Injection mold and injection molding apparatus
The injection mold with a cooling pipe featuring a fine uneven structure or spiral groove addresses the issue of mold temperature rise by enhancing heat exchange, allowing faster production of molded products.
Patent Information
- Application Number
- JP2023085869
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-25
- Publication Date
- 2024-12-05
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
In injection molding using existing molds, as the number of molding shots increases, the mold temperature rises, leading to defective products, and increasing the cooling time to reduce defects extends the cycle time, reducing productivity.
The injection mold incorporates a cooling pipe with a fine uneven structure or spiral groove on its inner surface to enhance turbulence and contact area for improved heat exchange, allowing faster cooling and solidification of molten resin.
This design improves heat exchange efficiency, enabling the production of more molded products in a shorter time without extending the cycle time.
Smart Images

Figure 2024168854000001_ABST
Abstract
Description
[Technical field]
[0001] The present disclosure relates to an injection mold and an injection molding apparatus. [Background technology]
[0002] Japanese Patent Application Laid-Open Publication No. 2015-189075 (Patent Document 1) discloses a mold for use in an injection molding method. The mold includes a heat transfer medium flow path. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2015-189075 A Summary of the Invention [Problem to be solved by the invention]
[0004] In injection molding using the mold disclosed in Patent Document 1, as the number of molding shots increases, the temperature of the mold rises, resulting in the generation of defective molded products. If the cooling time of the molten resin is extended to reduce the number of defective molded products, the cycle time per molding shot increases, and the productivity of molded products decreases. The present disclosure has been made in consideration of the above problems, and its purpose is to provide an injection molding mold and an injection molding device that can manufacture more molded products in a shorter time. [Means for solving the problem]
[0005] The injection molding die of the present disclosure includes a cooling pipe through which a cooling liquid flows. A fine concave-convex structure or a spiral groove is formed on at least a portion of the inner surface of the cooling pipe.
[0006] The injection molding apparatus of the present disclosure includes the injection mold of the present disclosure. Effect of the Invention
[0007] When the cooling liquid flows through the cooling pipe, the fine uneven structure and the spiral groove generate turbulence in the cooling liquid. This turbulence improves the efficiency of heat exchange between the cooling liquid and the injection mold. In addition, the fine uneven structure and the spiral groove increase the contact area between the cooling liquid and the inner surface of the cooling pipe. Therefore, the efficiency of heat exchange between the cooling liquid and the injection mold is improved. In this way, the molten resin in the injection mold is cooled and solidified in a shorter time. According to the injection mold and injection molding device of the present disclosure, more molded products can be manufactured in a shorter time. [Brief description of the drawings]
[0008] [Figure 1] FIG. 2 is a schematic diagram of an injection molding device according to the first and second embodiments. [Diagram 2] 1 is a schematic cross-sectional view of an injection molding die according to a first embodiment. [Diagram 3] 2 is a schematic partial enlarged cross-sectional view of an example of a cooling pipe according to the first embodiment. FIG. [Figure 4] 4 is a schematic partial enlarged cross-sectional view of another example of the cooling pipe of the first embodiment. FIG. [Diagram 5] FIG. 2 is a flowchart showing the injection molding method according to the first embodiment. [Figure 6] FIG. 4 is a schematic cross-sectional view of an injection molding die according to a modified example of the first embodiment. [Figure 7] FIG. 11 is a schematic cross-sectional view of an injection molding die according to a second embodiment. [Figure 8] FIG. 11 is a schematic partially enlarged cross-sectional view of a cooling pipe according to a second embodiment. [Figure 9] 9 is a schematic partially enlarged cross-sectional view of the cooling pipe of the second embodiment taken along the cross-sectional line IX-IX shown in FIG. 8. [Figure 10] FIG. 11 is a schematic cross-sectional view of an injection molding die according to a modified example of the second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] Hereinafter, embodiments of the present disclosure will be described. Note that the same reference numerals are used to refer to the same components, and the description thereof will not be repeated.
[0010] Embodiment 1 An injection molding apparatus 1 and an injection mold 3 according to a first embodiment will be described with reference to Figures 1 to 4. With reference to Figure 1, the injection molding apparatus 1 includes a hopper 11, a cylinder 12, and an injection mold 3.
