Ceramic Printed Fuse Products
Printed fuse elements on ceramic substrates address the challenges of size, weight, and premature failure in high voltage DC power systems by enhancing thermal and mechanical stability, ensuring reliable circuit protection in electric vehicles.
Patent Information
- Application Number
- JP2024531703
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-11-30
- Filing Date
- 2022-11-23
- Publication Date
- 2024-11-27
AI Technical Summary
High voltage DC power systems in electric vehicles face challenges with existing fuses that are too large, heavy, and prone to premature failure due to thermo-mechanical fatigue, which compromises circuit protection performance and efficiency.
The use of printed fuse elements on ceramic substrates, formed through additive processes without stamped or punched weak sections, combined with arc-quenching fillers, to enhance thermal and mechanical stability and reduce fuse fatigue.
The solution provides smaller, lighter fuses with improved arc extinguishing capabilities and reduced thermo-mechanical fatigue, ensuring reliable circuit protection in high voltage, high current DC power systems.
Smart Images

Figure 2024544051000001_ABST
Abstract
Description
[Technical field]
[0001] The field of the disclosure relates generally to electrical circuit protection fuses, and more specifically, to printed fuse fabrications on ceramic substrates for high voltage direct current (DC) power systems of electric vehicles (EVs). [Background technology]
[0002] Fuses are widely used as overcurrent and short circuit protection devices to prevent costly damage to electrical circuits. Fuse terminals typically form an electrical connection between a power source or power supply and an electrical component or combination of components arranged in the electrical circuit. One or more fusible links or elements, or fuse element assemblies, are connected between the fuse terminals such that when the current through the fuse exceeds a predetermined limit, the fusible elements melt, opening one or more circuits through the fuse and preventing damage to the electrical components.
[0003] High voltage DC power systems pose special challenges to fuse manufacturers in a market that increasingly demands smaller and lighter fuse packages. Achieving desired fuse opening times and managing increasingly stringent arc energies in high voltage, high current applications with limited physical space is difficult to achieve. Certain types of DC power systems with relatively extreme cyclic current loads impose an additional challenge in that they tend to result in premature fuse failure. In the context of EV power systems, premature fuse failure is inherently problematic and improvements are desired. [Brief description of the drawings]
[0004] Non-limiting and non-exhaustive embodiments are described with reference to the following figures, in which like reference numerals refer to like parts throughout the various drawings unless otherwise specified.
[0005] [Figure 1] 1 illustrates an exemplary transient current pulse profile generated in a power system.
[0006] [Figure 2A] FIG. 1 is a perspective view of a known power fuse.
[0007] [Figure 2B] FIG. 2B is a perspective view of a fuse element assembly of the power fuse shown in FIG. 2A.
[0008] [Figure 2C] FIG. 2C is a schematic diagram of a weak portion of the fuse element assembly shown in FIG. 2B.
[0009] [Figure 2D] FIG. 2C is a schematic diagram illustrating a weak portion of the fuse element assembly shown in FIG. 2B under a load current cycling event.
[0010] [Figure 2E] FIG. 2C is a schematic diagram illustrating a weak portion of the fuse element assembly shown in FIG. 2B failing after a load current cycling event.
[0011] [Diagram 3] FIG. 2 is a partial perspective view of an exemplary power fuse.
[0012] [Figure 4] 2 is an enlarged cross-sectional view of a portion of an exemplary fuse element assembly.
[0013] [Diagram 5] FIG. 1 is a schematic diagram of attaching a conductor to a weak portion.
[0014] [Figure 6] 1 is a schematic diagram of an exemplary embodiment of a fuse element assembly.
[0015] [Figure 7]7 is an alternative embodiment of a power fuse including the fuse element assembly shown in FIG. 6.
[0016] [Figure 8] FIG. 2 is a schematic diagram of a second dielectric layer covering the weak portion. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] Recent advances in electric vehicle technology present unique challenges to fuse manufacturers: electric vehicle manufacturers are seeking fusible circuit protection for power distribution systems that operate at much higher voltages than traditional vehicle power distribution systems, while at the same time requiring smaller fuses to meet the specifications and demands of electric vehicles.
