Using Different Work Functions to Reduce Gate-Induced Drain Leakage Current in Stacked Nanosheet Transistors

By employing different work function metals with varying work functions in the end and central regions of nanosheet channels, the electric field across the gate oxide is relaxed, effectively reducing gate-induced drain leakage current and enhancing the performance of stacked nanosheet transistors.

JP2024535949AActive Publication Date: 2024-10-04INTERNATIONAL BUSINESS MACHINE CORPORATION

Patent Information

Application Number
JP2022563497
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-09-24
Filing Date
2022-07-04
Publication Date
2024-10-04
Estimated Expiration
2042-07-04

AI Technical Summary

Technical Problem

Gate-induced drain leakage (GIDL) current is a significant issue in stacked nanosheet transistors due to high electric fields across thin gate oxides, particularly in modern semiconductor devices, which can lead to increased leakage currents and reduced device performance.

Method used

The use of different work function metals (WFMs) with varying work functions in the end and central regions of the nanosheet channel, creating a work function gradient to relax the electric field across the gate oxide, thereby reducing GIDL current.

Benefits of technology

The work function gradient effectively reduces GIDL current by modulating the electric field, improving the performance and reliability of stacked nanosheet transistors.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024535949000001_ABST
    Figure 2024535949000001_ABST
Patent Text Reader

Abstract

A transistor device is provided. The transistor device includes a channel stack having stacked and spaced apart channel layers. A first source or drain (S / D) region is communicatively coupled to the channel stack. A tunnel extends through the channel stack, where the tunnel includes a central region and a first set of end regions. The first set of end regions are located closer to the first S / D region than the central region is to the first S / D region. A first type of work function metal (WFM) is formed in the first set of end regions, the first type of WFM having a first work function (WF). A second type of WFM is formed in the central region, the second type of WFM having a second WF, where the first WF is different from the second WF.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates generally to methods and resulting structures for fabricating semiconductor devices, and more specifically, to methods and resulting structures for using differential work functions to reduce gate-induced drain leakage (GIDL) current in stacked nanosheet transistors. [Background technology]

[0002] In modern semiconductor device fabrication processes, a large number of metal-oxide-semiconductor field effect transistors (MOSFETs), such as n-type field effect transistors (nFETs) and p-type field effect transistors (pFETs), are fabricated on a single wafer. Nonplanar MOSFET architectures (e.g., FinFETs and nanosheet FETs) can increase device density and improve performance over planar MOSFETs. For example, in contrast to conventional planar MOSFETs, nanosheet FETs contain a gate stack that surrounds the entire periphery of multiple stacked and spaced apart nanosheet channel regions for reduced device footprint and improved control of channel current flow.

[0003] GIDL currents are undesirable and can occur in MOSFETs due to high electric fields between the gate and drain. Large GIDL currents can be detected in thin-gate oxide MOSFETs at drain voltages much lower than the junction breakdown voltage. The mechanism responsible for GIDL current in MOSFETs is band-to-band tunneling, which can occur at the reverse-biased channel-drain interface as well as at the channel-drain interface located within the gate-to-drain overlap region. Summary of the Invention

[0004] An embodiment of the present invention is directed to a transistor device including a channel stack having stacked and spaced apart channel layers. A first source or drain (S / D) region is communicatively coupled to the channel stack. A tunnel extends through the channel stack, where the tunnel includes a central region and a first set of end regions. The first set of end regions are located closer to the first S / D region than the central region is to the first S / D region. A first type of work function metal (WFM) is formed in the first set of end regions, the first type of WFM having a first work function (WF). A second type of WFM is formed in the central region, the second type of WFM having a second WF, where the first WF is different from the second WF.

[0005] An embodiment of the present invention is directed to a method of forming a transistor device, comprising forming a channel stack having stacked and spaced apart channel layers. A first S / D region is formed and communicatively coupled to the channel stack. A tunnel is formed extending through the channel stack, the tunnel including a central region and a first set of end regions. The first set of end regions are located closer to the first S / D region than the central region is to the first S / D region. A first type of WFM is formed in the first set of end regions, the first type of WFM having a first WF. A second type of WFM is formed in the central region, the second type of WFM having a second WF, where the first WF is different from the second WF.

[0006] Further features and advantages are realized by the techniques described herein. Other embodiments and aspects are described in detail herein. For a more detailed understanding, reference should be made to the specification and drawings.

[0007] The subject matter which is regarded as embodiments is particularly pointed out and distinctly claimed in the claims at the end of this specification. The foregoing and other features and advantages of these embodiments will become apparent from the following detailed description taken in conjunction with the accompanying drawings.

[0008] 1-12 show multiple cross-sectional views of nanosheet-based structures after various fabrication steps to form stacked nanosheet transistors having work function differences to reduce GIDL current, according to an embodiment of the present invention. [Brief description of the drawings]

[0009] [Figure 1] FIG. 1 is a cross-sectional view of a nanosheet-based structure after initial fabrication steps according to an embodiment of the present invention. [Diagram 2] FIG. 2 is a cross-sectional view of a nanosheet-based structure after additional fabrication steps according to an embodiment of the present invention. [Diagram 3] FIG. 3 is a cross-sectional view of a nanosheet-based structure after additional fabrication steps according to an embodiment of the present invention. [Figure 4] FIG. 4 is a cross-sectional view of a nanosheet-based structure after additional fabrication steps according to an embodiment of the present invention. [Diagram 5] FIG. 5 is a cross-sectional view of a nanosheet-based structure after additional fabrication steps according to an embodiment of the present invention. [Figure 6] FIG. 6 is a cross-sectional view of a nanosheet-based structure after additional fabrication steps according to an embodiment of the present invention. [Figure 7] FIG. 7 is a cross-sectional view of a nanosheet-based structure after additional fabrication steps according to an embodiment of the present invention. [Figure 8] FIG. 8 is a cross-sectional view of a nanosheet-based structure after additional fabrication steps according to an embodiment of the present invention. [Figure 9] FIG. 9 is a cross-sectional view of a nanosheet-based structure after additional fabrication steps according to an embodiment of the present invention. [Figure 10]FIG. 10 is a cross-sectional view of a nanosheet-based structure after additional fabrication steps according to an embodiment of the present invention. [Figure 11] FIG. 11 is a cross-sectional view of a nanosheet-based structure after additional fabrication steps according to an embodiment of the present invention. [Figure 12] FIG. 12 is a cross-sectional view of a nanosheet-based structure after additional fabrication steps according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0010] For the sake of brevity, conventional techniques relating to semiconductor device and integrated circuit (IC) fabrication may or may not be described in detail herein. Additionally, various tasks and process steps described herein may be combined into more comprehensive procedures or processes having additional steps or functions not described in detail herein. In particular, the various steps in the manufacture of semiconductor devices and semiconductor-based ICs are well known, and thus, for the sake of brevity, many conventional steps are only briefly mentioned herein or are omitted entirely without providing details of the well-known processes.

