Multi-layer wiring board

The multilayer wiring board addresses performance issues by incorporating a CuxSny alloy bonding layer and plating method to enhance electrical, thermal, and mechanical properties, reducing via hole diameter and overall size.

JP2024544299AActive Publication Date: 2024-11-28LG INNOTEK CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
JP2024535971
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-12-16
Filing Date
2022-11-25
Publication Date
2024-11-28
Estimated Expiration
2042-11-25

AI Technical Summary

Technical Problem

Conventional multilayer wiring boards face issues with reduced mechanical, thermal, and electrical properties due to voids and flux generation in conductive layers formed by conductive paste, leading to alloy formation with varying composition ratios, which affects adhesive strength and overall performance.

Method used

A multilayer wiring board design featuring a conductive layer within via holes and a bonding layer made of alloys like CuxSny, with adjusted proportions to enhance thermal, mechanical, and electrical properties, and a plating method to reduce via hole diameter.

Benefits of technology

The design improves adhesive force, electrical conductivity, thermal stability, and mechanical strength while reducing the overall size of the multilayer wiring board by using a bonding layer with optimized alloy composition and plating methods.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024544299000001_ABST
    Figure 2024544299000001_ABST
Patent Text Reader

Abstract

A multilayer wiring board according to one embodiment includes a plurality of insulating layers stacked in sequence, and a wiring pattern disposed on the insulating layers, the insulating layers including at least one via hole, a conductive layer disposed inside the via hole, and an adhesive layer disposed between the wiring pattern and the conductive layer, the adhesive layer including at least one of a first region and a second region having a chemical formula of CuxSny, the value of x / x+y of the second region being greater than the value of x / x+y of the first region, and the volume or area of ​​the second region being greater than the volume or area of ​​the first region.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The embodiment relates to a multilayer wiring board. [Background technology]

[0002] A multilayer wiring board is an insulating board on which a circuit line pattern is formed using a conductive material such as copper. The term "multilayer wiring board" refers to a board immediately before electronic components are mounted.

[0003] Signals generated from components mounted on the multilayer wiring board can be transferred via wiring patterns connected to each component.

[0004] Such a multilayer wiring board can be manufactured by thermocompression bonding a plurality of insulating substrates on which wiring patterns are formed, that is, the multilayer wiring board can be formed by bonding a plurality of insulating layers by thermocompression bonding.

[0005] The multilayer wiring board includes via holes formed in each insulating layer to electrically connect wiring patterns disposed on different insulating layers.

[0006] The via holes are filled with a conductive material, and wiring patterns disposed on different insulating layers are electrically connected to each other through a conductive layer formed of the conductive material.

[0007] Conventionally, the interior of the via hole is filled with a conductive paste to form a conductive layer, and therefore the via hole must have a size equal to or larger than a width set for filling the conductive paste, which increases the size of the multilayer wiring board.

[0008] In addition, the conductive paste contained foreign materials, which resulted in voids and flux being generated inside the conductive layer formed by hardening the paste, and the mechanical strength of the conductive layer inside the via hole was reduced due to the voids and flux.

[0009] In addition, when the conductive paste containing different materials is subjected to thermocompression bonding, multiple alloy layers are formed due to the reaction of the different materials. That is, the conductive layer inside the via hole contains multiple alloys with different composition ratios. This causes problems such as reduced electrical and thermal properties of the conductive layer and reduced adhesive strength with the wiring pattern.

[0010] This causes a problem that the mechanical, thermal and electrical properties of the multilayer wiring board including the conductive layer are reduced.

[0011] Therefore, a multilayer wiring board having a new structure capable of solving the above problems is required. Summary of the Invention [Problem to be solved by the invention]

[0012] The embodiments seek to provide a multilayer wiring board having improved electrical, mechanical, and thermal properties. [Means for solving the problem]

[0013] A multilayer wiring board according to one embodiment includes a plurality of insulating layers stacked in sequence, and a wiring pattern disposed on the insulating layers, the insulating layers including at least one via hole, a conductive layer disposed inside the via hole, and an adhesive layer disposed between the wiring pattern and the conductive layer, the adhesive layer including at least one of a first region and a second region having a chemical formula of CuxSny, the value of x / x+y of the second region being greater than the value of x / x+y of the first region, and the volume or area of ​​the second region being greater than the volume or area of ​​the first region. Effect of the Invention

[0014] The multilayer wiring board according to the embodiment includes a via hole for connecting a plurality of wiring patterns, a conductive layer disposed inside the via hole, and a bonding layer between the conductive layer and the wiring pattern.

[0015] The bonding layer may include at least one alloy. In particular, the bonding layer may include at least one alloy having a formula of CuxSny.

[0016] At this time, the alloy ratio of the bonding layer may be adjusted. In particular, the bonding layer may include a first copper-tin alloy and a second copper-tin alloy. The bonding layer may include a higher ratio of the first copper-tin alloy than the second copper-tin alloy. This may improve the thermal properties, electrical properties, mechanical properties, and adhesive properties with metals of the bonding layer.

[0017] Therefore, the multilayer wiring board according to the embodiment can improve the adhesive strength between the wiring pattern and the conductive layer through the bonding layer, and can have improved electrical properties, mechanical properties, and thermal properties through the adhesive layer.

[0018] The bonding layer is disposed both inside and outside the via hole, and the thickness of the bonding layer is smaller than the thickness of the conductive layer inside the via hole. That is, the conductive layer is disposed in a larger amount inside the via hole than the bonding layer.

[0019] Therefore, it is possible to prevent the electrical, mechanical and thermal properties inside the via hole from being deteriorated.

