Method for forming improved interfaces and thin films using high density radicals
High-density radicals are used to address semiconductor manufacturing issues by enhancing film formation through uniform diffusion and chemical bonding, reducing defects and impurities, thereby improving film quality and device performance.
Patent Information
- Application Number
- JP2024509098
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-11-03
- Filing Date
- 2023-06-19
- Publication Date
- 2024-11-27
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing semiconductor manufacturing processes face issues such as poor vapor deposition, high defect density at interfaces, and impurity generation in thin films, leading to poor electrical characteristics and reduced device yield.
The method involves using high-density radicals for post-deposition annealing to enhance film formation by promoting uniform diffusion and chemical bonding, reducing defects and impurities through reactive gas penetration and substitution reactions.
This approach results in films with low defect density and high bonding strength, improving electrical characteristics and device yield by forming homogeneous chemical bonds and densifying the film.
Smart Images

Figure 2024544040000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for improving interface and thin film properties using high density radicals. [Background technology]
[0002] As technology advances, semiconductors, which are the foundation of core technologies for the Fourth Industrial Revolution such as artificial intelligence, big data, 5G, and self-driving cars, are requiring multi-layer structures and complex circuit patterns to increase the speed of non-memory (System LSI) devices and the capacity of memory (DRAM, 3D_VNAND).
[0003] As a result, semiconductor patterning technology with a line width of 5nm or less has been achieved through the introduction of EUV (Extreme Ultraviolet) and other technologies. However, problems such as non-uniformity of thin film thickness, poor deposition of high aspect ratio contact holes, and low step coverage, which are emerging as limitations of existing thin film deposition technology, must be solved.
[0004] Furthermore, during the manufacture of semiconductor devices, the interface between the lower film and the deposited film has a high defect density, which deteriorates electrical characteristics and reduces the yield of devices.
[0005] In addition, impurities are generated inside the film during the deposition process, and in order to remove these impurities, a subsequent heat treatment process must be introduced to densify the film.
[0006] FIG. 1 is an exemplary diagram showing a conventional process for improving interface and thin film properties.
[0007] First, in the first embodiment, as shown in FIG. 1(a), SiO2 or high-k is deposited on a substrate (100) by a technique such as CVD or ALD. However, such a conventional technique results in a high density of interface defects at the interface between the substrate (100) and the deposition surface. In such a case, since there is only physical bonding between the substrate (100) and the insulating film, a considerable number of defects occur between the substrate (100) and the insulating film. In other words, the substrate (100) and the insulating film are not strongly bonded to each other.
[0008] In the second embodiment, which solves the problems of the first embodiment, as shown in Fig. 1(b), SiO2 is first thinly oxidized on the substrate, and then SiO2 or high-k is deposited using techniques such as CVD or ALD. In this case, the first SiO2 deposition is deposited using the oxidation method, and the substrate (100) has a low interface defect density. This increases the bonding strength between the substrate (100) and the insulating film, but the second embodiment also has the limitation that physical defects occur between the SiO2 and the insulating film. Summary of the Invention [Problem to be solved by the invention]
[0009] The present invention is intended to solve the problems of the prior art described above, and according to one embodiment of the present invention, in order to solve the problems of surface reaction of a film due to low reaction energy and defects due to non-uniform diffusion when applying a PDA (Post Deposition Anneal) technique, a reactive gas is penetrated to the interface during a subsequent heat treatment using high-density radicals.
[0010] Another objective is to form a film with low defect density and high density by inducing a penetration and substitution reaction using high density radicals to remove impurities within the film and form homogeneous chemical bonding with the interface. [Means for solving the problem]
[0011] As a technical means for achieving the above technical object, a method for forming an oxide film using a deposition apparatus includes the steps of: (a) depositing an insulating film on a silicon substrate; and (b) forming SiO2 between the silicon substrate and the insulating film by annealing the insulating film with OH radicals using the deposition apparatus.
[0012] Also, in step (a), the insulating film can be deposited based on either a CVD or ALD technique.
[0013] The insulating film can be made of either a silicon oxide film or a high-k film.
