Input-output device

A novel input/output device configuration with overlapping electrodes and an oxide semiconductor transistor reduces thickness and weight, enhancing detection sensitivity and reliability while lowering manufacturing costs.

JP2024163238AActive Publication Date: 2024-11-21SEMICON ENERGY LAB CO LTD
View PDF 12 Cites 0 Cited by

Patent Information

Application Number
JP2024151718
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2015-05-29
Filing Date
2024-09-03
Publication Date
2024-11-21
Estimated Expiration
2036-05-20

AI Technical Summary

Technical Problem

Existing input/output devices are bulky, heavy, and have a large number of components, which limits their integration into thinner and more compact electronic devices.

Method used

The input/output device incorporates a novel configuration with a first and second pixel electrode, a first and second common electrode, and a transistor with an oxide semiconductor channel, where the electrodes are connected through insulating films and overlap to reduce thickness and weight, and includes a capacitive sensing element for touch detection.

Benefits of technology

This configuration results in a thinner, lighter, and more reliable input/output device with enhanced detection sensitivity and reduced manufacturing costs, allowing for integration into various electronic devices.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024163238000001_ABST
    Figure 2024163238000001_ABST
Patent Text Reader

Abstract

To provide an input-output device with high reliability and smaller thickness.SOLUTION: An input-output device includes a first pixel electrode, a second pixel electrode, a first common electrode, a second common electrode, a liquid crystal, a first insulating film, a second insulating film, and a transistor. The first common electrode functions as one electrode of a detection element. The second common electrode functions as the other electrode of the detection element. The transistor includes a first gate, a second gate, and a semiconductor layer. The pixel electrode, the common electrode, and the second gate exist on different surfaces. The second gate includes one or more kinds of metal elements included in the semiconductor layer. Preferably, the second gate, the pixel electrode, and the common electrode contain one or more kinds of metal elements included in the semiconductor layer.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] One embodiment of the present invention relates to an input / output device and an electronic device.

[0002] Note that one embodiment of the present invention is not limited to the above technical field. The technical field of one embodiment is a semiconductor device, a display device, a light-emitting device, a power storage device, a memory device, Child devices, lighting devices, input devices (e.g., touch sensors), output devices, input / output devices (e.g., For example, touch panels, driving methods thereof, or manufacturing methods thereof. Some examples include: [Background technology]

[0003] It is used in many flat panel displays, such as liquid crystal displays and light-emitting displays. The transistors used are made of amorphous silicon and single crystal silicon formed on a glass substrate. The silicon semiconductor is made of silicon, such as polycrystalline silicon or polysilicon. Transistors, which use semiconductors, are also used in integrated circuits (ICs).

[0004] In recent years, metal oxides that exhibit semiconducting properties have been used in transistors instead of silicon semiconductors. In this specification, metal oxides that exhibit semiconducting properties are referred to as oxide semiconductors. For example, Patent Documents 1 and 2 describe the following as oxide semiconductors: A transistor using zinc oxide or In-Ga-Zn oxide is manufactured, and the transistor A technique for using a semiconductor device as a switching element for pixels of a display device has been disclosed.

[0005] In addition, the display device is provided with a user interface that allows input by touching the screen with a finger or the like. There is a demand for touch panels with added functions.

[0006] A display device or a display module equipped with a touch sensor is called a touch panel or a touch screen. Also, devices that have touch sensors but no display elements are called It is sometimes called a touch panel. Therefore, a display device or display device equipped with a touch sensor The modules are used as display devices with touch sensors, display devices with touch panels, and display devices with touch panels. In the following, the term "touch panel" is used. A display device equipped with a touch sensor will be referred to as a touch panel.

[0007] For example, Patent Documents 3 to 6 disclose touch panels using liquid crystal elements as display elements. It has been disclosed. [Prior art documents] [Patent documents]

[0008] [Patent Document 1] JP 2007-123861 A [Patent Document 2] JP 2007-96055 A [Patent Document 3] JP 2011-197685 A [Patent Document 4] JP 2014-44537 A [Patent Document 5] JP 2014-178847 A [Patent Document 6] US Patent Application Publication No. 2008 / 0158183 Summary of the Invention [Problem to be solved by the invention]

[0009] An object of one embodiment of the present invention is to reduce the thickness of an input / output device. Another object of the present invention is to reduce the weight of an input / output device. One object is to provide an output device.

[0010] Another object of one embodiment of the present invention is to provide a highly reliable input / output device. Another object of one embodiment of the present invention is to provide an input / output device with high detection sensitivity. Another object of one embodiment of the present invention is to provide a novel input / output device or the like.

[0011] The description of these problems does not preclude the existence of other problems. It is not necessary for the embodiment to solve all of these problems. It is possible to extract other problems from the description of the claims, etc. [Means for solving the problem]

[0012] One aspect of the present invention is a liquid crystal display device including a first pixel electrode, a second pixel electrode, a first common electrode, and a second common electrode. The input / output device includes a liquid crystal, a first insulating film, a second insulating film, and a transistor. The first common electrode can function as one electrode of the sensing element. The second common electrode can , which can serve as the other electrode of the sensing element. The semiconductor layer includes a second gate and a semiconductor layer. The semiconductor layer includes an oxide semiconductor in a channel formation region. The second gate includes an oxide conductor. The oxide conductor is included in an oxide semiconductor. The input / output device of one embodiment of the present invention has a first gate having one or more metal elements. A semiconductor layer is provided, a second gate is provided on the semiconductor layer, and a first insulating film is provided on the second gate. a first pixel electrode, a second pixel electrode, a first common electrode, and a The first pixel electrode and the first common electrode are mutually connected via a second insulating film. The second pixel electrode and the second common electrode are provided with a second insulating film therebetween. The first pixel electrode, the second pixel electrode, the first common electrode, and the second pixel electrode have overlapping portions. The first pixel electrode and the second pixel electrode are disposed on the same surface. The first common electrode and the second common electrode are located on the same plane and spaced apart from each other.

[0013] At least one of the display unit and the driver circuit unit includes the above transistor. According to one embodiment of the present invention, there is provided an input / output device including two of the above-described transistors. In one, the source or drain is electrically connected to the first pixel electrode, and in the other Alternatively, the source or drain may be electrically connected to the second pixel electrode. The transistor may be located in the drive circuitry.

[0014] Alternatively, in each of the above configurations, the second gate is electrically connected to the first gate. Good too.

[0015] Alternatively, in each of the above configurations, a second insulating film is formed on the first pixel electrode and the second pixel electrode. and a first common electrode and a second common electrode may be provided on the second insulating film. In each of the above configurations, a second insulating film is provided on the first common electrode and the second common electrode. A first pixel electrode and a second pixel electrode may be provided on the second insulating film.

[0016] Alternatively, in each of the above configurations, the first pixel electrode and the second pixel electrode are each made of an oxide. The first common electrode may include at least one metal element contained in the semiconductor. and the second common electrode each have at least one metal element contained in an oxide semiconductor. It is okay to do so.

[0017] Alternatively, in each of the above structures, the oxide semiconductor and the oxide conductor may each be made of indium. Furthermore, the first pixel electrode and the second pixel electrode may have an oxide containing Each of the first common electrode and the second common electrode may have an oxide containing indium. The common electrodes may each include an oxide containing indium.

[0018] Alternatively, in each of the above structures, the oxide semiconductor and the oxide conductor are each In-M1 -Zn oxide (M1 is Al, Ti, Ga, Y, Zr, La, Ce, Nd, Sn or Hf) Further, the first pixel electrode and the second pixel electrode may each have the above-mentioned I The first common electrode and the second common electrode may further include n-M1-Zn oxide. may each have the In-M1-Zn oxide.

[0019] Alternatively, in each of the above configurations, the first pixel electrode, the second pixel electrode, the first common electrode, and Each of the second common electrodes may have a function of transmitting visible light.

[0020] Alternatively, in each of the above configurations, a first conductive film is provided between the first insulating film and the first common electrode. The resistivity of the first conductive film is lower than the resistivity of the first common electrode. The first insulating film may be electrically connected to the first common electrode. a second conductive film having a resistivity lower than that of the second common electrode; The second conductive film is electrically connected to the second common electrode, and the first conductive film and the second conductive film are , may be spaced apart on the same plane.

[0021] Alternatively, in each of the above structures, a light-shielding film is provided, and the light-shielding film is the first conductive film or the second conductive film. The liquid crystal layer may have a portion overlapping with at least one of the above through liquid crystal.

[0022] In addition, one embodiment of the present invention is a method for manufacturing the input / output device, comprising: ed circuit) or TCP (Tape Carrier Package) Modules with connectors such as , or COG (Chip On Glass) Modules in which ICs are mounted using the COF (Chip On Film) method, etc. etc.

[0023] Alternatively, one aspect of the present invention is a semiconductor device including the above module, an antenna, a battery, a housing, and a speaker. , a microphone, an operation switch, or an operation button, It is. Effect of the Invention

[0024] According to one embodiment of the present invention, the input / output device can be made thinner. In addition, according to one embodiment of the present invention, the number of components can be reduced. It is possible to provide a simple input / output device.

[0025] According to one embodiment of the present invention, a highly reliable input / output device can be provided. According to one embodiment of the present invention, an input / output device with high detection sensitivity can be provided. According to one embodiment of the present invention, a novel input / output device or the like can be provided.

[0026] The description of these effects does not preclude the existence of other effects. An embodiment does not necessarily have all of these effects. It is possible to extract other effects from the descriptions in the sections etc. [Brief description of the drawings]

[0027] [Figure 1] 1A and 1B are a top view and a cross-sectional view illustrating an example of an input / output device. [Diagram 2] FIG. 1 is a cross-sectional view showing an example of an input / output device. [Diagram 3] FIG. 1 is a cross-sectional view showing an example of an input / output device. [Figure 4] FIG. 1 is a cross-sectional view showing an example of an input / output device. [Diagram 5] FIG. 1 is a cross-sectional view showing an example of an input / output device. [Figure 6] FIG. 1 is a cross-sectional view showing an example of an input / output device. [Figure 7] FIG. 2 is a diagram showing an example of a detector element and a pixel. [Figure 8] 1A and 1B are diagrams showing an example of the operation of a detector element and a pixel. [Figure 9] FIG. 2 is a top view showing an example of a detector element and a pixel. [Figure 10] FIG. 4 is a top view showing an example of a sensing element. [Figure 11] FIG. 4 is a top view showing an example of a sensing element. [Figure 12] FIG. 2 is a top view showing an example of an input / output device. [Figure 13] FIG. 2 is a top view showing an example of an input / output device. [Figure 14] FIG. 2 is a top view showing an example of an input / output device. [Figure 15] FIG. 1 is a block diagram showing an example of a touch panel module. [Figure 16] FIG. 1 is a diagram showing an example of a touch panel module. [Figure 17] 1A to 1C are cross-sectional views illustrating an example of a manufacturing method of a transistor or the like. [Figure 18]1A to 1C are cross-sectional views illustrating an example of a manufacturing method of a transistor or the like. [Figure 19] 1A to 1C are cross-sectional views illustrating an example of a manufacturing method of a transistor or the like. [Figure 20] 1A to 1C are cross-sectional views illustrating an example of a manufacturing method of a transistor or the like. [Figure 21] FIG. 1 is a cross-sectional view illustrating an example of a transistor. [Figure 22] 1A and 1B are a top view and a cross-sectional view illustrating an example of a transistor. [Figure 23] FIG. 1 is a cross-sectional view illustrating an example of a transistor. [Figure 24] FIG. 2 is a diagram for explaining a band structure. [Diagram 25] FIG. 1 is a cross-sectional view illustrating an example of a transistor. [Figure 26] 1A and 1B are diagrams illustrating structural analyses of a CAAC-OS and a single crystal oxide semiconductor by XRD, and diagrams showing selected-area electron diffraction patterns of a CAAC-OS. [Figure 27] Cross-sectional TEM image, planar TEM image, and corresponding image analysis images of CAAC-OS. [Figure 28] Electron diffraction pattern and cross-sectional TEM image of nc-OS. [Figure 29] Cross-sectional TEM image of a-like OS. [Diagram 30] FIG. 1 shows the change in the crystal part of an In-Ga-Zn oxide due to electron irradiation. [Diagram 31] FIG. 1 is a diagram showing an example of a touch panel module. [Diagram 32] 1A and 1B are diagrams illustrating examples of electronic devices. [Diagram 33] 1A and 1B are diagrams illustrating examples of electronic devices. [Diagram 34] FIG. 1 is a cross-sectional view showing an example of an input / output device. [Diagram 35] 1 is a photograph showing an input / output device according to an embodiment. [Diagram 36] FIG. 4 is a diagram for explaining the measurement results of the XRD spectrum of a sample. [Figure 37] 1A to 1C are diagrams illustrating a TEM image and an electron beam diffraction pattern of a sample. [Figure 38] FIG. 1 is a diagram illustrating EDX mapping of a sample. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0028] The embodiment will be described in detail with reference to the drawings. However, the present invention is not limited to the following description. The present invention is not limited to the above embodiment, and various changes and modifications may be made in the form and details without departing from the spirit and scope of the present invention. It will be easily understood by those skilled in the art that the above-mentioned invention can be obtained by the following embodiments. It should not be construed as being limited to the contents described.

[0029] In the configuration of the invention described below, the same parts or parts having similar functions are referred to as the same parts. The same reference numerals are used in common among different drawings, and the repeated explanations are omitted. When referring to a function, the same hatch pattern may be used and no particular reference number may be given.

[0030] In addition, the position, size, range, etc. of each component shown in the drawings are not necessarily the same as in the actual embodiment, for ease of understanding. Therefore, the disclosed invention may not necessarily represent the actual position, size, range, etc. The present invention is not necessarily limited to the position, size, range, etc. disclosed in the drawings.

[0031] The words "film" and "layer" may be interchangeable depending on the circumstances. For example, the term "conductive film" can be replaced with "conductive layer" Alternatively, for example, the term "insulating layer" may be used. may be changed to the term "insulating film."

[0032] In this specification, "parallel" means that two straight lines are arranged at an angle of -10° or more and 10° or less. Therefore, it includes the case where the angle is between -5° and 5°. "Line" refers to the state in which two straight lines are arranged at an angle between -30° and 30°. "Perpendicular" means that two straight lines are arranged at an angle of 80° or more and 100° or less. Therefore, the angle may be between 85° and 95°. This refers to a state in which two straight lines are arranged at an angle of 60° or more and 120° or less.

[0033] In addition, in this specification, when the crystal is a trigonal or rhombohedral crystal, it is expressed as a hexagonal crystal system.

[0034] (Embodiment 1) In this embodiment, an input / output device according to one embodiment of the present invention will be described with reference to FIGS. .

[0035] An input / output device of one embodiment of the present invention has a function of displaying an image, a function as a touch sensor, and It is an in-cell type touch panel having the above structure.

[0036] There is no limitation on the display element included in the input / output device of one embodiment of the present invention. Optical elements using cro Electro Mechanical System, Organic EL (Electro Luminescence) elements and light-emitting diodes (LEDs) Light emitting diodes (Light Emitting Diodes), electrophoretic elements, etc. Such an element can be applied as a display element.

[0037] In this embodiment, a transmissive liquid crystal display device using a lateral electric field type liquid crystal element will be described as an example. Reveal.

[0038] There is no limitation on a detection element (also referred to as a sensor element) included in the input / output device of one embodiment of the present invention. Various sensors that can detect the proximity or contact of a detection object such as a finger or a stylus are available. It can be applied as a knowledge element.

[0039] For example, the sensor types include capacitance type, resistive film type, surface acoustic wave type, and infrared type. Various methods such as optical methods and pressure-sensitive methods can be used.

[0040] In this embodiment, an input / output device having a capacitance type sensing element will be described as an example.

[0041] The capacitive touch sensor includes a surface capacitive touch sensor and a projected capacitive touch sensor. The electrostatic capacitance type includes the self-capacitance type and the mutual capacitance type. This is preferable because it enables simultaneous multi-point detection.

[0042] In the input / output device according to one embodiment of the present invention, an electric field constituting a detector element is provided only on a substrate supporting a display element. The input / output device of one embodiment of the present invention is a full-in-cell touch panel. Another in-cell type touch panel is a display element that supports a The structure in which electrodes constituting the sensing element are provided on both the facing substrate and the counter substrate or only on the counter substrate. In comparison with these configurations, full in-cell touch panels have a counter substrate configuration. This is preferable because it allows simplification.

[0043] In the input / output device according to one embodiment of the present invention, an electrode constituting a display element is connected to an electrode constituting a detector element. This is preferable because it is possible to simplify the manufacturing process and reduce the manufacturing cost.

[0044] By applying one embodiment of the present invention, a display panel and a sensing element that are separately manufactured are bonded together. In comparison with a configuration in which a detector element is fabricated on the opposing substrate side, the input / output device can be made thinner or The weight can be reduced, or the number of parts of the input / output device can be reduced.

[0045] The input / output device according to one embodiment of the present invention includes an FPC that supplies a signal for driving a pixel and a The FPC that supplies the signals to the electronic device is placed on one side of the board. This makes it easier to incorporate into the FPC and reduces the number of parts. Thus, signals for driving the pixels and signals for driving the detector elements may be provided.

[0046] The configuration of the input / output device of one embodiment of the present invention is described below.

[0047] [Example 1 of cross-sectional configuration of input / output device] FIG. 1A shows a top view of the input / output device 300, and FIG. 1B shows a part of FIG. 1 shows a cross-sectional view between dashed dotted line AB and dashed dotted line CD.

[0048] As shown in FIG. 1A, the input / output device 300 includes a display unit 301 and a scanning line driver circuit 302. The display unit 301 includes a plurality of pixels 303, a plurality of signal lines, and a plurality of scanning lines. The display unit 301 also functions as an input unit. The unit 301 includes a plurality of detection elements that detect the contact or proximity of a detection target to the input / output device 300. The scanning line driver circuit 302 has a function as a touch sensor. The pixel 303 has a function of outputting a scanning signal to a scanning line corresponding to the pixel 303. The pixel 303 has a plurality of sub-pixels. FIG. 1A illustrates an example in which the pixel 303 has three subpixels. In one embodiment of the present invention, Not limited to.

[0049] FIG. 1A shows an example in which the input / output device 300 has a scanning line driver circuit. The input / output device 300 includes a scanning line driving circuit, a signal line driving circuit, and It is not necessary to have all the sensor driving circuits, and it is also possible to have one or more of them.

[0050] In the input / output device 300, the IC 268 is mounted on the substrate 211 by a mounting method such as the COG method. The IC 268 is equipped with, for example, a signal line driver circuit, a scanning line driver circuit, and a sensor driver circuit. The device has at least one of the above operating circuits.

[0051] In addition, the input / output device 300 is electrically connected to an FPC 269. Signals are supplied from the outside to IC268 and the scanning line driver circuit via FPC2. A signal can be output from IC268 to the outside via 69.

[0052] An IC may be mounted on the FPC 269. For example, the FPC 269 may include a signal line driver. An IC having one or more of the following circuits is implemented: a driving circuit for a scanning line, a driving circuit for a sensor, and a driving circuit for a scanning line. For example, the COF method or TAB (Tape Automated Broadcasting) method may be used. ICs can be mounted on FPC269 using mounting methods such as the mounting method. .

[0053] For example, the IC 268 may include a signal line driver circuit and a sensor driver circuit. For example, IC 268 has a signal line driver circuit, and an IC mounted on FPC 269 is a sensor. The sensor may have a driver circuit.

[0054] As shown in FIG. 1B, the input / output device 300 includes a transistor 201a 203a, a connecting portion 205a, a liquid crystal element 207a, and the like.

[0055] FIG. 1B shows a cross section of one subpixel as an example of the display portion 301. For example, A pixel is made up of a red subpixel, a green subpixel, and a blue subpixel. By configuring the display unit 301, full color display can be performed. The colors that the pixels exhibit are not limited to red, green, and blue. For example, the pixels may be white, yellow, magenta, etc. Alternatively, a sub-pixel exhibiting a color such as cyan may be used.

[0056] The transistors 201a and 203a include a gate electrode 221, an insulating film 213, an oxide semiconductor film 223, a source electrode 225a, and a drain electrode 225b. a further includes a conductive film 226, an insulating film 215, and an oxide conductive film 227. The insulating film 215 can also be considered as a component of the transistor 203a.

[0057] The gate electrode 221 and the oxide conductive film 227 can each function as a gate. The transistor 201a has an oxide semiconductor film in which a channel is formed by two gates. The gate electrode 221 and the oxide conductive film 227 are sandwiched between the gate electrode 221 and the oxide conductive film 227 via the conductive film 226. The transistor with two gates electrically connected in this way Compared to other transistors, the field effect mobility of the on-type transistor can be increased. This allows the transistor to increase the on-state current, resulting in the creation of circuits capable of high-speed operation. Furthermore, it is possible to reduce the area occupied by the circuit section. By applying resistors, the input / output device can be made larger or more precise, and the number of wirings can be increased. It is also possible to reduce signal delays in each wiring, and to suppress display unevenness. In addition, by applying such a configuration, a highly reliable transistor can be realized. It is possible.

[0058] Transistors 201a and 203a may be of the same structure or of different structures. In other words, the transistors in the driver circuit and the transistors in the display section have the same structure. The driving circuit section may have a plurality of transistors of different structures. The display unit may have a transistor with a plurality of structures. For example, among the shift register circuit, the buffer circuit, and the protection circuit included in the scanning line driver circuit, In one or more circuits, a transistor having two gates electrically connected to each other is used. It is preferred.

[0059] The transistors 201a and 203a are covered with an insulating film 217 and an insulating film 219. The insulating film 217 and the insulating film 219 are formed as components of the transistors 201a and 203a. The insulating film 217 can be regarded as a barrier against impurities entering the semiconductor that constitutes the transistor. For example, the insulating film 217 may be formed of a material that suppresses diffusion of water, hydrogen, etc. It is preferable to use a material in which impurities are not easily diffused. In order to reduce the surface irregularities that may cause the problem, it is preferable to select an insulating film having a planarizing function.

[0060] The transistor 201a includes an oxide semiconductor film 223 as a semiconductor layer and an oxide In this case, the oxide semiconductor film 223 and the oxide conductive film 227 are used. The gate insulating film 227 is preferably formed using an oxide semiconductor.

[0061] The resistivity of an oxide semiconductor can be easily controlled in a manufacturing process of an input / output device. Therefore, it can be suitably used as a material for a semiconductor film and a conductive film. By using an oxide semiconductor having an element as two or more layers constituting an input / output device, It is possible to share manufacturing equipment (e.g., film formation equipment, processing equipment, etc.) in two or more processes. Therefore, the manufacturing cost can be reduced.

[0062] In addition, since oxide semiconductors are materials that transmit visible light, they are suitable for elements that transmit visible light. can be used.

[0063] In addition, by forming the oxide semiconductor film 223 and the oxide conductive film 227 using the same metal element, For example, a metal oxide target having the same metal composition can be used. By using the same metal composition, the manufacturing cost can be reduced. By using an oxide semiconductor target, the etching gas or However, the same etching solution can be used for the oxide semiconductor film 223 and the oxide The metallic conductive films 227 may have different compositions even if they contain the same metal element. For example, During the manufacturing process of the input / output device, metal elements in the film may be removed, resulting in a different metal composition. .

