Low-flow polymeric compositions containing acrylonitrile-butadiene-styrene copolymers and terpolymers, and method for reducing the flow properties of acrylonitrile-butadiene-styrene copolymers
A low fluidity polymer composition with acrylonitrile-butadiene-styrene copolymer and ethylene-based terpolymer addresses the challenges of recycling ABS by reducing melt flow index and enhancing impact strength, enabling efficient extrusion molding and high-quality product production.
Patent Information
- Application Number
- JP2024532342
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-12-09
- Filing Date
- 2022-11-25
- Publication Date
- 2024-11-21
AI Technical Summary
Existing acrylonitrile-butadiene-styrene (ABS) polymers face challenges in recycling due to reduced impact strength and high melt flow index, which complicates extrusion molding and affects the quality of recycled products.
A low fluidity polymer composition comprising an acrylonitrile-butadiene-styrene copolymer and a terpolymer with repeating units derived from ethylene and glycidyl groups is developed, reducing melt flow index and enhancing impact strength.
The composition achieves improved workability and impact strength in extrusion molding, producing high-quality molded articles with reduced fluidity, suitable for sheet and profile extrusion.
Smart Images

Figure 2024543570000001 
Figure 2024543570000002 
Figure 2024543570000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to low flow polymeric compositions comprising acrylonitrile-butadiene-styrene copolymers and terpolymers, and to a method for reducing the flow of acrylonitrile-butadiene-styrene copolymers. [Background technology]
[0002] Acrylonitrile-butadiene-styrene copolymer (ABS) has advantages such as excellent chemical resistance, dimensional stability, and processability, and is used in a wide range of fields such as washing machines, TVs, refrigerators, monitors, copiers, facsimiles, automobile side mirrors, mobile phone cases, toy materials, and game consoles.
[0003] There are various methods for molding the ABS, but the above-mentioned example products can usually be manufactured by injection molding. One of the important factors in such molding step is the melt flow index (MFI), which means the viscosity of the molten polymer, and injection molding usually uses a polymer composition with a high melt flow index, i.e., good fluidity.
[0004] On the other hand, as interest in eco-friendliness grows, the demand for recycling plastics is also increasing, and similarly, much research and development is being conducted on the recycling of ABS. However, when recycling ABS, there is a problem that the impact strength decreases, and in particular, when recycling the above-mentioned injection molded products, the melt flow index is so high that other molding methods such as sheet or profile extrusion molding cannot be used.
[0005] In addition, since ABS is inferior in impact strength compared to other thermoplastic polymers, the impact strength of ABS may be improved by adding an impact modifier, etc. However, the addition of such additives reduces the viscosity and has an increased melt flow index, which leads to problems of reduced workability during extrusion molding and reduced quality of the molded product.
[0006] Therefore, there is a need for research and development of a polymer composition having improved impact strength, reduced fluidity, and a melt flow index that is advantageous for extrusion molding. Summary of the Invention [Problem to be solved by the invention]
[0007] It is an object of the present invention to provide low flow polymeric compositions comprising acrylonitrile-butadiene-styrene copolymers and terpolymers.
[0008] Another object of the present invention is to provide a polymer composition suitable for molding methods requiring a low melt flow index, such as sheet and profile extrusion molding, by imparting low flowability to the polymer composition by including a terpolymer in an acrylonitrile-butadiene-styrene copolymer. In addition, the low flowability polymer composition can provide a high quality molded product having improved workability and improved impact strength. [Means for solving the problem]
[0009] In order to solve the above problems, the present inventors have found that when a polymer composition contains an acrylonitrile-butadiene-styrene copolymer and a terpolymer containing a first repeating unit derived from ethylene and a second repeating unit containing a glycidyl group, not only the melt flow index of the polymer composition is effectively reduced, but also a molded article having improved impact strength can be produced using the polymer composition, thereby completing the present invention.
[0010] The present disclosure provides a low flow polymeric composition comprising an acrylonitrile-butadiene-styrene copolymer (ABS) and a terpolymer, the terpolymer containing a first repeat unit derived from ethylene and a second repeat unit comprising a glycidyl group.
[0011] In one embodiment of the invention, the terpolymer may comprise a second repeat unit derived from glycidyl (meth)acrylate and a third repeat unit derived from methyl (meth)acrylate.
[0012] In one embodiment of the present invention, the second repeating unit may be contained in an amount of 3 to 20 wt % based on the total weight of the terpolymer.
