the center of the core is highly hindered, both for steric reasons and due to the reduced availability of reactive alkoxy groups. This is because the average connectivity (number of bridging oxygen bonds (Si-O-Si bonds per silicon center)) at the center of the core is higher than at the periphery of the core. Thus, the term "core-shell" is used in the context of the present invention to mean a hyPAS core with a diffusion shell according to the above discussion.

[0057] The degree of polymerization (DP) of the amorphous silicon oxide material is determined by the number of metal atoms (Si) in the system. tot It can be defined as the ratio of bridging oxygen BO (the number of Si-O-Si bonds) to the total number of Regarding the degree of polymerization: -DP=4, every Si atom is bonded to four other neighbors, i.e. this is the case in a perfect crystal (quartz) with four oxygen atoms located in the tetrahedral positions of each central Si, so that each Si atom sees exactly the same environment. -DP=3, on average each Si atom is bonded to three other Si atoms via bridging oxygen bonds (Si-O-Si). When a single component has a DP=3, its structure is an infinitely extended two-dimensional sheet, similar to the sheets found in clay minerals. -DP=2, on average each Si atom is connected via two bridging oxygen bonds. A single component analogue is, for example, a linear polymer such as a non-crosslinked PDMS (polydimethylsiloxane) type silicone resin.

[0058] The acetic anhydride reaction is quantitative with respect to its reagents (alkoxide and acetic anhydride). Therefore, the number of new bonds and DP formed as a result of its addition is directly proportional to the stoichiometric conversion factor f (and g) of the build-up reactions of the core i and shell ii, as shown below:

[0059] [ka]

[0060] For core formation from tetraalkoxide model compounds (equation i), the maximum stoichiometric coefficient f=2 corresponds to a ratio of acetic anhydride to tetraalkoxide of 2:1, which makes complete conversion to SiO2, DP=4, virtually impossible.

[0061] Mechanistically, Eq. a As shown in Figure 1, the acetic anhydride reaction proceeds through an acetoxy intermediate with the elimination of a first aliquot of acetate ester. The acetoxy intermediate is then converted to the product of formula i b As shown in Figure 2, elimination of a second aliquot of acetate ester undergoes intermolecular condensation with an alkoxy group on a second molecule.

[0062] [ka]

[0063] As already described in the original work of Moeller, organofunctional trialkoxysilanes can be converted to hyPAS using anhydride chemistry according to equation ii).

[0064] [ka]

[0065] However, due to the low number of alkoxy groups available for the condensation reaction (3 instead of 4), DP コア Mechanistically, di- and trialkoxysilanes react in the same way as tetraalkoxysilanes.

[0066] Most glasses and hyPAS are characterized by average DP values ​​that are significantly below the theoretical limit (complete conversion of all alkoxy groups). During preparation, the theoretical DP value is given by the stoichiometric ratios used in the reaction, and the effective DP value can be determined directly through quantitative analysis of the acetate reaction products. Independently, the DP of the material コア and D.P. シェル can be obtained directly from quantitative NMR data. For a simple model of a single-component hyPAS derived from tetraalkoxysilanes, DP is 29 From the Si NMR spectrum (FIG. 3), it can be calculated as follows:

[0067]

number

[0068] Here, A Qn Q n Species-related quantitative 29 The Si NMR peak area is given, which is a Si atom coordinated by n bridging oxygen (BO) atoms linked to the next nearest Si atom by a Si-O-Si bridge and 4-n non-bridging oxygen (NBO) atoms, i.e., alkoxy groups Si-OR.

[0069] For the pure tetraalkoxysilane model system, assuming quantitative conversion, DP is directly related to the stoichiometric f-coefficient (Eq. i) by the simple relationship:

[0070]

number

[0071] For organofunctional di- and trialkoxysilanes, 29 The Si spectral fingerprint region gradually shifts downfield, revealing different non-organic functionalities, Q, as seen in the model compound spectra after shell deposition. n The organic functional group T m and D. l The chemical structure shows that the two molecules can be clearly separated (Figure 4). Tm represents the peak area under the curve of each Si species belonging to an organofunctional trialkoxysilane having m BOs and (3-m) NBOs, and A Dl represents the peak area derived from an organofunctional dialkoxysilane having l BO and (2-l) NBO.

[0072] However, determining the degree of condensation and polymerization of the core-shell molecules is more complicated. The degree of polymerization (DP) of the core before the addition of the shell precursor and additional acetic anhydride is コア、最初 ) follows the equation for the pure system and is quantitative 29 It can be determined from Si NMR (FIG. 3) or from the stoichiometry.

[0073]

number

[0074] Here, A Qn is the quantitative concentration collected on an aliquot of the sample taken before the addition of the shell precursor. 29 Derived from Si NMR spectrum. For MBB materials featuring a shell grown from an organofunctional trialkoxysilane on an existing tetraalkoxysilane core in accordance with the present invention, the addition of new monomer and acetic anhydride (g is defined as the molar ratio of acetic anhydride to organofunctional trialkoxysilane) results in the following reaction: i) Continuation of core polymerization (QQ condensation), ii) homocondensation of T species (TT condensation), and iii) Grafting of functional silanes onto existing core siloxane branches (TQ condensation).

[0075] Homocondensation reaction (TT) is a shell (DP シェル ), whereas heterocondensation (TQ) can increase the degree of polymerization of DP according to the exemplary grafting reaction iii) shown below. コア and D.P. シェル Increase both.

