Method for determining the height of a foam blanket above an electroplating composition - Patents.com

Radar signal-based measurement of foam height in electroplating compositions addresses the unreliability of light-based methods, ensuring stable foam control and safety in hexavalent chromium processes.

JP2024537722AInactive Publication Date: 2024-10-16ATOTECH DEUT GMBH & CO KG
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2024518478
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-09-23
Filing Date
2022-09-23
Publication Date
2024-10-16
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing methods for determining the height of foam blankets in electroplating compositions, particularly those with colored or thin foams, are unreliable due to strong light absorption and scattering, posing risks from variable foam thickness and mist formation.

Method used

A method using radar signals to measure foam height by generating bubbles in a separate analysis compartment, emitting radar signals, and detecting reflections to determine the foam thickness accurately.

Benefits of technology

Provides reliable and stable foam height measurement, reducing the risk of hydrogen gas accumulation and mist escape, ensuring consistent foam control for hexavalent chromium electroplating compositions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024537722000001
    Figure 2024537722000001
  • Figure 2024537722000002
    Figure 2024537722000002
  • Figure 2024537722000003
    Figure 2024537722000003
Patent Text Reader

Abstract

The present invention relates to a method for determining the height of a foam blanket above an electroplating composition using a radar signal, as well as respective uses.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for determining the height of a foam blanket above an electroplating composition using a radar signal, as well as respective uses. [Background technology]

[0002] Chromium plating has a long history for decorative and functional applications. It started with hexavalent chromium plating, but in the last few decades the development of trivalent chromium plating was started to replace the environmentally questionable hexavalent chromium species. However, hexavalent chromium plating has not been replaced by trivalent chromium plating so far and is still being further developed and improved.

[0003] It is well known that hexavalent chromium plating typically results in the formation of undesirable foaming and mist due to the use of surfactants (also known as surface active compounds) and the vigorous formation of hydrogen gas during plating. Surfactants are typically required to reduce the surface tension and intensively form a foam blanket for the suppression of mist on the respective electroplating composition. However, if out of control, especially if too much surfactant is utilized, foaming can gradually result in a foam blanket with various thicknesses and an overall height that is too high. This is problematic because the foam blanket can entrap large amounts of hydrogen gas in its bubbles. If the excess hydrogen gas is so combined, the risk of explosion is very high.

[0004] Since hexavalent chromium plating is also a health hazard, it is very important to maintain the foam blanket so that it completely covers the electroplating composition so that no mist escapes, and at the same time, is evenly distributed throughout the electroplating bath to the absolutely required thickness.

[0005] It is therefore desirable to control the foam blanket in some way, particularly to keep its height very constant.

[0006] No. 5,597,950(A) relates to an instrument for monitoring the presence or absence of active surfactants or other surface active agents in a solution, which uses a light beam to detect the formation of foam.

[0007] US Patent No. 10,857,486 (B2) relates to an instrument that allows for the continuous measurement of varying foaming tendencies in a fluid system and provides a signal to adjust the defoamer feed rate accordingly to maintain foaming at an acceptable target level. The adjustment of the feed can be accomplished automatically or manually.

[0008] US Patent Application Publication No. 2020 / 353381(A1) relates to a method for managing foam in a gas processing system by automatically controlling the dosage delivery of an antifoam agent during an acid gas removal process.

[0009] However, hexavalent chromium electroplating compositions in particular are very demanding. The bubbles produced in such compositions typically have an orange color due to the presence of chromic acid. This further affects the bubbles such that typical means for determining the bubble height, such as light including laser light, do not adequately allow for proper interaction with the bubbles. In many instances, such light is so absorbed or scattered that no reflected signal is received by the sensor detector.

[0010] Thus, a need exists to provide a further and improved method for determining the height of the foam blanket on electroplating compositions, particularly on hexavalent chromium electroplating compositions. [Prior art documents] [Patent documents]

[0011] [Patent Document 1] U.S. Patent No. 5,597,950(A) [Patent Document 2] U.S. Patent No. 10,857,486 (B2) [Patent Document 3] U.S. Patent Application Publication No. 2020 / 353381(A1) Summary of the Invention [Problem to be solved by the invention]

[0012] It was therefore an object of the present invention to provide an improved method for determining the height of the foam blanket on an electroplating composition that is more universally applicable. This means that it is not only applicable to electroplating compositions that typically have a white (or at least light) foam blanket, but also to more demanding electroplating compositions that have a strongly colored foam blanket, which often have a relatively dense foam blanket (as is the case with hexavalent chromium electroplating compositions). In other words, it is an object to provide an improved method that is more independent of the characteristics of the foam blanket on the electroplating bath and therefore more variably applicable.