[0020] In addition, the bonding layer may be disposed inside the via hole between a side surface of the conductive layer and an inner side surface of the via hole, and thus the bonding layer can protect the conductive layer inside the via hole, thereby preventing an external impact from being directly transmitted to the conductive layer inside the via hole.

[0021] In addition, in the multilayer wiring board according to the embodiment, the conductive layer and the bonding layer may be disposed inside the via hole through a plating method and a thermocompression method, so that the diameter of the via hole may be reduced compared to filling the inside of the via hole with a paste method, and therefore the overall size of the multilayer wiring board may be reduced. [Brief description of the drawings]

[0022] [Figure 1] FIG. 1 is a cross-sectional view of a multilayer wiring board according to an embodiment of the present invention. [Diagram 2] 1A to 1C are diagrams for explaining a bonding process for a multilayer wiring board according to an embodiment of the present invention. [Diagram 3] FIG. 2 is an enlarged view of region A in FIG. [Figure 4] FIG. 4 is an enlarged view of region C in FIG. [Diagram 5] FIG. 4 is an enlarged view of region C in FIG. [Figure 6] 5A to 5C are diagrams for explaining changes in composition and composition ratio of a bonding layer of a multilayer wiring board according to an example. [Figure 7] 1 is a table for explaining the characteristics of a pass layer inside a bonding layer of a multilayer wiring board according to an example. [Figure 8] FIG. 2 is an enlarged view of region B in FIG. [Figure 9] FIG. 2 is an enlarged view of region B in FIG. [Figure 10] FIG. 2 is an enlarged view of region B in FIG. [Figure 11] FIG. 2 is an enlarged view of region B in FIG. [Figure 12] FIG. 13 is a diagram showing an optical photograph of a bonding layer according to an example. [Figure 13] 5A and 5B are diagrams for explaining the distribution of grain sizes of bonding layers according to an example and a comparative example, respectively. [Figure 14] 5A and 5B are diagrams for explaining the distribution of grain sizes of bonding layers according to an example and a comparative example, respectively. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0023] Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the accompanying drawings. However, the technical concept of the present invention is not limited to some of the embodiments described, and may be realized in various different forms, and one or more of the components of the embodiments may be selectively combined or substituted within the scope of the technical concept of the present invention.

[0024] Furthermore, unless otherwise clearly and specifically defined, terms (including technical and scientific terms) used in the embodiments of the present invention may be interpreted as having a meaning commonly understood by a person of ordinary skill in the art to which the present invention belongs, and commonly used terms such as predefined terms may have their meaning interpreted taking into account the contextual meaning of the relevant art.

[0025] In addition, the terms used in the examples of the present invention are intended to describe the examples and are not intended to limit the present invention. In the present specification, the singular form can include the plural form unless otherwise specified in the phrase, and when described as "A and (and) at least one (or more) of B and C", it can include one or more of all combinations that can be combined with A, B, and C.

[0026] In addition, in describing the components of the present invention, terms such as first, second, A, B, (a), (b), etc. are used. Such terms are merely used to distinguish the components from other components, and are not intended to limit the essence, order, or sequence of the components.

[0027] Furthermore, when a component is described as being "coupled," "coupled," or "connected" to another component, it includes not only cases where the component is directly coupled, coupled, or connected to the other component, but also cases where the component is "coupled," "coupled," or "connected" by another component between the component and the other component.

[0028] In addition, when it is described as being formed or disposed "on or under" each component, "on or under" includes not only the case where the two components are in direct contact with each other, but also the case where one or more other components are formed or disposed between the two components.

[0029] In addition, when it is expressed as "above" or "below," it can mean not only the upward direction but also the downward direction based on one component.

[0030] Hereinafter, a multilayer wiring board according to an embodiment will be described with reference to the drawings. The multilayer wiring board described below can include a rigid multilayer wiring board or a flexible multilayer wiring board. The multilayer wiring board can also be an antenna board.

[0031] Referring to FIG. 1, a multilayer wiring board 1000 according to the embodiment includes an insulating layer 100 and the wiring pattern 200. As shown in FIG.

[0032] The insulating layer 100 includes an insulating material, that is, the insulating layer 100 is an insulating substrate that has no electrical conductivity.

[0033] The insulating layer 100 supports the wiring pattern 200. In particular, the wiring pattern 200 is disposed on at least one of one surface and the other surface of the insulating layer 100. That is, the insulating layer 100 is a supporting substrate that supports the wiring pattern 200.

[0034] The multilayer wiring board 1000 includes a plurality of insulating layers 100. For example, the multilayer wiring board 1000 may include a first insulating layer 110, a second insulating layer 120 on the first insulating layer 110, a third insulating layer 130 on the second insulating layer 120, a fourth insulating layer 140 on the third insulating layer 130, and a fifth insulating layer 150 on the fourth insulating layer 140.

[0035] However, the embodiment is not limited thereto, that is, the multilayer wiring board 1000 may include less than five insulating layers. Or, the multilayer wiring board 1000 may include five or more insulating layers. Hereinafter, for convenience of explanation, the multilayer wiring board 1000 will be described as including the first insulating layer 110, the second insulating layer 120, the third insulating layer 130, the fourth insulating layer 140, and the fifth insulating layer 150.

[0036] The first insulating layer 110, the second insulating layer 120, the third insulating layer 130, the fourth insulating layer 140, and the fifth insulating layer 150 are sequentially stacked.

[0037] The insulating layer 100 may be bent with a curved surface in part. That is, the insulating layer 100 may be bent with a curved surface in part, and may be flat in part. In particular, an end of the insulating layer 100 may be bent with a curved surface. Alternatively, the insulating layer 100 may be bent with a surface including a random curvature.

[0038] Also, the insulating layer 100 may be a flexible insulating layer, and may be a curved or bent substrate.