[0076] [ka]

[0077] In the above grafting reaction example, R' organofunctional trialkoxysilane is T 0 From T 1 while the core species on the left side of the reaction (symbolized by three wavy siloxane bonds) is converted to Q 3 From Q 4 Note that each grafting reaction is simultaneously converted to DP コア and D.P. シェル Obviously, for example, T 2 The seed is Q 2 Grafted to T 3 and Q 3 Generate, or, T 1 The seed is Q 2 Grafted to T 2 and Q 3 There are all sorts of other combinations of grafting reactions possible, such as to produce

[0078] The experimental results suggest that TQ condensation (grafting) is the preferred reaction in the limits described by this invention. As can be seen from FIG. 29 Si- 29The Si INADEQUATE NMR spectrum shows clear signals related to QQ and QT correlations, while the peaks related to TT homocondensation are below the detection limit, providing evidence that the dominant T-condensation mechanism is the grafting of trifunctional silanes onto a preassembled core, rather than TT condensation and / or the formation of pure phase polycondensation species made with organofunctional trialkoxysilane building blocks.

[0079] The final degree of polymerization of the core-shell polymer is determined quantitatively after the reaction with the shell precursor is completed. 29 From the Si NMR spectrum, it can be determined as follows:

[0080]

number

[0081] Here, A Qn and A Tm is a quantitative analysis collected after the reaction with the shell precursor was completed. 29 This is derived from the Si NMR spectrum (Figure 4). Due to the above reactions i) to iii), DP コア、最終 and D.P. シェル f, g, and n シェル / n コア The ratio cannot be calculated directly from the TT and TQ reactions because the relative importance / selectivity of the TT and TQ reactions is not known a priori and the Q n and T m This depends on the relative reactivity of the monomer with the higher molecular weight hyPAS core species. Nevertheless, f, g, and n シェル / n コア is related to the respective degree of polymerization by the following equation:

[0082]

number

[0083] Here, ΔDP コア =DP コア、最終-DP コア、最初 and quantitative data collected after (Figure 4) and before (Figure 3) the addition of trifunctional monomer and acetic anhydride. 29 Determined from Si NMR spectra.

[0084] The MBB according to the present invention is composed of a tetraalkoxysilane-based hyPAS core. The selection of the f-factor in the core assembly is determined by the DP コア、最初 Determine (DP コア、最終 The claimed design parameters DP are identical to コア (not to be confused with ) and consequently also determines the size, molecular weight, and degree of branching of the core prior to shell growth. The shell is composed of a single polysiloxane layer made from organofunctional trialkoxysilane monomers or mixtures grown in a second (a) subsequent, time-separated step (possibly with additional subshells). Optionally, the shell monomer mixture includes a minority of organofunctional dialkoxysilanes.

[0085] The desired amount of acetic anhydride added during the growth of the shell (g factor) determines its size (average length of the polymer chains) and morphology. Higher g factors (g = 0.75-1.25) produce linear and slightly branched organodisiloxane shells, while lower g factors (g = 0.15-0.5) favor end-capping of the core with organofunctional monomers and short oligomers. On the other hand, low g factor conversions are always accompanied by a relatively large amount of unreacted monomers (T0 species) in the reaction mixture, which may be undesirable for practical applications, but can be removed by distillation if necessary.

[0086] The MBBs encompassed by the present invention span a wide range of structures with respect to the amount of material that constitutes the core and shell, as illustrated in the specific examples shown in Figure 6. This range of control over shell functionality can be achieved by varying the ratio of the molar amounts of precursor monomers used to construct the shell and core (n シェル / n コア ) can be best explained in terms of シェル / n コアRatios below 0.2 produce materials that are considered functional dendrimers and whose surface chemistry is dominated by the core composition, while n シェル / n コア Ratios above 0.5 produce materials that are clearly star polymer-like in nature, with their surface chemistry dominated by the shell composition. シェル / n コア In the intermediate composition range, the surface chemistry and reactivity are determined by both the core and shell compounds. シェル / n コア The bonding mode of the shell species is 29 It can be controlled by the amount of acetic anhydride added during the shell growth step (g factor), which directly affects the species population observed in the Si NMR spectrum.

[0087] DP 全体 When Q is greater than 2.0, the unreacted monomer species (Q for the corresponding tetra-, tri-, and dialkoxysilanes) in the crude MBB reaction mixture according to the present invention is 0 , T 0 , D 0 The total amount of unreacted monomer species (defined as 1 wt. %) is less than 10 wt. %, preferably less than 5 wt. %, and most preferably less than 2 wt. %. The amount of unreacted monomer species can be further reduced by distilling off the residual monomer after the core and before the shell growth step. The amount of unreacted monomer species in the NBB hydrolysis product according to the present invention is less than 1 wt. %.

[0088] In an advantageous embodiment, the core is derived from a silicon tetraalkoxide, preferably TEOS or TMOS, or a low molecular weight commercially available oligomer thereof, such as Dynasilan 40 (Evonik Industries) or equivalent, and the shell is derived from a single component monomeric organofunctional trialkoxysilane or a multicomponent trialkoxysilane mixture, respectively.

[0089] In a further advantageous embodiment, the core is derived from silicon tetraalkoxides, preferably TEOS or TMOS, or their low molecular weight commercial oligomers, such as Dynasilan 40 (Evonik Industries) or equivalents, and the single-component shell is composed of a mixture of monomeric organofunctional trialkoxysilanes and dialkoxysilanes. By replacing the organofunctional trialkoxysilanes with dialkoxysilanes, the content of hydrolyzable reactive crosslinker groups Si-OR can be precisely controlled. In this way, MBBs with more hydrophobic polydimethylsiloxane (PDMS, silicone)-like properties and reduced sensitivity to water can be obtained, with the exact properties being adjusted according to application-specific needs.

