Method for manufacturing p-type nitride semiconductor

The described method for forming P-type nitride semiconductor regions using an SOG liquid and annealing addresses the challenge of achieving high concentration and precise placement, enhancing device efficiency and reliability by minimizing crystal damage.

JP2024163422AInactive Publication Date: 2024-11-22SUMITOMO ELECTRIC INDUSTRIES LTD
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2023079007
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-12
Publication Date
2024-11-22
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing methods for forming P-type semiconductor regions in nitride semiconductors, such as GaN, face challenges in achieving sufficient concentration while minimizing crystal damage and ensuring precise placement, which affects the efficiency and reliability of devices like power converters and transistors.

Method used

A method involving the application of an SOG liquid containing group II atoms, followed by baking and annealing in an inert gas atmosphere to diffuse these atoms into a nitride semiconductor substrate, with subsequent removal of the SOG film, allows for the formation of a P-type semiconductor region with high concentration and minimal crystal damage.

Benefits of technology

This method efficiently forms a P-type semiconductor region with sufficient concentration, reducing crystal damage and improving device characteristics by ensuring precise placement and reducing the risk of deterioration.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024163422000001_ABST
    Figure 2024163422000001_ABST
Patent Text Reader

Abstract

To provide a method for manufacturing a P-type nitride semiconductor capable of efficiently forming a P-type semiconductor region of sufficient concentration.SOLUTION: A method for manufacturing a P-type nitride semiconductor includes: a step for applying SOG solution containing group II atoms on a substrate composed of nitride semiconductors; a step for firing a substrate coated with SOG solution containing group II atoms to form an SOG film; a step for annealing the substrate on which the SOG film is formed under an inert gas atmosphere to diffuse group II atoms into the substrate; and a step for removing the SOG film from the substrate after the step for diffusing group II atoms.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a method for producing a P-type nitride semiconductor. [Background technology]

[0002] Techniques relating to GaN-based devices such as GaN-based transistors have been disclosed (for example, see Patent Document 1, Patent Document 2, and Non-Patent Document 1). The GaN-based transistor disclosed in Patent Document 1 is characterized in that the semiconductor layer directly below the gate electrode is formed from a semiconductor material having a larger band gap than the semiconductor materials forming the other semiconductor layers. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2001-320042 A [Patent Document 2] JP 2020-25056 A [Non-patent literature]

[0004] [Non-Patent Document 1] H.Sakurai et al., “Highly effective activation of Mg-implanted p-type GaN by ultra-high-pressure annealing”, Appl.Phys.Lett.115,142104(2019) Summary of the Invention [Problem to be solved by the invention]

[0005] In devices using semiconductors such as power converters, a reduction in the on-resistance of transistors is required in order to improve efficiency. Here, using a nitride semiconductor such as GaN, which has a large breakdown voltage, is advantageous because the on-resistance can be significantly reduced. From the viewpoint of high voltage resistance and large current flow, vertical transistors such as MOSFETs and IGBTs are preferably used. For such vertical transistors, it is necessary to locally form a P-type semiconductor region. For example, when forming a P-type semiconductor region by ion implantation, it is extremely difficult to selectively form a P-type semiconductor region with a sufficient concentration.

[0006] Therefore, an object of the present invention is to provide a method for manufacturing a P-type nitride semiconductor that can efficiently form a P-type semiconductor region with a sufficient concentration. [Means for solving the problem]

[0007] A method for manufacturing a P-type nitride semiconductor according to the present disclosure includes the steps of applying an SOG (spin on glass) liquid containing Group II atoms onto a substrate made of a nitride semiconductor, baking the substrate onto which the SOG liquid containing Group II atoms has been applied to form an SOG film, annealing the substrate on which the SOG film has been formed in an inert gas atmosphere to diffuse the Group II atoms into the substrate, and removing the SOG film from the substrate after the step of diffusing the Group II atoms. Effect of the Invention

[0008] According to such a method for manufacturing a P-type nitride semiconductor, a P-type semiconductor region with a sufficient concentration can be efficiently formed. [Brief description of the drawings]