[0011] Turning now to a description of the technology more specifically related to embodiments of the present invention, semiconductor devices (e.g., FETs) are formed using active regions of a wafer. The active regions are defined by insulating regions used to separate and electrically isolate adjacent semiconductor devices. For example, in an IC having multiple MOSFETs, each MOSFET has a source and a drain that are formed in the active region of the semiconductor layer by implanting n-type or p-type impurities into the layer of semiconductor material. Disposed between the source and drain is a channel (or body) region. Disposed above the body region is a gate electrode. The gate electrode and the body are spaced apart by a gate dielectric layer.

[0012] MOSFET-based ICs are fabricated using the so-called Complementary Metal-Oxide Semiconductor (CMOS) fabrication technology. In general, CMOS is a technology that uses a complementary, symmetric pair of p-type and n-type MOSFETs to implement logic functions. A channel region connects the source and drain, and current flows through the channel region from the source to the drain. This current flow is induced in the channel region by a voltage applied at the gate electrode.

[0013] The wafer footprint of a FET is related to the electrical conductivity of the channel material. If the channel material has a relatively high conductivity, the FET can be fabricated with a correspondingly smaller wafer footprint. A known method to increase the channel conductivity and reduce the FET size is to form the channel as a nanostructure. For example, the so-called gate-all-around (GAA) nanosheet FET is a known architecture to provide a relatively small FET footprint by forming the channel region as a series of thin nanosheets (e.g., about 3 nm to about 8 nm thick). In the known GAA configuration, a nanosheet-based FET includes a source region, a drain region, and a stacked nanosheet channel between the source and drain regions. A gate surrounds the stacked nanosheet channel and regulates the flow of electrons through the nanosheet channel between the source and drain regions.

[0014] GAA nanosheet FETs are fabricated by forming alternating layers of non-sacrificial and sacrificial nanosheets. The sacrificial nanosheets are removed from the non-sacrificial nanosheets before the FET device is finished. For n-type FETs, the non-sacrificial nanosheets are typically silicon (Si) and the sacrificial nanosheets are typically silicon germanium (SiGe). For p-type FETs, the non-sacrificial nanosheets can be SiGe and the sacrificial nanosheets can be Si. In some implementations, the non-sacrificial nanosheets of p-type FETs can be SiGe or Si and the sacrificial nanosheets can be Si or SiGe. Forming GAA nanosheets from alternating layers of non-sacrificial nanosheets formed from a first type of semiconductor material (e.g., Si for n-type FETs, SiGe for p-type FETs) and sacrificial nanosheets formed from a second type of semiconductor material (e.g., SiGe for n-type FETs, Si for p-type FETs) provides the excellent non-sacrificial electrostatic control required for continuous scaling of gate lengths to 7 nanometer CMOS technology and below. The use of multiple layered SiGe / Si sacrificial / non-sacrificial nanosheets (or Si / SiGe sacrificial / non-sacrificial nanosheets) to form the channel region in a GAA FET semiconductor device provides desirable device properties, such as introducing strain at the interface between SiGe and Si.

[0015] Although nanosheet channel FET architectures increase device density over planar FET architectures, challenges remain when trying to fabricate nanosheet channel FETs that provide the performance characteristics required for a particular application. For example, as the size of MOSFETs and other devices decreases, the dimensions of the S / D regions, channel regions, gate electrodes, and gate oxides also decrease. As MOSFET gate oxides become thinner and higher VDD (i.e., higher potential between gate and drain) is driven, the electric field across the gate oxide increases, which in turn increases the GIDL current.

[0016] Turning now to a summary of aspects of the invention, embodiments of the invention provide a stacked nanosheet transistor designed and configured to provide a gate structure formed from a first work function metal (WFM) and a second work function metal (WFM). The first WFM has a first work function (WF) and the second WFM has a second WF. The nanosheet transistor is fabricated in accordance with embodiments of the invention to have a unique structure that allows the first WFM to be located closer to a source or drain (S / D) region than the second WFM is to the S / D region. In accordance with aspects of the invention, the first WF is different from the second WF, which creates a WF gradient between a central region of the nanosheet channel and either S / D region. This WF gradient relaxes the electric field across the gate oxide, thereby reducing the GIDL current in the stacked nanosheet transistor.

[0017] In an embodiment of the invention, the space for the first and second WFMs is created by increasing the depth of the recess that accommodates the internal spacer of the stacked nanosheet transistor. The increased recess depth allows the nanosheet structure to accommodate a channel trimming process during fabrication that creates a cavity (or tunnel) defined by the trimmed portion of the channel nanosheet and a portion of the internal spacer. The cavity / tunnel includes end cavity / tunnel regions and a central cavity / tunnel region between the end cavity / tunnel regions. Each end region is located closer to one of the S / D regions than the central region. According to an embodiment of the invention, a first WFM is formed in each end cavity / tunnel region and a second WFM is formed in the central cavity / tunnel region, thereby creating a WFM difference between the central cavity / tunnel region and either of the end cavity / tunnel regions. This WF difference relaxes the electric field across the gate oxide, thereby reducing the GIDL current in the stacked nanosheet transistor.

[0018] In embodiments of the invention, the first and second WFMs are formed from a combination of materials that provide the stacked nanosheet transistor with an appropriate threshold voltage and simultaneously provide a WF difference between the center cavity / tunnel region and either of the edge cavity / tunnel regions, thereby relaxing the electric field across the gate oxide, which reduces the GIDL current of the stacked nanosheet transistor. In some embodiments of the invention, the WF is a property of the selected WFM, and the value of the WF of the selected WFM is modulated (increased or decreased) by layering an oxygen gettering material over the WFM and separated from the gate oxide. In general, a "gettering" or "getter" material is a reactive material that exhibits the property of "getting" or removing another material. For example, an oxygen getter material exhibits the property of bonding with nearby oxygen molecules, either chemically or by adsorption, thereby removing oxygen from either the environment or another material to which the oxygen getter material is communicatively bonded. Al is an example of an oxygen gettering material because Al is effective at gettering (i.e., reacting with and removing) oxygen that is present either in the environment or in another material to which it is communicatively coupled. By placing an oxygen gettering material, such as aluminum, on the WFM, the oxygen gettering material draws oxygen out of the gate oxide, thereby creating oxygen vacancies in the gate oxide, which reduces the EFW of the selected WFM.

