Gum base for bubble gum

The gum base composition, devoid of low polymerization vinyl acetate resin and incorporating high polymerization vinyl acetate resin and natural rubber, addresses manufacturing and film stability issues, achieving enhanced inflation volume in bubble gum.

JP2024159225AActive Publication Date: 2024-11-08LOTTE CO LTD
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
JP2023075074
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-28
Publication Date
2024-11-08
Estimated Expiration
2043-04-28

AI Technical Summary

Technical Problem

Conventional bubble gum compositions using vinyl acetate resin with high polymerization degrees face issues with manufacturing suitability and film stability, while those with low polymerization degrees compromise on inflation volume and film strength.

Method used

A gum base composition that excludes vinyl acetate resin with a polymerization degree less than 500 and incorporates vinyl acetate resin with a degree of 750 or more and natural rubber, enhancing manufacturing suitability and film stability.

Benefits of technology

The new composition results in bubble gum with improved manufacturing ease and significantly increased maximum inflation volume, surpassing conventional gum by at least twice the expansion volume.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024159225000001
    Figure 2024159225000001
  • Figure 2024159225000002
    Figure 2024159225000002
Patent Text Reader

Abstract

To provide a bubble gum with enhanced production suitability and film stability over the prior art.SOLUTION: The present invention provides a gum base for a bubble gum characterized by not containing a vinyl acetate resin having a polymerization degree of less than 500 and by containing a natural rubber and a vinyl acetate resin having a polymerization degree of 750 or more.SELECTED DRAWING: None
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a gum base for bubble gum. [Background technology]

[0002] Among chewing gums, so-called "bubble gum" is designed to be inflated and played with, so it needs to have physical properties that make it easy to inflate when blowing into the gum base, which is the residue left over after chewing, and that make it difficult for the balloon shell to burst when inflated.

[0003] Conventionally, compositions mainly made of vinyl acetate resin, which has excellent elasticity and film strength, have been used for bubble gum bases. However, although vinyl acetate resin with a high degree of polymerization (1000 or more) has favorable properties in terms of increasing the film strength when inflated into a balloon, it has problems in terms of manufacturability (mixability of raw materials, fluidity, etc.) and quality (uniformity and stability of film, etc.), so that generally, vinyl acetate resin with a low to medium degree of polymerization (about 400 to 600) is used alone, or vinyl acetate resin with a low degree of polymerization (about 100 to 200) and a medium degree of polymerization (about 500 to 800) is used in combination.

[0004] In response to this, a bubble gum (Patent Document 1) has been proposed in which the maximum expansion volume when inflated into a balloon is increased by 2 to 3 times that of conventional bubble gums by using a mixture of vinyl acetate resins with a high degree of polymerization (1000 to 7000) and a low degree of polymerization (100 to 250). In addition, a gum base composition (Patent Document 2) has been proposed which is non-adhesive by containing a homogeneous premix of vinyl acetate polymers having a molecular weight of about 38,000 to about 94,000 (corresponding to a degree of polymerization of 440 to 1100) and an emulsifier, and a chewing gum composition (Patent Document 3) has been proposed which is made to have both cohesiveness (quality) and fluidity (manufacturability) by using a gum base made of vinyl acetate resin having a molecular weight of about 20,000 or more (corresponding to a degree of polymerization of 290 or more) to which a non-hygroscopic plasticizer has been added, in combination with a cohesive sweetening-weight-increasing component.

[0005] Furthermore, a bubble gum base composition has been proposed that has improved texture and storage stability by combining a mixture of vinyl acetate resins with low molecular weights of about 12,000 to about 16,000 (corresponding to a degree of polymerization of 140 to 190) and medium molecular weights of about 35,000 to about 55,000 (corresponding to a degree of polymerization of 410 to 640), with an elastomer such as synthetic rubber or natural rubber, and an acetylated monoglyceride (Patent Documents 4 and 5). [Prior art documents] [Patent documents]

[0006] [Patent Document 1] Special Publication No. 63-66497 [Patent Document 2] Special Publication No. 3-51382 [Patent Document 3] Japanese Patent Application Laid-Open No. 62-195251 [Patent Document 4] Special Publication No. 3-71098 [Patent Document 5] Japanese Patent Application Publication No. 3-172143 Summary of the Invention [Problem to be solved by the invention]

