Method for producing a soldered joint and assembly having a soldered joint - Patents.com

The use of magnetic nanoparticles in soldering methods allows for precise, localized heat input and automatic temperature control, addressing thermal damage issues in conventional soldering techniques by ensuring reliable solder joint formation without excessive heating.

JP2024537145AActive Publication Date: 2024-10-10SIEMENS AG
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2024520734
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-10-11
Filing Date
2022-10-04
Publication Date
2024-10-10
Estimated Expiration
2042-10-04

AI Technical Summary

Technical Problem

Existing soldering methods often cause thermal damage to soldering partners and adjacent components due to uncontrolled and widespread heat input, making it difficult to accurately measure and control the temperature at the soldering site.

Method used

A soldering method using magnetic nanoparticles embedded in the solder, which heats up under an alternating magnetic field, allowing precise localized heat input and automatic temperature control through the Curie temperature of the nanoparticles.

Benefits of technology

This method enables localized and controlled heat input, reducing thermal stress on soldering partners and adjacent components while ensuring reliable solder joint formation without excessive heating.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024537145000001_ABST
    Figure 2024537145000001_ABST
Patent Text Reader

Abstract

A method is proposed for producing a soldered joint between a first soldering partner (10) and a second soldering partner (20) by means of a solder (100), the solder comprising a metallic solder material (110) and a multitude of magnetic nanoparticles (120) and comprising at least: a) generating an alternating magnetic field (200) using at least one magnet coil (210, 220) and applying the alternating magnetic field (200) to the solder (100); b) heating the plurality of magnetic nanoparticles (120) by interaction with an alternating magnetic field (200); c) melting the metallic solder material (110) by heat transfer (300) from the plurality of magnetic nanoparticles (120) to the metallic solder material (110) and forming a soldered joint between the first soldering partner and the second soldering partner by the molten metallic solder material (110); Furthermore, an assembly (1) having such a soldered joint is proposed.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The invention relates to a method for producing a soldered joint between a first soldering partner and a second soldering partner by means of a solder, the solder comprising a metallic solder material which is melted during the implementation of the method. The invention further relates to an assembly comprising the soldered joint thus produced.

[0002] The prior art discloses various soldering methods with which a soldered joint can be produced between several soldering partners. As joining material, for example, a solid solder material can be used, for example a solder wire or a preform. It is also possible to use a solder paste, which can be applied, for example, by a printing method, to the circuit board on which the components are mounted. Such solder pastes usually contain a large number of metallic solder particles and furthermore a flux. Irrespective of the respective type of solder, the metallic material present therein must be melted or at least heated to such an extent that diffusion at the interface is possible in order to produce the desired soldered joint. The heat input required for this can be achieved according to the prior art, for example, by a soldering iron, a flame of a soldering torch, hot air, hot steam, thermal radiation, a laser or via electromagnetic induction by an induction coil.

[0003] A drawback of many of these heating methods is that the heat is not limited to the soldering site of the soldering partner, but is introduced over a larger area, with the result that there is a risk of thermal damage to the soldering partner. This applies in particular to soldering irons, soldering torches, hot air, hot steam and thermal radiation. Lasers can achieve localized, focused heating in some circumstances, but often not all areas to be soldered (e.g. in an electrical assembly) are fully accessible to the laser beam. Even in the case of induction soldering, there is often a risk of thermal damage to other conductive elements in the vicinity of the soldering site, where undesirable eddy currents are induced.

[0004] A further drawback of the heating methods mentioned above is that it is difficult to accurately measure and control the temperature reached in the area of ​​the soldering site, and therefore it is not possible to prevent an excessively high heat input when the temperature required for the creation of the soldered joint is reached. Thus, usually significantly more heat is introduced than is required for the soldering process, resulting in even greater thermal stresses on the soldering partner or even on adjacent components. Summary of the Invention [Problem to be solved by the invention]

[0005] The object of the present invention is therefore to provide an alternative method of producing a soldered joint which overcomes the abovementioned drawbacks. In particular, it is intended to provide a soldering method which allows a spatially narrowly limited heat input in the area of ​​the soldering site and which also advantageously allows a better controllable limitation of the reached soldering temperature. Another object is to provide an assembly which includes such a soldered joint. [Means for solving the problem]

[0006] These problems are solved by a method according to claim 1 and by an assembly according to claim 13.