[0039] That is, the multilayer wiring board including the insulating layer 100 may include a flexible multilayer wiring board.

[0040] The insulating layer 100 may include a resin material. For example, the insulating layer 100 may include a resin material whose physical properties change depending on temperature. In particular, the insulating layer 100 may include a thermoplastic resin.

[0041] As an example, the insulating layer 100 may include a liquid crystal polymer.

[0042] The liquid crystal polymer has properties in both a liquid state and a solid state, that is, the liquid crystal polymer has regular crystal orientation in the liquid state as in the solid state.

[0043] Therefore, since the insulating layer 100 contains a liquid crystal polymer, the heat resistance of the multilayer wiring board can be improved, and since the signal loss due to the dielectric constant of the material can be reduced, the signal transmission characteristics of the multilayer wiring board can be improved.

[0044] The insulating layer 100 has a thickness within a set range. In particular, the insulating layer 100 may have a thickness of 150 μm or less, a thickness of 25 μm to 150 μm, or a thickness of 50 μm to 100 μm.

[0045] If the thickness T2 of the insulating layer 100 is less than 25 μm, the insulating layer 100 may not be able to adequately support the wiring pattern 200, and the overall strength of the multilayer wiring board may be reduced. Also, if the thickness of the insulating layer 100 exceeds 150 μm, the increased thickness of the insulating layer 100 may lengthen the time required for the via hole V formation process, and the overall size of the multilayer wiring board may be increased.

[0046] The wiring pattern 200 is disposed on the insulating layer 100. In particular, the wiring pattern 200 is disposed on at least one of one surface and the other surface of the insulating layer 100.

[0047] The wiring pattern 200 may be in direct contact with the insulating layer 100. That is, no separate adhesive layer is disposed between the insulating layer 100 and the wiring pattern 200. This reduces the overall thickness of the multilayer wiring substrate 1000.

[0048] The wiring pattern 200 is a path for transmitting an electrical signal of the multilayer wiring board 1000. That is, the multilayer wiring board 1000 can transmit an electrical signal to another member connected to the multilayer wiring board 1000 through the wiring pattern 200. Alternatively, the multilayer wiring board 1000 can transmit an electrical signal generated from another member through the wiring pattern 200.

[0049] Thus, the wiring pattern 200 may include a highly conductive material. In particular, the wiring pattern 200 may include a metal. For example, the wiring pattern 200 may include at least one metal selected from the group consisting of gold (Au), silver (Ag), platinum (Pt), titanium (Ti), tin (Sn), copper (Cu), zinc (Zn), and alloys thereof. Preferably, the wiring pattern 200 includes copper (Cu). In other words, the wiring pattern 200 is copper (Cu).

[0050] The wiring pattern 200 may be disposed on the insulating layer 100 through an additive process, a subtractive process, a modified semi-additive process (MSAP), or a semi-additive process (SAP), which are typical manufacturing processes for printed multilayer wiring boards.

[0051] The wiring pattern 200 has a line width and a thickness within a set range. In particular, the wiring pattern 200 may have a line width of 40 μm to 150 μm. More particularly, the wiring pattern 200 may have a line width of 70 μm to 120 μm.

[0052] If the line width of the wiring pattern 200 is less than 40 μm, the process efficiency may decrease, and if the line width of the wiring pattern 200 is more than 150 μm, the size of the multilayer wiring board may increase.

[0053] Also, the wiring pattern 200 may have a thickness of 15 μm or less. More specifically, the wiring pattern 200 may have a thickness of 10 μm to 15 μm. More specifically, the wiring pattern 200 may have a thickness of 11 μm to 14 μm.

[0054] If the thickness T3 of the wiring pattern 200 is less than 10 μm, the electrical characteristics of the wiring pattern 200 may be degraded. If the thickness of the wiring pattern 200 is more than 15 μm, the size of the multilayer wiring board may be increased.

[0055] The insulating layer 100 includes at least one via hole V. In particular, at least one of the first insulating layer 110, the second insulating layer 120, the third insulating layer 130, the fourth insulating layer 140, and the fifth insulating layer 150 may include at least one via hole V.

[0056] The via hole V is formed penetrating the insulating layer 100. A conductive layer 600 is disposed inside the via hole V. In particular, the conductive layer 600 including a conductive material is disposed inside the via hole V. Wiring patterns disposed on different insulating layers are electrically connected to each other through the via hole V and the conductive layer 600.

[0057] The conductive layer 600 includes a conductive material. In particular, the conductive layer 600 includes a metal. For example, the conductive layer 600 may include at least one metal selected from the group consisting of copper (Cu), silver (Ag), tin (Sn), gold (Au), nickel (Ni), palladium (Pd), and alloys thereof. Preferably, the conductive layer 600 includes copper (Cu). That is, the conductive layer 600 is copper (Cu).

[0058] The conductive layer 600 may be disposed inside the via hole V by electroless plating, electrolytic plating, screen printing, sputtering, or evaporation. Preferably, the conductive layer 600 is disposed inside the via hole V by electroless plating or electrolytic plating.

[0059] Pad sections are disposed on the upper and lower parts of the multilayer wiring board 1000. In particular, a first pad section 310 is disposed on the upper part of the multilayer wiring board 1000. In addition, a second pad section 320 is disposed on the lower part of the multilayer wiring board 1000.

[0060] For example, the first pad unit 310 is disposed on the fifth insulating layer 150 which is the uppermost insulating layer of the multilayer wiring board 1000. At least one of the first pad units 310 may be disposed on the fifth insulating layer 150. At least one of the first pad units 310 may serve as a pattern for transmitting signals. Also, at least one other of the first pad units 310 may serve as an inner lead for connecting the multilayer wiring board 1000 to an electronic component 500 connected thereto.

