Discharge tube
The discharge tube's innovative design facilitates single-step bonding of cathode and anode sections with thinner regions and recesses, improving manufacturing efficiency and detection accuracy by reducing abnormal discharge.
Patent Information
- Application Number
- JP2023078046
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-10
- Publication Date
- 2024-11-21
AI Technical Summary
The existing discharge tube manufacturing process is complex and prone to unintended discharge, which affects detection accuracy.
The discharge tube design allows for the bonding regions of the cathode and anode sections to be exposed and joined in a single step, with thinner bonding regions and recesses to prevent overlap and reduce abnormal discharge, using laser welding for efficient assembly.
This simplifies the manufacturing process and enhances detection accuracy by reducing man-hours and minimizing abnormal discharge occurrences.
Smart Images

Figure 2024162497000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a discharge tube. [Background technology]
[0002] Patent Document 1 describes a discharge tube for ultraviolet detection that includes an anode part, a cathode part, and a plurality of lead wires connected to the anode part and the cathode part, respectively. When manufacturing the discharge tube described in Patent Document 1, after welding the cathode part to the lead wire, a spacer is placed between the cathode part and the anode part. Thereafter, the anode part is welded to the lead wire, and the spacer is removed. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2012-207971 A Summary of the Invention [Problem to be solved by the invention]
[0004] It is required to simplify the manufacturing process of the above-mentioned discharge tube. It is also required to suppress the occurrence of unintended discharge (abnormal discharge) and to improve the detection accuracy.
[0005] Therefore, the present invention provides a discharge tube that can simplify the manufacturing process of the discharge tube and can improve detection accuracy. [Means for solving the problem]
[0006] The discharge tube of the present invention comprises: [1] "a container filled with a discharge gas; an anode section comprising a plate-like member having an opening and disposed within the container; a cathode section comprising a plate-like member and disposed within the container so as to face the anode section and emitting photoelectrons in response to incidence of light that has passed through the opening; a rod-shaped anode electrode section extending along a direction in which the anode section and the cathode section face each other and joined to the anode section; and a rod-shaped cathode electrode section extending along the direction in which the anode section and the cathode section face each other and joined to the cathode section. and a cathode portion, wherein, in a direction in which the anode portion and the cathode portion face each other, a side where the anode portion is located relative to the cathode portion is defined as one side, and the side opposite to the one side is defined as the other side, the anode electrode portion extends from the anode portion to the other side, and the cathode electrode portion extends from the cathode portion to the other side, and a junction area of the cathode portion with the cathode electrode portion is exposed from the anode portion when viewed from the one side in the direction in which the cathode portion faces each other.
[0007] In this discharge tube, the joint area of the cathode part with the cathode electrode part is exposed from the anode part when viewed from one side in the opposing direction. This makes both the joint area of the cathode part with the cathode electrode part and the joint area of the anode part with the anode electrode part visible from one side in the opposing direction. Therefore, when manufacturing this discharge tube, for example, after positioning the cathode part with respect to the cathode electrode part and positioning the anode part with respect to the anode electrode part, the joining of the cathode part to the cathode electrode part and the joining of the anode part to the anode electrode part can be performed in one process. As a result, the manufacturing process can be simplified compared to the manufacturing method described in the above-mentioned Patent Document 1, in which the anode part is positioned with respect to the anode electrode part after the joining of the cathode part to the cathode electrode part, and then the anode part is joined to the anode electrode part. In addition, in this discharge tube, the joint area of the cathode with the cathode electrode does not overlap with the anode in the opposing direction, so that it is possible to suppress the occurrence of abnormal discharge caused by the joint area overlapping with the anode. Therefore, according to this discharge tube, it is possible to simplify the manufacturing process of the discharge tube and to improve the detection accuracy.
[0008] The discharge tube of the present invention may be [2] "the discharge tube according to [1], in which the joining region is formed thinner than a portion of the cathode part surrounding the joining region." In this case, it is possible to facilitate joining of the cathode part to the cathode electrode part.