[0007] The method according to the invention is for producing a soldered joint between a first soldering partner and a second soldering partner by means of a solder, the solder comprising a metallic solder material and a multiplicity of magnetic nanoparticles. The method comprises the following method steps: a) generating an alternating magnetic field by at least one magnet coil and applying the alternating magnetic field to the solder; b) heating the magnetic nanoparticles by interaction with said alternating magnetic field; c) melting the metallic solder material by heat transfer from the plurality of magnetic nanoparticles to the solder particles, and forming a soldered joint between the first soldering partner and the second soldering partner with the molten metallic solder material.

[0008] This sequence of the three method steps a) to c) shows first of all the causal relationship of the individual effects: the generation of an alternating magnetic field in step a) first causes heating of the magnetic nanoparticles in step b), which then leads to melting of the solder material in step c) as heat is transferred from the magnetic nanoparticles to the soldering material. Overall, steps a) and b) typically proceed simultaneously, and step c) is also carried out approximately simultaneously with steps a) and b), or at least with a temporal overlap.

[0009] That is, what is important for the present invention is that the solder contains both the above-mentioned magnetic nanoparticles and a metallic solder material. The melting of the metallic solder material results in the actual formation of the solder joint, as in the case of conventional solder pastes. In this case, the final, mechanically durable solder joint is formed at the moment when the heat input is stopped or limited and the solder material solidifies again to a solid state. The electrical conductivity of the formed solder joint is therefore essentially provided by the solidified metallic solder material.

[0010] These additionally present magnetic nanoparticles serve to allow a precise localized heat input to the solder. These nanoparticles are in particular ferromagnetic or ferrimagnetic. They can therefore be periodically magnetized by the alternating magnetic field acting in step a). The size scale of these particles must be in the nanometer range or below. Due to such small particle size, the magnetization caused by this magnetic field is not retained and is converted into thermal energy by Brownian and Neel relaxation on a very short time scale. Thus, via the alternating magnetic field acting in step a), a locally limited heating can be caused in the zone where these magnetic nanoparticles are present, in other words locally in the area of ​​the solder. Thus, an essential advantage of the method of the invention is that the undesired heating of the soldering partners to be joined and other adjacent components can be significantly reduced compared to other soldering methods, while nevertheless a reliable melting of the metal solder elements in the soldering zone is achieved.

[0011] Within the solder, the solder material can be present in particular in the form of metal solder particles. In this case, the magnetic nanoparticles can be mixed with the metal solder particles or be very close to them, so that heat transfer from the initially heated magnetic nanoparticles to the metal solder particles is possible as a whole, on the basis of which the solder particles can melt. This is the case, for example, of a mixture in which the two types of particles are present next to each other, in particular in which the magnetic nanoparticles, which are generally smaller in nature, are distributed more or less uniformly over the gaps between the larger solder particles. As an alternative to such a particle mixture, it is also possible for the solder to comprise a number of metal solder particles, each of which comprises a magnetic nanoparticle as a compartmented inclusion, composed of a heterogeneous material. In another alternative, the magnetic nanoparticles can be embedded in a larger expanded body made of solid solder material, for example distributed over the volume of a so-called preform or solder wire.

[0012] The assembly according to the invention comprises a first soldering partner and a second soldering partner. These two soldering partners are joined by a soldering joint comprising a metal solder element and a number of magnetic nanoparticles embedded therein. This soldering joint is produced in particular by the method according to the invention, which is detectable by the presence of the embedded magnetic nanoparticles. Unlike metal solder materials, these magnetic nanoparticles do not melt during the production of the soldering joint, but are still retained as nanoscale inclusions in the solidified solder. The advantages of the assembly according to the invention are similar to the above-mentioned advantages of the method according to the invention.

[0013] Advantageous embodiments and developments of the invention are evident from the dependent claims 1 and 13 and from the following description, whereby the described aspects of the method and the assembly can generally be advantageously combined with one another.