[0064] The transistors 201a and 203a are made of highly purified oxide semiconductors that suppress the formation of oxygen vacancies. It is preferable that the transistor has a dielectric film 223. This allows the current flow in the off state of the transistor to be Therefore, the retention time of electric signals such as image signals can be reduced. The write interval can be set to a longer value when the power is on. This reduces the frequency of flash operations, thereby reducing power consumption.

[0065] In addition, since the transistors 201a and 203a have a relatively high field effect mobility, High-speed operation is possible. Such high-speed transistors are used in input / output devices. This allows the transistors of the display section and the transistors of the driver circuit section to be formed on the same substrate. That is, a semiconductor formed of a silicon wafer or the like can be used as a driving circuit. Since there is no need to use a physical device, the number of parts in the input / output device can be reduced. The display also uses transistors capable of high-speed operation, providing high-quality images. It is possible.

[0066] The liquid crystal element 207a is in FFS (Fringe Field Switching) mode. The liquid crystal element 207a includes a conductive film 251, a conductive film 252, and The liquid crystal 249 is arranged on the substrate 21 by an electric field generated between the conductive film 251 and the conductive film 252. The conductive film 251 can function as a pixel electrode. The conductive film 252 can function as a common electrode.

[0067] By using a conductive material that transmits visible light for the conductive film 251 and the conductive film 252, The device 300 can function as a transmissive liquid crystal display device. A conductive material that reflects visible light is used for the conductive film 1, and a conductive material that transmits visible light is used for the conductive film 252. By using the above, the input / output device 300 can function as a reflective liquid crystal display device. Cut.

[0068] Examples of conductive materials that transmit visible light include indium (In), zinc (Zn), and tin. It is preferable to use a material containing one selected from the group consisting of indium oxide (Sn). , Indium Tin Oxide (ITO), Indium Zinc Oxide, Indium Oxide with Tungsten Oxide, Indium Oxide with Tungsten Oxide Zinc oxide, indium oxide with titanium oxide, indium tin oxide with titanium oxide Indium tin oxide doped with silicon oxide, zinc oxide, zinc oxide doped with gallium, etc. A film containing graphene may also be used. can be formed, for example, by reducing a film containing graphene oxide formed in a film shape.

[0069] It is preferable to use an oxide conductive film for the conductive film 251. The oxide conductive film is preferably a metal film containing a metal element contained in the oxide semiconductor film 223. For example, the conductive film 251 may contain indium. Preferably, In-M-Zn oxide (wherein M is Al, Ti, Ga, Ge, Y, Zr, La, Ce) is used. , Sn, Mg, Nd, or Hf) film. The insulating film preferably contains indium, and is more preferably an In-M-Zn oxide film. It is nice.

[0070] Note that at least one of the conductive films 251 and 252 is formed using an oxide semiconductor. As described above, the oxide semiconductors having the same metal element may be used to configure the input / output device. By using this material for two or more layers, the manufacturing equipment (e.g., deposition equipment, processing equipment, etc.) can be doubled. Since the above steps can be commonly used, the manufacturing cost can be reduced.

[0071] For example, the insulating film 253 is a silicon nitride film containing hydrogen, and the conductive film 251 is a silicon oxide semiconductor film. When the insulating film 253 is used, the conductivity of the oxide semiconductor is increased by hydrogen supplied from the insulating film 253. It is possible.

[0072] Examples of conductive materials that reflect visible light include aluminum, silver, and metal materials thereof. Examples of the alloys include those containing the material.

[0073] The conductive film 251 functioning as a pixel electrode is connected to the source or drain of the transistor 203a. Here, the conductive film 251 is electrically connected to the drain electrode 225b. Here are some examples of this.

[0074] The conductive film 252 has a comb-like top surface shape (also referred to as a planar shape) or a top surface shape with slits. The insulating film 253 is provided between the conductive film 251 and the conductive film 252. The conductive film 251 has a portion overlapping with the conductive film 252 via the insulating film 253. In the region where the conductive film 251 and the colored film 241 overlap, a conductive film 252 is disposed on the conductive film 251. It has a part that is not placed.

[0075] A conductive film 255 is provided over the insulating film 253. The conductive film 255 is The common electrode 252 is electrically connected to the conductive film 252 and can function as an auxiliary wiring for the conductive film 252. By providing auxiliary wiring that electrically connects to the common electrode, the voltage drop caused by the resistance of the common electrode is suppressed. In addition, at this time, the conductive film containing metal oxide and the conductive film containing metal can be When a laminated structure is used, it is formed by a patterning technique using a halftone mask. This is preferable because it can simplify the process.

[0076] The conductive film 255 has a lower resistance than the conductive film 252. The conductive film 255 is, for example, Molybdenum, titanium, chromium, tantalum, tungsten, aluminum, copper, silver, neodymium The material is a single layer or a laminated layer made of metal materials such as aluminum, scandium, etc., or alloy materials containing these elements. It can be formed in layers.

[0077] The conductive film 255 is arranged so as to overlap the light-shielding film 243 and the like so as not to be visible to the user of the input / output device. It is preferable that the sensor is provided at a position where the sensor is located.

[0078] The connection portion 205a is connected to the scanning line driving circuit 302 through an external signal (video signal, clock signal, etc.). , start signal, or reset signal, etc.) or an external input terminal that transmits potential. Here, an example is shown in which FPC269 is provided as an external input terminal.

[0079] The connection portion 205a has a conductive film 231 on the insulating film 213, and a conductive film 23 3 and a conductive film 235 is provided on the conductive film 233. The conductive film 235 is electrically connected to the conductive film 235 via the connector 267. It is electrically connected to FPC269 via the FPC269 connector.

[0080] The conductive film 231 is a conductive film for forming the source electrode 225a and the drain electrode 225b of the transistors 201a and 203a. The conductive film 233 can be formed of the same material and in the same process as the inner electrode 225b. The conductive film 251 of the liquid crystal element 207a can be formed of the same material and in the same process. The conductive film 235 is formed of the same material and in the same process as the conductive film 252 of the liquid crystal element 207a. In this way, the conductive film constituting the connection portion 205a can be formed by If the electrodes and wiring used in the moving circuit are fabricated using the same materials and processes, the number of processes can be prevented from increasing. This is preferable.

[0081] The substrate 261 is provided with a colored film 241, a light-shielding film 243, and an insulating film 245. In FIG. 1(B), an example in which the thickness of the substrate 261 is thinner than the thickness of the substrate 211 is shown. The embodiment is not limited to this. One of the substrates 261 and 211 may be thinner than the other. The thickness of the substrate on the display surface side (the side closest to the object to be detected) may be the same. This is preferable because it can increase the detection sensitivity of the element.

[0082] The colored film 241 has a portion overlapping with the liquid crystal element 207a. The sensor 201 has a portion overlapping at least one of the sensors 201a and 203a.

[0083] The insulating film 245 prevents impurities contained in the colored film 241, the light-shielding film 243, etc. from diffusing into the liquid crystal 249. It is preferable that the insulating film 245 has a function as an overcoat to prevent the It is not necessary to provide this if necessary.

[0084] An alignment film may be provided in contact with the liquid crystal 249. The alignment film is used to adjust the alignment of the liquid crystal 249. For example, in FIG. 1B, an alignment film is formed to cover the conductive film 252. In addition, in FIG. 1B, an alignment film may be provided between the insulating film 245 and the liquid crystal 249. The insulating film 245 may have a function as an alignment film and an overcoat. The present invention may have both functions.

[0085] The input / output device 300 also includes a spacer 247. The spacer 247 is disposed between the substrate 211 and It has the function of preventing the distance to the substrate 261 from becoming closer than a certain value.

[0086] In FIG. 1B, the spacer 247 is provided over the insulating film 253 and the conductive film 252. However, the embodiment of the present invention is not limited to this example. For example, the insulating film 245 may be provided on the substrate 261 side. A spacer 247 may be formed on the insulating layer 247. 253 and the insulating film 245, either the substrate 211 side or the substrate 261 side. It is not necessary for the structure to be in contact with the wall.

[0087] Granular spacers may be used as the spacers 247. For the granular spacers, silica However, it is more preferable to use materials having elasticity such as resin and rubber. At this time, the granular spacers may be crushed in the vertical direction.

[0088] The substrate 211 and the substrate 261 are bonded together by an adhesive layer 265. A liquid crystal 249 is sealed in the area surrounded by the substrate 261 and the adhesive layer 265 .

[0089] When the input / output device 300 is made to function as a transmissive liquid crystal display device, the polarizing plate is The light from the backlight placed outside the polarizing plate is The light is incident through a polarizing plate. At this time, the voltage applied between the conductive film 251 and the conductive film 252 is Therefore, the orientation of the liquid crystal 249 can be controlled, and the optical modulation of light can be controlled. The intensity of the light emitted through the light plate can be controlled. Since light outside of a specific wavelength range is absorbed by the Or the light will have a green color.

[0090] In addition to the polarizing plate, for example, a circular polarizing plate can be used. For example, a linear polarizing plate and a quarter-wave retardation plate can be laminated. This makes it possible to reduce the viewing angle dependency of the display of the input / output device.

[0091] In this example, an element to which the FFS mode is applied is used as the liquid crystal element 207a. Liquid crystal elements using various modes can be used, not limited to VA (V Vertical Alignment mode, TN (Twisted Nematic ) mode, IPS (In-Plane-Switching) mode, ASM (Axia lly Symmetric aligned Micro-cell mode, OCB (Optically Compensated Birefringence) mode , FLC (Ferroelectric Liquid Crystal) mode, AF LC (AntiFerroelectric Liquid Crystal) mode, etc. A liquid crystal element to which the above is applied can be used.

[0092] In addition, the input / output device 300 may be a normally black type liquid crystal display device, for example, a vertical alignment (VA A transmissive liquid crystal display device using a vertical alignment mode may be used. MVA (Multi-Domain Vertical Alignment) mode, PVA (Patterned Vertical Alignment) mode, ASV Modes, etc. can be used.

[0093] The liquid crystal element is an element that controls the transmission or non-transmission of light by the optical modulation action of liquid crystal. The optical modulation of liquid crystals is caused by the electric field applied to the liquid crystal (horizontal electric field, vertical electric field, or The liquid crystal used in the liquid crystal element is Thermotropic liquid crystal, low molecular weight liquid crystal, polymer liquid crystal, polymer dispersed liquid crystal (PDLC:Pol ymer Dispersed Liquid Crystal), ferroelectric liquid crystal, antiferroelectric Dielectric liquid crystals can be used. These liquid crystal materials can be cholesteric depending on the conditions. phase, smectic phase, cubic phase, chiral nematic phase, isotropic phase, etc.

[0094] In addition, the liquid crystal material may be either a positive type liquid crystal or a negative type liquid crystal, depending on the application. An optimum liquid crystal material can be used depending on the mode and design.

[0095] In addition, when the in-plane switching system is adopted, liquid crystal that exhibits a blue phase without using an alignment film may be used. The blue phase is one of the liquid crystal phases. When the temperature of a cholesteric liquid crystal is increased, the cholesteric The blue phase appears just before the transition from the crystalline phase to the isotropic phase. In order to improve the temperature range, a liquid crystal composition containing 5% by weight or more of chiral agent is used. The liquid crystal composition containing a liquid crystal exhibiting a blue phase and a chiral agent is used as the liquid crystal 249. The speed is short and the liquid crystal is optically isotropic. In addition, the liquid crystal exhibits a blue phase and contains a chiral agent. The composition does not require alignment treatment and has low viewing angle dependency. Since the rubbing process is unnecessary, electrostatic damage caused by the rubbing process is prevented. This can prevent the liquid crystal display device from being damaged or broken during the manufacturing process. .

[0096] Here, above the substrate 261, a substrate that is directly touched by a detection object such as a finger or a stylus is provided. In this case, a polarizing plate or a circular polarizing plate may be provided between the substrate 261 and the substrate. In that case, it is preferable to provide a protective layer (ceramic coat, etc.) on the substrate. The protective layer is preferably made of, for example, silicon oxide, aluminum oxide, yttrium oxide, yttrium oxide, or yttrium oxide. Inorganic insulating materials such as yttrium-stabilized zirconia (YSZ) can be used. The substrate may be made of tempered glass. The tempered glass is made by ion exchange or air-cooling tempering. The material can be used after being subjected to physical or chemical treatment and having its surface subjected to compressive stress. Cut.

[0097] FIG. 2(A) shows a cross-sectional view of two adjacent pixels. Each pixel is a sub-pixel that a different pixel has.

[0098] In the input / output device shown in FIG. 2A, the left subpixel has a conductive film 252 and the right subpixel has a conductive film 253. The capacitance formed between the conductive film 252 and the sensor is used to detect the proximity or contact of a detection object. That is, in the input / output device of one embodiment of the present invention, the conductive film 252 can be It serves as both a common electrode for the crystal element and an electrode for the detection element.

[0099] In this manner, in the input / output device of one embodiment of the present invention, the electrode constituting the liquid crystal element is Since the electrode also functions as a constituent electrode, the manufacturing process can be simplified and the manufacturing cost can be reduced. This makes it possible to reduce the thickness and weight of the input / output device.

[0100] The conductive film 252 is electrically connected to a conductive film 255 that functions as an auxiliary wiring. By providing the film 255, the resistance of the electrode of the sensing element can be reduced. By reducing the resistance of the electrodes, the time constant of the electrodes of the detection element can be reduced. The smaller the time constant of the element electrodes, the higher the detection sensitivity and the higher the detection accuracy. can be increased.

[0101] In addition, if the capacitance between the electrode of the detector element and the signal line is too large, the time constant of the electrode of the detector element Therefore, a planarizing function is provided between the transistor and the electrode of the detector element. It is preferable to provide an insulating film having the following structure to reduce the capacitance between the electrode of the detector element and the signal line. For example, in FIG. 2A, an insulating film 219 is provided as an insulating film having a planarizing function. By providing the insulating film 219, the capacitance between the conductive film 252 and the signal line can be reduced. This makes it possible to reduce the time constant of the electrodes of the sensing element. The smaller the time constant of the electrode, the higher the detection sensitivity and the higher the detection accuracy. It can be done.

[0102] For example, the time constant of the electrodes of the sensing element is greater than 0 seconds and is 1×10 -4 seconds or less, preferably 0 Seconds greater than 5 x 10 -5 seconds or less, more preferably greater than 0 seconds and 5×10 -6 seconds or less, More preferably, it is greater than 0 seconds and is 5×10 -7 seconds or less, more preferably greater than 0 seconds and 2× 10 -7 It is preferable that the time constant is less than 1×10-6 By keeping it to less than 2 seconds, noise It is possible to achieve high detection sensitivity while suppressing the influence of the above.

[0103] [Example of cross-sectional configuration of input / output device 2] FIG. 2B shows a cross-sectional view of two adjacent pixels, which is different from FIG. 2A. The two sub-pixels shown in FIG. 1 are sub-pixels that different pixels have. FIG. 3(A) shows a cross-sectional view between dashed dotted lines AB and CD in (A).

[0104] The second configuration example shown in FIG. 2B and FIG. 3A includes a conductive film 251, a conductive film 252, and an insulating film 25 3 and the conductive film 255 are stacked in a different order from those in the first structural example shown in FIG. In addition, in the configuration example 2, the above can be referred to for the same parts as those in the configuration example 1. do.

[0105] Specifically, in the configuration example 2, a conductive film 255 is provided over the insulating film 219. The conductive film 251 is formed on the insulating film 253. has.

[0106] As shown in FIG. 2B, the liquid crystal element 207b is provided in the upper layer and has a comb-like or slit-like The conductive film 251 having a top surface shape is used as a pixel electrode, and the conductive film 252 provided in the lower layer is used as a common electrode. The conductive film 251 can also be used as a source or drain of the transistor 203a. The input is electrically connected to the input.

[0107] In FIG. 2B, the conductive film 252 in the left subpixel and the conductive film 252 in the right subpixel are The capacitance formed between the sensor and the sensor can be used to detect the proximity or contact of a sensor object. That is, in the input / output device of one embodiment of the present invention, the conductive film 252 is a common electrode of a liquid crystal element. and serves as an electrode of the detection element.

[0108] In the configuration example 1 (Fig. 1(B) and Fig. 2(A)), the conductor that serves as both the electrode of the sensing element and the common electrode is The conductive film 252 is closer to the display surface side (the side closer to the object to be detected) than the conductive film 251 that functions as a pixel electrode. ) in the direction perpendicular to the display surface 251. As a result, the conductive film 251 is positioned closer to the display surface than the conductive film 252. In the configuration example 1, the detection sensitivity may be improved compared to the example 2.

[0109] In addition, in the configuration example 2, the product of the conductive film 251, the conductive film 252, the insulating film 253, and the conductive film 255 is Since the layer order is different from that of Configuration Example 1, the configuration of the connection portion is also different from that of Configuration Example 1.

[0110] The connection portion 205b shown in FIG. 3A has a conductive film 231 over the insulating film 213. A conductive film 233 is provided on the conductive film 233, and a conductive film 235 is provided on the conductive film 233. The conductive film 233 is It can be formed of the same material and in the same process as the conductive film 252 of the liquid crystal element 207b. The conductive film 235 is formed of the same material and in the same process as the conductive film 251 of the liquid crystal element 207b. It can be formed with.

[0111] Another structural example of a transistor included in the input / output device of one embodiment of the present invention is shown in FIG. As shown in FIG. 3B, in a transistor having two gates, In this case, the two gates may not be electrically connected. In this way, at least one of the driving circuit section and the display section is provided with a top-gate transistor.

[0043]

[0112] Another structural example of a liquid crystal element included in an input / output device of one embodiment of the present invention is shown in FIG. 1 to 3F. Both the conductive film 251 and the conductive film 252 have a comb-like upper surface shape (plan view). The upper surface of the plate may have a rectangular shape, or a slit-shaped upper surface.

[0113] For example, when viewed from above, the end of the slit in one conductive film and the end of the slit in the other conductive film The cross-sectional view of this case is shown in FIG.

[0114] Alternatively, when viewed from above, a portion where neither the conductive film 251 nor the conductive film 252 is provided is A cross-sectional view of this case is shown in FIG.

[0115] Alternatively, when viewed from above, the conductive film 251 and the conductive film 252 have a portion where they overlap each other. The cross-sectional view of this case is shown in FIG.

[0116] [Example 3 of cross-sectional configuration of input / output device] FIG. 4 shows a diagram of the area between the dashed dotted lines AB and AB in FIG. 1(A), which is different from FIG. 1(B) and FIG. 3(A). 1 and a cross-sectional view between dashed and dotted lines CD and C are shown.

[0117] In the configuration example 3 shown in FIG. 4, a transistor included in a display portion 301 and a scanning line driver circuit 302 are The structures of the transistors are different from those of the first structure shown in FIG. In addition, in the configuration example 3, for the parts similar to the configuration example 1, please refer to the above. can be done.

[0118] The transistor 201b has an oxide semiconductor film in which a channel is formed sandwiched between two gates. In the transistor 201b, the gate electrode 221 and the oxide conductive film 227 are directly connected to each other. The transistor 201a is different from the transistor 201a in that the two gates are in contact with each other. The electrical connection may be made without an intermediate connection.

[0119] The transistor 203b is formed of an oxide semiconductor layer in which a channel is formed, similar to the transistor 201b. The semiconductor film 223 is sandwiched between two gates. In addition, a transistor having two gates can be applied to the display portion. Although not shown, the gate electrode 221 and the oxide conductive film 227 are also formed in the transistor 203b. are preferably electrically connected.

[0120] In addition, the closer the distance between the oxide conductive film 227 and the electrode of the detection element, the This can cause problems such as a change in the potential of the electrodes of the detection element. In this embodiment, the oxide conductive film 227 and the electrodes of the detection element are provided in different layers. This electrode is less affected by the oxide conductive film 227 and is therefore preferable.

[0121] [Example 4 of cross-sectional configuration of input / output device] FIG. 5 shows a dashed line A in FIG. 1(A) which is different from FIG. 1(B), FIG. 3(A), and FIG. The cross-sectional view between -B and dashed line CD is shown.

[0122] The fourth example of the configuration shown in FIG. 5 is a configuration of a transistor included in the scanning line driver circuit 302 and a spacer The substrate on which 247 is provided is different from that in the configuration example 1 shown in FIG. 1(B) and FIG. 2(A). In the configuration example 4, the same parts as those in the configuration example 1 can be referred to above. .

[0123] The transistor 201c has an oxide semiconductor film in which a channel is formed sandwiched between two gates. In the transistor 201c, the oxide conductive film 227 is formed at a position Specifically, the insulating film 217 is provided on the insulating film 215. An insulating film 218 having a planarizing function is provided on the insulating film 218. An oxide conductive film 227 is provided on the insulating film 218. In this manner, the oxide conductive film 227 is provided on an insulating film having a planarizing function. The transistor 201c may be covered with an insulating film 219 having a planarization function. In FIG. 5, the oxide conductive film 227 is electrically connected to the gate electrode 221 via the conductive film 226. As shown in FIG. 4, the oxide conductive film 227 and the gate electrode are electrically connected. The poles 221 may be directly connected.

[0124] FIG. 5 shows an example in which a spacer 247 is provided on an insulating film 245. As shown, a spacer 247 may be disposed on the substrate 261 side.

[0125] [Example 5 of cross-sectional configuration of input / output device] FIG. 6 shows a point in FIG. 1(A) that is different from that in FIG. 1(B), FIG. 3(A), FIG. 4, and FIG. 1 shows a cross-sectional view between dashed line AB and dashed line CD.

[0126] In the configuration example 5 shown in FIG. 6, the formation position of the colored film 241 is different from that shown in FIG. Configuration Example 5 is different from Configuration Example 1. For the parts of Configuration Example 5 that are the same as those of Configuration Example 1, please refer to the above. It can be lit up.

[0127] The colored film 241 is not limited to being formed on the opposing substrate (substrate 261). As shown in FIG. 2, the semiconductor device may be formed on the substrate 211 on which the transistors and the like are formed. Due to the increase in the resolution of the display of the input device, the alignment accuracy of the substrate 211 and the substrate 261 is reduced. As a result, it is possible to suppress a decrease in yield and a decrease in display quality.

[0128] [Example 6 of cross-sectional configuration of input / output device] FIG. 34 shows a cross-sectional view of an input / output device different from the above configuration examples. The device is configured such that electrodes constituting the sensing element are provided only on the substrate supporting the display element (full The touch panel is not limited to the in-cell type. An electrode constituting a sensing element may be provided on the side.

[0129] In FIG. 34, a conductive film is formed on the surface of the substrate 261 opposite to the surface on which the colored film 241 and the like are formed. The conductive film 254 is connected to the FPC 2 via a connector 257. 59 are electrically connected. In the input / output device 300 shown in FIG. The capacitance formed between the conductive film 254 is used to detect the proximity or contact of a detection object. That is, in the input / output device of one embodiment of the present invention, the conductive film 252 is a liquid crystal element. The common electrode of the liquid crystal element is also used as one of the electrodes of the detection element. The conducting electrode may also serve as one electrode of the sensing element, or may also serve as a pair of electrodes of the sensing element. It's fine.

[0130] FIG. 34 shows an example in which a conductive film 255 is provided over the conductive film 252. The conductive film that can function as an auxiliary wiring for the electrode may be placed on either side. stomach.

