Device and method for manufacturing device
The use of protrusions and extending portions on liquid crystal cell substrates maintains a uniform cell gap, addressing thickness unevenness and enhancing display quality by preventing substrate separation and improving adhesive strength.
Patent Information
- Application Number
- JP2023073120
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-27
- Publication Date
- 2024-11-08
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing liquid crystal cells face issues with uneven thickness distribution, particularly when used vertically, leading to accumulation of liquid crystal material near the bottom, which can cause the thickness to exceed specified values.
The implementation of first and second protrusions and extending portions on opposing substrates, arranged to overlap with light shielding sections, which maintain a consistent distance between substrates and prevent excessive thickness variation by catching each other, ensuring uniform cell gap.
This configuration maintains a stable cell gap, preventing local thickness variations and ensuring high-quality display performance by minimizing substrate separation and enhancing adhesive strength through overlapping structures.
Smart Images

Figure 2024158159000001_ABST
Abstract
Description
[Technical field]
[0001] The technology disclosed in this specification relates to a device and a method for manufacturing a device. [Background technology]
[0002] Conventionally, one example of a liquid crystal cell (liquid crystal panel), which is a type of device, is known from the following Patent Document 1. Patent Document 1 describes a liquid crystal cell that includes a liquid crystal layer sandwiched between a first substrate and a second substrate, and a thickness control element that controls the thickness of the liquid crystal layer. In the liquid crystal cell described in Patent Document 1, the thickness control element includes a first spacer formed on the first substrate and a second spacer formed on the second substrate, and the two spacers abut against each other to control the thickness of the liquid crystal layer, and the spacers are formed in the non-display areas between the dots. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2002-162632 A Summary of the Invention [Problem to be solved by the invention]
[0004] The thickness control element described in the above-mentioned Patent Document 1 functions to control the thickness of the liquid crystal layer so that it does not fall below a certain value. However, for example, when the liquid crystal cell is used in a vertically oriented state, there is a concern that the liquid crystal material may accumulate near the bottom of the liquid crystal cell, causing the thickness of the liquid crystal layer near the bottom of the liquid crystal cell to be greater than the specified value. The thickness control element described in Patent Document 1 could not address such a problem.
[0005] The technology described in this specification was developed based on the above circumstances, and aims to keep the gap between the first substrate and the second substrate from exceeding a certain value. [Means for solving the problem]
[0006] (1) A device related to the technology described in this specification includes a first substrate having a first main surface, a second substrate having a second main surface facing the first main surface with a gap therebetween, a first protrusion provided on the first substrate and protruding from the first main surface toward the second main surface, a first extension extending from the first protrusion along the first main surface and disposed with a gap between the first main surface and the first extension, a second protrusion provided on the second substrate and protruding from the second main surface toward the first main surface, and a second extension extending from the second protrusion along the second main surface and disposed so as to sandwich the first extension between the second substrate and the first extension.
[0007] (2) In addition to the above (1), the device may further include a liquid crystal layer made of a liquid crystal material and sandwiched between the first substrate and the second substrate.
[0008] (3) In addition to the above (2), the device may further include a plurality of pixels and a light-shielding portion disposed between adjacent pixels to block light, and the first protrusion, the first extension, the second protrusion, and the second extension may be disposed to overlap the light-shielding portion.
[0009] (4) In addition to the above (2), the device may further include a sealing portion interposed between the first substrate and the second substrate, surrounding the liquid crystal layer and sealing the liquid crystal layer, and the first protrusion, the first extension, the second protrusion, and the second extension may be arranged to overlap the sealing portion.
[0010] (5) In addition to any one of (2) to (4) above, the device may further include a spacer provided on the first substrate protruding from the first main surface toward the second main surface, and a bump provided on the second substrate protruding from the second main surface toward the first main surface and arranged opposite the spacer, the first protruding portion and the first extending portion being made of the same material as the spacer, and the second protruding portion and the second extending portion being made of the same material as the bump.
[0011] (6) A method for manufacturing a device related to the technology described in this specification includes providing a first protruding portion protruding from a first main surface of a first substrate and a first extension portion extending from the first protruding portion along the first main surface and disposed at a distance from the first main surface, providing a second protruding portion protruding from a second main surface of a second substrate and a second extension portion extending from the second protruding portion along the second main surface and disposed at a distance from the second main surface, arranging the first substrate and the second substrate such that the first main surface and the second main surface face each other and the first protruding portion and the first extension portion do not overlap with the second protruding portion and the second extension portion, adjusting a distance between the first substrate and the second substrate, positioning the first extension portion between the second main surface and the second extension portion, and sliding the first substrate and the second substrate in a direction along the first main surface and the second main surface to sandwich the first extension portion between the second extension portion and the second main surface.