[0061] Also, the second pad unit 320 may be disposed under the first insulating layer 110, which is the lowest insulating layer of the multilayer wiring board 1000. At least one of the second pad units 320 may serve as a pattern for transmitting signals. Also, at least one other of the second pad units 320 may serve as an outer lead for connection to an external board.

[0062] Moreover, protective layers 160 and 170 are disposed on the uppermost and lowermost insulating layers of the multilayer wiring board 1000, respectively.

[0063] Meanwhile, the electronic component 500 connected to the multilayer wiring board 1000 may include all of the elements and chips. In conclusion, the electronic component 5000 includes all of the semiconductor chips, the light emitting diode chips, and other driving chips.

[0064] As described above, the multilayer wiring board 1000 is formed by stacking a plurality of insulating layers on which wiring patterns are formed. In particular, the insulating layers are bonded through thermocompression bonding at a set temperature range. In particular, the insulating layers 110, 120, 130, 140, and 150 are bonded to each other through a thermocompression process at a set temperature range.

[0065] 2, for example, a wiring pattern 200 and a via hole V are formed in each of a plurality of insulating layers 110, 120, 130, 140, and 150. A conductive layer 600 is disposed inside the via hole V. The plurality of insulating layers 110, 120, 130, 140, and 150 in which the wiring pattern 200 and the via hole V are formed may be bonded to each other through a thermocompression process within a set temperature range.

[0066] The conductive layer 600 may be formed simultaneously with a process of forming the wiring pattern 200. That is, the conductive layer 600 is disposed inside the via hole through a plating process.

[0067] The thermocompression process may be performed at a temperature equal to or higher than the melting points of the insulating layers 110, 120, 130, 140, and 150. That is, the insulating layers 110, 120, 130, 140, and 150 melt at a temperature equal to or higher than the melting points of the insulating layers 110, 120, 130, 140, and 150. Then, the molten insulating layers 110, 120, 130, 140, and 150 are bonded to each other.

[0068] At this time, the wiring patterns 200 disposed on different insulating layers are electrically connected through the conductive layer 600 inside the via hole V. That is, the region where the via hole V is formed on the insulating layers 110, 120, 130, 140, and 150 is a region where the metal material of the wiring pattern 200 and the metal material of the conductive layer 600 are bonded to each other, unlike other regions.

[0069] However, the melting point of the metal material of the wiring pattern 200 is higher than the melting point of the insulating layer. Therefore, when the conductive layer 600 and the wiring pattern 200 contain the same copper metal, the conductive layer 600 and the wiring pattern 200 do not melt at the melting temperature of the insulating layer. Therefore, the conductive layer 600 and the wiring pattern 200 may not be bonded to each other.

[0070] Therefore, the bonding material 770 may be disposed between the conductive layer 600 and the wiring pattern 200. The bonding material 770 may be disposed on the conductive layer 600 through a plating process.

[0071] The bonding material 770 includes a metal material having a lower melting point than the wiring pattern 200 and the conductive layer 600. Therefore, even if a thermocompression process is performed at a temperature close to the melting point of the insulating layer, the conductive layer in the via hole and the wiring pattern can be bonded through the bonding material 770.

[0072] Meanwhile, while the bonding material 770 is melting, the metal material of the bonding material 770, the metal material of the wiring pattern 200, and the metal material of the conductive layer 600 may react with each other to form an alloy.

[0073] Such alloys may have various electrical, thermal, and mechanical properties depending on the composition, and thus, the adhesive properties between the conductive layer and the wiring pattern, and the electrical, thermal, and mechanical properties of the multilayer wiring board vary depending on the composition of the alloy.

[0074] Therefore, in the following, a multilayer wiring board having improved electrical, thermal and mechanical properties will be described by adjusting the composition ratio of the bonding layer formed by the bonding material 770 between the conductive layer 600 and the wiring pattern 200.

[0075] Fig. 3 is an enlarged view of region A in Fig. 1. That is, Fig. 3 is an enlarged view of a region in which a via hole of a multilayer wiring board is formed.

[0076] 3, a conductive layer 600 is disposed within the insulating layer 100. In particular, a plurality of via holes V are formed in the insulating layer 100, and the conductive layer 600 is disposed within the via holes V.

[0077] With respect to the fourth insulating layer 140, wiring patterns 200 are respectively disposed on an upper surface and a lower surface of the conductive layer 600. For example, a first wiring pattern 210 is disposed on the lower surface of the conductive layer 600, and a second wiring pattern 220 is disposed on the upper surface of the conductive layer 600. The first wiring pattern 210 is a wiring pattern disposed on the third insulating layer 130, and the second wiring pattern 220 is a wiring pattern disposed on the fourth insulating layer 140.

[0078] The first wiring pattern 210 and the second wiring pattern 220, which are disposed on different insulating layers, are electrically connected to each other through a conductive layer 600 disposed inside the via hole V.

[0079] The conductive layer 600 and the first wiring pattern 210 are simultaneously formed by the same process. That is, the conductive layer 600 in the via hole V and the first wiring pattern 210 disposed on the fourth insulating layer 140 are simultaneously formed by a plating process. Thus, the conductive layer 600 and the first wiring pattern 210 are formed integrally.

[0080] An adhesive layer 700 is disposed between the conductive layer 600 and the second wiring pattern 220 on the fifth insulating layer 150. In particular, the adhesive layer 700 formed of the adhesive material 770 is disposed between the conductive layer 600 inside the via hole V and the second wiring pattern 220.

[0081] The bonding layer 700 is disposed on the upper portion of the via hole V. In particular, the bonding layer 700 is disposed on the upper portion of the via hole V having a larger diameter than the other via holes V.