[0131] Next, the details of materials that can be used for each component of the input / output device of this embodiment will be described. The following description will be given. Note that the description of components that have already been explained may be omitted. In addition, the following materials may be appropriately used for the input / output device and its components shown in the following embodiments. This can be done.

[0132] <Substrate> There is no particular restriction on the material of the substrate of the input / output device 300, but at least the following heat treatment For example, glass substrates and ceramic substrates are A substrate made of silicon or silicon carbide may be used. Single crystal semiconductor substrates, polycrystalline semiconductor substrates, compound semiconductor substrates such as silicon germanium, It is also possible to use SOI substrates, etc., and semiconductor elements are provided on these substrates. In addition, when a glass substrate is used as the substrate, the sixth generation (1500mm x 1850mm), 7th generation (1870mm x 2200mm), 8th generation (2200mm x 2400mm), 9th generation (2400mm x 2800mm), 10th generation By using large-area substrates such as 2950mm x 3400mm, it is possible to create large display devices. Alternatively, a flexible substrate may be used as the substrate 211, and the substrate may be directly formed on the flexible substrate. A transistor, a capacitor, and the like may be formed.

[0133] By using a thin substrate, the input / output device can be made lighter and thinner. By using a substrate that is thick enough to be flexible, a flexible input / output device can be realized. can.

[0134] In addition to these, various substrates can be used as the substrates 211 and 261 to form transistors. The type of the substrate is not limited to a specific one. An example of the substrate is Examples include plastic substrates, metal substrates, stainless steel substrates, and stainless steel Substrate with foil, tungsten substrate, substrate with tungsten foil, flexible These include substrates, laminated films, papers containing fibrous materials, or base films. Examples of the glass substrate include barium borosilicate glass, aluminoborosilicate glass, or silicon. An example of a flexible substrate is polyethylene terephthalate. (PET), polyethylene naphthalate (PEN), polyethersulfone (PES) Examples of materials that can be used include plastics such as acrylic and other flexible synthetic resins. Examples of laminated films include polypropylene, polyester, polyvinyl fluoride, and Examples of the base film include polyester and polyamide. , polyimide, inorganic deposition film, paper, etc. In particular, semiconductor substrates, single crystal substrates By manufacturing transistors using a SOI substrate, etc., the characteristics, size, The purpose of this method is to manufacture transistors that have little variation in shape, high current capacity, and small size. When a circuit is constructed using such transistors, the circuit can consume less power. It is possible to achieve a higher integration of the circuits.

[0135] Note that a transistor is formed using a certain substrate and then transferred to another substrate. However, the transistor may be disposed on another substrate. In addition to the substrate on which the above-mentioned transistors can be formed, the substrates include paper substrates, cellophane substrates, and the like. substrates made of natural fibers (silk, cotton, hemp), synthetic fibers (nylon, Polyurethane, polyester) or regenerated fiber (acetate, cupra, rayon, regenerated The substrates used are made of synthetic polyester, leather, or rubber. This allows the formation of transistors with good characteristics and low power consumption. It is possible to manufacture devices that are less likely to break, heat resistant, lightweight, or thin.

[0136] <Transistor> The structure of a transistor included in an input / output device of one embodiment of the present invention is not particularly limited. The transistors may be planar type, staggered type, or inversely. The transistor may be a staggered type. Also, the transistor may be either a top gate type or a bottom gate type. Alternatively, a gate electrode may be provided above and below the channel. The semiconductor material used for the transistor is not particularly limited, and may be, for example, an oxide semiconductor. , silicon, germanium, etc.

[0137] The crystallinity of the semiconductor material used in the transistor is not particularly limited. A semiconductor having crystallinity (a microcrystalline semiconductor, a polycrystalline semiconductor, a single crystal semiconductor, or a semiconductor having a partially crystalline region If a semiconductor having crystallinity is used, the transistor This is preferable because it can suppress deterioration of the star characteristics.

[0138] In addition, the semiconductor materials used in the transistors include, for example, group 14 elements and compound semiconductors. A semiconductor layer can be made of a silicon or oxide semiconductor. For example, a semiconductor containing gallium arsenide or an oxide semiconductor containing indium can be used.

[0139] In particular, it is preferable to use an oxide semiconductor as a semiconductor in which a channel of a transistor is formed. In particular, it is preferable to use an oxide semiconductor having a larger band gap than silicon. It is desirable to use a semiconductor material with a wider band gap and lower carrier density than silicon. This is preferable because it can reduce the current in the off state of the transistor.

[0140] For example, the oxide semiconductor may contain at least indium (In) or zinc (Zn). More preferably, the oxide contains In-M-Zn (wherein M is Al, Ti, Ga , Ge, Y, Zr, La, Ce, Sn, Mg, Nd, or Hf metals) Contains compounds.

[0141] In particular, the semiconductor layer has a plurality of crystal parts, and the c-axes of the crystal parts are aligned along the surface on which the semiconductor layer is formed, Or, the crystals are oriented approximately perpendicular to the upper surface of the semiconductor layer, and no grain boundaries are present between adjacent crystal portions. An oxide semiconductor film is preferably used.

[0142] Such an oxide semiconductor has no crystal grain boundaries, and therefore does not show any deformation when the display panel is bent. Therefore, the generation of cracks in the oxide semiconductor film due to the applied force can be suppressed. Such oxide semiconductors are suitable for use in input / output devices that are flexible and can be used in a curved state. It is possible.

[0143] In addition, by using such an oxide semiconductor as the semiconductor layer, fluctuations in electrical characteristics are suppressed. This makes it possible to realize a highly reliable transistor.

[0144] In addition, due to its low off-state current, the charge stored in the capacitance can be released through the transistor for a long period of time. By applying such transistors to pixels, It is also possible to stop the driving circuit while maintaining the grayscale of the image displayed in the display area. As a result, a display device with extremely reduced power consumption can be realized.

[0145] <Oxide semiconductor film> The oxide semiconductor film 223 contains at least indium (In), zinc (Zn), and M (Al, Metals such as Ti, Ga, Ge, Y, Zr, La, Ce, Sn, Mg, Nd, or Hf) It is preferable that the oxide semiconductor includes a film represented by In-M-Zn oxide. In order to reduce the variation in the electrical characteristics of the transistors used, stabilizers are also used. It is preferred that the compound contains

[0146] The stabilizer includes the metals described above under M, such as gallium (Ga), tin, etc. (Sn), hafnium (Hf), aluminum (Al), or zirconium (Zr), etc. Other stabilizers include the lanthanides lanthanum (La), selenium (Se), and lanthanides. Ce, Praseodymium (Pr), Neodymium (Nd), Samarium (Sm), Eu (Eu), Gd (Gd), Tb (Tb), Dysprosium (Dy ), Holmium (Ho), Erbium (Er), Thulium (Tm), Ytterbium (Y b), lutetium (Lu), etc.

[0147] As the oxide semiconductor constituting the oxide semiconductor film 223, for example, an In-Ga-Zn oxide In-Al-Zn oxides, In-Sn-Zn oxides, In-Hf-Zn oxides , In-La-Zn oxide, In-Ce-Zn oxide, In-Pr-Zn oxide, In-Nd-Zn oxide, In-Sm-Zn oxide, In-Eu-Zn oxide, I n-Gd-Zn oxide, In-Tb-Zn oxide, In-Dy-Zn oxide, In -Ho-Zn oxide, In-Er-Zn oxide, In-Tm-Zn oxide, In- Yb-Zn oxide, In-Lu-Zn ​​oxide, In-Sn-Ga-Zn oxide, I n-Hf-Ga-Zn oxide, In-Al-Ga-Zn oxide, In-Sn-Al- Zn-based oxide, In-Sn-Hf-Zn-based oxide, In-Hf-Al-Zn-based oxide are used. There can be.

[0148] In this case, the In-Ga-Zn oxide is an oxide having In, Ga, and Zn as main components. It means oxide, and the ratio of In, Ga, and Zn does not matter. Also, In, Ga, and Zn Metal elements other than those may be included.

[0149] When the oxide semiconductor film 223 is an In-M-Zn oxide, the sum of In and M is 10 When 0 atomic%, preferably In is higher than 25 atomic% and M is 75 atomic %, more preferably In is higher than 34 atomic %, and M is 66 atomic %. tomic% or less.

[0150] The oxide semiconductor film 223 has an energy gap of 2 eV or more, preferably 2.5 eV or more. More preferably, the energy gap is 3 eV or more. By using the body, the off-state current of a transistor can be reduced.

[0151] The thickness of the oxide semiconductor film 223 is 3 nm to 200 nm, preferably 3 nm to 10 0 nm or less, and more preferably 3 nm or more and 50 nm or less.

[0152] The oxide semiconductor film 223 is an In-M-Zn oxide (wherein M is Al, Ti, Ga, Ge, Y, or Zr , La, Ce, Sn, Mg, Nd, or Hf), an In-M-Zn oxide is formed. The atomic ratio of the metal elements in the sputtering target used for this purpose is In≧M, Zn≧M. It is preferable that the atomic ratio of the metal elements in such a sputtering target is In:M:Zn=1:1:1, In:M:Zn=1:1:1.2, In:M:Zn= 3:1:2, In:M:Zn=1:3:4, In:M:Zn=1:3:6, etc. The atomic ratio of the oxide semiconductor film 223 to be formed is determined by the above-mentioned sputtering method as an error. The atomic ratio of metal elements contained in the target varies by ±40%. nothing.

[0153] As the oxide semiconductor film 223, an oxide semiconductor film with low carrier density is used. For example, The oxide semiconductor film 223 has a carrier density of 1×10 17 pieces / cm 3 Below, preferably 1x 10 15 pieces / cm 3 Less than 1×10, more preferably 13 pieces / cm 3 The following is more preferable: is 1×10 11 pieces / cm 3 The following oxide semiconductor film is used.

[0154] In addition, the semiconductor characteristics and electrical characteristics (field effect In addition, a material with an appropriate composition can be used depending on the required properties (mobility, threshold voltage, etc.). In order to obtain semiconductor characteristics of the transistor, the carrier density of the oxide semiconductor film 223 or The impurity concentration, defect density, atomic ratio of metal elements to oxygen, interatomic distance, density, etc. are appropriately determined. It is preferable to do so.

[0155] The oxide semiconductor film 223 contains silicon or carbon, which is one of Group 14 elements. As a result, oxygen vacancies increase in the oxide semiconductor film 223, causing the oxide semiconductor film 223 to become an n-type film. The concentration of silicon and carbon in the semiconductor film 223 was measured by secondary ion mass spectrometry (SIMS). Concentration obtained by secondary ion mass spectrometry ) to 2 x 10 18 atoms / cm 3 Less than or equal to 2 x 10 17 atoms / cm 3 The following applies.

[0156] In addition, in the oxide semiconductor film 223, an alkali metal or alkali metal oxide obtained by SIMS The concentration of alkali earth metals is 1×10 18 atoms / cm 3 Less than or equal to 2 x 10 16 a toms / cm 3 Alkali metals and alkaline earth metals bond with oxide semiconductors. When the transistor is combined with a junction, carriers may be generated, increasing the off-state current of the transistor. For this reason, the concentration of the alkali metal or alkaline earth metal in the oxide semiconductor film 223 is It is preferable to reduce it.

[0157] When nitrogen is contained in the oxide semiconductor film 223, electrons serving as carriers are generated. The rear density increases and it becomes easier to make it n-type. As a result, A transistor having such an oxide semiconductor film tends to be normally on. It is preferable that the nitrogen content is reduced as much as possible. For example, The nitrogen concentration is 5 x 10 18atoms / cm 3 It is preferable to do the following:

[0158] The oxide semiconductor film 223 may have a non-single crystal structure, for example. , CAAC-OS (C Axis Aligned-Crystalline Oxide Semiconductor), polycrystalline structure, microcrystalline structure (described later), or non-crystalline structure Among non-single crystal structures, the amorphous structure has the highest defect level density and CAA C-OS has the lowest density of defect states.

[0159] The oxide semiconductor film 223 may have an amorphous structure, for example. For example, the atomic arrangement is disordered and does not have crystalline components. Or, the oxide film has an amorphous structure. For example, it has a completely amorphous structure and does not have any crystalline parts.

[0160] Note that the oxide semiconductor film 223 may have an amorphous structure, a microcrystalline structure, or a polycrystalline structure. The film may be a mixed film having two or more of the following regions: a region of a CAAC-OS structure, a region of a single crystal structure, and a region of a crystalline structure. The mixed film may have, for example, an amorphous structure region, a microcrystalline structure region, a polycrystalline structure region, a CAA In the case of a single-layer structure having two or more regions of either C-OS region or single crystal structure region, In addition, the mixed film may have, for example, an amorphous structure region, a microcrystalline structure region, and a polycrystalline structure region. The layered structure has two or more of the following regions: a CAAC-OS region, a single crystal region, and a layered structure of the This may be the case.

[0161] Alternatively, it is preferable to use silicon as a semiconductor in which a channel of a transistor is formed. Although amorphous silicon may be used as silicon, silicon having crystallinity is particularly preferred. For example, microcrystalline silicon, polycrystalline silicon, and single crystal silicon are preferably used. In particular, polycrystalline silicon can be used at a lower temperature than single crystal silicon. It can be formed and has higher field effect mobility and higher reliability than amorphous silicon. By applying such a polycrystalline semiconductor to the pixel, the aperture ratio of the pixel can be improved. Even when manufacturing an extremely high-resolution input / output device, the gate driver circuit and the source driver It is now possible to form circuits and pixels on the same substrate, reducing the number of components that make up electronic devices. It is possible.

[0162] <Method for controlling resistivity of oxide semiconductor> Oxide semiconductors have resistance due to oxygen vacancies and / or impurity concentrations such as hydrogen and water in the film. Therefore, the oxide semiconductor film is formed by adding oxygen vacancies or and / or a process that increases the impurity concentration, or a process that reduces the oxygen deficiency and / or the impurity concentration. By selecting the material, the resistivity of the oxide conductive film can be controlled.

[0163] Note that the oxide conductive film formed using the oxide semiconductor film has a carrier density A highly conductive oxide semiconductor film having a low resistance, a highly conductive oxide semiconductor film, or a highly conductive oxide semiconductor film It can also be called a semiconductor film.

[0164] Specifically, the oxide semiconductor film to be the oxide conductive film 227 functioning as a gate is The treatment is performed to increase oxygen vacancies in the oxide semiconductor film and / or to increase oxygen vacancies in the oxide semiconductor film. By increasing the amount of impurities such as hydrogen and water, the carrier density is increased and the oxide semiconductor with low resistance is obtained. In addition, the insulating film 217 containing hydrogen can be formed in contact with the oxide semiconductor film. Hydrogen is diffused from the insulating film 217 containing hydrogen to the oxide semiconductor film, An oxide semiconductor film with high carrier density and low resistance can be obtained.

[0165] On the other hand, on the oxide semiconductor film 223, the oxide semiconductor film 223 is exposed to the above-mentioned plasma treatment. In order to prevent this, the insulating film 215 is provided. The semiconductor film 223 is not in contact with the insulating film 217 containing hydrogen. By using an insulating film capable of releasing oxygen, oxygen can be supplied to the oxide semiconductor film 223. In the oxide semiconductor film 223 to which oxygen is supplied, oxygen vacancies in the film or at the interface can be eliminated. The insulating film capable of releasing oxygen is an oxide semiconductor having a high resistance. For example, a silicon oxide film or a silicon oxynitride film can be used.

[0166] In order to obtain an oxide semiconductor film with low resistivity, an ion implantation method, an ion doping method, Using plasma immersion ion implantation techniques, hydrogen, boron, phosphorus Alternatively, nitrogen may be implanted into the oxide semiconductor film.

[0167] The oxide conductive film 227 is typically subjected to plasma treatment using a rare gas (He, N e, Ar, Kr, Xe), phosphorus, boron, hydrogen, and gallium containing one selected from nitrogen. More specifically, plasma treatment in an Ar atmosphere is used. , plasma treatment in a mixed gas atmosphere of Ar and hydrogen, plasma treatment in an ammonia atmosphere plasma treatment under a mixed gas atmosphere of Ar and ammonia, or plasma treatment under a nitrogen atmosphere. Examples include Zuma processing.

[0168] By the above plasma treatment, the oxide conductive film 227 becomes a lattice from which oxygen has been desorbed (or Oxygen vacancies are formed in the area where the oxide is removed. These oxygen vacancies are a cause of carrier generation. In addition, in the vicinity of the oxide conductive film 227, more specifically, in the vicinity of the oxide conductive film 22 When hydrogen is supplied from the insulating film in contact with the upper or lower side of 7 and enters the oxygen vacancy, Therefore, oxygen vacancies caused by plasma treatment may generate electrons that are carriers. The increased oxide conductive film 227 has a higher carrier density than the oxide semiconductor film 223.

[0169] On the other hand, the oxide semiconductor film 223 in which oxygen vacancies are reduced and the hydrogen concentration is reduced is a high-purity intrinsic oxide semiconductor film. The substantially intrinsic oxide semiconductor film can be referred to as a highly purified oxide semiconductor film. means that the carrier density of the oxide semiconductor is 1×10 17 / cm 3 preferably less than 1×10 15 / cm 3 More preferably, it is less than 1×10 13 / cm 3 Less than Or, it means that the impurity concentration is low and the defect level density is low (there is little oxygen vacancy). High purity authentic or substantially high purity authentic. Since the oxide semiconductor has a small number of carrier generation sources, the carrier density can be reduced. Therefore, a transistor in which a channel region is formed in the oxide semiconductor film has a threshold voltage The electrical characteristics tend to be such that the applied voltage is positive (also called normally-off characteristics). The highly intrinsic or substantially highly purified intrinsic oxide semiconductor film 223 has a low density of defect states. Therefore, the trap state density can be reduced.

[0170] In addition, the highly purified intrinsic or substantially highly purified intrinsic oxide semiconductor film 223 has a significantly low off-state current. It is very small and has a channel width of 1×10 6 Even if the device has a channel length of 10 μm, When the voltage between the source and drain electrodes (drain voltage) is in the range of 1V to 10V, The current is below the measurement limit of the semiconductor parameter analyzer, i.e., 1×10 -13 Below A Therefore, a channel region is formed in the oxide semiconductor film 223. The transistor thus fabricated has small fluctuations in electrical characteristics and is highly reliable.

[0171] The insulating film 217 may be, for example, an insulating film containing hydrogen, in other words, capable of releasing hydrogen. By using an insulating film, typically a silicon nitride film, hydrogen is supplied to the oxide conductive film 227. The insulating film capable of releasing hydrogen has a hydrogen concentration of 1×1 0 22 atoms / cm 3 It is preferable that the insulating film is the oxide conductive film 22. By forming the oxide conductive film 227 in contact with the oxide conductive film 227, hydrogen can be effectively contained in the oxide conductive film 227. In this way, in combination with the above-described plasma treatment, the oxide semiconductor film (or the oxide conductive film By changing the configuration of the insulating film in contact with the oxide semiconductor film (or the oxide conductive film), The resistance can be adjusted arbitrarily.

[0172] The hydrogen contained in the oxide conductive film 227 reacts with the oxygen that bonds with the metal atoms to become water. In addition, oxygen vacancies are formed in the lattice from which oxygen has been removed (or in the portion from which oxygen has been removed). When hydrogen enters the gap, electrons, which act as carriers, can be generated. When it bonds with oxygen, which bonds with metal atoms, it can generate electrons, which act as carriers. Therefore, the oxide conductive film 227 containing hydrogen has a higher hydrogen content than the oxide semiconductor film 223. High carrier density.

[0173] The oxide semiconductor film 223 in which the channel region of the transistor is formed has as little hydrogen as possible. Specifically, the oxide semiconductor film 223 is preferably The hydrogen concentration obtained is 2×10 20 atoms / cm 3 Less than or equal to 5×10 19 atoms / cm 3 Less than or equal to 1×10 19 atoms / cm 3 The following is better Preferably 5 x 10 18 atoms / cm 3 Less than or equal to 1×10 18 atoms / cm 3 Less than or equal to 5×10 17 atoms / cm 3 More preferably, 1×10 16 atoms / cm 3 The following applies.

[0174] On the other hand, the oxide conductive film 227 functioning as a gate has a higher hydrogen concentration than the oxide semiconductor film 223. The degree and / or amount of oxygen vacancy is high, resulting in low resistance.

[0175] The oxide conductive film 227 can be formed using a material that can be used for the oxide semiconductor film 223 and an oxide semiconductor. The method for forming the conductive film 223 can be applied. The material conductive film 227 is light-transmitting.

[0176] Note that a material that can be used for the oxide conductive film 227 and a method for forming the oxide conductive film 227 The method can also be applied to the conductive film 251 and the conductive film 252.

[0177] <Insulating film> Insulating material that can be used for insulating films, overcoats, spacers, etc. in input / output devices As the material, an organic insulating material or an inorganic insulating material can be used. For example, acrylic resin, epoxy resin, polyimide resin, polyamide resin, polyamideimide resin, siloxane resin, benzocyclobutene resin, phenol resin, etc. The organic insulating film may be a silicon oxide film, a silicon oxynitride film, a silicon nitride oxide film, or a silicon nitride film. Silicon film, aluminum oxide film, hafnium oxide film, yttrium oxide film, zirconium oxide film tantalum oxide film, magnesium oxide film, lanthanum oxide film, oxide Examples of the film include a cerium film and a neodymium oxide film.

[0178] Conductive film In addition to the gate, source, and drain of a transistor, various wirings and electrodes of an input / output device Conductive films made of aluminum, titanium, chromium, nickel, copper, yttrium, zirconium, etc. Metals such as tungsten, molybdenum, silver, tantalum, or tungsten, or those containing these as the main components The alloy can be used as a single layer or a laminate structure. For example, A two-layer structure in which a titanium film is laminated on a tungsten film; a two-layer structure in which a titanium film is laminated on a tungsten film; Two-layer structure with copper film laminated on molybdenum film, copper film on alloy film containing molybdenum and tungsten a two-layer structure in which a copper film is laminated on a copper-magnesium-aluminum alloy film; The structure is a titanium film or titanium nitride film, and an aluminum film is laminated on the titanium film or titanium nitride film. A three-layer structure in which a titanium film or a copper film is laminated and a titanium film or a titanium nitride film is further formed on the aluminum film or a copper film. A molybdenum film or a molybdenum nitride film and a layer of the molybdenum film or the molybdenum nitride film Then, an aluminum film or a copper film is laminated, and a molybdenum film or a molybdenum nitride film is further laminated on the aluminum film or the copper film. For example, a three-layer structure is formed by forming a source electrode 225a and a drain electrode 225b. In the case of a three-layer structure, the first and third layers are titanium, titanium nitride, molybdenum, and tungsten. Alloys containing molybdenum and tungsten, alloys containing molybdenum and zirconium, or molybdenum nitride, and the second layer is copper, aluminum, gold, silver, or It is preferable to form a film made of a low resistance material such as an alloy of copper and manganese. Indium tin oxide, indium oxide with tungsten oxide, indium oxide with tungsten oxide Indium zinc oxide, indium oxide with titanium oxide, indium tin oxide with titanium oxide Translucency of oxide, indium zinc oxide, indium tin oxide doped with silicon oxide, etc. Alternatively, a conductive material having the above structure may be used.

[0179] Note that the conductive film may be formed by using the above-described method for controlling the resistivity of an oxide semiconductor.