[0012] (7) In addition to the above (6), the method for manufacturing the device may include the steps of: when providing the first protrusion and the first extension on the first substrate, forming a first film on the first main surface of the first substrate, patterning the first film to provide a first pedestal, forming a second film on an upper side of the first film, patterning the second film to provide the first protrusion and the first extension overlapping the upper side of the first pedestal, and etching and removing the first pedestal; and when providing the second protrusion and the second extension on the second substrate, forming a third film on the second main surface of the second substrate, patterning the third film to provide a second pedestal, forming a fourth film on the upper side of the third film, patterning the fourth film to provide the second protrusion and the second extension overlapping the upper side of the second pedestal, and etching and removing the second pedestal. Effect of the Invention
[0013] According to the technique described in this specification, the gap between the first substrate and the second substrate can be kept at a constant value or less. [Brief description of the drawings]
[0014] [Figure 1] FIG. 1 is a plan view of a liquid crystal panel, a driver, and a flexible substrate that constitute a liquid crystal display device according to a first embodiment; [Diagram 2] 1 is a cross-sectional view of a liquid crystal panel, a driver, and a flexible substrate according to a first embodiment. [Diagram 3] FIG. 1 is a plan view showing a pixel arrangement of a liquid crystal panel according to a first embodiment; [Figure 4] FIG. 2 is a cross-sectional view showing the configuration of pixels, spacers, bumps, and the like provided in the display area of the liquid crystal panel according to the first embodiment. [Diagram 5] FIG. 2 is a cross-sectional view showing the configuration of a first protrusion, a first extension, a second protrusion, and a second extension provided in a display area of the liquid crystal panel according to the first embodiment; [Figure 6] FIG. 11 is a cross-sectional view showing a state in which a first pedestal portion is provided by patterning a first metal film in a fourth step of a counter substrate manufacturing process constituting a manufacturing method of an array substrate according to the first embodiment; [Figure 7] FIG. 11 is a cross-sectional view showing a state in which a first protruding portion and a first extending portion are provided by patterning a first insulating film in a fourth step of a counter substrate manufacturing process constituting a manufacturing method of an array substrate according to the first embodiment. [Figure 8] FIG. 11 is a cross-sectional view showing a state in which the first metal film is etched and the first pedestal portion is removed in a fourth step of the counter substrate manufacturing process constituting the manufacturing method of the array substrate according to the first embodiment; [Figure 9] FIG. 11 is a cross-sectional view showing a state in which a second metal film is patterned to provide a second pedestal portion in a tenth step of the array substrate manufacturing process constituting the manufacturing method of the array substrate according to the first embodiment; [Figure 10] FIG. 13 is a cross-sectional view showing a state in which a second protruding portion and a second extending portion are provided by patterning a second insulating film in a tenth step of the array substrate manufacturing process constituting the manufacturing method of the array substrate according to the first embodiment; [Figure 11] FIG. 13 is a cross-sectional view showing a state in which the second metal film is etched and the second pedestal portion is removed in a tenth step of the array substrate manufacturing method according to the first embodiment; [Figure 12]FIG. 13 is a cross-sectional view showing a state in which the counter substrate and the array substrate are disposed opposite each other in a thirteenth step of a bonding process constituting a manufacturing method of the array substrate according to the first embodiment. [Figure 13] FIG. 13 is a cross-sectional view showing a state in which the gap between the counter substrate and the array substrate is adjusted in a thirteenth bonding step in the manufacturing method of the array substrate according to the first embodiment. [Figure 14] FIG. 11 is a cross-sectional view showing a case where the sliding amount when sliding the counter substrate and the array substrate is insufficient in a thirteenth step of a bonding process constituting a manufacturing method of the array substrate according to the first embodiment; [Figure 15] FIG. 11 is a cross-sectional view showing a case where the sliding amount when the counter substrate and the array substrate are slid in a thirteenth step of the bonding process constituting the manufacturing method of the array substrate according to the first embodiment is excessive. [Figure 16] FIG. 11 is a cross-sectional view showing the configuration of a first protrusion, a first extension, a second protrusion, and a second extension provided in a non-display area of a liquid crystal panel according to a second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] <Embodiment 1> The first embodiment will be described with reference to Fig. 1 to Fig. 15. In this embodiment, a liquid crystal display device 10 will be illustrated. Note that the X-axis, Y-axis, and Z-axis are shown in a part of each drawing, and each axis direction is drawn to be the direction shown in each drawing. Also, the upper side of Fig. 2, Fig. 4, Fig. 5, Fig. 12 to Fig. 15 is the front side, and the lower side of the drawings is the back side.
[0016] 1, a liquid crystal display device 10 includes at least a vertically elongated rectangular liquid crystal panel (device, display panel) 11 capable of displaying an image, and a backlight device (illumination device) which is an external light source that irradiates the liquid crystal panel 11 with light to be used for display. The backlight device is disposed on the rear side (back side) of the liquid crystal panel 11, and includes a light source (e.g., an LED) that emits white light, and an optical member that converts the light from the light source into planar light by applying an optical effect. The central portion of the screen of the liquid crystal panel 11 is a display area AA where an image is displayed. In contrast, a frame-shaped outer peripheral portion surrounding the display area AA on the screen of the liquid crystal panel 11 is a non-display area NAA where no image is displayed.
[0017] The liquid crystal panel 11 will be described in detail with reference to FIG. 1 and FIG. 2. As shown in FIG. 1 and FIG. 2, the liquid crystal panel 11 is formed by bonding a pair of almost transparent (translucent) substrates 11A and 11B. The front side (front side) of the pair of substrates 11A and 11B is the counter substrate (first substrate, CF substrate) 11A, and the back side (rear side) is the array substrate (second substrate, TFT substrate) 11B. The counter substrate 11A and the array substrate 11B are both formed by laminating various films on the inner side of a glass substrate. A predetermined gap is provided between the counter substrate 11A and the array substrate 11B, which are bonded together. A liquid crystal layer 11C containing liquid crystal molecules, which are a substance whose optical properties change with the application of an electric field, is sandwiched between the counter substrate 11A and the array substrate 11B. In this embodiment, the thickness (cell gap) of the liquid crystal layer 11C is, for example, about 3 μm. A sealing portion (sealing portion) 11D for sealing the liquid crystal layer 11C is provided between the outer peripheral ends of the pair of substrates 11A and 11B. The sealing portion 11D is formed in a rectangular frame shape so as to surround the liquid crystal layer 11C. A polarizing plate 14 is attached to the outer surface side of each of the substrates 11A and 11B.
[0018] 1 and 2, the array substrate 11B has a longer side dimension larger than that of the counter substrate 11A, and one end of the longer side is a protruding portion 11B1 that protrudes laterally from the counter substrate 11A. The protruding portion 11B1 is exposed and not covered by the counter substrate 11A. The entire protruding portion 11B1 is a non-display area NAA, and a driver 12 and a flexible substrate 13 for supplying various signals are attached to the protruding portion 11B1.
[0019] The pixel arrangement in the display area AA of the array substrate 11B will be described with reference to FIG. 3. As shown in FIG. 3, a plurality of gate lines (scanning lines) 15 and source lines (image lines) 16 are arranged in a lattice pattern on the inner surface of the display area AA of the array substrate 11B. A TFT (thin film transistor) 17 and a pixel electrode (electrode) 18 are provided near the intersection of the gate lines 15 and the source lines 16. The gate lines 15 extend generally along the X-axis direction across the display area AA and are connected to the gate electrodes 17A of the TFTs 17. A plurality of the gate lines 15 are arranged side by side at intervals in the Y-axis direction. The source lines 16 extend generally along the Y-axis direction across the display area AA and are connected to the source electrodes 17B of the TFTs 17. A plurality of the source lines 16 are arranged at intervals in the X-axis direction. The gate lines 15 and the source lines 16 cross each other, but are insulated from each other by an insulating film interposed therebetween. The TFTs 17 and the pixel electrodes 18 are regularly arranged in a matrix (rows and columns) along the X-axis and Y-axis directions. The pixel electrodes 18 are connected to the drain electrodes 17C of the TFTs 17. The pixel electrodes 18 are made of a transparent electrode material such as ITO (Indium Tin Oxide). The TFTs 17 have a semiconductor portion 17D in addition to the gate electrodes 17A, source electrodes 17B, and drain electrodes 17C. The semiconductor portion 17D is made of a semiconductor material and is connected to the source electrodes 17B and the drain electrodes 17C. When the TFTs 17 are driven based on a scanning signal supplied to the gate lines 15, they charge the pixel electrodes 18 to a potential based on an image signal (data signal) supplied to the source lines 16.