[0082] The wiring patterns 210 and 220, the conductive layer 600, and the bonding layer 700 may include different materials. In particular, the wiring patterns 210 and 220, the conductive layer 600, and the bonding layer 700 may include different metal materials.

[0083] For example, the wiring patterns 210 and 220 and the conductive layer 600 may include the same metal material. In addition, the bonding layer 700 may include a metal material different from at least one of the wiring patterns 210 and the conductive layer 600.

[0084] The bonding layer 700 includes a first region 1A and a second region 2A. In detail, the adhesive layer 700 includes the first region 1A and the second region 2A that form a boundary in the depth direction of the via hole V. The second region 2A is disposed above and below the first region 1A. Thus, the first region 1A is disposed between the second regions 2A.

[0085] The second region 2A is disposed closer to the wiring pattern 200 than the first region 1A. The second region 2A is disposed between the first region 1A and the wiring pattern 200.

[0086] An alloy is disposed in the first region 1A and the second region 2A of the bonding layer 700. Specifically, an alloy having the same composition is disposed in the first region 1A and the second region 2A of the bonding layer 700. Further, an alloy having the same composition ratio is disposed in the first region 1A and the second region 2A of the bonding layer 700. Also, an alloy having different composition ratios is disposed in the first region 1A and the second region 2A of the bonding layer 700.

[0087] Figures 4 and 5 are diagrams showing enlarged views of the bonding layer.

[0088] Referring to Figure 4, the bonding layer 700 has a first region 1A and a second region 2A defined therein. An alloy is disposed in each of the first region 1A and the second region 2A. Specifically, an alloy having the same composition and different composition ratios is disposed in the first region 1A and the second region 2A. For example, a first alloy 701 is disposed in the first region 1A, and a second alloy 702 is disposed in the second region 2A.

[0089] For example, an alloy having the chemical formula CuxSny is disposed in the first region 1A and the second region 2A. At this time, x + y satisfies 0 < x + y < 12, or x + y satisfies 4 ≤ x + y ≤ 11.

[0090] That is, a first copper-tin alloy is disposed in the first region 1A. Also, a second copper-tin alloy is disposed in the second region 2A. The first copper-tin alloy and the second copper-tin alloy have different composition ratios. Specifically, the value of x / (x + y) of the second copper-tin alloy is greater than the value of x / (x + y) of the first copper-tin alloy. In other words, the copper ratio of the second copper-tin alloy is greater than the copper ratio of the first copper-tin alloy.

[0091] As an example, the first copper-tin alloy has the chemical formula Cu6Sn5, and the second copper-tin alloy has the chemical formula Cu3Sn1. That is, a first copper-tin alloy having the chemical formula Cu6Sn5 is disposed in the first region 1A, and a second copper-tin alloy having the chemical formula Cu3Sn1 is disposed in the second region 2A.

[0092] Thus, a second copper-tin alloy having a chemical formula of Cu3Sn1 is disposed in an area close to the wiring pattern 200, and a first copper-tin alloy having a chemical formula of Cu6Sn5 is disposed in an area far from the wiring pattern 200.

[0093] As a result, the amount of copper in the bonding layer 700 increases as the bonding layer 700 extends from the first region 1A toward the second region OA, and the amount of tin in the bonding layer 700 increases as the bonding layer 700 extends from the second region 2A toward the first region 1A.

[0094] The first region 1A and the second region 2A are arranged to have different sizes from each other. For example, the first region 1A and the second region 2A are arranged to have different volumes from each other. Or, the first region 1A and the second region 2A are arranged to have different areas from each other.

[0095] In detail, the volume or area of ​​the second region 2A is larger than the volume or area of ​​the first region 1A.

[0096] Specifically, when the total volume of the first region 1A and the second region 2A is taken as 100%, the volume of the second region 2A is larger than the volume of the first region 1A. For example, the second region 2A may have a volume exceeding 50%. More specifically, the second region 2A may have a volume between 50% and less than 100%. Preferably, the second region 2A has a volume of 90% or more. More preferably, the second region 2A has a volume of 95% or more.

[0097] Furthermore, the first region 1A may have a volume of less than 50%. More specifically, the first region 1A may have a volume of more than 0% and less than 50%. Preferably, the first region 1A has a volume of 10% or less. More preferably, the first region 1A has a volume of 5% or less.

[0098] Alternatively, when the total area of ​​the first region 1A and the second region 2A is taken as 100%, the area of ​​the second region 2A is larger than the area of ​​the first region 1A. For example, the second region 2A may have an area exceeding 50%. More specifically, the second region 2A may have an area of ​​50% to less than 100%. Preferably, the second region 2A has an area of ​​90% or more. More preferably, the second region 2A has an area of ​​95% or more.

[0099] Moreover, the first region 1A may have an area of ​​less than 50%. More specifically, the first region 1A may have an area of ​​more than 0% and less than 50%. Preferably, the first region 1A has an area of ​​10% or less. More preferably, the first region 1A has an area of ​​5% or less.

[0100] 5, the bonding layer 700 may include only one region. In particular, the bonding layer 700 may include one region in which an alloy having a single composition and composition ratio is disposed. That is, the bonding layer 700 includes only the second region 2A described above.

[0101] That is, the bonding layer 700 includes only the second alloy 702 having a formula of CuxSny, That is, the bonding layer 700 includes only the second copper-tin alloy 702 having a formula of Cu3Sn1.

[0102] FIG. 6 is a diagram for explaining the changes in the composition and composition ratio of the bonding layer.

[0103] 6A, the bonding layer 700 before the thermocompression bonding of the insulating layers includes a metal of a single composition. For example, the bonding layer 700 before the thermocompression bonding includes a first metal layer 750. As an example, the first metal layer 750 is tin (Sn).