[0014] According to a generally advantageous embodiment, these magnetic nanoparticles can be superparamagnetic. In other words, these nanoparticles comprise ferromagnetic or ferrimagnetic material, in which case the remaining magnetization is not retained even below the Curie temperature after the previously acting external magnetic field is switched off. This effect occurs due to the small particle size, in which case the particle size that must not be exceeded for this purpose also depends on the respective material. In this regard, however, it is generally advantageous for the magnetic nanoparticles to have a diameter of 100 nm or less. In the case of non-spherical particles, the largest outer dimension is used instead of the diameter. A generally advantageous range for typical particle sizes is, for example, 10 nm to 50 nm, particularly advantageously 10 nm to 25 nm. In the case of magnetic nanoparticles of the abovementioned size scale, the energy from the acting alternating magnetic field can be converted particularly efficiently into heating of the nanoparticles by Brownian and Néel relaxation.

[0015] Furthermore, it is generally advantageous if the Curie temperature of these magnetic nanoparticles is in the range of 100 ° C. to 1200 ° C., particularly advantageously in the range of 150 ° C. to 400 ° C. In particular, all magnetic nanoparticles present must have a Curie temperature in the above-mentioned range. Their Curie temperature is thereby adapted to the temperature range of the soldering process used. In this case, in particular, the Curie temperature of the magnetic nanoparticles is higher than the melting temperature or melting range of the metal solder material. In this way, these magnetic nanoparticles can be heated to a sufficiently high temperature in an active alternating magnetic field, so that the solder material can be brought to melting. However, if the temperature of the magnetic nanoparticles exceeds the Curie temperature, further heating of the solder material is stopped, since above this temperature essentially no heat input from the energy of the magnetic field into the magnetic nanoparticles takes place. In this way, the heat input in the Curie temperature range of the nanoparticles is automatically stopped, which advantageously makes it possible to avoid excessive heat loads. That is to say, in particular in the case of this method, not only is the heat input concentrated locally in the area of ​​the solder, but also, by appropriate selection of the nanoparticle material, it is also possible to limit its maximum temperature to a range that is desired for a particular application. Since the Curie temperature of the nanoparticles is sensitive to the exact composition of the ferromagnetic or ferrimagnetic material involved, the material selection also allows the precise selection of the temperature at which the automatic stop mechanism occurs. In this way, the maximum achievable temperature of the solder can be appropriately matched not only to the melting temperature of the metallic solder material, but also to the thermal endurance of the soldering partners and possibly other elements present in the assembly. It is therefore advantageously possible for the assembly to include heat-sensitive elements, for example a housing and / or insulating layers of heat-sensitive polymers. The locally limited heating and its automatic limitation make it possible to avoid damage in the soldering process, while nevertheless ensuring the melting of the metallic solder material. In this case, it is also possible for the alternating magnetic field required for heating to penetrate other elements that are themselves hardly heated in the soldering process, since these elements have a small interaction with the magnetic field.Thus, for example, soldering through several components, in particular entire systems, is possible, and even soldering processes in or through liquids are possible.

[0016] A relatively consistent distribution of the Curie temperatures of the individual magnetic nanoparticles is particularly advantageous in connection with the above-mentioned stopping mechanism. These are preferably CNPs (Curie temperature tuned magnetic nanoparticles), i.e. magnetic nanoparticles with mutually consistent Curie temperatures. Such CNPs are described, for example, in Applied Materials Today 21 (2020) 100824 “Magnetocuring of temperature failsafe epoxy adhesives” R. Chaudhary, V. Chaudhary, RV Ramanujan, TWJ Steele.

[0017] It is therefore generally advantageous if the full width at half maximum (FWHM) of the distribution of the Curie temperatures of the individual magnetic nanoparticles is less than or equal to 50° C., particularly advantageously less than or equal to 30° C. Such a close match of the Curie temperatures of the individual nanoparticles provides for the above-mentioned automatic limitation of the heat input in a particularly precisely defined temperature range. The method can then accordingly comprise the following further steps: d) Allowing these magnetic nanoparticles to reach their Curie temperature, so that further heating of the solder is avoided.