[0007] As described above, bubble gum is produced by avoiding the use of vinyl acetate resin with a high degree of polymerization (degree of polymerization of 1000 or more) or by compensating for its drawbacks, but the bubble gums produced to date have not been fully satisfactory in terms of manufacturability and film stability. In view of this, the present invention aims to provide a bubble gum that is more manufacturable and has a more stable film than conventional bubble gums. [Means for solving the problem]

[0008] The present invention provides a gum base for bubble gum that does not contain a vinyl acetate resin with a degree of polymerization of less than 500, and contains a vinyl acetate resin with a degree of polymerization of 750 or more and natural rubber, thereby solving the above-mentioned problems. Effect of the Invention

[0009] The bubble gum gum base of the present invention has favorable physical properties in terms of suitability for manufacturing, and when bubble gum is manufactured using the same, the stability of the balloon shell is improved compared to conventional gum bases. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] The bubble gum gum base of the present invention is characterized in that it does not contain a vinyl acetate resin having a degree of polymerization of less than 500, and contains a vinyl acetate resin having a degree of polymerization of 750 or more and natural rubber. It is not a problem if the gum base contains a vinyl acetate resin having a degree of polymerization of 500 or more and less than 750, which is intermediate between the above two types of vinyl acetate resins, and it can even be said that it is preferable for the gum base to contain such a vinyl acetate resin in order to improve the chewing feel.

[0011] Since a polymer such as vinyl acetate resin (polyvinyl acetate) is generally a polydisperse system having a molecular weight distribution, its degree of polymerization is usually expressed as an average degree of polymerization. The average degree of polymerization can be number-average degree of polymerization, weight-average degree of polymerization, viscosity-average degree of polymerization, z-average degree of polymerization, etc., but in the present invention, the weight-average degree of polymerization, which can be measured by gel permeation chromatography (GPC), is adopted.

[0012] Generally, gum base is produced by mixing one or more raw resins. "Not containing vinyl acetate resin with a degree of polymerization less than 500" means that vinyl acetate resin with a weight-average degree of polymerization less than 500 is not used as a raw material of the gum base. "Containing vinyl acetate resin with a degree of polymerization 750 or more" means that vinyl acetate resin with a weight-average degree of polymerization 750 or more is used as a raw material of the gum base. Therefore, the weight-average degree of polymerization (hereinafter simply referred to as "degree of polymerization") of the entire vinyl acetate resin in the gum base of the present invention is 750 or more when only vinyl acetate resin with a degree of polymerization 750 or more is used as a raw material, but it is not necessarily 750 or more when vinyl acetate resin with a degree of polymerization 500 or more but less than 750 is used in combination. However, the degree of polymerization of the entire vinyl acetate resin in the gum base of the present invention is not less than 500.

[0013] Conventional bubble gum gum bases do not contain high-polymerization vinyl acetate resins with a degree of polymerization of 1000 or more, or, if they contain high-polymerization vinyl acetate resins with a degree of polymerization of 1000 or more, they are used in combination with low-polymerization vinyl acetate resins with a degree of polymerization of less than 500 to compensate for the difficulties in manufacturing suitability and balloon shell stability caused by using high-polymerization vinyl acetate resins. However, when low-polymerization vinyl acetate resins are included, although the chewing comfort and ease of inflation are improved, the proportion of high-polymerization vinyl acetate resins that relatively increase shell strength is reduced, which is disadvantageous in increasing the maximum expansion volume (the upper limit of the size that can be inflated into a balloon).

[0014] The bubble gum gum base of the present invention does not contain a low polymerization degree vinyl acetate resin with a degree of polymerization of less than 500, but instead contains natural rubber, which is a high molecular weight material but has smoother physical properties than synthetic rubber. This eliminates the problems with manufacturing suitability and film stability that arise when using a medium to high polymerization degree vinyl acetate resin with a degree of polymerization of 750 or more, and also avoids the problem of reduced film strength that arises when using a low polymerization degree vinyl acetate resin.