[0013] In one embodiment of the present invention, the third repeating unit may be contained in an amount of 20 to 30 wt % based on the total weight of the terpolymer.
[0014] In one embodiment of the present invention, the terpolymer may be contained in an amount of 0.1 to 10% by weight based on the total weight of the composition.
[0015] In one embodiment of the present invention, the polymeric composition may further comprise a copolymer containing repeat units derived from methyl (meth)acrylate and repeat units derived from ethylene.
[0016] In one embodiment of the present invention, the copolymer may be contained in an amount of 1 to 20% by weight based on the total weight of the composition.
[0017] In one embodiment of the present invention, the low fluidity polymer composition may satisfy the following formula 1.
[0018] [Formula 1]MFI COM / MFI ABS <1.0 (In the above formula 1, MFI COM is the melt flow index (g / 10 min.) of a low-fluidity polymer composition, and MFI ABSis the melt flow index of pure ABS copolymer, the melt flow index being measured according to ISO 1133-1 (2011).
[0019] In one embodiment of the invention, the low flow polymeric composition may be for extrusion.
[0020] In one embodiment of the present invention, the low flow polymer composition may be substantially free of polycarbonate.
[0021] In one embodiment of the present invention, a molded article produced by processing the low fluidity polymer composition may satisfy the following formula 2.
[0022] [Formula 2]IS COM / IS ABS >1.0 (IS COM is the impact strength (kJ / m) of a molded product produced by processing a low-flow polymer composition. 2 ), and IS ABS is the impact strength of a molded article produced by processing a pure ABS copolymer, said impact strength being measured according to ISO 179 1eA.
[0023] The present disclosure provides a molded article produced by processing the aforementioned low flow polymeric composition.
[0024] The present disclosure can provide a method for reducing the fluidity of an acrylonitrile-butadiene-styrene copolymer (ABS) comprising melt blending (melt extruding) in an extruder a polymeric composition comprising the ABS and a terpolymer, the terpolymer containing a first repeat unit derived from ethylene and a second repeat unit comprising a glycidyl group. Effect of the Invention
[0025] The present disclosure provides a low-fluidity polymer composition including an acrylonitrile-butadiene-styrene copolymer and a terpolymer. Specifically, the low-fluidity polymer composition can impart a melt flow index advantageous for extrusion molding, which requires low fluidity, due to the interaction between the terpolymer and the acrylonitrile-butadiene-styrene copolymer, and can be used to manufacture molded products having improved impact strength. Therefore, when the low-fluidity polymer composition is used, it is easy to adjust the viscosity of the composition, and not only can the workability in the polymer molding step be improved, but molded products having excellent impact strength can be manufactured in various forms. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0026] The present invention will be described in more detail below. However, the following embodiments or implementations are merely a reference for describing the present invention in detail, and the present invention is not limited thereto, and may be realized in various forms.
[0027] Additionally, unless otherwise defined, all technical and scientific terms have the same meaning as commonly understood by one of ordinary skill in the art to which this invention belongs.
[0028] The terms used in the description of the present invention are merely for the purpose of efficiently describing particular embodiments and are not intended to limit the present invention.
[0029] Additionally, as used in the specification and the appended claims, the singular forms "a," "an," and "the" are intended to include the plural forms as well, unless the context indicates otherwise.
[0030] In addition, when a part is described as "comprising" a certain component, this means that it may further include other components, rather than excluding other components, unless otherwise specified to the contrary.
[0031] In addition, the numerical ranges used herein include lower and upper limits, and all values within the ranges, increments logically derived in the form and width of the ranges defined, all values that are doubly limited, and all possible combinations of upper and lower limits of numerical ranges that are mutually limited in different ways. Unless otherwise defined herein, values outside the numerical ranges that may occur due to experimental error or rounding up are also included in the numerical ranges defined.
[0032] The term "low fluidity" as used herein means a property of a polymer composition having a melt flow index lower than that of a base polymer. Specifically, a polymer composition having a melt flow index lower than that of an acrylonitrile-butadiene-styrene copolymer can be defined as a low fluidity polymer composition.