[0020] The cross-sectional structure of the display area AA of the liquid crystal panel 11 will be described with reference to FIG. 4. In FIG. 4, the gate wiring 15, the source wiring 16, and the TFT 17 are simplified and illustrated as a "pixel circuit section (circuit section) 19". In the display area AA of the counter substrate 11A constituting the liquid crystal panel 11, as shown in FIG. 4, a large number of color filters 20 are provided at positions overlapping with each pixel electrode 18 provided on the array substrate 11B. The color filters 20 are arranged in a striped pattern as a whole, with three colors of red (R), green (G), and blue (B) repeatedly arranged alternately along the X-axis direction and extending along the Y-axis direction. The color filters 20 face the pixel electrodes 18 on the array substrate 11B side. The color filters 20 and the pixel electrodes 18 facing each other constitute a pixel PX, which is a display unit. In the display area AA of the counter substrate 11A, a light-shielding section (black matrix) 21 is provided to partition the adjacent color filters 20 to prevent color mixing. The light-shielding portion 21 is also provided in the non-display area NAA (see FIG. 16 of the second embodiment). The light-shielding portion 21 is in a lattice shape so as to overlap the gate wiring 15 and the source wiring 16 in the display area AA, but is in a solid shape in the non-display area NAA. An overcoat film 22 is formed on the upper layer side of the color filter 20 and the light-shielding portion 21. The overcoat film 22 is provided in a generally solid shape over almost the entire area of the counter substrate 11A. The overcoat film 22 is made of an organic material such as an acrylic resin (e.g. PMMA, etc.), and functions to flatten steps occurring on the lower layer side of the overcoat film 22. In this embodiment, the surface of the overcoat film 22 is the first main surface 11A1 of the counter substrate 11A. An alignment film for aligning the liquid crystal contained in the liquid crystal layer 11C is provided on the upper layer side of the overcoat film 22 (the innermost surface of the counter substrate 11A).
[0021] As shown in FIG. 4, the display area AA of the counter substrate 11A is provided with spacers 23 protruding from the first main surface 11A1 toward the array substrate 11B (second main surface 11B1). The spacers 23 can maintain the distance between the pair of substrates 11A and 11B, that is, the cell gap (the thickness of the liquid crystal layer 11C), at a constant level or higher. The spacers 23 are tapered and columnar. For example, a plurality of spacers 23 are arranged at positions overlapping the intersections of the gate wiring 15 and the source wiring 16 of the array substrate 11B. The spacers 23 include a first spacer (main spacer) 23α and a second spacer (sub-spacer) 23β. The first spacer 23α has a larger protruding dimension from the first main surface 11A1 than the second spacer 23β has a larger protruding dimension from the first main surface 11A1.
[0022] In the display area AA of the array substrate 11B constituting the liquid crystal panel 11, as shown in FIG. 4, a pixel circuit section 19, a planarization film 24, a common electrode 25, an interlayer insulating film 26, and a pixel electrode 18 are provided in this order from the bottom. The common electrode 25 is made of a transparent electrode material like the pixel electrodes 18. The common electrode 25 has a size equal to that of the display area AA as a whole. The common electrode 25 is arranged to overlap all the pixel electrodes 18 via the interlayer insulating film 26. A common potential (reference potential) is supplied to the common electrode 25. Therefore, a potential difference based on the potential charged in the pixel electrode 18 can be generated between the common electrode 25 and the pixel electrode 18. The electric field generated based on the potential difference between the common electrode 25 and the pixel electrode 18 includes a fringe electric field (oblique electric field) including a component along the main surface (including the second main surface 11B2 described later) of the array substrate 11B, as well as a component in the normal direction to the main surface of the array substrate 11B. Therefore, the display mode of the liquid crystal panel 11 according to this embodiment is a so-called FFS (Fringe Field Switching) mode in which the alignment state of the liquid crystal contained in the liquid crystal layer 11C is controlled by utilizing a fringe electric field. Note that an alignment film for aligning the liquid crystal contained in the liquid crystal layer 11C is provided on the upper layer side of the pixel electrodes 18 (the innermost surface of the array substrate 11B).
[0023] The interlayer insulating film 26 is made of, for example, silicon nitride (SiN x ), silicon oxide (SiO2), or other inorganic material. The planarization film 24 is made of an organic material, such as acrylic resin (e.g. PMMA), and functions to planarize steps occurring on the layer below the planarization film 24. As shown in FIG. 4, the planarization film 24 has a thickness larger than that of the interlayer insulating film 26, etc., made of an inorganic material. In this embodiment, the surface of the planarization film 24 is the second main surface 11B2 of the array substrate 11B. A plurality of contact holes 24A are opened and provided at positions of the planarization film 24 overlapping with the plurality of pixel electrodes 18. The pixel electrodes 18 are connected to the drain electrodes 17C (see FIG. 3) of the TFTs 17 included in the pixel circuit section 19 through the contact holes 24A. The common electrode 25 and the interlayer insulating film 26 are provided with openings 25A and 26A at positions of the planarization film 24 overlapping with the contact holes 24A, respectively. The openings 25A prevent short circuits between the pixel electrodes 18 and the common electrode 25.
[0024] As shown in FIG. 4, the array substrate 11B is provided with bumps 27 protruding from the second main surface 11B2 toward the counter substrate 11A (first main surface 11A1). The bumps 27 are arranged at positions overlapping the spacers 23 provided on the counter substrate 11A. For example, a plurality of bumps 27 are arranged at positions overlapping the intersections of the gate wiring 15 and the source wiring 16. The bumps 27 include a first bump 27α arranged overlapping the first spacer 23α and a second bump 27β arranged overlapping the second spacer 23β. The protruding dimension of the first bump 27α from the second main surface 11B2 is equal to the protruding dimension of the second bump 27β from the second main surface 11B2. The first bump 27α is always in contact with the overlapping first spacer 23α. In addition, two alignment films are interposed between the overlapping first bump 27α and first spacer 23α. The second bump 27β is not always in contact with the overlapping second spacer 23β. However, when an external force acts on the counter substrate 11A or the array substrate 11B and causes the counter substrate 11A or the array substrate 11B to bend, the second spacer 23β and the second bump 27β come into contact. This allows the counter substrate 11A and the array substrate 11B to bend to a certain extent.