[0090] In another advantageous embodiment, the shell is prepared to be composed of two or more layers of different organofunctional trialkoxysilanes and optionally dialkoxysilanes. In the same way that the shell is selectively grown on the core by temporarily separating the core and shell assembly, additional layers of organofunctional siloxanes can be grown by repeating the shell growth procedure one or more times. In a particularly preferred embodiment, the first shell has organofunctional groups selected from the group methyl, vinyl, etc., which serve the main purpose of controlling the hydrophobicity and hydrolysis / condensation properties of the resulting MBB material, and the outermost shell layer has specific functional groups selected to aid reactive crosslinking, polymerization, and interface compatibility with application-relevant matrices, such as thiol, (BOC or FMOC protected) amine, vinyl, acrylate, phosphonic acid or sulfonic acid ester.

[0091] In a further advantageous embodiment, preferably to control custom-tailored functionality, the core is prepared to also contain minor components (less than 25% on a molar basis) with selected chemical functional groups that can increase the adsorption / uptake of guest species, such as metal and transition metal ions or small molecule drugs, for example. Particularly suitable for this are tetraalkoxysilanes, preferably TEOS (tetraethoxysilane) or TMOS (tetramethoxysilane) or their oligomers, and specific ligand groups (-NH2, SH, -PO3H) or covalently bound positively or negatively charged species (-SO3 - , -PO3 -2 , COO - , -NR3 + The core is composed of a mixture of organofunctional trialkoxysilanes with the functional groups preferably introduced by core co-assembly of the main tetraalkoxide component with a protected functional group monomer precursor (e.g., -NH-BOC or -NH-FMOC, -NH(butylidene), -SO3R, -PO3R2 terminated trialkoxysilanes).

[0092] One of the main advantages of the new class of MBBs encompassed by the present invention is the fact that these materials are essentially free of hydroxyl species (Si-OH mass content less than 0.5%), which means that they offer significantly improved stability and shelf life and substantially more structural control than traditional sol-gel based hybrid materials. In practical applications, MBBs can be used "as is" in non-polar organic solvents, blends, etc., or directly incorporated into hydrophobic matrices such as polymer melts.

[0093] The relative amounts of core and shell materials can vary within a wide range. According to an advantageous embodiment, the shell to core molar ratio n シェル :n コア is 0.05 to 2.0, preferably 0.1 to 1.0.

[0094] According to a further embodiment, the relative atomic content of T species in the shell is at least 10%, preferably at least 20%. According to one embodiment, the MBB products are converted into nanoscale building blocks by hydrolysis in water directly or in a suitable water / solvent system in the presence of acid or base catalysts as required. The hydrolysis products according to the present invention are nanoscale building blocks (NBBs), but with fully controllable substructures and custom tailorable functional groups, as shown diagrammatically in Figure 7. Compared to the state of the art, such novel hydrolysis products NBBs have the advantages of improved composition control and more efficient use of shell components (functional groups bearing tri- and dialkoxysilanes), which are often cost-limiting components in practical applications.

[0095] Furthermore, an advantageous method for the preparation of MBBs is outlined. The hyPAS core is first prepared according to the core build-up reaction i), in which a silicon tetraalkoxide such as TEOS or TMOS is mixed with a selected substoichiometric amount of f of acetic anhydride in the presence of a catalyst and the mixture is heated to a typical reaction temperature in the range of 120-140 °C. Mechanistically, acetic anhydride first reacts with the free alkoxy groups in the rate-determining step to form an acetoxy intermediate (formula i a ) and the acetate ester reaction by-product of the first molecule. b In (3), the acetoxy intermediate then reacts with a second alkoxy group on a monomer, oligomer, or pre-existing hyPAS molecule to form a MOM (in this case Si-O-Si) bond and a second acetate ester by-product molecule. Initially, the concentration of starting materials (tetraalkoxide and acetic anhydride) is high, which means that the reaction rate is high and acetate esters are accumulating rapidly in the reaction mixture. Thus, following the initiation of the reaction, acetate ester by-product formation may boil off, which has a boiling point significantly lower than both the starting materials and the hyPAS primary reaction product. As the reaction progresses, more and more siloxane bonds are formed, increasing the average hyPAS core size, molecular weight, and therefore DP コア increases first. As the f factor increases, the NMR species also increases in Qn Since acetic anhydride is used in substoichiometric amounts in the starting mixture, at some point it will be used up and the reaction will self-terminate. Also, since the reaction is completely stoichiometric with respect to the starting materials, the progress of the reaction, or more technically the degree of polymerization DP コア、最初 is directly proportional to the f coefficient, and DP シェル and ΔDP コア The statistically weighted sum of is directly proportional to the g-factor, which means that the growth of the core and shell can be separated in time and controlled independently of each other.

[0096] Once core assembly is complete and acetate distillation has ceased, the organofunctional siloxane shell is end-capped and / or overgrown by at least one, and optionally multiple, subsequent controlled additions of an organofunctional trialkoxysilane compound or mixture, and optionally further organofunctional dialkoxysilane or mixture, and a selected substoichiometric amount (g factor) of acetic anhydride required for shell polymerization to the same reaction mixture with continued stirring and at temperature. During or immediately after the addition, distillation of additional acetate reaction by-product is resumed. It should be noted that since organofunctional trialkoxysilanes and dialkoxysilanes contain only three and two alkoxy groups available for acetic anhydride reaction, the effective g factor must be adjusted for a given particular shell or subshell mixture. The ratio of substoichiometric acetic anhydride to total shell silane monomer is defined as the g factor and is typically expressed as DP シェル is selected to remain in the range of 0.3 to 2.5. According to the invention, the molar fraction of trialkoxysilane-based T species in the shell must be at least 5%, 10%, preferably at least 20%.

[0097] In a further advantageous embodiment, a multicomponent shell structure is deposited by repeating the shell addition procedure multiple times with different organofunctional trialkoxysilane and optionally dialkoxysilane monomers, each monomer preferably being added along with its selected equivalent amount of acetic anhydride necessary to create the desired degree of condensation of the subshell in question.