[0013] It is a further object of the present invention to provide an improved method that is more generally applicable to electroplating compositions that typically form relatively thin foam blankets. As a general rule, the thinner the foam blanket, the more difficult it is to determine its height. [Means for solving the problem]

[0014] The object of the present invention is to provide a method for determining the height of a foam blanket over an electroplating composition, comprising: (a) providing an electroplating composition in an electroplating compartment; (b) separated from the electroplating compartment; (i) Means for injecting gas; and (ii) Radar emitters and radar sensors Providing an analysis zone comprising: (c) isolating a portion of the electroplating composition and transferring said portion to an analytical compartment such that the analytical compartment is filled with said portion at a constant fill level; (d) contacting the separated portion with a gas so that bubbles are produced with height in the analysis compartment; and (e) projecting a radar signal from a radar emitter onto the generated foam and receiving a reflected radar signal on a radar sensor to determine the height of the foam. The problem is solved by a method including the steps of:

[0015] Own experiments have shown that with a radar signal, preferably as defined throughout the text, most preferably as defined as preferred, even demanding and sophisticated, especially colored, foam blankets can be well monitored and their heights determined consistently (see the examples below). This is particularly useful in the case of hexavalent chromium electroplating compositions. However, the method of the invention is more universally applicable, i.e. also applicable to other electroplating compositions that form and / or require a foam blanket. In particular, it has been shown that radar signals are almost unabsorbed and very strongly reflected, which is very useful for reliable and stable signal detection. In contrast, reliable measurements are not possible with typical prior art means, including light, e.g. laser light, which is too strongly scattered and / or absorbed.

[0016] Own experiments have shown that a carefully controlled and monitored foam blanket, particularly in the case of hexavalent chromium electroplating compositions, provides good environmental protection from toxic hexavalent chromium mists while keeping the risk of excessive hydrogen gas buildup under control.

[0017] Therefore, it is highly desirable to control the foam blanket to prevent (i) under-foaming as well as (ii) over-foaming. In case (i), undesired mists can evaporate and contaminate the environment as well as induce illnesses in people working near such electroplating compositions. In case (ii), a foam blanket that is too thick can accumulate excess hydrogen gas, which dramatically increases the risk of explosion.

[0018] In addition, radar signals are less susceptible to mist and air contamination within the analysis compartment and are more independent of the nature of the generated foam: optical signals, especially laser signals, are easily scattered on their way from the emitter to the generated foam and when they strike the generated foam, whereas radar signals are significantly less susceptible and therefore provide more reliable results. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] In the context of the present invention, the terms "at least one", "one or more" or "one or more than one" refer to (or are interchangeable with) "one, two, three or more" and "one, two, three or more than three", respectively, where appropriate.

[0020] The term "substantially free" refers to an insignificant amount thereof that does not affect the various aspects of the present invention. The term "free" typically refers to the total amount of such compounds and components being below the detection range of prior art measuring equipment, and most preferably being completely absent.

[0021] Electroplating composition in the electroplating compartment: The electroplating composition utilized in the method of the present invention (i.e., prepared in step (a)) is preferably for plating a functional chromium layer. Preferably, in the electroplating compartment, a functional chromium layer, preferably a hard and wear-resistant functional chromium layer, is obtained as a result of each electroplating process.

[0022] In some cases, the electroplating composition utilized in the method of the present invention is preferably for plating a decorative chromium layer, respectively, in the electroplating compartment, preferably a decorative chromium layer is obtained as a result of the electroplating process.

[0023] Unless expressly stated otherwise, the features relating to the methods of the present invention are preferably adapted for functional as well as decorative applications.

[0024] More preferred is the method of the present invention, wherein in step (a), the electroplating composition comprises chromium, preferably a chromium electroplating composition.

[0025] Even more preferred is the method of the present invention, wherein in step (a), the electroplating composition is a trivalent chromium electroplating composition or a hexavalent chromium electroplating composition, preferably a hexavalent chromium electroplating composition.

[0026] Although foam blankets of trivalent chromium electroplating compositions do not exhibit the typical orange color as in the case of foam blankets of hexavalent chromium electroplating compositions, the principles utilized in the method of the present invention are preferably applicable as well.

[0027] In some cases, the methods of the present invention are preferred where the electroplating composition comprises zinc. Thus, preferably, the electroplating composition is a zinc or zinc alloy (e.g., nickel, iron as alloying elements) electroplating composition.

[0028] In some cases, the methods of the present invention are preferred where the electroplating composition comprises aluminum, and thus, preferably, the electroplating composition is an aluminum or aluminum alloy electroplating composition.

[0029] In some cases, the methods of the present invention are preferred where the electroplating composition comprises nickel, and thus, preferably, the electroplating composition is a nickel or nickel alloy electroplating composition.

[0030] In some cases, the methods of the present invention are preferred where the electroplating composition comprises copper, and thus, preferably, the electroplating composition is a copper or copper alloy electroplating composition.

[0031] Preferred is the method of the present invention wherein the electroplating composition is an aqueous electroplating composition, most preferably comprising greater than 50 vol.% water based on the total volume of the electroplating composition.

[0032] Preferred is a method of the invention where the electroplating composition is a chromium electroplating composition, which is acidic or alkaline, preferably acidic, and most preferably acidic, meaning that the pH is preferably 5 or less, more preferably 4 or less, even more preferably 3 or less, even more preferably 2 or less, most preferably 1 or less, and even most preferably 0 or less.

[0033] Foam-forming compounds in electroplating compositions: Preferred is the method of the present invention, wherein the electroplating composition comprises one or more foam-forming compounds, preferably one or more surfactants.

[0034] More preferred is the method of the present invention, wherein the one or more foam producing compounds comprise one or more betaines. More preferably, the one or more betaines are surface active, most preferably providing a surface tension of 40 mN / m or less, preferably 39 mN / m or less, more preferably 37 mN / m or less, based on DI water having a surface tension of 70 mN / m or more. Most preferably, this is based on a concentration of 30 mg / L of said one or more betaines. Preferably, said one or more betaines provide a surface tension of 36 mN / m or more.