[0025] As shown in FIG. 5, the counter substrate 11A is provided with a first protruding portion 28 that protrudes from the first main surface 11A1 toward the array substrate 11B (second main surface 11B2). The first protruding portion 28 is block-shaped, and the protruding dimension (dimension in the Z-axis direction) from the first main surface 11A1 is, for example, about 2.5 μm, the dimension in the Y-axis direction is, for example, about 9 μm, and the dimension in the X-axis direction is, for example, about 10 μm. The counter substrate 11A is provided with a first extending portion 29 that extends from the first protruding portion 28 along the first main surface 11A1. The extending direction of the first extending portion 29 coincides with the Y-axis direction in FIG. 5. The first extending portion 29 extends from the protruding tip of the first protruding portion 28 as a starting point, and is disposed with a gap between it and the first main surface 11A1. The first extending portion 29 has an extension dimension (dimension in the Y-axis direction) from the first protruding portion 28 of, for example, about 7.5 μm, a thickness dimension (dimension in the Z-axis direction) of, for example, about 0.8 μm, and a dimension in the X-axis direction of, for example, about 10 μm. The gap in the Z-axis direction between the first extending portion 29 and the first main surface 11A1 is, for example, about 1.7 μm.
[0026] On the other hand, the array substrate 11B is provided with a second protruding portion 30 protruding from the second main surface 11B2 toward the counter substrate 11A (first main surface 11A1) side, as shown in FIG. 5. The second protruding portion 30 is disposed at a position spaced apart from the first protruding portion 28 by a distance greater than the extension dimension of the first extension portion 29 in the Y-axis direction. The second protruding portion 30 is block-shaped, and the protruding dimension (dimension in the Z-axis direction) from the second main surface 11B2 is, for example, about 2.5 μm, the dimension in the Y-axis direction is, for example, about 9 μm, and the dimension in the X-axis direction is, for example, about 10 μm. The array substrate 11B is provided with a second extension portion 31 extending from the second protruding portion 30 along the second main surface 11B2. The extension direction of the second extension portion 31 coincides with the Y-axis direction in FIG. 5 and is parallel to the extension direction of the first extension portion 29. The second extension portion 31 extends from the protruding tip of the second protruding portion 30 as a starting point, and is disposed with a gap between it and the second main surface 11B2. The second extension portion 31 extends from the surface of the protruding tip of the second protruding portion 30 facing the first protruding portion 28 toward the first protruding portion 28. The second extension portion 31 has an extension dimension (dimension in the Y-axis direction) from the second protruding portion 30 of, for example, about 7.5 μm, a thickness dimension (dimension in the Z-axis direction) of, for example, about 0.8 μm, and a dimension in the X-axis direction of, for example, about 10 μm. The gap in the Z-axis direction between the second extension portion 31 and the second main surface 11B2 is, for example, about 1.7 μm. In this way, the gap between the second extension portion 31 and the second main surface 11B2 is larger than the thickness dimension of the first extension portion 29. Similarly, the distance between the first extension portion 29 and the first main surface 11A1 is greater than the thickness of the second extension portion 31.
[0027] 5, the first extending portion 29 is sandwiched between the second extending portion 31 and the second main surface 11B2, and the second extending portion 31 is sandwiched between the first extending portion 29 and the first main surface 11A1. Here, for example, when the first main surface 11A1 and the second main surface 11B2 are arranged along the vertical direction, the liquid crystal material constituting the liquid crystal layer 11C accumulates on the lower side in the vertical direction, and therefore stress in a direction moving them away from each other may act on the lower portions of the counter substrate 11A and the array substrate 11B. In this regard, as described above, the first extension portion 29 is sandwiched between the second extension portion 31 and the second main surface 11B2, and the second extension portion 31 is sandwiched between the first extension portion 29 and the first main surface 11A1. Therefore, the first extension portion 29 and the second extension portion 31 are caught by each other, so that the counter substrate 11A and the array substrate 11B are less likely to be displaced relative to each other in a direction away from each other. This makes it possible to keep the distance between the counter substrate 11A and the array substrate 11B from exceeding a certain value, and makes it difficult for the thickness of the liquid crystal layer 11C to become locally large. By keeping the thickness of the liquid crystal layer 11C uniform, the display quality of the image displayed on the liquid crystal panel 11 can be maintained at a good level. The specific arrangement of the first protrusion 28, the first extension portion 29, the second protrusion 30, and the second extension portion 31 in the display area AA can be set arbitrarily. For example, the first protrusion 28, the first extension 29, the second protrusion 30, and the second extension 31 may be disposed near the center of the display area AA, or may be disposed near the outer periphery. Also, when the first main surface 11A1 and the second main surface 11B2 are disposed along the vertical direction, the first protrusion 28, the first extension 29, the second protrusion 30, and the second extension 31 may be disposed in a lower portion of the display area AA in the vertical direction, or may be disposed near the center or upper portion in the vertical direction.
[0028] As shown in FIG. 5, the first protrusion 28, the first extension 29, the second protrusion 30, and the second extension 31 are arranged so as to overlap with the light shielding portion 21 in the display area AA of the liquid crystal panel 11. In detail, the first protrusion 28, the first extension 29, the second protrusion 30, and the second extension 31 are arranged so as to overlap with the portion extending along the Y-axis direction of the light shielding portion 21 that forms a lattice shape in a plan view in the display area AA. That is, the first protrusion 28, the first extension 29, the second protrusion 30, and the second extension 31 are arranged between the pixels PX adjacent to each other in the X-axis direction. In this way, the first protrusion 28, the first extension 29, the second protrusion 30, and the second extension 31 are arranged so as to overlap with the light shielding portion 21, so that the first protrusion 28, the first extension 29, the second protrusion 30, and the second extension 31 are difficult to see from the outside. This makes it possible to maintain good display quality.
[0029] 4 and 5, the first protrusion 28 and the first extension 29 provided on the counter substrate 11A are made of the same material as the spacer 23. Since the first protrusion 28 and the first extension 29 are made of the same material as the spacer 23, the first protrusion 28 and the first extension 29 can be provided in the process of providing the spacer 23 on the counter substrate 11A during manufacturing. The second protrusion 30 and the second extension 31 provided on the array substrate 11B are made of the same material as the bump 27. Since the second protrusion 30 and the second extension 31 are made of the same material as the bump 27, the second protrusion 30 and the second extension 31 can be provided in the process of providing the bump 27 on the array substrate 11B during manufacturing.