[0009] The discharge tube of the present invention may be [3] "the discharge tube according to [2], in which the joining region is formed thinner than the portion surrounding the joining region by forming a recess opening to the one side in the cathode portion." In this case, for example, the recess can be used as a mark during joining, which can facilitate joining of the cathode portion to the cathode electrode portion.
[0010] The discharge tube of the present invention may be [4] "the discharge tube according to any one of [1] to [3], in which the cathode portion has a notch portion formed in an outer edge portion, and the notch portion is exposed from the anode portion when viewed from the one side in the facing direction." In this case, it is possible to suppress the occurrence of abnormal discharge caused by the notch portion overlapping with the anode portion.
[0011] The discharge tube of the present invention may be [5] "the discharge tube according to [4], in which the cathode further has a protruding portion protruding from an inner surface of the notch, and the protruding portion is located within the notch when viewed from the opposing direction." In this case, it is possible to suppress the occurrence of abnormal discharge caused by the protruding portion protruding from the notch. Effect of the Invention
[0012] According to the present invention, it is possible to provide a discharge tube that can simplify the manufacturing process of the discharge tube and improve the detection accuracy. [Brief description of the drawings]
[0013] [Figure 1] FIG. 2 is a perspective view of a discharge tube according to an embodiment. [Diagram 2] FIG. [Diagram 3] FIG. 11 is a plan view of a discharge tube according to a first modified example. [Figure 4] FIG. 13 is a perspective view of a discharge tube according to a second modified example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] Hereinafter, an embodiment of the present invention will be described in detail with reference to the drawings. In the following description, the same or corresponding elements are designated by the same reference numerals, and duplicated description will be omitted.
[0015] As shown in Fig. 1 and Fig. 2, the discharge tube 1 includes a container 10, an anode section 20, a cathode section 30, a pair of anode electrode sections 40, and a pair of cathode electrode sections 50. The anode section 20 and the cathode section 30 are arranged in the container 10 so as to face each other. Hereinafter, the direction in which the anode section 20 and the cathode section 30 face each other is referred to as a direction D1 (facing direction), the side where the anode section 20 is located relative to the cathode section 30 in the direction D1 is referred to as one side S1 (upper side in Fig. 1), and the side where the cathode section 30 is located relative to the anode section 20 in the direction D1 is referred to as the other side S2 (lower side in Fig. 1). The discharge tube 1 is a sensor that detects ultraviolet rays by utilizing the characteristics due to the work function of the cathode section 30. The discharge tube 1 is used for applications such as flame detection, combustion monitoring, discharge detection, and safety devices during hydrogen or ammonia combustion.
[0016] The vessel 10 has a stem 11 and a glass bulb 12. The stem 11 is formed, for example, in the shape of a circular ring plate. An exhaust pipe 13 is connected to the center of the stem 11. The glass bulb 12 is formed, for example, in a substantially cylindrical shape with an end (top) on one side S1 in the direction D1 closed, and an end (bottom) on the other side S2 in the direction D1 joined to the outer edge of the stem 11. This makes the vessel 10 airtightly sealed. A discharge gas 2 is sealed in the vessel 10. The glass bulb 12 is formed, for example, from a material having ultraviolet light transparency. Examples of materials for the glass bulb 12 include borosilicate glass, ultraviolet light transmitting glass, quartz glass, and crystalline materials such as MgF2.
[0017] The anode portion 20 is formed in a flat plate shape from a metal material. The anode portion 20 is formed, for example, in a substantially rhombus shape when viewed from the direction D1. In this example, the anode portion 20 is formed in a substantially rhombus shape with one diagonal longer than the other diagonal, and the longer diagonal is along the direction D2 in which the pair of anode electrode portions 40 face each other. Each corner of the anode portion 20 in a plan view is curved so as not to have a sharp apex. The anode portion 20 is formed, for example, from tungsten, nickel, molybdenum, copper, stainless steel, Kovar metal, or the like.