[0009] [Figure 1] FIG. 1 is a flowchart showing typical steps of a method for manufacturing a P-type nitride semiconductor according to the first embodiment. [Diagram 2] FIG. 2 is a schematic cross-sectional view showing the prepared substrate. [Diagram 3]FIG. 3 is a schematic cross-sectional view showing a state in which the insulating film has been formed. [Figure 4] FIG. 4 is a schematic cross-sectional view showing a state in which a part of the surface of the substrate is exposed. [Diagram 5] FIG. 5 is a schematic cross-sectional view showing a state in which the substrate has been subjected to a firing process. [Figure 6] FIG. 6 is a schematic cross-sectional view showing a process of carrying out a group II atom diffusion step. [Figure 7] FIG. 7 is a schematic cross-sectional view showing a state in which Mg atoms are diffused into the substrate. [Figure 8] FIG. 8 is a schematic cross-sectional view showing a state after the SOG film and the insulating film have been removed. [Figure 9] FIG. 9 is a schematic cross-sectional view showing a state in which a protective film is formed. [Figure 10] FIG. 10 is a schematic cross-sectional view showing activation treatment of Mg atoms. [Figure 11] FIG. 11 is a schematic cross-sectional view showing a part of a transistor which is an example of a device to which a P-type nitride semiconductor manufactured by the method for manufacturing a P-type nitride semiconductor according to the first embodiment is applied. [Figure 12] FIG. 12 is a flowchart showing typical steps of a method for manufacturing a P-type nitride semiconductor according to the second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] [Description of the embodiments of the present disclosure] First, the embodiments of the present disclosure will be described. The method for producing a P-type nitride semiconductor according to the present disclosure includes the steps of: (1) The method includes the steps of applying an SOG (spin on glass) liquid containing group II atoms onto a substrate made of a nitride semiconductor, baking the substrate onto which the SOG liquid containing group II atoms has been applied to form an SOG film, annealing the substrate on which the SOG film has been formed in an inert gas atmosphere to diffuse the group II atoms into the substrate, and removing the SOG film from the substrate after the step of diffusing the group II atoms.

[0011] When forming a P-type semiconductor region in a P-type nitride semiconductor, for example, ion implantation may be used. However, ion implantation may damage the crystals constituting the substrate, which may deteriorate the device characteristics. In particular, when forming a P-type semiconductor region with a sufficient concentration locally, the damage to the crystals becomes significant, and the damaged crystals cannot be fully restored even by the subsequent annealing process. According to the above-mentioned method for manufacturing a P-type nitride semiconductor, an SOG liquid containing II group atoms is applied and baked to form an SOG film, and then the II group atoms are diffused into the substrate by the annealing process, so that a P-type semiconductor region with a sufficient concentration locally can be formed. In this case, the crystals are not damaged, so that the device characteristics can be prevented from deteriorating. In addition, the P-type semiconductor region is formed by thermal diffusion, which is a relatively simple process. Therefore, according to the above-mentioned method for manufacturing a P-type nitride semiconductor, a P-type semiconductor region with a sufficient concentration can be efficiently formed.

[0012] In addition, a method for producing a P-type nitride semiconductor according to the present disclosure includes the steps of: (2) The method includes the steps of forming an insulating film on a substrate made of a nitride semiconductor, removing a portion of the insulating film formed on the substrate to expose a portion of the surface of the substrate, applying an SOG liquid containing group II atoms onto the exposed surface of the substrate and onto the insulating film, baking the substrate onto which the SOG liquid containing group II atoms has been applied to form an SOG film, annealing the substrate on which the SOG film has been formed in an inert gas atmosphere to diffuse group II atoms into the substrate, and removing the SOG liquid from the substrate after the step of diffusing group II atoms.

[0013] According to this method for manufacturing a P-type nitride semiconductor, an insulating film is formed on a substrate, and then a portion of the insulating film is exposed. Then, a P-type semiconductor region is formed in the exposed region. In this manner, the region other than the exposed region is covered with the insulating film, so that the risk of the SOG liquid being applied can be significantly reduced, and the P-type semiconductor region can be more reliably formed in a desired position.

