Method for depositing material into two-dimensional layered materials

A pulsed plasma deposition process addresses the challenge of depositing high-quality dielectric layers on two-dimensional materials by minimizing surface damage and eliminating additional growth steps, facilitating integration into semiconductor manufacturing.

JP2024544271APending Publication Date: 2024-11-28OXFORD INSTR NANOTECHNOLOGY TOOLS LTD
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2024535469
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-12-15
Filing Date
2022-12-14
Publication Date
2024-11-28

AI Technical Summary

Technical Problem

Existing methods for depositing materials onto two-dimensional materials like graphene result in poor-quality dielectric layers due to surface damage from plasma radicals and ions, and require additional steps that hinder scalability.

Method used

A pulsed plasma deposition process is used to deposit a protective layer directly onto the two-dimensional material, followed by a second layer, minimizing exposure to reactive species and reducing damage, while ensuring high-quality deposition without additional growth or transfer steps.

Benefits of technology

The method achieves high-quality layered materials on two-dimensional layers without damage, maintaining the integrity of the underlying material and enabling integration into semiconductor processes.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024544271000001_ABST
    Figure 2024544271000001_ABST
Patent Text Reader

Abstract

1. A method for plasma depositing a material onto a two-dimensional layer of a first substrate, the method comprising: depositing a protective layer directly onto the two-dimensional layer in a pulsed plasma deposition process; and depositing a second layer onto the protective layer in a second plasma deposition process.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for depositing material onto a two-dimensional layered material. [Background technology]

[0002] Two-dimensional materials such as graphene have been demonstrated to enable high performance in a variety of proof-of-concept devices. These materials can be ideally combined with a variety of other materials to provide functional devices. However, the surfaces of two-dimensional materials such as graphene are relatively inert, making it difficult to deposit other materials, such as dielectric layers, onto the surfaces of two-dimensional materials using thermal and plasma-based deposition processes such as atomic layer deposition (ALD). At the same time, the surfaces of two-dimensional materials are susceptible to damage, for example, by plasma radicals and ions generated in plasma processes.

[0003] Attempts have been made to use atomic layer deposition to deposit dielectric layers on two-dimensional materials. For example, atomic layer deposition of Al2O3 on graphene has been attempted by seeding the surface of graphene with evaporated Al, followed by oxidation of the Al to produce Al2O3. Attempts have also been made to perform thermal atomic layer deposition using long dosing times. However, both of these methods result in low quality dielectric layers.

[0004] A high-quality interlayer that can be used to protect graphene during Al2O3 deposition is hBN (hexagonal boron nitride). This material is also inert, but more resistant to damage than graphene, and can therefore be used to protect graphene during plasma-enhanced atomic layer deposition (PEALD). However, deposition of hBN on a graphene surface adds a two-dimensional material growth and transport step to the process flow, making it difficult to scale.

[0005] 2D materials have attracted increasing interest in recent years because they promise to significantly improve the performance of telecommunications and data communication components by enabling ultra-high bandwidth and low power consumption. In addition, the unprecedented surface area / volume ratio of 2D materials, combined with their excellent electronic properties, makes them attractive for a wide range of sensors. Such data communication and sensor applications require the integration of high-quality dielectric layers, especially on graphene and other 2D materials.

[0006] Therefore, there is a need for improved methods for depositing materials into two-dimensional layers. Summary of the Invention

[0007] According to a first aspect of the invention there is provided a method of plasma depositing a material onto a two-dimensional layer of a first substrate, the method comprising depositing a protective layer directly onto the two-dimensional layer in a pulsed plasma deposition process and depositing a second layer onto the protective layer in a second plasma deposition process.

[0008] The first aspect of the invention allows a material to be deposited on a two-dimensional layer (meaning a layer of a two-dimensional material such as graphene) without damaging the two-dimensional layer, while ensuring that the deposited material is of high quality, i.e. the material is deposited in dense closed layers, the interfaces between the layers are clean, there are few physical and electronic defects, and in the case of dielectrics, there is a high breakdown voltage, a high dielectric constant (considered a dielectric constant of 3 or more) and a low leakage current. The properties of two-dimensional materials such as graphene mean that their surfaces have a low density of nucleation sites, and thus have a delayed nucleation of the deposited material. This means that the chemical processes used to deposit these materials must be carried out with sufficient exposure of reactive species (such as plasma species). However, two-dimensional materials are also very sensitive to damage, so that prolonged exposure to reactive species can lead to excessive damage of the two-dimensional material.