[0018] In other words, when the nanoparticles reach their Curie temperature, the heat input is abruptly cut off. It is thus possible to particularly reliably avoid exceeding a predetermined maximum temperature and, as a consequence, to avoid thermal damage to adjacent elements. In particular, in this case, it is also possible to dispense with complex sensor systems for temperature detection and additional closed-loop control devices for avoiding overheating.

[0019] In a generally advantageous embodiment, these magnetic nanoparticles comprise a ferromagnetic or ferrimagnetic material, in particular present in the form of a metal alloy or metal oxide, which preferably comprises at least one of the elements iron, cobalt and nickel. Here, the metal oxide is in particular a mixed oxide, for example Mn x Zinc 1-x The compound may be of the type Fe2O4, where x may in particular take a value between 0.4 and 0.7. The tuning of the precisely defined Curie temperature for compounds of this type is described in the above cited article by R. Chaudhary et al.

[0020] Furthermore, it is generally advantageous if the weight percentage of such metal alloys or metal oxides in the overall solder is between 1% and 30%. A weight percentage of at least 1% is adequate to provide sufficient heat input to the solder through the nanoparticles, which in turn leads to melting of the metal solder material. On the other hand, an excessively high weight percentage of more than 30% is generally inappropriate, since the mechanical and electrical properties of the soldered joint are too strongly impaired. This weight percentage should therefore be advantageously limited to 10% or less, taking into account the particularly good electrical conductivity of the soldered joint. However, if it is particularly important to obtain a long-lasting mechanical bond and the importance of electrical conductivity is subordinated, the weight percentage of the magnetic nanoparticles can be in the upper part of this range, i.e. between 10% and 30%.

[0021] In a particularly advantageous variant, these magnetic nanoparticles can have a core made of a ferromagnetic or ferrimagnetic material and a non-magnetic shell. Here, non-magnetic material means a material that is at least not ferromagnetic or ferrimagnetic. This shell can therefore also be formed, for example, of an organic material and can contain, for example, oleic acid and / or bisphenol A diglycidyl ether. However, inorganic substances such as silicon dioxide (SiO2) or graphene can also be used for this shell. Such shells serve in particular for the colloidal stabilization of the magnetic nanoparticles. In other words, these shells avoid the aggregation of the particles, which can be caused, for example, by the influence of moisture. For this purpose, the thickness of such a colloidal stabilizing shell can be, for example, in the range of 2 nm to 10 nm. Such a thin shell is sufficient to prevent the nanoparticles from agglomerating to form larger clusters and thus to allow a fine and almost uniform distribution of the nanoparticles throughout the solder. In this way, a particularly uniform heating of the entire solder can be achieved.

[0022] However, as an alternative to this embodiment, it is in principle also possible to use uncoated magnetic nanoparticles. In some cases, the formation of clusters of such nanoparticles can be accepted. In particular when using a particle mixture of magnetic nanoparticles and metallic solder particles, it can be advantageous if the size scale of the formed agglomerates is in the range of the size scale of the solder particles used or less. Then, despite the agglomeration of these nanoparticles, a homogeneous solder can be provided that is sufficient to allow uniform heat transfer from the magnetic nanoparticles to the metallic solder particles.

[0023] According to a first embodiment of the solder, the solder can be a solder paste. Such a solder paste can in particular comprise a mixture of a plurality of magnetic nanoparticles and a plurality of metal solder particles. Such solder particles are preferably approximately spherical and have a diameter in the range of 1 μm to 160 μm, preferably 2 μm to 50 μm. This corresponds to the usual particle size in typical conventional solder pastes having relatively fine solder particles.

[0024] However, according to a second alternative embodiment of the solder, the solder can also be a solid solder preform, also called a preform in the industry. Such a solder preform can be, for example, a soldering ring or can take the form of a disk, a tape, a flat rectangle or a horseshoe. Alternatively, a soldering wire or another solid soldering element can be used.

[0025] Whether it is a solder paste containing solder particles or a soldering preform, the solder material is generally a low-melting alloy, for example a soft solder, a hard solder or a high-temperature solder. Basically all customary solder alloys are suitable as solder materials, in particular alloys containing tin, bismuth, silver, copper, zinc, lead and / or antimony.