[0018] Power systems for conventional internal combustion engine powered vehicles operate at relatively low voltages, typically around 48 VDC or less. However, power systems for electric vehicles, referred to herein as electric vehicles (EVs), operate at much higher voltages. The relatively high voltage systems of EVs (e.g., 200 VDC or higher) generally allow the batteries to store more energy from the power source and provide more energy to the vehicle's electric motor with lower losses (e.g., heat losses) than conventional batteries and more recent 48 V power systems that store energy at the 12 volts (V) or 24 V used by internal combustion engines.
[0019] EV original equipment manufacturers (OEMs) use circuit protection fuses to protect electrical loads in all Battery Electric Vehicles (BEVs), Hybrid Electric Vehicles (HEVs), and Plug-in Hybrid Electric Vehicles (PHEVs). Across each EV type, EV manufacturers are seeking to maximize EV driving range per charge while reducing cost of ownership. Achieving these goals depends on the size, volume, and mass of the vehicle components that go into the power system, in addition to the EV system's energy storage and power delivery. Smaller, lighter vehicles meet these demands more effectively than larger, heavier vehicles. As such, all EV components are currently under scrutiny for potential size, weight, and cost reductions.
[0020] Generally, larger components tend to have higher associated material costs, tend to increase the overall size of the EV or occupy excessive space in a shrinking vehicle volume, and tend to introduce significant mass that directly reduces vehicle mileage per battery charge. However, known high-voltage circuit protection fuses are relatively large and relatively heavy components. Historically, and for good reasons, circuit protection fuses have tended to be large in size to meet the demands of high-voltage power systems as opposed to low-voltage systems. As such, existing fuses required to protect high-voltage EV power systems are much larger than existing fuses required to protect the low-voltage power systems of conventional internal combustion engine powered vehicles. Smaller and lighter high-voltage power fuses are desired to meet the needs of EV manufacturers without sacrificing circuit protection performance.
[0021] Power systems in state-of-the-art EVs may operate at high voltages of 450 VDC or more. The increased power system voltage desirably provides EVs with more power per battery charge. However, the operating conditions for electrical fuses in such high-voltage power systems are much more stringent than in low-voltage systems. In particular, specifications regarding electrical arcing conditions when fuses open may be particularly difficult to meet for high-voltage power systems, especially when coupled with industry preferences for reducing the size of electrical fuses. Also, the current cycling loads imposed on power fuses by state-of-the-art EVs tend to impose mechanical strain and wear that may lead to premature failure of conventional fuse elements. Although known power fuses are currently available for use by EV OEMs in the high-voltage circuits of state-of-the-art EV applications, the size and weight of conventional power fuses capable of meeting the requirements of high-voltage power systems for EVs are impractically high to implement in new EVs, not to mention the cost.
[0022] Providing a relatively small power fuse that can handle the high currents and high battery voltages of state-of-the-art EV power systems while providing acceptable interrupting performance when the fuse element operates at high voltages is challenging, to say the least. Recently, efforts have been made to improve fuses and fuse elements with higher current capabilities in smaller package sizes for use in EV power systems that can handle the increased amount of arc energy in the operation of the fuse and provide the desired circuit protection performance. Such improved fuses include stamped and formed fuse elements connected in tandem with the specific application of arc barrier materials and silicated filler materials. However, the stamping process to form the fuse element makes the fuse element vulnerable to premature mechanical failure when exposed to extreme thermal cycles in EV power systems. This is sometimes referred to in the art as fuse fatigue.
[0023] Printed fuse fabrication on ceramic material substrates has attracted renewed interest to meet the specific needs of state-of-the-art DC power systems in electric vehicles. Printing fuse elements on ceramic substrates advantageously avoids thermo-mechanical fatigue during EV power system load cycles and associated disruptive operation of fuses that have been found to occur undesirably in fuse elements alternatively formed via stamping or punching processes in freestanding metallic fuse elements. Combinations of printed fuse elements and freestanding conductor materials have been proposed with some success for EV power system applications. See, for example, U.S. Pat. No. 11,087,943. While these can be reliably performed in EV power systems in a manner that is not susceptible to fuse fatigue due to thermo-mechanical cycling, smaller, less complex fuse elements are desired without compromising circuit protection performance. Thus, improvements are needed to meet a long-standing and unmet need in the art.