[0018] In the center of the anode part 20, a plurality of openings 21 (through holes) are formed that penetrate the anode part 20 along the direction D1. Each opening 21 is formed, for example, in a hexagonal shape. The plurality of openings 21 are regularly arranged in a two-dimensional manner at regular intervals. In other words, the anode part 20 has, in its center, a substantially diamond-shaped mesh part formed by the plurality of openings 21 provided along the outer edge part 20a of the anode part 20, and the outer edge part has a frame part that surrounds the mesh part. The shape of the openings 21 may be a polygonal shape other than a hexagonal shape or a circular shape, and the arrangement, size, number, etc. of the openings 21 may be selected from various forms depending on the application.
[0019] A recess 22 is formed at each end of the anode section 20 in the direction D2. In this example, the recess 22 opens to one side S1 in the direction D1 and is formed in a circular shape when viewed from the direction D1. The recess 22 is formed, for example, by half etching, and is formed thinner than a portion of the anode section 20 surrounding the recess 22. In this embodiment, the plate material constituting the anode section 20 has a uniform thickness, so that the recess 22 is formed thinner than a portion of the anode section 20 other than the recess 22 (excluding the opening 21). As will be described later, the anode section 20 is joined to the anode electrode section 40 at the position of the recess 22 on the other side S2 in the direction D1. That is, the recess 22 constitutes a joining region R1 with the anode electrode section 40.
[0020] A plurality of (four in this example) notches 23 are formed in the outer edge 20a of the anode 20. The notches 23 are portions where bridges are formed that connect the anode 20 to a metal member surrounding the anode 20 when the anode 20 is formed, for example, by etching a plate-shaped metal member in a manufacturing process of the anode 20. That is, the notches 23 are a necessary configuration for manufacturing, and are not a configuration that performs any function as an electrode. In this embodiment, no bridges remain in the anode 20. The two notches 23 are arranged so as to face each other on both sides of one recess 22 in a direction perpendicular to the direction D2 when viewed from the direction D1. The remaining two notches 23 are arranged so as to face each other on both sides of the other recess 22 in a direction perpendicular to the direction D2 when viewed from the direction D1. Each notch 23 is formed, for example, in a semicircular shape when viewed from the direction D1.
[0021] The cathode section 30 is formed in a flat plate shape from a metal material. In this example, the cathode section 30 has the same shape as the anode section 20. That is, the cathode section 30 is formed in a substantially rhombus shape when viewed from the direction D1. The cathode section 30 is formed in a substantially rhombus shape with one diagonal longer than the other diagonal, and the longer diagonal is along the direction D3 in which the pair of cathode electrode sections 50 face each other. Each corner of the cathode section 30 in a plan view is curved so as not to have a sharp top. The cathode section 30 is formed from, for example, tungsten, nickel, molybdenum, copper, Kovar metal, or the like.
[0022] Unlike the anode section 20, the cathode section 30 has no opening formed therein. In the discharge tube 1, light that has passed through the opening 21 of the anode section 20 is incident on the surface 30b of the cathode section 30. The surface 30b is a surface (flat surface) on one side S1 in the direction D1 of the cathode section 30, and functions as a photocathode. The surface 30b emits photoelectrons in response to the incidence of light that has passed through the opening 21.
[0023] A recess 32 is formed at each end of the cathode section 30 in the direction D3. In this example, the recess 32 opens to one side S1 in the direction D1 and is formed in a circular shape when viewed from the direction D1. The recess 32 is formed, for example, by half etching, and is formed thinner than the part of the cathode section 30 surrounding the recess 32. In this embodiment, the plate material constituting the cathode section 30 has a uniform thickness, so that the recess 32 is formed thinner than the part of the cathode section 30 other than the recess 32. As will be described later, the cathode section 30 is joined to the cathode electrode section 50 at the position of the recess 32 on the other side S2 in the direction D1. That is, the recess 32 constitutes a joining region R2 with the cathode electrode section 50.