[0011] The hopper 11 stores a resin material. The resin material is supplied from the hopper 11 to the cylinder 12. The resin material is not particularly limited, but may be, for example, polystyrene (PS), acrylonitrile-butadiene-styrene (ABS), polypropylene (PP), polycarbonate (PC), polyphenylene sulfide (PPS), polybutylene terephthalate (PBT), or the like.
[0012] The resin material is heated and melted in the cylinder 12. The molten resin is supplied from the cylinder 12 to the injection molding die 3.
[0013] With reference to FIGS. 1 and 2, the injection mold 3 includes a fixed mold 14 and a movable mold 20.
[0014] The fixed mold 14 includes a mold body 15, a primary sprue 16, a runner 17, and a secondary sprue 18. The primary sprue 16, the runner 17, and the secondary sprue 18 are provided in the mold body 15. The primary sprue 16 communicates with the runner 17. The runner 17 communicates with the secondary sprue 18.
[0015] The movable mold 20 is movable relative to the fixed mold 14. The movable mold 20 includes a mold body 21, a gate 22, a cavity 23, and a cooling pipe 30. When the injection molding mold 3 is closed, the gate 22 communicates with the secondary sprue 18. The cavity 23 communicates with the gate 22. The gate 22 and the cavity 23 are provided in the mold body 21. The cooling pipe 30 is provided inside the mold body 21. A cooling liquid 35, such as water, oil, or ethylene glycol, flows through the cooling pipe 30.
[0016] The cooling pipe 30 is connected to a temperature regulator (not shown) and a pump (not shown). Cooling liquid 35 circulates through the temperature regulator, the pump, and the cooling pipe 30. Specifically, the pump supplies the cooling liquid 35, the temperature of which has been adjusted to a target temperature by the temperature regulator, to the cooling pipe 30. When the cooling liquid 35 flows through the cooling pipe 30, heat exchange occurs between the injection molding die 3 and the cooling liquid 35, and the injection molding die 3 is cooled. The temperature regulator adjusts the temperature of the cooling liquid 35, which has been increased by this heat exchange, to the target temperature. The pump supplies the cooling liquid 35, the temperature of which has been adjusted to the target temperature, to the cooling pipe 30 again.
[0017] 2, the fine uneven structure 31 is formed on the inner surface 30a of the cooling pipe 30. The fine uneven structure 31 may be formed on at least a portion of the inner surface 30a facing the cavity 23. The fine uneven structure 31 may be formed on the entire inner surface 30a. The fine uneven structure 31 has a maximum height roughness Rz of, for example, 100 μm or more. The maximum height roughness Rz is the maximum height roughness Rz of Japanese Industrial Standards (JIS) B 0601:2013.
[0018] The fine uneven structure 31 is formed on the inner surface 30a of the cooling pipe 30 by performing a surface treatment such as etching or blasting.
[0019] Etching is a processing method that uses the corrosive action of acid, alkali, or ions to dissolve the surface of a material such as metal or glass. There are two types of etching methods used in etching: wet etching and dry etching. In wet etching, the surface of a material is processed by using the corrosive action of acid or alkali. In dry etching, the surface of a material is processed by removing atoms from the surface of the material using high vacuum plasma (ion beam).
[0020] Blasting is a process in which particulate abrasives are collided with the surface of a material to roughen or remove it. Blasting includes grit blasting and shot blasting.
[0021] Grit blasting is a method of processing the surface of a material by blasting an abrasive material having sharp edges against the surface of the material. As the material of the abrasive material, a high-hardness material such as ceramics such as alumina, glass, or silicon carbide, or a low-hardness material such as plastics such as polyester, can be used. By performing the grit blasting process on the inner surface 30a of the cooling pipe 30, the inner surface 30a of the cooling pipe 30 becomes an uneven surface with sharp edges, as shown in FIG. 3.
[0022] Shot blasting is a method for processing the surface of a material by blasting spherical abrasives against the surface of the material. By subjecting the inner surface 30a of the cooling pipe 30 to shot blasting, the inner surface 30a of the cooling pipe 30 becomes a rounded uneven surface, as shown in FIG.