[0104] 6(b) to 6(d) are diagrams for explaining the change in the composition and composition ratio of the bonding layer 700 during the thermocompression bonding process.

[0105] 6(b), at the beginning of the thermocompression process, the composition and composition ratio of the first metal layer 750 may vary. In particular, the first metal layer 750 reacts with the wiring pattern 200 and the conductive layer 600 to form a plurality of alloys. Thus, the bonding layer 700 may include the first metal layer 750 and a plurality of alloys.

[0106] In detail, a first alloy layer 761 and a second alloy layer 762 having a chemical formula of CuxSny are formed in a region between the first metal layer 750 and the wiring pattern 200 and a region between the first metal layer 750 and the conductive layer 600. More specifically, the first alloy layer 761 is formed between the second alloy layer 762. In addition, the second alloy layer 762 is formed in a region between the first alloy layer 761 and the wiring pattern 200 and a region between the first alloy layer 761 and the conductive layer 600.

[0107] The first alloy layer 761 and the second alloy layer 762 have the same composition. The first alloy layer 761 and the second alloy layer 762 have different composition ratios. For example, the x value and the y value of the first alloy layer 761 and the second alloy layer 762 are different from each other.

[0108] For example, the first alloy layer 761 may have a formula of Cu6Sn5 and the second alloy layer 762 may have a formula of Cu3Sn1.

[0109] Moreover, the sizes of the first alloy layer 761 and the second alloy layer 762 may be different. In particular, the volume or area of ​​the first alloy layer 761 is larger than the volume or area of ​​the second alloy layer 762.

[0110] Next, referring to FIG. 6(c), in the middle of the thermocompression bonding process, the sizes of the first alloy layer 761 and the second alloy layer 762 change.

[0111] 6(c), the amount of copper diffusing into the bonding layer 700 increases in the middle of the thermocompression bonding process. As a result, the volume or area of ​​the second pass layer 762 may be equal to or larger than the volume or area of ​​the first alloy layer 761.

[0112] Next, referring to FIG. 6(d), at the end of the thermocompression bonding process, the sizes of the first alloy layer 761 and the second alloy layer 762 change.

[0113] 6(d), at the end of the thermocompression bonding process, the amount of copper diffused into the bonding layer 700 increases, so that the volume or area of ​​the second pass layer 762 becomes larger than the volume or area of ​​the first alloy layer 761.

[0114] That is, the volume or area of ​​the second alloy layer 762 changes to be larger than the volume or area of ​​the first alloy layer 761 .

[0115] Therefore, the bonding layer 700 may be modified such that the volume or area of ​​the second alloy layer 762 is greater than the volume or area of ​​the first alloy layer 761. Alternatively, the bonding layer 700 may be modified to include only the second alloy layer 762.

[0116] That is, the first alloy layer 761 and the second alloy layer 762 may correspond to the first alloy 701 and the second alloy 702 of FIG. 4, respectively.

[0117] FIG. 7 is a table illustrating the characteristics of alloy layers having different compositions.

[0118] 7, a first alloy 701 and a second alloy 702 disposed in a first region 1A and a second region 2A of the bonding layer 700 have different physical properties. That is, the first alloy 701 and the second alloy 702 have different composition ratios, and therefore have different physical properties.

[0119] In detail, the thermal diffusivity of the second alloy 702 is greater than that of the first alloy 701. The heat capacity of the second alloy 702 is greater than that of the first alloy 701. The thermal conductivity of the second alloy 702 is greater than that of the first alloy 701.

[0120] As a result, the second region 2A has improved thermal properties compared to the first region 1A. That is, the bonding layer 700 includes the second region 2A at a higher ratio than the first region 1A, improving the thermal properties. Therefore, the multilayer wiring substrate 100 including the bonding layer 700 has improved thermal properties.

[0121] Moreover, the density of the second alloy 702 is greater than the density of the first alloy 701. Therefore, the second region 2A has improved strength compared to the first region 1A. That is, the second region 2A has improved mechanical properties compared to the first region 1A. Therefore, the bonding layer 700 contains a greater proportion of the second region 2A than the first region 1A, and therefore the mechanical properties are improved. Therefore, the multilayer wiring substrate 100 including the bonding layer 700 has improved mechanical properties.

[0122] Moreover, the resistance of the second alloy 702 is smaller than the resistance of the first alloy 701. Therefore, the second region 2A has improved electrical characteristics compared to the first region 1A. That is, the bonding layer 700 contains a larger proportion of the second region 2A than the first region 1A, and therefore the electrical characteristics are improved. Therefore, the multilayer wiring substrate 100 including the bonding layer 700 has improved electrical characteristics.

[0123] Hereinafter, the arrangement of the bonding layers of the multilayer wiring board according to the embodiment will be described in detail with reference to FIGS.

[0124] 8 to 10, the bonding layer 700 is disposed between the wiring pattern 200 and the conductive layer 600. As shown in FIG.

[0125] In detail, the bonding layer 700 includes the via hole V, an overlapping area OLA overlapping the via hole V in the longitudinal direction, and a non-overlapping area NOLA not overlapping the via hole V. More specifically, the bonding layer 700 includes a contact area CA in contact with the conductive layer 600 and a non-contact area NCA not in contact with the conductive layer 700.

[0126] The thickness of the bonding layer 700 is different from that of the insulating layer 100. The thickness of the bonding layer 700 is also different from that of the wiring pattern 700. The thickness of the bonding layer 700 is also different from that of the conductive layer 600.

[0127] In detail, the thickness T1 of the bonding layer 700 is smaller than the thickness of the insulating layer 100. In addition, the thickness T1 of the bonding layer 700 is smaller than the thickness of the wiring pattern 200. Here, the thickness T1 of the bonding layer 700 is defined as the maximum thickness of the bonding layer.