[0180] ≪Adhesive layer≫ The adhesive layer 265 is made of a hardening resin such as a thermosetting resin, a photocurable resin, or a two-liquid mixed hardening resin. Resins can be used. For example, acrylic resins, urethane resins, epoxy resins, or A resin having a siloxane bond can be used.

[0181] <Connector> The connector may be, for example, an anisotropic conductive film (ACF). Anisotropic Conductive Film (ACP) or Anisotropic Conductive Paste (ACP) c Conductive Paste) can be used.

[0182] ≪Colored film≫ A colored film is a colored layer that transmits light in a specific wavelength range. Materials that can be used for the colored film Examples of the material include a metal material, a resin material, and a resin material containing a pigment or dye.

[0183] <Light-shielding film> The light-shielding film is provided between the adjacent colored films. The light-shielding film may be made of, for example, a metal material, The black matrix can be formed by using a resin material containing a pigment or a dye. However, if the light-shielding film is provided in an area other than the display area, such as the driving circuit area, unintended light interference caused by guided light, etc. may occur. This is preferable because it can suppress unwanted light leakage.

[0184] [Example of how I / O devices work] Next, an example of a method for operating the input / output device of one embodiment of the present invention will be described.

[0185] FIG. 7A illustrates a part of a pixel circuit provided in a display portion of an input / output device of one embodiment of the present invention. FIG.

[0186] One pixel has at least a transistor 3503 and a liquid crystal element 3504. A wiring 3501 is electrically connected to the gate of the transistor 3503. A wiring 3502 is electrically connected to one of the source and drain of the transistor 3503 .

[0187] The pixel circuit includes a plurality of wirings (for example, wiring 3510_1, wiring 3510_ 2) and a plurality of wirings (for example, wiring 3511_1) extending in the Y direction, which are mutually The electrodes are arranged to cross each other, forming a capacitance therebetween.

[0188] In addition, among the pixels provided in the pixel circuit, some of the adjacent pixels are provided The electrodes of the liquid crystal elements are electrically connected to each other to form one block. The blocks are divided into island-like blocks (e.g., block 3515_1, block 3515_2) and Linear blocks extending in the X or Y direction (for example, blocks 3 extending in the Y direction) 516) and 517). Note that FIG. 7(A) shows only a part of the pixel circuit. However, in reality, these two types of blocks are repeatedly arranged in the X and Y directions. Here, one of the electrodes of the liquid crystal element may be, for example, a common electrode. The other electrode of the element is, for example, a pixel electrode.

[0189] The wiring 3510_1 (or 3510_2) extending in the X direction is an island-shaped block 3515_ 1 (or block 3515_2). Although not shown, The extending wiring 3510_1 is arranged discontinuously along the X direction via linear blocks. A plurality of island-shaped blocks 3515_1 are electrically connected to each other. The wiring 3511_1 is electrically connected to a line-shaped block 3516.

[0190] FIG. 7B shows a plurality of wirings (wirings 3510_1 to 3510_6, Also collectively referred to as wiring 3510), and a plurality of wirings extending in the Y direction (wirings 3511_1 to 3511_6, collectively referred to as wiring 3511) is shown in the equivalent circuit diagram. Each of the wirings 3510 extending in the X direction and each of the wirings 3511 extending in the Y direction A common potential can be input to each of the wirings 3510 extending in the X direction. A pulse voltage can be input from the pulse voltage output circuit. Each of the wirings 3511 can be electrically connected to a detection circuit. 0 and wiring 3511 can be swapped.

[0191] An example of a method for operating the input / output device of one embodiment of the present invention will be described with reference to FIGS. Reveal.

[0192] Here, one frame period is divided into a writing period and a detection period. This is the period in which image data is written, and the wiring 3501 (also called the gate line or the scanning line) On the other hand, the detection period is a period during which sensing is performed by the detection element. .

[0193] FIG. 8A is an equivalent circuit diagram during the writing period. A common potential is input to both the wiring 3510 extending in the Y direction and the wiring 3511 extending in the Y direction. .

[0194] FIG. 8B is an equivalent circuit diagram during the detection period. During the detection period, Each of the lines 3511 is electrically connected to a detection circuit. A pulse voltage is input to 0 from the pulse voltage output circuit.

[0195] FIG. 8C is an example of a timing chart of input and output waveforms in a mutual capacitance type sensing element. It is.

[0196] In FIG. 8C, detection of an object is performed in each row and column in one frame period. In FIG. 8(C), the difference between when the object is not detected (non-touch) and when the object is not detected (non-touch) during the detection period is shown. The figures show two cases: when detecting (touch) and when detecting (non-touch).

[0197] The wirings 3510_1 to 3510_6 are supplied with a pulse voltage from a pulse voltage output circuit. A pulse voltage is applied to the wirings 3510_1 to 3510_6. An electric field is generated between the pair of electrodes that form the capacitance, and a current flows through the capacitance. The electric field generated by the sensor changes when it is blocked by a finger or pen. This causes a change in the capacitance of the capacitor. It can be known.

[0198] The wirings 3511_1 to 3511_6 are each 1 to 3511_6. In the lines 3511_1 to 3511_6, the proximity or contact of the object to be detected is not detected. When there is no change in the current value, but the capacitance value decreases due to the proximity or contact of the object to be detected The current value decreases. The current may be detected by detecting the total current amount. The detection may be performed using an integrating circuit or the like. Alternatively, the peak value of the current may be detected. In that case, the current may be converted into a voltage and the peak value of the voltage may be detected.

[0199] In FIG. 8C, the wirings 3511_1 to 3511_6 are not detected. The waveforms are shown as voltage values ​​corresponding to the current values. It is desirable that the timing of the operation and the timing of the detection operation are synchronized.

[0200] In response to the pulse voltages applied to the wirings 3510_1 to 3510_6, the wirings 35 The waveforms in the wirings 11_1 to 3511_6 change. In response to a change in the voltage of the wirings 3510_1 to 3510_6, The waveform of the wiring 3511_6 changes uniformly. On the other hand, at the point where the object to be detected approaches or comes into contact with Since the current value decreases, the waveform of the corresponding voltage value also changes.

[0201] In this way, by detecting the change in capacitance, the proximity or contact of the object to be detected can be detected. In addition, the object to be detected, such as a finger or pen, can be detected by approaching the input / output device without touching it. A signal may still be detected.

[0202] In FIG. 8C, the common potential applied to the wiring 3510 during the writing period and Although an example in which the low potentials applied during the detection period are equal is shown, one embodiment of the present invention is not limited thereto. The energizing potential and the lower potential may be different potentials.

[0203] The pulse voltage output circuit and the detection circuit may be formed in a single IC. The IC is preferably mounted in an input / output device or in the housing of an electronic device. It is preferable that the input / output device is mounted on a flexible substrate. The parasitic capacitance increases at the bent part, which may increase the effect of noise. It is preferable to use an IC that uses a driving method that is less susceptible to noise. It is preferable to use an IC that uses a driving method that increases the null-to-noise ratio (S / N ratio). .

[0204] In this way, the image writing period and the sensing period by the detector element are independent. This prevents the sensing element from sensing noise caused by pixel writing noise. The decrease in the degree of reflection can be suppressed.

[0205] In one embodiment of the present invention, as shown in FIG. 8(D), one frame period includes a writing period and a detection period. Alternatively, as shown in FIG. 8E, one frame period may have one detection period. By providing a plurality of detection periods in one frame period, the detection sensitivity can be improved. For example, if one frame period has two to four detection periods, This is also fine.

[0206] [Example of top surface configuration of detector element] Next, examples of the top surface configuration of a sensing element included in an input / output device according to one embodiment of the present invention will be described with reference to FIGS. 1 will be used to explain.

[0207] 9A is a top view of the detector element. The detector element includes a conductive film 56a and a conductive film 56b. The conductive film 56a functions as one electrode of the sensing element, and the conductive film 56b functions as one electrode of the sensing element. The sensing element is formed between the conductive film 56a and the conductive film 56b. The capacitance generated can be used to detect the proximity or contact of a detection object. The conductive film 56a and the conductive film 56b have a comb-like upper surface shape or a slit-like upper surface shape. However, they are omitted here.

[0208] In one embodiment of the present invention, the conductive film 56a and the conductive film 56b are used as a common electrode of a liquid crystal element. It also has the function of.

[0209] The conductive films 56a arranged in the Y direction each extend in the X direction. In addition, the conductive films 56b arranged in the Y direction are connected to the conductive film 58 extending in the Y direction. In FIG. 9A, m conductive films 56a and n conductive films 56b are electrically connected. An example having a membrane 58 is shown.

[0210] In addition, the conductive film 56a may be provided in a plurality of positions in the X direction. In this case, the conductive film 56a extends in the Y direction. Also, the conductive film 58 extending in the X direction may be used to A plurality of conductive films 56b arranged in the same direction may be electrically connected to each other.

[0211] As shown in FIG. 9B, the conductive film 56 functioning as an electrode of the detection element is provided with a plurality of pixels 60. The conductive film 56 is provided over the conductive films 56a and 56b in FIG. The pixel 60 is made up of a number of sub-pixels each of which exhibits a different color. 1 shows an example in which a pixel 60 is composed of three sub-pixels 60a, 60b, and 60c.

[0212] In addition, the pair of electrodes of the detection element are electrically connected to the auxiliary wiring. In FIG. 10, the conductive film 56a is electrically connected to the auxiliary wiring 57a. In addition, the conductive film 56b is electrically connected to the auxiliary wiring 57b. In the example shown, the auxiliary wiring is provided overlapping the conductive film. The support member 10 may be provided so as to be folded.

[0213] The resistance of the conductive film that transmits visible light may be relatively high. It is preferable to reduce the resistance of each of the pair of electrodes of the sensing element by connecting the pair of electrodes to the sensing element. It is nice.

[0214] By reducing the resistance of the pair of electrodes of the detection element, the time constant of each of the pair of electrodes can be reduced. This can improve the detection sensitivity of the detection element and further reduce the This can improve the accuracy of detecting children.

[0215] In the writing period, as shown in FIG. 11A, the conductive film 56a extending in the X direction and the conductive film 56b extending in the Y direction are The conductive film 58 extending in the direction of the slit 56b is electrically connected to the conductive film 58. During the detection period, the common potential VCOM is input. On the other hand, as shown in FIG. Each of the conductive film 58 (and the conductive film 56b electrically connected to the conductive film 58) extending in the direction The conductive film 56a extending in the X direction is electrically connected to the detection circuit. It is electrically connected to an output circuit and a pulse voltage is input thereto.

[0216] [Example of pixel top surface configuration] Next, examples of top surface structures of pixels included in the input / output device of one embodiment of the present invention will be described with reference to FIGS. This will be explained using:

[0217] FIG. 12 is a top view of a pixel, and FIG. 13 shows the conductive film 252 in FIG. 12 by a dotted line. The stacking order of each layer is the same as that of the cross-sectional configuration example 1 (FIGS. 1(A) and 2(A)). It can be referred to.

[0218] The conductive films 251 each have an island-like upper surface shape and are arranged in a matrix. The conductive film 251 is electrically connected to the source or drain of the transistor 203a. It is being done.

[0219] The conductive film 252 is disposed so as to overlap with a plurality of conductive films 251. In addition, the conductive film 252 is provided with a slit at a position overlapping with the transistor 203a. The device has an opening at its location.

[0220] Here, the conductive film 251 functions as a pixel electrode of the liquid crystal element, and the conductive film 252 functions as a pixel electrode of the liquid crystal element. 12 and 13, the upper conductive film 252 functions as a common electrode. 13, an example is shown in which the conductive film 251 on the upper side is a pixel electrode and the conductive film 252 on the lower side is a pixel electrode. The lower conductive film may be a common electrode.

[0221] The conductive film 252 functions as an electrode of the sensing element.

[0222] In the region 277 indicated by the dashed line, the conductive film 275 and the conductive film 255 are electrically connected. The conductive film 255 functions as an auxiliary wiring for the conductive film 252 and is electrically connected to the conductive film 252. The conductive film 275 is made of the same material as the source and drain of the transistor 203a. , can be formed in the same process.

[0223] The conductive films 252 arranged in the Y direction correspond to the conductive film 56b in FIG. The conductive film 275 extending in the Y direction is the same as the conductive film 58 in FIG. The conductive films 252 arranged in the Y direction correspond to the conductive films 252 extending in the Y direction. The conductive film 252 is electrically connected to the conductive film 275 via the conductive film 255. In the case of using an oxide conductive film, it is preferable to connect the conductive film 252 and the conductive film 275 directly to each other. The conductive film 255 and the conductive film 275 formed of metal or alloy are connected to each other, and the conductive film 255 is The contact resistance can be reduced by electrically connecting the conductive film 252 and the conductive film 275. ,preferable.

[0224] 12 and 13 show an example in which the pixel 273 has three sub-pixels, but in one embodiment of the present invention, is not limited to this.

[0225] 14A and 14B show examples of the top surface shape of an electrode of a liquid crystal element.

[0226] The pixel electrode and the common electrode of the liquid crystal element 207 are not limited to being flat, and may be of various shapes. It may have an opening pattern (also called a slit), or it may have a bent portion or a branched comb-like shape. The shape may include

[0227] The liquid crystal element 207 shown in FIGS. 14(A) and 14(B) has a conductive layer that can function as a pixel electrode. The pixel has a conductive film 251 and a conductive film 252 that can function as a common electrode.

[0228] The transistor 203 shown in FIGS. 14A and 14B includes a gate electrode 221, an oxide semiconductor film The conductive film 251 has a drain electrode 223, a source electrode 225a, and a drain electrode 225b. It is electrically connected to the rain electrode 225b.

[0229] FIG. 14A shows an example in which the conductive film 251 has slits, and FIG. In this example, the film 251 has a comb-like shape. In the example shown, the conductive film 251 is located above the conductive film 252. It may be located above.

[0230] [Touch panel module] Next, a touch panel module including an input / output device according to one embodiment of the present invention and an IC will be described. This will be described with reference to FIG. 15 and FIG.

[0231] FIG. 15 shows a block diagram of the touch panel module 6500. The module 6500 includes a touch panel 6510 and an IC 6520. The input / output device of one embodiment of the present invention can be applied to the above.

[0232] The touch panel 6510 includes a display unit 6511, an input unit 6512, and a scanning line driver circuit 651 The display portion 6511 has a plurality of pixels, a plurality of signal lines, and a plurality of scanning lines. The input unit 6512 has a function of displaying an image. It has multiple detection elements that detect contact or proximity and functions as a touch sensor. The scanning line driver circuit 6513 has a function of outputting a scanning signal to the scanning lines of the display unit 6511. Yes.

[0233] For ease of explanation, the touch panel 6510 is configured as a display unit 6511. The input unit 6512 is shown separately, but it has a function of displaying an image and a function as a touch sensor. It is preferable to use a so-called in-cell type touch panel having both functions. The input / output device of one embodiment of the present invention is preferable because it is an in-cell touch panel.

[0234] The display unit 6511 supports HD (1280 x 720 pixels) and FHD (1920 x 108 0), WQHD (pixel count 2560 x 1440), WQXGA (pixel count 2560 x 1600 ), 4K (3840 x 2160 pixels), 8K (7680 x 4320 pixels) It is preferable for the image quality to be as high as possible, particularly 4K, 8K, or higher resolution. In addition, it is preferable that the pixel density (definition) of the pixels provided in the display portion 6511 is 300 ppi or more, preferably 500 ppi or more, more preferably 800 ppi or more, More preferably, the resolution is 1000 ppi or more, and even more preferably, 1200 ppi or more. Such a high-resolution and high-definition display 6511 makes it possible to For personal use such as at home, it is important to enhance the sense of realism and depth. It becomes possible.

[0235] The IC 6520 includes a circuit unit 6501, a signal line driver circuit 6502, and a sensor driver circuit 65 The circuit unit 6501 includes a timing controller 6503 and a detection circuit 6504. The image processing circuit 6505 includes an image processing circuit 6506.

[0236] The signal line driver circuit 6502 outputs an analog signal to a signal line of the display unit 6511. For example, the signal line driver circuit 6502 and In addition, the shift register circuit and the buffer circuit may be combined. The touch panel 6510 may also have a demultiplexer circuit connected to the signal lines. stomach.

[0237] The sensor driving circuit 6503 outputs a signal for driving the detection element of the input unit 6512. The sensor driver circuit 6503 includes, for example, a shift register circuit and a buffer A combination of circuits may be used.

[0238] The detection circuit 6504 receives an output signal from the detection element of the input section 6512 and outputs it to the circuit unit 6 For example, the detection circuit 6504 may include an amplifier circuit and an analog Equipped with a digital conversion circuit (ADC: Analog-Digital Converter) In this case, the detection circuit 6504 receives the output from the input unit 6512. The analog signal inputted is converted into a digital signal and outputted to the circuit unit 6501 .

[0239] The image processing circuit 6506 of the circuit unit 6501 is a display unit of the touch panel 6510. The function of generating and outputting a signal to drive the input section 6511 and the function of generating a signal to drive the input section 6512 are and a function of analyzing the signal output from the input unit 6512 and outputting the signal. and a function of outputting the same to the

[0240] As a more specific example, the image processing circuit 6506 performs the following in accordance with an instruction from the CPU 6540: The image processing circuit 6506 has a function of generating a video signal. The video signal is then subjected to signal processing in accordance with the received signal, converted into an analog video signal, and transmitted to the signal line drive circuit 65. The image processing circuit 6506 also has a function of supplying the image data to the CPU 6540. In accordance with the above, the sensor driver circuit 6503 generates a driving signal. The image processing circuit 6506 analyzes the signal input from the detection circuit 6504 and outputs it as position information. It has the function of outputting to the CPU 6540.

[0241] The timing controller 6505 also receives the video signal processed by the image processing circuit 6506. Based on the synchronization signals included in the It has a function of outputting to the scanning line driver circuit 6513 and the sensor driver circuit 6503. The timing controller 6505 determines the timing at which the detection circuit 6504 outputs a signal. The timing controller 6 may have a function of generating and outputting a signal corresponding to the timing. 505 is a signal to be output to the scanning line driver circuit 6513 and a signal to be output to the sensor driver circuit 6503. It is preferable that the display unit 6511 outputs a signal synchronized with the signal being output. The period during which the pixel data is rewritten and the period during which the input unit 6512 senses the pixel data are respectively For example, one frame period is preferably divided into a period for rewriting pixel data and a period for The touch panel 6510 can be driven in separate periods for sensing and disabling. For example, by providing two or more sensing periods in one frame period, the detection sensitivity and detection accuracy can be improved. The degree can be increased.

[0242] The image processing circuit 6506 may have a processor, for example. For example, DSP (Digital Signal Processor), GPU (Graphics Processing Unit) Microprocessors such as the Intelligent Microprocessing Unit (MICS) can be used. These microprocessors can also be implemented as FPGAs (Field Programmable Gate Arrays). e Gate Array) and FPAA (Field Programmable An PLDs (Programmable Logic Devices) such as The processor may execute various programs. It performs various data processing and program control by interpreting and executing instructions. The program that can be executed by the above may be stored in a memory area of ​​the processor. Alternatively, the information may be stored in a separately provided storage device.

[0243] Note that the display portion 6511 or the scanning line driver circuit 6513 of the touch panel 6510, The circuit unit 6501, the signal line driver circuit 6502, and the sensor driver circuit included in the IC 6520 6503, or a detection circuit 6504, or an external CPU 6540, etc. A transistor that uses an oxide semiconductor in the panel formation region and has an extremely low off-state current is used. Since the off-state current of the transistor is extremely low, The capacitor functions as a memory element, and the switch is used to hold the charge (data) that has flowed into the capacitor. By using it as a switch, data retention period can be secured for a long period. For example, This characteristic is used for at least one of the register and cache memory of the image processing circuit 6506. By doing so, the image processing circuit 6506 operates only when necessary, and in other cases, the previous processing By storing the information in the storage element, normally-off computing becomes possible. This enables the touch panel module 6500 and the electronic device in which it is mounted to have low power consumption. This will enable us to strengthen our capabilities.

[0244] In this example, the circuit unit 6501 is a timing controller 6505 and an image processing circuit. However, the image processing circuit 6506 itself or the image processing circuit 6506 A circuit having some of the functions of the image processing circuit 6506 may be provided externally. For example, the circuit unit 6501 may be a signal processor. A signal line driver circuit 6502, a sensor driver circuit 6503, a detection circuit 6504, and a timing controller It may also be configured with a controller 6505.

[0245] In this example, the IC 6520 includes the circuit unit 6501. The 6501 can be configured not to be included in the IC6520. In this case, the IC6520 is A configuration including a signal line driver circuit 6502, a sensor driver circuit 6503, and a detection circuit 6504. For example, when multiple ICs are mounted on the touch panel module 6500, In the touch panel module 6500, a circuit unit 6501 is provided outside the touch panel module 6500. It is also possible to arrange a plurality of ICs 6520 that do not have a slot 6501, or to arrange ICs 6520 and It is also possible to combine and arrange an IC having only the signal line driver circuit 6502 .

[0246] In this way, the touch panel 6510 has a function of driving the display unit 6511 and an input unit 6512. The touch panel module is made by incorporating the function to drive the touch panel and the touch panel driver into a single IC. This reduces the number of ICs mounted on the module 6500, which reduces costs. do.

[0247] 16(A), (B), and (C) show a touch panel module 65 equipped with IC 6520. 00 is a schematic diagram.

[0248] In FIG. 16A, a touch panel module 6500 includes a substrate 6531 and an opposing substrate 653 2. It has multiple FPC6533, IC6520, IC6530, etc. Also has a board 6531 A display portion 6511, an input portion 6512, and a scanning line driver circuit 65 are disposed between the substrate 6532 and the counter substrate 6532. 13. The IC6520 and IC6530 are mounted using a COG method or other mounting method. It is mounted on board 6531.

[0249] The IC6530 is the above-mentioned IC6520, except that only the signal line driver circuit 6502 or The IC 6520 includes a signal line driver circuit 6502 and a circuit unit 6501. Signals are supplied to IC6530 from the outside via FPC6533. 33, a signal is output from at least one of IC6520 and IC6530 to the outside. It is possible.

[0250] In FIG. 16A, two scanning line driver circuits 6513 are provided so as to sandwich a display portion 6511. Also shown is a configuration having IC6530 in addition to IC6520. Such a configuration can be suitably used when the display unit 6511 has an extremely high resolution. can.

[0251] Figure 16(B) shows an example of mounting one IC6520 and one FPC6533. In this way, by consolidating the functions into one IC6520, the number of parts can be reduced. In FIG. 16B, the scanning line driver circuit 6513 is connected to the display portion 6511. This shows an example of placement along the side closest to the FPC6533 of the two short sides.

[0252] FIG. 16C shows a PCB (Printed Circuit) on which an image processing circuit 6506 and the like are mounted. The figure shows an example of a configuration having an IC on a substrate 6531. 6520 and IC6530 are electrically connected to PCB6534 by FPC6533. Here, the IC 6520 does not have the image processing circuit 6506 described above. can be applied.

[0253] In each diagram of FIG. 16, IC6520 and IC6530 are mounted on a substrate 6531. Instead, it may be mounted on FPC6533. For example, IC6520 and IC6530 can be mounted on the FPC6533 using mounting methods such as the COF method or the TAB method. Cut.