[0033] The term "substantially free" as used herein may mean that the composition contains 1 part by weight or less, specifically 0.1 part by weight or less, per 100 parts by weight of acrylonitrile-butadiene-styrene copolymer (ABS). For example, the term "substantially free of polycarbonate or polymer containing maleic anhydride functional group" in a low-flow polymer composition may mean that the composition contains 1 part by weight or less, specifically 0.1 part by weight or less, of polycarbonate or polymer containing maleic anhydride functional group per 100 parts by weight of acrylonitrile-butadiene-styrene copolymer (ABS).
[0034] The present invention will now be described in more detail.
[0035] The present disclosure provides a low flow polymeric composition comprising an acrylonitrile-butadiene-styrene copolymer (ABS) and a terpolymer, the terpolymer containing a first repeat unit derived from ethylene and a second repeat unit comprising a glycidyl group.
[0036] The acrylonitrile-butadiene-styrene copolymer (hereinafter, referred to as ABS copolymer) may be an acrylonitrile-butadiene-styrene copolymer obtained by polymerizing butadiene, styrene, and acrylonitrile by a conventional or known method. For example, it may be a polymer polymerized by an emulsion polymerization method or a suspension polymerization method, and commercially available products may be used without limitation.
[0037] As a non-limiting example, the repeating unit derived from butadiene may be 5 to 50 wt%, specifically 20 to 40 wt%, the repeating unit derived from styrene may be 20 to 70 wt%, specifically 25 to 60 wt%, and the repeating unit derived from acrylonitrile may be 5 to 40 wt%, specifically 10 to 35 wt%, based on the total weight of the ABS copolymer. The weight average molecular weight (Mw) of the ABS copolymer may be 10,000 to 500,000 g / mol, or 50,000 to 300,000 g / mol, or 80,000 to 250,000 g / mol. The glass transition temperature (Tg) of the ABS copolymer may be 70 to 150°C, or 80 to 130°C, and the melting temperature (Tm) of the ABS copolymer may be 150 to 300°C, or 180 to 250°C. The melt flow index (MFI) of the ABS copolymer may be, but is not limited to, 1 to 100 g / 10 min., or 1 to 50 g / 10 min., or 5 to 30 g / 10 min.
[0038] In one embodiment, the terpolymer may include a first repeat unit derived from ethylene, a second repeat unit derived from glycidyl (meth)acrylate, and a third repeat unit derived from methyl (meth)acrylate. Specifically, the terpolymer may include a first repeat unit derived from ethylene, a second repeat unit derived from glycidyl methacrylate, and a third repeat unit derived from methyl acrylate.
[0039] The terpolymer may be a terpolymer in which methyl (meth)acrylate, glycidyl (meth)acrylate, and ethylene are polymerized by a normal or known method, or a commercially available product may be used without any limitation.
[0040] Specifically, the second repeating unit may be contained in an amount of 0.1 to 50 wt%, specifically 1 to 30 wt%, more specifically 2 to 20 wt%, based on the total weight of the terpolymer. The third repeating unit may be contained in an amount of 0.1 to 50 wt%, specifically 5 to 40 wt%, more specifically 20 to 30 wt%, based on the total weight of the terpolymer. The weight average molecular weight (Mw) of the terpolymer may be 10,000 to 500,000 g / mol, or 50,000 to 250,000 g / mol, and the melt flow index (MFI, 190°C / 2.16 kg) of the terpolymer may be, but is not limited to, 1 to 100 g / 10 min., 1 to 40 g / 10 min., or 1 to 30 g / 10 min. A polymer composition containing a terpolymer satisfying the above range can effectively reduce the melt flow index (MFI), improve the workability in extrusion molding, and improve the impact strength of the molded product produced.
[0041] In one embodiment, the terpolymer may be contained in an amount of 0.1-20 wt% or 0.1-10 wt%, specifically 0.5-7 wt%, more specifically 1-5 wt% based on the total weight of the composition. When the above range is satisfied, the melt flow index (MFI) of the polymer composition can be more easily adjusted, and a molded article having improved impact strength can be produced. In addition, by appropriately adjusting the content of the terpolymer, the target melt flow index (MFI) of the polymer composition and the impact strength of the produced molded article can be easily achieved.
[0042] In one embodiment, the polymer composition may further include a copolymer containing a repeating unit derived from methyl (meth)acrylate and a repeating unit derived from ethylene. Specifically, a copolymer obtained by polymerizing methyl (meth)acrylate and ethylene by a conventional or known method may be used, and a commercially available product may be used without limitation. Specifically, the copolymer may be poly(ethylene-co-methyl methacrylate) or poly(ethylene-co-methyl acrylate).