[0009] This problem is addressed by the first aspect of the invention by using a pulsed plasma deposition process to initially deposit a protective layer on the two-dimensional layer. A pulsed plasma deposition process is a plasma deposition process in which one or both of the precursor gas and the plasma are pulsed, i.e., the precursor gas and / or the plasma are periodically supplied. In the case of a precursor gas, this means supplying the precursor gas for a first time interval and then purging the deposition chamber (also referred to herein as the process chamber) for a second time interval and repeating this cycle over the course of the deposition process. For the avoidance of doubt, the precursor gas is provided without plasma (as is the case in the first layer of a deposition cycle during plasma enhanced atomic layer deposition), whereas the gas (or gases) provided in the presence of plasma to generate reactive species such as radicals and ions is referred to as the plasma gas (or gases). The plasma is pulsed by pulsing the plasma gas, i.e., supplying the plasma gas for a first time interval and then purging the deposition chamber for a second time interval and repeating this cycle over the course of the deposition process, or by supplying power to the plasma in pulses.

[0010] The use of a pulsed plasma deposition process can ensure that the surface of the two-dimensional layer is sufficiently exposed to reactive species for deposition to occur while minimizing exposure of the two-dimensional layer to reactive species that may damage the two-dimensional layer, such as high energy ions or excessive levels of radicals.

[0011] Therefore, the use of pulsed plasma deposition processes is very effective in reducing damage caused by reactive species. However, depending on the type of radicals and / or the amount of radicals supplied, the reactive radicals used in the pulsed plasma deposition process can damage the two-dimensional layer.

[0012] A particular example of radicals damaging 2D layers occurs when depositing Al2O3 on graphene. Even if damage from ions in the plasma is minimized, oxygen radicals in the plasma gas for depositing Al2O3 have been found to be highly reactive with and damaging to the graphene surface. This also occurs with other material combinations, and avoiding damage from radicals in the plasma gas is a key issue to address.

[0013] In a first aspect of the invention, this is achieved by providing a protective layer that does not exhibit the same sensitivity to damage as the two-dimensional layer, such that a deposition process that would damage the two-dimensional layer can be used to deposit a second layer without damaging either the protective layer or the two-dimensional layer.

[0014] The first aspect of the invention therefore enables a high quality layered material to be deposited onto a two-dimensional layer without damaging said two-dimensional layer.

[0015] The first aspect of the invention is particularly in contrast to the use of an hBN protective layer, as it does not require a separate ex-situ material growth and transfer step. Instead, the deposition of the protective layer is performed in-situ, allowing graphene to be integrated into semiconductor manufacturing processes without the need for additional steps, such as ex-situ seed layer or hBN deposition, which pose significant scaling and infrastructure challenges and therefore device cost issues.

[0016] In the above description and throughout this specification, the terms "on" and "uponto" when used in the context of one layer material being deposited or provided on or above another layered material should not be interpreted as excluding the possibility of depositing or providing one or more intermediate layers. In such cases where there is no intermediate layer between the two layered materials, the phrase "directly on" or "directly onto" is used. For example, in the first aspect of the invention, the protective layer is deposited directly on the two-dimensional layer, meaning there is no intermediate layer. However, one or more intermediate layers may be provided between the protective layer and the second layer.

[0017] For the avoidance of doubt, the first substrate may comprise additional layers in addition to the two-dimensional layer, or alternatively, may only comprise the two-dimensional layer.

[0018] As is evident from the above, the first aspect of the invention is particularly suitable for deposition of materials onto graphene, as damage to the graphene layer is difficult to avoid. In particular, the low density of nucleation sites on the graphene surface makes material deposition difficult, while graphene's susceptibility to damage means that it cannot be overcome simply by using more aggressive deposition processes (i.e. deposition processes involving prolonged exposure to reactive species).

[0019] Other materials that can be used to form the two-dimensional layer and that benefit from the first aspect of the invention include molybdenum disulfide (MoS2), tungsten disulfide (WS2), molybdenum or tungsten selenides, borophene, and silicene.

[0020] For this purpose, the composition of the protective layer is selected to allow the use of plasma gases whose radicals do not damage the underlying two-dimensional layer, examples being metal or semiconductor nitrides, metal or semiconductor carbides, and metal or semiconductor carbonitrides.

[0021] For the avoidance of doubt, the expression "metal or semiconductor nitride" means a nitride of a metal element or a nitride of a semiconductor element. The metal or semiconductor nitride compound itself does not have to be a metal or a semiconductor, but may be, for example, a dielectric. Similarly, the expression "metal or semiconductor carbide" means a carbide of a metal element or a carbide of a semiconductor element, where the metal or semiconductor carbide compound itself does not have to be a metal or a semiconductor, but may be, for example, a dielectric, and the expression "metal or semiconductor carbonitride" means a carbonitride of a metal element or a carbonitride of a semiconductor element, where the metal or semiconductor carbonitride compound itself does not have to be a metal or a semiconductor, but may be, for example, a dielectric.