[0014] In addition, in the step (c), the OH radicals penetrate into the insulating film and react with the silicon contained in the silicon substrate, thereby forming a thin film of SiO2.
[0015] In addition, in step (c), the thickness of the SiO2 layer between the silicon substrate and the insulating film can be adjusted by adjusting the annealing temperature and time.
[0016] In addition, the process of injecting OH radicals in step (b) may be carried out at a process temperature between 480 and 730 degrees.
[0017] Furthermore, the steps (a) to (c) can be included in the process of forming a gate oxide film in the process of forming a semiconductor element. Effect of the Invention
[0018] The present invention is intended to solve the problems of the prior art described above. According to one embodiment of the present invention, when applying a PDA (Post Deposition Anneal) technique, in order to solve the problems of surface reaction of a film due to low reaction energy and defects due to non-uniform diffusion, a reactive gas can be penetrated to an interface during a subsequent heat treatment by using high-density radicals.
[0019] In addition, by using high-density radicals to induce penetration and substitution reactions, impurities within the film are removed and homogeneous chemical bonding is performed with the interface, resulting in a film with low defect density and high density. [Brief description of the drawings]
[0020] [Figure 1] 1 is an exemplary diagram showing a conventional process for improving interface and thin film properties; [Diagram 2] 2 is an operational flow chart of a deposition process using high-density radicals to improve interface and thin film properties according to one embodiment of the present invention. [Diagram 3] 1A and 1B are diagrams illustrating a deposition process for improving interface and thin film properties using high-density radicals according to an embodiment of the present invention. [Figure 4a] FIG. 2 is an exemplary diagram showing the thickness of a deposition surface when annealing is performed using high-density radicals and other gases according to an embodiment of the present invention. [Figure 4b] FIG. 4 is an exemplary diagram showing the thickness of a deposition surface according to an embodiment of the present invention as a function of annealing time. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0021] Hereinafter, the embodiments of the present invention will be described in detail with reference to the accompanying drawings so that a person having ordinary skill in the art to which the present invention pertains can easily carry out the embodiments. However, the present invention may be embodied in several different forms and is not limited to the embodiments described herein. In order to clearly explain the present invention in the drawings, parts that are not related to the description are omitted, and similar parts are designated by similar reference numerals throughout the specification.
[0022] Throughout the specification, when a part is "connected" to another part, this includes not only "directly connected" but also "electrically connected" with another element therebetween. Furthermore, when a part is said to "include" a certain component, this does not mean that the other component is excluded, but that the part can further include the other component, unless otherwise specified.
[0023] The following examples are detailed descriptions to aid in understanding the present invention, and are not intended to limit the scope of the present invention. Therefore, inventions that perform the same function as the present invention and have the same scope also belong to the scope of the present invention.
[0024] The term "thin film" or "deposition" as defined in the following specification of the present invention may refer to a process in semiconductor manufacturing in which a thin oxide or metal is coated on a wafer (substrate) surface by alternating the adsorption and replacement of molecules. Therefore, each process described in the following specification may be carried out by a radical unit or deposition device, and thin film deposition is achieved through techniques such as atomic layer deposition (ALD) and chemical vapor deposition (CVD).
[0025] FIG. 2 is an operational flow chart of a deposition process using high-density radicals to improve interface and thin film properties according to one embodiment of the present invention.
[0026] At this time, steps S110 to S130 described below may be included in the process of forming a gate oxide film among the processes of forming a semiconductor device.
[0027] Referring to FIG. 2, a deposition apparatus can deposit an insulating film (110) on a silicon substrate (100) (S110).
[0028] As shown in (a) and (b) of FIG. 3, the process of step (S110) deposits an insulating film (110) on a substrate (100) made of silicon, and the deposition of the insulating film (110) can be performed based on either a CVD or ALD technique.
[0029] Also, the insulating film 110 formed in step S110 may be composed of either a silicon oxide film or a high-k film.
[0030] Next, a deposition apparatus is used to form a SiO2 thin film (120) between the silicon substrate (100) and the insulating film (110) by annealing with OH radicals on the insulating film (110) (S120).