[0254] As shown in FIG. 16(A) and (B), the FPC 6533 and the IC The configuration in which IC6520 (and IC6530) etc. are arranged allows for a narrow frame, so for example It can be suitably used in electronic devices such as smartphones, mobile phones, and tablet terminals. In addition, the configuration using PCB6534 as shown in FIG. 16(C) is suitable for use in televisions, for example. Suitable for use in mobile devices, monitors, tablet terminals, and notebook personal computers. It can be used appropriately.

[0255] This embodiment mode can be combined with other embodiment modes as appropriate.

[0256] (Embodiment 2) In this embodiment, a manufacturing method of an input / output device of one embodiment of the present invention will be described with reference to FIGS. In this embodiment, a method for manufacturing a transistor will be mainly described. For the materials, reference can be made to the description in embodiment 1.

[0257] First, the gate electrode 221 is formed on the substrate 211. Then, the substrate 211 and the gate electrode An insulating film 213 including insulating films 106 and 107 is formed on the film 221 (FIG. 17(A)).

[0258] In this embodiment, a glass substrate is used as the substrate 211, and a tongue is used as the gate electrode 221. A stainless steel film is used as the insulating film 106, and a silicon nitride film capable of releasing hydrogen is used as the insulating film 107. For the insulating film 107, a silicon oxide film capable of releasing oxygen is used.

[0259] The insulating film 106 functions as a blocking film that suppresses oxygen permeation. For example, At least one of the insulating film 107, the insulating film 215, the insulating film 217, and the oxide semiconductor film 223 When excess oxygen is supplied to either layer, the insulating film 106 suppresses the permeation of oxygen. It is possible.

[0260] Note that the insulating film in contact with the oxide semiconductor film 223 which functions as a channel region of the transistor The insulating film 107 is preferably an oxide insulating film containing oxygen in excess of the stoichiometric composition. In other words, the insulating film 107 has a region where the oxygen content is excessive. The insulating film 107 is capable of releasing oxygen. For example, the insulating film 107 can be formed in an oxygen atmosphere. Oxygen may be introduced into the insulating film 107 to form an oxygen excess region. The following methods are used: ion implantation, ion doping, plasma immersion ion implantation, plasma Processing such as masking can be used.

[0261] When hafnium oxide is used for one or both of the insulating films 106 and 107, Hafnium oxide has the following advantages: Therefore, compared with the case where silicon oxide is used, the insulating film 106 and the insulating film Since the thickness of one or both of the layers 107 can be increased, the leakage current due to the tunnel current can be reduced. That is, a transistor with a small off-state current can be realized. Furthermore, hafnium oxide having a crystalline structure has a higher melting point than hafnium oxide having an amorphous structure. Therefore, in order to make a transistor with a small off-current, It is preferable to use hafnium oxide having a crystal structure. Examples of the crystal system include a crystalline system such as a cubic system and a crystalline system. However, one embodiment of the present invention is not limited to these. .

[0262] In this embodiment, a silicon nitride film is formed as the insulating film 106, and a silicon nitride film is formed as the insulating film 107. The silicon nitride film has a lower dielectric constant than the silicon oxide film. The film thickness required to obtain the same capacitance as a silicon oxide film is large. The insulating film 213 that functions as the gate insulating film of the insulating film 213 includes a silicon nitride film. This makes it possible to physically thicken the insulating film. Furthermore, the dielectric strength can be improved, and electrostatic breakdown of the transistor can be suppressed.

[0263] The gate electrode 221 is formed by depositing a conductive film on the substrate 211 and then depositing the conductive film in a desired region. The pattern can be formed by patterning the area and then etching away the unnecessary areas.

[0264] Next, an oxide semiconductor film 223 is formed on the insulating film 213 at a position overlapping with the gate electrode 221. (Figure 17(B)).

[0265] In this embodiment, the oxide semiconductor film 223 is an In—Ga—Zn oxide film (In:Ga A metal oxide target with an atomic ratio of a:Zn=1:1:1.2 is used.

[0266] The oxide semiconductor film 223 was formed by depositing an oxide semiconductor film over the insulating film 213 and then The conductive film is patterned so that the desired area remains, and then the unnecessary area is etched away. It can be formed by:

[0267] After the oxide semiconductor film 223 is formed, heat treatment is preferably performed. 50°C or less, preferably 300°C to 500°C, more preferably 350°C to 450°C At temperatures below ℃, in an inert gas atmosphere, an atmosphere containing 10 ppm or more of oxidizing gas, or reduced pressure The heat treatment can be performed in an inert gas atmosphere. In order to compensate for oxygen released from the oxide semiconductor film 223, an oxidizing gas is added at 10 ppm or more. The heat treatment here may be performed in a fluorine-containing atmosphere. Impurities such as hydrogen and water can be removed from at least one of the conductive films 223. The heat treatment may be performed before the oxide semiconductor film 223 is processed into an island shape.

[0268] Note that the transistor in which the oxide semiconductor film 223 is used as a channel region can have stable electrical characteristics. In order to achieve this, impurities in the oxide semiconductor film 223 are reduced so that the oxide semiconductor film 223 becomes a pure oxide semiconductor film. It is advantageous to make the ion exchange material true or substantially true.

[0269] Next, a conductive film is formed over the insulating film 213 and the oxide semiconductor film 223. Then, the unnecessary areas are etched away to form the insulating film 21. 3 and a source electrode 225a and a drain electrode 225b are formed on the oxide semiconductor film 223. (Figure 17(C)).

[0270] In this embodiment, the source electrode 225a and the drain electrode 225b are made of tungsten. It uses a three-layer laminate structure of a silicon film, an aluminum film, and a titanium film.

[0271] After the source electrode 225a and the drain electrode 225b are formed, the oxide semiconductor film 223 The surface of the substrate may be cleaned. The cleaning method may be, for example, cleaning using a chemical solution such as phosphoric acid. By cleaning with a chemical solution such as phosphoric acid, the surface of the oxide semiconductor film 223 is Impurities attached to the source electrode 225a and the drain electrode 225b (for example, However, this cleaning is not always necessary and may be omitted depending on the circumstances. In some cases, cleaning may not be necessary.

[0272] In addition, the process of forming the source electrode 225a and the drain electrode 225b and the cleaning process In either one or both of the source electrode 225a and the drain electrode 225b of the oxide semiconductor film 223, The area exposed from the pin electrode 225b may become thin.

[0273] Next, the insulating film 213, the oxide semiconductor film 223, the source electrode 225a, and the drain electrode 2 An insulating film 215 including the insulating films 114 and 116 is formed on the insulating film 25b. The desired area is patterned so that it remains, and then the unnecessary area is etched away to open the A mouth 141 is formed (FIG. 17(D)).

[0274] After the insulating film 114 is formed, the insulating film 116 is successively formed without exposing the insulating film 114 to the air. After the insulating film 114 is formed, it is preferable to adjust the flow rate, pressure, and frequency of the source gas without exposing the insulating film 114 to the atmosphere. By adjusting one or more of the wave power and the substrate temperature, the insulating film 116 is continuously formed, thereby forming an insulating The concentration of impurities derived from atmospheric components can be reduced at the interface between the film 114 and the insulating film 116. At the same time, oxygen contained in the insulating films 114 and 116 is transferred to the oxide semiconductor film 223. As a result, the amount of oxygen vacancies in the oxide semiconductor film 223 can be reduced.

[0275] In addition, in the step of forming the insulating film 116, the insulating film 114 serves as a protective film for the oxide semiconductor film 223. Therefore, it is possible to reduce damage to the oxide semiconductor film 223 and increase the power density. The insulating film 116 can be formed using low high frequency power.

[0276] In this embodiment, the insulating films 114 and 116 are formed of oxynitride film capable of releasing oxygen. A silicon membrane is used.

[0277] The insulating film 114 in contact with the oxide semiconductor film 223 which functions as a channel region of the transistor The insulating film is preferably an oxide insulating film, and an insulating film capable of releasing oxygen is used. In other words, an insulating film capable of releasing oxygen is one that contains more oxygen than the stoichiometric composition. The insulating film 114 has an oxygen excess region. In order to provide the insulating film 114, for example, the insulating film 114 can be formed in an oxygen atmosphere. Alternatively, oxygen may be introduced into the insulating film 114 after it is formed to form an oxygen excess region. The methods include ion implantation, ion doping, and plasma immersion ion implantation. , plasma treatment, etc. can be used.

[0278] By using an insulating film capable of releasing oxygen as the insulating film 114, Oxygen is transferred to the oxide semiconductor film 223 which functions as a channel region of the oxide semiconductor film 223. For example, it is possible to reduce the amount of oxygen vacancies in 223 by thermal desorption spectroscopy (T DS (Thermal Desorption Spectroscopy) analysis The surface temperature of the film measured by the method is 100°C or higher and 700°C or lower, or 100°C or higher. The amount of oxygen molecules released at 500℃ or less is 1.0×10 18 molecule / cm 3 That's it By using an insulating film, the amount of oxygen vacancies in the oxide semiconductor film 223 can be reduced. can be done.

[0279] In addition, it is preferable that the insulating film 114 has a small number of defects. Typically, the insulating film 114 has a small number of defects as determined by ESR measurement. , the spin density of the signal at g=2.001 originating from silicon dangling bonds is 3×10 17 spins / cm 3 This is because the insulating film 114 contains If the density of defects is high, oxygen will be bonded to the defects, and the oxygen in the insulating film 114 will be In addition, the amount of light transmitted between the insulating film 114 and the oxide semiconductor film 223 is reduced. It is preferable that the number of defects at the interface is small. Typically, the oxide semiconductor is The spin density of the signal that appears when the g value due to defects in the conductive film 223 is between 1.89 and 1.96 Degree is 1×10 17 spins / cm 3 or less, and more preferably, less than the lower detection limit. .

[0280] In addition, in the insulating film 114, all of the oxygen that has entered the insulating film 114 from the outside is Alternatively, some of the oxygen that has entered the insulating film 114 from the outside may move to the outside of the insulating film 114. In some cases, oxygen may enter the insulating film 114 from the outside, and the insulating film 114 may become insulated. When oxygen contained in the insulating film 114 moves to the outside of the insulating film 114, In some cases, oxygen may move due to the oxide film that can transmit oxygen as the insulating film 114. When the insulating film 114 is formed, oxygen desorbed from the insulating film 116 is formed on the insulating film 114. The oxide semiconductor film 223 can be transferred through the insulating film 114.

[0281] The insulating film 114 is formed using an oxide insulating film having a low density of states caused by nitrogen oxides. Note that the density of states caused by the nitrogen oxides can be determined by the valence charge of the oxide semiconductor film. The energy at the top of the nucleus (E V_OS ) and the conduction band minimum of the oxide semiconductor film ( E C_OS As the oxide insulating film, a nitrogen oxide film may be formed between the insulating film and the insulating film. Silicon oxynitride film with low emission or aluminum oxynitride film with low emission of nitrogen oxide A rubber film or the like can be used.

[0282] In addition, the silicon oxynitride film, which emits a small amount of nitrogen oxide, was found to emit a small amount of nitrogen oxide in the TDS analysis. This is a membrane that releases more ammonia than chlorides, and typically releases ammonia molecules. The amount is 1×10 18 molecule / cm 3 5×10 or more 19 molecule / cm 3 The following is the case. The amount of NiA released is determined when the surface temperature of the film is 50°C or higher and 650°C or lower, preferably 50°C or higher and 550°C or lower. The amount released is determined by heating at or below ℃.

[0283] Nitrogen oxides (NO x , x is greater than 0 and less than or equal to 2, preferably greater than or equal to 1 and less than or equal to 2), typically NO or NO forms a level in the insulating film 114 or the like. The level is 23. Therefore, the nitrogen oxide is in the insulating film 114 and the oxide When the charge-transfer level diffuses to the interface of the compound semiconductor film 223, the charge-transfer level traps electrons on the insulating film 114 side. As a result, the trapped electrons may be trapped in the insulating film 114 and the oxide semiconductor Since it remains near the interface of the film 223, it shifts the threshold voltage of the transistor in the positive direction. It ends up like this.

[0284] Nitrogen oxide reacts with ammonia and oxygen during heat treatment. The nitrogen oxide contained therein reacts with ammonia contained in the insulating film 116 during heat treatment. Therefore, nitrogen oxides contained in the insulating film 114 are reduced. Electrons are less likely to be trapped at the interface with the oxide semiconductor film 223.

[0285] By using the oxide insulating film as the insulating film 114, the threshold voltage of the transistor can be reduced. It is possible to reduce the shift and the variation in the electrical characteristics of the transistor. Cut.

[0286] The heat treatment in the manufacturing process of the transistor is typically performed at a temperature of less than 400° C. or less than 375° C. ( The insulating film 114 is heated at 100 K or more (preferably at a temperature of 340° C. or more and 360° C. or less). In the spectrum obtained by measuring the following ESR, the g value is 2.037 or more and 2.039 or less. The first signal below, the second signal with a g-value between 2.001 and 2.003, and the g-value The third signal is observed, which is between 1.964 and 1.966. and the split width of the second signal, and the split width of the second signal and the third signal. The bit width is about 5 mT in the X-band ESR measurement. The first signal is less than or equal to 2.039, the second signal is greater than or equal to 2.001 and less than or equal to 2.003. The sum of the spin densities of the third signal with g values ​​between 1.964 and 1.966 is 1×10 18 spins / cm 3 is less than 1×10 17 spins / cm 3 More than 1×10 18 spins / cm 3 is less than.

[0287] In addition, in the ESR spectrum below 100K, the g value is 2.037 to 2.039. The first signal, the second signal with a g value between 2.001 and 2.003, and the g value between 1. The third signal, between 964 and 1.966, is nitrogen oxide (NO x , x is greater than 0 2 or less, preferably 1 to 2). Representative examples of nitrogen oxides include Examples of nitrogen oxide include nitrogen monoxide and nitrogen dioxide. A first signal, a second signal with a g value of 2.001 to 2.003, and a g value of 1 The lower the sum of the spin densities of the third signals (between .964 and 1.966), the higher the oxidation It can be said that the content of nitrogen oxides in the insulating film is small.

[0288] The nitrogen concentration of the oxide insulating film measured by SIMS is 6×10 20 atoms / cm 3 The following is the result.

[0289] PECV using silane and nitrous oxide with a substrate temperature of 220°C to 350°C By forming the oxide insulating film using the D method, a dense and hard film can be formed. It can be achieved.

[0290] The insulating film 116 formed in contact with the insulating film 114 has a stoichiometric composition of oxygen. The oxide insulating film contains more oxygen than the stoichiometric composition. When an oxide insulating film containing a large amount of oxygen is heated, some of the oxygen is released. The oxide insulating film containing more oxygen than satisfies the condition is converted to oxygen atoms by TDS analysis. The amount of oxygen released is 1.0×10 19 atoms / cm 3 More than 3.0x1, preferably 0 20 atoms / cm 3 The oxide insulating film is as described above. The surface temperature of the film is in the range of 100°C to 700°C or 100°C to 500°C. The range is preferably 100-200 mm.

[0291] In addition, it is preferable that the insulating film 116 has a small amount of defects. Typically, the insulating film 116 has a small amount of defects as determined by ESR measurement. , the spin density of the signal at g=2.001 originating from silicon dangling bonds is 1.5×10 18 spins / cm 3 Less than or even 1×10 18 spins / cm 3 below Note that the insulating film 116 is preferably an oxide semiconductor film as compared with the insulating film 114. Since it is separated from the insulating film 223, it is acceptable for the insulating film 223 to have a higher defect density than the insulating film 114.

[0292] The thickness of the insulating film 114 is 5 nm or more and 150 nm or less, preferably 5 nm or more and 50 nm or less. The thickness of the insulating film 116 is preferably 30 nm or more and more preferably 10 nm or more and 30 nm or less. The thickness can be 0 nm or more and 500 nm or less, preferably 150 nm or more and 400 nm or less. do.

[0293] In addition, the insulating films 114 and 116 can be formed using insulating films made of the same material. In some cases, the interface between the insulating film 114 and the insulating film 116 may not be clearly visible. In the embodiment, the interface between the insulating film 114 and the insulating film 116 is illustrated by a dashed line. In this embodiment, the two-layer structure of the insulating film 114 and the insulating film 116 has been described. However, the present invention is not limited to this. For example, the insulating film 114 may have a single layer structure, the insulating film 116 may have a single layer structure, or It may have a laminated structure of three or more layers.

[0294] After the insulating films 114 and 116 are formed, heat treatment (hereinafter referred to as first heat treatment) is performed. The first heat treatment is preferably performed to remove nitrogen oxides contained in the insulating films 114 and 116. Alternatively, the first heat treatment can reduce the amount of oxides contained in the insulating films 114 and 116. Part of the oxygen contained in the oxide semiconductor film 223 is moved to the oxide semiconductor film 223. The amount of oxygen deficiency can be reduced.

[0295] The temperature of the first heat treatment is typically less than 400° C., preferably less than 375° C., and The temperature is preferably 150° C. or higher and 350° C. or lower. The first heat treatment is carried out in the presence of nitrogen, oxygen, or ultra-drying. Air (water content is 20 ppm or less, preferably 1 ppm or less, more preferably 10 ppm or less) This can be done under an atmosphere of air (<300 nm) or rare gas (argon, helium, etc.). It is preferable that the nitrogen, oxygen, ultra-dry air, or rare gas does not contain hydrogen, water, or the like. The heat treatment is carried out using an electric furnace, RTA (Rapid Thermal Anneal), etc. There can be.

[0296] The opening 141 is formed so as to expose the drain electrode 225b. As a method for forming the opening 14, for example, a dry etching method can be used. The method for forming 1 is not limited to this, and may be a wet etching method or a dry etching method. The opening 141 may be formed by a combination of a bonding method and a wet etching method. The thickness of the drain electrode 225b may be reduced by the etching process for forming the drain electrode 225b. be.

[0297] Next, an oxide conductive film 227 that will be formed later is formed on the insulating film 116 so as to cover the opening 141. A semiconductor film is formed (FIGS. 18(A) and 18(B)).

[0298] Note that FIG. 18A illustrates the inside of a film formation apparatus when an oxide semiconductor film is formed over the insulating film 116. FIG. 18(A) is a schematic cross-sectional view of a sputtering device used as a film forming device. A target 193 is installed inside the sputtering device, and a The formed plasma 194 is shown diagrammatically.

[0299] First, when forming an oxide semiconductor film, plasma is discharged in an atmosphere containing a third oxygen gas. At that time, oxygen is added to the insulating film 116 which is a surface on which the oxide semiconductor film is to be formed. In addition, when the oxide semiconductor film is formed, an inert gas (e.g., For example, argon gas may be mixed with other gases such as helium gas, argon gas, and xenon gas. The flow rate of the third oxygen gas is set higher than that of the argon gas. It is preferable to increase the flow rate of the third oxygen gas. For example, the oxide semiconductor film can be formed under the following conditions: The ratio of the third oxygen gas in the entire deposition gas is set to 50% or more and 100% or less, preferably It can be between 80% and 100%.

[0300] In FIG. 18A, oxygen or excess oxygen added to the insulating film 116 is broken down as a schematic diagram. It is represented by a line arrow.

[0301] The substrate temperature during the formation of the oxide semiconductor film is preferably from room temperature to 340° C. Preferably, the temperature is from room temperature to 300° C., more preferably from 100° C. to 250° C., and even more preferably The temperature is 100° C. or higher and 200° C. or lower. The crystallinity of the semiconductor film can be improved. On the other hand, the substrate 211 is a large glass substrate. When using a semiconductor device (e.g., 6th to 10th generation), the substrate temperature during the formation of the oxide semiconductor film If the temperature is set to 150° C. or higher and lower than 340° C., the substrate 211 may deform (distort or warp). Therefore, when a large glass substrate is used, the oxide semiconductor film is formed on the large glass substrate. By keeping the substrate temperature at 100°C or higher but lower than 150°C during the process, deformation of the glass substrate can be suppressed. This can be done.

[0302] In this embodiment, an In-Ga-Zn metal oxide target (In:Ga:Zn=1:3) is used. :6 [atomic ratio]) by a sputtering method to form an oxide semiconductor film.

[0303] Next, the oxide semiconductor film is processed into a desired shape to form an island-shaped oxide semiconductor film 227a. (Figure 18(C)).

[0304] The oxide semiconductor film 227a is formed by depositing an oxide semiconductor film over the insulating film 116 and then The film is patterned to leave the desired areas and then etched away the unwanted areas. It can be formed.

[0305] Next, the insulating film 217 is formed over the insulating film 116 and the oxide semiconductor film 227a (FIG. 19( A)).

[0306] The insulating film 217 can block oxygen, hydrogen, water, alkali metals, alkaline earth metals, etc. By providing the insulating film 217, oxygen from the oxide semiconductor film 223 can be prevented from being generated. The oxygen in the insulating film 215 is diffused to the oxide semiconductor film 214 from the outside. It can prevent hydrogen, water, alkali metals, alkaline earth metals, etc. from entering 223. .

[0307] The insulating film 217 preferably contains either hydrogen or nitrogen, or both. For example, a silicon nitride film is preferably used as the insulating film 217. For example, the film can be formed by sputtering or PECVD. For example, when the insulating film 217 is formed by the PECVD method, the substrate temperature is preferably less than 400° C. The temperature is preferably less than 375° C., more preferably 180° C. or higher and 350° C. or lower. By setting the substrate temperature in the above range when depositing the film, it is possible to form a dense film, which is preferable. In addition, by setting the substrate temperature in the above range when forming the insulating film 217, the insulating film 1 Oxygen or excess oxygen in the oxide semiconductor film 14 or 116 can be moved to the oxide semiconductor film 223. become.

[0308] In addition, it has a blocking effect against oxygen, hydrogen, water, alkali metals, alkaline earth metals, etc. Instead of a nitride insulating film, an oxide insulating film having a blocking effect against oxygen, hydrogen, water, etc. is used. As the oxide insulating film having a blocking effect against oxygen, hydrogen, water, and the like, an oxide insulating film having an oxide blocking effect against oxygen, hydrogen, water, and the like may be provided. Aluminum oxide, aluminum oxynitride, gallium oxide, gallium oxynitride, yttrium oxide Examples of oxides that can be used include hafnium oxide, hafnium oxynitride, yttrium oxide, hafnium oxide nitride, and the like.

[0309] After the insulating film 217 is formed, a heat treatment similar to the first heat treatment described above (hereinafter, the first heat treatment) is performed. In this manner, the oxide semiconductor film that becomes the oxide conductive film 227 may be formed by the heat treatment of the oxide semiconductor film 227. After oxygen is added to the insulating film 116 during the formation of the conductor film, the insulating film 116 is heated at a temperature of less than 400° C., preferably at 37° C. By carrying out a heat treatment at a temperature of less than 5°C, more preferably at a temperature of 180°C or higher and 350°C or lower, In this case, oxygen or excess oxygen in the insulating film 116 is transferred to the oxide semiconductor film 223, and the oxide semiconductor This can compensate for the oxygen deficiency in the membrane 223.

[0310] Here, oxygen moving into the oxide semiconductor film 223 will be described with reference to FIG. FIG. 20 shows the temperature of the substrate during the formation of the insulating film 217 (typically less than 375° C.) or the temperature of the insulating film 21 The oxide semiconductor film 22 is formed by a second heat treatment (typically at a temperature lower than 375° C.) after the formation of the oxide semiconductor film 22. 20 is a model diagram showing oxygen moving into the oxide semiconductor film 223. The oxygen (oxygen radical, oxygen atom, or oxygen molecule) migrating to the oxygen atom is represented by a dashed arrow. FIG. 20 is a cross-sectional view of the transistor and its vicinity after the insulating film 217 is formed.