[0022] For example, AlN is particularly suitable for use as a protective layer for graphene because nitrogen radicals in the plasma gas do not damage graphene if provided in a low enough dose, as opposed to oxygen radicals in the plasma gas used to deposit Al2O3. The second layer may contain oxygen because the first layer shields the sensitive 2D layer from oxidation during processing, and the use of AlN as a protective layer allows the deposition of an Al2O3 layer on the graphene.

[0023] Other layered materials suitable for use as the protective layer include silicon nitride, titanium nitride, silicon carbide, titanium carbonitride, silicon carbonitride, and titanium aluminum nitride.

[0024] The protective layer preferably comprises a dielectric. As is evident from the above description, in many embodiments of the present invention, the second layer comprises a dielectric. In such cases, it is advantageous for the protective layer to also comprise a dielectric, since it forms the first interface with the two-dimensional layer. A dielectric protective layer can also be advantageous when the second layer (or any intermediate layer between the protective layer and the second layer) is a metal layer, since the protective layer can be configured to function as a dielectric tunnel barrier. For example, a titanium nitride (TiN) layer can be provided directly on a protective layer formed from AlN. However, in other embodiments, the protective layer can also be formed from a metal layer or a semiconductor layer, such as TiN.

[0025] It is particularly advantageous for one or both of the protective layer and the second layer to comprise a high-k dielectric, ie, a dielectric having a dielectric constant of 3 or greater.

[0026] To minimize damage to the two-dimensional layer and maximize the quality of the protective layer, the pulsed plasma deposition process advantageously comprises a plasma-enhanced atomic layer deposition process.

[0027] The plasma enhanced atomic layer deposition process is an example of a pulsed plasma deposition process, which is a cyclic deposition process carried out under near vacuum conditions, with a maximum pressure of about 1 mbar during the process. First, a precursor (commonly referred to as a precursor vapor, which can be a gas or, in some cases, a liquid that has been highly diffusively evaporated under low pressure) is supplied into the deposition chamber together with the substrate on which the material to be deposited is attached. The precursor reacts with the substrate surface in a self-limiting reaction. That is, the reaction ends when all nucleation sites on the substrate surface have reacted with the precursor, forming a solid thin film of adsorbed species (usually less than one atom thick) on the substrate surface. The excess precursor is then purged from the deposition chamber (typically by supplying a purge gas such as argon), and then a plasma is used to supply radicals that react with the adsorbed species on the substrate surface, providing new reaction sites for the precursor to adsorb in the next step, leaving the deposited layered material. Any reaction products formed are then purged from the deposition chamber, and the process is repeated as many times as necessary to leave the desired number of deposited layered materials.

[0028] In plasma-enhanced atomic layer deposition, the plasma is only supplied for a small portion of each deposition cycle, thereby reducing the time that the substrate is exposed to the ions and radicals in the plasma. This means that when plasma-enhanced atomic layer deposition is used to deposit a protective layer, the resulting exposure of plasma species on the two-dimensional layer of the first substrate can be easily controlled, especially when the composition of the protective layer is selected such that the radicals formed in the plasma used to deposit the protective layer do not damage the two-dimensional layer of the first substrate. For example, the plasma used to deposit AlN on a graphene layer contains reactive species such as nitrogen radicals, which do not damage the surface of the graphene layer if supplied in a sufficiently low dose. Thus, low-energy plasma-enhanced atomic layer deposition is particularly suitable for depositing a protective layer directly on the two-dimensional layer of the first substrate.

[0029] An alternative to plasma enhanced atomic layer deposition is pulsed plasma enhanced chemical vapor deposition. In plasma enhanced chemical vapor deposition, a large number of reactive species are present in the plasma, which react with the surface of the substrate to form the deposited layered material. In general, this means that ions and (potentially damaging) radicals are present throughout the deposition process, which can damage substrates made of sensitive materials, such as the two-dimensional layer of the first substrate in the first aspect of the invention. This can be mitigated by pulsing the power to the plasma source and / or pulsing the supply of plasma gas to the deposition chamber, which can reduce the exposure of the substrate to ions and / or radicals. Nevertheless, plasma enhanced atomic layer deposition is preferred over pulsed plasma enhanced chemical vapor deposition, as it generally causes less damage to the substrate and allows for more precise layer thickness and quality control of the layer / film. This is because in plasma enhanced atomic layer deposition, the plasma is only supplied for a small portion of the deposition cycle. Even though the power to the plasma is pulsed in a pulsed plasma-enhanced chemical vapor deposition process, the plasma typically exists for a longer time than in a comparable plasma-enhanced atomic layer deposition process, resulting in greater damage to the substrate from ions and / or radicals. Also, plasma-enhanced atomic layer deposition deposits the deposited material in layers one atom thick, resulting in a more uniform and dense deposited layer, whereas plasma-enhanced chemical vapor deposition does not provide such precise control over the deposition of material.