[0024] To best understand the present invention, the following provides a discussion of the state of the art regarding power fuses and the challenges presented in EV power system applications, followed by exemplary embodiments of the present invention that overcome the shortcomings of existing fuse solutions. Although described in the context of an EV application and a particular type and rating of fuses, the advantages of the present disclosure are not necessarily limited to the EV application or the particular ratings described. Rather, the advantages of the present disclosure are believed to accrue more broadly to many different power system applications, and may also be implemented in part or in whole to construct different types of fuses having similar or different ratings to those described herein. Method aspects will be partly apparent and partly explicit in the discussion that follows.
[0025] FIG. 1 illustrates an exemplary current drive profile 100 in an EV power system application that can render a conventional power fuse, particularly a fuse element therein that includes a stamped weak portion, susceptible to load current cycle fatigue. Current is illustrated along the vertical axis of FIG. 1, and time is illustrated along the horizontal axis. In a typical EV power system application, the power fuse is used as a circuit protection device to prevent damage to an electrical load from an electrical fault condition. The power system may operate at voltages of over 500V and / or currents of over 150 amperes (A). Considering the example of FIG. 1, the EV power system experiences large, seemingly random fluctuations in current load over a relatively short period of time, e.g., between −250A and 150A. The seemingly random fluctuations in current generate current pulses of various magnitudes in a sequence caused by seemingly random driving habits based on the EV vehicle driver's actions, traffic conditions, and / or road conditions. This creates a virtually infinite current duty cycle on the EV drive motor, the primary drive battery, and any protective power fuses included in the system.
[0026] Such random current loading conditions are illustrated in the current pulse profile of FIG. 1 and are periodic in nature for both EV acceleration (corresponding to battery depletion) and EV deceleration (corresponding to regenerative battery charging). This current cyclic loading imparts thermal cycling stresses to the fuse element, and more specifically to the weak portion of the fuse element assembly within the power fuse, through a Joule effect heating process. This thermal cycling loading of the fuse element imparts mechanical expansion and contraction cycles, particularly to the weak portion of the fuse element. This repeated mechanical cyclic loading of the weak portion of the fuse element imparts accumulating strain that over time damages the weak portion to the point of failure. For purposes of this description, this thermo-mechanical process and phenomenon is referred to herein as fuse fatigue. As further described below, fuse fatigue is primarily due to creep strains as the fuse endures the actuation profile. Heat generated in the weak portion of the fuse element is the primary mechanism leading to the initiation of fuse fatigue.
[0027] 2A illustrates an exemplary high voltage power fuse 200 proposed for use in an EV power system. The power fuse 200 includes a housing 202, terminal blades 204, 206 configured to connect to a line and load side circuit, and a fuse element assembly 208 that completes the electrical connection between the terminal blades 204, 206 via terminal contact blocks 222, 224 provided on end plates 226, 228. Upon exposure to a predetermined current condition, at least a portion of the fuse element assembly 208 melts, decomposes, or otherwise structurally fails, opening a circuit path between the terminal blades 204, 206. Thus, the load side circuit is electrically isolated from the line side circuit, protecting the load side circuit components from damage when an electrical fault condition occurs.
[0028] 2B shows in further detail the fuse element assembly 208 of the power fuse 200. The fuse element assembly 208 is generally formed from a free-standing strip of conductive material into a series of co-planar sections 240 connected by angled sections 242, 244. The angled sections 242, 244 are formed or bent out of plane from the planar section 240.
[0029] In the illustrated example, planar portion 240 defines a number of portions of reduced cross-sectional area, referred to in the art as weakened portions. Weakened portions 241 are defined by openings in planar portion 240. Weakened portions 241 correspond to narrow portions of planar portion 240 between adjacent openings. The reduced cross-sectional area of weakened portions 241 results in higher heat concentrations than the remainder of fuse element assembly 208 when electrical current flows through fuse element assembly 208.