[0035] Preferably, one or more betaines contain a quaternary nitrogen. The quaternary nitrogen is preferably positively charged. Most preferably, the positive charge cannot be removed by deprotonation. This means that the positive charge is stable.

[0036] Preferred is a method according to the invention, wherein the quaternary nitrogen has a substituent such that said positive charge is permanently stabilized, with the proviso that said substituent is not hydrogen. Preferably, said substituent comprises at least an organic residue, preferably an alkyl residue, an ester residue, a carboxyalkyl residue, and / or an amide residue. Preferably, the alkyl residue, the ester residue, the carboxyalkyl residue and the amide residue each individually comprise from 1 to 20 carbon atoms.

[0037] Preferably, the one or more betaines independently further comprise a sulfonic acid group and / or a carboxylate group, preferably a sulfonic acid group, said groups being preferably negatively charged.

[0038] Preferred is a method according to the invention, wherein the one or more betaines have a net neutral charge.

[0039] Preferred is the process of the invention, wherein the one or more betaines independently comprise at least 5 carbon atoms, preferably at least 7 carbon atoms, more preferably at least 9 carbon atoms, even more preferably at least 11 carbon atoms, even more preferably at least 12 carbon atoms, and most preferably at least 14 carbon atoms. Preferably, the one or more betaines have 50 or less carbon atoms.

[0040] Preferably, the one or more betaines comprise at least one compound of formula (I) (R 1 )N+(R 2 R 3 )-XY (I) (Wherein, independently, R 1 represents alkyl, alkyl ester or alkyl amide, preferably alkyl, R 2 and R 3 represents a C1 to C5 linear or branched alkyl, preferably a C1 to C5 linear alkyl, X represents a divalent moiety; Y represents a sulfonic acid group or a carboxylic acid group, preferably a sulfonic acid group. The method of the present invention comprises:

[0041] Preferably, R 1 is branched or linear, preferably linear.

[0042] Preferably, R 1 contains 4 to 26, preferably 6 to 24, more preferably 8 to 20, and most preferably 12 to 18 carbon atoms. 1 contains 18 carbon atoms.

[0043] Preferably, R 2 and R 3 independently contain 1 to 4 carbon atoms, preferably 1 to 3 carbon atoms, more preferably 1 or 2 carbon atoms, and most preferably 1 carbon atom.

[0044] Preferably, X contains from 1 to 8 carbon atoms, preferably from 1 to 6 carbon atoms, more preferably from 2 to 4 carbon atoms, and most preferably 3 or 4 carbon atoms.

[0045] More preferably, X represents an alkylene, hydroxy-alkylene or alkoxylene moiety, preferably an alkylene moiety. Most preferably, X represents propylene, preferably linear propylene.

[0046] Preferred are, independently: R 1 represents a C16 to C18 linear alkyl, preferably a C18 linear alkyl; R 2 and R 3 represents methyl or ethyl, preferably methyl, X represents a C2-C4 alkylene moiety, preferably a C3 alkylene moiety; The method of the present invention, wherein Y represents a sulfonic acid group.

[0047] More preferred is the method of the invention, wherein said one or more betaines are sulfobetaines.

[0048] Even more preferred is when the one or more foam producing compounds, most preferably the one or more betaines, are at least N,N-dimethyl-N-(3-cocoamidopropyl)-N-(2-hydroxy-3-sulfopropyl)ammonium betaine, N-dodecyl-N,N-dimethyl-3-ammonio-1-propanesulfonate, N-octyl-N,N-dimethyl-3-ammonio-1-propanesulfonate, N- ... , N-dodecyl-N,N-dimethyl-3-ammonio-1-propanesulfonate, N-tetradecyl-N,N-dimethyl-3-ammonio-1-propanesulfonate, N-hexadecyl-N,N-dimethyl-3-ammonio-1-propanesulfonate, N-octadecyl-N,N-dimethyl-3-ammonio-1-propanesulfonate and N,N-dimethyl-N-dodecylglycine betaine.

[0049] Preferred is the method of the present invention, wherein the one or more foam-forming compounds, most preferably the one or more betaines, have a total concentration ranging from 0.0005 g / L to 1 g / L, preferably 0.001 g / L to 0.5 g / L, more preferably 0.005 g / L to 0.3 g / L, and most preferably 0.01 g / L to 0.2 g / L, based on the total volume of the electroplating composition.

[0050] Preferred is the process of the present invention, wherein the one or more foam-producing compounds do not contain fluorine atoms, in other words, the one or more foam-producing compounds are not fluorinated, not perfluorinated, but rather do not contain fluorine.

[0051] The one or more foam-forming compounds described above preferably form a foam blanket over the electroplating composition, similar to the foam produced in step (d).

[0052] Antifoam Compounds in Electroplating Compositions: Preferred is the method of the present invention, wherein the electroplating composition further comprises one or more antifoam compounds, preferably one or more organosiloxanes, most preferably one or more polyorganosiloxanes. Thus, the preferred organosiloxanes and polyorganosiloxanes are each preferred antifoam compounds.

[0053] In the context of the present invention, the one or more foam-producing compounds and the one or more anti-foam compounds are distinct from one another.

[0054] The antifoam compound preferably represents a means for controlling the thickness and density of the foam blanket, and thus is not only a means for countering overdosing of one or more foam-producing compounds, but also a means for controlling the density of the foam, preferably by affecting the size of the bubbles in the foam blanket.

[0055] Preferably, the one or more polyorganosiloxanes are crosslinked, more preferably crosslinked in at least two dimensions, and most preferably crosslinked in three dimensions.