[0311] The oxide semiconductor film 223 shown in FIG. 20 is a film in contact with the oxide semiconductor film 223 (here, an insulating film). Oxygen vacancies are compensated for by the migration of oxygen from the insulating film 107 and the insulating film 114. In the input / output device of one embodiment of the present invention, When oxygen gas is used to add oxygen to the insulating film 107 during sputtering, the insulating The film 107 has an excess oxygen region. In the sputtering process, oxygen is added to the insulating film 116 using oxygen gas. 116 has an excess oxygen region. Therefore, the oxide sandwiched between the insulating films having the excess oxygen region In the organic semiconductor film 223, oxygen vacancies are suitably compensated for.

[0312] In addition, the insulating film 106 is provided below the insulating film 107, and the insulating films 114 and 116 An insulating film 217 is provided above the insulating films 106 and 217. By forming the insulating films 107, 114, and 116 from a material such as silicon nitride, Since oxygen contained in the oxide semiconductor film 223 can be trapped on the oxide semiconductor film 223 side, Oxygen can be transferred to the semiconductor film 223 .

[0313] In addition, the insulating film 217 preferably has a function of reducing the resistivity of the oxide conductive film 227. I wish.

[0314] By forming the insulating film 217 containing either hydrogen or nitrogen or both, the insulating film 2 The oxide semiconductor film 227a in contact with the oxide semiconductor film 17 is doped with either hydrogen or nitrogen or both. As a result, the carrier density of the oxide semiconductor film 227a is increased, and the oxide conductive film It can function as:

[0315] As the resistivity of the oxide semiconductor film 227a decreases, the oxide conductive film 227b is It is shown as membrane 227 .

[0316] The resistivity of the oxide conductive film 227 is at least lower than that of the oxide semiconductor film 223, and is preferably is 1 x 10 -3 Ωcm or more 1×10 4 Less than Ωcm, more preferably less than 1×10 -3 Ω cm or more 1×10 -1 It is preferable that the resistivity is less than Ωcm.

[0317] Next, an insulating film 219 is formed on the insulating film 217, and desired regions of the insulating films 217 and 219 are left. Then, the unnecessary area is etched to form the opening 142. (Figure 19(B)).

[0318] In this embodiment, the insulating film 219 is made of an acrylic resin.

[0319] The opening 142 is formed so as to expose the drain electrode 225b. As a method for forming the opening 14, for example, a dry etching method can be used. The method for forming 2 is not limited to this, and may be a wet etching method or a dry etching method. The opening 142 may be formed by a combination of a bonding method and a wet etching method. The thickness of the drain electrode 225b may be reduced by the etching process for forming the drain electrode 225b. be.

[0320] In addition, the step of forming the opening 142 is performed without performing the step of forming the opening 141 described above. The openings may be formed continuously in the insulating films 114, 116, 217, and 219. This makes it possible to reduce the manufacturing process of the input / output device of one embodiment of the present invention. This allows production costs to be reduced.

[0321] Next, a conductive film is formed on the insulating film 219 so as to cover the opening 142, and a desired region of the conductive film is The conductive film 25 is patterned so that unnecessary regions remain, and then the unnecessary regions are etched away. Further, an insulating film 253 is formed on the conductive film 251. Next, A conductive film is formed on the substrate, and the conductive film is patterned so that a desired region of the conductive film remains. Then, the unnecessary region is removed. The conductive film 255 is formed by etching the region. A conductive film is formed on the film 255 and patterned so that a desired region of the conductive film remains. After that, unnecessary regions are etched to form a conductive film 252 (FIG. 19(C)).

[0322] In this embodiment, an ITO film is used as the conductive film 251 and the conductive film 252, and an insulating film 253 is used. A silicon nitride film was used as the conductive film 255, and an alloy of silver, palladium and copper (Ag-P A d-Cu (also referred to as APC) membrane is used.

[0323] The conductive film 252 and the conductive film 255 may be formed in any order. It is preferable that the conductive film 255 is formed before the conductive film 252 is formed by etching. It is possible to reduce the damage received.

[0324] Note that the conductive film 251 is formed using an oxide semiconductor film by a method similar to that for the oxide conductive film 227. In this case, the insulating film 253 formed on the conductive film 251 may be the insulating film 217. In addition, a material that can be used for the above-mentioned can be used for forming an oxide semiconductor film. The conductive film 252 may be formed by performing treatment to reduce the resistivity of the oxide semiconductor film. .

[0325] Through the above steps, the transistor 203b and the pair of electrodes of the liquid crystal element shown in FIG. It can be made.

[0326] Although the insulating film 219 is provided in FIG. 19C, the insulating film 219 is not provided. The configuration may be as follows (FIG. 21).

[0327] This embodiment mode can be combined with other embodiment modes as appropriate.

[0328] (Embodiment 3) In this embodiment, a transistor that can be used for an input / output device of one embodiment of the present invention will be described. The materials for each layer will be described with reference to FIGS. 22 to 25. Please refer to the above.

[0329] <Transistor configuration example 1> FIG. 22A is a top view of a transistor 270, and FIG. 22B is a top view of the transistor 270 shown in FIG. FIG. 22(C) is a cross-sectional view taken along dashed line A1-A2, and FIG. 22(D) is a cross-sectional view taken along dashed line B1-B2. The dashed dotted line A1-A2 direction is the channel length direction, and the dashed dotted line B1-B2 direction is the channel length direction. This may be referred to as the channel width direction.

[0330] The transistor 270 includes a conductive film 504 over a substrate 502, the conductive film 504 serving as a first gate electrode, and a an insulating film 506 on the substrate 502 and the conductive film 504; an insulating film 507 on the insulating film 506; The oxide semiconductor film 508 over the insulating film 507 and the insulating film 508 The conductive film 512a serving as a source electrode and the oxide semiconductor film 508 The conductive film 512b functions as a drain electrode, and the oxide semiconductor film 508 and the conductive film 512 The insulating films 514 and 516 on the conductive film 512a and the conductive film 512b, and the oxide conductive film 51 on the insulating film 516 An insulating film 518 is provided over the oxide conductive film 511b.

[0331] In the transistor 270, the insulating film 514 and the insulating film 516 The oxide semiconductor film 511a functions as a second gate insulating film. 14 and the insulating film 516 through an opening 552c. The oxide semiconductor film 511a functions as, for example, a pixel electrode of a display element. In addition, in the transistor 270, the oxide conductive film 511b is a second gate electrode (back gate electrode). It functions as a gate electrode.

[0332] As shown in FIG. 22C, the oxide conductive film 511b is formed by insulating films 506 and 507 and insulating The first gate electrode is formed in the openings 552a and 552b in the film 514 and the insulating film 516. The conductive film 504 functions as a conductive electrode. The same potential is applied to 511b.

[0333] In this embodiment, the openings 552a and 552b are provided, and the oxide conductive film 511 b and the conductive film 504 are connected to each other. Only one of the openings 552a and 552b is formed, and the oxide conductive film 5 11b and the conductive film 504 are connected, or the openings 552a and 552b are not provided. Alternatively, the oxide conductive film 511b and the conductive film 504 may not be connected to each other. In the case where the conductive film 511b and the conductive film 504 are not connected, the oxide conductive film 511b and the conductive film Each of the electrodes 504 can be given a different potential.

[0334] As shown in FIG. 22B, the oxide semiconductor film 508 functions as a first gate electrode. The conductive film 504 functions as a second gate electrode, and the oxide conductive film 511b functions as a second gate electrode. It is located opposite to the gate electrode and is sandwiched between two conductive films that function as gate electrodes. The length in the channel length direction of the oxide conductive film 511b functioning as the gate electrode of The length in the channel width direction is the sum of the length in the channel length direction and the channel width direction of the oxide semiconductor film 508. The length of the oxide semiconductor film 508 is longer than that of the insulating film 514 and the insulating film 51. 6. Also, the second gate electrode 511b is covered with the oxide conductive film 511b. The oxide conductive film 511b and the conductive film 504 functioning as the first gate electrode are formed by insulating film 5 06, 507, the insulating film 514 and the openings 552a, 552b provided in the insulating film 516. In order to form a connection in the channel width direction, the side surface of the oxide semiconductor film 508 is covered with the insulating film 514. and faces the oxide conductive film 511b functioning as a second gate electrode with the insulating film 516 interposed therebetween. is doing.

[0335] In other words, in the channel width direction of the transistor 270, The conductive film 504 functioning as the second gate electrode and the oxide conductive film 511b functioning as the second gate electrode are The insulating films 506 and 507 function as first gate insulating films, and the insulating film 508 functions as a second gate insulating film. The insulating film 514 and the insulating film 516 are connected to each other through an opening formed therein, and the insulating film 516 is also connected to the insulating film 516 through an opening formed therein. The insulating films 506 and 507 function as the first gate insulating film and the insulating film 5 14 and surrounds the oxide semiconductor film 508 with the insulating film 516 interposed therebetween.

[0336] With such a structure, the oxide semiconductor film 508 included in the transistor 270 A conductive film 504 functions as a first gate electrode and an oxide film 505 functions as a second gate electrode. The transistor 270 can be electrically surrounded by the electric field of the nitride conductive film 511b. As shown in FIG. 1, a channel region is formed by the electric field of the first gate electrode and the second gate electrode. The device structure of the transistor is electrically surrounded by an oxide semiconductor film. This can be called a channel (s-channel) structure.

[0337] Since the transistor 270 has an s-channel structure, The functioning conductive film 504 effectively applies an electric field to induce a channel in the oxide semiconductor. Since the voltage can be applied to the film 508, the current driving capability of the transistor 270 is improved, and It is possible to obtain a high on-current characteristic. Therefore, it is possible to miniaturize the transistor 270. A conductive film 504 serving as a first gate electrode and an oxide film 505 serving as a second gate electrode are Since the transistor 270 has a structure surrounded by the conductive film 511b, the mechanical strength of the transistor 270 is can be increased.

[0338] <Transistor configuration example 2> 23(A) and (B) are cross-sectional views of a modification of the transistor 270 shown in FIGS. 22(B) and (C). 23(C) and (D) are side views of the transistors shown in FIGS. 22(B) and (C). FIG. 270 is a cross-sectional view of a modified example of the embodiment shown in FIG.

[0339] The transistor 270A shown in FIGS. 23A and 23B is the same as the transistor 270 shown in FIGS. The oxide semiconductor film 508 included in the transistor 270 has a three-layer structure. The oxide semiconductor film 508 included in the transistor 270A is an oxide semiconductor film 508a , an oxide semiconductor film 508b, and an oxide semiconductor film 508c.

[0340] The transistor 270B shown in FIGS. 23C and 23D is a transistor having a capacitance similar to that shown in FIGS. The oxide semiconductor film 508 included in the transistor 270 has a two-layer structure. In the transistor 270B, the oxide semiconductor film 508 is an oxide semiconductor film 508b. and an oxide semiconductor film 508c.

[0341] Here, the band structure of the oxide semiconductor film 508 and the insulating film in contact with the oxide semiconductor film 508 is This will be explained with reference to FIG.

[0342] FIG. 24A illustrates an insulating film 507, oxide semiconductor films 508a, 508b, and 508c, and an insulating FIG. 24(B) is an example of a band structure in the thickness direction of a laminated structure having an insulating film 514. 5A is a stack including an insulating film 507, oxide semiconductor films 508b and 508c, and an insulating film 514. 1 is an example of a band structure in the film thickness direction of the structure. Note that the band structure is shown in Fig. 1 for ease of understanding. Conductivity of the insulating film 507, the oxide semiconductor films 508a, 508b, and 508c, and the insulating film 514 The energy level (Ec) at the lower band edge is shown.

[0343] FIG. 24(A) shows a case where a silicon oxide film is used as the insulating films 507 and 514, and an oxide semiconductor The metal oxide film 508a has an atomic ratio of In:Ga:Zn=1:1:1.2. The oxide semiconductor film 508b was formed using an oxide semiconductor film formed using a metal target. A metal oxide target with an atomic ratio of metal elements of In:Ga:Zn=4:2:4.1 was used. The oxide semiconductor film 508c is formed by using an oxide semiconductor film having an atomic ratio of metal elements The oxide formed using a metal oxide target of In:Ga:Zn=1:1:1.2 FIG. 1 is a band diagram of a configuration using a semiconductor film.

[0344] FIG. 24B shows that silicon oxide films are used as the insulating films 507 and 514, and that the oxide semiconductor The metal oxide film 508b has an atomic ratio of In:Ga:Zn=4:2:4.1. The oxide semiconductor film 508c was formed using an oxide semiconductor film formed using a metal target. A metal oxide target with an atomic ratio of metal elements of In:Ga:Zn=1:1:1.2 was used. FIG. 1 is a band diagram of a structure using an oxide semiconductor film formed by

[0345] As shown in FIGS. 24A and 24B, in the oxide semiconductor films 508a, 508b, and 508c, In other words, the energy level at the bottom of the conduction band changes smoothly. In order to have such a band structure, the oxide At the interface between the semiconductor film 508a and the oxide semiconductor film 508b or at the interface between the oxide semiconductor film 508b and the oxide semiconductor film 508a At the interface with the oxide semiconductor film 508c, defect levels such as trap centers and recombination centers are generated. Assume that there are no impurities that would cause the formation of

[0346] In order to form a continuous junction in the oxide semiconductor films 508a, 508b, and 508c, Each film is deposited using a multi-chamber deposition system (sputtering system) equipped with a It is necessary to laminate continuously without exposing the layers to the air.

[0347] With the structure shown in FIGS. 24A and 24B, the oxide semiconductor film 508b serves as a well. In the transistor using the above stacked structure, the channel region is formed of the oxide semiconductor film 5 It can be seen that it is formed in 08b.

[0348] Note that by providing the oxide semiconductor films 508a and 508c, the oxide semiconductor film 508b This can make trap states that can be formed in the oxide semiconductor film 508b farther away from the oxide semiconductor film 508b.

[0349] In addition, the trap state is the minimum of the conduction band of the oxide semiconductor film 508b functioning as a channel region. The energy level (Ec) is farther from the vacuum level, and electrons tend to accumulate in the trap level. When electrons accumulate in the trap level, the negative fixed charge This causes a load and the threshold voltage of the transistor to shift in the positive direction. The trap level is lower than the energy level (Ec) of the conduction band minimum of the oxide semiconductor film 508b. It is preferable to configure the trap level so that the potential is close to the trap level. This makes it difficult for atoms to accumulate, which makes it possible to increase the on-state current of the transistor. The field effect mobility can be increased.

[0350] The oxide semiconductor films 508a and 508c have a lower conduction band minimum than the oxide semiconductor film 508b. The energy level of the oxide semiconductor film 508b is close to a vacuum level. and the energy levels of the conduction band minimums of the oxide semiconductor films 508a and 508c. The difference between the That is, the electron affinity of the oxide semiconductor films 508a and 508c and the The difference in electron affinity from 08b is 0.15 eV or more, or 0.5 eV or more and 2 eV or less , or 1 eV or less.

[0351] With such a structure, the oxide semiconductor film 508b serves as a main current path. The oxide semiconductor film 508b functions as a channel region. The oxide semiconductor film 508a and the oxide semiconductor film 508c function as oxide insulating films. 508c is a metal element constituting the oxide semiconductor film 508b in which a channel region is formed. Since the oxide semiconductor film is formed of one or more kinds of oxide semiconductors, the oxide semiconductor film 508a and the oxide semiconductor At the interface with the conductive film 508b or at the interface between the oxide semiconductor film 508b and the oxide semiconductor film 508c At the interface, interfacial scattering is unlikely to occur. Therefore, the movement of carriers is not hindered at the interface. This increases the field effect mobility of the transistor.

[0352] In addition, the oxide semiconductor films 508a and 508c function as part of a channel region. In order to prevent this, a material having a sufficiently low electrical conductivity is used. The layers 508a and 508c are also called oxide insulating films based on their physical properties and / or functions. In addition, the oxide semiconductor films 508a and 508c have a high electron affinity (vacuum level and conduction the energy level difference between the conduction band minimum and the conduction band minimum of the oxide semiconductor film 508b is smaller than that of the oxide semiconductor film 508b. The energy level of the oxide semiconductor film 508b is different from the energy level of the conduction band minimum of the oxide semiconductor film 508b (Band In addition, the material that has a drain offset is used. In order to suppress the difference in threshold voltage, the oxide semiconductor films 508a and 508 The energy level of the conduction band minimum of the oxide semiconductor film 508c is equal to the energy level of the conduction band minimum of the oxide semiconductor film 508b. For example, the lower conduction band of the oxide semiconductor film 508b is preferably closer to a vacuum level than the lower conduction band of the oxide semiconductor film 508b. and the energy levels of the conduction band minimums of the oxide semiconductor films 508a and 508c. The difference between the potentials is preferably 0.2 eV or more, more preferably 0.5 eV or more.

[0353] In addition, the oxide semiconductor films 508a and 508c do not include a spinel crystal structure. It is preferable that the oxide semiconductor films 508a and 508c each contain a spinel crystal structure. In this case, the conductive films 512a and 512b are formed at the interface between the spinel type crystal structure and other regions. In some cases, the constituent elements of b may diffuse into the oxide semiconductor film 508b. When the conductive films 508a and 508c are made of CAAC-OS, the conductive films 512a and 512b are made of An element such as copper is preferred because it has high blocking properties.

[0354] The thicknesses of the oxide semiconductor films 508a and 508c are determined by determining whether the constituent elements of the conductive films 512a and 512b are oxides or not. The thickness of the insulating film is greater than or equal to the thickness at which diffusion of the insulating film into the oxide semiconductor film 508b can be suppressed. The thickness of the oxide semiconductor film 508b is set to be less than the thickness at which supply of oxygen from the oxide semiconductor film 514 to the oxide semiconductor film 508b is suppressed. For example, When the oxide semiconductor films 508a and 508c have a thickness of 10 nm or more, the conductive films 512a and 512b are Diffusion of the constituent elements of the oxide semiconductor film 12b into the oxide semiconductor film 508b can be suppressed. When the thickness of the oxide semiconductor films 508a and 508c is 100 nm or less, Therefore, oxygen can be effectively supplied to the oxide semiconductor film 508b.

[0355] In this embodiment, the oxide semiconductor films 508a and 508c are formed using a metal The metal oxide target with the atomic ratio of In:Ga:Zn=1:1:1.2 was used. However, the present invention is not limited to this structure. The compound semiconductor films 508a and 508c are made of In:Ga:Zn=1:1:1 [atomic ratio], I n:Ga:Zn=1:3:2[atomic ratio], In:Ga:Zn=1:3:4[atomic ratio] or formed using a metal oxide target with In:Ga:Zn=1:3:6 [atomic ratio] Alternatively, an oxide semiconductor film having a low resistance may be used.

[0356] The oxide semiconductor films 508a and 508c are made of In:Ga:Zn=1:1:1 [atomic When a metal oxide target having a ratio of 1:1 to 1:1 is used, the oxide semiconductor films 508a and 508c are There are cases where n:Ga:Zn=1:β1(0<β1≦2):β2(0<β2≦3). The oxide semiconductor films 508a and 508c are made of In:Ga:Zn=1:3:4 [atomic When a metal oxide target having a ratio of 1:1 to 1:1 is used, the oxide semiconductor films 508a and 508c are There are cases where n:Ga:Zn=1:β3(1≦β3≦5):β4(2≦β4≦6). The oxide semiconductor films 508a and 508c are made of In:Ga:Zn=1:3:6 [atomic When a metal oxide target having a ratio of 1:1 to 1:1 is used, the oxide semiconductor films 508a and 508c are In some cases, n:Ga:Zn=1:β5(1≦β5≦5):β6(4≦β6≦8).

[0357] In addition, the oxide semiconductor film 508 included in the transistor 270 and the transistors 270A and 2 The oxide semiconductor film 508c in 70B is the conductive film 512a and the conductive film 512b in the drawing. In other words, a part of the oxide semiconductor film becomes a recess. However, one embodiment of the present invention is not limited to this. The oxide semiconductor film in the region not overlapping with the films 512a and 512b does not necessarily have to have a recess. An example of this case is shown in Figures 25(A) and 25(B). 25A and 25B are cross-sectional views showing an example of the transistor 270 shown above. The oxide semiconductor film 508 in B has a structure that does not have a recess.

[0358] As shown in FIGS. 25C and 25D, the thickness of the oxide semiconductor film 508c is set to 100 nm by pre-oxidizing. The oxide semiconductor film 508c and the insulating film 507 are formed thinner than the oxide semiconductor film 508b. In this case, the insulating film 519 may be formed over the oxide semiconductor film 508. The insulating film 519 is formed with openings so that the insulating film 519 c is in contact with the conductive film 512 a and the conductive film 512 b. can be formed by the same material and method as the insulating film 514.

[0359] In addition, the transistor according to the present embodiment can be freely combined with each of the above structures. It is possible.

[0360] This embodiment mode can be combined with other embodiment modes as appropriate.

[0361] (Embodiment 4) In this embodiment, an oxide semiconductor will be described with reference to FIGS.

[0362] <Structure of oxide semiconductor> The structure of an oxide semiconductor will be described below.

[0363] Oxide semiconductors are classified into single-crystal oxide semiconductors and other non-single-crystal oxide semiconductors. As a non-single-crystal oxide semiconductor, c-axis-aligned (CAAC-OS) crystalline oxide semiconductor, polycrystalline oxide Semiconductor, nc-OS (nanocrystalline oxide semiconducting uctor), pseudo-amorphous oxide semiconductor (a-like OS: amorphous-l ike oxide semiconductor and amorphous oxide semiconductor. .

[0364] From another point of view, the oxide semiconductor is classified into an amorphous oxide semiconductor and a crystalline oxide semiconductor other than the amorphous oxide semiconductor. Crystalline oxide semiconductors are classified into single crystal oxide semiconductors, CAAC- Examples of such materials include OS, polycrystalline oxide semiconductors, and nc-OS.

[0365] Amorphous structures are generally isotropic, have no inhomogeneous structure, and are metastable arrangements of atoms. The bond angles are flexible, and the short-range order is not fixed. It is said that...

[0366] That is, the stable oxide semiconductor is transformed into a completely amorphous In addition, it is not isotropic (for example, it does not have a periodic structure in a small region). On the other hand, an oxide semiconductor having an a-li structure cannot be called a completely amorphous oxide semiconductor. The ke OS is not isotropic, but has an unstable structure with voids. In terms of instability, a-like OS is similar in physical properties to amorphous oxide semiconductors. .

[0367] <caac-os> First, let me explain about CAAC-OS.

[0368] CAAC-OS is an oxide semiconductor that has multiple crystal parts (also called pellets) aligned along the c-axis. It is a type of conductor.

[0369] CAAC-OS was analyzed by X-ray diffraction (XRD). For example, the InGaZnO4, which is classified into the space group R-3m, The structure of CAAC-OS with crystals is analyzed by the out-of-plane method. As shown in FIG. 26(A), a peak appears at a diffraction angle (2θ) of about 31°. The peak is attributed to the (009) plane of the InGaZnO4 crystal, so The crystal has a c-axis orientation, and the c-axis is the surface on which the CAAC-OS film is to be formed (also called the surface on which the film is to be formed). It can be confirmed that the crystal is oriented in a direction perpendicular to the upper surface. In addition to the peaks near the 2θ of 36°, a peak may also appear near the 2θ of 36°. The peak is due to the crystal structure classified into the space group Fd-3m. It is preferred that the OS does not exhibit such a peak.