[0030] The weak portion 241 of the fuse element assembly 208 is typically manufactured by a metal stamping or punching process. However, such stamped or punched fuse elements to form the weak portion 241 have been found to be disadvantageous for EV applications having cyclic current loads of the type described above. Such stamped or punched fuse element designs undesirably introduce mechanical strains and stresses into the weak portion 241 of the fuse element, which tend to result in a shortened life. This shortened fuse life manifests itself in the form of troublesome fuse operation resulting from thermo-mechanical fatigue cycling of the fuse element at the weak portion 241.
[0031] 2C shows a cross-sectional view of metal sheet 250 after openings 252 have been punched into metal sheet 250. After the punching or stamping process, micro tears 254 form along the boundaries 256 of openings 252.
[0032] As shown in Figures 2D and 2E, the weak portion 241 of the fuse element assembly 208 experiences repeated high current pulses and cyclic current events (Figure 2D), which leads to metal fatigue from intergranular fracture and subsequent crack propagation and failure of the fuse element assembly 208 at the weak portion 241 (Figure 2E). The mechanical constraints of the fuse element assembly 208 are inherent in the design and manufacture of stamped fuse elements, which unfortunately have been found to promote in-plane buckling of the weak portion 241 during repeated load current cycles. This in-plane buckling is the result of damage to the metal grain boundaries, which causes separation or slippage between adjacent metal grains. Such buckling of the weak portion 241 occurs over time and is accelerated and more pronounced with larger transient current pulses. The larger the heating-cooling delta of the transient current pulse, the greater the mechanical effect and therefore the greater the in-plane buckling deformation of the weak portion 241.
[0033] The repeated physical and mechanical manipulation of the metal caused by the heating effect of the transient current pulse then causes changes in the grain structure of the metallic fuse element. These mechanical manipulations are sometimes referred to as working the metal. Working the metal causes strengthening of grain boundaries where adjacent grains are tightly bound to adjacent grains. Overworking the metal results in the fracture of the grain boundaries, causing grains to slide over one another, inducing what are called slip bands or slip planes. This inter-particle sliding and separation results in a localized increase in electrical resistance that accelerates the fatigue process by increasing the heating effect of the current pulse. The formation of slip bands is where fatigue cracks first initiate.
[0034] As will be appreciated, the manufacturing method of stamping or punching metal to form the fuse element assembly 208 will generate localized slip bands at all stamped edges of the weak portion 241 of the fuse element since the stamping process to form the weak portion 241 is a mechanical process of shear and tearing. This tearing process prestresses the weak portion 241 with many slip band areas. The slip bands and fatigue cracks, combined with the above-mentioned buckling due to thermal effects, will ultimately lead to premature structural failure of the weak portion 241 unrelated to an electrical fault condition. Such premature failure modes unrelated to a problematic electrical condition in the power system may be referred to as a disruptive operation of the fuse. Avoiding such disruptive operation is highly desirable in EV power systems from both the perspective of the EV manufacturer and the consumer since the circuit connected to the fuse will not be operational once the fuse element fails until the fuse is replaced. Indeed, given the growing interest in EV vehicles and their power systems, the impact of fuse fatigue is considered a negative Critical to Quality (CTQ) attribute in vehicle design.
[0035] 3 illustrates an alternative power fuse 300 including an element assembly 302 in a housing 308 with terminal blades 304, 306 configured to connect the power fuse 300 to line and load side circuits. Electrical connection of the fuse element assembly 302 is completed via end plates 332, 334 and terminal contact blocks 322, 324 provided on the terminal blades 304, 306. Upon exposure to a predetermined current condition, at least a portion of the fuse element assembly 302 melts, disintegrates, or otherwise structurally fails, opening a circuit path between the terminal blades 304, 306. Thus, the load side circuitry is electrically isolated from the line side circuitry, protecting the load side circuitry components from damage when an electrical fault condition occurs.