[0056] Preferably, the one or more polyorganosiloxanes are crosslinked through vinyl moieties.

[0057] Preferred is the process of the present invention, wherein in the electroplating composition one or more polyorganosiloxanes are 3D siloxanes, i.e. 3D polyorganosiloxanes, which are available, for example, from Munzing Chemie GmbH.

[0058] More preferably, the one or more antifoam compounds, more preferably the one or more polyorganosiloxanes, are surface active, and most preferably the one or more antifoam compounds, preferably the one or more polyorganosiloxanes, are themselves less surface active than said one or more foam-producing compounds, preferably said one or more betaines, in terms of reducing surface tension relative to water without any surface active compound.

[0059] Most preferably, the one or more polyorganosiloxanes and the one or more betaines are synergistically more surface active together than each by itself in terms of reducing surface tension relative to water without any surface active compounds.

[0060] Preferably, the one or more antifoam compounds, more preferably the one or more polyorganosiloxanes, are non-ionic.

[0061] Preferred is the method of the invention, wherein the antifoam compound, preferably the one or more polyorganosiloxanes, in the electroplating composition has a total concentration of 0.01 mg / L to 5000 mg / L, preferably 0.05 mg / L to 3000 mg / L, more preferably 0.1 mg / L to 1500 mg / L, even more preferably 0.15 mg / L to 1000 mg / L, still even more preferably 0.2 mg / L to 500 mg / L, and most preferably 0.25 mg / L to 150 mg / L, based on the total volume of the electroplating composition.

[0062] More preferred is the method of the present invention, wherein the antifoam compound, preferably the one or more polyorganosiloxanes, in the electroplating composition has a total concentration of 0.01 mg / L to 100 mg / L, preferably 0.05 mg / L to 70 mg / L, more preferably 0.1 mg / L to 50 mg / L, even more preferably 0.15 mg / L to 25 mg / L, still even more preferably 0.2 mg / L to 10 mg / L, and most preferably 0.3 mg / L to 5 mg / L, based on the total volume of the electroplating composition.

[0063] Preferably, one or more polyorganosiloxanes contain one or more, preferably more than one, vinyl moiety.More preferably, one or more polyorganosiloxanes contain at least one vinyl moiety that contains unsaturated double bond, while other vinyl moieties participate in crosslinking such that their double bond is no longer present.This preferably means that the polyorganosiloxanes utilized in the method of the present invention are partially crosslinked through vinyl moiety, but not all vinyl moieties are used in crosslinking.

[0064] Preferably, the one or more antifoam compounds, more preferably the one or more polyorganosiloxanes, comprise, preferably consist of, carbon, hydrogen, silicon and oxygen atoms.

[0065] Preferably, the one or more antifoam compounds, more preferably the one or more polyorganosiloxanes, do not contain nitrogen atoms.

[0066] Preferably, the one or more antifoam compounds, more preferably the one or more polyorganosiloxanes, do not contain sulfur atoms.

[0067] Preferably, the one or more antifoam compounds, more preferably the one or more polyorganosiloxanes, do not contain fluorine atoms, in other words, the one or more polyorganosiloxanes are not fluorinated and not perfluorinated.

[0068] Further compounds and properties in electroplating compositions; Preferred is the method of the present invention, wherein the electroplating composition further comprises at least one emulsifier, which preferably emulsifies the one or more antifoam compounds, and more preferably the one or more polyorganosiloxanes, in the electroplating composition. Thus, the emulsifier is preferably for emulsifying the one or more polyorganosiloxanes in the aqueous solution.

[0069] Preferably, the electroplating composition does not exhibit any phase separation, floating surface droplets, surface film formation of oil, and / or density gradients.

[0070] In some cases, preferred is a method of the present invention in which the electroplating composition is substantially free, and preferably free, of polydimethylsiloxane, and most preferably substantially free, and preferably free, of silicone oil, although in some other cases this may be preferred.

[0071] The combination of one or more foam-forming compounds and one or more antifoam compounds described above effects the surface tension of the electroplating composition in terms of the overall average surface tension.

[0072] Preferred is a method of the present invention where the electroplating composition has a surface tension of 50 mN / m or less, preferably 45 mN / m or less, more preferably 40 mN / m or less, even more preferably 38 mN / m or less, even more preferably 36 mN / m or less, and most preferably 35 mN / m or less, as measured with a tensiometer. In some cases, most preferably 34 mN / m or less or 33 mN / m or less. In the context of the present invention, it is most preferred to utilize a Wilhelmy plate in the tensiometer to determine the surface tension.

[0073] More preferred is the method of the present invention, wherein the electroplating composition has a surface tension ranging from 28 mN / m to 40 mN / m, preferably from 30 mN / m to 38 mN / m, and most preferably from 31 mN / m to 36 mN / m, based on measurement with a surface tensiometer.

[0074] Preferred is the method of the present invention, wherein the foam blanket on the electroplating composition in the electroplating compartment covers more than 50% of the coatable surface of the electroplating composition with said foam blanket having a thickness preferably ranging from 0.5 cm to 6 cm, preferably 1 cm to 3 cm, which is suitable for both functional and decorative applications.