[0023] An injection molding method of this embodiment using the injection molding die 3 of this embodiment will be described with reference to Fig. 5. The injection molding method of this embodiment includes a mold clamping step (S1), an injection step (S2), a cooling step (S3), a mold opening step (S4), and a demolding step (S5).
[0024] In the mold clamping step (S1), the movable mold 20 is moved toward the fixed mold 14 to close the injection molding mold 3. The fixed mold 14 and the movable mold 20 are pressed against each other.
[0025] The injection step (S2) includes a filling step and a pressure holding step. In the filling step, a resin material is supplied from a hopper 11 to a cylinder 12. The cylinder 12 heats and melts the resin material. The molten resin is supplied from the cylinder 12 to an injection mold 3. Specifically, the molten resin is supplied to a cavity 23 through a primary sprue 16, a runner 17, a secondary sprue 18, and a gate 22. For example, the molten resin is supplied to the cavity 23 until about 95% to about 99% of the volume of the cavity 23 is filled with the molten resin. After the filling step, a pressure holding step is performed. In the pressure holding step, the injection of the molten resin from the gate 22 is continued at a constant pressure for a certain period of time. In this way, the molten resin at the gate 22 solidifies, and the molten resin can be prevented from flowing back from the gate 22.
[0026] In the cooling step (S3), the molten resin filled in the cavity 23 is cooled so that the temperature of the molten resin approaches the mold temperature, and the molten resin is solidified. In this way, a molded product that matches the shape of the cavity 23 is obtained.
[0027] In the mold opening process (S4), the movable mold 20 is moved away from the fixed mold 14 to open the injection mold 3. In the mold releasing process (S5), an ejector pin (not shown) is used to push the molded product out of the injection mold 3. The molded product is then removed from the injection mold 3. In this manner, the molded product is manufactured.
[0028] The operation of this embodiment will be described in comparison with a comparative example. The injection molding die of the comparative example has a similar configuration to the injection molding die 3 of this embodiment, but differs from the injection molding die 3 of this embodiment in that the micro concave-convex structure 31 is not formed on the inner surface 30a of the cooling pipe 30, and the inner surface 30a of the cooling pipe 30 is a smooth surface.
[0029] When 20 shots of continuous molding are performed using the comparative injection molding die with a set die temperature of 40°C, a molten resin temperature of 210°C, a cooling time of 10 seconds, and a cycle time of 30 seconds, the die temperature rises to 42.6°C, which is higher than the set die temperature. If the die temperature exceeds the set die temperature, the molten resin in the injection molding die 3 is not sufficiently cooled and solidified within the cooling time, resulting in defective molded products. If the cooling time of the molten resin is extended to reduce defective molded products, the cycle time per molding shot will be extended, and the productivity of molded products will decrease.
[0030] In contrast, in the injection molding die 3 of this embodiment, a fine uneven structure 31 is formed on the inner surface 30a of the cooling tube 30. When the cooling liquid 35 flows through the cooling tube 30, the fine uneven structure 31 generates turbulence in the cooling liquid 35. This turbulence improves the efficiency of heat exchange between the cooling liquid 35 and the injection molding die 3. In addition, the fine uneven structure 31 increases the contact area between the cooling liquid 35 and the inner surface 30a of the cooling tube 30. Therefore, the efficiency of heat exchange between the cooling liquid 35 and the injection molding die 3 is improved. When 20 shots of continuous molding are performed using the injection molding die 3 of this embodiment with a set mold temperature of 40°C, a molten resin temperature of 210°C, a cooling time of 10 seconds, and a cycle time of 30 seconds, the mold temperature can be kept below the set mold temperature. In this way, the molten resin in the injection molding die 3 is cooled and solidified in a shorter time. According to the injection molding die 3 and the injection molding device 1 of this embodiment, more molded products can be manufactured in a shorter time.
[0031] (Modification) 6, in a modification of the present embodiment, the fine uneven structure 31 may be formed on a part of the inner surface 30a of the cooling pipe 30. The part of the inner surface 30a on which the fine uneven structure 31 is formed may be a part of the inner surface 30a facing the cavity 23.
[0032] In another modified example of this embodiment, the cooling pipe 30 may be provided in the fixed mold 14 or in both the movable mold 20 and the fixed mold 14 .
