Method for producing CNF-containing resin molded product
By adding a CNF solution to thermoplastic resin with controlled cellulose nanofiber content, the method improves fiber dispersibility and mechanical strength, addressing uneven properties in conventional cellulose fiber plastics.
Patent Information
- Application Number
- JP2023077508
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-09
- Publication Date
- 2024-11-21
AI Technical Summary
Conventional plastics containing cellulose fibers suffer from poor fiber dispersibility and uneven mechanical properties, leading to decreased toughness and tensile modulus.
A method involving the addition of a CNF solution, where cellulose nanofibers are dispersed in an organic solvent and mixed with a thermoplastic resin, with a controlled addition ratio of 0.1wt% to 4.5wt%, followed by molding to improve dispersibility and mechanical strength.
The method enhances the tensile modulus by 50% or more and maintains elongation at break, resulting in a resin molded article with uniform mechanical properties.
Smart Images

Figure 2024162189000001 
Figure 2024162189000002 
Figure 2024162189000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for producing a CNF-containing resin molded body in which cellulose nanofibers are added to a resin material. [Background technology]
[0002] In the field of plastic molding, fiber-containing plastics, which are formed by adding fibers to resin materials, are well known, and the addition of fibers can improve the mechanical strength and change the appearance compared to resins that do not contain fibers. In addition, various fibers are used as fiber materials, and those using cellulose fibers are also known (for example, see Patent Document 1).
[0003] However, the conventional plastics containing cellulose fibers have poor dispersion of the fibers in the resin, which tends to cause unevenness in the mechanical properties of the molded product as a whole.Furthermore, the addition of cellulose-based fibers tends to significantly reduce the elongation at break, which is a drawback in that the toughness of the resin is significantly impaired. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Special Publication No. 9-505329 DISCLOSURE OF THEINVENTION [Problem to be solved by the invention]
[0005] The present invention aims to solve the problems of the above-mentioned conventional technology, and in summary, to provide a manufacturing method for CNF-containing resin moldings that can improve the mechanical strength, such as the tensile modulus of elasticity, of resin moldings, and further has excellent dispersion of fibers in the resin and uniformity of mechanical properties. [Means for solving the problem]
[0006] As a means of solving the above problems, the inventors added a CNF solution in which cellulose nanofibers were dispersed in an organic solvent to a thermoplastic resin and performed molding, setting the addition ratio of the cellulose fibers to 0.1 wt% to 4.5 wt% of the total molding material (the effects will be described later).
[0007] In this specification, "cellulose nanofiber (CNF)" refers to cellulose microfibrils (single nanofibers) alone, or longitudinally torn, tangled, or aggregates of these with a mesh-like structure, with a width of 3 nm to 100 nm, an aspect ratio of 10 or more, and a length of up to 100 μm.
[0008] Regarding the above-mentioned CNF solution, one that is preferably used is one produced by adding plant fibers or chemical fibers made from plant fibers to an ammonium salt including a quaternary ammonium salt, and then heating the mixture as is or after adding alcohol to defibrate the fibers.
[0009] It is preferable that the CNF-containing resin has a tensile modulus that is at least 50% greater than that of the same resin without CNF.
[0010] In the case of non-foamed resin molded bodies, in order to suppress the occurrence of voids, it is preferable to add a CNF solution to the thermoplastic resin and stir it before molding, and then heat-treat it to volatilize the organic solvent before molding. Effect of the Invention
[0011] The CNF-containing resin molded article of the present invention can improve mechanical properties such as tensile modulus of elasticity of the resin molded article and also suppress a decrease in elongation at break by adding a CNF solution to a resin so that the cellulose nanofiber is added in a predetermined ratio, and molding the resin molded article. In addition, since the cellulose nanofiber is easily dispersed in the resin, a resin molded article with no unevenness in mechanical properties can be produced. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] "Method of manufacturing CNF-containing resin moldings" [1] Basic process An embodiment of the present invention will be described below. First, as a basic manufacturing process, a CNF solution in which cellulose nanofibers (CNF) are dispersed in an organic solvent is added to a thermoplastic resin before or when the resin is put into a resin molding machine, and the resin is molded while being heated and kneaded. At that time, the ratio of CNF added to the resin molding is set to 0.1 wt% to 4.5 wt% of the total amount of molding material.