[0014] (3) In the above (1) or (2), the method for producing a P-type nitride semiconductor may further include a step of activating the Group II atoms after the step of diffusing the Group II atoms. In this way, the Group II atoms in the formed P-type semiconductor region can be activated and effectively utilized when applied to a device.

[0015] (4) In the above (3), the method for producing a P-type nitride semiconductor may further include a step of forming a protective film on the substrate for suppressing the detachment of constituent elements of the substrate after the step of diffusing the group II atoms and before the step of activating the group II atoms. In this way, damage to the crystals constituting the substrate caused by the detachment of the constituent elements of the substrate from the substrate can be suppressed, and the risk of deterioration of the characteristics of a device to which the P-type nitride semiconductor is applied can be reduced.

[0016] (5) In any of the above (1) to (4), the step of applying the SOG liquid containing II group atoms may include a step of applying the SOG liquid containing II group atoms on the substrate by spin coating. In this way, the SOG liquid can be applied efficiently and uniformly on the substrate, that is, while minimizing the difference in thickness between the regions. Therefore, the P-type semiconductor region can be formed with higher accuracy.

[0017] (6) In any one of the above (1) to (5), the group II atom may be Mg (magnesium). Such group II atoms are effectively used when forming a P-type semiconductor region.

[0018] (7) In any of the above (1) to (6), the temperature of the annealing treatment may be 1100° C. or higher and 1300° C. or lower. This makes it possible to more reliably promote the thermal diffusion of Group II atoms into the substrate and to reliably form a P-type semiconductor region.

[0019] (8) In any of the above (1) to (6), the insulating film may contain at least one of SiN (silicon nitride), SiO2 (silicon dioxide) and SiON (silicon oxynitride). Such materials are preferably used because they have relatively high strength and can be firmly bonded to a substrate made of a nitride semiconductor.

[0020] (9) In any of the above (1) to (8), the step of removing the SOG liquid from the substrate may include a step of removing the SOG liquid from the substrate using buffered hydrofluoric acid. In this way, the SOG film can be more reliably removed from the substrate. Therefore, the P-type semiconductor region can be formed with higher accuracy.

[0021] (10) In any of the above (4) to (9), the protective film may contain at least one of diamond-like carbon, SiN, SiO2, and SiON. Such materials are effectively used as a protective film that suppresses desorption of N (nitrogen) from the substrate.

[0022] [Details of the embodiment of the present disclosure] Next, an embodiment of a method for manufacturing a P-type nitride semiconductor according to the present disclosure will be described with reference to the drawings. In the following drawings, the same or corresponding parts are designated by the same reference characters and their description will not be repeated.

[0023] (Embodiment 1) A method for manufacturing a P-type nitride semiconductor according to the first embodiment of the present disclosure will be described below. Fig. 1 is a flowchart showing typical steps of the method for manufacturing a P-type nitride semiconductor according to the first embodiment.

[0024] With reference to FIG. 1, in the method for producing a P-type nitride semiconductor in the first embodiment, first, as a step (S11), a substrate preparation step is performed in which a substrate made of a nitride semiconductor is prepared. FIG. 2 is a schematic cross-sectional view showing the prepared substrate. In FIG. 2 and the following drawings, the direction indicated by the arrow T indicates the thickness direction of the substrate. With reference to FIG. 2, in this step, a substrate made of epitaxially grown GaN is prepared as the substrate. That is, in this embodiment, GaN (gallium nitride) is selected as the nitride semiconductor. The flatness and cleanliness of a surface 2 located in the thickness direction of the substrate 1 is ensured by carrying out a polishing step and a cleaning step.