[0098] As is known from the first published work on hyPAS reported by Moeller et al. (Macromolecules 2006,39,1701-1708), the degree of polymerization / f-factor is limited to values ​​of about 2.5 / 1.25, respectively, for single-component tetraalkoxysilane compounds. The explanation lies in the fact that as DP / f increases, the pure hyPAS core continues to grow with the formation of more and more MOM bonds. At some point, a situation is reached where most of the low molecular species are no longer reactive, and from then on, the dendritic arms of the hyPAS will bond by additional condensation reactions. This explains why the viscosity of such compounds increases dramatically for DP / f values ​​above 2.2 / 1.1, respectively, leading to a considerable range of accessible liquid material viscosities as well. For single-precursor TEOS hyPAS model compounds prepared using Moeller's method, f-factors above 1.3 result in solid three-dimensional crosslinked products that are no longer soluble. The core-shell MBBs according to the invention also exhibit a high degree of polymerization, with the sum of the f- and g-factors (DP 全体) are limited in size by a general limitation that is directly related to the hyPAS core. Following the same logic as in Moeller's original model system, MBBs are grown by grafting trifunctional organofunctional trialkoxysilanes onto the hyPAS core with additional acetic anhydride. As the organofunctional trialkoxysilane monomers are grafted and transformed into stages T0 → T1 → T2 → T3 with increasing g-factor, the same situation occurs for the pure hyPAS component; that is, most of the monomers and small molecular species have reacted, and it becomes statistically more likely that the new bonds formed are connecting the two arms via the residual alkoxy groups. In experimental studies, the same rapid increase in viscosity is observed as a core of a given f-factor is further transformed into a core-shell MBB with a steady increase in g-factor, eventually leading to the formation of a fully three-dimensionally crosslinked rubber- or gel-like material.

[0099] Characterization of the reaction product with respect to viscosity is described, for example, in ASTM E2975-15: "Standard Test Method for Calibration of Concentric Cylinder Rotational Viscometers." These are easily analyzed by standardized viscosity measurements such as cylindrical rotational viscometers (Curtain Rotational Viscometers). Other viscosity test methods are possible, such as Staudinger type capillary viscometers and more modern dynamic viscosimetry.

[0100] Characterization of the molecular precursors for both the core and shell and the reaction products in terms of DP allows the core and shell species to be quantitatively determined in solution. 29 This is easiest for single-component core / single-component shell materials that are easily analyzed from Si NMR measurements. For more complex compositions, generally, 29 Si NMR can clearly separate the organic functional components of the core and shell, given the spectral shifts characteristic of the organic functional groups. A chemically specific analysis protocol for the general case (including the optional functional admixtures of claim 1) involves preparing the core as described in claim 1, drawing an aliquot sample, and then29 This includes subjecting the sample to Si-NMR analysis. コア、最初 followed by performing one or more shell growth steps; 29 The final material was analyzed again using Si-NMR and DP コア、最終 , and D.P. シェル Gives.

[0101] In the specified case where the incorporation of functional silane components in the core growth step is zero (claim 2) and its dependent material claim (claim 9), the relative amounts can be derived directly from the NMR spectral signatures of Q-type and T, D-type, respectively, so that the single 29 The Si NMR spectrum confirmed that コア and D.P. シェル It is sufficient to characterize the

[0102] One of the central aspects of the present invention is the grafting of shell monomers onto a preformed core. 2D INADEQUATE of TEOS-core / MTES (methyl-triethoxysilane)-shell model compounds 29 Si- 29 Si NMR studies revealed strong cross-peaks between Q2 / T2, Q2 / T1, which is strong evidence for the direct grafting of functional T species onto Q. More importantly, the high selectivity is highlighted by the absence of TT cross-peaks in the 2D NMR spectrum. Surprisingly, the rate of dosing of the shell monomer did not significantly change the product distribution, as would be expected by analogy with seeded-grown type core-shell nanoparticles. This is supported by the observation that the rate of the shell assembly reaction, measured by the distillation rate of the acetate reaction product, was found to be quite independent of the rate of addition of the trifunctional silane.

[0103] The use of high temperatures in combination with a catalyst is required for non-hydrolytic acetic anhydride chemistry to allow for sufficiently fast reaction rates to result in reasonable reaction times. The reaction temperatures for steps b) to e) are in the range of 70°C to 170°C, preferably in the range of 100°C to 150°C, and most preferably in the range of 120°C to 140°C. The pressure during steps b) to d) is in the range of 0.1 bar to 2 bar, preferably in the range of 0.5 bar to 1.4 bar, and most preferably in the range of 0.9 bar to 1.2 bar.

[0104] Depending on the reaction temperature, some monomers and acetic anhydride reagents will be close to their boiling points. During each reaction step (core and shell / subshell formation), which typically takes from 30 minutes to several hours depending on the type and concentration of catalyst used, some reagents tend to distill off together with the acetate by-product. This leads to a gradual loss of selected reagents depending on their boiling points, resulting in lower or higher effective f / g coefficients and DP values ​​than would be expected from the use of stoichiometry. These losses can be quantified as the difference between the molar amount of acetic anhydride used (f,g coefficients) and the effectively formed bonds (NMR analysis, quantification of acetate reaction products).

[0105] In an advantageous embodiment (claim 6), the loss of monomer and / or acetic anhydride reagent in the course of the reaction is countered by equipping the reactor with a distillation attachment comprising a separation stage with several theoretical plates connected to a distillation bridge. It is thus possible to quantitatively separate the low-boiling acetate reaction by-products from the unused high-boiling volatile reagents, the former being then fed back directly to the reactor. This significantly improves both the precision (effective DP value matches the amounts of selected reagents used) and the reproducibility (deviation of theoretical vs. effective f, g coefficients depending on starting monomers and reaction temperature, etc.) of the production process.