[0075] More preferred is the method of the present invention, wherein the foam blanket over the electroplating composition in the electroplating compartment covers more than 60% of the coatable surface of the electroplating composition with said foam blanket, preferably more than 70%, even more preferably more than 80%, even more preferably more than 90%, most preferably more than 95%, and even most preferably entirely, of the coatable surface of the electroplating composition with said foam blanket. This is most preferably accommodated with preferred foam blanket heights ranging from 0.5 cm to 6 cm, preferably 1 cm to 3 cm. This is accommodated for both functional and decorative applications.

[0076] Preferred is the method of the present invention, wherein the electroplating composition further comprises sulfate ions, preferably in a concentration ranging from 0.1 g / L to 10 g / L, preferably from 1 g / L to 8.5 g / L, more preferably from 1.5 g / L to 7.5 g / L, even more preferably from 2 g / L to 6.5 g / L, and most preferably from 3 g / L to 5 g / L based on the total volume of the electroplating composition.

[0077] Preferred is the method of the present invention, wherein the electroplating composition comprises one or more sulfonic acids and / or salts thereof having two, three or more sulfonic acid groups, preferably one or more alkylsulfonic acids and / or salts thereof having two, three or more sulfonic acid groups.

[0078] Preferred is the method of the present invention, wherein the electroplating composition further optionally comprises silver ions, preferably at a total concentration ranging from 0.0001 g / L to 3 g / L, preferably 0.001 g / L to 1 g / L, most preferably 0.01 g / L to 0.3 g / L, based on the total volume of the electroplating composition, which is most preferably suitable for functional applications.

[0079] Preferred is the method of the present invention wherein the electroplating composition is substantially free, preferably free, and most preferably substantially free, preferably free, of fluorinated organic compounds.

[0080] However, this does not preclude the use of inorganic fluorine compounds that are significantly less problematic, such as fluoride anions. Preferred therefore are methods of the present invention in which, in some cases, the electroplating composition further comprises fluoride anions, which are most preferably suited for decorative applications.

[0081] Preferred is the method of the present invention, wherein the electroplating composition further comprises a fluorine-containing inorganic compound, preferably a fluoro-silicate, most preferably SiF6, which is most preferably suited for decorative applications to increase the gloss and uniformity of the respective decorative chrome layer, thus improving the visual appearance.

[0082] Preferably, the fluorine-containing inorganic compounds (preferably fluoro-silicates, most preferably SiF6) have a total concentration ranging from 0.2 g / L to 2 g / L based on the total volume of the electroplating composition.

[0083] Analysis section and method for determining foam blanket height: The method of the present invention is for determining the height of a foam blanket above an electroplating composition, preferably an electroplating composition as defined above.

[0084] Preferably, the electroplating composition in the electroplating compartment has a foam blanket. In the context of the present invention, the foam generated in step (d) of the method of the present invention represents a foam blanket that is present or can be obtained upon application of the electroplating composition in the electroplating compartment (i.e., upon electroplating a substrate). In fact, the method of the present invention preferably does not rely on any active application of the electroplating composition. This means that the height of the foam blanket can be determined even when the electroplating composition is not being used in the electroplating compartment.

[0085] Preferably, the analysis compartment has a certain size or dimension so that the generated foam has enough space to form a form-stable foam blanket. Preferably, the separated electroplating composition has an area of ​​at least 100 cm. 2 , preferably at least 150 cm 2 , more preferably at least 200 cm 2 , most preferably at least 220 cm 2 Preferably, the surface area is 100 cm 2 ~1000cm 2 , more preferably 150 cm 2 ~800cm 2 , more preferably 200 cm 2 ~600cm 2 , most preferably 220 cm 2 ~400cm 2 The range is as follows:

[0086] The analysis compartment is separated from the electroplating compartment and contains (i) a means for injecting a gas.

[0087] Preferred is the process of the invention, wherein in step (b) the means for injecting gas comprises a valve, preferably a ball valve or a needle valve, most preferably a needle valve, which is designed to pass gas, preferably under pressure, most preferably a needle valve to obtain a high precision gas passing fraction.

[0088] Basically, the gas can be any gas, as long as it is appropriate in the context of the entire method, including the electroplating process. However, preferred is the method of the present invention, in which in step (b) the gas comprises an inert gas and / or ambient air, preferably ambient air. A preferred inert gas comprises nitrogen, preferably nitrogen gas. An inert gas offers the advantage that no oxidative interaction with the electroplating composition occurs. This is particularly relevant when the separated parts are returned to the electroplating compartment. In contrast, ambient air is widely available and cost-effective, but its oxygen can have an oxidative effect. However, it typically serves well for the purposes of the method of the present invention and is therefore highly preferred.

[0089] Preferred is the process of the invention, wherein in step (d) the gas is blown in at a flow rate ranging from 0.1 L / h to 7 L / h (expressed in liters per hour), preferably from 0.4 L / h to 5.5 L / h, more preferably from 0.6 L / h to 4 L / h, even more preferably from 0.9 L / h to 3 L / h, most preferably from 1 L / h to 2.5 L / h. Each of the respective equipments is applicable.

[0090] Preferred is the method of the invention, wherein the analytical compartment comprises a filter, preferably a glass filter. Most preferably, said filter is arranged such that at least a gas blowing is blown through said filter to generate bubbles in step (d). Most preferably, the filter is solid.

[0091] The analytical compartment further preferably comprises a pipe for transferring a portion of the electroplating composition to the analytical compartment. More preferably, the pipe is regulated with respect to flow rate. Most preferably, the pipe is connected to a pump such that said portion of the electroplating composition reaches the analytical compartment, preferably with the aid of pressure. Preferably, the pump is a diaphragm pump. Thus, said separated portion is preferably actively transferred to the analytical compartment. Most preferably, the separated portion is transferred at a constant flow rate.