[0015] As described above, generally, a high polymerization degree vinyl acetate resin refers to one having a polymerization degree of 1000 or more, a medium polymerization degree vinyl acetate resin refers to one having a polymerization degree of 500 or more but less than 1000, and a low polymerization degree vinyl acetate resin refers to one having a polymerization degree of less than 500. However, the bubble gum gum base of the present invention does not contain a low polymerization degree vinyl acetate resin having a polymerization degree of less than 500, and contains a vinyl acetate resin having a polymerization degree of 750 or more and natural rubber. Therefore, in the following description of this specification, a vinyl acetate resin having a polymerization degree of 750 or more will be referred to as a "high polymerization degree resin", a vinyl acetate resin having a polymerization degree of 500 or more but less than 750 will be referred to as a "medium polymerization degree resin", and a vinyl acetate resin having a polymerization degree of less than 500 will be referred to as a "low polymerization degree resin".

[0016] The gum base for bubble gum of the present invention preferably contains about 4 to 20% by weight of a high polymerization degree resin, and more preferably about 12 to 15% by weight. As described above, the gum base for bubble gum of the present invention preferably contains a medium polymerization degree resin in addition to the high polymerization degree resin. In this case, the medium polymerization degree resin is preferably contained in the gum base at about 0 to 35% by weight, and more preferably at about 10 to 20% by weight. The high polymerization degree resin and the medium polymerization degree resin are preferably contained in the gum base at about 15 to 40% by weight in total.

[0017] The bubble gum base of the present invention contains natural rubber in addition to the high polymerization degree resin (and the medium polymerization degree resin). Natural rubber is a product obtained by refining the sap (latex) of rubber trees through coagulation, washing, dehydration, and drying, and is chemically a high cis-polyisoprene (polyisoprene composed mostly of cis-isoprene monomers).

[0018] The bubble gum gum base of the present invention preferably contains about 2 to 9% by weight of natural rubber, more preferably about 4 to 9% by weight. If the natural rubber content is less than 2% by weight, the effect of adding natural rubber is not exhibited, so improvement in manufacturing suitability cannot be expected, and even if a bubble gum is formed using it, it becomes difficult to inflate a balloon. If the natural rubber content is 4% by weight or more, more preferable manufacturing suitability is obtained, and if a bubble gum is formed using it, it becomes possible to inflate a balloon more smoothly. On the other hand, if the natural rubber content exceeds 9% by weight, the physical properties of the gum become too hard, and the flexible extensibility of the balloon is lost, making it difficult to inflate the balloon to a large size.

[0019] The bubble gum base of the present invention can contain, in addition to vinyl acetate resin and natural rubber, synthetic rubber such as polyisobutylene or polybutene, waxes such as microcrystalline wax or candelilla wax, emulsifiers such as glycerin fatty acid ester or lecithin, fillers such as talc or calcium carbonate, or ester gum, etc. The blending amounts of these additives are usually about 3 to 25% by weight of synthetic rubber, 10 to 25% by weight of waxes, 5 to 25% by weight of emulsifiers, 5 to 30% by weight of fillers, and 0 to 25% by weight of ester gum.

[0020] The bubble gum base of the present invention is used to add and knead typical bubble gum additives such as sugars (sugar, glucose, starch syrup, etc.), sweeteners (xylitol, etc.), flavorings, colorings, etc., and the mixture is passed through an extruder, after which it is cut and molded into plates, blocks, spheres, etc. to produce a bubble gum product.

[0021] The ease of expansion of bubble gum is usually evaluated by a sensory test by a panel consisting of multiple panelists, but it can also be evaluated by measuring the moisture content (wt%) and compression load (kgf) of the gum residue after chewing the gum until the sweetness disappears (usually about 10 to 15 minutes). In general, the higher the moisture content of the gum residue, the smoother the balloon will expand. For bubble gum using the gum base of the present invention, the moisture content suitable for expanding a balloon is preferably 18.0% or more, more preferably 20.0% or more, and even more preferably 22.0% or more. In addition, the higher the compression load of the gum residue, the stronger the film strength and the larger the balloon can be expanded, but if the compression load is too high, an excessive breath pressure is required to inflate the balloon. The maximum compression load is preferably 2.0 kgf or more, more preferably 2.1 kgf or more. It is particularly preferable that the moisture content is 18.0% or more and the maximum compressive load is 2.0 kgf or more.