[0013] This improves the tensile stress and tensile modulus of the resin molded body, and further improves the dispersibility of the CNF to make the physical properties of the molded body uniform. If the CNF addition ratio is less than 0.1 wt%, the effect of improving mechanical properties such as the tensile modulus of elasticity is reduced, and if it exceeds 4.5 wt%, the dispersibility of the CNF is reduced, making the molded body more likely to have uneven physical properties. In addition, the use of the above-mentioned cellulose nanofibers can suppress the decrease in the elongation at break.
[0014] [2] About CNF solution [2-1] Defibration treatment of cellulose nanofibers For the above-mentioned cellulose nanofibers, it is preferable to use ammonium salts including quaternary ammonium salts, to which plant fibers or chemical fibers made from plant fibers are added, and the mixture is heated either as is or after adding alcohol to defibrate the fibers into nano-order sizes.
[0015] [2-1] Raw materials for cellulose nanofiber The plant fibers that are the raw material for the cellulose nanofibers are preferably cotton fibers or chemical fibers made from cotton fibers, and can be cotton, cotton linters, cupra made from cotton linters, etc. In addition, plant fibers other than cotton fibers, such as wood pulp and hemp fibers such as Manila hemp, can also be used as the raw material for the CNFs. Furthermore, these plant fibers can be mixed and used, and discarded cotton products such as clothes and towels can also be used as raw materials.
[0016] Furthermore, after the above-mentioned defibration treatment, a solvent that dissolves in the ammonium salt but does not dissolve the defibrated fibers can be added to separate and recover the defibrated fibers as cellulose nanofibers. The heat treatment during the above-mentioned defibration can also be performed by adding the fibers to an ammonium salt containing a quaternary ammonium salt and heating from a low temperature, but in terms of defibration treatment speed, it is preferable to add the fibers to an ammonium salt containing a quaternary ammonium salt that has been heated to a predetermined temperature. This allows the cellulose nanofibers to be defibrated in a short time, improving production efficiency.
[0017] Furthermore, since the cellulose nanofibers are defibrated by chemical treatment using non-aqueous ionic liquids or solvents, they are compatible with resins (e.g., thermoplastic resins such as polypropylene resin, polyethylene resin, polyvinyl chloride resin, polystyrene resin, polyester resin, and acrylic resin, and thermosetting resins such as phenolic resin, urethane resin, and epoxy resin), and the nanofibers are well dispersed in the resin when mixed with thermoplastic or thermosetting resins and molded.
[0018] [2-2] Ammonium salts including quaternary ammonium salts As the raw material of the ammonium salt including the quaternary ammonium salt, amine and halide can be used, and as the amine, the compound represented by the following [Chemical formula 1] to [Chemical formula 4] shown in the embodiment of Japanese Patent No. 6295495 and Japanese Patent Publication No. 2015-20954 can be preferably used, and as the halide, the benzyl halide represented by the following [Chemical formula 5] can be preferably used. For example, among them, it is preferable to use 1-benzylpyridinium chloride obtained by chemically reacting pyridine and benzyl chloride by heating. In addition, as the raw material of the ammonium salt, those having a skeleton represented by [Chemical formula 6] to [Chemical formula 15] can be appropriately selected or used in combination. The ratio of the amine to the halide in the ammonium salt is not particularly limited, but it is preferable to prepare it in the range of 1 to 650: 1 (preferably 1: 1) in molar ratio. [ka] (In the formula, R1 independently represents hydrogen, a hydroxyl group, a halogen, an alkyl group, an alkenyl group, an alkynyl group, a nitro group, a cyano group, an alkoxycarbonyl group, or an aromatic group.) [ka] [ka] (In the formula, R2, R3, and R4 independently represent hydrogen, a hydroxyl group, a halogen, an alkyl group, an alkenyl group, an alkynyl group, a nitro group, a cyano group, an alkoxycarbonyl group, or an aromatic group.) [ka] [ka] (In the formula, X independently represents a halogen.) [ka] (In the formula, R1, R2, R3, R4, and R5 independently represent hydrogen, a hydroxyl group, a halogen, an alkyl group, an alkenyl group, an alkynyl group, a nitro group, a cyano group, an alkoxycarbonyl group, or an aromatic group.) [ka] (In the formula, R1, R2, R3, and R4 independently represent hydrogen, a hydroxyl group, a halogen, an alkyl group, an alkenyl group, an