[0106] As reported by Moeller in his original patent application, the catalyst used in the non-hydrolytic process of acetic anhydride is advantageously selected from the family of tetraalkoxy titanates Ti(OR)4 or zinc diethanolates Zn(OR)2, where R = -CH2CH3, -CH(CH3)2, -CH2CH2CH3, -C(CH3)3 or -CH2CH2CH2CH3. More recent studies have identified tetrakis(trimethylsiloxy)titanium Ti(O-Si(CH3)3)4 as a particularly suitable catalyst. Catalyst concentrations are generally in the range of 0.02% mol to 1.5% mol, based on the total molar amount of silicon alkoxide used in the MBB preparation. The catalyst is typically added during the core build-up step, and additional catalyst dosage during the shell growth step is optional but usually unnecessary.

[0107] Advantageously (claim 7), the catalyst is selected from the group of Ti(OR'')4 or Zn(II) alkanolates Zn(OR'')2, where R''=-CH2CH3, -CH(CH3)2, -CH2CH2CH3, -C(CH3)3, -CH2CH2CH2CH3, or the catalyst is Ti(O-Si(CH3)3)4, the amount of catalyst being between 0.01 and 1.5% on a molar basis of the total alkoxysilane precursors used in the core growth step.

[0108] In summary, the present invention solves the problem of selective shell growth of organofunctional trialkoxysilanes, optionally also including organofunctional dialkoxysilanes, onto hyPAS "cores" by time-separated reactions, resulting in a new group of functional molecular building blocks (MBBs) with extreme variability in terms of composition, structure, and properties within a limited window of stoichiometric core / shell compound ratios. Furthermore, the hydrolysis products derived from MBBs encompassed by the present invention provide a new way to prepare nanoscale building blocks (NBBs) with great precision and control over their sub-nanometer structure and composition. The corresponding method for the production of core-shell MBBs involves a two- or multi-step reaction in which the preparation of a core mainly derived from a selected silicon tetraalkoxide or its oligomers by a non-hydrolytic acetic anhydride method is followed by the selected deposition of a mixture containing at least an organofunctional trialkoxysilane and optionally an organofunctional dialkoxysilane using the same acetic anhydride reaction. The time-separated shell deposition can be repeated multiple times, allowing the assembly of complex multi-layer shell structures.

[0109] The above and other features and objects of the present invention, as well as the manner in which the same are accomplished, will become more apparent, and the invention itself will be better understood, by reference to the preceding description of various embodiments of the invention taken in conjunction with the accompanying drawings. [Brief description of the drawings]

[0110] [Figure 1] Diagram of the broad classification of molecular and nanosciences in terms of the number and effective size of constituent atoms. [Diagram 2] Illustration of the limitations of the classical hydrolytic sol-gel method for preparing functional nanoscale building blocks (NBBs). The product distribution of NBBs is poorly controlled because it is determined by stochastic events in solution and the relative reaction rates of the various alkoxide and silane precursors. [Diagram 3]Quantitative 29Si NMR spectrum of the core collected before shell growth: DP core, first = 1.87. [Figure 4] Figure 1. Quantitative 29Si NMR spectrum of the core-shell sample with TEOS-based core and MTES-based shell: DP core, final = 2.40, ΔDP core = 2.40-1.87 = 0.53, DP shell = 1.86, n shell / n core = 0.09, DP total = 2.35. [Diagram 5] 29Si-29Si INADEQUATE NMR spectrum and its projections of a core-shell sample with a TEOS-based core and an MTES-based shell (n shell / n core = 0.38, DP core, final = 2.33, DP shell = 2.08, DP total = 2.26 from quantitative 29Si NMR). The peaks are evidence of covalent Si-O-Si bridges between the various T and Q species, while the diagonal peaks are evidence of adjacent pairs of the same species (e.g., Q2-Q2 or Q3-Q3). Different adjacent species appear as pairs of peaks symmetric around the diagonal (e.g., T2-Q2 and Q2-T2 peak pairs). [Figure 6a] Model sketches of various molecular building blocks showing their terminal chemical functionality, and diagrams of their classification with respect to relative content of functional groups (n-shell / n-core) and other defining parameters. [Figure 6b] Model sketches of various molecular building blocks showing their terminal chemical functionality, and diagrams of their classification with respect to relative content of functional groups (n-shell / n-core) and other defining parameters. [Figure 6c] Model sketches of various molecular building blocks showing their terminal chemical functionality, and diagrams of their classification with respect to relative content of functional groups (n-shell / n-core) and other defining parameters. [Figure 6d] Model sketches of various molecular building blocks showing their terminal chemical functionality, and diagrams of their classification with respect to relative content of functional groups (n-shell / n-core) and other defining parameters. [Figure 7]Schematic of potential uses of MBBs according to the present invention in applications. Condensation and / or self-assembly leads to the formation of NBBs with uniform composition and custom tailorable surface chemistry. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0111] Example 1: コア :n シェル Synthesis of TEOS / MTES core-shell MBB at 1:0.43 i)DP コア Manufacturing hyPAS cores with a target of =1.8 / f=0.9 52 g / 250 mmol of tetraethoxysilane (TEOS) and 0.83 ml of tetrakis(trimethylsiloxy)titanium (0.75 mol % relative to TEOS) were placed in a 250 ml round bottom flask equipped with a distillation bridge. 23.2 g / 225 mmol of acetic anhydride Ac2O was added to the mixture and the glassware setup was briefly purged with nitrogen, sealed, placed under nitrogen pressure (balloon) and immersed in a hot oil bath at 140 °C. The reaction mixture was brought to temperature while stirring at 500 rpm. Approximately 10 min after the time of immersion, the start of the reaction was evidenced by an accelerating reflux rate of the reaction by-product ethyl acetate that began to move up the distillation tube. After approximately 15 min, a continuous stream of ethyl acetate was distilled through the distillation bridge and collected in a catch vessel. The reaction continued for approximately another 45 min, at which point the reaction stopped, corresponding to the cessation of distillation of ethyl acetate. After 1 hour total reaction time the collection vessel was removed and emptied resulting in a total collected reaction by-product mixture of 41 ml.