[0026] In addition to the solder material and the magnetic nanoparticles, the solder preferably generally comprises a flux. This is also true whether it is, for example, a solder paste or a solid soldering preform. All conventional materials are useful for the flux. For example, the flux can be a resin, an oil, a solvent, a salt or water, or can include these compounds as constituents. Overall, the solder is a mixture of materials, which in addition to the solder material, the magnetic nanoparticles and the optional flux, can also include other optional components as required.

[0027] According to a generally advantageous variant of the embodiment of the method, at least two magnet coils with different pole arrangement directions can be used in step a). In this embodiment, two alternating magnetic fields superimposed on each other are thereby generated, preferably with multiple areas of high magnetic flux density superimposed in a focal range. Thus, in this variant, a focal spot acts on a narrowly limited area for local heating, which is stronger than the focal spot that can be created by only one magnet coil or by only one pole direction. The size of this focal spot is quite different depending on the application: for example, the focal spot size in the case of soldering surface mounted devices or ball grid arrays can be in the sub-millimeter range. For large-area soldering areas, such as for example in the railway technology field or for soldering pipes, the focal spot size can be significantly larger and even in the meter range.

[0028] Instead of generating one narrow focal range by two overlapping magnetic fields, the focusing of the magnetic field can be achieved by one or more magnetic flux guide elements. In order to focus the magnetic field into one focal range of suitable size, it is possible to arrange, for example, two cone-shaped iron cores facing each other on either side of the soldering site.

[0029] In general, regardless of the number and spatial arrangement of the magnet coils used, the frequency of the alternating magnetic field can be in the range of several hundreds of kHz, preferably between 100 kHz and 1000 kHz, and for example in the range of about 400 kHz. For frequencies in this range, efficient heat input into the solder can be achieved due to the corresponding relaxation processes in the magnetic nanoparticles.

[0030] According to an advantageous development of the invention, independent of the number of magnet coils and the number of poles, the at least one magnet coil can be moved relative to the two soldering partners during the soldering process. In this case, it is irrelevant whether the soldering partners are fixed and the at least one magnet coil is moved or vice versa. In any case, the overall result in this embodiment is a translational relative movement, so that the focal range or the range of maximum energy input moves across the assembly in question, so that a targeted local melting of the solder at several successive positions is possible. This alternative embodiment of the method also advantageously allows a progression in which the respective active soldering zone is moved from the inner region of the assembly to the outside (and of course vice versa). This alternative therefore also makes it possible to create individual local soldering sites in complex assemblies, especially if the positions of maximum energy input are narrowly defined in space, and also allows a later repair of such internal, locally defined soldering sites, if necessary. Repairs include, for example, replacement of parts and melting and repositioning misplaced parts that have already been soldered. Alternatively or additionally, a later locally limited heat treatment is possible to relieve stresses in the soldered joints already made by the above-mentioned heat input regime.

[0031] According to a generally advantageous development of the method, different solders with different melting temperatures can be used in one assembly to produce different types of soldered joints. The soldering method of the invention is then used for at least one type of these soldered joints. For other types of soldered joints, it is also possible to use the method of the invention together with other solders, or for one or more other soldered joints, it is also possible to use a conventional soldering method. For example, for SMD soldered joints, it is possible to use a different method than for the soldering of plugs or load connections. It is also possible to use a different soldering method for the soldering of joints for high frequencies, high currents and / or high voltages than for the low frequency, low current or low voltage range. Finally, it is also possible to use a different method for certain materials, such as for example solders containing lead, than for lead-free solders elsewhere in the assembly.

[0032] According to an advantageous embodiment, the assembly according to the invention can be an electronics assembly, in particular a power electronics assembly with one or more power electronic components, in which case the advantages of the invention are particularly effective, since here it is very important to produce reliable and highly conductive soldered joints, but on the other hand there is also the need to protect other elements in the same assembly from excessive thermal stresses.

[0033] It is generally advantageous if the assembly comprises at least one solder joint produced by the method of the invention, which is capable of forming a suitable electrically conductive joint between the associated soldering partners.