[0025] Next, as a step (S12), an insulating film forming step is performed. FIG. 3 is a schematic cross-sectional view showing a state in which the insulating film is formed. Referring to FIG. 3, in this step, an insulating film 3 is formed on a surface 2 of a substrate 1. In this embodiment, specifically, the insulating film 3 is formed so as to cover the entire surface 2 of the substrate 1. In this case, a surface 4 of the insulating film 3 is exposed on the substrate 1. The insulating film 3 includes at least one of SiN (silicon nitride), SiO2 (silicon dioxide), and SiON (silicon oxynitride). That is, at least one of SiN, SiO2, and SiON is selected as the material of the insulating film 3. The surface 4 of the insulating film 3 is flat. The insulating film 3 is formed by, for example, PECVD (Plasma Enhanced Chemical Vapor Deposition). The thickness of the insulating film 3 is appropriately selected according to need.

[0026] Next, an exposure step is carried out as a step (S13). FIG. 4 is a schematic cross-sectional view showing a state in which a part of the surface 2 of the substrate 1 is exposed. Referring to FIG. 4, in this step, a part of the insulating film 3 formed on the surface 2 of the substrate 1 is removed. The region to be removed is a region in which a P-type semiconductor region is to be formed. Specifically, a pattern is formed by photolithography on the substrate 1 on which the insulating film 3 is formed. Then, the substrate 1 is subjected to dry etching or wet etching to remove a part of the insulating film 3. In this way, a part of the surface 2 of the substrate 1 is exposed. Of course, the part of the insulating film 3 may be removed by other methods.

[0027] Next, in step (S14), an SOG liquid application step is performed. In this step, an SOG liquid containing group II atoms is applied onto the substrate 1 having a portion of the surface 2 exposed and the other regions covered with the insulating film 3. In this embodiment, Mg is selected as the group II atom. That is, the group II atom is Mg (magnesium). Such group II atoms are effectively used when forming a P-type semiconductor region.

[0028] Here, the application of the SOG liquid is performed by spin coating. Specifically, for example, an SOG liquid containing Mg is used, and the substrate 1 with a part of the surface 2 exposed is rotated at a main rotation speed of 4000 rpm to spin coat and apply the SOG liquid. In this case, the surface 4 of the insulating film 3 and the exposed surface 2 of the substrate 1 are all covered with the SOG liquid. The main rotation speed and application time are appropriately selected depending on the state of the SOG liquid used, the size of the substrate 1, etc.

[0029] Next, a baking step is carried out as a step (S15). Fig. 5 is a schematic cross-sectional view showing a state in which the baking step has been carried out on the substrate 1. Referring to Fig. 5, this step is carried out by, for example, applying an SOG liquid by spin coating, and then baking for 30 minutes using an electric furnace at a temperature of 200°C. This step is also called a pre-bake step, and by this step, an SOG film 5 is formed on the surface 2 of the substrate 1 and on the surface 4 of the insulating film 3.

[0030] Next, as step (S16), a group II atom diffusion step is performed. In this embodiment, a Mg atom diffusion step is performed as the group II atom diffusion step. FIG. 6 is a schematic cross-sectional view when the group II atom diffusion step is performed. Referring to FIG. 6, in this step, an annealing treatment device 6 in an inert gas atmosphere, in this embodiment, a nitrogen atmosphere, is used to perform the annealing treatment. Specifically, for example, the substrate 1 on which the SOG film 5 is formed is placed in the annealing treatment device 6 used as a thermal diffusion furnace, and the annealing treatment is performed for 10 minutes at a temperature of 1100° C. or more and 1300° C. or less, more specifically, at a temperature of 1200° C. The annealing treatment may be performed for several tens of minutes. In this case, the diffusion of the Mg atoms into the substrate 1 is solid-phase diffusion. In this way, the thermal diffusion of the group II atoms, i.e., Mg, into the substrate 1 can be more reliably promoted, and a P-type semiconductor region with a sufficient concentration can be reliably formed.

[0031] In this manner, Mg atoms are diffused into the substrate 1. Fig. 7 is a schematic cross-sectional view showing a state in which Mg atoms have been diffused into the substrate 1. Referring to Fig. 7, in the exposed region of the substrate 1, Mg atoms are diffused into a region 7 indicated by a dashed line extending from the surface 2 to the inside. This region 7 into which the Mg atoms have been diffused will later form a P-type semiconductor region.