[0370] On the other hand, in-pla, X-rays are incident on the CAAC-OS in a direction parallel to the surface on which the film is to be formed. When the structure is analyzed by the NE method, a peak appears at 2θ of about 56°. This peak is I The lattice constant is assigned to the (110) plane of the nGaZnO4 crystal. The 2θ is fixed at around 56°. The analysis (φ scan) is performed while rotating the sample around the axis (φ axis) of the normal vector of the sample surface. Even if the annealing is performed, no clear peak appears as shown in FIG. When φ was scanned with 2θ fixed at around 56° for nO4, the results were as shown in Figure 26(C). As shown in Fig. 1, six peaks are observed that are attributable to crystal planes equivalent to the (110) plane. From the structural analysis using RD, it was found that the orientation of the a-axis and b-axis of CAAC-OS is irregular. can be confirmed.

[0371] Next, we will explain the CAAC-OS analyzed by electron diffraction. For CAAC-OS with nO4 crystals, a probe was applied parallel to the CAAC-OS surface. When an electron beam with a diameter of 300 nm is incident, a diffraction pattern (control pattern) as shown in FIG. This is also called the limited-area electron diffraction pattern.) may appear. This diffraction pattern includes In The spots are due to the (009) plane of the GaZnO4 crystal. In some cases, the pellets contained in the CAAC-OS have a c-axis orientation, and the c-axis is aligned with the surface on which the material is formed. On the other hand, for the same sample, the direction perpendicular to the sample surface was The diffraction pattern when an electron beam with a probe diameter of 300 nm was directly incident is shown in Figure 26(E). A ring-shaped diffraction pattern is confirmed in FIG. 26(E). Electron diffraction using an electron beam with a diameter of 300 nm also revealed that the pellets contained in CAAC-OS It can be seen that the a-axis and b-axis of the crystal have no orientation. The gluing is thought to be due to the (010) and (100) planes of the InGaZnO4 crystal. The second ring in FIG. 26(E) is thought to be due to the (110) plane, etc. can be.

[0372] In addition, a transmission electron microscope (TEM) A combined analysis image of the bright-field image and the diffraction pattern of CAAC-OS was obtained using a microscope. (also called high-resolution TEM image), multiple pellets can be confirmed. On the other hand, even in high-resolution TEM images, the boundaries between pellets, i.e., grain boundaries (grain bows), are not clearly visible. In some cases, it may not be possible to clearly identify the CAAC It can be said that the -OS is less susceptible to the decrease in electron mobility caused by grain boundaries.

[0373] Figure 27(A) shows a high-resolution T The TEM image is shown. For high-resolution TEM imaging, spherical aberration correction is used. The spherical aberration correction function was used. A high-resolution TEM image is specifically called a Cs-corrected high-resolution TEM image. For example, the atomic resolution analytical electron microscope JEM-ARM200F manufactured by JEOL Ltd. It can be observed that.

[0374] From FIG. 27(A), a pellet, which is an area where metal atoms are arranged in layers, can be confirmed. It has been found that the size of a single pellet can be 1 nm or more, or 3 nm or more. Therefore, the pellets are called nanocrystals (nc). CAAC-OS can also be used with CANC (C-Axis Aligned nan The pellets can also be called oxide semiconductors with CAAC The surface on which the CAAC-OS is formed or the top surface of the CAAC-OS are formed. It becomes parallel.

[0375] In addition, Fig. 27(B) and Fig. 27(C) show the CAAC- Cs-corrected high-resolution TEM images of the OS plane are shown in Fig. 27(D) and Fig. 27(E). These are images obtained by processing the images shown in Fig. 27(B) and Fig. 27(C). First, let us consider the case where FIG. 27B is subjected to a fast Fourier transform (FFT). Then, the FFT image is obtained by performing FFT (Frequency Transform) processing. 2.8 nm based on the origin in the FT image -1 From 5.0 nm -1 The area between the squares is left Next, the masked FFT image is subjected to inverse fast Fourier transform (IFFT). The image is processed by using the Fast Fourier Transform (FFT) The image obtained in this way is called an FFT filtered image. The ring image is an image in which the periodic components are extracted from a Cs-corrected high-resolution TEM image, and the lattice arrangement is It shows.

[0376] In FIG. 27(D), the area where the lattice arrangement is disturbed is indicated by a dashed line. The area surrounded by the dashed line is The area indicated by the dashed line is the connection between the pellets. The broken line indicates a hexagonal shape, so it can be seen that the pellets are hexagonal. The shape of the dot is not limited to a regular hexagon, and is often a non-regular hexagon.

[0377] In FIG. 27(E), a dotted line separates an area with a uniform lattice arrangement from an area with a different uniform lattice arrangement. Even in the vicinity of the dotted line, no clear grain boundaries can be confirmed. When you connect the neighboring lattice points, you can get a distorted hexagon, pentagon, or heptagon. In other words, the formation of grain boundaries is suppressed by distorting the lattice arrangement. This is because the atomic arrangement of CAAC-OS is not dense in the ab-plane direction. The metal elements are replaced by other elements, which changes the bond distance between atoms, resulting in distortion. This is thought to be because it is possible to tolerate

[0378] As described above, the CAAC-OS has a c-axis orientation and multiple crystals in the ab-plane direction. A number of pellets (nanocrystals) are connected to form a distorted crystal structure. AC-OS, CAA crystal(c-axis-aligned ab-pl It can also be called an oxide semiconductor having an ane-anchored crystal. do.

[0379] CAAC-OS is a highly crystalline oxide semiconductor. The crystallinity of oxide semiconductors is improved by the incorporation of impurities. CAAC-OS is a material that can be degraded by impurities and defects ( It can also be said that the oxide semiconductor has few oxygen vacancies.

[0380] The impurities are elements other than the main components of the oxide semiconductor, such as hydrogen, carbon, silicon, and transition metals. For example, oxygen is more abundant than metal elements such as silicon that constitute oxide semiconductors. Elements with strong bonding strength with the oxide semiconductor remove oxygen from the oxide semiconductor, thereby changing the atomic arrangement of the oxide semiconductor. In addition, heavy metals such as iron and nickel, argon, and nitrogen Carbon oxide and other substances have a large atomic radius (or molecular radius), and therefore they disrupt the atomic arrangement of oxide semiconductors. This leads to a decrease in crystallinity.

[0381] When an oxide semiconductor has impurities or defects, its characteristics may change due to light, heat, etc. For example, impurities contained in an oxide semiconductor can become carrier traps or can displace carriers. For example, oxygen vacancies in oxide semiconductors can act as carrier traps. In some cases, the SiO 2 can become a carrier generation source by capturing hydrogen.

[0382] CAAC-OS, which has few impurities and oxygen vacancies, is an oxide semiconductor with low carrier density. Specifically, 8×10 11 pieces / cm 3 Less than 1 x 10 11 pieces / cm 3 less than, More preferably, 1×10 10 pieces / cm 3 Less than 1 x 10 -9 pieces / cm 3 The above Such an oxide semiconductor can be a high-purity intrinsic oxide semiconductor. The CAAC-OS has a low impurity concentration and is a substantially high-purity intrinsic oxide semiconductor. The density of defect states is low, that is, the oxide semiconductor has stable characteristics.

[0383] <nc-os> Next, we will explain nc-OS.

[0384] The following describes the case where nc-OS is analyzed by XRD. For example, When structural analysis is performed using the out-of-plane method, no peaks indicating orientation appear. That is, the crystals of the nc-OS do not have any orientation.

[0385] For example, an nc-OS having InGaZnO4 crystals was sliced ​​to a thickness of 34 nm. When an electron beam with a probe diameter of 50 nm is incident parallel to the surface to be formed on the region shown in FIG. A ring-shaped diffraction pattern (nanobeam electron diffraction pattern) as shown in (A) was observed. In addition, the diffraction pattern (nm) when an electron beam with a probe diameter of 1 nm was incident on the same sample was The electron diffraction pattern (B) is shown in FIG. 28(B). From FIG. 28(B), a ring-shaped region Therefore, nc-OS has a probe diameter of 50 nm. Although no order was observed by irradiating the electron beam, the order was observed by irradiating the electron beam with a probe diameter of 1 nm. By projecting the images, order is confirmed.

[0386] In addition, when an electron beam with a probe diameter of 1 nm is incident on an area with a thickness of less than 10 nm, As shown in FIG. 28(C), an electron diffraction pattern was observed in which the spots were arranged in a roughly regular hexagonal shape. Therefore, in the range of thickness less than 10 nm, the nc-OS is ordered. It can be seen that the crystals have highly crystalline regions. Therefore, there are some areas where no regular electron diffraction pattern is observed.

[0387] FIG. 28(D) shows the Cs-corrected high resolution image of the cross section of nc-OS observed from a direction approximately parallel to the surface on which the film was formed. The nc-OS is shown in the high-resolution TEM image, with the areas indicated by the auxiliary lines. As shown in Fig. 1, there are areas where crystals can be confirmed, and areas where no clear crystals can be confirmed. The crystal part in the nc-OS has a size of 1 nm to 10 nm. In particular, the size of the crystal part is often between 1 nm and 3 nm. An oxide semiconductor having a diameter of more than 0 nm and less than 100 nm is called a microcrystalline oxide semiconductor. It is sometimes called a crystalline oxide semiconductor. For example, in the case of nc-OS, the grain boundaries may not be clearly visible in high-resolution TEM images. It is possible that the nanocrystals originate from the same source as the pellets in CAAC-OS. Therefore, hereinafter, the crystalline parts of the nc-OS may be referred to as pellets.

[0388] In this way, the nc-OS can be used in microscopic regions (e.g., regions of 1 nm to 10 nm, especially The atomic arrangement has periodicity in the region of 1 nm to 3 nm. There is no regularity in the crystal orientation between different pellets. Therefore, no orientation is observed throughout the film. Therefore, depending on the analytical method, nc-OS may be classified as a-like OS or amorphous OS. It may be difficult to distinguish it from an oxide semiconductor.

[0389] In addition, since the crystal orientation between pellets (nanocrystals) is not regular, nc-OS is Oxide with RANC (Random Aligned nanocrystals) Semiconductor or NANC (Non-Aligned nanocrystals) It can also be called an oxide semiconductor.

[0390] The nc-OS is an oxide semiconductor with higher order than an amorphous oxide semiconductor. The nc-OS has a lower density of defect states than the a-like OS and amorphous oxide semiconductors. However, the crystal orientation of nc-OS is not regular among different pellets. , the nc-OS has a higher density of defect states than the CAAC-OS.

[0391] <a-like OS> The a-like OS is an oxide semiconductor that has a structure between the nc-OS and the amorphous oxide semiconductor. It is a conductor.

[0392] Figure 29 shows a high-resolution cross-sectional TEM image of the a-like OS. This is a high-resolution cross-sectional TEM image of the a-like OS at the start of electron irradiation. ) is 4.3 × 10 8 e - / nm 2 Electrons (e - ) High a-like OS after irradiation 29(A) and 29(B) show that the a-like OS is It can be seen that striped bright regions extending in the vertical direction are observed from the start of electron irradiation. It can be seen that the shape of the bright regions changes after electron irradiation. The bright regions are voids or low-density regions. It is speculated to be the area.

[0393] Because of the porosity, the a-like OS is an unstable structure. To demonstrate that the OS has a less stable structure than the CAAC-OS and nc-OS, This shows the change in structure due to electron irradiation.

[0394] As samples, a-like OS, nc-OS and CAAC-OS were prepared. The sample is also an In-Ga-Zn oxide.

[0395] First, high-resolution cross-sectional TEM images of each sample are obtained. Each of the above has a crystalline portion.

[0396] The unit cell of the InGaZnO4 crystal has three In-O layers and a Ga-Zn- It is known that the structure has a total of nine layers, including six O layers, stacked in layers in the c-axis direction. The spacing between these adjacent layers is the same as the lattice spacing (also called the d value) of the (009) plane. The value is about 0.29 nm, which is determined by crystal structure analysis. In the figure below, the areas where the lattice spacing is between 0.28 nm and 0.30 nm are InGaZn The lattice fringes correspond to the ab plane of the InGaZnO4 crystal. do.

[0397] Figure 30 shows an example of the average size of the crystal parts (22 to 30 places) of each sample. The length of the lattice fringes mentioned above is the size of the crystal part. The crystal part of the OS grows larger according to the cumulative dose of electrons used in obtaining the TEM image. As can be seen from Fig. 30, in the early stages of TEM observation, the size of the particles was about 1.2 nm. The part of the crystal that was a nucleus (also called the initial nucleus) is filled with electrons (e - ) cumulative exposure of 4.2 × 10 8 e - / nm 2 It can be seen that the size of the crystals grows to about 1.9 nm in the nc The cumulative electron dose from the start of electron irradiation was 4.2 × 10 8 e - / nm 2 From Figure 30, it can be seen that there is no change in the size of the crystals within the range. Regardless of the cumulative dose of electron irradiation, the size of the crystalline parts of the nc-OS and CAAC-OS was The results show that the average particle size distribution is about 1.3 nm and 1.8 nm, respectively. The observation of M was performed using a Hitachi transmission electron microscope H-9000NAR. The electron beam irradiation conditions were: Voltage: 300 kV, current density: 6.7 × 10 5 e - / (nm 2 s), the diameter of the irradiated area The wavelength was set to 230 nm.

[0398] Thus, in a-like OS, the growth of crystals can be observed by electron irradiation. On the other hand, the nc-OS and CAAC-OS hardly show any growth of crystals due to electron irradiation. That is, a-like OS is less likely to cause anxiety than nc-OS and CAAC-OS. It can be seen that it has a stable structure.

[0399] In addition, because of the porosity, a-like OS is more difficult to treat than nc-OS and CAAC-OS. It is a low-density structure. Specifically, the density of the a-like OS is 100 times lower than that of a single crystal of the same composition. The density of nc-OS is 78.6% or more and less than 92.3% of the density of CAAC-O. The density of S is 92.3% or more but less than 100% of the density of a single crystal of the same composition. It is difficult to form a film of an oxide semiconductor having a conductivity of less than 78%.

[0400] For example, in an oxide semiconductor with an atomic ratio of In:Ga:Zn=1:1:1, The density of single crystal InGaZnO4 with a hexagonal crystal structure is 6.357 g / cm 3 That is it. For example, in an oxide semiconductor having an atomic ratio of In:Ga:Zn=1:1:1, , the density of a-like OS is 5.0g / cm 3 Less than 5.9 g / cm 3 Furthermore in, for example, an oxide semiconductor satisfying In:Ga:Zn = 1:1:1 [atomic ratio], the density of nc-OS and the density of CAAC-OS are 5.9 g / cm 3 or more and 6.3 g / cm 3 not satisfied.

[0401] In addition, when there is no single crystal of the same composition, the density corresponding to the single crystal in the desired composition can be estimated by combining single crystals with different compositions at an arbitrary ratio. The density corresponding to the single crystal of the desired composition may be estimated using the weighted average with respect to the ratio of combining single crystals with different compositions. However, it is preferable to estimate the density by combining as few types of single crystals as possible. As described above, the oxide semiconductor has various structures, each having various characteristics. Also, the oxide semiconductor may be, for example, a laminated film having two or more of amorphous oxide semiconductor, a-like OS, nc-OS, CAAC-OS. This embodiment can be appropriately combined with other embodiments.

[0402] As described above, the oxide semiconductor has various structures, each having various characteristics. Also, the oxide semiconductor may be, for example, a laminated film having two or more of amorphous oxide semiconductor, a-like OS, nc-OS, CAAC-OS. This embodiment can be appropriately combined with other embodiments.

[0403] This embodiment can be appropriately combined with other embodiments.

[0404] (Embodiment 5) (Configuration of CAC) Hereinafter, the configuration of CAC (Cloud Aligned Complementary)-OS that can be used in one aspect of the present invention will be described.

[0405] CAC is, for example, a configuration of a material in which the elements constituting the oxide semiconductor are unevenly distributed in a size of 0.5 nm or more and 10 nm or less, preferably 1 nm or more and 2 nm or less, or in the vicinity thereof. In the following, it is assumed that one or more metal elements are unevenly distributed in an oxide semiconductor. The region having the metal element is 0.5 nm or more and 10 nm or less, preferably 1 nm or more and 2 nm or less. A state in which the pixels are mixed in a size similar to or close to this size is also called a mosaic or patch pattern.

[0406] For example, CAC-IGZ in In-Ga-Zn oxide (hereinafter also referred to as IGZO) O stands for indium oxide (InO X1 (X1 is a real number greater than 0.) or indium zinc oxide (hereinafter referred to as In X2 Zinc Y2 O Z2 (X2, Y2, and Z2 are 0) and gallium oxide (GaO X3 (X3 is from 0 ) or gallium zinc oxide (Ga X4 Zinc Y4 O Z4 ( X4, Y4, and Z4 are real numbers greater than 0.) The mosaic pattern is formed by InO X1 Or In X2 Zinc Y2 O Z2 But in the membrane It is a uniformly distributed configuration (hereinafter also referred to as a cloud-like configuration).

[0407] In other words, CAC-IGZO is GaO X3 The region where In is the main component and X2 Zinc Y2 O Z 2 or InO X1 A composite oxide semiconductor having a structure in which a region in which In this specification, for example, the number of In atoms relative to the element M in the first region is The first region has a ratio of In to the element M that is greater than the atomic ratio of In to the element M in the second region. It is assumed that the concentration of In is higher than that of the second region.

[0408] Note that IGZO is a common name and refers to a compound made of In, Ga, Zn, and O. A typical example is InGaO3(ZnO). m1 (m1 is a natural number) or In (1+ x0) Ga (1-x0) O3(ZnO) m0 (-1≦x0≦1, m0 is an arbitrary number) Examples of the crystalline compounds include

[0409] The crystalline compound has a single crystal structure, a polycrystalline structure, or a CAAC structure. The CAAC structure is a structure in which multiple IGZO nanocrystals have a c-axis orientation and It is a non-oriented, connected crystal structure.

[0410] On the other hand, CAC is related to the material composition. CAC is a material containing In, Ga, Zn, and O. In the structure, there are areas where Ga is the main component and areas where In is the main component. The main component, nanoparticle-like regions, are randomly distributed in a mosaic pattern. Therefore, the crystal structure is a secondary element in CAC.

[0411] Note that CAC does not include a laminated structure of two or more films with different compositions. For example, However, this does not include a two-layer structure consisting of a film containing In as a main component and a film containing Ga as a main component.

[0412] In addition, GaO X3 The region where In is the main component and X2 Zinc Y2 O Z2 or InO X1 Mainly The region that is a component may not have a clearly observable boundary.

[0413] <Analysis of CAC-IGZO> Subsequently, using various measurement methods, the results of measuring the oxide semiconductor formed on the substrate will be described.

[0414] ≪Sample composition and fabrication method≫ Hereinafter, nine samples according to one aspect of the present invention will be described. Each sample is an oxide semiconductor fabricated under conditions where the substrate temperature and the oxygen gas flow rate ratio during film formation are different. Note that the samples each have a structure having a substrate and an oxide semiconductor on the substrate.

[0415] The fabrication method of each sample will be described.

[0416] First, a glass substrate is used as the substrate. Subsequently, using a sputtering apparatus, In-Ga-Zn oxide with a thickness of 100 nm is formed as an oxide semiconductor on the glass substrate. The film formation conditions are such that the pressure in the chamber is 0.6 Pa, and an oxide target ( In:Ga:Zn = 4:2:4.1 [atomic ratio]) is used for the target. Also, 2500 W of AC power is supplied to the oxide target installed in the sputtering apparatus . In addition, as the conditions for forming the oxide film, the substrate temperature is set to a temperature that is not intentionally heated (hereinafter,

[0417] also referred to as R.T.), 130 °C, or 170 °C. Also, the flow rate ratio of oxygen gas to the mixed gas of Ar and oxygen (hereinafter, also referred to as the oxygen gas flow rate ratio) is set to 10%, 30%, or 100% to fabricate nine samples.

[0418] ≪Analysis by X-ray diffraction≫ ​​In this section, we will explain the results of XRD measurements on nine samples. The D device used was the Bruker D8 ADVANCE. The scanning range is 15deg. to 50deg. using the -of-plane method for θ / 2θ scanning. For example, the step width was 0.02 deg. and the scanning speed was 3.0 deg. / min.

[0419] FIG. 36 shows the results of measuring the XRD spectrum using the out-of-plane method. In addition, in FIG. 36, the upper part shows the measurement results for a sample where the substrate temperature during film formation was 170° C. As a result, the middle row shows the measurement results for a sample with a substrate temperature of 130°C during film formation, and the bottom row shows the measurement results for a sample with a substrate temperature of 130°C during film formation. The left column shows the results of measurements taken with the substrate temperature at room temperature. The center column shows the measurement results for the sample with a flow rate ratio of 10%. The center column shows the measurement results for the sample with a flow rate ratio of 3%. The right column shows the measurement results for the sample with an oxygen gas flow rate of 100%. The measurement results are shown below.

[0420] The XRD spectrum shown in FIG. 36 shows that the increase in the substrate temperature during film formation or the increase in the amount of oxygen during film formation By increasing the gas flow rate ratio, the peak intensity around 2θ=31° increases. The peak at 2θ=31° is aligned along the c-axis in a direction substantially perpendicular to the surface on which the film is formed or the upper surface. crystalline IGZO compound (CAAC(c-axis aligned crystall It is also called ine)-IGZO.

[0421] In addition, the XRD spectrum shown in FIG. 36 shows that the substrate temperature during film formation was low or the oxygen gas flow was low. The smaller the ratio, the less clear the peak. In the case of samples with a small oxygen gas flow rate, the orientation of the ab plane direction and the c axis direction of the measurement area is I know I can’t see it.

[0422] Analysis by electron microscope In this section, the samples were prepared at a substrate temperature of RT and an oxygen gas flow rate of 10% during film formation. HAADF(High-Angle Annular Dark Field)-STE M(Scanning Transmission Electron Microsc The results of the observation and analysis using HAADF-STE (hereinafter referred to as HAADF-STE) are described below. Images obtained by M are also called TEM images.

[0423] Planar images obtained by HAADF-STEM (hereinafter also referred to as planar TEM images), and The results of image analysis of the cross-sectional image (hereinafter also referred to as the cross-sectional TEM image) will be explained. The TEM images were observed using a spherical aberration correction function. The images were taken using an atomic resolution analytical electron microscope, JEM-ARM200F, manufactured by JEOL Ltd. The specimen was irradiated with an electron beam having an accelerating voltage of 200 kV and a beam diameter of approximately 0.1 nmφ.

[0424] FIG. 37(A) shows a sample prepared at a substrate temperature of RT during film formation and an oxygen gas flow rate of 10%. FIG. 37(B) shows the relationship between the substrate temperature RT and the oxygen gas flow rate during the film formation. This is a cross-sectional TEM image of a sample prepared at a ratio of 10%.