[0019] In some embodiments of the present invention, the nanosheet transistor is an nFET, the first WFM is a tri-layer including an oxygen-gettering (or WF-modulating) layer, and the second WFM is also a tri-layer including an oxygen-gettering (or WF-modulating) layer. The first WFM tri-layer is on the gate oxide and is formed of a layer of TiN with a first thickness (T1), a layer of an Al-containing alloy (e.g., TiAlC), and a layer of TiN. The second WFM tri-layer is on the gate oxide and is formed of a layer of TiN with a second thickness (T2), a layer of an Al-containing alloy (e.g., TiAlC), and a layer of TiN. According to an aspect of the present invention, T1 is relatively thin and T2 is relatively thick, which means T1 < T2. By providing a tri-layer WFM configuration for both the first WFM and the second WFM and keeping T1 relatively thin and smaller than T2, the oxygen-gettering effect on the first WFM becomes higher than that on the second WFM. As a result, the threshold voltage near the S / D region becomes lower compared to the central region of the channel. This helps to reduce the GIDL current.

[0020] In some embodiments of the present invention, the nanosheet transistor is a pFET, the first WFM is a WFM without an oxygen-gettering layer, and the second WFM is a tri-layer including an oxygen-gettering layer. The first WFM layer is on the gate oxide and is formed of a layer of TiN. The second WFM tri-layer is on the gate oxide and is formed of a layer of TiN with a third thickness (T3), a layer of an Al-containing alloy (e.g., TiAlC), and a layer of TiN. According to an aspect of the present invention, T3 is relatively thick. In some embodiments of the present invention, T3 > T2 > T1. By providing a tri-layer WFM configuration only for the second WFM and keeping T3 relatively thicker than T2 and larger than T2, a lower threshold voltage can be obtained near the S / D region compared to the central region on the channel. At the same time, the threshold voltage of the central region remains acceptable for the pFET device.

[0021] Turning now to a more detailed description of the fabrication steps and resulting structures according to embodiments of the invention, Figures 1-12 illustrate a nanosheet-based structure 100 after various fabrication steps to form a nanosheet FET having a first WFM closest to the S / D that is distinct from a second WFM closest to the channel nanosheet. For ease of illustration, the fabrication steps illustrated in Figures 1-12 are described in the context of forming one nanosheet stack 130 (shown in Figure 1) that is etched into three nanosheet stacks 130 (shown in Figures 3-13). However, the fabrication steps described herein are intended to be equally applicable to the fabrication of any number of nanosheet stacks 130.

[0022] It is understood that while the cross-sectional views illustrated in Figures 1-12 are two-dimensional, the diagrams illustrated in Figures 1-12 represent three-dimensional structures. To aid in visualization of the three-dimensional features, a top-down reference diagram 101 shown in Figure 1 provides a reference point for the various cross-sectional views (X, Y1, and Y2 views) shown in Figures 1-12. The X view is a side view across the three gates, the Y1 view is an end view through the active gate, and the Y2 view is an end view through a portion of the nanosheet (NS) stack in which one of the S / D regions is (or will be) formed.

[0023] FIG 1 illustrates a cross-sectional view of a nanosheet-based structure 100 after an initial fabrication step according to an embodiment of the present invention. As shown in FIG 1, a nanosheet stack 130 is formed on a substrate 102. The nanosheet stack 130 includes an alternating series of SiGe sacrificial nanosheet layers 120, 122, 124, 126, 127 and Si nanosheet layers 114, 116, 118. According to an embodiment of the present invention, the alternating nanosheet layers 120, 122, 114, 124, 116, 126, 118, 127 of the nanosheet stack 130 are formed by epitaxially growing one nanosheet layer and then the next nanosheet layer until a desired number of nanosheet layers and a desired thickness are achieved. A hard mask layer (not shown) is deposited over the alternating nanosheet layers 120, 122, 114, 124, 116, 126, 118, 127, and the hard mask layer and the alternating nanosheet layers 120, 122, 114, 124, 116, 126, 118, 127 are etched to define a hard mask (HM) 128, the nanosheet stack 130, and the sub-fin 102A of the substrate 102. The hard mask layer and the resulting HM 128 can be any suitable dielectric, including, but not limited to, SiN.

[0024] In embodiments of the invention, each of the nanosheet layers 120, 122, 114, 124, 116, 126, 118, 127 can have a vertical thickness ranging from about 5 nm to about 20 nm, from about 10 nm to about 15 nm, or about 10 nm. Other vertical thicknesses are contemplated. Although eight alternating layers 120, 122, 114, 124, 116, 126, 118, 127 are shown, any number of alternating layers can be provided.

[0025] Epitaxial materials can be grown from gaseous or liquid precursors using, for example, vapor phase epitaxy (VPE), molecular beam epitaxy (MBE), liquid phase epitaxy (LPE), or other suitable processes. Epitaxial silicon, silicon germanium, or carbon-doped silicon (Si:C), or combinations thereof, can be doped during deposition (in-situ doped) by adding dopants, n-type dopants (e.g., phosphorus or arsenic) or p-type dopants (e.g., boron or gallium), depending on the type of transistor.

[0026] The terms "epitaxially grown and / or deposited" and "epitaxially formed and / or grown" refer to the growth of a semiconductor material (a crystalline material) on a deposition surface of another semiconductor material (a crystalline material) where the semiconductor material being grown (the crystalline overlayer) has substantially the same crystalline properties as the semiconductor material (the seed material) of the deposition surface. In an epitaxial deposition process, chemical reactants provided by source gases are controlled and system parameters are set so that the deposited atoms arrive at the deposition surface of the semiconductor substrate with sufficient energy to move around the surface so that the deposited atoms orient themselves in the crystalline arrangement of the atoms of the deposition surface. Thus, epitaxially grown semiconductor material has substantially the same crystalline properties as the deposition surface on which it is formed. For example, epitaxially grown semiconductor material deposited on a {100} oriented crystalline surface will adopt a {100} orientation. In some embodiments of the present invention, the epitaxial growth and / or deposition process is selective to forming on semiconductor surfaces and generally does not deposit material on non-crystalline surfaces such as silicon dioxide or silicon nitride.