[0112] ii)DP シェル Growth of MTES shells on hyPAS cores aiming for =3.6 / g=1.8 In the shell growth step, the reaction mixture from the previous step a) was left stirring at the same reaction temperature (oil bath set at 140 °C) and a mixture consisting of 19.15 g / 107 mmol of MTES (methyltriethoxysilane) and 19.6 g / 192 mmol of acetic anhydride Ac2O was added slowly with a syringe pump over a period of about 100 min with continued stirring. About 10-15 min after the start of dosing the MTES / Ac2O mixture, the start of distillation of ethyl acetate was observed again. After the addition was complete, the reaction mixture was kept stirring at temperature for another 20 min, the total reaction time for the shell growth step was about 2 h. At the end of the reaction, there was no further boiling of ethyl acetate, the heat source was removed from the reaction vessel and the mixture was allowed to cool to room temperature. The crude product yield was 32.8 g of a viscous yellowish oil. The shell growth step also resulted in 34 ml of distillate, which was collected from the capture vessel.

[0113] Example 2: コア :n シェル Synthesis of TEOS / VTES core-shell MBB at 1:0.15 i)DP コア Manufacturing hyPAS cores with a target of =2.4 / f=1.2 TEOS-derived hyPAS cores were prepared as in Example 1 i) with the same catalyst amount, temperature, and stirring speed. The amounts of TEO and Ac2O used in the synthesis were 52 g / 250 mmol and 30.6 g / 300 mmol, respectively, resulting in a theoretical f-factor of 1.2. The total reaction time was 1 h 30 min, producing 55 ml of distilled by-product.

[0114] ii) Growth of VTES shells on hyPAS cores at g = 1.12 Overgrowth of TEOS hyPAS cores was prepared similarly to Example 1 ii), with the main difference being the type and amount of functional trialkoxysilane used for shell growth. Thus, 7.13 g / 37.5 mmol of vinyltriethoxysilane (VTES) and 4.32 g / 42 mmol of Ac2O were dosed over 30 min. The crude product yield was 32.8 g of a slightly viscous yellowish oil. The shell growth step also resulted in 10 ml of distillate, which was collected from the capture vessel.

[0115] Examples 3-9: Synthesis of various two-component core-shell MMBs via trialkoxysilane shell chemistry i) hyPAS core fabrication Pure tetraalkoxide hyPAS and mixed cores were prepared as in Example 1 i) with the same catalyst amount, temperature and stirring speed. The amount of tetraalkoxide and optional functional trialkoxysilane second precursor component used in the synthesis, as well as the selected amount of Ac2O, are given in millimoles [mmol] for each experiment in the table above. The total reaction time was 1 hour and 30 minutes.

[0116] ii) Growth of the organofunctional trialkoxysilane shell In a second step, shells based on various organofunctional trialkoxysilanes and their mixtures were grown following the general process described in ii) of Example 1. The exact reaction parameters are given in the table below. Furthermore, the reaction products were 29 Characterized by Si NMR spectroscopy and material parameters (DP コア、最初 , D.P. コア,最終 , D.P. コア , D.P. シェル、 DP 全体 , n シェル / n コア ) was calculated using the formula given above.

[0117] The set of examples presented here is taken as experimental evidence of the broad applicability of the present method and the wide range of materials chemistries accessible via it. Examples 10 to 12:コア :n シェル Synthesis of TEOS core / (MTES / DMDES) shell MBBs at =1:(0.25-0.3) The TEOS-derived hyPAS core material was prepared in a water bath at 140° C. with the same catalyst amount and stirring speed as in Example 1 i). The amounts of TEOS and AcO used in the synthesis were 52 g / 250 mmol and 25.5 g / 250 mmol, respectively, with a theoretical f-factor (DP コア、最初 = 2.0). The total reaction time for the core formation was 1 hour and 30 minutes. The amount of condensate recovered from the core formation step in each case was 45 ml, indicating good reproducibility of the core formation step.

[0118] Following core formation, the temperature of the water bath was reduced to 120°C to partially suppress the loss of the more volatile DMDES monomer, and the system was allowed to equilibrate for 15 min. Shell growth was then induced by adding a mixture of methyltriethoxysilane (MTES) / dimethyldiethoxysilane (DMDES) over a 40 min period via a laboratory syringe pump. The following table shows selected shell composition parameters (grey shaded cells) defined by the stoichiometry of the added reagents for Examples 11 to 13. The theoretical g-factor used in this series is approximately 1.1.

[0119] [Table 1]

[0120] The as-obtained material was a clear, slightly yellow oily liquid. The reaction mixture was then further purified by distilling off the unreacted monomer and acetic anhydride by evacuating the reaction vessel to 50 mbar and heating the mixture to 150° C. with continued stirring and holding at temperature / vacuum for 40 minutes.

[0121] Examples 13-18: Gelation tests of NBB hydrolysis products derived from (TEOS / MTES) and (TEOS / VTES) core-shell NBBs Using a standard hydrolysis recipe, the same conditions as those given in Example 1 were used, but with varying n シェル :n コア The TEOS / MTES and TEOS / VTES core-shells prepared with the ratio and adjusted f-factor were converted to the corresponding NBB hydrolysis products, respectively. The following preparation scheme was used to prepare the NBB sol (hydrolysis product): A crude NBB mixture containing 4.32 g (6.4 ml) of ethanol and 3.84 TEOS core / MTES shell was weighed out and heated to 40°C with stirring in an Erlenmeyer flask. After a waiting period of 5 minutes, 15 microliters of 10% H2SO4 and 0.27 ml of distilled water were added to the mixture. After a brief homogenization period, the beaker was sealed with parafilm, removed from the heat source, and left under ambient conditions for 60 hours.