[0033] The effects of the injection molding die 3 and the injection molding apparatus 1 of this embodiment will be described. The injection molding die 3 of this embodiment includes a cooling pipe 30 through which a cooling liquid 35 flows. A fine concave-convex structure 31 is formed on at least a part of an inner surface 30a of the cooling pipe 30.
[0034] When the cooling liquid 35 flows through the cooling tube 30, the fine uneven structure 31 generates turbulence in the cooling liquid 35. This turbulence improves the efficiency of heat exchange between the cooling liquid 35 and the injection molding die 3. In addition, the fine uneven structure 31 increases the contact area between the cooling liquid 35 and the inner surface 30a of the cooling tube 30. Therefore, the efficiency of heat exchange between the cooling liquid 35 and the injection molding die 3 is improved. In this way, the molten resin in the injection molding die 3 is cooled and solidified in a shorter time. According to the injection molding die 3 of this embodiment, it is possible to manufacture more molded products in a shorter time.
[0035] In the injection molding die 3 of this embodiment, at least a portion of the inner surface 30a is the entire inner surface 30a.
[0036] Therefore, the turbulence generated in the cooling liquid 35 and the contact area between the cooling liquid 35 and the inner surface 30a of the cooling pipe 30 are increased. The efficiency of heat exchange between the cooling liquid 35 and the injection molding die 3 is improved. The molten resin in the injection molding die 3 is cooled and solidified in a shorter time. According to the injection molding die 3 of this embodiment, it is possible to manufacture more molded products in a shorter time.
[0037] In the injection molding die 3 of this embodiment, at least a part of the inner surface 30a is a part of the inner surface 30a.
[0038] Since the area in which the fine concave-convex structure 31 is formed is reduced, the manufacturing cost of the injection molding die 3 is reduced.
[0039] The injection molding die 3 of the present embodiment further includes a cavity 23. At least a part of the inner surface 30a is a portion of the inner surface 30a that faces the cavity 23.
[0040] The portion of the injection mold 3 near the cavity 23 is the portion of the injection mold 3 that becomes the hottest during injection molding. The fine uneven structure 31 is formed on the portion of the inner surface 30a of the cooling pipe 30 that faces the portion of the injection mold 3 that becomes the hottest during injection molding. Therefore, the portion of the injection mold 3 that becomes the hottest during injection molding is efficiently cooled. The molten resin in the injection mold 3 is cooled and solidified in a shorter time. According to the injection mold 3 of this embodiment, it is possible to manufacture more molded products in a shorter time.
[0041] In the injection molding die 3 of this embodiment, a fine concave-convex structure 31 having a maximum height roughness of 100 μm or more is formed on at least a part of the inner surface 30a.
[0042] Therefore, turbulence occurs in the cooling liquid 35 more. The efficiency of heat exchange between the cooling liquid 35 and the injection molding die 3 is improved. The molten resin in the injection molding die 3 is cooled and solidified in a shorter time. According to the injection molding die 3 of this embodiment, it is possible to manufacture more molded products in a shorter time.
[0043] An injection molding apparatus 1 of this embodiment includes an injection molding die 3 of this embodiment. When the cooling liquid 35 flows through the cooling pipe 30, the fine uneven structure 31 generates turbulence in the cooling liquid 35. This turbulence improves the efficiency of heat exchange between the cooling liquid 35 and the injection mold 3. In addition, the fine uneven structure 31 increases the contact area between the cooling liquid 35 and the inner surface 30a of the cooling pipe 30. Therefore, the efficiency of heat exchange between the cooling liquid 35 and the injection mold 3 is improved. In this way, the molten resin in the injection mold 3 is cooled and solidified in a shorter time. According to the injection molding apparatus 1 of this embodiment, it is possible to manufacture more molded products in a shorter time.
[0044] Embodiment 2 An injection molding apparatus 1 and an injection molding die 3 according to the second embodiment will be described with reference to Figures 1 and 7 to 9. The injection molding apparatus 1 and the injection molding die 3 according to the present embodiment have the same configuration as the injection molding apparatus 1 and the injection molding die 3 according to the first embodiment, but differ mainly in the following points.