[0027] In some embodiments of the present invention, the gas source for deposition of epitaxial semiconductor material may be a silicon-containing gas source, a germanium-containing gas source, or a combination thereof. For example, an epitaxial Si layer may be deposited from a silicon gas source selected from the group consisting of silane, disilane, trisilane, tetrasilane, hexachlorodisilane, tetrachlorosilane, dichlorosilane, trichlorosilane, methylsilane, dimethylsilane, ethylsilane, methyldisilane, dimethyldisilane, hexamethyldisilane, and combinations thereof. An epitaxial germanium layer may be deposited from a germanium gas source selected from the group consisting of germane, digermane, halogermane, dichlorogermane, trichlorogermane, tetrachlorogermane, and combinations thereof. Meanwhile, an epitaxial silicon-germanium alloy layer may be formed utilizing a combination of such gas sources. A carrier gas such as hydrogen, nitrogen, helium, or argon may be used.

[0028] In some embodiments of the present invention, the SiGe sacrificial nanosheet layers 122, 124, 126, 127 can be about 20% SiGe. The designation "20% SiGe" is used to indicate that 20% of the SiGe material is Ge and 80% of the SiGe material is Si. In some embodiments of the present invention, the Ge percentage in the SiGe sacrificial nanosheet layers 122, 124, 126, 127 can be any value, including, for example, values ​​within a range of about 20% to about 45%.

[0029] In an embodiment of the present invention, the SiGe sacrificial nanosheet layer 120 has a Ge percentage that is significantly greater than the Ge percentage in the SiGe sacrificial nanosheet layers 122, 124, 126, 127 to provide an etch selectivity between the sacrificial nanosheet layer 120 and the sacrificial nanosheet layers 122, 124, 126, 127. In some aspects of the present invention, the Ge percentage in the SiGe sacrificial nanosheet layer 120 is greater than about 55%. In some aspects of the present invention, the sacrificial nanosheet layers 122, 124, 126, 127 can be 25% SiGe and the sacrificial nanosheet layer 120 can be greater than about 55% SiGe.

[0030] 2, known fabrication processes have been used to deposit a thin layer of gate oxide (not shown separately) onto the nanosheet stack 130 prior to the formation of the dummy gate 204. In FIG. 2, the dummy gate 204 represents a combination of a thin layer of gate oxide (e.g., SiO2) and the material (e.g., amorphous silicon (a-Si)) from which the dummy gate 204 is formed.

[0031] With further reference to FIG. 2 , known fabrication processes (e.g., RIE) have been used to form the dummy gate 204. In embodiments of the invention, the dummy gate 204 may be formed by depositing and planarizing a layer of dummy gate material (not shown) on top of the gate oxide (not shown apart from the top nanosheet 127). In some embodiments of the invention, the dummy gate material may be polycrystalline Si. In some embodiments of the invention, the dummy gate material may be amorphous Si (a-Si). Once deposited, the dummy gate material is planarized (e.g., by CMP) to a desired level. Known semiconductor fabrication processes are used to form a patterned / etched hard mask 206 on top of the planarized dummy gate material. In embodiments of the invention, the hard mask 206 may be formed by depositing a layer of hard mask material, patterning the deposited hard mask layer, and then etching to form the hard mask 206. The pattern used to form the hard mask 206 defines the footprint of the dummy gate 204 and the gate oxide. In an embodiment of the present invention, the hard mask 206 may be formed from an oxide material or a nitride material, or both. The dummy gate material is selectively etched such that the portions of the dummy gate material not under the hard mask 206 are selectively removed, thereby forming the dummy gate 204 over the gate oxide and nanosheet stack 130.

[0032] Still referring to FIG. 2, known fabrication processes were used to selectively remove the portions of the gate oxide that were not under the dummy gate 204, and a DHF (diluted HF) clean was performed to ensure that all of the gate oxide not under the dummy gate 204 was removed.

[0033] 2, known fabrication processes were used to selectively remove the bottom-most SiGe sacrificial nanosheet layer 120 (shown in FIG. 1) and subsequently deposit a dielectric material used to form an offset gate spacer 208 on the sidewalls of the dummy gate 204. The deposited dielectric material also fills the space previously occupied by the removed sacrificial nanosheet layer 120, thereby forming a bottom insulating region 202, which will insulate the substrate 102 from the active region of the final nanosheet transistor 1200 (shown in FIG. 12). In embodiments of the invention, the offset gate spacer 208 can be formed by depositing a dielectric material on top of the nanosheet-based structure 100 and then directionally etching (e.g., using RIE) the dielectric material to form the gate spacer 208. In embodiments of the invention, the offset gate spacer 208 and the bottom insulating region 202 can be formed from any suitable dielectric material, including, for example, silicon oxide, silicon nitride, silicon oxynitride, SiBCN, SiOCN, SiOC, or any suitable combination of these materials. In some embodiments of the present invention, the offset gate spacer 208 and / or the bottom insulating region 202 may be a low-k dielectric material.

[0034] 2, as best seen in the Y2 view, shallow trench isolation (STI) regions 204 are formed adjacent to the sub-fin 102A. In an embodiment of the invention, the STI regions 204 may be formed as an oxide. An example process for forming the STI regions 204 includes depositing an STI dielectric material (e.g., an oxide) (not shown) adjacent to the sub-fin 102a, followed by CMP planarization and recessing the STI dielectric material to form the STI regions 204.