[0043] As a non-limiting example, the repeating unit derived from methyl (meth)acrylate may be 1 to 50 wt%, specifically 15 to 35 wt%, and the repeating unit derived from ethylene may be 50 to 99 wt%, specifically 65 to 85 wt%, based on the total weight of the copolymer. The weight average molecular weight (Mw) of the copolymer may be 10,000 to 500,000 g / mol, or 50,000 to 250,000 g / mol, and the melt flow index (MFI, 190°C / 2.16 kg) of the copolymer may be, but is not limited to, 1 to 800 g / 10 min., 1 to 50 g / 10 min., or 1 to 45 g / 10 min.
[0044] The copolymer may be included in an amount of 0.1 to 30 wt%, 1 to 20 wt%, or 1 to 15 wt% based on the total weight of the composition. The weight ratio of the terpolymer and the copolymer may be, but is not limited to, 1:0.1 to 50, or 1:0.5 to 10. The polymer composition can easily achieve the target melt flow index (MFI) of the polymer composition and the impact strength of the molded product produced by appropriately adjusting the content of the copolymer.
[0045] In one embodiment, the low flow polymer composition may further include a thermoplastic polymer in addition to the acrylonitrile-butadiene-styrene polymer. As a non-limiting example, the thermoplastic polymer may be one selected from the group consisting of polyvinyl chloride (PVC), polypropylene (PP), polyacrylate, polyethylene terephthalate (PET), polybutylene terephthalate (PBT), polymethyl methacrylate (PMMA), polyamide, styrene-acrylonitrile copolymer (SAN), and acrylonitrile-styrene-acrylate (ASA), or a mixture thereof. The thermoplastic polymer may be included in an amount of 0.1 to 100 parts by weight, 1 to 50 parts by weight, or 1 to 25 parts by weight, based on 100 parts by weight of the ABS copolymer, but is not limited thereto, and the content of the composition may be adjusted to produce a molded product having a desired physical property.
[0046] In one embodiment of the present invention, the low fluidity polymer composition may be substantially free of polycarbonate. If the polycarbonate (PC) is contained in the polymer composition, the viscosity of the polymer composition is significantly decreased, which is not preferable because it is difficult to easily realize low fluidity.
[0047] In one embodiment of the present invention, the low fluidity polymer composition may be substantially free of a polymer containing a maleic anhydride functional group. If the polymer composition contains a polymer containing a maleic anhydride functional group, it may be difficult to achieve the desired viscosity (fluidity) of the present invention.
[0048] In one embodiment of the present invention, the low fluidity polymer composition may further include additives commonly used in the art according to the purpose and application. For example, UV stabilizers, UV absorbers, antioxidants, viscosity modifiers, plasticizers, heat stabilizers, dyes, pigments, colorants, release agents, antistatic agents, antibacterial agents, processing aids, metal deactivators, flame retardants, antifriction agents, antiwear agents, and lubricants may further be included. In this case, the additives may be included in an appropriate amount within a range that does not impair the physical properties targeted by the present invention.
[0049] In one embodiment of the present invention, the low fluidity polymer composition satisfies the following formula 1, and specifically, may satisfy the following formula 3.
[0050] [Formula 1]MFI COM / MFI ABS <1.0
[0051] [Formula 3]MFI COM / MFI ABS ≦0.8 (In the above formulas 1 and 3, MFI COM is the melt flow index (g / 10 min.) of the polymer composition, and MFI ABS is the melt flow index of pure ABS copolymer, the melt flow index being measured according to ISO 1133-1 (2011).
[0052] When formula 1, specifically formula 3, is satisfied, the polymer composition may have low fluidity, and the polymer composition may have a more favorable melt flow index during extrusion molding, thereby improving workability.
[0053] The present invention can provide a molded article manufactured by processing the above-mentioned low fluidity polymer composition. The processing method of the molded article can be any commonly used or known method without any particular limitation, and can be, for example, injection, extrusion, profile extrusion, calendaring, and direct blow molding. In particular, the low fluidity polymer composition has a reduced melt flow index (MFI) during extrusion molding by including the ABS copolymer and the above-mentioned terpolymer, and when the low fluidity polymer composition is used for extrusion, the processability can be further improved, and a high-quality molded article can be manufactured.