[0032] Next, in step (S17), an SOG film removal step is performed. In this step, the SOG film is removed from the surface of the substrate 1 using, for example, buffered hydrofluoric acid (B-HF). At this time, the insulating film 3 may also be removed. Fig. 8 is a schematic cross-sectional view showing a state after the SOG film 5 and the insulating film 3 have been removed. Referring to Fig. 8, a region 7 in which Mg atoms have diffused from a portion of the surface 2 to the inside of the substrate 1 is formed.

[0033] Next, a protective film forming step is carried out as a step (S18). In this step, for example, diamond-like carbon (DLC) is used as the protective film. The protective film suppresses the detachment of the constituent elements of the substrate 1, specifically N (nitrogen) in this embodiment, on the substrate 1. FIG. 9 is a schematic cross-sectional view showing a state in which the protective film is formed. Referring to FIG. 9, a protective film 8 is formed on the surface 2 of the substrate 1 including the region 7 in which Mg atoms are diffused. The protective film 8 is formed over the entire surface 2 of the substrate 1 including the region 7.

[0034] Next, as a step (S19), a group II atom activation process is performed. In this embodiment, a Mg atom activation process is performed as the group II atom activation process. FIG. 10 is a schematic cross-sectional view when activating Mg atoms. With reference to FIG. 10, in this process, for example, Mg atoms diffused in the substrate 1 are activated by annealing. Specifically, as shown in FIG. 10, the substrate 1 on which the protective film 8 is formed is placed in an annealing treatment device 6. Then, the Mg atoms are activated at a temperature higher than that in the above-mentioned group II atom diffusion process (S16), for example, at a temperature of 1400° C. In this manner, the Mg atoms are activated to manufacture a P-type nitride semiconductor.

[0035] The manufactured P-type nitride semiconductor is effectively used, for example, when manufacturing transistors, specifically, MOSFETs (Metal-Oxide-Semiconductor Field Effect Transistors) and IGBTs (Insulated Gate Bipolar Transistors).

[0036] According to this method for manufacturing a P-type nitride semiconductor, an SOG liquid containing Mg atoms is applied and baked to form an SOG film, and then the Mg atoms are diffused into the substrate by annealing, so that a P-type semiconductor region with a sufficient concentration can be formed locally. In this case, the crystal is not damaged, so that deterioration of device characteristics can be prevented. In addition, the P-type semiconductor region is formed by thermal diffusion, which is a relatively simple process. Therefore, according to the above method for manufacturing a P-type nitride semiconductor, a P-type semiconductor region with a sufficient concentration can be efficiently formed.

[0037] In this embodiment, after forming an insulating film 3 on the substrate 1, a part of the insulating film 3 is exposed. Then, a P-type semiconductor region is formed in the exposed region. Since the region other than the exposed region is covered with the insulating film 3, the risk of the SOG liquid being applied can be significantly reduced, and the P-type semiconductor region can be more reliably formed in a desired position.

[0038] In this embodiment, the method for producing a P-type nitride semiconductor includes a step of forming a protective film on the substrate for suppressing the detachment of constituent elements of the substrate after the step of diffusing group II atoms and before the step of activating the group II atoms. This suppresses damage to the crystals constituting the substrate caused by the detachment of the constituent elements of the substrate from the substrate, thereby reducing the risk of deterioration of the characteristics of a device to which the P-type nitride semiconductor is applied.

[0039] In the above embodiment, in the SOG film removal step (S17), the insulating film is removed together with the SOG film. However, this is not limited to the above, and the insulating film may be left behind and only the SOG film may be removed, so that the insulating film can be effectively utilized in a subsequent manufacturing step.

[0040] In the above embodiment, the protective film is formed in the protective film forming step (S18), but this is not limiting, and the protective film may not be formed as necessary.