[0034] According to an advantageous embodiment of the assembly, the first soldering partner can be an electrical circuit board, i.e. it can be, for example, a circuit board or a ceramic circuit board. In either case, this circuit board forms the mechanical and / or electrical basis of the assembly, by which the other elements are supported. Thus, according to the method of the invention, one or more other elements forming the second and any other soldering partners can be soldered onto this circuit board.

[0035] The second soldering partner can therefore be an electric or electronic component. This also applies to further soldering partners that are optionally present. In particular, the circuit board can be equipped with one or more such components, which are joined to them by the soldering method of the invention. In this case, a conductive joint is generally preferably made, whereby the component in question is also electrically contacted. Such a component can be, for example, an IGBT, a diode, a MOSFET, a thyristor, a shunt or a capacitor.

[0036] However, these soldering partners do not necessarily have to be electrical circuit boards and electrical components. Any other component, for example a pipe or a machine housing, can also form the first soldering partner and any other component can form the second soldering partner. For example, a sensor (especially for temperature or mechanical stress) can be soldered onto a pipe or a machine housing. Alternatively, this soldering technique can be used in the field for repairs, for example to solder several pipe parts together.

[0037] The invention will now be described by way of example only and with reference to the accompanying drawings, in which: [Brief description of the drawings]

[0038] [Figure 1]1 is a schematic cross-sectional view of a part of an assembly during a soldering method according to a first embodiment of the invention; [Diagram 2] A detailed view of the solder for such a soldered joint [Diagram 3] FIG. 1 is a schematic perspective view of a portion of an assembly shown with a magnet coil array used in the present soldering method; [Figure 4] 4A-4D are cross-sectional views of an assembly during the production of a solder joint according to another example of the invention, in which identical or functionally identical elements are provided with the same reference numbers. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0039] FIG. 1 is a schematic cross-sectional view of a part of an assembly 1 in a first example of the invention. In the illustrated detailed view of this assembly 1, a soldered joint is produced by the method of the invention between a first soldering partner 10 and a second soldering partner 20. These are in principle any elements of the assembly that should be permanently mechanically joined by soldering. Also in this case, a good conductive joint and thus an electrical contact of the two soldering partners 10 and 20 is obtained if necessary. In this case, the soldered joint produced is mediated by a solder 100, which comprises as its components, on the one hand, a metallic solder material and, in addition, a number of magnetic nanoparticles 120, which are embedded in the solder 100. This solder 100 can in principle be constructed in different ways. It can be, for example, a solder paste or any other solid solder preform. In each case, these magnetic nanoparticles 120 are distributed over the volume of the solder. In the example of FIG. 1, the solder 100 is specifically a solder paste that includes a particle mixture of metallic solder particles and magnetic nanoparticles.

[0040] To form a soldered joint between the two soldering partners 10 and 20, an alternating magnetic field 200 is generated, which is indicated by the corresponding double-headed arrow in FIG. 1. This alternating magnetic field acts on the area of ​​the solder 100. In particular, a magnetic interaction occurs with the magnetic nanoparticles 120 present therein, which heats them up. Thus, the magnetic nanoparticles embedded in the solder 100 become, under the action of the alternating magnetic field 200, a number of localized heat sources in the solder 100, from where heat transfer takes place to the other components of this solder. This heat input is so localized and essentially limited to the area of ​​the solder 100 that the metallic solder material in the solder melts. After the alternating magnetic field is switched off, the solder cools and its melt correspondingly solidifies, thus forming a permanent soldered joint between the two soldering partners 10, 20.

[0041] If the Curie temperature is exceeded due to the local heating of the magnetic nanoparticles, the heat input to the solder is automatically stopped. The temperature reached is therefore automatically limited. This effect, in conjunction with the locally limited heating zone, therefore makes the method a particularly gentle soldering method, advantageously avoiding thermal damage to other elements of the assembly that are optionally present. The heat input to the two soldering partners 10, 20 to be joined is also relatively low.