[0122] The so obtained NBB sol was then gelled using the following standard protocol: 7 ml of NBB sol was diluted with 16.3 ml of absolute ethanol denatured with 2% methyl ethyl ketone and 0.78 ml of distilled water in a 100 ml beaker. Then, 0.28 ml of 5.5 M ammonia solution was added to the diluted sol and the mixture was stirred for 5 minutes. The activated sol was then transferred to a 50 x 50 x 20 mm square plastic mould and allowed to gel at room temperature and the gelling time was recorded.

[0123] [Table 2]

[0124] From the above examples, especially when compared to the comparative examples shown below, it can be seen that the gelation time is quite fast. シェル / n コア Although it is not very dependent on the ratio, n シェル / n コア increases rapidly as

[0125] Comparative Examples 19-24: Gelation tests of (TEOS / MTES) and (TEOS / VTES) sols obtained by classical hydrolysis of alkoxide mixtures Standard sols were prepared from identical compound mixtures of TEOS / MTES and TEOS / VTES using classical hydrolysis and their gel times were measured and compared with the MBB→NBB approach according to the invention. The molar ratio of TEO to (MTES / VTES) was varied in a similar range to the above examples, within the functional silane to TEOS molar ratio window ranging from 0.15 to 0.47.

[0126] The sols were prepared in the same manner as the hydrolyzed NBB sols described above: 4.32 g (6.4 ml) of ethanol and 3.84 shells of TEOS / MTES or TEOS VTES mixtures, respectively, were weighed and heated to 40°C with stirring in an Erlenmeyer flask. After a waiting period of 5 minutes, 15 microliters of 10% H2SO4, 0.27 ml of distilled water were added to the mixture. After a brief homogenization period, the beaker was sealed with parafilm, removed from the heating source, and left under ambient conditions for 60 hours.

[0127] Again, the same gelation protocol was used as in Examples 18 to 23 above. A summary of the comparative experiments is given in the table below.

[0128] [Table 3]

[0129] All samples required more than 5 hours to gel and were left overnight. Surprisingly, all samples had gelled the next morning. In conclusion, the comparison reveals that sols obtained by classical hydrolysis gel much slower than their analogues derived from MBB → NBB sols. This is due to the higher degree of control over the molecular-scale building blocks of the sols obtained using the methodology described in this invention.

[0130] Summary table with examples:

[0131] [Table 4]

[0132] [Table 5]

[0133] [Table 6]