[0024] A plurality of (four in this example) notches 33 are formed in the outer edge portion 30a of the cathode portion 30. The notches 33 have the same configuration as the notches 23, and therefore will not be described here. When viewed from the direction D1, the two notches 33 are arranged to face each other on both sides of one recess 32 in a direction perpendicular to the direction D2. When viewed from the direction D1, the remaining two notches 33 are arranged to face each other on both sides of the other recess 32 in a direction perpendicular to the direction D2. Each notch 33 is formed, for example, in a semicircular shape when viewed from the direction D1.
[0025] The anode electrode portion 40 is a rod-shaped electrode pin (stem pin) that is provided to penetrate the stem 11 and is fixed to the stem 11. The anode electrode portion 40 extends straight from the stem 11 along direction D1. When viewed from direction D1, the pair of anode electrode portions 40 are disposed to face each other in direction D2 across the center of the stem 11. The anode electrode portion 40 is formed of, for example, kovar metal.
[0026] The anode electrode unit 40 is joined to the joining region R1 of the anode unit 20 at an end 40a on one side S1 in the direction D1, and extends from the anode unit 20 to the other side S2 in the direction D1. More specifically, the end 40a is joined to a portion of the surface 20b of the other side S2 in the direction D1 of the anode unit 20 that overlaps with the recess 22 in the direction D1. In this example, the anode electrode unit 40 is joined to the anode unit 20 by laser welding.
[0027] During welding, for example, with the end portion 40a in contact with the anode portion 20 on the other side S2 of the recess 22, laser light is irradiated onto the recess 22 from one side S1 in the direction D1 to melt and solidify at least one of the anode portion 20 and the anode electrode portion 40 in the recess 22, thereby joining the anode portion 20 to the anode electrode portion 40. The heights of the pair of anode electrode portions 40 are the same, and the anode portion 20 is held perpendicular to the direction D1 by the pair of anode electrode portions 40. That is, the anode electrode portion 40 also functions as a holding member that holds the anode portion 20.
[0028] The cathode electrode portion 50 is a rod-shaped electrode pin (stem pin) that is provided to penetrate the stem 11 and is fixed to the stem 11. The cathode electrode portion 50 extends straight from the stem 11 along direction D1. When viewed from direction D1, the pair of cathode electrode portions 50 are disposed to face each other in direction D3 across the center of the stem 11. The cathode electrode portion 50 is formed of, for example, kovar metal.
[0029] The cathode electrode portion 50 is joined to the joining region R2 of the cathode portion 30 at an end 50a on one side S1 in the direction D1, and extends from the cathode portion 30 to the other side S2 in the direction D1. More specifically, the end 50a is joined to a portion of the surface 30c of the other side S2 in the direction D1 of the cathode portion 30 that overlaps with the recess 32 in the direction D1. In this example, the cathode electrode portion 50 is joined to the cathode portion 30 by laser welding.
[0030] During welding, for example, while the end 50a is in contact with the cathode portion 30 on the other side S2 of the recess 32, a laser beam is irradiated from one side S1 in the direction D1 to the recess 32, and at least one of the cathode portion 30 and the cathode electrode portion 50 is melted and solidified in the recess 32, thereby joining the cathode portion 30 to the cathode electrode portion 50. The heights of the pair of cathode electrode portions 50 are the same, and the pair of cathode electrode portions 50 hold the cathode portion 30 perpendicular to the direction D1 and parallel to the anode portion 20. That is, the cathode electrode portion 50 also functions as a holding member that holds the cathode portion 30. As described above, the anode portion 20 is located on one side S1 in the direction D1 with respect to the cathode portion 30. Therefore, the height of the pair of anode electrode portions 40 is set higher than the height of the pair of cathode electrode portions 50.
[0031] In the discharge tube 1, a joint region R2 of the cathode section 30 with the cathode electrode section 50 is exposed from the anode section 20 when viewed from one side S1 in the direction D1. That is, the anode section 20 is not disposed on one side S1 of the joint region R2, and the joint region R2 does not overlap with the anode section 20 in the direction D1. In addition, when viewed from one side S1 in the direction D1, the notch section 23 of the anode section 20 is exposed from the cathode section 30, and the notch section 33 of the cathode section 30 is exposed from the anode section 20.