alkynyl group, a nitro group, a cyano group, an alkoxycarbonyl group, or an aromatic group.) [ka] (In the formula, R1, R2, and R3 independently represent hydrogen, a hydroxyl group, a halogen, an alkyl group, an alkenyl group, an alkynyl group, a nitro group, a cyano group, an alkoxycarbonyl group, or an aromatic group.) [ka] (In the formula, R1, R2, R3, R4, and R5 independently represent hydrogen, a hydroxyl group, a halogen, an alkyl group, an alkenyl group, an alkynyl group, a nitro group, a cyano group, an alkoxycarbonyl group, or an aromatic group.) [ka] (In the formula, R1, R2, R3, and R4 independently represent hydrogen, a hydroxyl group, a halogen, an alkyl group, an alkenyl group, an alkynyl group, a nitro group, a cyano group, an alkoxycarbonyl group, or an aromatic group.) [ka] (In the formula, R1, R2, R3, R4, R5, and R6 independently represent hydrogen, a hydroxyl group, a halogen, an alkyl group, an alkenyl group, an alkynyl group, a nitro group, a cyano group, an alkoxycarbonyl group, or an aromatic group.) [ka] (In the formula, R1, R2, R3, R4, and R5 independently represent hydrogen, a hydroxyl group, a halogen, an alkyl group, an alkenyl group, an alkynyl group, a nitro group, a cyano group, an alkoxycarbonyl group, or an aromatic group.) [ka] (In the formula, R1, R2, and R4 independently represent hydrogen, a hydroxyl group, a halogen, an alkyl group, an alkenyl group, an alkynyl group, a nitro group, a cyano group, an alkoxycarbonyl group, or an aromatic group.) [ka] (In the formula, R1, R2, and R3 independently represent hydrogen, a hydroxyl group, a halogen, an alkyl group, an alkenyl group, an alkynyl group, a nitro group, a cyano group, an alkoxycarbonyl group, or an aromatic group.) [ka] (In the formula, R independently represents hydrogen, a hydroxyl group, a halogen, an alkyl group, an alkenyl group, an alkynyl group, a nitro group, a cyano group, an alkoxycarbonyl group, or an aromatic group.)
[0019] As the ammonium salt including the quaternary ammonium salt, there can be used 1-benzyl-4-(dimethylamino)pyridinium chloride obtained by reacting benzyl chloride with 4-dimethylaminopyridine by heating, N,N,N-triethylbenzeneaminium chloride obtained by reacting benzyl chloride with triethylamine by heating, 1-benzylpyrrolidine hydrochloride obtained by reacting benzyl chloride with pyrrolidine by heating, 1-benzylimidazolium chloride obtained by reacting benzyl chloride with imidazole by heating, and the like.
[0020] When synthesizing the ammonium salt, the synthesis can be performed without using a solvent, but non-aqueous alcohol, ether, acetonitrile, etc. can also be used as a solvent. Regarding the heating when synthesizing the ammonium salt, although it varies depending on the type of amine, the reaction time can be shortened by increasing the reaction temperature. In the case of pyridine and benzyl chloride, it is preferable to react them by heating at a temperature of 120°C to 150°C (preferably 125°C or higher) for 1 to 10 minutes.
[0021] [2-3] Heat treatment in the fiber defibration process Regarding the heat treatment of a mixture of an ammonium salt containing the above-mentioned quaternary ammonium salt and cotton fiber or a chemical fiber made from cotton fiber, it is preferable to carry out the defibration treatment by heating for 5 to 60 minutes (preferably 5 to 40 minutes) at a temperature of 120° C. to 160° C. The heating temperature and reaction time vary depending on the type of ammonium salt and cotton fiber, but when 1-benzylpyridinium chloride and cotton fiber are used, the defibration treatment can be carried out by heating for about 30 minutes.
[0022] [2-4] Separation and recovery of CNF There is no particular limitation on the solvent that dissolves the above ammonium salt but does not dissolve the defibrated fibers. However, when 1-benzylpyridinium chloride is used as the ammonium salt, it is preferable to use an alcohol-based solvent (more preferably methanol) as the solvent. By adding methanol to the ammonium salt containing the defibrated fibers, cellulose nanofibers can be precipitated and recovered by filtration.
[0023] [2-5] Organic solvents As the organic solvent for the CNF solution, methanol is preferably used, but other organic solvents such as alcohol-based organic solvents such as ethanol, ether-based organic solvents, acetonitrile-based organic solvents, ketone-based organic solvents such as acetone, pyridine, toluene, chloroform, etc. can also be used. When adding to polyvinyl chloride resin (PVC resin), a CNF solution in which cellulose nanofibers are dispersed in pyridine can be mixed with a solution in which resin is dispersed in pyridine to volatilize the pyridine, and this can be added to the resin for molding.