[0134] (Additional Note) The technical ideas that can be understood from the above-described embodiment and modified examples will be described. [Item 1] A method for preparing a polymeric liquid material formed from molecular building blocks of core-shell structure, each building block being composed of a hyperbranched polysiloxane core and a functional siloxane shell peripherally attached to said core, said method comprising the steps of: a) at least one silicon tetraalkoxide Si(OR)4, where R is an unbranched or branched alkyl group having up to 4 carbon atoms; and optionally: - one R''-organofunctional trialkoxysilane R''-Si(OR)3, and optionally an R,R-organofunctional dialkoxysilane R3-Si(OR)2-R4; or - a mixture of different R''-organofunctional trialkoxysilanes and, optionally, at least one R3,R4-organofunctional dialkoxysilane; A functional mixture of In the form of monomers or oligomers, in the presence of a catalyst, the desired DP コア charging a reaction vessel with a first stoichiometric amount of acetic anhydride selected according to b) heating the reaction mixture provided in step a) with stirring in a water-free inert atmosphere to reach a desired reaction temperature and distilling off the resulting acetate reaction product until said reaction and distillate flow ceases, thereby forming said hyperbranched polysiloxane cores; c) - one R'-organofunctional trialkoxysilane R'-Si(OR)3 and optionally an R1,R2-organofunctional dialkoxysilane R1-Si(OR)2-R2, or - a mixture of different R'-organofunctional trialkoxysilanes and, optionally, at least one R1,R2-organofunctional dialkoxysilane, シェル and optionally in the presence of a catalyst, to the hot reaction mixture formed in step b) with continued stirring to initiate the selective accumulation of said functional siloxane shells onto said cores formed in step b), whereby additional acetate esters are formed and distilled, and said reaction continues until the flow of distillate is again stopped; R' and R'' are independently selected substituents, each of which may be represented as LZ; -L is -C6H4-, -C6H4-CH2-, -CH2-CH2-C6H4-CH2- and -[(CH)2] n - a linker group selected from the group consisting of (n=0, 1, 2, 3, 4); -Z is: [ka] is a terminal functional group selected from R * -H, -CH3, -C2H5, -C3H8, -C4H 10 and -C6H5; or Z is -[(CH)2] m -CH3 (m = 0, 1, 2, ..., 11); and R1, R2, R3 and R4 are -CH3, -C2H5, -C6H5, -C6H, provided that the triplets (R', R1, R2) and (R'', R3, R4) are not identical. 11 , -CH=CH2, -CH2-CH2-Cl, and -C5H5; Process and; d) optionally building up an additional functional layer on said shell by repeating the addition and reaction protocol described in step c) at least once; e) optionally removing low molecular weight reaction products and / or residual starting materials in the reaction mixture by vacuum distillation by gradually reducing the pressure in the reaction vessel and maintaining the final pressure in the range of 5-250 mbar for 10-120 minutes; f) cooling and isolating the polymeric liquid material thus obtained; The method, wherein steps a) to e) are carried out in one and the same reaction vessel. [Item 2] 2. The method of claim 1, wherein the functional admixture is zero. [Item 3] 3. The method according to item 1 or 2, wherein R is methyl or ethyl. [Item 4] The process according to any one of items 1 to 3, wherein the reaction temperature in steps b) to e) is in the range of 70°C to 170°C, preferably in the range of 100°C to 150°C, and most preferably in the range of 120°C to 140°C, and the pressure during steps b) to d) is in the range of 0.1 bar to 2 bar, preferably in the range of 0.5 bar to 1.4 bar, and most preferably in the range of 0.9 bar to 1.2 bar. [Item 5] 5. The method according to any one of items 1 to 4, wherein the silicon tetraalkoxide Si(OR)4 is tetraethoxysilane (TEOS) or tetramethoxysilane (TMOS), or a mixture of monomers and oligomers thereof. [Item 6] 6. The process according to any one of items 1 to 5, wherein the acetate reaction product is removed from the system via a distillation column comprising a number of theoretical plates such that the lower boiling reaction products are separated from the higher boiling residual reactants in solution, whereby the latter are continuously fed back into the reaction mixture. [Item 7] 7. The method according to any one of items 1 to 6, wherein the catalyst is selected from the group of Ti(OR″)4, or Zn(II) alkanolates Zn(OR″)2, where R″=-CH2CH3, -CH(CH3)2, -CH2CH2CH3, -C(CH3)3, -CH2CH2CH2CH3, or the catalyst is Ti(O-Si(CH3)3)4, and the amount of the catalyst is 0.01-1.5% on a molar basis of the total alkoxysilane precursor used in the core growth step. [Item 8] R' is: i) R' = -CH 5、 -CH=CH2, ii) R'=LZ, L is -CH2- and Z=[(CH)2] p -CH3 (p=0, 1, 2, 4, 6, 8, 10, 12, 14), iii) R'=LZ, L=-CH2CH2CH2-(n-propyl) and Z=-Br, -Cl, -I, -SH, -OH, -NH2, -NH-(BOC), -NH-(FMOC), -(2-oxiranyl), -methoxy-(2-oxiranyl), -N3, -SO3R, -PO3R2, -acrylate, -methacrylate, -ethacrylate, -propacrylate, -butacrylate; or iv) R'=LZ, L=CH2 and Z=vinyl, -acrylate, -methacrylate, -ethacrylate, -propacrylate, -butacrylate; is selected from the group The method according to any one of items 1 to 7, wherein R1 and R2 are the same and selected from the group consisting of -CH3, -C6H5, and -CH=CH2, where R1=-CH3 and R2=-CH=CH2. [Item 9] A polymeric liquid material prepared by the method according to claim 2, wherein the material is formed from molecular building blocks of a core-shell structure, each building block being composed of a hyperbranched polysiloxane core and a functional siloxane shell peripherally attached to the core; the material comprises less than 0.5 weight percent hydroxy moieties (Si—OH); The core has a degree of polymerization DP in the range of 1.3 to 2.7, in particular in the range of 1.5 to 2.5. コア having The shell is formed from R'-substituted siloxane moieties and, optionally, R1-, R2-substituted siloxane moieties and has a degree of polymerization DP in the range of 0.3 to 2.5, in particular in the range of 1.0 to 2.3. シェル having the molar ratio of total silicon to free hydrolyzable alkoxy in said material is from 1:1.25 to 1:2.75; The material has a viscosity in the range of 10 to 100,000 cP; The core is comprised of a non-organofunctional siloxane moiety, the non-organofunctional siloxane moiety being -General formula [ka] The non-organofunctional end-linked siloxane moiety (Q 1 chemical species) and / or -General formula [ka] The non-organofunctional disiloxane portion (Q 2 chemical species) and / or -General formula [ka] The non-organofunctional trisiloxane portion (Q 3 chemical species) and / or -General formula [ka] The non-organofunctional tetraloxane moiety (Q 4 chemical species) Including, The shell comprises: -General formula [ka] Monoorganofunctional end-linked siloxane moieties (T 1 chemical species) and / or -General formula [ka] The monoorganofunctional disiloxane moiety (T 2 chemical species) and / or -General formula [ka] Monoorganofunctional trisiloxane (T 3 chemical species) part, and, optionally, -General formula [ka] End-linked diorganofunctional siloxane (D 1 chemical species) part and / or -General formula [ka] Diorganofunctional disiloxane (D 2 Chemical species) portion, The polymeric liquid material, wherein R, R', R1 and R2 are as defined in item 1. [Item 10] 10. The polymeric liquid material according to item 9, wherein the relative atomic ratio of T species to Q species is in the range of 0.03:1 to 1:1, preferably 0.03:1 to 0.75:1, most preferably 0.05:1 to 0.5:1. [Item 11] 11. A hydrolysis product obtained by reacting the polymeric liquid material according to item 9 or 10 with a predetermined amount of water or a predetermined amount of a water-solvent mixture. [Item 12] Use of the polymeric liquid material according to any one of items 9 to 11 or the corresponding hydrolysis product according to item 7 in coating or adhesive formulations or as a coupling agent for mediating the incorporation of fillers into a polymer matrix. [Item 13] Use of the polymeric liquid material according to any one of items 9 to 11 or the corresponding hydrolysis products according to item 7 as precursors in sol-gel chemistry techniques for the preparation of organofunctional gels and inorganic / organic nanocomposites, as well as aerogels and xerogels derived therefrom.

Claims

[Claim 1] The invention described herein.

Citation Information

Patent Citations

  • Use of star-shaped polymers with peripheral negatively charged groups and / or peripheral silyl groups for surface finishing

    DE102008063070A1

  • Method for preparation of polyorganosiloxane resin, optionally alkoxylated, through non-hydrolytic condensation

    EP0728793A1

  • Composite particles, composite particle dispersion composition, and method of preparing composite particle dispersion composition

    EP1118632A2

  • Preparation of branched siloxane

    EP1510520A1

  • Specific nanostructured material, as a protective coating for metal surfaces.