[0032] The operation of the discharge tube 1 will be described. In a use state, a voltage is applied between the anode section 20 and the cathode section 30 via the anode electrode section 40 and the cathode electrode section 50. In a use state, when ultraviolet light is incident on the cathode section 30 (surface 30b) via the container 10 (glass bulb 12) and the opening 21 of the anode section 20, photoelectrons are emitted from the cathode section 30. These photoelectrons are attracted to the anode section 20 and collide with discharge gas molecules in the container 10 to ionize the discharge gas molecules. Of the electrons and positive ions generated by the ionization, the electrons further collide with other discharge gas molecules and ionize them repeatedly to reach the anode section 20. On the other hand, the positive ions are accelerated toward the cathode section 30 and collide with the cathode section 30 to generate many secondary electrons. By repeating the above phenomenon, a current flows between the anode section 20 and the cathode section 30, and a discharge state is established. In the discharge tube 1, this discharge phenomenon is utilized to detect light in the ultraviolet region. [Effects]
[0033] In the discharge tube 1, a joint region R2 of the cathode section 30 with the cathode electrode section 50 is exposed from the anode section 20 when viewed from one side S1 in the direction D1 (opposing direction). As a result, both the joint region R2 of the cathode section 30 with the cathode electrode section 50 and the joint region R1 of the anode section 20 with the anode electrode section 40 are visible from the one side S1 in the direction D1. Therefore, when manufacturing the discharge tube 1, for example, after positioning the cathode section 30 with respect to the cathode electrode section 50 and positioning the anode section 20 with respect to the anode electrode section 40, a laser beam for laser welding is irradiated from the one side S1 in the direction D1, thereby joining the cathode section 30 to the cathode electrode section 50 and joining the anode section 20 to the anode electrode section 40 in one process. As a result, the manufacturing process can be simplified compared to the manufacturing method described in the above-mentioned Patent Document 1, in which the anode section 20 is positioned relative to the anode electrode section 40 after the cathode section 30 is joined to the cathode electrode section 50, and then the anode section 20 is joined to the anode electrode section 40. This can reduce the number of steps in the manufacturing process, making it possible to mass-produce the discharge tube 1. In addition, in the discharge tube 1, the joining region R2 of the cathode section 30 with the cathode electrode section 50 does not overlap with the anode section 20 in the direction D1, so that the occurrence of abnormal discharge caused by the joining region R2 overlapping with the anode section 20 can be suppressed. Therefore, according to the discharge tube 1, the manufacturing process of the discharge tube can be simplified and the detection accuracy can be improved. Furthermore, in the discharge tube 1, since the anode portion 20 and the cathode portion 30 are made of flat plate-shaped members, the number of processes that may involve deformation of the members can be reduced compared to, for example, when the anode portion and the cathode portion have bent portions, and therefore the accuracy of the spacing between the anode portion 20 and the cathode portion 30 can be improved.
[0034] The joining region R2 is formed thinner than the portion of the cathode section 30 surrounding the joining region R2. This makes it possible to easily join the cathode section 30 to the cathode electrode section 50. For example, when joining the cathode section 30 to the cathode electrode section 50 by laser welding, the joining region R2 is formed thinner than the portion of the cathode section 30 surrounding the joining region R2, so that laser welding can be performed using a laser beam with a lower output than when the joining region R2 is not formed thinner. This makes it possible to easily join the cathode section 30 to the cathode electrode section 50. In addition, the joining region R1 is formed thinner than the portion of the anode section 20 other than the joining region R1, so that it makes it possible to easily join the anode section 20 to the anode electrode section 40.