[0042] FIG. 2 is a detailed view in the region of a solder 100, as can be used, for example, in the soldering method of FIG. 1. Here again, the solder 100 is a solder paste with a multitude of metallic solder particles 110. These are here formed as approximately spherical solder spheres, composed of a metal alloy with a relatively low melting point. Their diameter d110 can be, for example, in the range of a few micrometers to a few tens of micrometers. In addition to these metallic particles, the paste also contains a multitude of magnetic nanoparticles 120, as already mentioned. Furthermore, the solder paste in this example also contains an (optional) organic flux 130. The diameter d120 of the magnetic nanoparticles 120 is significantly smaller than the diameter d110 of the metallic solder spheres 110. Advantageously, the size scale of the magnetic nanoparticles 120 is in the range of 100 nm or less. These nanoparticles contain ferromagnetic or ferrimagnetic material components. Due to their small particle size, these nanoparticles are entirely superparamagnetic. This property allows for strong localized heating of the magnetic nanoparticles in an alternating magnetic field and therefore the energy input required for the soldering method to the solder 100. As shown by the exemplary arrows 300, heat transfer again occurs from the nanoparticles 120 to the metallic solder particles 110, resulting in the melting of these metallic solder particles.

[0043] In the example of Fig. 2, the magnetic nanoparticles have two material components, a core 121 made of a ferromagnetic or ferrimagnetic material and a non-magnetic shell 122. This is not essential and the nanoparticles may alternatively consist of only a single ferromagnetic or ferrimagnetic material. However, the core-shell structure shown here is advantageous since the coating with the shell material makes it possible in particular to avoid excessive agglomeration of the individual nanoparticles.

[0044] FIG. 3 shows a partial perspective view of a part of an assembly 1 positioned in the focal range F of an alternating magnetic field 200 for carrying out the method of the invention. Otherwise, this assembly 1 is formed similarly to the one in the example of FIG. 1, and in particular includes a similar solder 100 for forming a soldered joint. The focal range F is formed relatively narrow so that the energy input to the solder is spatially narrowly limited. To achieve this, two magnet coil arrays 210 and 220 are provided here to generate the alternating magnetic field 200. In this example, they are on either side of the assembly 1, such that the assembly 1 is in the middle of the two coil arrays. In this example, the magnetic poles of the two coil arrays 210 and 220 are concentric with each other. However, instead of this, it is also possible to use two or more magnet coils whose corresponding magnetic poles have different orientations. In particular, these magnetic poles can then intersect within the focal range F, which allows, under certain circumstances, a stronger focus of the energy input.

[0045] FIG. 4 shows a cross-sectional view of another assembly 1, in which a soldered joint is likewise produced by the method of the invention. In this example, the first soldering partner is an electric circuit board 10 and the second soldering partner is an electronic component 20. This second soldering partner is in particular a semiconductor chip, which is inserted into the circuit board and which is conductively connected to a conductor track on the circuit board 10 by the present soldering method. Here too, between the two soldering partners 10 and 20, there is a solder 100, which like in the previous example comprises a metallic solder component and a number of magnetic nanoparticles distributed on the solder 100. Here too, an alternating magnetic field 200 acts on the soldering area, forming a relatively narrow focal range F, within which the energy input from the magnetic field 200 is sufficiently high to melt the metallic solder elements. In particular, the lateral extent of the focal range is smaller than the lateral extent of the chip, as a result of which a point-like local melting of the solder 100 in a partial area under the chip is possible. The arrows 400 indicate that a relative movement takes place between the alternating magnetic field (or the magnetic field generating coil array) and the assembly 1 during the soldering method. This allows the heated soldering area to be precisely limited to one small sub-area of ​​the assembly. Furthermore, Fig. 4 shows that this alternating magnetic field can also penetrate the electronic component 20 and / or other elements of the assembly without causing significant heating of the chip 20 and / or other elements of the assembly, since the substantial energy input is limited to the area of ​​the solder 100 with the magnetic nanoparticles. [Explanation of symbols]

