Method and system for making biosensors - Patents.com
Patent Information
- Application Number
- JP2024522172
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-10-15
- Filing Date
- 2022-10-14
- Publication Date
- 2024-10-10
Smart Images

Figure 2024537336000001_ABST
Abstract
Description
[Technical field]
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS This application claims priority to U.S. Provisional Patent Application No. 63 / 256,086, entitled “Methods and Systems for Fabricating Biosensors,” filed October 15, 2021, the disclosure of which is incorporated by reference in its entirety into this specification.
[0002] The present disclosure relates to the preparation of coatings for biosensors. In particular, the present disclosure relates to the preparation of coating biosensors with biocompatible biopolymers. [Background technology]
[0003] Implantable sensors for measuring biomarkers, such as enzyme assays, have a limited lifespan due to exposure to defensive foreign body responses. These responses include inflammation, recruitment of immune cells, and the subsequent formation of a fibrotic capsule. This leads to reduced enzyme activity and thus reduced biosensing capacity, as well as dense capsules that can limit the diffusion of analytes, thus reducing the functional measurement window. Immune molecules also foul the electrochemical electrode surface, blocking and inactivating the redox capabilities of the electrode. It is also true that current methods for making enzyme biosensors are difficult to tune without variability, requiring significant individual calibration. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] EP21202802.1 [Patent Document 2] PCT / EP2022 / 078635 Summary of the Invention
[0005] Described herein are methods and systems for creating precise coatings on biosensors with biocompatible biopolymers via spin-coating and curing hydrogels. These thin, geometrically defined pullulan films have consistent pore size, chemical resistance, and provide a stable protective environment for enzymes.
[0006] In a first aspect of the present invention, a method of making a biosensor is disclosed, the method comprising the steps of: providing a wafer or other solid material having electrodes on a surface thereof; disposing a droplet of hydrogel on the electrodes; rotating the wafer while it is exposed to a partial vacuum; and heating the wafer or other solid material. Instead of a wafer, another solid material such as glass, polymer, etc. can be used to support the electrodes.
[0007] In a second aspect of the present invention, a biosensor is disclosed, the biosensor comprising: an electrode comprising a conductive layer on a substrate layer; and a hydrogel layer on the conductive layer; the hydrogel layer is less than 3 micrometers thick and comprises an enzyme immobilized within the hydrogel layer. In some embodiments of the second aspect, the hydrogel layer is less than 1 micrometer thick. In some embodiments, the enzyme is in the oxidase family, such as glucose oxidase, lactate oxidase, uricase oxidase, alcohol oxidase, cortisol oxidase, xanthine oxidase, cholesterol oxidase, and / or sarcosine oxidase.
[0008] The details of one or more embodiments of the disclosure are set forth in the accompanying drawings and the description below. Other features, objects, and advantages will become apparent from the description, drawings, and claims. [Brief description of the drawings]
[0009] The accompanying drawings, which are incorporated in and constitute a part of this specification, illustrate one or more embodiments of the present disclosure and, together with the description of the exemplary embodiments, serve to explain the principles and implementations of the present disclosure. [Figure 1A] FIG. 1 shows an example setup for a drop-spin process. [Figure 1B] FIG. 1 illustrates an example setup for a drop-spin process. [Figure 2A] FIG. 1 shows an example of drop-spin of pullulan coated with sputtered platinum on top. [Figure 2B] FIG. 1 shows an example of a drop-spin of pullulan that is not coated with platinum sputtered on top. [Figure 3A] FIG. 1 shows an example scanning electron microscope (SEM) image of a drop-spin sensor, showing an example of a sensor made by a drop-coat process. [Figure 3B] FIG. 1 shows an example scanning electron microscope (SEM) image of a drop-and-spin sensor, illustrating an example of a sensor based on the drop-and-spin process. [Figure 4] FIG. 1 shows an example of multiple layers formed using a drop-and-spin process. [Figure 5A] FIG. 13 shows an example of adhesion between pullulan hydrogel and platinum electrode in a biosensor fabricated by drop-spin deposition. [Figure 5B] FIG. 13 shows an example of adhesion between pullulan hydrogel and platinum electrode in a biosensor fabricated by drop-spin deposition. [Figure 5C] FIG. 13 shows an example of adhesion between pullulan hydrogel and platinum electrode in a biosensor fabricated by drop-spin deposition. [Figure 5D] FIG. 13 shows an example of adhesion between pullulan hydrogel and platinum electrode in a biosensor fabricated by drop-spin deposition. [Figure 6A]FIG. 1 illustrates the longevity of drop-spin deposition in an exemplary one-layer embodiment; FIG. 2 shows an example of a one-layer embodiment. [Figure 6B] FIG. 1 illustrates the longevity of drop-spin deposition in an illustrative bilayer embodiment; FIG. 2 shows an example of a bilayer embodiment. [Figure 6C] FIG. 1 illustrates the longevity of drop-spin deposition for illustrative one-layer and two-layer embodiments, showing an example of normalized sensitivity over time. [Figure 6D] FIG. 1 illustrates the longevity of drop-spin deposition for illustrative 1-layer and 2-layer embodiments, showing an example comparison of normalized sensitivity (relative to initial measurements) over a period of 36 days. [Figure 7] FIG. 1 shows an example of concentration versus current for a sensor fabricated, for example, by drop-and-spin. [Figure 8] FIG. 13 shows a further exemplary comparison between one-layer and two-layer sensors (coated by drop-spin fabrication method) in terms of concentration versus current. [Figure 9A] FIG. 9 shows an exemplary comparison between a one-layer sensor (FIG. 9A) and a two-layer sensor (FIG. 9B) stored in phosphate buffered saline (coated by drop-spin fabrication method). [Figure 9B] FIG. 9 shows an exemplary comparison between a one-layer sensor (FIG. 9A) and a two-layer sensor (FIG. 9B) stored in phosphate buffered saline (coated by drop-spin fabrication method). [Figure 10] FIG. 1 shows an exemplary comparison of a 1-layer sensor versus a 2-layer sensor (each coated by drop-spin fabrication method) in terms of Km values over time. [Figure 11] FIG. 13 shows an example enzyme saturation curve for sensors coated by drop-spin fabrication method on a dry wafer over a period of 24 days. [Figure 12] FIG. 13 shows an example graph of the long term lifetime of sensors coated by drop-and-spin fabrication method. [Figure 13A]FIG. 1 shows an example of data relating to bilayer hydrogels. FIG. 2 shows an example of a bilayer hydrogel. [Figure 13B] FIG. 1 shows an example of data for a bilayer hydrogel, showing an example graph of sensitivity over time. [Figure 13C] FIG. 1 shows an example of data for bilayer hydrogels, showing an example graph of K values over time. [Figure 13D] FIG. 13 shows an example of data for a bilayer hydrogel, showing an example graph of normalized maximum