[0036] To address the fuse fatigue problem, each fuse element assembly 302 includes a substrate 310, a plurality of weak portions 312 printed on the substrate, and a separately provided free-standing conductor 314 assembled to and interconnected with the substrate 310. For more information, see U.S. Pat. No. 11,087,943, which is incorporated herein by reference. Advantageously, the fuse element assembly 302 does not include stamped or punched weak portions (or associated tearing or shearing of material processes) anywhere in the structure, and thus the power fuse 200 does not suffer from the fuse fatigue problem associated with stamped or punched weak portions. Thus, the power fuse 300 is more suitable for EV power system applications than the power fuse 200, but the manufacture of the fuse is relatively complicated. A simpler yet more reliable fuse manufacture is desired.
[0037] Power fuse 300 may be referred to as a hybrid approach due to the combination of a printed fuse element that defines a weak spot on substrate 310 and a metal conductor 314 that is not a printed element but also does not include punched or stamped features. Conductor 314 improves fuse clearing times and also assists in clearing arc energy in the high voltage, high current DC power system of an EV. It is desired to achieve the desired fuse clearing times in a non-hybrid structure (i.e., one that includes only elements printed on the substrate).
[0038] However, the inventors have recognized that the opening time of fuses in non-hybrid structures may be unacceptably high in EV power systems. For example, in EV power system applications, the desired opening time for an 800% overcurrent is approximately 20 ms, while experimentally observed values for existing non-hybrid fuse structures capable of handling 400 A in a 500 VDC operating system are as high as 300 ms. Furthermore, known non-hybrid printed fuse structures generally cannot contain the arc energy in the operation of the fuse in a high voltage, high current DC power system such as an EV power system.
[0039] Exemplary embodiments of non-hybrid printed fuse elements and methods of manufacturing such fuse elements are described below that advantageously avoid distortion damage in the weak portions from the stamping or punching manufacturing process while providing a desired opening time and effective arc extinguishing mechanism for EV power system applications. The weak portions in the exemplary embodiments are formed directly on the planar substrate via additive printing processes, avoiding micro-tears of material from the punching or stamping process. The entire fuse element is formed on the substrate without the need for the separately provided conductor elements of the hybrid solutions described above. Thus, the manufacturing costs and assembly steps associated with the separately provided conductor elements are avoided.
[0040] 4 and 5 show an exemplary embodiment of a printed manufacture of fuse element assembly 400 proposed to overcome the deficiencies of the fuse elements in power fuses 200 and 300 described above.
[0041] The printed fuse product in the illustrated example includes a substrate 405 and a series of successively printed metal layers 410 on the surface of the substrate. The successively printed layers provide a patterned metallization on the substrate that can act as a fuse element with different thicknesses of metal material provided by the layers of the pattern utilized. The substrate 405 in the contemplated embodiment is fabricated from a known ceramic material, but the metal layers can be silver or another metal or metal alloy known in the art. The metal layers can be copper, copper alloy, aluminum, or aluminum alloy. The metal layers are printed to form thick portions 415 and thin portions 420 separated from one another. The thick portions 415 have more layers than the thin portions 420, and the thin portions 420 function as weakened portions of reduced cross-sectional area to open circuit paths on the substrate at various locations corresponding to the thin portions 420 in the illustrated example, which includes three spaced apart thin portions 420 separated by the thick portions 415 on the substrate 405. As shown in Figure 5, a dielectric layer 425, such as glass, may be printed on the substrate beneath the thin portions 420 that define the weak portions. The metallization layer that defines the thin portions 420 and the thick portions 415 generally covers the entire surface of the substrate 405 in the example of Figures 4 and 5, with the thin portions 420 extending continuously between the thick portions 415. That is, the thin portions 420 cover the entire area between the thick portions 415 across the entire width of the substrate, as shown in Figures 4 and 5.
[0042] The inventors have discovered that the successful (or failure) operation of the printed fuse element 400 in an EV power system depends on the substrate material and thermal conductivity of the substrate 405 balanced with the desired opening time and arc suppression considerations. This presents a complex set of issues that must be reconciled.