[0054] In one embodiment of the present invention, a molded article manufactured by processing the low fluidity polymer composition satisfies the following formula 2, specifically, the following formula 4. The molded article may include known molded articles such as films and sheets without being limited thereto. Specifically, the molded article of the following formulas 2 and 4 may be a sheet.
[0055] [Formula 2]IS COM / IS ABS >1.0
[0056] [Formula 4]IS COM / IS ABS ≧1.2 (IS COM is the impact strength (kJ / m) of a molded product produced by processing a low-flow polymer composition. 2 ), and IS ABS is the impact strength of a molded article produced by processing a pure ABS copolymer, said impact strength being measured according to ISO 179 1eA.
[0057] When the low fluidity polymer composition contains the ABS copolymer and the above-mentioned terpolymer, a molded article produced using the composition satisfies the formula 2, specifically, the formula 4, and can thereby achieve excellent impact strength.
[0058] More specifically, the low fluidity polymer composition can satisfy both of the formulas 1 and 2, and more specifically, can satisfy both of the formulas 3 and 4. In this case, a molded article having improved impact strength can be produced by using a low fluidity polymer composition having a reduced melt flow index (MFI).
[0059] The present disclosure can provide a method for reducing the flowability of an acrylonitrile-butadiene-styrene copolymer (ABS) comprising melt blending a polymeric composition comprising the ABS and a terpolymer in an extruder, the terpolymer containing a first repeat unit derived from ethylene and a second repeat unit comprising a glycidyl group.
[0060] The acrylonitrile-butadiene-styrene copolymer (ABS) and the terpolymer are as described above, and therefore a detailed description thereof will be omitted.
[0061] The method for reducing the fluidity of the ABS copolymer is carried out in order to provide more favorable viscosity conditions in the molding step of the ABS. Specifically, the method for reducing the fluidity of the ABS copolymer can be used in order to obtain a reduced melt flow index during extrusion molding of the ABS.
[0062] In one embodiment, the method for reducing the fluidity of the ABS copolymer may include a step of melt-kneading the polymer composition using an extruder. The melt-kneading process may be any conventional method for melt-kneading a thermoplastic resin, and may be performed using a twin-screw melt-kneading extruder at a temperature of 200 to 260°C, but is not limited thereto. The polymer composition may then be melt-kneaded and used in an extruder to produce molding pellets, and the molding pellets produced may be used to produce a molded product, but is not limited thereto.
[0063] In one embodiment, the polymer composition contains both the ABS copolymer and the terpolymer, so that low fluidity can be easily achieved. As a result, the polymer composition can be applied to a molding method that requires low fluidity, such as extrusion molding, and can have improved workability and produce molded products with improved impact strength and high quality.
[0064] The present invention will be described in more detail with reference to the following examples and comparative examples. However, the following examples and comparative examples are merely illustrative examples for explaining the present invention in more detail, and the present invention is not limited by the following examples and comparative examples.
[0065] The physical properties of the following examples and comparative examples of the present invention were measured by the following methods.
[0066] [Physical property evaluation method] 1.Melt Flow Index (MFI) [g / 10min.] The melt flow index (MFI) was measured at 220°C under a load of 10 kg in accordance with ISO 1133-1 (2011). The measured values are shown in Table 1 below. When the measured MFI value satisfied the following formula 1, it was determined that the material had low fluidity.
[0067] [Formula 1]MFI COM / MFI ABS <1.0 (In the above formula 1, MFI COM is the melt flow index of the polymer compositions according to the examples and comparative examples, and MFI ABS is the melt flow index of the pure ABS copolymer.
[0068] 2.Impact strength [kJ / m 2 ] The notched Charpy impact strength was measured according to ISO 179 1eA, and the measured values are shown in Table 1 below.
[0069] 3.Flexural modulus [MPa] Flexural modulus was measured according to ISO 178. The measured values are reported in Table 1 below.
[0070] [Examples 1 to 5 and Comparative Examples 1 to 2] A polymer composition was prepared by mixing an acrylonitrile-butadiene-styrene copolymer (Terluran GP22), an ethylene-methyl acrylate-glycidyl methacrylate terpolymer (Lotader AX8900), and an ethylene-methyl acrylate copolymer (Lotryl 29MA03T) in the content ratio of the raw materials shown in Table 1 below. Specifically, the raw materials shown in Table 1 below were dry mixed, quantitatively continuously fed into the feed section of a twin-screw extruder, melt-kneaded, and pelletized. The pellets prepared were thoroughly dried, and test pieces conforming to the standards described in the physical property evaluation method were prepared, and the physical properties were measured.