[0031] In steps S120 to S130, as shown in (c) and (d) of Figure 3, OH radicals are injected onto the insulating film (110) to perform annealing using OH radicals. At this time, the OH radicals penetrate into the insulating film (110) and react with silicon contained in the silicon substrate (100), thereby forming a thin SiO2 film (120) at the interface, as shown in (d) of Figure 3.
[0032] This is because OH radicals penetrate the insulating film (110) and oxidize the area between the insulating film (110) and the silicon substrate (100), resulting in the formation of SiOx (meaning SiO or SiO2) at the interface between the insulating film (110) and the silicon substrate (100).
[0033] At this time, the first interface (121) where the SiO2 thin film (120) and the insulating film (110) come into contact, and the second interface (122) where the silicon substrate (110) and the SiO2 thin film (120) come into contact both have low interface bonding density (chemical bonding), which reduces impurities in the film and provides high bonding strength.
[0034] The conventional annealing process aims to improve the interface characteristics on the top surface of the insulating film (110), and various gases such as N2, H2, and O2 are conventionally used in the annealing process. Such conventional processes have a limitation in that gases such as N2 do not penetrate deeply into the insulating film (110).
[0035] However, the purpose of the annealing process performed in step S130 is to cause the OH radicals to penetrate deeply into the insulating film 110. Therefore, the OH radicals that penetrate the insulating film 110 according to the process proposed in the present invention can form an oxide film 130 between the silicon substrate 100 and the insulating film 110, thereby forming a strong bond between the silicon substrate 100 and the insulating film 110. That is, the OH radicals reduce impurities in the insulating film 110, densification of the insulating film 110 progresses, and SiO2 with a strong bond can be formed between the substrate 100 and the insulating film 110.
[0036] In addition, the SiO2 layer produced through steps S110 to S130 is different from the conventional technology in that it is not formed sequentially, but is formed in the reverse order after forming the insulating film (110).
[0037] Generally, the thin film formed first on the substrate is preferably high-k (e.g., Al2O3, but includes various other high-k materials), but may be SiO2 in some cases. In this case, the SiO2 thin film (120) in the process proposed in the present invention must be deposited by CVD (Chemical Vapor Deposition) or ALD (Atomic Layer Deposition), and the SiO2 thin film (120) formed through thermal oxidation is not included in the technology proposed in the present invention. This is because the interface layer formed at the interface through the technology proposed in the present invention reacts with the silicon substrate (100) to form SiO2.
[0038] FIG. 4a is a diagram for comparing the thickness of an insulating film formed when annealing is performed through a conventional gas in the process of the present invention using High-k.
[0039] Figure 4a (a) shows an example of a cross section when only a high-k insulating film is deposited. At this time, the high-k Al2O3 (210) is formed to a specified thickness, but it can be seen that a thin SiO2 layer (220) is formed between the substrate and the high-k.
[0040] 4a(b) shows an optimal embodiment formed by applying the technology of the present invention, that is, an embodiment in which a thin film is formed using Al2O3 as a high-k component and OH radicals.
[0041] In the cross section formed when steps S110 to S120 are performed, a SiO2 layer (220) having a predetermined thickness may be formed under the high-k. The graph below the cross-sectional photograph of the thin film is a graph showing the concentration of each component according to the depth of the thin film, with the y-axis representing the intensity and the x-axis representing the depth of the thin film. Unlike the other graphs, in the case of FIG. 4a (b), it can be seen that the N concentration is always uniform as the depth changes. It can also be seen that the SiO2 layer (220) formed through the process proposed in the present invention is the thickest.
[0042] (c) of Figure 4a is an example of a cross section of the deposition surface when high-k is deposited and then annealed with O2 gas, and (d) of Figure 4a is an example of a cross section of the deposition surface when high-k is deposited and then annealed with N2 gas.