current over time. [Figure 14A] FIG. 1 shows exemplary scanning electron microscope (SEM) images of drop-coated versus drop-spun layer thickness. [Figure 14B] FIG. 1 shows exemplary scanning electron microscope (SEM) images of drop-coated versus drop-spun layer thickness. [Figure 14C] FIG. 1 shows exemplary scanning electron microscope (SEM) images of drop-coated versus drop-spun layer thickness. [Figure 14D] FIG. 1 shows exemplary scanning electron microscope (SEM) images of drop-coated versus drop-spun layer thickness. [Figure 15] FIG. 13 shows an example of a SEM image showing layer thickness from the drop-and-spin method. [Figure 16A] FIG. 1 shows an example for a double layer hydrogel sensor, depicting the general composition of the sensor coating. [Figure 16B] FIG. 13 shows an example for a double-layer hydrogel sensor, showing an example graph of the enzyme saturation curve for one sensor over a period of 948 days. [Figure 16C] FIG. 13 shows an example for a double-layer hydrogel sensor, showing an example graph of the enzyme saturation curve for one sensor over a period of 948 days. [Figure 16D] FIG. 13 shows an example for a double-layer hydrogel sensor, showing an example graph of current as a function of glucose concentration at 1148 days. [Figure 16E]FIG. 13 shows an example graph of the enzyme saturation curve on day 1148. [Figure 17A] FIG. 1 shows example data for a bilayer coated hydrogel sensor, showing an example of a bilayer hydrogel. [Figure 17B] FIG. 13 shows example data for a dual-layer coated hydrogel sensor, showing an example graph of current as a function of glucose concentration on day 1. [Figure 17C] FIG. 13 shows example data for a dual-layer coated hydrogel sensor, showing an example graph of an enzyme saturation curve on day 1. [Figure 18A] FIG. 1 shows an example of data relating to bilayer hydrogels. FIG. 2 shows an example of a bilayer hydrogel. [Figure 18B] FIG. 1 shows an example of data for a bilayer hydrogel, showing an example graph of an enzyme saturation curve over a 15 day period. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Creating precise coatings on biosensors with biocompatible biopolymers can be achieved through spin-coating and curing hydrogels on electrodes. Spin-coating ("drop-spin") allows deposition of geometrically defined films with consistent pore size and chemical resistance, providing a stable, protective environment for the enzymes immobilized therein. An exemplary process for immobilizing enzymes in hydrogels can be found in U.S. Patent Application Publication No. 2020 / 0133994, entitled "HYDROGEL FOR IMMOBILIZATION OF ONE OR MORE ENZYME(S) AND METHOD FOR PREPARING THE SAME," invented by Oliver Plettenburg et al. and filed on October 15, 2021.
[0011] As used herein, an electrode is typically a conductive layer (such as Pt) on a substrate (such as Si, silicon nitride, or Si / SiO2).
[0012] As used herein, a diffusion barrier is a layer used to protect a conductive metal layer from the diffusion of impurities from another metal and from corrosion from the environment.
[0013] In some embodiments, the drop-spin process involves placing one or more spaced droplets of hydrogel (e.g., pullulan, etc.) on the electrodes of the wafer and then spinning the wafer at high speed. The wafer can be placed under vacuum (e.g., at 60-70 psi) to help hold the wafer to the spin coater platform. The wafer can alternatively be held in place with an adhesive in addition. In some embodiments, the electrode is platinum. In some embodiments, the electrode is made of a biocompatible material such as another noble metal (e.g., gold, silver, etc.), a platinum group element, a metal such as graphite or titanium, or an oxide (e.g., SiO2, titanium oxide, or Al2O3, etc.), a non-noble metal, a layer of nanoparticles or nanotubes, or other suitable conductive material for deposition on a sensor known in the art. In some embodiments, this process is followed by a heating step.
[0014] Hydrogels are three-dimensional networks of hydrophilic polymers. Polysaccharide polymers can be used in all applications, but other polymers may be used when the hydrogel is used as a second protective layer. Hydrogels may contain, for example, one or more polysaccharides with different carbohydrate compositions or molecular weights. Furthermore, carbohydrate polymers can be functionalized to covalently bond with each other or with other species. In addition, hydrogels can be used in combination with other non-carbohydrate polymers, such as polyurethane layers or glutaraldehyde / albumin mixtures.
[0015] The term "hydrogel" as used herein and in relation to the present invention is a term familiar to those skilled in the art and includes any network of covalently crosslinked polymer chains that are hydrophilic. Hydrogels typically build three-dimensional solids that include hydrophilic polymer chains held together by specific crosslinkers. Due to the inherent crosslinkers, the structural integrity of the hydrogel network is not dissolved in water. Hydrogels are highly absorbent (can contain more than 90% water) natural or synthetic polymer networks.
[0016] In some aspects of the invention, it may be useful to use layers of different polymers. These polymers may differ in composition, polarity, pore size, and degree of crosslinking. These layers can be applied sequentially using the process described below.
[0017] In one embodiment of the present invention, one or more enzymes can be added to the mixture of polymers. Additionally, the viscosity of the resulting mixture can be adjusted by adding additional solvent, water, surfactants, or other ingredients known to those skilled in the art.
[0018] The thermally induced drop-spin gelation process allows for the application of geometrically precise layers onto the sensor chip surface. It offers a modular fabrication system since the degree of crosslinking, linker polarity, linker length, and correspondingly pore size can be controlled. After mixing and drop-spin coating non-viscous solutions of the individual gel components, the formation of a covalent, non-degradable network can be induced within the layer by heating the sensor to a mild temperature compatible with maintaining enzyme activity (e.g., at 40°C for 1 to 15 hours).
[0019] As used herein, a "covalent network" includes at least two polymeric components bound together by covalent chemical bonds, i.e., not relying exclusively on electrostatic or van der Waals interactions (although these may contribute to the formation of the network). The term "non-degradable" refers to the formation of bonds that cannot be cleaved by enzymatic reactions (e.g., by peptidases or esterases) or by autohydrolysis.
[0020] The solution can be dropped onto the center of the electrode pattern set and then rotated to spread it over the target area. Multiple droplets spreading across the pattern set can also be used. The layer thickness can be varied by varying the rotation speed (e.g., 1000-6000 rpm, etc.), with higher speeds producing thinner films. The process is compatible with microfabrication tooling and the resulting layers are compatible with microfabrication vacuum systems and organic solvents. Thin layers of 20 nm to 1000 nm are achievable, although thicker layers can be achieved if desired. In general, thin electrode coating layers provide superior signal efficiency due to the shorter diffusion time of the generated reaction products to reach the electrodes.