[0043] Varying the printed thickness of the weak portions of fuse element 400 can tune the opening time of the fuse. Generally, thinner weak portions open faster than thicker weak portions, but the printing process may exhibit limited ability to achieve some desired opening time with the successive weak portions shown in FIGS.
[0044] The thermal conductivity of the substrate 405 also affects the opening time of the fuse element 400 at the weak portion. In general, a higher thermal conductivity of the substrate 405 will draw heat away from the weak portion, increasing the opening time at the weak portion, while a lower thermal conductivity of the substrate 405 will more efficiently concentrate heat at the weak portion itself, decreasing the opening time at the weak portion.
[0045] The substrate material, and thus its electrical conductivity, also influences the arcing conditions. Certain ceramic substrate materials (e.g., alumina) with higher thermal conductivity may break down when exposed to arcing energy (specifically, heat generated by the arcing) and release elements that may undesirably prolong electrical arcing, whereas substrates with lower thermal conductivity (e.g., forsterite and steatite) may not break down as quickly and release elements that contribute to electrical arcing, thus shortening the arcing burnout time. Thus, electrical arcing burns out faster on lower electrical conductivity substrates than on higher electrical conductivity substrates.
[0046] The dielectric layer 425 shown in FIG. 5 may also affect heat transfer to the substrate 405 during operation of the weak spot and may affect the breakdown point of the substrate 405 and therefore may be a consideration from an arcing management perspective.
[0047] It is recognized that many substrate materials are available having various material properties. For example, alumina oxide (Al2O3) substrate materials are known to range from about 8 Watts per meter-Kelvin (W / (m·K)) to about 32 W / (m·K). In contrast, forsterite substrate materials are known to have a thermal conductivity of about 5 W / (m·K) and steatite substrate materials are known to have a thermal conductivity of about 2 to about 3 W / (m·K). For purposes of the present invention, a thermal conductivity in the range of about 2 to 14 W / (m·K) is preferred for higher voltage, higher current DC power systems such as those discussed above. However, for comparison, experiments have shown that substrates having a thermal conductivity of about 24 W / (m·K) tend to extend the open time to levels that are unacceptable for EV power system applications.
[0048] 6 illustrates another exemplary embodiment of a printed fuse element assembly 600 including further enhancements for EV power system operation. The fuse element assembly 600 includes a substrate 615 metallized with a printed layer of patterned portions of increased and decreased printed thickness. When the metal layer is printed with the increased and decreased printed portions, the decreased printed thickness defines a weak portion for fusible operation of the fusible element 605 printed on the substrate 615. In some embodiments, the substrate 615 has an increased printed thickness of up to about 1.2 mm and a decreased printed thickness that defines a weak portion of up to about 10 microns.
[0049] 4 and 5, the weak portions extend in discrete segments that cover only a portion of the substrate and / or dielectric layer beneath the weak portions and only a portion of the area between the thicker portions. In the illustrated example, the defined weak portions extend with a width dimension substantially less than the substrate width dimension 640 and a length dimension equal to the substrate length dimension 635. In some embodiments, the defined weak portions extend with a width dimension of up to about 5 mm and a length dimension of about 1 mm.
[0050] In the illustrated exemplary embodiment, the fuse element assembly 600 may be at least partially surrounded by an arc extinguishing filler 610. The arc extinguishing filler 610 may extend between the defined weak portions. The material of the arc extinguishing filler 610 is selected to have a relatively high thermal conductivity and absorption capacity. When the defined weak portions melt under a given current condition, an arc may initiate and migrate from the defined weak portions and substrate 615 to the surrounding arc extinguishing filler 610 for efficient cooling and more rapid dissipation.
[0051] In some embodiments, the fusible element 605 printed on the substrate 615 comprises silver. The substrate 615 is a low thermal conductivity substrate. In some embodiments, the substrate 615 may have a thermal conductivity substantially less than 24 W / (m·K). In other embodiments, the substrate 615 may have a thermal conductivity of about 5 W / (m·K) or less.