[0030] In order to further reduce damage to the two-dimensional layer, the plasma used in the pulsed plasma deposition process is preferably low energy, i.e., the power supplied to the plasma source is 100 W or less, or more preferably 25 W or less. In the specific case of a low-energy PEALD process, a "low-energy PEALD process" can also be defined as a PEALD process in which the ion flux to the wafer during any plasma step is 0.2 mA per square centimeter or less, and the ion energy is 30 eV or less. Suitable plasma sources are described in GB2577697. The use of a low-energy plasma results in the generation of fewer ions, and means that the ions reaching the substrate have less energy, thereby reducing the damage caused to the two-dimensional layer.

[0031] Deposition of the protective layer means that any conventional deposition process can be used to deposit the second layer, including a non-pulsed plasma deposition process such as non-pulsed plasma enhanced chemical vapor deposition. Nevertheless, it is preferred that the second plasma deposition process comprises a pulsed plasma deposition process such as plasma enhanced atomic layer deposition or pulsed plasma enhanced chemical vapor deposition.

[0032] Although the protective layer is less susceptible to damage than the two-dimensional layer, it is nevertheless desirable to reduce the likelihood of damage to the protective layer (and possibly the two-dimensional layer below it). Also, the second plasma deposition process is preferably of the same type as the pulsed plasma deposition process used to deposit the second layer. This means that it is easier to perform both processes in the same deposition chamber. For example, it is easier to perform two plasma-enhanced atomic layer deposition processes in the same chamber than to provide a deposition chamber in which the protective layer can be deposited with a plasma-enhanced atomic layer deposition process and the second layer can be deposited with another pulsed plasma deposition process such as pulsed chemical vapor deposition. For this reason, and because of the advantages of plasma-enhanced atomic layer deposition discussed above, it is preferred that the protective layer and the second layer are both deposited with a plasma-enhanced atomic layer deposition process.

[0033] Nonetheless, in preferred embodiments of the first aspect of the invention, the protective layer and the second layer are formed from different layered materials, and thus, even in embodiments where the same type of deposition process is used to deposit both layers, the deposition process itself differs to suit the materials deposited to form each layer.

[0034] In order to reduce or eliminate the presence of potentially harmful radicals (such as oxidizing radicals in the case of graphene 2D layers) in the deposition chamber or chambers used to deposit the protective layer and the second layer, the method of the first aspect of the invention preferably includes one or more conditioning steps.

[0035] To this end, the step of depositing the protective layer is preferably carried out in a first deposition chamber, and the method further comprises, prior to the step of depositing the protective layer, depositing a protective layer on a second substrate in the first deposition chamber, removing the second substrate from the first deposition chamber, and providing the first substrate to the first deposition chamber.

[0036] In this conditioning step, a protective layer having a similar composition to the protective layer deposited on the first substrate is deposited on the second substrate. This significantly reduces the level of undesired species such as oxygen that may be present in the deposition chamber, in the plasma used in the pulsed plasma deposition process, or on the deposition chamber walls. This improves the subsequent deposition of the protective layer by reducing the possibility of damage to the two-dimensional layer of the first substrate and the possibility of defects in the deposited layered material.

[0037] This first conditioning step may also include depositing a protective layer in a first deposition chamber without a substrate being present in said chamber to condition the first chamber.

[0038] For similar reasons, a chamber conditioning step may be performed prior to the step of depositing the second layer.

[0039] The step of depositing the second layer may be carried out in a second deposition chamber using a method comprising the steps of depositing a third layer on a third substrate in the second deposition chamber prior to the step of depositing the second layer, removing the second substrate from the second deposition chamber, and providing the first substrate in the second deposition chamber. However, the first deposition chamber is preferably the second deposition chamber, i.e. both the step of depositing the protective layer and the step of depositing the second layer, together with one or both conditioning steps, are preferably carried out in the same deposition chamber.

[0040] This second conditioning step may also include depositing the protective layer in a first deposition chamber without the substrate being present in said chamber so as to condition the first chamber.