[0030] The present embodiment has the above-described structure, and next, a description will be given of a manufacturing method for the liquid crystal panel 11. The manufacturing method for the liquid crystal panel 11 includes a counter substrate manufacturing process (first substrate manufacturing process) for manufacturing the counter substrate 11A, an array substrate manufacturing process (second substrate manufacturing process) for manufacturing the array substrate 11B, and a bonding process for bonding the manufactured counter substrate 11A and array substrate 11B together.
[0031] The counter substrate manufacturing process includes at least a first step of forming the light-shielding portion 21, a second step of forming the color filter 20, a third step of forming the overcoat film 22, and a fourth step of forming the spacer 23, the first protruding portion 28, and the first extending portion 29. The fourth step will be described with reference to Figs. 6 to 8.
[0032] In the fourth step, first, as shown by the two-dot chain line in FIG. 6, a first metal film (first film) F1 made of a metal material (e.g., copper, etc.) is formed on the upper layer side of the overcoat film 22 of the counter substrate 11A. The formed first metal film F1 is patterned by a known photolithography method. Specifically, a photoresist film is formed on the upper layer side of the first metal film F1, and the photoresist film is exposed through a photomask having a predetermined opening pattern. After the exposed photoresist film is developed, the first metal film F1 is etched (e.g., wet-etched) using the developed photoresist film as a mask. Then, the first metal film F1 is patterned, and a first pedestal portion 32 is provided as shown in FIG. 6. The first pedestal portion 32 is block-shaped, and each dimension in the X-axis direction and the Y-axis direction is slightly larger than each dimension in the X-axis direction and the Y-axis direction of the first extension portion 29, respectively.
[0033] Subsequently, as shown by the two-dot chain line in FIG. 7, a first insulating film (second film) F2 is formed on the upper layer side of the first metal film F1. Since the first insulating film F2 is made of a photosensitive organic material (for example, an acrylic resin material, etc.), the first insulating film F2 can be directly exposed through a photomask having a predetermined opening pattern. When the exposed first insulating film F2 is developed, the first insulating film F2 is patterned, and a first protruding portion 28 and a first extending portion 29 are provided as shown in FIG. 7. The provided first extending portion 29 is arranged so as to overlap the upper layer side of the first pedestal portion 32. In association with the patterning of the first insulating film F2, a spacer 23 is also provided (see FIG. 4). Thereafter, the first metal film F1 is etched (for example, wet etching) to remove the first pedestal portion 32 as shown in FIG. 8. In this state, the first extension portion 29 is disposed opposite to the surface of the overcoat film 22, that is, at a position spaced apart by the thickness of the first pedestal portion 32 from the first main surface 11A1.
[0034] The array substrate manufacturing process includes at least a fifth step of forming the pixel circuit portion 19, a sixth step of forming the planarization film 24, a seventh step of forming the common electrode 25, an eighth step of forming the interlayer insulating film 26, a ninth step of forming the pixel electrode 18, and a tenth step of forming the bump 27, the second protrusion 30, and the second extension 31. The tenth step will be described with reference to Figs. 9 to 11.
[0035] In the tenth step, first, as shown by the two-dot chain line in FIG. 9, a second metal film (third film) F3 made of a metal material (e.g., copper, etc.) is formed on the upper layer side of the planarization film 24 in the array substrate 11B. The formed second metal film F3 is patterned by a known photolithography method. Specifically, a photoresist film is formed on the upper layer side of the second metal film F3, and the photoresist film is exposed through a photomask having a predetermined opening pattern. After the exposed photoresist film is developed, the second metal film F3 is etched (e.g., wet-etched) using the developed photoresist film as a mask. Then, the second metal film F3 is patterned, and a second pedestal portion 33 is provided as shown in FIG. The second pedestal portion 33 is block-shaped, and each dimension in the X-axis direction and the Y-axis direction is slightly larger than each dimension in the X-axis direction and the Y-axis direction of the second extension portion 31, respectively.
[0036] 10, a second insulating film (fourth film) F4 is formed on the upper layer side of the second metal film F3. Since the second insulating film F4 is made of an organic material (e.g., an acrylic resin material) having photosensitivity, the second insulating film F4 can be directly exposed through a photomask having a predetermined opening pattern. When the exposed second insulating film F4 is developed, the second insulating film F4 is patterned, and the second protruding portion 30 and the second extending portion 31 are provided as shown in FIG. 10. The provided second extending portion 31 is arranged so as to overlap the upper layer side of the second pedestal portion 33. Along with the patterning of the second insulating film F4, the bump 27 is also provided (see FIG. 4). Thereafter, the second metal film F3 is etched (e.g., wet etching) to remove the second pedestal portion 33 as shown in FIG. 11. In this state, the second extension portion 31 is disposed opposite to the surface of the planarizing film 24, that is, at a position spaced apart by the thickness of the second pedestal portion 33 from the second main surface 11B2.
[0037] The bonding process includes at least an 11th process of applying a sealing portion 11D to the outer peripheral edge of the counter substrate 11A or the array substrate 11B, a 12th process of dropping a liquid crystal material onto the counter substrate 11A or the array substrate 11B, a 13th process of bonding the two substrates 11A and 11B together, and a 14th process of hardening the sealing portion 11D. The 13th process will be described with reference to Figs. 12 to 15.
[0038] In the 13th step, first, as shown in Fig. 12, the counter substrate 11A and the array substrate 11B are arranged so that the first main surface 11A1 and the second main surface 11B2 face each other with a gap larger than the thickness of the liquid crystal layer 11C. At this time, the first protrusion 28 and the first extension 29, and the second protrusion 30 and the second extension 31 are arranged so as not to overlap each other. In this embodiment, the first extension 29 and the second extension 31 are arranged adjacent to each other with a predetermined gap in the Y-axis direction, which is the direction along the first main surface 11A1 and the second main surface 11B2. By relatively displacing the opposing substrate 11A and the array substrate 11B so that they approach each other in the Z-axis direction (the normal direction of each main surface 11A1, 11B2), the distance between the opposing substrate 11A and the array substrate 11B is adjusted, and the first extension portion 29 is positioned between the second main surface 11B2 and the second extension portion 31, and the second extension portion 31 is positioned between the first main surface 11A1 and the first extension portion 29, as shown in FIG. 13.