[0071] [Table 1]
[0072] As can be seen from Table 1, when comparing Comparative Example 1, which is a pure ABS copolymer, with Examples 1 to 3, which are polymer compositions containing ABS and the above-mentioned terpolymer, it was confirmed that the MFI of the Examples was effectively reduced and showed improved impact strength.
[0073] Comparing Example 3 with Comparative Example 2 containing a methyl acrylate-ethylene copolymer, it was found that, despite containing the same amount of ABS copolymer, the MFIs were inconsistent, and as the content of the terpolymer increased in Examples 1 to 3, the MFI further decreased. This confirmed that the polymer composition according to one embodiment of the present invention can effectively achieve low fluidity by containing an ABS copolymer and a terpolymer.
[0074] As described above, the present disclosure has been described in the present specification by using specific details and limited embodiments, but this is merely provided for a more general understanding of the present disclosure, and the present disclosure is not limited to the above embodiments. A person having ordinary knowledge in the field to which the present disclosure belongs can make various modifications and variations from such descriptions.
[0075] Therefore, the spirit of the present invention should not be limited to the above-described embodiments, and it can be said that not only the scope of the attached claims, but also anything that has equivalent or equivalent modifications to the scope of the claims falls within the scope of the spirit of the present invention.
Claims
1. A low flowability polymeric composition comprising an acrylonitrile-butadiene-styrene copolymer (ABS) and a terpolymer, the terpolymer containing a first repeat unit derived from ethylene and a second repeat unit comprising a glycidyl group.
2. 2. The low flow polymeric composition of claim 1, wherein the terpolymer comprises a second repeat unit derived from glycidyl (meth)acrylate and a third repeat unit derived from methyl (meth)acrylate.
3. 3. The low fluidity polymer composition according to claim 2, wherein the second repeating unit is contained in an amount of 3 to 20 wt % based on the total weight of the terpolymer.
4. 3. The low fluidity polymer composition according to claim 2, wherein the third repeat unit is contained in an amount of 20 to 30 wt % based on the total weight of the terpolymer.
5. 2. The low flowability polymer composition according to claim 1, wherein the terpolymer is contained in an amount of 0.1 to 10% by weight based on the total weight of the composition.
6. 10. The low flow polymeric composition of claim 1 further comprising a copolymer containing repeat units derived from methyl (meth)acrylate and repeat units derived from ethylene.
7. 7. The low fluidity polymer composition according to claim 6, wherein the copolymer is contained in an amount of 1 to 20% by weight based on the total weight of the composition.
8. The low fluidity polymer composition according to claim 1, which satisfies the following formula 1: [Formula 1] MFI COM / MFI ABS <1.0 (In the above formula 1, MFI COM is the melt flow index (g / 10 min.) of the low-fluidity polymer composition, and MFI ABS is the melt flow index of a pure ABS copolymer, the melt flow index being measured in accordance with ISO 1133-1 (2011).
9. 2. The low flow polymer composition according to claim 1, which is for extrusion.
10. 10. The low flow polymeric composition of claim 1, which is substantially free of polycarbonate.
11. The low fluidity polymer composition according to claim 1, wherein a molded article produced by processing the low fluidity polymer composition satisfies the following formula 2: [Formula 2] IS COM / IS ABS > 1.0 (IS COM is the impact strength (kJ / m) of a molded product produced by processing a low-fluidity polymer composition. 2 ) and IS ABS is the impact strength of a molded article produced by processing a pure ABS copolymer, said impact strength being measured according to ISO 179 1eA.
12. A molded article produced by processing the low fluidity polymer composition according to any one of claims 1 to 11.
13. The method includes melt-blending a polymer composition including an acrylonitrile-butadiene-styrene copolymer (ABS) and a terpolymer in an extruder, A method for reducing the flowability of an ABS copolymer, wherein the terpolymer contains a first repeat unit derived from ethylene and a second repeat unit comprising a glycidyl group.
Citation Information
Patent Citations
Thermoplastic resin composition
JP1995003114A
Thermoplastic resin composition and molded article
JP2009256647A
Polybutylene terephthalate resin composition
JP2014001374A
Low-gloss heat-resistant abs resin composition and its preparation method
US20170355847A1