[0035] 3, the portions of the nanosheet stack 130 not covered by the gate spacer 208 and the dummy gate 204 are etched, thereby forming multiple instances of the nanosheet stack 130, forming alternating layers of SiGe sacrificial nanosheets 122, 124, 126, 127 and Si nanosheets 114, 116, 118 in each instance of the nanosheet stack 130, forming S / D trenches 302, 304, providing access to the end regions of the SiGe sacrificial nanosheets 122, 124, 126, 127, and providing access to the end regions of the Si nanosheets 114, 116, 118. The rightmost and leftmost nanosheet stacks 130 can be part of active or inactive transistors, respectively, depending on the requirements of the IC design into which the nanosheet-based structure 100 is incorporated. If the rightmost and / or leftmost nanosheet stacks 130 are part of an active transistor, then the active transistor formed from the rightmost and / or leftmost nanosheet stacks 130 will be in series with the transistor formed from the central nanosheet stack 130 and will share a source or drain region with the transistor formed from the central nanosheet stack 130. Whether or not the transistor formed from the rightmost and leftmost nanosheet stacks 130 are active, the rightmost and leftmost nanosheet stacks 130 define portions of the S / D trenches 302, 304 in which the S / D regions 602, 604 (shown in FIG. 6) are formed.

[0036] 4, known semiconductor fabrication processes have been used to partially remove end regions of the SiGe sacrificial nanosheets 122, 124, 126, 127 to form end regions or interior spacer cavities 402. In an embodiment of the invention, the end regions of the SiGe sacrificial nanosheets 122, 124, 126, 127 may be removed using a so-called "pull-back" process in which the SiGe sacrificial nanosheets 122, 124, 126, 127 are pulled back an initial pull-back distance such that the ends of the SiGe sacrificial nanosheets 122, 124, 126, 127 terminate well past the inner edges of the gate spacer 208 according to an aspect of the invention. The pull-back process takes advantage of the fact that the sacrificial nanosheets 122, 124, 126, 127 are formed from SiGe, which can be selectively etched relative to the Si nanosheets 114, 116, 118 using, for example, a gas-phase hydrogen chloride (HCL) gas isotropic etching process.

[0037] In FIG. 5, known semiconductor fabrication processes (e.g., ALD) were used to conformally deposit a layer of inner spacer liner material 502 on the nanosheet-based structure 100. The inner spacer liner layer 502 can be silicon nitride, silicon carbonitride boron, silicon carbonitride, silicon carbon oxynitride, or any other type of dielectric material (e.g., a dielectric material with a dielectric constant k less than about 5). Furthermore, known semiconductor device fabrication processes were used to form the inner spacer 502 by applying an isotropic etch back on the inner spacer layer 502 to remove excess dielectric material on the exposed vertical and horizontal surfaces of the nanosheet-based structure 100, thus leaving the portion of the inner spacer layer 502 sandwiched between the inner spacer cavity 402 (shown in FIG. 4), thereby forming the inner spacer 502.

[0038] In Figure 6, known fabrication processes are used to form doped S / D regions 602, 604 in S / D trenches 302, 304 (shown in Figure 5). In embodiments of the invention, an epitaxial growth process may be used to grow the doped S / D regions 602, 604 from the exposed ends of the Si nano-sheets 114, 116, 118. In embodiments of the invention, the doped S / D regions 602, 604 may be epitaxially grown from gaseous or liquid precursors using, for example, vapor phase epitaxy (VPE), molecular beam epitaxy (MBE), liquid phase epitaxy (LPE), or other suitable processes. In embodiments of the invention, the doped S / D regions 602, 604 may be doped during deposition (e.g., in-situ doped) by adding a dopant, such as an n-type dopant (e.g., phosphorus or arsenic) or a p-type dopant (e.g., Ga, B, BF, or Al), during the above-described methods of forming the doped S / D regions 602, 604.

[0039] As also shown in Figure 6, known semiconductor device fabrication processes were used to deposit an interlayer dielectric (ILD) 610 to fill the remaining open spaces of the nanosheet-based structure 100 and stabilize the nanosheet-based structure 100. The structure 100 was planarized to a predetermined level by removing the hard mask 206 and some portions of the gate spacer 208. In an embodiment of the invention, the deposited ILD region 610 can be formed from low-k dielectrics (e.g., k less than about 4) and / or ultra-low-k (ULK) dielectrics (e.g., k less than about 2.5).

[0040] In FIG. 7, known semiconductor fabrication processes were used to remove the sacrificial nanosheets 122, 124, 126, 127 and the dummy gate 204. The dummy gate 204 and gate dielectric (not shown) can be removed by any suitable known etching process, for example, RIE or a wet stripping process. Known semiconductor fabrication processes can be used to remove the SiGe sacrificial nanosheets 122, 124, 126, 127 selectively to the Si non-sacrificial nanosheets 114, 116, 118. In an embodiment of the present invention, since the sacrificial nanosheets 122, 124, 126, 127 are formed from SiGe, they can be etched selectively to the Si nanosheets 114, 116, 118, for example, using a gas phase hydrogen chloride (HCL) gas isotropic etching process.

[0041] In Figure 8, known fabrication processes (e.g., wet etching) were used to trim the Si nano-sheets 114, 116, 118 to a profile that forms a cavity / tunnel 802 defined by portions of the trimmed Si nano-sheets 114, 116, 118 and portions of the inner spacer 502, in accordance with an embodiment of the present invention. According to an aspect of the present invention, the amount of Si trimming is adjusted to have a proper overlap between the junction and the gate in the final structure 1200 (shown in Figure 12).

[0042] In Figure 9, known fabrication processes (e.g., ALD deposition) were used to deposit a high-k gate dielectric layer 902. According to an embodiment of the invention, the high-k gate dielectric layer 902 lines the cavity / tunnel 802 and can be a layer of HfO2.

[0043] 10, known metal deposition and recess processes can be used to deposit a first WFM 1002 at an edge region of the cavity 802, leaving a central region of the cavity 802 open. According to an embodiment of the invention, the first WFM 1002 is configured and arranged to provide a first WF. According to an embodiment of the invention, the edge region of the cavity 802 is located closer to the S / D regions 602, 604 than the central region of the cavity 802 is located relative to the S / D regions 602, 604, thereby placing the first WFM 1002 closer to the S / D regions 602, 604 than the central region of the cavity 802 is located relative to the S / D regions 602, 604.

[0044] 11, a known metal deposition process can be used to deposit a second WFM 1102 in a central region of the cavity 802. According to an embodiment of the invention, the second WFM 1102 is configured and arranged to provide a second WF. According to an embodiment of the invention, the central region of the cavity 802 is located further away from the S / D regions 602, 604 than the edge regions of the cavity 802 are located from the S / D regions 602, 604, thereby placing the second WFM 1102 further away from the S / D regions 602, 604 than the edge regions of the cavity 802 are located from the S / D regions 602, 604.

