Weldless T-tube

The non-welded T-tube manufacturing method integrates a cylindrical piping part with a perpendicular branch part, addressing welding-related issues by ensuring high strength and a smooth, mirror-like surface without welding, thus enhancing sanitary quality and reducing costs.

JP3249064UActive Publication Date: 2024-11-08SANWA METAL CO LTD
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
JP2024003059U
Authority / Receiving Office
JP · JP
Patent Type
Utility models
Current Assignee / Owner
Filing Date
2024-09-11
Publication Date
2024-11-08
Estimated Expiration
2034-09-11

AI Technical Summary

Technical Problem

Existing sanitary T-tube manufacturing methods require welding, which leads to brittleness, increased costs, and difficulty in achieving a smooth, mirror-like surface due to welding imperfections and the need for advanced techniques to join stainless steel pipes without embrittlement.

Method used

The method involves integrally forming a non-welded T-tube using a hydraulic bulge manufacturing process, where a cylindrical piping part and a perpendicular branch part are made from the same material, ensuring a seamless joint and stable wall thickness, with a branch length of 50 mm or more, and a thickness deviation rate of 5% or less, without the need for welding.

Benefits of technology

This approach results in a T-tube with high strength, stable wall thickness, and a mirror-finished surface, reducing the risk of brittleness and manufacturing costs while ensuring a smooth, sanitary finish.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0003249064000001_ABST
    Figure 0003249064000001_ABST
Patent Text Reader

Abstract

To provide a T-shaped pipe that is strong and achieves lower cost. [Solution] A T-shaped pipe 1 has a cylindrical pipe section 10 with a linear central axis, and a cylindrical branch section 20 extending perpendicularly to the central axis from the center of the pipe section. The pipe section 10 and the branch section 20 are made of cylindrical raw material made of stainless steel, and the raw material is filled with water and integrally formed with the pipe section 10 and the branch section 20 by a hydraulic bulge process. This provides a non-welded T-shaped pipe 1 in which the branch section 20 extends seamlessly from the pipe section 10, the length of the branch section 20 is 50 mm or more, and the wall thickness deviation expressed as (maximum wall thickness - minimum wall thickness) / (average wall thickness) x 100 is 5% or less.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention applies to sanitary piping, and in particular to weldless T-pipes. [Background technology]

[0002] Sanitary piping is used in places where hygiene is important, and both the front and back surfaces are treated to be smooth and mirror-like so that they do not easily get dirty.

[0003] Sanitary T-shaped pipes are manufactured by a manufacturing method known as a hydraulic bulge manufacturing method, for example. A conventional hydraulic bulge manufacturing method is disclosed in Patent Document 1.

[0004] FIG. 6 is an explanatory diagram showing a schematic configuration of a conventional forming apparatus 100 used for manufacturing a T-shaped pipe, and FIG. 7 is a diagram showing a conventional manufacturing process of the T-shaped pipe.

[0005] The molding apparatus 100 includes an installation section 101 for installing a mold 200 , an injection section 105 for injecting liquid into the mold 200 , and a compression section 110 for applying pressure to raw material placed inside the mold 200 .

[0006] The mold 200 is composed of an upper mold 201 and a lower mold 202. The upper mold 201 has a half-pipe-shaped upper semi-cylindrical recess 201a. The lower mold 202 has a half-pipe-shaped lower semi-cylindrical recess 202a and a cylindrical recess 202b extending downward from the center of the lower semi-cylindrical recess 202a. By combining the upper mold 201 and the lower mold 202, the upper semi-cylindrical recess 201a and the lower semi-cylindrical recess 202a are integrated, and as shown in FIG. 7(b), a cylindrical space 203 with both longitudinal ends open is formed, and a space formed by the cylindrical recess 202b extends continuously downward from the lower center of the space 203. The inner diameter of the cylindrical space 203 is set to be equal to the inner diameter of the cylindrical recess 202b. The height of the cylindrical recess 202b is set to be longer than the thickness of the raw material. In other words, the bottom surface of the cylindrical recess 202b is set to be lower than the lowest part of the space 203 by the thickness of the raw material.

[0007] The installation section 101 includes an upper mold installation section 102 for installing an upper mold 201 and a lower mold installation section 103 for installing a lower mold 202 .

[0008] The compression section 110 is disposed on both sides of the mold 200 and includes two cylindrical pistons 110a, 110a that can be inserted into both sides of the space 203. The pistons 110a, 110a include holes 110b, 110b in the center that extend along the central axis.

[0009] The upper die 201 is placed on the upper die installation section 102, the lower die 202 is placed on the lower die installation section 103, and the upper die installation section 102 is moved downward to combine the upper die 201 and the lower die 202. As a result, spaces facing both sides of the space 203 are formed on both sides of the installation section 101, and the pistons 110a, 110a are inserted into the space 203 from both sides of the space 203 through these spaces.

[0010] When the pistons 110a, 110a are inserted from both sides of the space 203, the holes 110b, 110b face both sides of the space 203. The liquid sent from the injection part 105 is injected into the mold 200 through the holes 110b, 110b.

[0011] Next, a conventional manufacturing process for a T-shaped pipe will be described with reference to Fig. 7. In Fig. 7, the installation part 101 and the injection part 105 are omitted.

[0012] In the initial state, the molding apparatus 100 raises the upper die 201 to open the lower die 202. First, as shown in FIG. 7(a), the raw material A is positioned between the upper die 201 and the lower die 202 and set in the lower die 202. The raw material A is made of a stainless steel cylindrical body. Next, as shown in FIG. 7(b), the upper die 201 is lowered to hold the raw material A between the upper die 201 and the lower die 202. Next, as shown in FIG. 7(c), the left and right pistons 110a, 110a are advanced to seal both ends of the raw material A and inject oil into the raw material A. Then, the pistons 110a, 110a are advanced to compress the raw material A from both sides, and the internal pressure of the raw material A is increased by the oil injection. As a result, the center of the raw material A bulges toward the inside of the cylindrical recess 202b as shown in FIG. 7(d).