[0021] As demonstrated herein, the drop-and-spin process and various microfabrication processes allow multiple layers in multiple configurations to be constructed. These drop-and-spin hydrogels show good adhesion to repeating layers and biosensor electrodes.
[0022] FIG. 1A illustrates an example of a drop-spin method. In the drop-coating method, an applicator (110) (e.g., a pipette, etc.) applies a droplet (115) of a coating (e.g., a hydrogel, etc.) to the surface of a wafer (120), which spreads (125) over time to a thickness of 1-3 micrometers. In the drop-spin coating method, a rotating platform (130) compresses the coating (135) to a thickness of only 200-600 nm. An exemplary droplet size is 20 microliters (μL) for a mixture (e.g., pullulan + enzyme, two-component system, etc.). An exemplary rotation speed is 4000 rpm for 30 seconds. In some embodiments, the rotation speed is in the range of 1000-6000 rpm. In some embodiments, the droplet size is in the range of 2 μL to 100 μL. In some embodiments, the droplet size is greater than 100 μL. In some embodiments, the rotation starts at a low speed (such as 500 rpm) for a first interval (such as 10 seconds), and then increases to a high speed (such as 4000 rpm) for a second interval (such as 30 seconds). For example, the low speed can be less than 1000 rpm and the high speed can be greater than 1000 rpm. After the drop-spin, the hydrogel is allowed to polymerize on top of the electrodes (e.g., in an oven at 40° C.).
[0023] FIG. 1B shows a wafer (150) having a number of droplets (145) placed on a rotating assembly (155) prior to the spinning step.
[0024] The drop-spin method is compatible with microelectronic methods for wafer processing, such as ultraviolet (UV) induced functionalization, vacuum, clearing / cleaning with organic solvents, etc. Figures 2A and 2B show examples of platinum sputtered onto pullulan deposited by the drop-spin method (Figure 2A) and pullulan deposited by the drop-spin method without platinum (Figure 2B). The deposition process allows for precise placement of a thin layer of biopolymer on the electrode and, with it, a metal coating on top. In some embodiments, the coating is in the range of 0.2 μL to 100 μL per sensor, or about 2-15 mL (preferably 3-10 mL) per 100 mm diameter wafer. Also, small volumes, i.e., 0.1 μL to 10 μL, can be used. In some embodiments, the biopolymer layer is less than 600 nm thick. In some embodiments, the biopolymer layer is 200-600 nm thick. In some embodiments, the biopolymer layer is 200-400 nm thick. In some embodiments, the biopolymer layer is less than 200 nm thick. In some embodiments, the layer on the biopolymer (e.g., platinum, etc.) is up to 50 nm thick. In some embodiments, the layer on the biopolymer is 50-100 nm thick. In some embodiments, the layer on the biopolymer is up to 100 nm thick. In some embodiments, the layer on the biopolymer is more than 100 nm thick.
[0025] An example scanning electron microscope image of a sensor in which the pullulan-enzyme mixture was deposited by the drop-spin method is shown in Figure 3. As shown, very thin layers (e.g., 20 nm to 1 micrometer) without deep 3D structures are possible.
[0026] FIG. 4 shows examples of coating techniques. Panel A shows a monolayer hydrogel (e.g. pullulan, etc.) on top of an electrode (e.g. platinum on silicon / SiO2, etc.). Panel B shows a monolayer hydrogel with enzyme immobilized in the hydrogel network. Panel C shows a two-layer coating, where the top layer can be a biopolymer layer without enzyme, thereby acting as a diffusion or protective barrier. These layers can be made by dropwise spin coating, especially when thin / multilayer layers are desired, and other methods of making can also be used, as will be understood by those skilled in the art. Panel D shows a different two-layer system with sputtered platinum on the top layer. Panel E shows a three-layer system, where both the sputtered platinum layer and the enzyme-free hydrogel layer are on top of the hydrogel-enzyme layer. This provides an improved approach in terms of the body's immune response system, and therefore works well for implantable chips. Furthermore, layers can be added depending on the desired properties and applications.
[0027] 5A to 5D show an example of adhesion between hydrogel and electrodes. In this example, the sensor (platinum electrode) was coated with pullulan-enzyme by drop-spin and then incubated in deionized water for 2 to 3 days in a chamber large enough to allow it to be completely covered by deionized water. This washed away everything except the bound biopolymer and immobilized enzyme. After removing the wafer from the chamber, all the hydrogel areas not overlying the electrodes were washed away. There are certain areas where the pullulan attaches very strongly to the electrode areas. Photolithography and lift-off processes can be used to define the location of the electrodes on the substrate. In other areas of the wafer (e.g. Si3N4, etc.), the pullulan is removed. The individual network properties and density depend on the nature of the polymer used and its degree of cross-linking. This can be illustrated by the optical appearance of electrodes covered with PCM1 and PCM9. However, the electrode adhesion properties are comparable for the two different cross-linked polymers. Depending on the particular biosensing problem, differently modified materials can provide the optimal coating for the desired application, as will be understood by those skilled in the art. 5C and 5D show examples of adhesion of singly carboxymethylated (CM)1 pullulan (FIG. 5C) and nine times carboxymethylated (CM9) pullulan (FIG. 5D).
[0028] In the context of the present invention, the degree of carboxymethylation of pullulan is represented by the designation "PCM" followed by a number (e.g., PCM1, PCM3, PCM5, etc.). This number characterizes the respective degree of carboxymethylation and refers to the carboxymethyl groups introduced into pullulan by applying the designated number of repeated carboxymethylation reaction cycles. As used herein, CM1, CM2, CM3, etc. describe the respective degree of carboxymethylation of polysaccharides in general (without specific reference to pullulan).
[0029] CM1 (or PCM1 in the case of pullulan) is considered a low level modified biopolymer. CM9 (or PCM9) is considered a high level modified biopolymer. Highly modified biopolymers (PCM5-PCM9) have short gelation times (2-5 hours; 40 mg / ml material). Low level modified biopolymers (PCM1-3) have gelation times (40 mg / ml material) of 3-10 hours.
[0030] Figures 6A to 6D illustrate the long life of the drop-spin deposited sensor system. In one example, a single wafer had two sensor types drop-spin deposited on it: a single layer of pullulan CM9 (Figure 6A) and pullulan CM9 with a top platinum layer (Figure 6B). The hydrogel layer here was pullulan CM (PCM) with glucose oxidase (GOX) isolated in the PCM. The layers deposited on the electrode system were stored in either phosphate buffered saline or air. Note that in the drop-spin process, the enzyme and sensor were still active after dry storage at room temperature, which is different from the previous method. Glucose concentrations ranged up to 42 mM. Both sensor types were exposed to high vacuum followed by acetone incubation (1-2 hours) and then washed with isopropyl alcohol prior to measurements. It can be seen that the functionality of the sensor was maintained even under these challenging conditions.