[0045] According to an aspect of the invention, the first WFM 1002 has a first WF and the second WFM 1102 has a second WF. The profile of the cavity / tunnel 802 according to an embodiment of the invention allows the cavity / tunnel 802 to be located closer to the S / D regions 602, 604 than the second WFM 1102 is located relative to the S / D regions 602, 604. According to an aspect of the invention, the first WF is different from the second WF, which creates a WF gradient between the center region of the cavity / tunnel 802 and the end regions of the cavity / tunnel 802. This WF gradient relaxes the electric field across the gate oxide 902, which reduces the GIDL current in the stacked nanosheet transistor 1200 (shown in FIG. 12).

[0046] In embodiments of the invention, the first WFM 1002 and the second WFM 1102 are formed from a combination of materials that provide the appropriate threshold voltage for the stacked nanosheet transistor 1200 (shown in FIG. 12) while simultaneously providing a WF difference between the center region of the cavity 802 and the edge region of the cavity 802, thereby relaxing the electric field across the gate oxide 902 and reducing the GIDL current in the stacked nanosheet transistor 1200. In some embodiments of the invention, the WF is a property of the selected WFM, and the value of the WF of the selected WFM is modulated (increased or decreased) by layering an oxygen gettering material over the WFM and separated from the gate oxide. In general, a "gettering" or "getter" material is a reactive material that exhibits the property of "getting" or removing another material. For example, an oxygen getter material exhibits the property of bonding with nearby oxygen molecules, either chemically or by adsorption, thereby removing oxygen from either the environment or another material to which the oxygen getter material is communicatively bonded. Al is an example of an oxygen gettering material because Al is effective at gettering (i.e., reacting with and removing) oxygen that is present either in the environment or in another material to which it is communicatively bonded. By disposing an oxygen gettering material, such as aluminum, on the WFM, the oxygen gettering material draws oxygen out of the gate oxide, creating oxygen vacancies in the gate oxide and reducing the EFW of the selected WFM.

[0047] In some embodiments of the present invention, the nanosheet transistor 1200 (shown in FIG. 12) is an nFET, the first WFM 1002 is a three-layer including an oxygen-gettering (or WF-modulating) layer, and the second WFM 1102 is also a three-layer including an oxygen-gettering (or WF-modulating) layer. The first WFM 1002 can be a three-layer formed from a layer of TiN with a first thickness (T1), a layer of an Al-containing alloy (e.g., TiAlC), and a layer of TiN. The second WFM 1102 can be a three-layer formed from a layer of TiN with a second thickness (T2), a layer of an Al-containing alloy (e.g., TiAlC), and a layer of TiN. According to an aspect of the present invention, T1 is relatively thin and T2 is relatively thick, which means T1 < T2. By giving both the first WFM 1002 and the second WFM 1102 a three-layer WFM configuration and maintaining T1 relatively thin and less than T2, the oxygen-gettering effect on the first WFM 1002 becomes higher than the oxygen-gettering effect on the second WFM 1102. As a result, the threshold voltage near the S / D regions 602, 604 becomes lower compared to the central region on the channels 114, 116, 118. This helps to reduce the GIDL current.

[0048] In some embodiments of the present invention, the nanosheet transistor 1200 is a pFET, the first WFM 1002 is a WFM without an oxygen-gettering layer, and the second WFM 1102 is a three-layer including an oxygen-gettering layer. The first WFM layer 1002 is formed from a layer of TiN. The second WFM 1102 is a three-layer formed from a layer of TiN with a third thickness (T3), a layer of an Al-containing alloy (e.g., TiAlC), and a layer of TiN. According to an aspect of the present invention, T3 is relatively thick. In some embodiments of the present invention, T3 > T2 > T1. By giving only the second WFM 1002 a three-layer WFM configuration and maintaining T3 relatively thick and greater than T2, it is possible to achieve a lower threshold voltage near the S / D regions 602, 604 compared to the central region on the channels 114, 116, 118, while the threshold voltage of the central region remains acceptable for the pFET device.

[0049] In FIG. 12, a completed nanosheet transistor 1200 is formed by depositing a metal gate (MG) 1202. The MG 1202 can be formed using any suitable known fabrication process. The MG 1202, the gate dielectric 902, the first WFM 1002, and the second WFM 1102 form a high-k MG (HKMG) stack structure with WF gradient, according to an embodiment of the present invention. The HKMG stack structure surrounds the trimmed non-sacrificial nanosheets 114, 116, 118, respectively, and regulates the flow of electrons through the non-sacrificial nanosheets 114, 116, 118. The metal gate 1202 structure can include a metal liner. The dielectric layer 902 can include an interfacial layer (IL) and a high-k dielectric layer. The high-k dielectric layer can be made of, for example, silicon oxide, silicon nitride, silicon oxynitride, boron nitride, high-k materials, or any combination of these materials. Examples of high-k materials include, but are not limited to, metal oxides such as hafnium oxide, hafnium silicon oxide, hafnium silicon oxynitride, lanthanum oxide, lanthanum aluminum oxide, zirconium oxide, zirconium silicon oxide, zirconium silicon oxynitride, tantalum oxide, titanium oxide, titanium barium strontium oxide, titanium barium oxide, titanium strontium oxide, yttrium oxide, aluminum oxide, tantalum lead scandium oxide, and zinc lead niobate. High-k materials can further include dopants such as lanthanum and aluminum.

[0050] The methods and resulting structures described herein can be used in the fabrication of IC chips. The resulting IC chips can be delivered by the fabricator in raw wafer form (i.e., as a single wafer having multiple unpackaged chips), as bare die, or in packaged form. In the latter case, the chips are mounted in a single-chip package (such as a plastic carrier with leads attached to a motherboard or other top carrier) or in a multi-chip package (such as a ceramic carrier with one or both surface or buried interconnects). In either case, the chips are integrated with other chips, discrete circuit elements, or other signal processing devices, or a combination thereof, as part of either (a) an intermediate product such as a motherboard, or (b) a final product. The final product can be any product that contains the IC chip, from toys and other low-end applications to advanced computer products with displays, keyboards or other input devices, and a central processor.

[0051] The following definitions and abbreviations are to be used for interpreting the claims and the specification. As used herein, the terms "comprises," "comprising," "includes," "including," "has," "having," "contains," or "containing," or any other variation thereof, are intended to include a non-exclusive inclusion. For example, a composition, mixture, process, method, article, or device that includes a list of elements is not necessarily limited to only those elements but can include other elements that are not expressly listed or that are inherent to such composition, mixture, process, method, article, or device.