[0041] According to a second aspect of the invention there is provided a method of depositing material onto a two-dimensional layer of a first substrate, the method comprising depositing a protective layer directly onto the two-dimensional layer in a radical enhanced atomic layer deposition process and depositing a second layer onto the protective layer in a second deposition process.

[0042] A second aspect of the invention provides an alternative method of depositing material onto a two-dimensional layer without damaging the two-dimensional layer and while ensuring that the deposited material is of high quality, i.e. that defects in the layer of deposited material are reduced.

[0043] As mentioned above, the surface of a two-dimensional material such as graphene has a low density of nucleation sites and is highly sensitive to damage, so deposition processes involving long exposure to reactive species are generally inappropriate and lead to excessive damage of the two-dimensional layer. This problem is solved according to the second aspect of the present invention by using a radical-enhanced atomic layer deposition process.

[0044] The radical-enhanced atomic layer deposition process is another form of pulsed plasma deposition and is similar to the plasma-enhanced atomic layer deposition process in that both are cyclic deposition processes in which a first precursor is delivered to deposit adsorbed species on the surface of the substrate and then purged from the deposition chamber in each deposition cycle. However, rather than exposing the substrate to a plasma, the radical-enhanced atomic layer deposition process uses a flux of reactive species comprised essentially of radicals or a mixture of radicals and a non-ionized gas with little or no ionized species to deliver reactive species that react with the adsorbed species on the substrate surface.

[0045] One way to supply the radical gas is to supply the plasma to a separate plasma chamber from the deposition chamber in which the substrate is located, and direct the radical stream toward the deposition chamber. Because the mean free path of ions in a plasma is much shorter than the mean free path of radicals, the plasma chamber can be designed so that at most a negligible percentage of the ions in the plasma chamber reach the deposition chamber. Thus, the substrate is not exposed to enough ions to damage its surface.

[0046] Nevertheless, the radical-enhanced atomic layer deposition process is preferably a hot-wire-assisted atomic layer deposition (HWALD) process. In a hot-wire-assisted atomic layer deposition process, a flux of radicals is provided by heating a precursor gas to a temperature in the range of 1300°C to 2000°C using a hot wire (such as a tungsten filament) to dissociate molecules in the precursor gas to form radicals that undergo little or no ionization. The radicals react with adsorbed species on the substrate surface to form the layered material.

[0047] The hot-wire assisted atomic layer deposition process has the advantage that no ions are formed that can damage the substrate surface.

[0048] Many of the same considerations discussed in relation to the first aspect of the invention also apply to the second aspect of the invention, for example the second aspect of the invention is particularly advantageous when the two-dimensional layer comprises graphene.

[0049] Similarly, the protective layer and / or the second layer preferably comprise a dielectric material, and it is particularly advantageous if one or both of the protective layer and the second layer comprise a high-k dielectric, i.e. a dielectric having a dielectric constant of 3 or higher.

[0050] It is also preferred that the protective layer comprises a metal or semiconducting nitride; a metal or semiconducting carbide; or a metal or semiconducting carbonitride.

[0051] The protective layer is deposited in a radical enhanced deposition process, while the second deposition process may comprise a plasma deposition process, which is advantageously a pulsed plasma deposition process such as plasma enhanced atomic layer deposition or pulsed chemical vapor deposition. The protective layer and the second layer are preferably formed from different materials, which may be preferred if the second layer is formed from a material that is more easily deposited in a plasma deposition process than in other deposition processes.

[0052] The deposition chamber or chambers used in the second aspect of the invention may also be subjected to the conditioning steps described above with reference to the first aspect of the invention.

[0053] The present invention will now be described with reference to the accompanying drawings. [Brief description of the drawings]

[0054] [Figure 1] FIG. 1 illustrates an exemplary plasma processing tool suitable for use in embodiments of the present invention. [Figure 2(a)] 2a, 2b, and 2c show a comparison of the Raman spectra of the substrate before and after deposition of the second layer. [Figure 2(b)] 2a, 2b, and 2c show a comparison of the Raman spectra of the substrate before and after deposition of the second layer. [Figure 2(c)] 2a, 2b, and 2c show a comparison of the Raman spectra of the substrate before and after deposition of the second layer. [Diagram 3] 1 is a cross-sectional view of a device manufactured in accordance with an embodiment of the present invention. [Figure 4] 1 is a cross-sectional view of a device manufactured in accordance with another embodiment of the present invention. [Diagram 5] FIG. 5 is a perspective view of the device shown in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0055] A schematic example of an exemplary plasma processing tool 101 for use in a process according to an embodiment of the present invention is shown in FIG.