[0039] Next, the counter substrate 11A and the array substrate 11B are slid in the Y-axis direction, and the first extension portion 29 is sandwiched between the second extension portion 31 and the second main surface 11B2, and the second extension portion 31 is sandwiched between the first extension portion 29 and the first main surface 11A1 (see FIG. 5). According to the liquid crystal panel 11 manufactured in this way, even if the counter substrate 11A and the array substrate 11B are relatively displaced in a direction to separate, the first extension portion 29 and the second extension portion 31 are caught on each other, so that the counter substrate 11A and the array substrate 11B are unlikely to be relatively displaced in a direction to separate. This is suitable for keeping the distance between the counter substrate 11A and the array substrate 11B from being greater than a certain value. When performing the above-mentioned sliding operation, there is a risk that the first extension portion 29 and the second extension portion 31 will interfere with each other. In this regard, in the above-mentioned 10th step, the first extension portion 29 and the second extension portion 31 are provided using the first base portion 32 and the second base portion 33 (see Figures 8 and 11), and the dimensional accuracy of the distance between the first main surface 11A1 and the first extension portion 29, and the distance between the second extension portion 31 and the second main surface 11B2 is made sufficiently high, making it less likely that the first extension portion 29 and the second extension portion 31 will interfere with each other when sliding.
[0040] Furthermore, when performing the sliding operation, there is a risk of variation in the amount of sliding. In this regard, the amount of overlap in the Y-axis direction between the first extension portion 29 and the second extension portion 31, which are in an overlapping relationship with each other, is set to be larger than the variation in the amount of sliding, as shown in FIG. 5. Specifically, the variation in the amount of sliding is set to about ±3 μm, whereas the amount of overlap in the Y-axis direction between the first extension portion 29 and the second extension portion 31 is set to, for example, about 4 μm. Therefore, for example, if the amount of sliding is insufficient by 3 μm, the amount of overlap in the Y-axis direction between the first extension portion 29 and the second extension portion 31 is secured to be about 1 μm, as shown in FIG. On the other hand, if the sliding amount is, for example, 3 μm excessive, as shown in FIG. 15, the overlap amount in the Y-axis direction between the first extension portion 29 and the second extension portion 31 is secured to be approximately 7 μm, and it is possible to avoid a situation in which the first extension portion 29 interferes with the second protrusion portion 30 or the second extension portion 31 interferes with the first protrusion portion 28.
[0041] As described above, the liquid crystal panel (device) 11 of this embodiment includes a counter substrate (first substrate) 11A having a first main surface 11A1, an array substrate (second substrate) 11B having a second main surface 11B2 facing the first main surface 11A1 with a gap therebetween, a first protrusion 28 provided on the counter substrate 11A and protruding from the first main surface 11A1 toward the second main surface 11B2, a first extension 29 extending from the first protrusion 28 along the first main surface 11A1 and arranged with a gap between it and the first main surface 11A1, a second protrusion 30 provided on the array substrate 11B and protruding from the second main surface 11B2 toward the first main surface 11A1, and a second extension 31 extending from the second protrusion 30 along the second main surface 11B2 and arranged so as to sandwich the first extension 29 between the second main surface 11B2 and the second main surface 11B2.
[0042] The second extending portion 31 extending from the second protruding portion 30 along the second main surface 11B2 of the array substrate 11B is disposed between the second main surface 11B2 and the first extending portion 29 extending from the first protruding portion 28 along the first main surface 11A1 of the counter substrate 11A. In this way, even if the counter substrate 11A and the array substrate 11B are relatively displaced in a direction away from each other, the first extending portion 29 and the second extending portion 31 are caught by each other, so that the counter substrate 11A and the array substrate 11B are unlikely to be relatively displaced in a direction away from each other. This is suitable for keeping the distance between the counter substrate 11A and the array substrate 11B from exceeding a certain value.
[0043] In addition, the liquid crystal layer 11C is sandwiched between the counter substrate 11A and the array substrate 11B and is made of a liquid crystal material. For example, when the first main surface 11A1 and the second main surface 11B2 are arranged along the vertical direction, the liquid crystal material constituting the liquid crystal layer 11C accumulates on the lower side in the vertical direction, and therefore stress in a direction moving the counter substrate 11A and the array substrate 11B away from each other may act on the counter substrate 11A and the array substrate 11B. In this regard, the first extension portion 29 and the second extension portion 31 are hooked on each other, making it difficult for the counter substrate 11A and the array substrate 11B to relatively displace in a direction moving away from each other, and therefore it is difficult for the thickness of the liquid crystal layer 11C to become locally large.
[0044] The liquid crystal display further includes a plurality of pixels PX and a light shielding portion 21 arranged between adjacent pixels PX to block light, and the first protrusion 28, the first extension portion 29, the second protrusion 30, and the second extension portion 31 are arranged to overlap with the light shielding portion 21. The light that passes between adjacent pixels PX is blocked by the light shielding portion 21, so that color mixing between the pixels PX is unlikely to occur. The first protrusion 28, the first extension portion 29, the second protrusion 30, and the second extension portion 31 are arranged to overlap with the light shielding portion 21, so that the first protrusion 28, the first extension portion 29, the second protrusion 30, and the second extension portion 31 are unlikely to be visible from the outside. This makes it possible to maintain good display quality.
[0045] The counter substrate 11A is provided with a spacer 23 protruding from the first main surface 11A1 toward the second main surface 11B2, and the array substrate 11B is provided with a bump 27 protruding from the second main surface 11B2 toward the first main surface 11A1 and arranged opposite the spacer 23, the first protruding portion 28 and the first extending portion 29 being made of the same material as the spacer 23, and the second protruding portion 30 and the second extending portion 31 being made of the same material as the bump 27. The spacer 23 and the bump 27 arranged opposite each other can keep the distance between the counter substrate 11A and the array substrate 11B from being smaller than a certain value. Since the first protruding portion 28 and the first extending portion 29 are made of the same material as the spacer 23, the first protruding portion 28 and the first extending portion 29 can be provided in the process of providing the spacer 23 on the counter substrate 11A during manufacturing. Since the second protruding portion 30 and the second extending portion 31 are made of the same material as the bumps 27, the second protruding portion 30 and the second extending portion 31 can be provided in the process of providing the bumps 27 on the array substrate 11B during manufacturing.