[0052] The term "exemplary" is used herein to mean "serving as an example, instance, or illustration." Any embodiment or design described herein as "exemplary" is not necessarily to be construed as preferred or advantageous over other embodiments or designs. The terms "at least one" and "one or more" are understood to include any integer greater than or equal to one, i.e., 1, 2, 3, 4, etc. The term "plurality" is understood to include any integer greater than or equal to two, i.e., 2, 3, 4, 5, etc. The term "connected" can include indirect and direct "connections."

[0053] References herein to "one embodiment," "embodiment," "exemplary embodiment," and the like indicate that the embodiment being described may include a particular feature, structure, or characteristic, but all embodiments may or may not include the particular feature, structure, or characteristic. Moreover, such phrases do not necessarily refer to the same embodiment. Furthermore, when a particular feature, structure, or characteristic is described in connection with an embodiment, it is understood that it is within the knowledge of one of ordinary skill in the art to affect such feature, structure, or characteristic in connection with other embodiments, whether or not expressly described.

[0054] For purposes of the following description, the terms "top", "bottom", "right", "left", "vertical", "horizontal", "top", "bottom" and their derivatives shall refer to the described structures and methods as oriented in the drawing figures. The terms "overlying", "atop", "on top" or "positioned on" or "positioned atop" mean that a first element, such as a first structure, is on a second element, such as a second structure, where an intervening element, such as an interface structure, may be between the first and second elements. The term "direct contact" means that a first element, such as a first structure, and a second element, such as a second structure, are connected at the interface of the two elements without an intermediate conductive, insulating or semiconducting layer.

[0055] Spatially relative terms, such as "beneath," "below," "lower," "above," "upper," and the like, may be used herein to facilitate descriptions to describe the relationship of one element or feature to another element or feature as illustrated in the figures. It will be understood that the spatially relative terms are intended to encompass different orientations of the device during use or operation in addition to the orientation depicted in the figures. For example, if the device in the figures is turned over, elements described as "below" or "below" the other elements or features would then be oriented "above" the other elements or features. That is, the term "below" can encompass both an upward and downward orientation. The device can be otherwise oriented (rotated 90 degrees or to other orientations) and the spatially relative descriptors used herein will be interpreted accordingly.

[0056] The terms "about," "substantially," "approximately," and variations thereof are intended to include the degree of error associated with the measurement of a particular quantity based on the equipment available at the time of filing. For example, "about" can include a range of ±8% or 5%, or 2% of a given value.

[0057] For example, the phrase "selective," such as "a first element that is selective to a second element," means that the first element is etched and the second element can act as an etch stop.

[0058] The term "conformal" (e.g., a conformal layer) means that the thickness of a layer is substantially the same on all surfaces or that the thickness varies by less than 15% of the nominal thickness of the layer.

[0059] References herein to terms such as "vertical," "horizontal," and "lateral" are made by way of example, and not by way of limitation, to establish a frame of reference. Terms such as "horizontal" and "lateral" refer to directions in a plane parallel to a top surface of a semiconductor substrate, regardless of actual three-dimensional spatial orientation. Terms such as "vertical" and "normal" refer to directions orthogonal to "horizontal" and "lateral."

[0060] As noted earlier herein, for the sake of brevity, conventional techniques related to semiconductor device and IC fabrication may or may not be described in detail herein. However, by way of background, a more general description of semiconductor device fabrication processes that may be utilized in practicing one or more embodiments of the present invention is now provided. While the specific fabrication steps used in practicing one or more embodiments of the present invention may be individually known, the described combination of inventive steps and / or resulting structures is unique. That is, the unique combination of steps described in connection with the fabrication of semiconductor devices in accordance with the present invention utilizes a variety of individually known physical and chemical processes performed on a semiconductor (e.g., silicon) substrate, some of which are described in the immediately following paragraphs.

[0061] In general, the various processes used to form microchips that are packaged into ICs fall into four general categories: film deposition, removal / etching, semiconductor doping, and patterning / lithography. Deposition is any process that grows, coats, or otherwise transfers material onto a wafer. Available techniques include physical vapor deposition (PVD), chemical vapor deposition (CVD), electrochemical deposition (ECD), molecular beam epitaxy (MBE), and more recently atomic layer deposition (ALD). Removal / etching is any process that removes material from a wafer. Examples include etching processes (either wet or dry), chemical mechanical planarization (CMP), and others. Reactive ion etching (RIE) is a type of dry etching that removes material, such as a masked pattern of semiconductor material, by exposing the material to a bombardment of ions that use a chemically reactive plasma to displace portions of the material from the exposed surface. The plasma is usually generated under low pressure (vacuum) by an electromagnetic field. Semiconductor doping is the modification of electrical properties, typically by doping transistor sources and drains, by diffusion or ion implantation, or both. These doping processes are followed by furnace annealing or rapid thermal annealing (RTA). The annealing serves to activate the implanted dopants. Films of both conductors (e.g., polysilicon, aluminum, copper, etc.) and insulators (e.g., various forms of silicon dioxide, silicon nitride, etc.) are used to connect and insulate transistors and their components. Selective doping of various regions of a semiconductor substrate allows the conductivity of the substrate to be changed by the application of a voltage. Creating structures of these various components allows millions of transistors to be constructed and wired together to form the complex circuits of modern microelectronic devices. Semiconductor lithography is the formation of three-dimensional relief images or patterns on a semiconductor substrate for subsequent transfer of the pattern to the substrate. In semiconductor lithography, the patterns are formed by light-sensitive polymers called photoresists.To build the intricate structures that make up the transistors and the numerous wires that connect the circuit's millions of transistors, lithography and etching pattern transfer steps are repeated multiple times. Each pattern printed on the wafer is aligned with the previous one, and slowly, conductors, insulators and selectively doped regions are built up to form the final device.

[0062] The flow charts and diagrams in the figures illustrate possible implementations of methods of making and / or operating according to various embodiments of the present invention. Various functions / operations of the methods are represented in blocks in the flow diagrams. In some alternative implementations, the functions noted in the blocks may occur out of the order noted in the figures. For example, two blocks shown in succession may in fact be executed substantially simultaneously or the blocks may be executed in the reverse order, depending on the functionality involved.