[0041] An example of the structure of a device applying a P-type nitride semiconductor manufactured using the manufacturing method for a P-type nitride semiconductor in the above-mentioned embodiment 1 will be briefly described. Fig. 11 is a schematic cross-sectional view showing a part of a transistor, which is an example of a device applying a P-type nitride semiconductor manufactured using the manufacturing method for a P-type nitride semiconductor in the embodiment 1. Fig. 11 is a cross-sectional view taken along a plane perpendicular to the thickness direction of a substrate.

[0042] 11, the transistor 11 includes a drain electrode 12, a GaN substrate 13, a gate insulating film 15, a gate electrode 16, an interlayer insulating film 17, a gate pad (not shown), and a source pad 20. A nitride semiconductor 14 is formed on the GaN substrate 13. The transistor 11 in this embodiment has a planar gate structure. The nitride semiconductor 14 is a n-type nitride semiconductor 14 disposed on the drain electrode 12 side. - The drift region 23 and the p + The transistor cell 22 of the nitride semiconductor 14 includes a p - Body region 25, n + A source region 26 and p + A contact region 27 is formed. - The body region 25 includes the channel region 21 .

[0043] In the transistor 11, a voltage is applied to the gate electrode 16 to generate an electric field in the channel region 21, and the n-channel MOSFET 22 of the transistor cell 22 is connected from the source pad 20 to the gate electrode 16. + Source region 26, p - Body area 25, n - It controls the current that passes through the drift region 23 and reaches the drain electrode 12. When manufacturing a P-type nitride semiconductor in such a transistor 11, the manufacturing method in the above-mentioned first embodiment is adopted.

[0044] (Embodiment 2) Another embodiment, that is, embodiment 2, will now be described. Fig. 12 is a flowchart showing typical steps of a method for manufacturing a P-type nitride semiconductor in embodiment 2.

[0045] 12, the method for manufacturing a P-type nitride semiconductor in the second embodiment includes a substrate preparation step (S21) of preparing a substrate made of a nitride semiconductor, an SOG liquid application step (S22) of applying an SOG liquid containing Mg atoms, which are group II atoms, onto the prepared substrate, a firing step (S23) of firing the substrate onto which the SOG liquid containing the group II atoms has been applied to form an SOG film, a group II atom diffusion step (S24) of annealing the substrate on which the SOG film has been formed in an inert gas atmosphere of nitrogen to diffuse group II atoms into the substrate, and an SOG film removal step (S25) of removing the SOG film from the substrate after the step of diffusing group II atoms. The step (S21) corresponds to the step (S11) in the manufacturing method of the first embodiment. The step (S22) corresponds to the step (S14) in the manufacturing method of the first embodiment. The step (S23) corresponds to the step (S15) in the manufacturing method of the first embodiment. The step (S24) corresponds to the step (S16) in the manufacturing method of the first embodiment. Step (S25) corresponds to step (S17) in the manufacturing method of embodiment 1. In this embodiment, for example, the group II atoms are Mg atoms, that is, step (S24) is a Mg atom diffusion step.

[0046] This method of manufacturing a P-type nitride semiconductor also makes it possible to efficiently form a P-type semiconductor region with a sufficient concentration.

[0047] In the second embodiment, the group-II atom diffusing step (S24) may be performed by forming a resist film, patterning the SOG by photolithography, and diffusing the group-II atoms by annealing, or by diffusing the group-II atoms over the entire surface by annealing, removing the SOG film, and then physically removing the substrate to perform patterning.

[0048] (Other embodiments) In the above embodiment, diamond-like carbon is used as the protective film, but SiN, SiO2, and SiON, which partially contain N, may be used. The protective film may also contain at least one of diamond-like carbon, SiN, SiO2, and SiON. Such materials are effectively used as protective films that suppress the desorption of N from the substrate.

[0049] In the above embodiment, Mg is used as the group II atom, but the present invention is not limited to this, and other group II atoms such as Be (beryllium) and Ca (calcium) may be used. In addition, nitrogen gas is used as the inert gas, but the present invention is not limited to this, and other inert gas such as Ar (argon) may be used.