[0128] For example, the thickness T1 of the bonding layer 700 may be 1% to 20% of the thickness of the insulating layer 100. In addition, the thickness T1 of the bonding layer 700 may be 5% to 25% of the thickness of the wiring pattern 200.

[0129] For example, the thickness T1 of the bonding layer 700 may be 1 μm or more. In particular, the thickness T1 of the bonding layer 700 may be 1 μm to 4 μm. More particularly, the thickness T1 of the bonding layer 700 may be 1 μm to 3 μm. More particularly, the thickness T1 of the bonding layer 700 may be 1.5 μm to 2 μm.

[0130] If the thickness T1 of the bonding layer 700 is less than 1 μm, voids may be formed inside the bonding layer 700 due to surface roughness formed on the surface of the bonding layer 700. As a result, the reliability of the bonding layer 700 may be reduced.

[0131] Furthermore, if the thickness T1 of the bonding layer 700 is less than 1 μm, the adhesive strength between the wiring pattern 700 and the bonding layer 700 may decrease.

[0132] The bonding layer 700 is disposed inside the via hole V. Also, the bonding layer 700 is disposed outside the via hole V. That is, the bonding layer 700 is disposed both inside and outside the via hole V.

[0133] 8 to 10, the bonding layer 700 includes an inner region IA disposed inside the via hole V and an outer region OA disposed outside the via hole V. The inner region IA is disposed in contact with the conductive layer 600 inside the via hole V. In addition, the outer region OA is disposed outside the via hole V in contact with the wiring pattern 200.

[0134] The inner region IA and the outer region OA may be disposed to have different thicknesses. For example, as shown in FIG. 8, the thickness of the inner region IA may be greater than the thickness of the outer region OA. In particular, the bonding layer 700 may have a greater thickness disposed inside the via hole V than a greater thickness disposed outside the via hole V.

[0135] 9, the thickness of the inner region IA may be smaller than the thickness of the outer region OA. In particular, the bonding layer 700 may have a smaller thickness inside the via hole V than the thickness outside the via hole V.

[0136] Alternatively, the inner region IA and the outer region OA may be disposed to have the same or similar thickness. For example, as shown in FIG. 10, the thickness of the inner region IA and the thickness of the outer region OA may be the same within a tolerance. In particular, the thickness of the bonding layer 700 disposed inside the via hole V and the thickness of the bonding layer disposed outside the via hole V may be the same within a tolerance.

[0137] The bonding layer 700 is also disposed inside the via hole V, so that two layers may be disposed inside the via hole V. That is, the conductive layer 600 and the bonding layer 700 are disposed inside the via hole V.

[0138] Inside the via hole V, the conductive layer 600 and the bonding layer 700 are disposed to have different thicknesses. In detail, the thickness of the conductive layer 600 inside the via hole V is greater than the thickness of the bonding layer 700. More specifically, the thickness of the bonding layer 700 inside the via hole V is 3% to 10% of the thickness of the conductive layer 600.

[0139] Therefore, the conductive layer 600 having relatively higher electrical conductivity and thermal conductivity is disposed in the via hole V more than the bonding layer 700. As a result, the heat dissipation effect and the connection characteristics of the wiring pattern can be improved through the conductive layer 600 of the via hole V.

[0140] 11 and 12 , the bonding layer 700 may be disposed on a side surface of the conductive layer 600. In particular, the bonding layer 700 may be disposed in contact with a side surface of the conductive layer 600. More particularly, the bonding layer 700 may be disposed between a side surface of the conductive layer 600 and an inner surface of the via hole V.

[0141] The bonding layer 700 melts due to the process of thermocompression bonding the insulating layer 100. The melted bonding layer 700 can be moved between the side surface of the conductive layer 600 and the inner side surface of the via hole V. As a result, the bonding layer 700 can also be disposed between the side surface of the conductive layer 600 and the inner side surface of the via hole V.

[0142] This can prevent damage to the conductive layer 600 inside the via hole V. That is, an additional layer is further disposed between the side surface of the conductive layer 600 and the inner side surface of the via hole V. This can prevent an external impact from being directly transmitted to the conductive layer 600 inside the via hole V. That is, the bonding layer 700 can serve as a buffer layer for protecting the conductive layer 600.

[0143] 13 and 14 are diagrams showing the grain size of the bonding layer according to the embodiment and the comparative example. In detail, Fig. 13 is a graph showing the grain size distribution of the bonding layer, and Fig. 14 is a graph showing the grain size distribution of the conductive layer obtained by filling the inside of the via hole with a copper-tin paste and hardening it.

[0144] 13 and 14, it can be seen that the grain size of the bonding layer formed by plating a bonding material and performing a thermocompression process is different from the grain size of the conductive layer formed by filling the inside of a via hole with a copper-tin paste.

[0145] That is, referring to Fig. 13, it can be seen that the bonding layer according to the embodiment has a very wide distribution of crystal grain size, while referring to Fig. 14, it can be seen that the conductive layer according to the comparative example has a very narrow distribution of crystal grain size.

[0146] That is, it can be seen that the bonding layer according to the embodiment has a crystal grain size distribution similar to that of the conductive layer of copper metal disposed inside the via hole.

[0147] A multilayer wiring board according to an embodiment includes a via hole for connecting a plurality of wiring patterns, a conductive layer disposed inside the via hole, and a bonding layer between the conductive layer and the wiring patterns.

[0148] The bonding layer may include at least one alloy. In particular, the bonding layer may include at least one alloy having a formula of CuxSny.

[0149] In this case, the alloy ratio of the bonding layer may be adjusted. In particular, the bonding layer may include a first copper-tin alloy and a second copper-tin alloy. The bonding layer may include a higher ratio of the first copper-tin alloy than the second copper-tin alloy. This may improve the thermal properties, electrical properties, mechanical properties, and adhesive properties with metals of the bonding layer.