[0092] Preferred is a process according to the invention, wherein in step (c) the portions are separated continuously or at intervals, preferably continuously.

[0093] More preferred is a process according to the invention, wherein steps (c) to (e) of the process according to the invention are carried out continuously, ie preferably repeatedly.

[0094] Most preferred is a method according to the invention, wherein the entire method according to the invention is carried out continuously, ie preferably iteratively.

[0095] Preferred is a method according to the invention, wherein in step (c) said portion is transferred to the analytical compartment at a flow rate ranging from 0.5 L / h to 10 L / h (expressed in liters per hour), preferably from 1 L / h to 9 L / h, more preferably from 2 L / h to 8 L / h, even more preferably from 3 L / h to 7 L / h, most preferably from 4 L / h to 6 L / h. Each instrument is adapted to the respective one.

[0096] During the transfer of the separated portion to the analytical compartment, the analytical compartment is filled to a certain level in said portion, which is maintained throughout the method. Thus, the analytical compartment has a constant filling level. Preferably, this constant filling level is obtained by using an overflow, which allows the return of excess electroplating composition to the electroplating compartment. Thus, preferred is a method of the invention, wherein the analytical compartment comprises an overflow, preferably fluidly connected with the electroplating compartment.

[0097] An essential feature in the analysis section is (ii) a radar emitter and a radar sensor. It has been found that these instruments can meet the technical demands, most particularly for relatively thin foam height, even for hexavalent chromium electroplating compositions. Moreover, such emitters and sensors, respectively, can be utilized to determine foam blanket height over other electroplating compositions, and even other than chromium electroplating compositions.

[0098] Preferred is a method according to the invention, wherein a radar emitter is positioned above the foam produced in step (d).

[0099] Preferred is a method of the present invention where the radar emitter radiates the radar signal perpendicularly onto the generated foam, most preferably perpendicular and at a right angle to the generated foam.

[0100] Most preferred is a method of the present invention wherein in step (b) the radar emitter is positioned above the foam and in step (e) the radar signal is emitted perpendicularly, at right angles to the foam.

[0101] Preferred is a method of the invention, wherein in step (e) the emitted radar signal has a frequency ranging from 10 GHz to 150 GHz, preferably from 20 GHz to 125 GHz, more preferably from 35 GHz to 110 GHz, even more preferably from 50 GHz to 100 GHz, even more preferably from 60 GHz to 95 GHz, most preferably from 70 GHz to 90 GHz, even more preferably from 75 GHz to 85 GHz, and a radar emitter is respectively adapted to provide such a signal.

[0102] In some cases, preferred is a method of the invention, wherein the radar signal emitted in step (e) has a frequency ranging from 75 GHz to 110 GHz, preferably from 77 GHz to 100 GHz, more preferably from 79 GHz to 90 GHz, and the radar emitter is adapted to provide such a signal, respectively.

[0103] Preferred is the method of the invention, in which the emitted radar signal in step (e) is the basis for the distance measurement, preferably for the distance measurement based on surface area. This is a major advantage over commonly known measurements, such as those by laser, which typically only include small area points and are therefore sensitive to local variations in the generated foam. In contrast, the emitted radar signal typically includes a larger surface area and therefore provides a reflected radar signal based on surface area as the reaction signal.

[0104] Upon reaching the generated foam, the emitted radar signal is typically reflected and / or scattered. At least a portion of it is reflected back onto the radar sensor, most preferably without significant change in frequency. In the context of the present invention, the term "radar sensor" corresponds to (and is interchangeable with) the terms "radar detector" or "radar signal detector."

[0105] The height of the generated foam is determined by correlating with the constant filling level, which is a fixed height information due to overflow, and the reflected radar signal, which provides another height information. By determining the difference, the height of the generated foam and the foam blanket, respectively, is most preferably determined. Thus, in the context of the present invention, the terms "height" of the foam blanket and "height" of the generated foam mean (and are preferably interchangeable with) its thickness. Generally, in the context of the present invention, the height is preferably determined directly by the radar, most preferably measured directly thereby.

[0106] Preferred in some cases is a method of the present invention wherein in step (e) the emitted radar signal and the reflected radar signal have the same frequency within a variation range delta of ±3%.

[0107] Preferably, the height of the foam blanket above the electroplating composition present in the electroplating compartment ranges from 0.5 cm to 6 cm, preferably from 0.7 cm to 5 cm, more preferably from 0.9 cm to 4 cm, and most preferably from 1 cm to 3 cm. Most preferably, in the analysis compartment, the foam generated is of substantially the same height, thus representing a foam blanket in the electroplating composition. This is typically ensured by adjusting the flow rate of the gas blowing. Thus, preferred is a method of the invention, wherein in step (e), the foam has a height ranging from 0.5 cm to 6 cm, preferably from 0.7 cm to 5 cm, more preferably from 0.9 cm to 4 cm, and most preferably from 1 cm to 3 cm.

[0108] Since the desired height of the generated foam and foam blanket, respectively, are typically known, the determined height of the generated foam preferably informs whether additional foam-generating or anti-foaming compounds are required and therefore must be added to the electroplating composition. (f) adding one or more foam-generating compounds or one or more antifoaming compounds to the electroplating composition. The method of the present invention further comprises:

[0109] More preferred is a process according to the invention, wherein the addition in step (f) is carried out by means of one or more pumps.