[0031] Figure 6C shows the normalized sensitivity over time for the sensors. In Figures 6C, 6D, and 7-11, sensors 1, 2, 5, 6, and 7 are single-layer sensors (Figure 6A, PCM9+GOX) and sensors 3, 4, 8, 9, and 10 are double-layer sensors (Figure 6B, PCM9+GOX+100 nm Pt). Tests were performed on two wafers, one stored in PBS and the other stored dry.
[0032] Figure 6D shows the average sensitivity over 36 days for each: 1 layer (Figure 6A) has an average sensitivity (normalized) of 0.75, and 2 layers (Figure 6B) has a sensitivity of 0.89 due to the diffusion barrier effect.
[0033] Figure 7 shows a graph of concentration versus current for the sensors of the previous example (Figures 6A and 6B) over a period of 43 days. The wafers were stored in phosphate buffered saline (PBS). The one-layer sensors (here 1, 2, and 7) had a different slope than the two-layer sensors (here 3, 9, and 10), and the initial slope changed with time.
[0034] Figure 8 also shows the difference between sensor types (Figures 6A and 6B) in concentration versus current: the two-layer sensor has a better (slower) initial slope and a larger linear range.
[0035] 9A and 9B show an exemplary comparison between a one-layer sensor (FIGS. 6A and 9A) and a two-layer sensor (FIGS. 6B and 9B), the two-layer sensor having a thickness of 100 nm (top layer of platinum), both stored in PBS. As shown, the two-layer sensor shows a better linear range. The observed current density is, for example, 10.5 A / m 2 which is obtained by dividing the measured current (vertical axis in nA) by the area of the working electrode, e.g., a measured 150 nA = 10.5 A / m 2 It is.
[0036] Figure 10 shows a comparison of Km (substrate affinity of the enzyme) values for the one-layer sensor (Figure 6A) and the two-layer "sandwich" sensor (Figure 6B) from 3 to 24 days. The Km values are significantly higher for the two-layer sensor than for the one-layer sensor. The one-layer sensor had Km values of 9-12 mM, and the two-layer sensor had Km values of 25-38 mM.
[0037] Figure 11 shows example enzyme saturation curves (from the sensors in the previous example). Data was acquired over 24 days from dried wafers. The two-layer sensors (here 4 and 8; see e.g. Figure 6B) had a 100 nm Pt diffusion barrier, a 200-600 nm GOX hydrogel layer, a 200 nm Pt conductive layer, 2000 nm SiO2, and a 0.5 mm Si substrate. The two-layer sensors exhibit a larger linear range and are therefore more stable over time compared to the one-layer sensors. The one-layer sensors (here 1 and 2; see e.g. Figure 6A) are PCM9.
[0038] 12 shows an example graph of the long-term (e.g., 200 days) lifetime of a sensor that is a bilayer sensor (see, e.g., FIG. 4C) with a 50 nm sputtered platinum top layer on top of PCM5 hydrogel. The sensor was stored in 1× PBS at room temperature (rt).
[0039] 13A-13D show example data for two bilayer sensors (see sensors 7 and 9 in FIG. 4C). FIG. 13A shows the sensor structure, which is a bilayer sensor covered with hydrogel (without enzyme) instead of Pt sandwich. FIG. 13B shows the normalized sensitivity over time, showing good stability of sensitivity over time. FIG. 13C shows the Knee (K) value (mM) over time, which is also shown to be very stable. FIG. 13D shows the normalized maximum current over time, showing only a drop from 100 to 60 over 160 days. These results are from tests performed in PBS buffer (pH 7.4) at room temperature. The hydrogel is PCM5 (mid-range) and glucose oxidase is the enzyme.
[0040] 14A-14D show example scanning electron microscope (SEM) images of a drop-coat (older technology) coating. As shown, the drop-spin coating method provides a thinner layer.
[0041] Figure 14A shows drop-coating of PCM5 with hydrogel in distilled water (dH2O). Figures 14B and 14C show drop-coating of PCM9 with hydrogel in dH2O. Figure 14D shows a close-up of drop-coating of PCM6 with hydrogel in PBS.
[0042] FIG. 15, in contrast to FIGS. 14A-14D, shows an example of SEM images of different layers and the estimated layer thicknesses for drop-spin coating with hydrogel (pullulan) in dH2O.
[0043] 16A-16D show illustrative data for a two-layer sensor (see, e.g., FIG. 4C). FIG. 16A shows the composition of the sensor, and the data refers to a two-layer sensor covered with a hydrogel layer (without enzyme). FIGS. 16B and 16C show the enzyme saturation curves over a period of 948 days. The graphs in FIG. 16D and FIG. 16EE show the sensitivity of the sensor at 1148 days, thus illustrating the robustness of the sensor and the stabilizing effect of the hydrogel on the enzyme. Both hydrogel layers contained PCM5, and glucose oxidase was used as the enzyme. The sensors were stored in PBS (pH 7.4) at room temperature over the measurement period.
[0044] 17A-17C show illustrative data for a two-layer sensor (see, e.g., FIG. 4C). FIG. 17A shows the composition of the sensor, and the data refers to a two-layer sensor covered with a hydrogel layer (no enzyme). The graphs in FIGS. 17B-17C show the sensitivity of the sensor over a high glucose concentration range (0-42 mM). A particularly high sensitivity of 49 nA / mM was determined for the sensor. The first hydrogel layer is composed of a PCM4 hydrogel with immobilized glucose oxidase, and the second hydrogel layer includes an alginate hydrogel. The sensor was stored in PBS (pH 7.4) at 37° C. for 1 day.
[0045] 18A-18B show example data for a two-layer sensor (see, e.g., FIG. 4C). The composition of the sensor is depicted in FIG. 18A, and the data refers to a two-layer sensor covered with hydrogel (no enzyme). The graph in FIG. 18B shows the enzyme saturation curve over 15 days. Over a continuous incubation period of 15 days at 37° C., these results demonstrate the stability and longevity of the immobilized glucose oxidase, as well as the positive benefit of the second alginate hydrogel layer. The first hydrogel layer is composed of a PCM4 hydrogel with immobilized glucose oxidase, and the second hydrogel layer comprises an alginate hydrogel. The sensor was stored in PBS (pH 7.4) at 37° C. for 15 days.