[0046] Furthermore, the manufacturing method of the liquid crystal panel 11 according to this embodiment includes providing a first protruding portion 28 protruding from the first main surface 11A1 of the counter substrate 11A, and a first extending portion 29 extending from the first protruding portion 28 along the first main surface 11A1 and disposed at a distance from the first main surface 11A1, and providing a second protruding portion 30 protruding from the second main surface 11B2 of the array substrate 11B, and a second extending portion 31 extending from the second protruding portion 30 along the second main surface 11B2 and disposed at a distance from the second main surface 11B2, The counter substrate 11A and the array substrate 11B are arranged so that the second main surface 11B2 faces the first main surface 11A1 and the first extension portion 29 does not overlap with the second protrusion portion 30 and the second extension portion 31, the distance between the counter substrate 11A and the array substrate 11B is adjusted, the first extension portion 29 is positioned between the second main surface 11B2 and the second extension portion 31, and the counter substrate 11A and the array substrate 11B are slid in a direction along the first main surface 11A1 and the second main surface 11B2, and the first extension portion 29 is sandwiched between the second extension portion 31 and the second main surface 11B2. When bonding the counter substrate 11A provided with the first protrusion 28 and the first extension 29 and the array substrate 11B provided with the second protrusion 30 and the second extension 31, first, the counter substrate 11A and the array substrate 11B are arranged so that the first main surface 11A1 and the second main surface 11B2 face each other and the first protrusion 28 and the first extension 29 do not overlap with the second protrusion 30 and the second extension 31. The distance between the counter substrate 11A and the array substrate 11B is adjusted to position the first extension 29 between the second main surface 11B2 and the second extension 31. Then, the counter substrate 11A and the array substrate 11B are slid in a direction along the first main surface 11A1 and the second main surface 11B2 to sandwich the first extension 29 between the second extension 31 and the second main surface 11B2. In the liquid crystal panel 11 thus manufactured, even if the counter substrate 11A and the array substrate 11B are displaced relative to each other in a direction separating them, the first extending portion 29 and the second extending portion 31 hook together, making it difficult for the counter substrate 11A and the array substrate 11B to displace relative to each other in a direction separating them. This is advantageous in keeping the distance between the counter substrate 11A and the array substrate 11B from exceeding a certain value.
[0047] Furthermore, when providing the first protrusion 28 and the first extension 29 on the counter substrate 11A, a first metal film (first film) F1 is formed on the first main surface 11A1 of the counter substrate 11A, the first metal film F1 is patterned to provide the first pedestal 32, a first insulating film (second film) F2 is formed on the upper layer side of the first metal film F1, the first insulating film F2 is patterned to provide the first protrusion 28 and the first extension 29 overlapping the upper layer side of the first pedestal 32, and the first pedestal 32 is etched away, To provide the second protruding portion 30 and the second extending portion 31 on the array substrate 11B, a second metal film (third film) F3 is formed on the second main surface 11B2 of the array substrate 11B, the second metal film F3 is patterned to provide the second pedestal portion 33, a second insulating film (fourth film) F4 is formed on the upper layer side of the second metal film F3, the second insulating film F4 is patterned to provide the second protruding portion 30 and the second extending portion 31 overlapping the upper layer side of the second pedestal portion 33, and the second pedestal portion 33 is etched and removed. The first metal film F1 formed on the first main surface 11A1 of the counter substrate 11A is patterned to provide the first pedestal portion 32. The first insulating film F2 formed on the upper layer side of the first metal film F1 is patterned to provide the first protruding portion 28 and the first extending portion 29. The first extension 29 overlaps the upper layer side of the first pedestal 32. When the first pedestal 32 is removed by etching, the first main surface 11A1 and the first extension 29 face each other, and a gap for the first pedestal 32 is provided between the first main surface 11A1 and the first extension 29. When the second metal film F3 formed on the second main surface 11B2 of the array substrate 11B is patterned, the second pedestal 33 is provided. When the second insulating film F4 formed on the upper layer side of the second metal film F3 is patterned, the second protrusion 30 and the second extension 31 are provided. The second extension 31 overlaps the upper layer side of the second pedestal 33. When the second pedestal portion 33 is removed by etching, the second main surface 11B2 and the second extending portion 31 face each other, and a gap corresponding to the second pedestal portion 33 is provided between the second main surface 11B2 and the second extending portion 31. By providing the first extending portion 29 and the second extending portion 31 in this manner, the dimensional accuracy of the gap between the first main surface 11A1 and the first extending portion 29 and the gap between the second main surface 11B2 and the second extending portion 31 can be improved.
[0048] <Embodiment 2> A second embodiment will be described with reference to Fig. 16. In this second embodiment, the arrangement of the first protruding portion 128, the first extending portion 129, the second protruding portion 130, and the second extending portion 131 is changed. Note that a duplicated description of the structure, action, and effect similar to those of the first embodiment will be omitted.
[0049] The first protrusion 128, the first extension 129, the second protrusion 130, and the second extension 131 according to this embodiment are arranged so as to overlap with the sealing portion 111D in the non-display area NAA, as shown in FIG. 16. Specifically, the first protrusion 128, the first extension 129, the second protrusion 130, and the second extension 131 are provided in multiples so as to overlap with a portion of the sealing portion 111D having a frame-like planar shape, the portion extending along the X-axis direction, and the portion extending along the Y-axis direction, respectively. In this way, the first protrusion 128, the first extension 129, the second protrusion 130, and the second extension 131 are arranged so as to overlap with the sealing portion 111D, thereby improving the adhesive strength of the sealing portion 111D to the counter substrate 111A and the array substrate 111B.
[0050] As described above, according to this embodiment, the sealing portion 111D is provided between the counter substrate 111A and the array substrate 111B, surrounds the liquid crystal layer 11C, and seals the liquid crystal layer 11C. The first protrusion 128, the first extension 129, the second protrusion 130, and the second extension 131 are arranged so as to overlap with the sealing portion 111D. The liquid crystal layer 11C is sealed by the sealing portion 111D, thereby preventing leakage of the liquid crystal material. The first protrusion 128, the first extension 129, the second protrusion 130, and the second extension 131 are arranged so as to overlap with the sealing portion 111D, thereby improving the adhesive strength of the sealing portion 111D to the counter substrate 111A and the array substrate 111B.
[0051] <Other embodiments> The technology disclosed in this specification is not limited to the embodiments described above and illustrated in the drawings, and the following embodiments, for example, are also included in the technical scope.