[0110] Most preferred is a method of the invention that is automated. Preferred is therefore a method of the invention, where the addition in step (f) is controlled by a computing device, preferably a computing device in communication with at least a radar sensor. Typically, the radar sensor generates an output signal that is calculated in the computing device to determine (i.e. obtain) the height of the generated foam. Based on this foam height, the computing device communicates, preferably by a control signal, with preferably one or more pumps.

[0111] Preferred is the method of the present invention, wherein in step (f) one or more foam-generating compounds are added by a first pump for pumping said one or more foam-generating compounds from a first reservoir comprising said one or more foam-generating compounds into the electroplating compartment.Also preferred is the method of the present invention, wherein in step (f) one or more anti-foam compounds are added by a second pump for pumping said one or more anti-foam compounds from a second reservoir comprising said one or more anti-foam compounds into the electroplating compartment.

[0112] Most preferably, the computing device individually switches on or off the one or more pumps, most preferably the first and second pumps, and preferably also individually controls their flow rates. In that way, the ratio between the one or more foam-producing compounds and the one or more anti-foam compounds can be manipulated and adjusted to a desired degree. All this allows for careful control of the height of the foam blanket above the electroplating composition.

[0113] Preferably, the control signal is an analog control signal or a digital control signal, preferably an analog control signal. More preferably, the analog control signal comprises current information or voltage information. Preferably, the analog control signal is split into two individual signals that are different from each other, preferably a first analog control signal and a second analog control signal, most preferably a first analog control signal for the first pump and a second analog control signal for the second pump. Most preferably, the analog control signals are transmitted via a cable.

[0114] In some cases however the method of the present invention is preferred, wherein the control signal is a digital control signal, preferably transmitted wirelessly, preferably via WLAN and / or Bluetooth, most preferably via Bluetooth.

[0115] As mentioned above, the electroplating composition preferably already contains one or more fluorine-free foam-forming compounds, and preferably further contains one or more fluorine-free antifoam compounds. Therefore, it is also preferred that the corresponding compounds are added in step (f). Therefore, preferred is the method of the present invention, in which the one or more foam-forming compounds and the one or more antifoam compounds in step (f) do not contain fluorine atoms.

[0116] In case the foam-generating and antifoaming compounds do not contain any fluorine atoms, an analysis compartment, preferably having a (preferably automatic) dosing unit, is highly preferred. Typically, fluorinated / perfluorinated compounds have been used in the past, which show relatively high inherent resistance to very harsh electroplating composition conditions. However, these are becoming more and more often banned and therefore must be replaced by alternative compounds. In many cases, such compounds are less resistant and therefore more susceptible to degradation. As a result, more frequent dosing is required to maintain a constant total concentration of such compounds and the corresponding foam blanket. Therefore, automated monitoring / dosing is helpful, highly efficient, and most preferred.

[0117] What has been said above in relation to the one or more foam-producing compounds and the one or more antifoam compounds preferably applies equally to the one or more foam-producing compounds and the one or more antifoam compounds added in step (f). More preferred is the process of the invention, in which in step (f) the one or more foam-producing compounds comprise one or more betaines and the one or more antifoam compounds comprise one or more organosiloxanes. In particular, what has been said above in relation to the one or more betaines and the one or more organosiloxanes preferably applies equally to the respective compounds added in step (f).

[0118] The present invention further relates to the use of radar signals to determine the height (i.e., thickness) of a foam blanket over a hexavalent chromium electroplating composition.

[0119] What has been said above in relation to the method of the invention preferably applies equally to the use of the invention.

[0120] The present invention further relates to an instrument for determining the height of bubbles on an electroplating composition, the instrument comprising a radar emitter, a radar sensor and an analysis compartment with an overflow to provide a constant fill level.

[0121] What has been said above in relation to the method of the invention preferably applies analogously to the device of the invention.

[0122] The present invention will now be described in more detail by the following non-limiting examples. EXAMPLES

[0123] The following electroplating compositions were used in the electroplating compartment: (i) Chromic acid, 250 g / L; (ii) N-octadecyl-N,N-dimethyl-3-ammonio-1-propanesulfonate as a foam-forming compound; (iii) as antifoaming compound, emulsified and homogeneously distributed 3D-polyorganosiloxane (i.e. 3D Siloxane from Munzing Chemie GmbH), (iv) sulfate ion, 2-5 g / L (added as sulfuric acid); (v) methane-disulfonic acid, 1.5-10 g / L; pH Strongly acidic

[0124] A portion of the electroplating composition was continuously separated and transferred (5 L / h) to an analytical compartment designed as a separate unit, which was equipped with a pipe fluidly connecting it to the electroplating compartment so that said portion of the electroplating composition could reach the analytical compartment with the aid of an electrical diaphragm pump.

[0125] The analytical compartment was further equipped with an overflow to maintain a constant fill level in the analytical compartment. Excess electroplating composition was returned to the electroplating compartment.

[0126] The analytical compartment was further equipped with a needle valve as a means for infusing gas, in this particular example ambient air. Flow rates ranging from 0.5 L / h to 4 L / h were tested, with a range of 1 L / h to 2 L / h determined to be optimal. With the assistance of ambient air, bubbles were continuously generated at a certain height in the analytical compartment.