[0046] Example Hydrogels The drop-spin method can be used with a method of immobilizing enzymes in a biocompatible hydrogel (identified in this example as "biocompatible hydrogel") that does not require covalent attachment of one or more enzymes. The hydrogel provides a perfect stabilizing environment for the enzyme, resulting in better longevity and stability of the enzyme. The hydrogel protects the enzyme from biofouling and the body's immune response. The hydrogel was invented by Oliver Plettenburg et al. and is described in U.S. Patent No. 5,399,433, entitled "HYDROGEL FOR IMMOBILIZATION OF ONE OR MORE ENZYME(S) AND METHOD FOR PREPARING THE SAME," filed on October 15, 2021, and U.S. Patent No. 5,399,433, having the same title, filed on October 14, 2022, and published as WO / , all of which are incorporated herein by reference.
[0047] A method for preparing such a biocompatible hydrogel includes the following steps: a) providing a first polysaccharide and a second polysaccharide, preferably the first polysaccharide and / or the second polysaccharide are independently selected from the group comprising pullulan, alginic acid, cellulose, hyaluronic acid, dextran, lichenin, lentinan, and mixtures thereof, and n is the number of monomer repeat units of the first and / or second polysaccharide, n being an integer between 10 and 10000; b) optionally carboxymethylating at least one OH group of the first and / or second polysaccharide; c) functionalizing the first polysaccharide with one or more linker units of structure -AX, if the monomer repeat unit of the first polysaccharide does not contain a carboxylic acid residue, or with one or more linker units of structure -X, if the monomer repeat unit of the first polysaccharide contains a carboxylic acid residue, where A is -(CH2) d -C(O)- or -C(O)-NH-, d is an integer from 1 to 3, and X is -NH-(CH r -N3, -NH-(CH2CH2O) s -CH2CH2N3 and -NH-(CH2-CH2-C(O)) t -CH2-CH2-N3, r is an integer from 2 to 20, s is an integer from 1 to 15, and t is an integer from 1 to 15; and, functionalizing the second polysaccharide with one or more linker units of the structure -A'-Y, if the monomer repeat unit of the second polysaccharide does not contain a carboxylic acid residue, or functionalizing the second polysaccharide with one or more linker units of the structure -Y, if the monomer repeat unit of the second polysaccharide contains a carboxylic acid residue, where A' is -(CH2) d -C(O)- or -C(O)-NH-, and d is an integer from 1 to 3; Y is -NH-(CH2) r -Q, -NH-(CH2CH2O) s -CH2CH2Q, and -NH-(CH2-CH2-C(O)) t -CH2-CH2-Q, Q is
[0048] [ka] or
[0049] [ka] and M, M'=H or Me, and W=OMe, OEt, OH, NH2, or NHMe; d) optionally adding one or more enzymes to the mixture formed by steps a) to c); e) incubating the mixture formed by steps a) to d) in an aqueous medium at a temperature in the range of 25° C. to 70° C., preferably 40° C., for at least 1 hour, preferably 1 to 10 hours; may include.
[0050] Biocompatible hydrogels are: The following structure: a first polysaccharide and a second polysaccharide, Preferably, the first polysaccharide and / or the second polysaccharide are independently selected from the group comprising pullulan, alginic acid, cellulose, hyaluronic acid, dextran, lichenin, lentinan, and mixtures thereof, and n is the number of monomer repeat units of the first polysaccharide and / or the second polysaccharide, and n is an integer from 10 to 10000. - one or more linker units linking the first polysaccharide to the second polysaccharide, the structure of the one or more linker units being: -A-Z1-B-Z2-A´-, A and A' are each independently -(CH2) d -C(O)- or -C(O)-NH-, and d is an integer from 1 to 3; Z1 is -O-, -(CH2) r -, -NH-(CH2CH2O) s -CH2CH2- and -NH-(CH2-CH2-C(O)) t-CH2-CH2-, d is an integer from 1 to 4, r is an integer from 2 to 20, s is an integer from 1 to 15, and t is an integer from 1 to 15; moreover, Z2 is -O-, -(CH2) r -, -NH-(CH2CH2O) s -CH2CH2- and -NH-(CH2-CH2-C(O)) t -CH2-CH2-, B is,
[0051] [ka] and further, R' is one or more linker units selected from the group comprising -CF3, -C(O)-OMe, -C(O)-OEt, -C(O)-OH, -C(O)-NH2 and -C(O)-NHMe for non-covalent immobilization of one or more enzymes; The polymer may include a crosslinked polymer comprising:
[0052] As used herein, the term "biocompatible", particularly in relation to hydrogels, means that each material that is referred to or evaluated as being biocompatible has the quality of not having toxic or deleterious effects on biological systems, performs its desired function without inducing any undesirable local or systemic effects in the recipient, but has the ability to generate the most appropriate beneficial response in its particular situation, or to exist in harmony with tissues without causing deleterious changes. Favorable properties of biocompatible materials are reduced inflammatory and immune responses, and / or low / limited fibrous encapsulation.
[0053] The first and / or second polysaccharide may optionally be carboxymethylated in step b), at least one OH group of the first and / or second polysaccharide as described herein above may be carboxymethylated. In one embodiment, carboxymethylation is preferably carried out when the first and / or second polysaccharide is pullulan or dextran.
[0054] As used herein, the term "functionalization" or "functionalized" generally refers to the addition of specific functional groups to provide new desired properties to a compound, such as the addition of one or more linker units to an existing polysaccharide structure.
[0055] The functionalization of said second polysaccharide in step c) may be carried out with one or more linker units of the structure -A'-Y when the monomer repeat unit of the second polysaccharide does not contain a carboxylic acid residue, or the functionalization of said second polysaccharide in step c) may be carried out with one or more linker units of the structure -Y when the monomer repeat unit of the second polysaccharide contains a carboxylic acid residue, where A' is -(CH2) d -C(O)- or -C(O)-NH-, d is an integer from 1 to 3, and Y is -NH-(CH2) r -Q, -NH-(CH2CH2O) S -CH2CH2Q and -NH-(CH2-CH2-C(O)) t -CH2-CH 2- Q is selected from the group Q is
[0056] [ka] or
[0057] [ka] and M, M'=H or Me, and W=OMe, OEt, OH, NH2, or NHMe.
[0058] As used herein, Q is
[0059] [ka] or
[0060] [ka] may be M, M'=H or Me, and W=OMe, OEt, OH, NH2, or NHMe.
[0061] [ka] For the structural formula
[0062] [ka] However, when used elsewhere in this specification, this does not mean that for the latter structural formula, both M must be the same (each H or each Me). Rather, the invention can include that in one embodiment, both M can be H, in one embodiment, both M can be Me, and even in one embodiment, one M can be H and the other M can be Me (there are two possibilities, one M is H and the other M is Me, regardless of the position of M). Thus, in the context of the present invention, two structural formulas
[0063] [ka] and
[0064] [ka] can be used interchangeably herein.