[0425] <Analysis of electron diffraction patterns> In this section, the samples were prepared at a substrate temperature of RT and an oxygen gas flow rate of 10% during film formation. By irradiating an electron beam with a probe diameter of 1 nm (also called a nano-beam electron beam), The results of obtaining the diffraction patterns will now be described.

[0426] As shown in FIG. 37(A), the film was formed at a substrate temperature of RT and an oxygen gas flow rate of 10%. In the planar TEM image of the sample, black spots a1, a2, a3, a4, and a5 The electron beam diffraction pattern shown in FIG. 1 is observed. The sunspot a1 is moved from the 0 second position to the 35 second position at a constant speed while shooting. The results of the black point a1 are shown in Figure 37(C), the results of the black point a2 are shown in Figure 37(D), and the results of the black point a3 are shown in Figure 37(E). The results for black point a4 are shown in FIG. 37(F), and the results for black point a5 are shown in FIG. 37(G).

[0427] From Figures 37(C), 37(D), 37(E), 37(F), and 37(G), A bright area that looks like a ring can be observed. Spots of the above can be observed.

[0428] In addition, as shown in FIG. 37(B), the substrate temperature during film formation was RT and the oxygen gas flow rate ratio was 10%. In the cross-sectional TEM image of the prepared sample, black spots b1, b2, b3, b4, and Observe the electron beam diffraction pattern shown by point b5. The results for black point b1 are shown in Figure 37(H), and the results for black point b2 are shown in Figure 37(H). The results of black point b1 are shown in Figure 37(I), the results of black point b3 are shown in Figure 37(J), and the results of black point b4 are shown in Figure 37(K). The results for black point b5 are shown in Figure 37(L).

[0429] From Figures 37(H), 37(I), 37(J), 37(K), and 37(L), A ring-shaped area of ​​high brightness can be observed. Also, multiple spots can be observed in the ring-shaped area. Cut.

[0430] Here, for example, for a CAAC-OS having InGaZnO4 crystals, When an electron beam with a probe diameter of 300 nm is incident on the InGaZnO4 crystal, ) planes. It is found that the film has a c-axis orientation, and the c-axis is oriented in a direction substantially perpendicular to the surface on which the film is formed or the upper surface. On the other hand, an electron beam with a probe diameter of 300 nm is incident perpendicularly to the surface of the same sample. In other words, CAAC-OS has a ring-shaped diffraction pattern along the a-axis and b-axis. It can be seen that the film has no orientation.

[0431] In addition, a nanocrystalline oxide semiconductor nc-OS) with a large probe diameter ( For example, when electron diffraction is performed using an electron beam of 50 nm or more, a halo pattern is observed. In addition, a small probe diameter electron beam (e.g. When nanobeam electron diffraction is performed using a material with a diameter of less than 50 nm, bright spots are observed. In addition, when nanobeam electron diffraction was performed on nc-OS, the ) A bright area may be observed. In addition, multiple bright spots may be observed in a ring-shaped area. This may be the case.

[0432] The electron diffraction pattern of the sample prepared at the substrate temperature RT and oxygen gas flow rate of 10% during film formation. The ring has a ring-shaped area of ​​high brightness and multiple bright points in the ring area. The electron diffraction pattern of the sample was obtained by fabricating the film at a substrate temperature of RT and an oxygen gas flow rate of 10%. The layer becomes an nc-OS and has no orientation in the planar and cross-sectional directions.

[0433] From the above, an oxide semiconductor having a low substrate temperature or a low oxygen gas flow rate during deposition has the following properties: It is clearly different from an oxide semiconductor film having an amorphous structure and an oxide semiconductor film having a single crystal structure. It can be presumed that the substance has the following properties:

[0434] ≪Elemental analysis≫ In this article, we will discuss energy dispersive X-ray spectroscopy (EDX). EDX mapping was obtained and evaluated using EDX (Electron Doppler X-ray spectroscopy). By this, the sample was fabricated at the substrate temperature RT and oxygen gas flow rate ratio of 10% during film formation. The results of elemental analysis of the material are described below. The energy dispersive X-ray analyzer JED-2300T manufactured by JEOL Ltd. is used. A Si drift detector is used to detect the X-rays emitted from the sample.

[0435] In EDX measurement, each point in the analysis area of ​​the sample is irradiated with an electron beam, and the resulting The energy and frequency of the characteristic X-rays of the material are measured, and the EDX spectrum corresponding to each point is obtained. In this embodiment, the peaks in the EDX spectrum at each point are determined as electron transitions to the L shell of the In atom. , electron transition to the K shell of Ga atom, electron transition to the K shell of Zn atom, and electron transition to the K shell of O atom The ratio of each atom at each point is calculated. By performing this on a region, it is possible to obtain EDX mapping that shows the distribution of the ratio of each atom. This can be done.

[0436] FIG. 38 shows a cross section of a sample fabricated at a substrate temperature of RT and an oxygen gas flow rate of 10% during film formation. FIG. 38(A) shows EDX mapping of Ga atoms (all The ratio of Ga atoms to Ga atoms is in the range of 1.18 to 18.64 [atomic%]. ). Figure 38(B) shows the EDX mapping of In atoms (the ratio of In atoms to the total atoms). The ratio is in the range of 9.28 to 33.74 [atomic%]. ) was EDX mapping of Zn atoms (ratio of Zn atoms to total atoms is 6.69 to 24 .99[atomic%] range.) Also, Fig. 38(A) and Fig. 38(B) 38(C) and 38(D) are fabricated at a substrate temperature of RT and an oxygen gas flow rate of 10%. The cross-section of the sample shows the same area. The more the measured element, the brighter the image becomes, and the less the measured element, the darker the image becomes. The EDX mapping shown in Figure 38 is at a magnification of 7.2 million times. do.

[0437] In the EDX mapping shown in FIG. 38(A), FIG. 38(B), and FIG. 38(C), The film was formed at a substrate temperature of RT and an oxygen gas flow rate of 10%. In the sample prepared, it can be seen that each atom exists with a certain distribution. The areas surrounded by solid lines and dashed lines in Figs. 38(A), 38(B), and 38(C) are Pay attention.

[0438] In FIG. 38(A), the area enclosed by the solid line contains many relatively dark areas, and the area enclosed by the dashed line contains many relatively dark areas. In FIG. 38(B), the area enclosed by the solid line is relatively bright. The area surrounded by the dashed line contains many bright areas, while the area surrounded by the dashed line contains many relatively dark areas.

[0439] In other words, the area surrounded by the solid line is the area where the In atoms are relatively abundant, and the area surrounded by the dashed line is the area where the In atoms are relatively abundant. In FIG. 38(C), the area surrounded by the solid line is The right side is a relatively bright area, and the left side is a relatively dark area. Therefore, The range is In X2 Zinc Y2 O Z2 , or InO X1 This is an area where the main components are:

[0440] The area surrounded by the solid line is the area with relatively few Ga atoms, and the area surrounded by the dashed line is the area with relatively few Ga atoms. In Figure 38(C), the upper left area in the area enclosed by the dashed line is The upper right area is a relatively bright area, and the lower right area is a relatively dark area. The area enclosed by the dashed line is GaO X3 , or Ga X4 Zinc Y4 O Z4 Areas where the main components are It is.

[0441] In addition, from FIG. 38(A), FIG. 38(B), and FIG. 38(C), the distribution of In atoms is The distribution is relatively uniform compared to InO X1 The region where is the main component is In X2 Z n Y2 O Z2 It appears to be connected to each other through the area where it is mainly composed. In this way, X2 Zinc Y2 O Z2 , or InO X1 The region where is the main component is the cloud. It is formed in a burdock-like shape.

[0442] In this way, GaO X3 The region where In is the main component and X2 Zinc Y2 O Z2 , or InO X1 In-Ga-Zn oxide with a structure in which the In-Ga-Zn oxide is unevenly distributed and mixed with the In-Ga-Zn oxide. The material can be referred to as CAC-IGZO.

[0443] The crystal structure of CAC is an nc structure. The nc structure of CAC is In the X-ray diffraction pattern, bright spots due to IGZO, including single crystal, polycrystalline, and CAAC structures, In addition to the spots, there are several bright spots. In addition to the bright spots, the crystal structure is defined as having ring-shaped areas of high brightness. do.

[0444] In addition, from Fig. 38(A), Fig. 38(B), and Fig. 38(C), GaO X3 is the main component Area, and In X2 Zinc Y2 O Z2 , or InO X1 The size of the region in which is the principal component is The observed size is 0.5 nm or more and 10 nm or less, or 1 nm or more and 3 nm or less. In EDX mapping, the diameter of the area where each metal element is the main component is 1 nm or more. nm or less.

[0445] From the above, it can be seen that CAC-IGZO has a structure different from that of IGZO compounds in which metal elements are uniformly distributed. CAC-IGZO has a different structure and properties from IGZO compounds. X3 The main components are In X2 Zinc Y2 O Z2 , or InO X1 The main component is The structure is such that the regions with one element as the main component are separated into a mosaic pattern. Therefore, when CAC-IGZO is used in semiconductor devices, GaO X3 Due to factors such as Properties and In X2 Zinc Y2 O Z2 , or InO X1 The properties resulting from this act in a complementary manner. This allows for a high on-state current (I on ) and high field-effect mobility (μ This can be done.

[0446] In addition, semiconductor elements using CAC-IGZO are highly reliable. O is ideal for a variety of semiconductor devices, including displays.

[0447] This embodiment mode can be combined with other embodiment modes as appropriate.

[0448] (Embodiment 6) In this embodiment, a touch panel module including an input / output device according to one embodiment of the present invention and a The child device will be described with reference to FIGS.

[0449] The touch panel module 8000 shown in FIG. 31 includes an upper cover 8001 and a lower cover 8002. Between the FPC8003 and the frame 8009, It includes a printed circuit board 8010 and a battery 8011 .

[0450] The input / output device of one embodiment of the present invention can be used for the touch panel 8004, for example.

[0451] The upper cover 8001 and the lower cover 8002 are designed to fit the size of the touch panel 8004. The shape and dimensions can be changed appropriately.

[0452] In addition, when a transmission type liquid crystal element is used, a backlight 8007 is provided as shown in FIG. The backlight 8007 has a light source 8008. Although the configuration in which the light source 8008 is disposed above the backlight 8007 has been illustrated, the present invention is not limited to this. For example, a light source 8008 is arranged at the end of the backlight 8007, and a light diffusion layer is also arranged. A diffuser plate may be used. When a self-luminous light-emitting element such as an organic EL element is used, In the case of a reflective panel, the backlight 8007 is not provided. Good too.

[0453] The frame 8009 protects the touch panel 8004 and also supports the movement of the printed circuit board 8010. It also functions as an electromagnetic shield to block electromagnetic waves generated by the operation of the frame. The frame 8009 may also function as a heat sink.

[0454] The printed circuit board 8010 includes a power supply circuit, a signal circuit for outputting a video signal, and a clock signal. The power supply circuit is supplied with power from an external commercial power source. Alternatively, the power source may be a battery 8011 provided separately. This can be omitted if a commercial power source is used.

[0455] In addition, the touch panel 8004 is equipped with additional components such as a polarizing plate, a retardation plate, and a prism sheet. It may also be provided.

[0456] 32(A) to (H) and FIG. 33 are diagrams showing electronic devices. These electronic devices are A body 5000, a display unit 5001, a speaker 5003, an LED lamp 5004, and an operation key 50 05 (including a power switch or an operation switch), a connection terminal 5006, a sensor 5007 ( Force, displacement, position, velocity, acceleration, angular velocity, rotation speed, distance, light, liquid, magnetism, temperature, chemical substances , sound, time, hardness, electric field, current, voltage, power, radiation, flow rate, humidity, gradient, vibration, 5008, etc.) can.

[0457] FIG. 32(A) shows a mobile computer, which includes, in addition to the above, a switch 5009, The portable terminal 5010 may have an infrared port 5010. FIG. A type of image reproducing device (for example, a DVD reproducing device) that, in addition to the above, also has a second display 32C shows a television. In addition to the above, the device may also include a stand 5012. The television device can be operated using an operation switch provided in the housing 5000 or a separate remote control. This can be done by operating the operation device 5013. The channel and volume can be controlled by using the In addition, the remote control device 5013 can receive the A display unit for displaying the output information may be provided. In addition to the above, the device may have a recording medium reading unit 5011, etc. 2(E) is a digital camera with a television receiving function, and in addition to the above, it also has an antenna 5 014, a shutter button 5015, an image receiving unit 5016, etc. (F) is a portable gaming machine, and in addition to the above, it has a second display unit 5002, a recording medium reader, FIG. 32(G) shows a portable television receiver. In addition to the above, it may have a charger 5017 capable of transmitting and receiving signals, etc. FIG. 32(H) shows a wristwatch-type information terminal, which, in addition to the above, includes a band 5018, a clasp, The display 5000 may have a gold plated 5019, etc. The display unit 5001 has a non-rectangular display area. 5020, other icons 5021, etc. can be displayed. Digital signage (digital signage). Figure 33(B) is a digital signage mounted on a cylindrical pillar.

[0458] The electronic devices shown in FIGS. 32(A) to (H) and 33 can have various functions. For example, the function to display various information (still images, videos, text images, etc.) on the display, Panel function, calendar, date or time display function, various software (platform A function to control processing by a program, a wireless communication function, and a function to control various Functions for connecting to computer networks, wireless communication functions for transmitting various data, The function of receiving, reading out the program or data recorded on the recording medium and displaying it on the display Furthermore, in an electronic device having multiple display units, In this case, one display section is used mainly to display image information, and the other display section is used mainly to display text information. A function to display a stereoscopic image by displaying images that take parallax into account on multiple displays. Furthermore, in electronic devices having an image receiving unit, The camera has the functions of taking still images, taking videos, and automatically or manually correcting the captured images. function to store the captured images on a recording medium (external or built-in to the camera); The image can be displayed on the display unit. The functions that the electronic device shown in FIG. 33 can have are not limited to those described above, and the electronic device may have various functions. It is possible.

[0459] The electronic device of the present embodiment is characterized by having a display unit for displaying some information. The input / output device of one embodiment of the present invention can be used in the display portion.

[0460] This embodiment mode can be combined with other embodiment modes as appropriate. EXAMPLES

[0461] In this embodiment, an input / output device according to one embodiment of the present invention will be described.

[0462] First, the specifications of the input / output device of this embodiment will be described. The size is 4.3 inches diagonally. The effective pixel count is 1080(H) x 1920(V) FHD (Full High Definition) The pixel size was 49.5 μm (H) × 49.5 μm (V). The outer dimensions of the panel are 69.76mm (H) x 141.4mm (V). The sensor area is 53.46 mm (H) × 95.04 mm (V). The transistor has an oxide semiconductor in the channel formation region. An E (channel etch) type transistor was used.

[0463] The input / output device of this embodiment can function as a transmissive liquid crystal display device. The element used was a liquid crystal element in FFS mode. The aperture ratio was set to 48.0%. The driving frequency was 60Hz. The video signal format used was analog line sequential.

[0464] The gate driver is built-in, and the source driver uses COF.

[0465] The detection element is a projected capacitance type (mutual capacitance type). The common electrode of the liquid crystal element is The number of sensor units was 18 (H) x 32 (V). Specifically, the conductive film 56a in FIG. 9(A) has 32 pieces, and the conductive film 58 has 18 pieces. The size of one sensor unit is 2.970 mm × 2.970 mm. One conductive film 56b in (A) has a size of 30×60 pixels. The conductive film 56a has a size of 30×1080 pixels.

[0466] One frame period shown in FIG. 8(E) is 16.667 ms, and the writing period is 8.33 3 ms, and the two detection periods are 4.167 ms each.

[0467] The cross-sectional schematic diagram of the input / output device of this embodiment corresponds to FIG. 1(B). For details, refer to Embodiment 1. can.

[0468] The substrate 211 was a glass substrate having a thickness of about 0.7 mm. The substrate 261 was a glass substrate having a thickness of about 0. A glass substrate having a thickness of 1 mm, about 0.2 mm, or about 0.3 mm was used. The gate electrode 221 was The insulating film 213 is a laminated structure of a tungsten nitride film and a copper film. The oxide semiconductor film 223 has a stacked structure of a CAAC-OS film and a silicon oxide film. The oxide semiconductor film 223 is made of CAAC-IGZO, which has a different atomic ratio of metal elements. The two layers were formed using the sputtering targets, and the total thickness of the two layers was The oxide semiconductor film 223 and the oxide conductive film 227 were formed of In-G The oxide conductive film 227 is formed of a-Zn oxide. The oxide conductive film 227 has a single layer structure and a thickness of about The source electrode 225a and the drain electrode 225b are made of a tungsten film. The insulating film 215 has a stacked structure of an aluminum film and a titanium film. The insulating film 217 was a silicon nitride film. The insulating film 219 was an acrylic film. The conductive film 251 and the conductive film 252 were each made of silicon having a thickness of about 100 nm. The insulating film 253 was a silicon nitride film. A negative liquid crystal was used for the substrate 249. The surface of the substrate 261 was covered with a polarizing plate having a thickness of about 200 μm. In this embodiment, an APC film having a thickness of about 100 nm was used for the conductive film 255. Two types of input / output devices were fabricated: one using a TiN film and the other using Ti with a thickness of approximately 200 nm.

[0469] FIG. 35 is a photograph showing the display state of the input / output device of this embodiment. Display area in FIG. The right side and the top side (not shown) of each are connected to FPCs. In the power device, a glass substrate having a thickness of about 0.3 mm was used as the substrate 261. As shown in FIG. 35, an embodiment of the present invention was applied to the APC. By using this, we were able to create an input / output device that can display images well. The input / output device shown in the figure has good detection sensitivity of the touch sensor and is capable of simultaneous multi-point detection. .

[0470] The striped display marks are arranged at intervals approximately equal to the width of the conductive film 56a (the length in the Y direction in FIG. 9(A)). Therefore, in order to make the parasitic capacitances of the conductive film 56a and the conductive film 56b uniform, As shown in FIG. 1, the widths of the conductive films 56a and 56b were changed. After the change, one conductive film 56b has a width of 2 The size of each conductive film 56a is 1×60 pixels. As a result, the resistance value of the conductive film 56b is reduced from 1.66 kΩ to 1.19 kΩ. As a result, the capacitance of the conductive film 56b changed from 534 pF to 674 pF. The value is changed from 0.86 kΩ to 1.35 kΩ, and the capacitance of the conductive film 56a is changed from 930 pF to 68 By making the parasitic capacitance of the conductive film 56a and the conductive film 56b uniform, the display unevenness is reduced. The touch sensing signal is transmitted to the conductive film 56. When the electric current is alternately input to the conductive film 56a and the conductive film 56b, the electric current is more uniform than when the electric current is input to the conductive film 56b. Display unevenness was reduced, and a better display was achieved. [Explanation of symbols]

[0471] 56 Conductive Film 56a Conductive film 56b Conductive film 57a Auxiliary wiring 57b Auxiliary wiring 58 Conductive Film 60 pixels 60a subpixel 60b subpixel 60c subpixel 106 Insulating film 107 Insulating film 114 Insulating film 116 Insulating film 141 Aperture 142 Aperture 193 Target 194 Plasma 201a Transistor 201b Transistor 201c Transistor 203 Transistor 203a Transistor 203b Transistor 205a Connection 205b Connection 207 Liquid crystal element 207a Liquid crystal element 207b Liquid crystal element 211 Substrate 213 Insulating film 215 Insulating film 217 Insulating Film 218 Insulating film 219 Insulating Film 221 Gate electrode 223 Oxide Semiconductor Film 225a Source electrode 225b Drain electrode 226 Conductive Film 227 Oxide Conductive Film 227a Oxide semiconductor film 231 Conductive Film 233 Conductive Film 235 Conductive Film 241 Colored film 243 Light-shielding film 245 Insulating Film 247 Spacer 249 Liquid Crystal 251 Conductive Film 252 Conductive Film 253 Insulating Film 254 Conductive Film 255 Conductive Film 257 Connectors 259 FPC 261 Substrate 265 Adhesive layer 267 Connectors 268 IC 269 ​​FPC 270 Transistors 270A Transistor 270B Transistor 273 pixels 275 Conductive Film 277 areas 300 I / O devices 301 Display section 302 Scanning line driving circuit 303 pixels 502 Substrate 504 Conductive film 506 Insulating film 507 Insulating film 508 Oxide Semiconductor Film 508a Oxide semiconductor film 508b Oxide semiconductor film 508c Oxide semiconductor film 511a Oxide semiconductor film 511b Oxide conductive film 512a Conductive film 512b Conductive film 514 Insulating film 516 Insulating film 518 Insulating film 519 Insulating film 552a opening 552b Opening 552c opening 3501 Wiring 3502 Wiring 3503 Transistor 3504 Liquid crystal elements 3510 Wiring 3510_1 Wiring 3510_2 Wiring 3511 Wiring 3515_1 Block 3515_2 Block 3516 Block 5000 cabinet 5001 Display section 5002 Display section 5003 Speaker 5004 LED Lamp 5005 Operation key 5006 Connection terminal 5007 Sensor 5008 Microphone 5009 Switch 5010 Infrared port 5011 Recording medium reading unit 5012 Stand 5013 Remote control device 5014 Antenna 5015 Shutter button 5016 Image receiving unit 5017 charger 5018 Band 5019 Clasp 5020 Icon 5021 Icon 6500 Touch Panel Module 6501 Circuit Unit 6502 Signal line driver circuit 6503 Sensor driver circuit 6504 Detection circuit 6505 Timing Controller 6506 Image processing circuit 6510 Touch Panel 6511 Display section 6512 Input section 6513 Scanning line driver circuit 6520 IC 6530 IC 6531 Board 6532 Opposing substrate 6533 FPC 6534 PCB 6540 CPU 8000 Touch Panel Module 8001 Top cover 8002 Lower cover 8003 FPC 8004 Touch Panel 8007 Backlight 8008 light source 8009 Frame 8010 Printed Circuit Board 8011 Battery

Claims

[Claim 1] a first pixel electrode, a second pixel electrode, a first common electrode, a second common electrode, a liquid crystal, a first insulating film, a second insulating film, and a transistor; The first common electrode functions as one electrode of the sensing element; the second common electrode functions as the other electrode of the sensing element; the transistor has a first gate, a second gate, and a semiconductor layer; the semiconductor layer has an oxide semiconductor in a channel formation region, the second gate has an oxide conductor; the oxide conductor has one or more metal elements contained in the oxide semiconductor, The semiconductor layer is disposed on the first gate. The second gate is provided on the semiconductor layer; the first insulating film is provided on the second gate; the first pixel electrode, the second pixel electrode, the first common electrode, and the second common electrode are disposed on the first insulating film; the first pixel electrode and the first common electrode have a portion that overlaps with each other via the second insulating film, the second pixel electrode and the second common electrode have a portion overlapping with each other via the second insulating film, The liquid crystal is disposed on the first pixel electrode, the second pixel electrode, the first common electrode, and the second common electrode; the first pixel electrode and the second pixel electrode are located on the same plane and spaced apart from each other; The input / output device, wherein the first common electrode and the second common electrode are located on the same plane and spaced apart from each other.

Citation Information

Patent Citations

  • Integrated touch screen

    JP2010231773A

  • Liquid crystal display device

    JP2013238820A

  • Liquid crystal display device and touch panel

    JP2014095895A

  • In-Plane Switching mode Liquid Crystal Display device having Touch sensing function

    KR1020120054184A