[0022] The limit of how far a balloon can be inflated when a particular bubble gum is used (maximum expansion volume) can be determined by an inflation test conducted by an experienced panel, but it can be more objectively evaluated by measuring with a device that can optimally adjust the gas pressure and inflow rate. The bubble gum using the gum base of the present invention showed a maximum expansion volume more than twice as large as that of conventional bubble gum under the same conditions, indicating high film stability. EXAMPLES

[0023] Example 1 As the high polymerization resin, we prepared a vinyl acetate resin with a molecular weight of 55,000 to 75,000 (average polymerization degree: approximately 750), as the medium polymerization resin, a vinyl acetate resin with a molecular weight of 47,000 to 57,000 (average polymerization degree: approximately 580), and as the low polymerization resin, a vinyl acetate resin with a molecular weight of 12,000 to 18,000 (average polymerization degree: approximately 180). The gum base was produced by combining the components in the following ratios (unit: weight %) shown in Table 1 using a 3 L heater-equipped kneader and heating and melt-mixing them at 135° C. for 50 minutes. Resin admixtures 29.2 (Low polymerization degree resin: 0.0) (Medium polymerization resin: 15.3) (High polymerization degree resin 13.9) Rubber content 9.0 (Of which, natural rubber 2.3) Other Ingredients Ester gum 24.4 Wax 20.8 Emulsifier 10.0 Filler 6.6 Total 100.0

[0024] (Examples 2-4, Comparative Examples 1-3) A gum base was produced in the same manner as in Example 1, except that the blending ratio of each component was changed as shown in Table 1.

[0025] (Evaluation of Examples 1-4 and Comparative Examples 1-3) <Evaluation of manufacturing suitability> The ease of production when producing the gum bases in Examples 1-4 and Comparative Examples 1-3 was evaluated according to the following criteria. A The raw materials were well compatible and had good manufacturing suitability. B: The raw materials were not sufficiently compatible, the mixture was rough, and the suitability for manufacturing was not very good. C The raw materials were incompatible and could not be manufactured into a gum base. The evaluation results are shown in Table 2.

[0026] <Evaluation of gums using gum base> The gum bases produced in Examples 1-4 and Comparative Examples 1-3 were mixed with 42% gum base, 36% sugar, 13% starch syrup, 4% softener, 2.5% acidulant, 1.3% flavoring, 1% gelatin, 0.1% antioxidant, and 0.1% colorant, respectively, and molded into spheres. After that, a sensory evaluation test and an objective evaluation of the maximum expansion volume, moisture content, and compression load were measured. <Sensory evaluation test> Three panelists were asked to chew gums using the gum bases produced in Examples 1-4 and Comparative Examples 1-3 for three minutes, and then to inflate the chewed gums into balloons and evaluate how large the balloons were using the following five-point scale. The arithmetic mean of the evaluation results of all panelists was calculated to represent the evaluation results. 1 It doesn't inflate at all. 2 It doesn't expand much. 3 It rises quite well. 4 It rises well. 5. Rise extremely well. The results are shown in Table 2.

[0027] <Evaluation of maximum expansion volume (film stability)> Using a test device having a sample attachment part made to simulate the inside of a human mouth, a gas supply part for supplying gas to the sample attachment part, and a flow control part for controlling the flow rate of the gas supplied, the gums using the gum bases produced in Examples 1-4 and Comparative Examples 1-3 were evaluated for film stability by measuring the maximum expansion volume. Specifically, each sample that had been chewed for 10 to 15 minutes was attached to the sample attachment part of the test device, and nitrogen gas was passed through at the optimal flow rate (L / min) confirmed in advance in a preliminary test, and the total flow rate (mL) until the sample no longer expanded was measured. The measurement was performed 10 times for each sample, and the arithmetic average was taken. The results are shown in Table 2.

[0028] <Moisture content measurement> The moisture content of the gums using the gum bases produced in Examples 1-4 and Comparative Examples 1-3 was measured by the following procedure. That is, 3 g of each sample was chewed at a rate of 80 times / min for 15 minutes, and the chewed material was immediately weighed. Next, the chewed material was dried under reduced pressure at 105°C for 1 hour, and the dried chewed material was weighed, and the moisture content was calculated by the following formula. Moisture content (%) = 100 - (dry masticated material weight / masticated material weight x 100) The measurements were carried out three times for each sample, and the arithmetic mean was calculated. The results are shown in Table 2.