[0065] Furthermore, in the context of the present invention, the functionalization of the second polysaccharide with one or more linker units of the structure -A'-Y, Y is -NH-(CH2) r -Q, -NH-(CH2CH2O) s -CH2CH2Q and -NH-(CH2-CH2-C(O)) t -CH2-CH2-Q, Q is
[0066] [ka] or
[0067] [ka] and M, M'=H or Me, and W=OMe, OEt, OH, NH2, or NHMe, -NH-(CH2) r -Q, -NH-(CH2CH2O) s -CH2CH2Q or -NH-(CH2-CH2-C(O)) t The linkage of Q in -CH2-CH2-Q is represented by the structural formula
[0068] [ka] and
[0069] [ka] It will be perfectly clear to a person skilled in the art that the above is via the dashed lines given in
[0070] In one embodiment, in step d), it may be carried out optionally to add one or more enzymes to the mixture formed by steps a) to c). In this embodiment, any enzyme is in principle possible.
[0071] In step e), the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 25° C. to 70° C. for at least 1 hour. More preferably, in step e), the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 25° C. to 70° C. for 1 to 15 hours. Even more preferably, in step e), the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 25° C. to 70° C. for 1 to 10 hours.
[0072] It is preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 30° C. to 60° C. for at least 1 hour. It is more preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 30° C. to 60° C. for 1 to 15 hours. It is even more preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 30° C. to 60° C. for 1 to 10 hours.
[0073] It is further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 35° C. to 50° C. for at least 1 hour. It is further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 35° C. to 50° C. for 1 to 15 hours. It is even further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 35° C. to 50° C. for 1 to 10 hours.
[0074] It is further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 35°C to 45°C for at least 1 hour. It is further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 35°C to 45°C for 1 to 15 hours. It is even further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 35°C to 45°C for 1 to 10 hours.
[0075] It is more preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature of about 40° C. for at least 1 hour. It is even more preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature of about 40° C. for 1 to 15 hours. It is even more preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature of about 40° C. for 1 to 10 hours. It is further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 30° C. to 60° C. for 4 to 10 hours. It is further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 35° C. to 50° C. for 4 to 10 hours. It is further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 35° C. to 45° C. for 4 to 10 hours. It is further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature of about 40° C. for 4 to 10 hours.
[0076] It is further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 30° C. to 60° C. for 4 to 6 hours. It is further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 35° C. to 50° C. for 4 to 6 hours. It is further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 35° C. to 45° C. for 4 to 6 hours. It is further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature of about 40° C. for 4 to 6 hours.
[0077] It is further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 30° C. to 60° C. for 6 to 8 hours. It is further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 35° C. to 50° C. for 6 to 8 hours. It is further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature in the range of 35° C. to 45° C. for 6 to 8 hours. It is further preferred that in step e) the incubation of the mixture formed by steps a) to d) is carried out in an aqueous medium at a temperature of about 40° C. for 6 to 8 hours.
[0078] This method of preparing biocompatible hydrogels may also include, together with step e), a step involving thermally induced gelation, which allows the formation of specific form factors, for example, by complete bubble-free filling of a suitably formed template or by dropping a mixture of two non-viscous solutions of the individual components in a lipophilic organic medium to form droplets of defined diameter. The formation of a covalent, non-degradable network of the biocompatible hydrogel can be induced by heating to a mild temperature, as described above, compatible with maintaining the enzyme activity when an enzyme is encapsulated therein. The method may also include crosslinking via 1,3-dipolar cycloaddition, thermal gelation under very mild reaction conditions (for example, 40 ° C in aqueous medium) without side reactions and toxic reagents (for example glutaraldehyde, etc.). Optimization of the pore size of the biocompatible hydrogel is possible by feasible adjustment of the parameters and of the optional degree of carboxymethylation. When the enzymes are added as described in step d), the enzyme(s) are immobilized in the biocompatible hydrogel produced, and the enzyme(s) are then stable and active significantly longer than the free enzymes in solution at ambient or elevated temperatures, e.g., body temperature, 37°C. Unstable sensitive enzymes, such as alcohol oxidase or glucose oxidase, have better longevity performance under these conditions. This embodiment is also applicable to other sensitive enzymes. Such biocompatible hydrogels produced can be stored in a dry state without losing significant amounts of enzyme activity. Furthermore, no or little leaching of the enzymes can be achieved. Such hydrogels prepared according to this method can be suspended in aqueous or organic solvents (e.g., acetone, etc.) while maintaining the enzyme activity. The viscosity of the individual components as well as the mixture can be easily adjusted.
[0079] In one embodiment of the method of preparing a biocompatible hydrogel, the first polysaccharide and the second polysaccharide are independently selected from the group including pullulan, alginic acid, cellulose, hyaluronic acid, dextran, lichenin, lentinan, and mixtures thereof.
[0080] Pullulan is a polysaccharide polymer containing maltotriose units. Three glucose units of maltotriose are connected by α-1,4-glycosidic bonds, and successive maltotriose units are connected to each other by α-1,6-glycosidic bonds. Pullulan may be produced from starch by the fungus Aureobasidium pullulans and may be primarily utilized by cells to resist desiccation and feeding. The presence of this polysaccharide also facilitates the diffusion of molecules both in and out of the cell. In the context of the present invention, the respective monomer repeat units for pullulan are
[0081] [ka] where n is the number of repeating monomer units of the pullulan, and n is an integer from 10 to 10,000.
[0082] Alginic acid, also called algin, is a polysaccharide widely distributed in the cell walls of brown algae; it is hydrophilic and forms a viscous gum when hydrated. Alginic acid is a linear copolymer of homopolymer blocks of (1-4)-linked β-D-mannuronic acid (M) and its C-5 epimer α-L-guluronic acid (G) residues covalently linked together in different sequences or blocks. The monomers may occur in homopolymer blocks of consecutive G residues (G blocks), homopolymer blocks of consecutive M residues (M blocks), or homopolymer blocks of alternating M and G residues (MG blocks). In metals such as sodium and calcium, the salts are known as alginates. In the context of the present invention, the respective monomer repeat units for alginic acid are:
[0083] [ka] where n and m are the number of repeating monomer units of alginic acid, and n and m are each, independently of the other, an integer in the range of 10 to 10,000.
[0084] Hyaluronic acid, also called hyaluronan (abbreviated to HA; conjugate base: hyaluronate), is an anionic, non-sulfated glycosaminoglycan that is widely distributed in connective, epithelial, and neural tissues, and is unique among glycosaminoglycans in that it is non-sulfated, forms in cell membranes instead of the Golgi apparatus, and can become very large. Hyaluronic acid is itself a disaccharide polymer composed of D-glucuronic acid and N-acetyl-D-glucosamine, linked via alternating β-(1→4) and β-(1→3) glycosidic bonds. In the context of the present invention, the respective monomeric repeat units for hyaluronan are:
[0085] [ka] where n is the number of monomer repeat units of the hyaluronan described above, and n is an integer from 10 to 10,000.