[0063] The description of various embodiments of the present invention has been presented for illustrative purposes, but is not intended to be exhaustive or limited to the described embodiments. Many modifications and variations will be apparent to those skilled in the art without departing from the scope of the described embodiments. The terms used in this specification have been selected to most clearly explain the principles of the embodiments, practical applications or technical improvements to the technology found in the market, or to enable those skilled in the art to understand the embodiments described herein.

Claims

1. 1. An integrated circuit (IC) having a transistor device including a first transistor type, the first transistor type comprising: a channel stack including stacked and spaced apart channel layers; a first source or drain (S / D) region communicatively coupled to the channel stack; a tunnel extending through the channel stack, the tunnel includes a central region and a first set of end regions; the tunnel, the first set of end regions being located closer to the first S / D region than the central region is to the first S / D region; a first type of work function metal (WFM) formed in the first set of end regions, the first type of WFM having a first work function (WF); and a second type of WFM formed in the central region, the second type of WFM having a second WF; Including, the first WF is different from the second WF; Integrated circuit (IC).

2. The IC of claim 1 further comprising a second S / D region communicatively coupled to the channel stack.

3. The IC of claim 2 , wherein the tunnel further comprises a second set of end regions.

4. 4. The IC of claim 3, wherein the second set of end regions are located closer to the second S / D region than the central region is to the second S / D region.

5. The IC of claim 4 , wherein the first type of WFM is formed in the second set of edge regions.

6. The IC of claim 1 further comprising an internal spacer.

7. The IC of claim 6 , wherein a boundary of the tunnel includes a pair of the inner spacers and a first of the stacked spaced apart channel layers.

8. The IC of claim 7 , wherein the boundary of the tunnel further comprises a second one of the stacked spaced apart channel layers.

9. further comprising a gate dielectric within the tunnel; The first type of WFM comprises: a first layer of metal having a first thickness; an aluminum alloy layer; a second layer of metal; The second type of WFM comprises: a third layer of metal of a second thickness; and an aluminum alloy layer; and a fourth layer of metal; The first thickness is less than the second thickness. The IC of claim 1.

10. The transistor device includes a second transistor type, the second transistor type comprising: a channel stack of a second transistor type including stacked and spaced apart channel layers; a second transistor type S / D region communicatively coupled to the second transistor type channel stack; a tunnel of a second transistor type extending through the channel stack of the second transistor type; a gate dielectric of a second transistor type within a tunnel of the second transistor type, the tunnel of the second transistor type includes a central region of the second transistor type and a set of end regions of the second transistor type; a gate dielectric for the second transistor type, the end regions of the second set of transistor types being located closer to the S / D regions of the second transistor type than a central region of the second transistor type is located relative to the S / D regions of the second transistor type; a work function metal (WFM) of a first type of a second transistor type formed in an end region of the set of second transistor types, the first type WFM having a first work function (WF); and a second transistor-type WFM of a second type formed in the central region, the second type WFM having a second WF; a second transistor type WFM of the first type including a first layer of metal; a second transistor type WFM of the second type, a second layer of metal having a predetermined thickness; an aluminum alloy layer; a third layer of metal; Including, The predetermined thickness is greater than the second thickness. The IC of claim 9.

11. 1. A method of forming an integrated circuit (IC) having transistor devices including a first transistor type, the method comprising forming the first transistor type by performing a fabrication process, the fabrication process comprising: forming a channel stack including stacked and spaced apart channel layers; forming a first source or drain (S / D) region communicatively coupled to the channel stack; forming a tunnel extending through the channel stack, the tunnel includes a central region and a first set of end regions; the first set of end regions being located closer to the first S / D region than the central region is to the first S / D region; forming a first type of work function metal (WFM) on the first set of end regions, the first type of WFM having a first work function (WF); and forming a second type of WFM in the central region, the second type of WFM having a second WF; the first WF is different from the second WF; method.

12. The method of claim 11 , further comprising forming a second S / D region communicatively coupled to the channel stack.

13. The method of claim 12 , wherein the tunnel further comprises a second set of end regions.

14. 14. The method of claim 13, wherein the second set of end regions are located closer to the second S / D region than the central region is to the second S / D region.

15. The method of claim 14 , wherein the first type of WFM is formed in the second set of end regions.

16. forming the tunnel forming a set of interior spacers extending beneath a gate structure of the transistor device; and The method of claim 11 including trimming a first one of the stacked spaced apart channel layers.

17. The method of claim 16 , wherein a boundary of the tunnel includes the set of the inner spacers and the first of the stacked, spaced apart channel layers.

18. the method further comprising trimming a second one of the stacked spaced apart channel layers; The method of claim 17 , wherein the boundary of the tunnel further comprises the second of the stacked spaced apart channel layers.

19. forming a gate dielectric in the tunnel; The first type of WFM comprises: a first layer of metal having a first thickness; an aluminum alloy layer; a second layer of metal; The second type of WFM comprises: a third layer of metal having a second thickness; and an aluminum alloy layer; and a fourth layer of metal; the first thickness is less than the second thickness; The method of claim 11.

20. the transistor device comprises a second transistor type, and the fabrication process comprises: forming a channel stack of a second transistor type including stacked and spaced apart channel layers; forming an S / D region of a second transistor type communicatively coupled to the channel stack of the second transistor type; forming a tunnel of a second transistor type extending through the channel stack of the second transistor type; forming a gate dielectric of a second transistor type within the tunnel of the second transistor type, the tunnel of the second transistor type includes a central region of the second transistor type and a set of end regions of the second transistor type; forming an end region of the second set of transistor types that is located closer to the S / D regions of the second transistor type than a central region of the second transistor type is located relative to the S / D regions of the second transistor type; forming a WFM of a second transistor type of a first type formed in an end region of the set of second transistor types, the WFM of the first type having a first work function (WF); and forming a second transistor type WFM of a second type formed in the central region, the second type WFM having a second WF; a second transistor type WFM of the first type including a first layer of metal; a second transistor type WFM of the second type, a second layer of metal having a predetermined thickness; An aluminum alloy layer, and a third layer of metal; The predetermined thickness is greater than the second thickness.

20. The method of claim 19.

Citation Information

Patent Citations

  • Reduction of drain leakage in nanosheet device

    US20210217846A1

Cited By

  • Semiconductor device and semiconductor device production method

    WO2026224962A1