[0056] The plasma processing tool 101 includes a process chamber 102 (also referred to herein as a deposition chamber), which typically includes a near vacuum established by a vacuum pumping system (not shown). Inside the chamber 102 is a substrate table 111, on which a substrate 104 to be processed using the plasma processing tool 101 can be placed. The substrate table 111 is configured to be electrically connected to a signal generator 112, which is configured to electrically bias the substrate table 111 with an RF waveform, as described further below. Alternatively, the substrate table 111 may be grounded, as in an exemplary embodiment described below with reference to FIG. 2. The substrate table 111 may be supported by a lift 113 that is controllable to raise or lower the substrate table 111 to a selected height within the chamber 102. This may be used, for example, to move the table 111 between a substrate loading position and a substrate processing position, the substrate processing position forming a smaller volume inner chamber for rapid change of gas species in a cyclic process. The chamber 102 is also provided with means (not shown) for loading and unloading the substrate 104 onto the table 111 without breaking vacuum, referred to herein as a cassette load lock.

[0057] An electrode array 200 is supported within the chamber 102 above the substrate table 103. The electrode array 200 may include a panel (not shown) that forms part or all of the upper wall of the plasma chamber 102. The electrode array 200 includes a series of alternating ground electrodes (i.e., electrically grounded electrodes, not shown) and one or more live electrodes (not shown), which are electrically connected to a power supply 270. The power supply 270 is configured to electrically power the live electrodes to generate a voltage between the live and ground electrodes. In use, a precursor gas or plasma for plasma generation may be supplied to the electrode array 200, and the voltage between the live and ground electrodes causes the gas to break down into plasma. The electrode array 200 and the power supply 270 are part of a plasma generation apparatus 300.

[0058] The plasma processing tool 101 includes one or more gas sources, as shown at 105a, 105b. The number and type of gas sources provided depend on the nature of the plasma process being performed. For example, if a layered material is to be deposited (e.g., in an atomic layer deposition process), the gas source includes one or more gases for that chemical reaction. In addition to depositing a protective layer and a second layer, embodiments of the invention can include depositing a further layered material or etching a layered material. If the process includes etching a material, the gas source includes one or more etchant gases. Some processes, such as the Bosch etch process, include both deposition and etching, so both types of gases are available. Any of these reactive gases can be converted into a plasma by the apparatus 300. However, in some cases, additional gases may be provided specifically for plasma generation. Examples of gases suitable for plasma generation include noble gases (e.g., neon, Ne, and xenon, Xe), oxidizing gases (e.g., oxygen, O2, and nitrous oxide, N2O), reducing gases (e.g., hydrogen, H2), and nitrogen-containing gases (e.g., molecular nitrogen, N2, and ammonia, NH3). One or more of the gas sources may also provide a purge gas to limit the ingress of other gases and / or to evacuate the gas environment prior to forming the chamber 102. The purge gas may be, for example, a stable gas such as N2 or argon (Ar).

[0059] As a specific example, a typical cyclic plasma-enhanced atomic layer deposition (ALD) process has the following steps in each cycle: - Precursor gas administration - A pump or purge step that removes the precursor gas from the chamber and leaves the adsorbed species on the substrate surface. - Exposure to plasma-excited gases to react with adsorbed species to form a solid thin film on the substrate - Optionally, a pumping or purging step to remove the plasma excited gas from the chamber.

[0060] It is advantageous to have cycle times as short as possible to minimize plasma exposure time. Low pressures are used for the process, typically up to 1 mbar absolute. Most of the inner surfaces of the process chamber are coated simultaneously with the substrate, and the coating power to the plasma must be reliable, even if the deposited layer is conductive. The precursor gases used in many ALD processes are vapors and tend to condense easily unless all surfaces are heated, typically in the range of 100-200 °C.

[0061] In the apparatus depicted in FIG. 1, the plasma generating gas source 105a is shown as supplying gas directly into the chamber 102 through its wall, while the gas source 105b is shown as supplying gas through the electrode array 200, but in practice either or both options may be employed for different gases. For example, reactive gases for the plasma treatment step may be supplied through the wall of the chamber (i.e., according to source 105a), while a conduit through the electrode array 200 (i.e., according to source 105b) may be used to supply a purge gas during the plasma treatment step, as will be further described below. Also, there may be multiple gas introduction points into the process chamber for each gas source, if desired. The supply of precursor gases and plasma generating gases from the sources 105a, 105b to the chamber 102 may be controlled using the respective valves 106a, 106b. The valves are preferably adjusted for the injection of short gas pulses.

[0062] The plasma processing tool 101 is connected to a control unit 121 which may be commanded by a processor 122. The control unit 121 may control, for example, the power supply 270, the signal generator 112, the valves 106a, 106b and the lift 113 in accordance with the process being performed on the substrate.