[0050] In the above embodiment, the SOG film is removed from the substrate using buffered hydrofluoric acid, but the present invention is not limited to this, and other methods, for example, the SOG film may be removed from the substrate using hydrofluoric acid. In the above embodiment, GaN is used as the nitride semiconductor, but the present invention is not limited to this, and other nitride semiconductors, for example, AlN (aluminum nitride), may be used.

[0051] It should be understood that the embodiments disclosed herein are illustrative in all respects and are not limiting in any respect. The scope of the present invention is defined by the claims, not the above description, and is intended to include all modifications within the meaning and scope of the claims. [Explanation of symbols]

[0052] 1,13 Board 2,4 surface 3. Insulating film 5 SOG membrane 6 Annealing treatment equipment 7 areas 8 Protective film 11 Transistor 12 Drain electrode 14. Nitride Semiconductors 15 Gate insulating film 16 Gate electrode 17 Interlayer insulating film 20 Sauce Pad 21 Channel Region 22 Transistor Cell 23 Drift Region 24,27 p + Contact Area 25 p - Body Region 26 n + Source Region T Arrow

Claims

1. A step of applying an SOG liquid containing group II atoms onto a substrate made of a nitride semiconductor; baking the substrate coated with the SOG liquid containing the group II atoms to form an SOG film; annealing the substrate on which the SOG film is formed in an inert gas atmosphere to diffuse the Group II atoms into the substrate; removing the SOG film from above the substrate after the step of diffusing the Group II atoms.

2. forming an insulating film on a substrate made of a nitride semiconductor; removing a portion of the insulating film formed on the substrate to expose a portion of a surface of the substrate; applying an SOG liquid containing group II atoms onto the exposed surface of the substrate and onto the insulating film; baking the substrate coated with the SOG liquid containing the group II atoms to form an SOG film; annealing the substrate on which the SOG film is formed in an inert gas atmosphere to diffuse the Group II atoms into the substrate; removing the SOG liquid from above the substrate after the step of diffusing the Group II atoms.

3. 3. The method for producing a P-type nitride semiconductor according to claim 1, further comprising the step of activating said Group II atoms after said step of diffusing said Group II atoms.

4. 4. The method for producing a P-type nitride semiconductor according to claim 3, further comprising the step of forming a protective film on the substrate for suppressing detachment of constituent elements of the substrate after the step of diffusing the group II atoms and before the step of activating the group II atoms.

5. 3. The method for producing a P-type nitride semiconductor according to claim 1, wherein the step of applying the SOG liquid containing the group II atoms includes the step of applying the SOG liquid containing the group II atoms by spin coating on the substrate.

6. 3. The method for producing a P-type nitride semiconductor according to claim 1, wherein the group II atom is Mg.

7. 3. The method for producing a P-type nitride semiconductor according to claim 1, wherein the annealing temperature is 1100° C. or higher and 1300° C. or lower.

8. The insulating film is made of SiN, SiO 2 3. The method for producing a P-type nitride semiconductor according to claim 2, wherein the P-type nitride semiconductor comprises at least one of Nb, Nb, and SiON.

9. 3. The method for producing a P-type nitride semiconductor according to claim 1, wherein the step of removing the SOG film from the substrate includes the step of removing the SOG liquid from the substrate using buffered hydrofluoric acid.

10. The protective film is made of diamond-like carbon, SiN, SiO 2 5. The method for producing a P-type nitride semiconductor according to claim 4, wherein the P-type nitride semiconductor comprises at least one of Nb, Fe, and SiON.

Citation Information

Patent Citations

  • Field effect transistor

    JP2005285924A

  • Method for manufacturing nitride semiconductor device

    JP2006156914A

  • Semiconductor device and manufacturing method thereof

    JP2007234972A

  • Method of manufacturing needle-like electron emitter for electron-emitting element and method of manufacturing electron-emitting element

    JP2007257894A

  • Semiconductor device

    JP2020155784A