[0052] In some embodiments, the substrate 615 may be steatite or forsterite, as opposed to an alumina oxide. As magnesium-based substrates, steatite and forsterite absorb more energy than alumina, aluminum-based substrates. Greater energy absorption is desirable to extend the life of the substrate 615 during high current pulses experienced by the fuse element assembly 600 to avoid metal fatigue. In addition to increased energy absorption, steatite and forsterite are silicates, as opposed to metal oxides such as alumina, providing steatite and forsterite with increased arc suppression capabilities to avoid metal fatigue in the fuse element assembly 600.
[0053] Additionally, steatite and forsterite have reduced thermal conductivity compared to alumina oxide, 3 W / m / K for steatite and 5 W / m / K for forsterite. The reduced thermal conductivity is desirable to increase the speed at which the substrate 615 melts and quenches the arc, reducing the melt time of the fuse element assembly 600. An alternative substrate material to alumina is desirable to reduce the melt time to 300 ms at 800% of 300VDC. The use of an alternative substrate material with a lower thermal conductivity, such as steatite, reduces the amount of time required to reach the 800 amp value. Reduced melt times of 16 ms using 0.6 mm thick steatite and 3.3 ms using 0.7 mm thick forsterite can be achieved as opposed to 160 ms using 0.6 mm thick alumina for the substrate 615.
[0054] Additionally, steatite and forsterite have a coefficient of thermal expansion at room temperature that is close to the coefficient of thermal expansion at room temperature of the metal used to print the fusible element 605. A reduced difference in the coefficient of thermal expansion between the substrate 615 and the printed fusible element 605 is desirable to extend the life of the substrate 615 to avoid metal fatigue.
[0055] 7 illustrates an alternative embodiment of a power fuse 700 including a fuse element assembly 600. The fuse element 600 includes a conductor having a flush connector portion mounted over the weak portion and an angled portion extending over the substrate such that an arc-quenching filler can be positioned to surround at least a portion of the fuse element assembly, thereby effectively quenching an arc that occurs after the fuse element assembly opens under a predetermined current condition. The arc-quenching filler can include quartz sand.
[0056] 7 are optional and are not limited by the components shown. For example, power fuse 700 may include alternative housings, alternative structures, and / or more than one fuse element.
[0057] 8 shows a second dielectric layer on the weak portion 810 as part of an alternative fuse element assembly 800. The dielectric layer 815 includes a first dielectric layer on the substrate 805 and a second dielectric layer on the weak portion 810. The dielectric layer 815 may affect heat transfer to the substrate in the operation of the weak portion, may affect the destruction of the substrate, and therefore should be considered from an arcing management perspective. The alternative fuse element assembly 800 may be used in the power fuse 700 instead of the fuse element assembly 600.
[0058] It is believed that the benefits and advantages of the present disclosure have been fully described with respect to the disclosed exemplary embodiments.
[0059] Various embodiments of power fuses and fuse element assemblies and methods of manufacture thereof are described herein, which include a plurality of weak portions formed on a substrate without stamped weak portion openings, thereby avoiding thermo-mechanical fatigue strain of the fuse element assembly when subjected to a transient load current cycle event. Furthermore, the fuse assembly includes a conductor having a coplanar connector portion attached to the weak portion and an obliquely extending portion extending above the substrate such that an arc-quenching filler can be positioned to surround at least a portion of the fuse element assembly, thereby effectively extinguishing an arc that occurs after the fuse element assembly opens under a predetermined current condition.
[0060] Although exemplary embodiments of components, assemblies, and systems have been described, variations of the components, assemblies, and systems can achieve similar benefits and advantages. In particular, the shape and geometry of the components and assemblies, as well as the relative locations of the components within the assemblies, may be varied from that described and illustrated without departing from the inventive concepts described. Also, in certain embodiments, certain components within the assemblies described may be omitted to accommodate the needs of a particular type of fuse or a particular installation, while still providing the required performance and functionality of the fuse.
[0061] An embodiment of a printed fuse is disclosed. The printed fuse includes a substrate and a fusible element printed on the substrate. The fusible element printed on the substrate includes a series of sections of reduced printed thickness each separated by a section of increased printed thickness that define a weakened portion for fusible actuation of the fusible element.