[0150] Therefore, the multilayer wiring board according to the embodiment can improve the adhesive strength between the wiring pattern and the conductive layer through the bonding layer, and can have improved electrical, mechanical, and thermal properties through the adhesive layer.

[0151] The bonding layer is disposed both inside and outside the via hole, and the thickness of the bonding layer is smaller than the thickness of the conductive layer inside the via hole. That is, the conductive layer is disposed in a larger amount inside the via hole than the bonding layer.

[0152] Therefore, it is possible to prevent the electrical, mechanical and thermal properties inside the via hole from being deteriorated.

[0153] In addition, the bonding layer may be disposed inside the via hole between a side surface of the conductive layer and an inner side surface of the via hole, and thus the bonding layer can protect the conductive layer inside the via hole, thereby preventing an external impact from being directly transmitted to the conductive layer inside the via hole.

[0154] In addition, in the multilayer wiring board according to the embodiment, the conductive layer and the bonding layer may be disposed inside the via hole through a plating method and a thermocompression method, so that the diameter of the via hole can be reduced compared to filling the inside of the via hole with a paste method, and therefore the overall size of the multilayer wiring board can be reduced.

[0155] The features, structures, effects, etc. described in the above-mentioned embodiments are included in at least one embodiment of the present invention, and are not necessarily limited to only one embodiment. Furthermore, the features, structures, effects, etc. exemplified in each embodiment can be combined or modified in other embodiments by a person having ordinary skill in the art to which the embodiment belongs. Therefore, the contents related to such combinations and modifications should be interpreted as being included in the scope of the present invention.

[0156] In addition, although the above description has focused on the embodiments, these are merely illustrative and do not limit the present invention, and a person having ordinary skill in the art to which the present invention pertains will understand that various modifications and applications not exemplified above are possible within the scope of the essential characteristics of the present embodiments. For example, each component specifically illustrated in the embodiments can be modified and implemented. Differences related to such modifications and applications should be interpreted as being included in the scope of the present invention as defined in the appended claims.

Claims

1. A plurality of insulating layers laminated in sequence; a wiring pattern disposed on the insulating layer, the insulating layer including at least one via hole, a conductive layer disposed inside the via hole, a bonding layer is disposed between the wiring pattern and the conductive layer; The bonding layer includes at least one of a first region and a second region having a chemical formula of CuxSny; the value of x / x+y in the second region is greater than the value of x / x+y in the first region; A multilayer wiring board, wherein the volume or area of ​​the second region is larger than the volume or area of ​​the first region.

2. the bonding layer includes a first layer disposed in the first region and a second layer disposed in the second region, The first layer is Cu 6 Sn 5 is a copper-tin alloy having the chemical formula The second layer is Cu 3 Sn 1 2. The multilayer wiring board according to claim 1, wherein the second copper-tin alloy has a chemical formula:

3. 3. The multilayer wiring board according to claim 1, wherein the second region is disposed closer to the wiring pattern than the first region.

4. 3. The multilayer wiring board according to claim 1, wherein the bonding layer includes an overlapping region that overlaps with the via hole in a depth direction of the via hole and a non-overlapping region that does not overlap with the via hole.

5. The multilayer wiring board according to claim 1 , wherein the bonding layer includes a contact region in contact with the conductive layer and a non-contact region not in contact with the conductive layer.

6. 3. The multilayer wiring board according to claim 1, wherein the bonding layer includes an inner region disposed inside the via hole and an outer region disposed outside the via hole.

7. 3. The multilayer wiring board according to claim 1, wherein a thickness of the internal region is smaller than a thickness of the conductive layer.

8. 3. The multilayer wiring board according to claim 1, wherein the bonding layer has a thickness of 1 μm to 4 μm.

9. 3. The multilayer wiring board according to claim 1, wherein the bonding layer is disposed between a side surface of the conductive layer and an inner side surface of the via hole.

10. 3. The multilayer wiring board according to claim 1, wherein the insulating layer comprises a liquid crystal polymer.

11. 3. The multilayer wiring board according to claim 1, wherein the wiring pattern and the conductive layer are made of copper (Cu).

12. the bonding layer includes only a second region, The second region is Cu 3 Sn 1 2. The multilayer wiring board of claim 1, further comprising a second copper-tin alloy having a chemical formula:

13. The multilayer wiring board according to claim 1 , wherein the melting points of the wiring pattern and the conductive layer are higher than the melting point of the insulating layer.

14. The bonding layer includes a bonding material, The multilayer wiring board according to claim 1 , wherein the melting point of the bonding material is lower than the melting points of the wiring pattern and the conductive layer.

15. The multilayer wiring board according to claim 1 , wherein the insulating layers are bonded by a thermocompression bonding method.

16. The multilayer wiring board according to claim 1 , wherein the wiring pattern and the conductive layer are integrally formed.

17. the bonding layer includes a first layer disposed in the first region and a second layer disposed in the second region, The multilayer wiring board according to claim 1 , wherein the second layer has a thermal diffusivity greater than that of the first layer.

18. The multilayer wiring board according to claim 17 , wherein the second layer has a larger heat capacity than the first layer.

19. The multilayer wiring board according to claim 17 , wherein the density of the second layer is greater than the density of the first layer.

20. The multilayer wiring board according to claim 17 , wherein the resistance of the second layer is smaller than the resistance of the first layer.

Citation Information

Patent Citations

  • Wiring board and electronic device using the same

    JP2004179362A

  • Flexible circuit board and chip package including the same

    JP2021500750A

  • Multilayer wiring board and method for manufacturing multilayer wiring board

    WO2019003729A1