[0052] (1) In step 13 included in the manufacturing method of the liquid crystal panel 11, the first extension portions 29, 129 and the second extension portions 31, 131 are arranged adjacent to each other with a predetermined gap therebetween in the X-axis direction, which is a direction along the first main surface 11A1 and the second main surface 11B2 and perpendicular to the extension direction of the first extension portions 29, 129 and the second extension portions 31, 131, and the counter substrates 11A, 111A and the array substrates 11B, 111B may be slid in the X-axis direction.
[0053] (2) The first extending portions 29, 129 and the second extending portions 31, 131 may be provided to extend along the X-axis direction.
[0054] (3) The first protrusions 28, 128, the first extending portions 29, 129, the second protrusions 30, 130, and the second extending portions 31, 131 may be arranged to overlap with portions extending along the X-axis direction of the light-shielding portion 21 that has a lattice shape in a plan view in the display area AA. In this case, the first protrusions 28, 128, the first extending portions 29, 129, the second protrusions 30, 130, and the second extending portions 31, 131 are arranged between the pixels PX adjacent to each other in the Y-axis direction.
[0055] (4) The liquid crystal panel 11 described in embodiment 1 may be combined with the configuration described in embodiment 2 (first protrusion 128, first extension portion 129, second protrusion 130, and second extension portion 131 superimposed on sealing portion 111D).
[0056] (5) In the display area AA, the light blocking portion 21 may be in the form of stripes extending along the Y-axis direction.
[0057] (6) Specific values relating to the dimensions of the first protrusions 28, 128, the first extensions 29, 129, the second protrusions 30, 130, and the second extensions 31, 131 can be changed as appropriate. In addition, specific values relating to the thickness of the liquid crystal layer 11C can also be changed as appropriate.
[0058] (7) The pixel electrode 18 may be located on the lower layer side of the interlayer insulating film 26, and the common electrode 25 may be located on the upper layer side of the interlayer insulating film 26. In that case, it is preferable to form a slit in the common electrode 25 for alignment control.
[0059] (8) The planar shape of the liquid crystal panel 11 may be a horizontally long rectangle, a square, a circle, a semicircle, an oval, an ellipse, a trapezoid, or the like.
[0060] (9) The liquid crystal panel 11 may be of a semi-transmissive or reflective type other than a transmissive type.
[0061] (10) The display mode of the liquid crystal panel 11 may be VA mode, IPS mode, or the like other than FFS mode.
[0062] (11) A device other than the liquid crystal panel 11 may be used. An example of a device other than the liquid crystal panel 11 is an indoor photovoltaic device. The indoor photovoltaic device has a configuration in which a dye and an electrolyte are sandwiched between a first substrate and a second substrate facing each other and sealed with a sealing part. The indoor photovoltaic device has a dye-sensitized solar cell. [Explanation of symbols]
[0063] 11...liquid crystal panel (device), 11A, 111A...opposing substrate (first substrate), 11A1...first main surface, 11B, 111B...array substrate (second substrate), 11B2...second main surface, 11C...liquid crystal layer, 11D, 111D...sealing portion, 21...light shielding portion, 23...spacer, 27...bump, 28, 128...first protrusion, 29, 129...first extension, 30, 130...second protrusion, 31, 131...second extension, 32...first base, 33...second base, F1...first metal film (first film), F2...first insulating film (second film), F3...second metal film (third film), F4...second insulating film (fourth film), PX...pixel
Claims
1. a first substrate having a first major surface; a second substrate having a second main surface facing the first main surface with a gap therebetween; a first protrusion provided on the first substrate and protruding from the first main surface toward the second main surface; a first extension portion extending from the first protruding portion along the first main surface and disposed at a distance from the first main surface; a second protruding portion provided on the second substrate and protruding from the second main surface toward the first main surface; A device comprising: a second extension portion extending from the second protrusion portion along the second main surface and arranged to sandwich the first extension portion between the second protrusion portion and the second main surface.
2. 2. The device of claim 1 further comprising a liquid crystal layer of liquid crystal material sandwiched between said first substrate and said second substrate.
3. A plurality of pixels; a light shielding portion disposed between adjacent pixels to block light, The device according to claim 2 , wherein the first protrusion, the first extension, the second protrusion, and the second extension are arranged to overlap the light blocking portion.
4. a sealing portion interposed between the first substrate and the second substrate, surrounding the liquid crystal layer and sealing the liquid crystal layer; The device according to claim 2 , wherein the first protrusion, the first extension, the second protrusion, and the second extension are arranged to overlap the sealing portion.
5. the first substrate is provided with a spacer protruding from the first main surface toward the second main surface; The second substrate is provided with a bump protruding from the second main surface toward the first main surface and disposed opposite the spacer, the first protruding portion and the first extending portion are made of the same material as the spacer, The device according to claim 2 , wherein the second protruding portion and the second extending portion are made of the same material as the bump.
6. a first protruding portion protruding from a first main surface of a first substrate; and a first extending portion extending from the first protruding portion along the first main surface and disposed at a distance from the first main surface; a second protruding portion protruding from a second main surface of the second substrate; and a second extending portion extending from the second protruding portion along the second main surface and disposed at a distance from the second main surface; The first substrate and the second substrate are arranged such that the first main surface and the second main surface face each other, and the first protruding portion and the first extending portion do not overlap with the second protruding portion and the second extending portion; adjusting a distance between the first substrate and the second substrate, and positioning the first extension portion between the second main surface and the second extension portion; A method for manufacturing a device, comprising sliding the first substrate and the second substrate in a direction along the first main surface and the second main surface, and sandwiching the first extension portion between the second extension portion and the second main surface.
7. When providing the first protruding portion and the first extending portion on the first substrate, a first film is formed on the first main surface of the first substrate, the first film is patterned to provide a first pedestal portion, a second film is formed on an upper layer side of the first film, the second film is patterned to provide the first protruding portion and the first extending portion overlapping the upper layer side of the first pedestal portion, and the first pedestal portion is etched and removed.
7. The device manufacturing method of claim 6, wherein when providing the second protrusion and the second extension on the second substrate, a third film is formed on the second main surface of the second substrate, the third film is patterned to provide a second pedestal, a fourth film is formed on the upper side of the third film, the fourth film is patterned to provide the second protrusion and the second extension overlapping the upper side of the second pedestal, and the second pedestal is etched away.
Citation Information
Patent Citations
Liquid crystal display device
JP2002162632A