[0045] 7 to 9, the spiral groove 32 is formed on the inner surface 30a of the cooling pipe 30. The spiral groove 32 may be formed on at least a portion of the inner surface 30a facing the cavity 23. The spiral groove 32 may be formed on the entire inner surface 30a. The spiral groove 32 includes a recess 32a and a protrusion 32b. The groove depth of the spiral groove 32 is, for example, 0.5 mm or more. The groove depth of the spiral groove 32 is the difference in height between the bottom of the recess 32a and the top of the protrusion 32b. The spiral groove 32 is formed by cutting, polishing, or etching the inner surface 30a of the cooling pipe 30.
[0046] When the cooling liquid 35 flows through the cooling pipe 30, the spiral groove 32 generates turbulence in the cooling liquid 35. This turbulence improves the efficiency of heat exchange between the cooling liquid 35 and the injection molding die 3. In addition, the spiral groove 32 increases the contact area between the cooling liquid 35 and the inner surface 30a of the cooling pipe 30. Therefore, the efficiency of heat exchange between the cooling liquid 35 and the injection molding die 3 is improved. In this way, the molten resin in the injection molding die 3 is cooled and solidified in a shorter time. According to the injection molding die 3 and the injection molding device 1 of this embodiment, more molded products can be obtained in a shorter time.
[0047] (Modification) 10, in a modification of the present embodiment, the spiral groove 32 may be formed in a part of the inner surface 30a of the cooling pipe 30. The part of the inner surface 30a in which the spiral groove 32 is formed may be a part of the inner surface 30a facing the cavity 23.
[0048] In another modified example of this embodiment, the cooling pipe 30 may be provided in the fixed mold 14 or in both the movable mold 20 and the fixed mold 14 .
[0049] The injection molding die 3 and injection molding apparatus 1 of the present embodiment have the following advantages similar to those of the injection molding die 3 and injection molding apparatus 1 of the first embodiment.
[0050] The injection molding die 3 of this embodiment includes a cooling pipe 30 through which a cooling liquid 35 flows. A spiral groove 32 is formed on at least a part of an inner surface 30a of the cooling pipe 30.
[0051] When the cooling liquid 35 flows through the cooling pipe 30, the spiral groove 32 generates turbulence in the cooling liquid 35. This turbulence improves the efficiency of heat exchange between the cooling liquid 35 and the injection mold 3. In addition, the spiral groove 32 increases the contact area between the cooling liquid 35 and the inner surface 30a of the cooling pipe 30. Therefore, the efficiency of heat exchange between the cooling liquid 35 and the injection mold 3 is improved. In this way, the molten resin in the injection mold 3 is cooled and solidified in a shorter time. According to the injection mold 3 of this embodiment, it is possible to manufacture more molded products in a shorter time.
[0052] In the injection molding die 3 of this embodiment, at least a portion of the inner surface 30a is the entire inner surface 30a.
[0053] Therefore, the turbulence generated in the cooling liquid 35 and the contact area between the cooling liquid 35 and the inner surface 30a of the cooling pipe 30 are increased. The efficiency of heat exchange between the cooling liquid 35 and the injection molding die 3 is improved. The molten resin in the injection molding die 3 is cooled and solidified in a shorter time. According to the injection molding die 3 of this embodiment, it is possible to manufacture more molded products in a shorter time.
[0054] In the injection molding die 3 of this embodiment, at least a part of the inner surface 30a is a part of the inner surface 30a.
[0055] Since the area in which the spiral groove 32 is formed is reduced, the manufacturing cost of the injection molding die 3 is reduced.
[0056] The injection molding die 3 of the present embodiment further includes a cavity 23. At least a part of the inner surface 30a is a portion of the inner surface 30a that faces the cavity 23.
[0057] The portion of the injection mold 3 near the cavity 23 is the portion of the injection mold 3 that becomes the hottest during injection molding. The spiral groove 32 is formed in a portion of the inner surface 30a of the cooling pipe 30 that faces the portion of the injection mold 3 that becomes the hottest during injection molding. Therefore, the portion of the injection mold 3 that becomes the hottest during injection molding is efficiently cooled. The molten resin in the injection mold 3 is cooled and solidified in a shorter time. According to the injection mold 3 of this embodiment, it is possible to manufacture more molded products in a shorter time.