[0086] Dextran is a complex branched glucan (polysaccharide resulting from the condensation of glucose). IUPAC defines dextran as "a branched poly-α-D-glucoside of microbial origin with predominantly C-1→C-6 glycosidic bonds". Dextran chains are of different lengths (from 3 to 2000 kilodaltons). The backbone of the polymer contains α-1,6-glycosidic bonds between glucose monomers, with random branching from α-1,3-linkages. This characteristic branching distinguishes dextran from dextrins, which are linear glucose polymers anchored by α-1,4 or α-1,6-linkages. In the context of the present invention, the respective monomer repeat units for dextran are:
[0087] [ka] where n is the number of repeating monomer units of the dextran and n is an integer from 10 to 10,000.
[0088] Lichenin, also known as lichenan or moss starch, is a complex glucan present in certain species of lichens and is chemically a mixed linkage glycan, containing repeating glucose units linked by β-1,3- and β-1,4-glycosidic bonds. In the context of the present invention, the individual monomeric repeat units for lichenin are
[0089] [ka] where n is the number of repeating monomer units of the above lichenin, and n is an integer from 10 to 10,000.
[0090] Lentinan is a polysaccharide isolated from the fruiting body of the shiitake mushroom. Chemically, lentinan is a β-1,3-beta-glucan with β-1,6-branches. For the purposes of the present invention, the individual monomer repeat units for lentinan are:
[0091] [ka] where n is the number of repeating monomer units of the lentinan, and n is an integer from 10 to 10,000.
[0092] In one embodiment of the method for preparing a biocompatible hydrogel, the first and / or second polysaccharide is dextran or pullulan, and carboxymethylation of at least one OH group of dextran or pullulan is carried out in step b). For this embodiment, carboxymethylation of at least one OH group of dextran or pullulan is preferably carried out in step b) at C6 of dextran and / or pullulan. For this embodiment, carboxymethylation of at least one OH group of dextran or pullulan is preferably carried out in step b) at C2 of dextran and / or pullulan. For this embodiment, carboxymethylation of at least one OH group of dextran or pullulan is preferably carried out in step b) at C3 of dextran and / or pullulan. For this embodiment, carboxymethylation of at least one OH group of dextran or pullulan is preferably carried out in step b) at C4 of dextran and / or pullulan.
[0093] In a further embodiment of the method for preparing a biocompatible hydrogel, in step c) the first polysaccharide is functionalized with an A of 0.01 to 1.5 per monomer repeat unit of the first polysaccharide. In a further preferred embodiment of the method for preparing a biocompatible hydrogel, in step c) the first polysaccharide is functionalized with an A of 0.05 to 1.5 per monomer repeat unit of the first polysaccharide. In a further preferred embodiment of the method for preparing a biocompatible hydrogel, in step c) the first polysaccharide is functionalized with an A of 0.05 to 1.0 per monomer repeat unit of the first polysaccharide.
[0094] It is preferred for the method for preparing a biocompatible hydrogel that in step c) the second polysaccharide is functionalized with an A' between 0.01 and 1.5 per monomer repeat unit of the second polysaccharide. In a further preferred embodiment of the method for preparing a biocompatible hydrogel, in step c) the second polysaccharide is functionalized with an A' between 0.05 and 1.5 per monomer repeat unit of the second polysaccharide. In a further preferred embodiment of the method for preparing a biocompatible hydrogel according to the invention, in step c) the second polysaccharide is functionalized with an A' between 0.05 and 1.0 per monomer repeat unit of the second polysaccharide.
[0095] In a further embodiment of the method for preparing a biocompatible hydrogel, in step c) the first polysaccharide is functionalized with an X of 0.01 to 1.5 per monomer repeat unit of the first polysaccharide. In a further preferred embodiment of the method for preparing a biocompatible hydrogel according to the invention, in step c) the first polysaccharide is functionalized with an X of 0.05 to 1.5 per monomer repeat unit of the first polysaccharide. In a further preferred embodiment of the method for preparing a biocompatible hydrogel according to the invention, in step c) the first polysaccharide is functionalized with an X of 0.05 to 1.0 per monomer repeat unit of the first polysaccharide.
[0096] Preferably, in step c) the second polysaccharide is functionalized with a Y of 0.01 to 1.5 per monomer repeat unit of the second polysaccharide. In a further preferred embodiment of the method for preparing a biocompatible hydrogel, in step c) the second polysaccharide is functionalized with a Y of 0.05 to 1.5 per monomer repeat unit of the second polysaccharide. In a further preferred embodiment of the method for preparing a biocompatible hydrogel, in step c) the second polysaccharide is functionalized with a Y of 0.05 to 1.0 per monomer repeat unit of the second polysaccharide.
[0097] In one embodiment of the method of preparing a biocompatible hydrogel, d is 1.
[0098] It is further preferred that for the method of preparing a biocompatible hydrogel, step e) is a thermally induced cycloaddition reaction between X and Y to form a crosslinked polymer.
[0099] In one embodiment of the method for preparing a biocompatible hydrogel, the content of N3 is 0.01-1.5 N3 per monomer repeat unit of the first polysaccharide. In one preferred embodiment of the method for preparing a biocompatible hydrogel, the content of N3 is 0.01-1.0 N3 per monomer repeat unit of the first polysaccharide. In one further preferred embodiment of the method for preparing a biocompatible hydrogel, the content of N3 is 0.1-1.0 N3 per monomer repeat unit of the first polysaccharide.
[0100] In one embodiment of the method for preparing a biocompatible hydrogel, the content of Q is 0.01 to 1.5 per monomer repeat unit of the second polysaccharide. In one preferred embodiment of the method for preparing a biocompatible hydrogel, the content of Q is 0.01 to 1.0 per monomer repeat unit of the second polysaccharide. In one preferred embodiment of the method for preparing a biocompatible hydrogel, the content of Q is 0.1 to 1.0 per monomer repeat unit of the second polysaccharide.
[0101] In one preferred embodiment of the method for preparing a biocompatible hydrogel, in step c), -AX is linked to at least one primary or secondary OH group of the first polysaccharide, preferably via at least one of C2, C3, C4 or C6 of the monomeric repeat unit of the first polysaccharide, more preferably via C6 of the monomeric repeat unit of the first polysaccharide.
[0102] In one preferred embodiment of the method for preparing a biocompatible hydrogel, in step c), -A'-Y is linked to at least one primary or secondary OH group of the second polysaccharide, preferably via at least one of C2, C3, C4, or C6 of the monomeric repeat unit of the second polysaccharide, more preferably via C6 of the monomeric repeat unit of the second polysaccharide.