[0046] 1 Assembly 10 First soldering partner (circuit board) 20 Second Soldering Partner (Component) 100 solder 110 Metal solder material (solder particles) 120 Magnetic Nanoparticles 121 cores 122 Shell 130 Flux 200 Alternating magnetic field 210 First magnet coil array 220 Second Magnet Coil Array 300 Heat Transfer 400 Relative Movement d110 Diameter of metal solder particles d120 Diameter of magnetic nanoparticles F Focal range

Claims

1. A method for producing a soldered joint between a first soldering partner (10) and a second soldering partner (20) by means of a solder (100), said solder comprising a metallic solder material (110) and a multitude of magnetic nanoparticles (120), the method comprising at least the steps of: a) generating an alternating magnetic field (200) using at least one magnet coil (210, 220) and applying the alternating magnetic field (200) to the solder (100); b) heating the plurality of magnetic nanoparticles (120) by interaction with the alternating magnetic field (200); c) melting the metallic solder material (110) by heat transfer (300) from the plurality of magnetic nanoparticles (120) to the metallic solder material (110) and forming a soldered joint between the first soldering partner and the second soldering partner by the molten metallic solder material (110); Methods including:

2. 2. The method of claim 1, wherein the plurality of magnetic nanoparticles (120) are superparamagnetic and comprise a ferromagnetic or ferrimagnetic material, in particular in the form of a metal alloy or metal oxide, the alloy or metal oxide comprising at least one of the elements iron, cobalt and nickel, and the weight percentage of the metal alloy or metal oxide in the overall solder is between 1% and 30%.

3. The method of claim 1 or 2, wherein the diameter (d120) of the plurality of magnetic nanoparticles (120) is less than 100 nm.

4. The method according to any one of claims 1 to 3, wherein the Curie temperature of the plurality of magnetic nanoparticles (120) is in the range of 100°C to 1200°C, preferably in the range of 150°C to 400°C.

5. 5. The method according to any one of claims 1 to 4, wherein the full width at half maximum (FWHM) of the distribution of Curie temperatures of each of the plurality of magnetic nanoparticles (120) is 50°C or less, preferably 30°C or less.

6. The method of any one of claims 1 to 5, further comprising the step of: d) allowing the plurality of magnetic nanoparticles (120) to reach their Curie temperature such that further heating of the solder (100) is avoided.

7. The method according to any one of claims 1 to 6, wherein the magnetic nanoparticles (120) have a core (121) made of a ferromagnetic or ferrimagnetic material and a non-magnetic shell (122).

8. 8. The method according to claim 1, wherein in step a) at least two magnet coils (210, 220) with different pole arrangement directions are used, and these magnet coils (210, 220) are moved relative to the two soldering partners (10, 20).

9. The method of claims 5 and 8, wherein the heat transfer (300) is abruptly interrupted to avoid exceeding a predetermined maximum temperature.

10. 10. The method according to any one of the preceding claims, wherein different solders (100) having different melting temperatures are used in one assembly (1) to produce different types of soldered joints.

11. An assembly (1) having one first soldering partner (10) and one second soldering partner (20), the two soldering partners (10, 20) being joined by a solder (100) comprising one metallic solder material (110) and a number of magnetic nanoparticles (120) embedded therein.

12. 12. The assembly of claim 11, wherein the plurality of magnetic nanoparticles (120) are superparamagnetic and comprise a ferromagnetic or ferrimagnetic material, in particular in the form of a metal alloy or metal oxide, the alloy or metal oxide comprising at least one of the elements iron, cobalt and nickel, and the weight percentage of the metal alloy or metal oxide in the entire solder (100) is between 1% and 30%.

13. Assembly (1) according to claim 11 or 12, wherein the first soldering partner (10) is an electric circuit board.

14. Assembly (1) according to any one of claims 11 to 13, wherein the second soldering partner (20) is an electrical or electronic component, in particular a power electronic component.

Citation Information

Patent Citations

  • Soldering method, device and composition by induction heating

    JP1993505345A

  • Solder material containing magnetic particle and its preparation

    JP1994277871A

  • Electronic component, printed wiring board, and method for attaching and detaching electronic component on and from printed wiring board

    JP2001044616A

  • Soldering material and solder feeding method

    JP2008200720A

  • Multi-functional nano / micro solders and their methods for preparing the same

    KR1020160027452A