[0058] In the injection molding die 3 of this embodiment, a spiral groove 32 having a groove depth of 0.5 mm or more is formed on at least a part of the inner surface 30a.
[0059] Therefore, turbulence occurs in the cooling liquid 35 more. The efficiency of heat exchange between the cooling liquid 35 and the injection molding die 3 is improved. The molten resin in the injection molding die 3 is cooled and solidified in a shorter time. According to the injection molding die 3 of this embodiment, it is possible to manufacture more molded products in a shorter time.
[0060] An injection molding apparatus 1 of this embodiment includes an injection molding die 3 of this embodiment. When the cooling liquid 35 flows through the cooling pipe 30, the spiral groove 32 generates turbulence in the cooling liquid 35. This turbulence improves the efficiency of heat exchange between the cooling liquid 35 and the injection mold 3. In addition, the spiral groove 32 increases the contact area between the cooling liquid 35 and the inner surface 30a of the cooling pipe 30. Therefore, the efficiency of heat exchange between the cooling liquid 35 and the injection mold 3 is improved. In this way, the molten resin in the injection mold 3 is cooled and solidified in a shorter time. According to the injection molding apparatus 1 of this embodiment, it is possible to manufacture more molded products in a shorter time.
[0061] Various aspects of the present disclosure are summarized below as appendices. (Appendix 1) A cooling pipe through which a cooling liquid flows is provided, An injection molding die, wherein a fine uneven structure or a spiral groove is formed on at least a part of an inner surface of the cooling pipe. (Appendix 2) 2. The injection molding die of claim 1, wherein the at least a portion of the inner surface is the entire inner surface. (Appendix 3) 2. The injection mold of claim 1, wherein the at least a portion of the inner surface is a portion of the inner surface. (Appendix 4) Further provided with a cavity, 4. The injection molding die of claim 3, wherein the at least a portion of the inner surface is a portion of the inner surface that faces the cavity. (Appendix 5) The injection molding die according to any one of claims 1 to 4, wherein the fine uneven structure having a maximum height roughness of 100 μm or more is formed on at least the portion of the inner surface. (Appendix 6) 5. The injection molding die according to claim 1, wherein the spiral groove has a groove depth of 0.5 mm or more formed on at least a portion of the inner surface. (Appendix 7) 7. An injection molding apparatus comprising the injection mold according to any one of claims 1 to 6.
[0062] The first and second embodiments disclosed herein and their modified examples should be considered to be illustrative and not restrictive in all respects. The scope of the present disclosure is indicated by the claims, not the above description, and is intended to include all modifications within the meaning and scope of the claims. [Explanation of symbols]
[0063] 1 injection molding apparatus, 3 injection molding mold, 11 hopper, 12 cylinder, 14 fixed mold, 15 mold body, 16 primary sprue, 17 runner, 18 secondary sprue, 20 movable mold, 21 mold body, 22 gate, 23 cavity, 30 cooling tube, 30a inner surface, 31 fine uneven structure, 32 spiral groove, 32a concave portion, 32b convex portion, 35 cooling liquid.
Claims
1. A cooling pipe through which a cooling liquid flows is provided, An injection molding die, wherein a fine uneven structure or a spiral groove is formed on at least a part of an inner surface of the cooling pipe.
2. The injection mold of claim 1 , wherein the at least a portion of the inner surface is the entire inner surface.
3. The injection mold of claim 1 , wherein the at least a portion of the inner surface is a portion of the inner surface.
4. Further provided with a cavity, The injection mold according to claim 3 , wherein the at least a portion of the inner surface is a portion of the inner surface facing the cavity.
5. The injection molding die according to claim 1 , wherein the fine uneven structure having a maximum height roughness of 100 μm or more is formed on at least the portion of the inner surface.
6. 2. The injection mold according to claim 1, wherein the spiral groove has a groove depth of 0.5 mm or more formed on at least the portion of the inner surface.
7. An injection molding apparatus comprising the injection mold according to any one of claims 1 to 6.
Citation Information
Patent Citations
Metal mold and injection molding method