[0024] [2-6] CNF content in CNF solution The CNF content of the CNF solution when added to the thermoplastic resin is not particularly limited, but if the CNF content of the CNF solution is too low (too dilute), the amount of volatilization of the organic solvent increases, and if the CNF content is too high (too thick), the viscosity increases and it becomes difficult to mix with the resin, so it is preferable to adjust it in the range of 10 wt% to 30 wt%. In addition, in the case of a non-foamed molded product, if the organic solvent remains in the resin during molding, it will cause voids in the resin molded product, so it is preferable to add the CNF solution to the thermoplastic resin before molding, stir it, and further heat-treat it to volatilize the organic solvent before molding. Furthermore, if a vacuum is drawn in the molding machine, the organic solvent remaining in the resin can also be volatilized.
[0025] [3] Thermoplastic resins The thermoplastic resin to which the CNF solution is added may be any resin that can be used for extrusion molding, injection molding, blow molding, etc., such as polylactic acid resin (PLA resin), polyvinyl chloride resin (PVC resin), polypropylene resin, polyethylene resin, polystyrene resin, polyester resin, acrylic resin, etc. Among these, it is preferable to use a thermoplastic resin with a molding temperature of 180°C or less so that the cellulose nanofibers or organic solvent do not discolor due to heating during molding.
[0026] [4] Mechanical properties of CNF-containing resin moldings Regarding the mechanical properties of the CNF-containing resin molded body, the tensile stress and tensile modulus are greater than those of the same resin not containing CNF. In particular, the tensile modulus can be increased by 50% or more (preferably 60% or more) compared to the same resin not containing CNF. Meanwhile, although the decrease in the elongation at break can be suppressed by using cellulose nanofibers, it is preferable to maintain a value of 50% or more (preferably 80% or more) compared to the same resin not containing CNF.
[0027] [5] Applications of CNF-containing resin molded products The CNF-containing resin molded article may be a non-foamed or foamed article, and may be a final molded article or a pellet. The final molded article can be used for automobile parts by improving the elastic modulus of the resin, and can be used for table tennis rackets and speakers by taking advantage of its high strength. It can also be used for foamed articles such as shoe soles by taking advantage of the foam-stabilizing effect of cellulose nanofibers.
[0028] [6] Final molded products Regarding the final molded product of the CNF-containing resin molded body, the thermoplastic resin and the CNF solution can be mixed and molded into the final molded product in one step, or the final molded product can be produced by first molding into pellets and then molding again. Also, the final molded product can be produced by first molding into a foamed molded product and then molding again to volatilize the organic solvent. EXAMPLES
[0029] Next, a demonstration test of the effect will be described. In this test, polyvinyl chloride resin (PVC resin) and polylactic acid resin (PLA resin) were used as the thermoplastic resin, and CNF solution was added to them and extrusion molding was performed in the same shape to prepare test pieces of Examples 1 to 4. The tensile stress, tensile modulus, elongation at break, and flexural modulus of these test pieces were measured according to JIS K7161.
[0030] "Example 1" In this example, cotton fibers were used as the raw material for cellulose nanofibers, and the cotton fibers were added to an ammonium salt (1-benzylpyridinium chloride) containing a quaternary ammonium salt and heated to perform a fiberization process. The cellulose nanofibers were then separated and collected, dispersed in methanol, and the resulting CNF solution (CNF content: 20 wt%) was added to a polyvinyl chloride resin at 5.0 wt%, and extrusion molding was performed to prepare a test piece so that the cellulose nanofiber content was 1.0 wt% of the total molding material. The mechanical properties of the test piece were measured, and the tensile strength was 39.0 MPa, the tensile modulus was 4.66 GPa, and the elongation at break was 104.3%.
[0031] "Example 2" In this example, the same CNF solution as in Example 1 was added to polyvinyl chloride resin at 10.0 wt%, extrusion molding was performed, and a test piece was prepared so that the ratio of cellulose nanofibers added was 2.0 wt% of the total amount of molding material. The mechanical properties of this test piece were measured, and the results were tensile strength 37.5 MPa, tensile modulus 5.37 GPa, elongation at break 66.4%, and flexural modulus 2.90 GPa.