[0043] In this case, in both (c) and (d) of FIG. 4a, annealing is performed at a high temperature of 920°C, and it can be seen that the thickness of the high-k (Al2O3 layer (210)) is thinner than in (a) and (b) of FIG. 4a. In other words, the conventional process shown in (c) and (d) of FIG. 4a has a problem that the high-k (Al2O3 layer (210)) becomes thinner than the thickness at which it was initially deposited after the process is performed. As a result, it can be seen that the process proposed in the present invention is superior in that the thickness of the high-k (Al2O3 layer (210)) formed does not become thinner, and the SiO2 layer (220) is deposited at a predetermined thickness, reducing the density of interface defects.
[0044] Meanwhile, the process proposed in the present invention can adjust the thickness of the SiO2 thin film (120) between the silicon substrate (100) and the insulating film (110) by adjusting the annealing temperature and time, and the process of injecting OH radicals can be carried out at a process temperature between 480 to 730°C.
[0045] For example, (a) to (d) of FIG. 4b are illustrative diagrams showing thicknesses of the deposition surface produced by annealing the OH radicals for 5 minutes, 30 minutes, 45 minutes, and 60 minutes, respectively.
[0046] In this case, in Fig. 4b (a) after 5 minutes of annealing, it can be seen that the Al2O3 layer (210) and SiO2 layer (220) corresponding to high-k have thicknesses of 109.7A and 40.5A, respectively, and in Fig. 4b (b), it can be seen that the Al2O3 layer (210) and SiO2 layer (220) have thicknesses of 106.9A and 79.1A, respectively. Also, in Fig. 4b (c) and (d), it can be seen that the Al2O3 layer (210) and SiO2 layer (220) have thicknesses of 93.5A, 119.0A, 96.8A, and 205.8A, respectively. Therefore, it can be seen that as the annealing time increases, the SiO2 layer (220) becomes thicker while minimizing the change in thickness of the Al2O3 layer (210), and the user can select the annealing time that suits the desired thickness of the SiO2 layer (220) to perform thin film formation work.
[0047] The above description of the present invention is for illustrative purposes only, and those skilled in the art will understand that the present invention can be easily modified into other specific forms without changing the technical idea or essential features of the present invention. Therefore, the above-described embodiments should be understood to be illustrative in all respects and not limiting. For example, each component described as a single type can be implemented in a distributed manner, and similarly, each component described as a distributed manner can be implemented in a combined form.
[0048] The scope of the present invention is indicated by the claims set forth below rather than by the above detailed description, and all modifications and variations that fall within the meaning and scope of the claims and their equivalent concepts should be construed as being included within the scope of the present invention.
Claims
1. A method for forming an oxide film using a deposition apparatus, comprising: (a) depositing an insulating film on a silicon substrate; (b) Using the deposition equipment, annealing is performed on the insulating film using OH radicals to form a SiO 2 and forming an oxide film by using a deposition apparatus.
2. The above step (a) 2. A method for forming an oxide film by using the deposition apparatus according to claim 1, which deposits the insulating film based on either a CVD or ALD technique.
3. The method for forming an oxide film by using a deposition apparatus according to claim 1 , wherein the insulating film is made of either a silicon oxide film or a high-k film.
4. The above step (b) The OH radicals penetrate into the insulating film and react with silicon contained in the silicon substrate to form SiO 2 2. A method for forming an oxide film by using the deposition apparatus according to claim 1, wherein a thin film of
5. The above step (b) By adjusting the annealing time, the SiO 2 2. A method for forming an oxide film by using the deposition apparatus according to claim 1, wherein the thickness of the oxide film is adjusted.
6. 2. The method for forming an oxide film by using a deposition apparatus according to claim 1, wherein the step (b) of injecting the OH radicals is performed at a process temperature between 480 and 730 degrees.
7. 2. The method for forming an oxide film by using a deposition apparatus according to claim 1, wherein the steps (a) and (b) are included in a process for forming a gate oxide film in a process for forming a semiconductor device.
Citation Information
Patent Citations
Insulating film-forming method, and semiconductor device and manufacturing method thereof
JP2003179049A
Forming method of gate oxide film
JP2006120965A
Method of forming insulating film
JP2008277844A
Use of dilute steam ambient for improvement of flash devices
US20020117709A1