[0103] It is further preferred for the method of preparing a biocompatible hydrogel that the method does not use toxic reagents, preferably does not use glutaraldehyde.
[0104] In one embodiment of the method for preparing a biocompatible hydrogel, the molecular weight of the non-functionalized first polysaccharide is in the range of 5 to 2000 kDa. In one embodiment of the method for preparing a biocompatible hydrogel, the molecular weight of the functionalized first polysaccharide is in the range of 5 to 2500 kDa. In one preferred embodiment of the method for preparing a biocompatible hydrogel, the molecular weight of the functionalized first polysaccharide is in the range of 5 to 2000 kDa. In one more preferred embodiment of the method for preparing a biocompatible hydrogel, the molecular weight of the functionalized first polysaccharide is in the range of 5 to 1500 kDa. In an even more preferred embodiment of the method for preparing a biocompatible hydrogel, the molecular weight of the functionalized first polysaccharide is in the range of 10 to 1500 kDa.
[0105] In one embodiment of the method for preparing a biocompatible hydrogel, the molecular weight of the non-functionalized second polysaccharide is in the range of 5 to 2000 kDa. In one embodiment of the method for preparing a biocompatible hydrogel, the molecular weight of the functionalized second polysaccharide is in the range of 5 to 2500 kDa. In one preferred embodiment of the method for preparing a biocompatible hydrogel, the molecular weight of the functionalized second polysaccharide is in the range of 5 to 2000 kDa. In one more preferred embodiment of the method for preparing a biocompatible hydrogel, the molecular weight of the functionalized second polysaccharide is in the range of 5 to 1500 kDa. In an even more preferred embodiment of the method for preparing a biocompatible hydrogel, the molecular weight of the functionalized second polysaccharide is in the range of 10 to 1500 kDa.
[0106] The hydrogel can be obtained by any method for preparing a biocompatible hydrogel as described above. Preferably, said hydrogel comprises one or more encapsulated enzymes. More preferably, the hydrogel is a swellable or swollen hydrogel matrix.
[0107] A number of embodiments of the present disclosure have been described. Nevertheless, it will be understood that various modifications can be made without departing from the spirit and scope of the disclosure. Accordingly, other embodiments are within the scope of the following claims.
[0108] The above examples are provided to those of ordinary skill in the art as a complete disclosure and description of how to make and use the embodiments of the present disclosure, and are not intended to limit the scope of what the inventor or inventors regard as their disclosure.
[0109] Modifications of the above-mentioned aspects for implementing the methods and systems disclosed herein that are obvious to those skilled in the art are intended to be within the scope of the appended claims.All patents and publications mentioned in this specification are indicative of the level of skill of those skilled in the art to which this disclosure pertains.All references cited in this disclosure are incorporated by reference to the same extent as if each reference was individually incorporated by reference in its entirety.
[0110] It is to be understood that the present disclosure is not limited to a particular method or system, which may, of course, vary. It is also to be understood that the terminology used herein is for the purpose of describing particular embodiments only, and is not intended to be limiting. As used herein and in the appended claims, the singular forms "a", "an", and "the" include the plural unless expressly indicated otherwise. The term "plurality" includes two or more referents unless expressly indicated otherwise. Unless otherwise specified, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which the present disclosure pertains. It is to be understood that the terms "upper" and "lower" refer to a relative position relative to other elements, and not to an absolute position relative to the ground.
Claims
1. 1. A method of making a biosensor, comprising: Providing a wafer or other solid material having an electrode on a surface thereof; placing a droplet of hydrogel on the electrode; rotating the wafer or other solid material while the wafer is exposed to a partial vacuum; heating the wafer or other solid material while in the aqueous medium for at least one hour; The method includes:
2. The method of claim 1 , wherein the hydrogel comprises pullulan, dextran, alginic acid, hyaluronic acid, or a mixture thereof.
3. The method of claim 1 , wherein the hydrogel comprises pullulan.
4. The method of claim 1 , wherein the electrode is platinum, gold, graphite, titanium, or nanoparticles.
5. The method of claim 1 , wherein the rotation has a maximum speed of up to 10,000 rpm.
6. The method of claim 1 , wherein the rotation proceeds from a lower speed for a first time interval to a higher speed in a second time interval.
7. 7. The method of claim 6, wherein the lower speed is less than 1000 rpm and the higher speed is greater than 1000 rpm.
8. 10. The method of claim 1, wherein the step of heating the wafer comprises heating the wafer to at least 37°C for one hour or more.
9. The method of claim 1 , wherein the hydrogel comprises one or more immobilized enzymes.
10. 10. The method of claim 1, further comprising depositing a further hydrogel layer not containing an enzyme.
11. The method of claim 10, wherein the further hydrogel layer comprises an enzyme from the oxidase family.
12. 12. The method of claim 11, wherein the enzyme from the oxidase family comprises at least one of glucose oxidase, lactate oxidase, uricase oxidase, alcohol oxidase, cortisol oxidase, xanthine oxidase, cholesterol oxidase, sarcosine oxidase.
13. The method of claim 10 further comprising depositing a metal layer over the further hydrogel layer.
14. 10. The method of claim 1, further comprising the step of depositing a metal layer on the hydrogel after the step of heating the wafer.
15. 10. The method of claim 1, wherein the droplets are in the range of 2 μL to 100 μL.
16. The method of claim 1 , wherein the droplet is greater than 100 μL.
17. an electrode including a conductive layer on a substrate layer; a hydrogel layer on the conductive layer; wherein the hydrogel layer is less than 3 micrometers thick and comprises an enzyme immobilized within the hydrogel layer, the hydrogel layer having a covalent, non-degradable network.
18. The biosensor of claim 17 , further comprising a diffusion barrier over the hydrogel layer.
19. The biosensor of claim 18 , wherein the diffusion barrier comprises a metal.
20. 20. The biosensor of claim 18, wherein the diffusion barrier comprises a hydrogel without an immobilized enzyme.
21. 21. The biosensor of claim 20, further comprising a second diffusion barrier over the diffusion barrier, the second diffusion barrier comprising a metal.
22. 22. The biosensor of claim 17, wherein the hydrogel layer has a thickness of 200 to 600 nm.
23. 20. The biosensor of claim 19, wherein the diffusion barrier is 50 to 100 nm thick.
Citation Information
Patent Citations
Analyte sensors having nanostructured electrodes and methods for making and using them
US20090198117A1
Biosensor coating composition and methods thereof
US20090255811A1
Biosensor structures for improved point of care testing and methods of manufacture thereof
US20140262777A1
Metal-enzyme sandwich layers
US20190307378A1
EP21202802.1