[0035] The joining region R2 is formed thinner than the portion surrounding the joining region R2 by forming the recess 32 opening to one side S1 in the cathode portion 30. In this case, for example, the recess 32 can be used as a mark, and the joining of the cathode portion 30 to the cathode electrode portion 50 can be facilitated. For example, when the joining of the cathode portion 30 to the cathode electrode portion 50 is performed by laser welding from one side S1 of the cathode portion 30, the recess 32 serves as a mark for the welding portion, so the welding portion can be more easily identified than when the recess 32 is not present. Therefore, the joining of the cathode portion 30 to the cathode electrode portion 50 can be facilitated. In addition, since the recess 32 is formed to open to one side S1, the joining region R2 is separated from the anode portion 20 in the direction D1 more than the portion other than the joining region R2. Therefore, even if the joining region R2 is deformed or the like by the joining, the distance from the anode portion 20 in the direction D1 can be suppressed from becoming small. Therefore, the possibility of discharge caused by the bonding region R2 can be reduced. In addition, the bonding region R1 is formed thinner than the portion other than the bonding region R1 by forming the recess 22 opening to one side S1 in the anode part 20. In this case, the recess 22 can be used as a marker, and the bonding of the anode part 20 to the anode electrode part 40 can be facilitated.
[0036] The cathode section 30 has a notch 33 formed in the outer edge section 30a, and the notch 33 is exposed from the anode section 20 when viewed from one side S1 in the direction D1. This makes it possible to suppress the occurrence of abnormal discharge caused by the notch 33 overlapping with the anode section 20. That is, when the notch 33 overlaps with the anode section 20, abnormal discharge may occur between the notch 33 and the anode section 20, but the cathode section 30 in this embodiment makes it possible to suppress the occurrence of such abnormal discharge. In addition, the anode section 20 has a notch 23 formed in the outer edge section 20a, and the notch 23 is exposed from the cathode section 30 when viewed from the other side S2 in the direction D1. This makes it possible to suppress the occurrence of abnormal discharge caused by the notch 23 overlapping with the cathode section 30. [Variations]
[0037] 3, the anode 20 has a protrusion 24 protruding from the inner surface of the cutout 23. The protrusion 24 is a burr that is generated, for example, when the anode 20 is separated from a metal member in a manufacturing process of the anode 20, and is a part of the above-mentioned bridge portion that remains in the anode 20. When viewed from the direction D1, the protrusion 24 is located within the cutout 23. That is, when viewed from the direction D1, the protrusion 24 is located more inward than the outer edge 20a of the anode 20 (the outer edge when it is assumed that the cutout 23 is not formed).
[0038] Further, the cathode portion 30 has a protrusion 34 protruding from the inner surface of the cutout portion 33. The protrusion 34 is a burr that is generated, for example, when the cathode portion 30 is separated from a metal member in the manufacturing process of the cathode portion 30, and is a part of the above-mentioned bridge portion that remains in the cathode portion 30. When viewed from the direction D1, the protrusion 34 is located within the cutout portion 33. In other words, when viewed from the direction D1, the protrusion 34 is located more inward than the outer edge portion 30a of the cathode portion 30 (the outer edge when it is assumed that the cutout portion 33 is not formed).
[0039] In the first modified example, the protruding portion 34 is located within the cutout portion 33 when viewed from the direction D1. This makes it possible to suppress the occurrence of abnormal discharge caused by the protruding portion 34 protruding from the cutout portion 33. In other words, if the protruding portion 34 is not located within the cutout portion 33, abnormal discharge may occur between the protruding portion 34 and the anode portion 20, but according to the first modified example, the occurrence of such abnormal discharge can be suppressed.
[0040] The discharge tube 1 may be configured as a second modified example shown in FIG. 4. In FIG. 4, the glass bulb 12 is omitted. In the second modified example, the anode section 20 and the cathode section 30 are formed in a substantially triangular shape when viewed from the direction D1. Three anode electrode sections 40 are joined to the anode section 20, and the anode section 20 has three joining regions R1. The anode section 20 also has six notches 23. Similarly, three cathode electrode sections 50 are joined to the cathode section 30, and the cathode section 30 has three joining regions R2. The cathode section 30 also has six notches 33. In the second modified example, the joining region R2 of the cathode section 30 with the cathode electrode section 50 is exposed from the anode section 20 when viewed from one side S1 in the direction A. According to the second modified example, the manufacturing process of the discharge tube can be simplified and the detection accuracy can be improved, as in the above embodiment.