[0029] <Compression load measurement> The compressive load of the gums using the gum bases prepared in Examples 1-4 and Comparative Examples 1-3 was measured by the following procedure. That is, 3 g of each sample was chewed at a speed of 80 times / min for 15 minutes, and the chewed material was sandwiched between wax paper and molded to a thickness of 3.2 mm. Then, 20 seconds after the chewed material was removed from the mouth, the compressive load was measured under the following conditions. That is, using an Instron universal testing machine 68SC-05, the sample was compressed with a stainless steel hemispherical plunger with a diameter of 20 mm at a speed of 2 mm / sec and a clearance of 0.3 mm, and after holding for 0.1 seconds, the plunger was raised at a speed of 2 mm / sec to measure the maximum compressive load (kgf). The measurement environment was set to 30°C using a precision air conditioner and a temperature-controlled stage. The measurement was performed three times for each sample, and the arithmetic average was calculated. The results are shown in Table 2.

[0030] [Table 1]

[0031] [Table 2] (-: Unmeasurable) Industrial Applicability

[0032] By using the bubble gum base of the present invention, it is possible to produce a bubble gum which produces a larger bubble than conventional bubble gums.

[0033] [Aspects of the invention] Various aspects of the invention include the following. 1. A gum base for bubble gum, which does not contain vinyl acetate resin having a degree of polymerization of less than 500, and contains vinyl acetate resin having a degree of polymerization of 750 or more and natural rubber. 2. A gum base for bubble gum as described above in 1, containing 12 to 15% by weight of vinyl acetate resin having a degree of polymerization of 750 or more. 3. A gum base for bubble gum according to 1 or 2 above, containing 2 to 9% by weight of natural rubber. 4. A gum base for bubble gum according to 1 or 2 above, containing 4 to 9% by weight of natural rubber. 5. A gum base for bubble gum according to any one of 1 to 4 above, further comprising a vinyl acetate resin having a degree of polymerization of 500 to 750. 6. A gum base for bubble gum according to claim 5, containing 10 to 20% by weight of vinyl acetate resin having a degree of polymerization of 500 to 750. 7. A gum base for bubble gum according to any one of 1 to 6 above, further comprising at least one component selected from the group consisting of synthetic rubbers, waxes, emulsifiers, fillers and ester gums. 8. A bubble gum comprising any one of the bubble gum bases 1 to 7 above and a normal bubble gum component. 9. The bubble gum according to claim 8, having a moisture content of 18% or more after chewing and a maximum compressive load of 2.0 kgf or more.

Claims

1. A gum base for bubble gum, which does not contain a vinyl acetate resin having a degree of polymerization of less than 500, and contains a vinyl acetate resin having a degree of polymerization of 750 or more and natural rubber.

2. 2. The bubble gum base according to claim 1, wherein the vinyl acetate resin having a degree of polymerization of 750 or more is contained in an amount of 12 to 15% by weight.

3. 2. The bubble gum gum base according to claim 1, wherein the natural rubber is contained in an amount of 2 to 9% by weight.

4. 2. The bubble gum gum base according to claim 1, wherein the natural rubber is contained in an amount of 4 to 9% by weight.

5. 2. The bubble gum base according to claim 1, further comprising a vinyl acetate resin having a degree of polymerization of 500 to 750.

6. 6. The bubble gum base according to claim 5, wherein the vinyl acetate resin having a degree of polymerization of 500 to 750 is contained in an amount of 10 to 20% by weight.

7. 2. The bubble gum base according to claim 1, further comprising at least one component selected from the group consisting of synthetic rubbers, waxes, emulsifiers, fillers and ester gums.

8. A bubble gum comprising the bubble gum base according to any one of claims 1 to 7 and conventional bubble gum ingredients.

9. 9. The bubble gum according to claim 8, which has a moisture content after chewing of 18% or more and a maximum compressive load of 2.0 kgf or more.

Citation Information

Patent Citations

  • Chewing gum composition having flow property

    JP1985186249A

  • Decorative bubble gum and its preparation

    JP1986028349A

  • Decorative bubble gum

    JP1986158751A

  • Decorative bubble gum

    JP1986158752A

  • Polyvinyl acetate balloon gum base composition and its production

    JP1987236447A