[0127] A radar emitter (80 GHz; VEGAPULS C 21) containing a radar sensor is used on the generated foam, the emitted and reflected radar signals are conducted perpendicular and at right angles to the generated foam formed on the surface of the separated part through the surrounding air.

[0128] The foam produced had a continuous height of about 1 cm. This was obtained using a constant flow of foam-producing compound at 0.15 mL / L / h (based on the total volume of the electroplating composition) in combination with a constant flow of antifoam compound at 0.075 mL / L / h (based on the total volume of the electroplating composition). It has been found that such continuous and low volume dosing is quite well achieved by the method of the present invention. In that way, the continuous decomposition of the fluorine-free organic compound is compensated for without compromising the stable foam blanket in the electroplating compartment.

[0129] The computing device was in electrical communication with the radar emitter and / or radar sensor to automatically control a first pump for adding a foam generating compound and a second pump for adding an antifoam compound to the electroplating composition. The computing device was preferably already incorporated into the housing of the radar emitter (VEGAPULS).

[0130] In the electroplating section, electroplating was performed using a steel substrate (rod) at approximately 50 A / dm 2at a current density of about 1000 s, at a temperature of about 55° C., and for about 5 to 7 hours to obtain hard and wear-resistant chromium layers, respectively.

[0131] The foam produced on the separated portion of the electroplating composition closely corresponded (i.e., had the same height) to the foam blanket present above the electroplating composition in the electroplating compartment.

[0132] It is an additional advantage that the foam blanket height can still be determined even when the electroplating composition in the electroplating compartment is not being actively utilized, and reliable information about the ratio between foam-forming and antifoaming compounds can still be obtained since only a small portion of the electroplating composition is required for the analysis compartment.

[0133] In a comparative example, the radar emitter was replaced by a laser, but no reliable information was detected: it is assumed that the laser provides an overly focused beam, which is not in a position to reliably detect the overall condition on the surface of the separated part.

Claims

1. 1. A method for determining the height of a foam blanket over an electroplating composition, comprising: (a) providing the electroplating composition in an electroplating compartment; (b) separated from the electroplating compartment; (i) a means for injecting gas; and (ii) Radar emitters and radar sensors Providing an analysis zone comprising: (c) separating a portion of said electroplating composition and transferring said portion to an analytical compartment such that said analytical compartment is filled with said portion at a constant fill level; (d) contacting the separated portion with the gas so as to produce a foam with height in the analytical compartment; and (e) emitting a radar signal from the radar emitter onto the created bubble and receiving a reflected radar signal on the radar sensor to determine a height of the bubble. The method includes:

2. 2. The method of claim 1, wherein in step (a), the electroplating composition is a trivalent chromium electroplating composition or a hexavalent chromium electroplating composition, preferably a hexavalent chromium electroplating composition.

3. 3. The method according to claim 1 or 2, wherein in step (b), the means for injecting gas comprises a valve, preferably a ball valve or a needle valve, most preferably a needle valve.

4. 4. The method according to any one of claims 1 to 3, wherein in step (b) the gas comprises an inert gas and / or ambient air, preferably ambient air.

5. 5. The method of claim 1, wherein in step (b), the radar emitter is positioned above the bubble, and in step (e), the radar signal is emitted perpendicularly, perpendicular to the bubble.

6. 6. The method according to any one of claims 1 to 5, wherein in step (c) the portions are separated continuously or at intervals, preferably continuously.

7. 7. The process according to any one of claims 1 to 6, wherein in step (d), the gas is injected at a flow rate ranging from 0.1 L / h to 7 L / h, preferably from 0.4 L / h to 5.5 L / h, more preferably from 0.6 L / h to 4 L / h, even more preferably from 0.9 L / h to 3 L / h, and most preferably from 1 L / h to 2.5 L / h.

8. 8. The method according to any one of claims 1 to 7, wherein in step (e), the emitted radar signal has a frequency ranging from 10 GHz to 150 GHz, preferably from 20 GHz to 125 GHz, more preferably from 35 GHz to 110 GHz, even more preferably from 50 GHz to 100 GHz, even more preferably from 60 GHz to 95 GHz, most preferably from 70 GHz to 90 GHz, even more preferably from 75 GHz to 85 GHz.

9. 9. The method according to any one of claims 1 to 8, wherein in step (e) the emitted radar signal is a reference for distance measurements, preferably for surface area based distance measurements.

10. 10. The method according to any one of claims 1 to 9, wherein in step (e), the foam has a height ranging from 0.5cm to 6cm, preferably from 0.7cm to 5cm, more preferably from 0.9cm to 4cm, and most preferably from 1cm to 3cm.

11. (f) adding one or more foam-forming compounds or one or more antifoam compounds to the electroplating composition.

10. The method of claim 1, further comprising:

12. 12. The method of claim 11, wherein in step (f), the one or more foam-producing compounds and the one or more anti-foam compounds do not contain fluorine atoms.

13. 13. The method of claim 11 or 12, wherein in step (f), the one or more foam-producing compounds comprise one or more betaines and the one or more anti-foam compounds comprise one or more organosiloxanes.

14. Use of a radar signal to determine the height of a foam blanket above a hexavalent chromium electroplating composition.

15. An apparatus for determining the height of bubbles on an electroplating composition comprising a radar emitter, a radar sensor and an analytical compartment with an overflow to provide a constant fill level.

Citation Information

Patent Citations

  • US10,857,486B2

  • Managing Foam In Gas Processing Systems

    US20200353381A1

  • Surfactant monitoring by foam generation

    US5597950A