[0041] The present invention is not limited to the above-described embodiment and modified examples. For example, the materials and shapes of the components are not limited to those described above, and various materials and shapes can be adopted.
[0042] In the above embodiment, the cathode electrode section 50 is joined to the surface 30c of the other side S2 of the cathode section 30, but the cathode electrode section 50 may be joined to the surface 30b of one side S1 of the cathode section 30. For example, the cathode electrode section 50 may be disposed so as to penetrate the cathode section 30, and the protruding portion from the cathode section 30 may be joined to the surface 30b of one side S1 of the cathode section 30. That is, the cathode electrode section 50 may be joined to either the surface 30b of one side S1 of the cathode section 30 or the surface 30c of the other side S2. However, it is preferable that the cathode electrode section 50 is joined to the surface 30c of the other side S2 of the cathode section 30 as in the above embodiment from the viewpoint of suppressing abnormal discharge, etc. Similarly, the anode electrode unit 40 may be joined to the surface of one side S1 of the anode unit 20, or may be joined to either the surface of one side S1 or the surface 20b of the other side S2 of the anode unit 20. In addition, the cathode electrode unit 50 and the cathode unit 30, and the anode electrode unit 40 and the anode unit 20 may be connected by indirect joining using a joining material such as brazing material, without being limited to direct joining by welding or the like.
[0043] The cathode section 30 may not have a recess 32, and the cathode section 30 may have the same thickness throughout. The anode section 20 may not have a recess 22, and the anode section 20 may have the same thickness throughout. The recess 32 of the cathode section 30 may be formed so as to open to the other side S2. The recess 22 of the anode section 20 may be formed so as to open to the other side S2. The cutout section 33 of the cathode section 30 may overlap with the anode section 20 when viewed from one side S1 in the direction D1. The cathode section 30 may not have a cutout section 33. The anode section 20 may not have a cutout section 23. In the first modification, the protrusion section 34 of the cathode section 30 may have a portion located outside the cutout section 33 when viewed from the direction D1. In the first modification, the protruding portion 24 of the anode assembly 20 may have a portion located outside the cutout portion 33 when viewed from the direction D1. [Explanation of symbols]
[0044] 1...discharge tube, 10...container, 20...anode portion, 21...opening, 30...cathode portion, 30a...outer edge portion, 32...recess, 33...notch portion, 34...protrusion, 40...anode electrode portion, 50...cathode electrode portion, D1...direction (facing direction), R2...joint area.
Claims
1. A container in which a discharge gas is sealed; an anode portion that is made of a plate-like member having an opening and that is disposed within the container; a cathode section made of a plate-like member, disposed within the container so as to face the anode section, and emitting photoelectrons in response to incidence of light that has passed through the opening; a rod-shaped anode electrode portion extending along a direction in which the anode portion and the cathode portion face each other and joined to the anode portion; a rod-shaped cathode electrode portion extending along the opposing direction and joined to the cathode portion; a side where the anode section is located relative to the cathode section in a direction in which the anode section and the cathode section face each other is defined as one side, and a side opposite to the one side is defined as the other side, the anode electrode section extends from the anode section to the other side, and the cathode electrode section extends from the cathode section to the other side, a joint region of the cathode portion with the cathode electrode portion is exposed from the anode portion when viewed from the one side in the opposing direction.
2. 2. The discharge tube according to claim 1, wherein the junction region is formed to be thinner than a portion of the cathode portion surrounding the junction region.
3. 3. The discharge tube according to claim 2, wherein the joint region is formed thinner than the portion surrounding the joint region by forming a recess that opens to the one side in the cathode portion.
4. the cathode portion has a notch formed on an outer edge thereof, 3. The discharge tube according to claim 1, wherein the cutout portion is exposed from the anode portion when viewed from the one side in the opposing direction.
5. The cathode portion further includes a protrusion protruding from an inner surface of the cutout portion, The discharge tube according to claim 4 , wherein the protruding portion is located within the notch portion when viewed from the opposing direction.
Citation Information
Patent Citations
Flame sensor and method for manufacturing the same
JP2012207971A
Cited By