[0032] "Example 3" In this example, the same CNF solution as in Example 1 was added to polylactic acid resin at 2.5 wt%, extrusion molding was performed, and a test piece was prepared so that the ratio of cellulose nanofibers added was 0.5 wt% of the total amount of molding material. The mechanical properties of this test piece were measured, and the tensile strength was 68.3 MPa and the flexural modulus was 3.65 GPa.
[0033] "Example 4" In this example, wood pulp was used as the raw material for cellulose nanofibers, and cotton fibers were added to ammonium salt (1-benzylpyridinium chloride) containing a quaternary ammonium salt and heated to perform defibration processing. Furthermore, the cellulose nanofibers were separated and collected, dispersed in methanol, and the resulting CNF solution (CNF content 20 wt%) was added to polylactic acid resin at 1.5 wt%, and extrusion molding was performed to prepare a test piece so that the addition ratio of cellulose nanofibers was 0.3 wt% of the total molding material. The mechanical properties of the test piece were measured, and the tensile strength was 71.7 MPa and the flexural modulus was 3.61 GPa.
[0034] "Example 5" In this example, Manila hemp was used as the raw material for cellulose nanofibers, and cotton fibers were added to ammonium salt (1-benzylpyridinium chloride) containing a quaternary ammonium salt and heated to perform defibration processing. Furthermore, this cellulose nanofiber was separated and collected, dispersed in methanol, and the resulting CNF solution (CNF content 20 wt%) was added to polylactic acid resin at 2.5 wt% and extrusion molding was performed, and a test piece was prepared so that the addition ratio of cellulose nanofiber to the total amount of molding material was 0.5 wt%. The mechanical properties of this test piece were measured, and the tensile strength was 69.6 MPa and the flexural modulus was 3.78 GPa.
[0035] "Comparative Example 1" In this comparative example, a test piece was prepared by extrusion molding of a polyvinyl chloride resin without adding a CNF solution. The mechanical properties of the test piece were measured, and the results were tensile strength 37.1 MPa, tensile modulus 2.80 GPa, elongation at break 105.4%, and flexural modulus 2.76 GPa.
[0036] "Comparative Example 2" In this comparative example, a test piece was prepared by extrusion molding of polylactic acid resin without adding CNF solution. The mechanical properties of the test piece were measured, and the tensile strength was 57.3 MPa and the flexural modulus was 3.48 GPa.
[0037] [Summary of the effects of the demonstration test] From the results of Examples 1-2 and Comparative Example 1, it was confirmed that Examples 1-2, in which a CNF solution was added to polyvinyl chloride resin (PVC resin), had a significantly improved tensile modulus and improved tensile strength compared to Comparative Example 1, in which no CNF solution was added. It was also confirmed that the decrease in elongation at break was suppressed. From the results of Examples 3-5 and Comparative Example 2, it was confirmed that Examples 3-5, in which a CNF solution was added to polylactic acid resin, had improved tensile strength and flexural modulus compared to Comparative Example 2, in which no CNF solution was added. The test results are summarized in a table below. [Table 1]
Claims
1. A method for producing a CNF-containing resin molded body, comprising adding a CNF solution in which cellulose nanofibers are dispersed in an organic solvent to a thermoplastic resin and molding the resin, and the addition ratio of the cellulose fibers is 0.1 wt% to 4.5 wt% of the total molding material.
2. The method for producing a CNF-containing resin molding described in claim 1, wherein the CNF solution is produced by adding plant fibers or chemical fibers made from plant fibers to an ammonium salt containing a quaternary ammonium salt, and heating the mixture as is or with the addition of alcohol to defibrate the fibers.
3. The method for producing a CNF-containing resin molded article according to claim 1, wherein the tensile modulus of the CNF-containing resin is at least 50% greater than that of the same resin not containing CNF.
4. The method for producing a CNF-containing resin molded article according to claim 1, wherein the CNF solution is added to the thermoplastic resin and stirred, and the resulting mixture is then heated to volatilize the organic solvent before molding.
Citation Information
Patent Citations
Fine fiber and / or microcrystalline dispersions, especially of cellulose, in organic solvents
JP2003528935A
Composite body of micro cellulose fiber, liquid dispersion of micro cellulose fiber and composite material
JP2011140738A
Method for producing nano-cellulose
JP2013155445A
Method for synthesizing ammonium salt and composition obtained by incorporating polysaccharides into ammonium salt
JP2015020954A
Resin composition and molding
JP2020147637A
Cited By
Automatic bill handling system
US12444263B2