[0063] In a preferred embodiment of the invention, the protective layer and the second layer are deposited in a plasma enhanced atomic layer deposition process using the apparatus described above, with the substrate table grounded.

[0064] The first stage of the process (optional) is to condition the deposition chamber by depositing an approximately 100 nm thick layer of AlN on a dummy wafer using TMA (trimethylaluminum) precursor and N2 / Ar mixed plasma to passivate the chamber walls and remove the presence of unwanted radicals (especially oxygen radicals) in the plasma. This is followed by supplying the plasma with 100 W RF power for 4 seconds and finally purging for 2 seconds. The pressure in the deposition chamber is 400 mtorr.

[0065] Then, in the second step of the process, a protective layer of AlN is deposited. The substrate used in this step is made by transferring graphene onto a 6-inch (15 cm) Si wafer covered with 90 nm of thermally grown SiO2.

[0066] In this step, N2 and Ar gas are pulsed along with the TMA precursor. A plasma is then applied for 100 ms with RF power ranging from 25 W to 100 W. The pressure in the deposition chamber remains at 400 mtorr.

[0067] The same precursor and plasma gas mixture is used in the first and second stages, but the second stage uses lower RF power of the plasma source and shorter plasma time. The mild plasma conditions and low temperature allow the growth of a thin layer of AlN without etching the underlying graphene. In doing so, the AlN protective layer effectively protects the graphene and forms functional groups that allow the subsequent growth of an Al2O3 film without damaging the graphene.

[0068] Stage 3 includes an (optional) chamber conditioning stage prior to Al2O3 deposition. Prior to this stage, the substrate processed in step 2 is transferred to a cassette load lock without breaking vacuum. The chamber is then conditioned by depositing an approximately 70 nm thick Al2O3 layer on a dummy wafer using a TMA precursor and an O2 / Ar mixture plasma to passivate the chamber walls to eliminate the presence of unwanted radicals in the plasma.

[0069] In this step, O2 and Ar are pulsed together with TMA. Then, the plasma is turned on for 100 ms with an RF power of 100 W. The pressure in the deposition chamber is 400 mTorr in this step.

[0070] In the final stage, the dummy substrate is removed and the substrate processed in step 2 is transferred from the cassette load lock to the deposition chamber. Al2O3 is then deposited using the same process as in stage 3. The protective layer allows the substrate table temperature to be increased without damaging the device, and this high temperature improves the quality and uniformity of the Al2O3 layer.

[0071] The AlN deposition and subsequent material deposition can also be performed in separate chambers using a vacuum transfer cluster tool.

[0072] To investigate the structural changes of graphene due to encapsulation, we directly recorded Raman spectra of graphene before and after encapsulation. Figures 2a to 2c show the Raman spectra of Gr / SiO2 / Si wafers before and after Al2O3 deposition, with and without an AlN protective layer.

[0073] Generally, the Raman spectrum of graphene shows peaks at specific wavenumbers. The most prominent peak is the D peak at 1350 cm. -1 Near the G peak at 1582cm -1 and the 2D peak at 2700 cm -1 The D peak provides information about the number of defects in the graphene lattice, and a larger D peak indicates more defects and damage to the graphene lattice. As shown in Figure 2a, no D peak is observed before the dielectric deposition, indicating good graphene quality. For the device without the AlN protective layer, after encapsulation, the D peak is observed at 1350 cm -1A clear D peak is observed near the junction, indicating that direct deposition of Al2O3 on graphene without a protective layer significantly damages the graphene. In the device protected with an AlN protective layer, the D peak is negligible, indicating that the graphene layer is efficiently protected.

[0074] The intensity ratio of the D peak and the G peak (I D / I G ) is typically used to measure the defect level of graphene. Figure 2b shows the histogram of ID / IG obtained from the Raman maps. For the Al2O3 encapsulated device without the AlN protective layer, the ID / IG increases significantly from 0.05 to 1.27. This is mainly due to the damage of the graphene lattice caused by the O2 plasma exposure. On the other hand, for the AlN protected sample, the I D / I G is similar, 0.035 compared to 0.05 for graphene, the difference being due to a reduction in noise levels caused by changes in the interference pattern.

[0075] Another useful index is the full width at half maximum (FWHM) of the 2D peak, which represents the strain change of graphene. The lower the FWHM(2D), the smaller the strain fluctuation of graphene and the higher the carrier mobility. The histogram of FWHM(2D) obtained from the Raman map is shown in Figure 2c. For the sample without the AlN protective layer, the FWHM(2D) is 34 cm -1 From 43cm -1 In contrast, the sample with the AlN protective layer showed a significant increase of 34 cm -1 36cm from the vicinity -1 The increase has been moderate.