[0062] Optionally, the printed fuse further includes a defined weak portion of about 10 microns thickness extending with a width dimension substantially less than a width dimension of the substrate and a length dimension equal to a length dimension of the substrate. The defined weak portion's width dimension may be about 5 mm or less and the length dimension may be about 1 mm. The arc-quenching filler may extend between the defined weak portions. The defined weak portion opens with a melt time of about 20 ms or less for a current that is 800% of the rated current of the printed fuse. The defined weak portion may open with a melt time of about 10 ms or less for a current that is 800% of the rated current of the printed fuse.
[0063] Optionally, the printed fuse further includes a substrate of low thermal conductivity material having a thermal conductivity substantially less than 24 W / m / K, approximately 1.2 mm thick. The thermal conductivity of the substrate may be approximately 5 W / m / K or less. The printed fuse further includes a first dielectric layer underlying only the weak portion and a second dielectric layer covering only the weak portion. The first and second dielectric layers are glass approximately 12 microns thick.
[0064] Optionally, the printed fuse further comprises a silver fusible element and a steatite or forsterite substrate. The printed fuse has a voltage rating of at least 300V and a current rating of at least 400A.
[0065] This written description uses examples to disclose the invention, including the best mode, and also enables any person skilled in the art to practice the invention, including making and using any devices or systems and performing any incorporated methods. The patentable scope of the invention is defined by the claims, and may include other examples that occur to those skilled in the art. Such other examples are intended to be within the scope of the claims if they have structural elements that do not differ from the literal language of the claims, or if they include equivalent structural elements that are not substantially different from the literal language of the claims.
Claims
1. A substrate; and a fusible element printed on the substrate, the fusible element including a series of portions of reduced printed thickness each separated by a portion of increased printed thickness, the portions of reduced printed thickness defining weakened portions for fusible actuation of the fusible element; having Printed fuse products.
2. the fusible element comprises silver; 2. The printed fuse product of claim 1.
3. The weakened portion has a thickness of about 10 microns.
2. The printed fuse product of claim 1.
4. The substrate has a thickness of about 1.2 mm.
2. The printed fuse product of claim 1.
5. a first dielectric layer underlying only the weakened portion; 2. The printed fuse product of claim 1.
6. the first dielectric layer is glass; 6. The printed fuse product of claim 5.
7. the first dielectric layer and the second dielectric layer having a thickness of about 12 microns; 6. The printed fuse product of claim 5.
8. The substrate is a low thermal conductivity substrate; 2. The printed fuse product of claim 1.
9. The low thermal conductivity substrate has a thermal conductivity substantially less than 24 W / m / K.
9. The printed fuse product of claim 8.
10. The low thermal conductivity substrate has a thermal conductivity of about 5 W / m / K or less.
10. The printed fuse product of claim 9.
11. The substrate is steatite; 2. The printed fuse product of claim 1.
12. The substrate is forsterite; 2. The printed fuse product of claim 1.
13. the substrate has a length dimension and a width dimension, the weakened portion extending in a width dimension substantially less than the width dimension of the substrate; 2. The printed fuse product of claim 1.
14. each of the weakened portions extends in the width dimension as a plurality of separate portions each of which is about 5 mm or less in the width dimension; 14. The printed fuse product of claim 13.
15. the separated portions extend about 1 mm in the length dimension; 15. The printed fuse product of claim 14.
16. an arc-quenching filler material extends between the separated portions; 16. The printed fuse product of claim 15.
17. the weak portion opens with a melt time of about 20 ms or less for a current that is 800% of the rated current of the fuse; 2. The printed fuse product of claim 1.
18. the weak portion opens with a melting time of about 10 ms or less for a current that is 800% of the rated current of the fuse.
20. The printed fuse product of claim 17.
19. The fuse has a rated voltage of at least 300V.
20. The printed fuse product of claim 18.
20. The fuse has a rated current of 400A.
20. The printed fuse product of claim 19.