[0076] The following is a brief description of examples of devices manufactured in accordance with some embodiments of the present invention.

[0077] A first such example of a device 300 is depicted in Figure 3, in which a protective layer 302 is provided directly on a substrate 301, on which an additional layer 303 is provided. The upper layer of the substrate 301 is a two-dimensional layer, i.e. a layer of a two-dimensional material, and the substrate 301 may include one or more additional layers.

[0078] 4 and 5 show more complex structures provided according to the same principle. In this case, a semiconductor device 400 is provided in which a substrate 401 includes a back gate 402, a Si layer 403, a SiO2 layer 404 and a graphene layer 405. As can be seen, the graphene layer does not extend over the entire surface of the SiO2 layer 404. In an embodiment of the invention used to manufacture the device 400, a protective AlN layer 406 is deposited on the substrate 401 as a first layer, followed by an Al2O3 layer 407, and finally the source 408, drain 409 and top gate 410 layers. However, it is also possible that one or both of the source 408 and drain 409 layers are provided before the AlN 406 and / or Al2O3 407 layers. [Explanation of symbols]

[0079] 300 devices 301 Substrate 302 Protective layer 303 Additional layer

Claims

1. 1. A method for plasma deposition of a material onto a two-dimensional layer of a first substrate, comprising the steps of: depositing a protective layer directly onto the two-dimensional layer in a pulsed plasma deposition process; depositing a second layer on the protective layer in a second plasma deposition process; A method comprising:

2. The plasma deposition method of claim 1 , wherein the two-dimensional layer comprises graphene.

3. The plasma deposition method of any of claims 1 to 2, wherein the protective layer comprises a dielectric material.

4. The plasma deposition method of any of claims 1 to 3, wherein the protective layer comprises a metal or semiconducting nitride, a metal or semiconducting carbide, or a metal or semiconducting carbonitride.

5. The plasma deposition method of any of claims 1 to 4, wherein the pulsed plasma deposition process comprises a plasma enhanced atomic layer deposition process or a pulsed plasma enhanced chemical vapor deposition process.

6. The plasma deposition method of any of claims 1 to 5, wherein the step of depositing a protective layer directly onto the substrate in a plasma enhanced atomic layer deposition process comprises using a low energy plasma.

7. The plasma deposition method of any of claims 1 to 6, wherein the second plasma deposition process comprises a pulsed plasma deposition process.

8. The plasma deposition method of claim 7 , wherein the second plasma deposition process comprises a plasma enhanced atomic layer deposition process or a pulsed plasma enhanced chemical vapor deposition process.

9. The plasma deposition method of any of claims 1 to 8, wherein the second layer comprises a dielectric material.

10. 10. The plasma deposition method of at least claim 3 or 9, wherein the protective layer and / or the second layer each have a dielectric constant greater than 3.

11. The plasma deposition method of any of claims 1 to 10, wherein the protective layer and the second layer are formed from different materials.

12. The step of depositing a protective layer is performed in a first deposition chamber; 12. The plasma deposition method of claim 1, further comprising the steps of depositing a protective layer on a second substrate in the first deposition chamber prior to the step of depositing a protective layer, removing the second substrate from the first deposition chamber, and providing the first substrate to the first deposition chamber.

13. the step of depositing a second layer is performed in a second deposition chamber; 13. The plasma deposition method of claim 1, further comprising the steps of: depositing a third layer on a third substrate in the second deposition chamber prior to the step of depositing a second layer; removing the second substrate from the second deposition chamber; and providing the first substrate to the second deposition chamber.

14. 14. The plasma deposition method of claim 12 or 13, wherein the first deposition chamber is the second deposition chamber.

15. 1. A method for depositing a material onto a two-dimensional layer of a first substrate, comprising the steps of: depositing a protective layer directly onto the two-dimensional layer in a radical enhanced atomic layer deposition process; depositing a second layer on the protective layer in a second deposition process; The deposition method comprising:

16. 16. The deposition method of claim 15, wherein the radical enhanced atomic layer deposition process is a hot wire assisted atomic layer deposition process.

Citation Information

Patent Citations

  • FORMATION OF SiOCN THIN FILM

    JP2017092475A

  • Single- and multilayer silicene prepared by plasma-enhanced chemical vapor deposition.

    JP2020531682A

  • Conformal damage-free encapsulation of chalcogenide materials

    US20200066987A1

  • Method for forming aluminum oxide film using Al compound containing alkyl group and alkoxy or alkylamine group

    US8784950B2

  • Graphene integration

    WO2021168134A1