[0013] Next, oil is further injected to increase the internal pressure of raw material A, and pistons 110a, 110a are advanced to compress raw material A from both sides, as shown in Fig. 7(e), causing the center of raw material A to bulge further into cylindrical recess 202b. As a result, a cylindrical portion with a dome-shaped closed tip is formed in the center of raw material A.

[0014] Next, as shown in FIG. 7(f), the oil is drained, the pistons 110a, 110a are retracted, and the upper die 201 is raised, and the raw material A formed into a T shape is removed.

[0015] Next, as shown in Fig. 7(g), the dome-shaped portion of the bulging portion in raw material A is cut to open the tip of the bulging portion. Next, a cylindrical tube B of the same diameter as raw material A as shown in Fig. 8(a) is prepared in advance, and raw material B is placed opposite the tip of the central bulging portion of raw material A as shown in Fig. 7(h), and welded to the tip of the central bulging portion of raw material A as shown in Fig. 8(b).

[0016] After welding, a burn (scale) occurs in the welded area, as shown in Figure 8(b). Therefore, polishing is performed to eliminate the step at the welded joint, and the thickness is adjusted. Finally, this burn (scale) is removed, and a mirror finish is performed to remove minute irregularities and dirt from the surface, making the welded area difficult to see.

[0017] As a result of the above steps, a T-shaped pipe having a glossy surface and inner surface is manufactured.

[0018] However, T-shaped pipes formed by welding are exposed to high temperature environments at the joints, which can cause brittleness depending on the stainless steel material. For this reason, welding stainless steel together requires highly skilled techniques to ensure reliable joining while maintaining a temperature range where brittleness is unlikely to occur, which increases the cost of the work. In addition, burns (scale) occur at the welded parts, which must be removed, which increases the manufacturing cost.

[0019] In addition, in the sanitary field, it is desirable for the surface to be smooth with almost no unevenness so that foreign matter contained in the water does not remain inside the pipe. For this reason, the surface is polished, so the thickness of the T-shaped pipe is thinner than that of raw material A. However, since the welded parts are also polished, the welded parts that may be brittle become thin, and there is a risk of reducing their strength.

[0020] In order to solve such problems, it has been proposed to form metal pipes by hydroforming (Patent Document 2). In the method described in Patent Document 2, when forming metal pipes by hydroforming, a local softening treatment is performed before the hydroforming process on the part of the metal pipe that is scheduled to be bulged or expanded. This makes it possible to practically form complex shapes without causing buckling or bursting. For example, a stainless steel pipe is used as the metal pipe, and hydroforming is performed to provide a right-angled branch protruding part. This makes it possible to realize a T-shaped pipe with a protruding part located in the center, a diameter of 25.0 mm, a protruding height of 25.0 mm, and a main pipe length L of 300 mm. [Prior art documents] [Patent documents]

[0021] [Patent Document 1] JP2006-088165A [Patent Document 2] JP 2001-150050 A Summary of the Invention [Problem to be solved by the invention]

[0022] However, localized softening treatment requires a high level of skill. In addition, the extension height is limited to 25.0 mm, and if an attempt is made to extend the pipe longer than this, the stainless steel pipe is so hard that cracks and uneven wall thickness may occur.

[0023] The purpose of this invention is to solve these problems and to provide a high-strength, weldless T-pipe with a projection height of 50 mm or more, with a consistent wall thickness and at low cost. [Means for solving the problem]

[0024] To achieve the above object, the present invention has the following configuration.

[0025] (1) A pipe having a cylindrical piping section with a central axis extending linearly, and a cylindrical branch section extending perpendicular to the central axis from a central portion of the pipe section, The piping portion and the branching portion are formed by integral molding using the same material, The length of the branch is 50 mm or more, An unwelded T-shaped pipe with a wall thickness deviation of 5% or less, calculated as (maximum wall thickness - minimum wall thickness) / (average wall thickness) x 100.

[0026] According to (1), since the piping section and the branching section are integrally molded, the joint between the piping section and the branching section is seamless, and the composition of the branching section between the piping section and the branching section is continuous. Therefore, the composition is more stable than the welded section of a T-shaped pipe made by conventional welding. In addition, the conventional welding process is no longer necessary. In this way, it is possible to provide a high-strength non-welded T-shaped pipe with a branching section length of 50 mm or more, a stable wall thickness with a wall thickness deviation rate of 5% or less, and at low cost.

[0027] (2) In (1), a non-welded T-pipe is formed by filling a cylindrical raw material made of stainless steel with water and integrally forming the piping section and the branch section using a hydraulic bulge process.

[0028] According to (2), the piping section and the branch section can be integrally molded, eliminating the need for a welding process as in the past. In this way, it is possible to provide a T-shaped pipe that is strong and has a lower cost.

[0029] (3) In the above (1) and (2), a non-welded T-pipe having a mirror finish on the surface and inside.

[0030] According to (3), dirt is less likely to adhere to the inside of the T-pipe, making it possible to use it as piping in sanitary areas.

[0031] (4) A non-welded T-pipe according to any one of (1) to (3), wherein the curvature of the base of the branched portion is 5 mm or less.

[0032] According to (4), when piping is arranged on a flat plate, a circular hole is formed in the flat plate, and a branch section is passed through the circular hole, it is possible to reduce the occurrence of an incident in which the portion of curvature R abuts against the edge of the circular hole, causing the piping section to separate from the surface of the flat plate. Effect of the Invention

[0033] According to the present invention, a non-welded T-shaped pipe with high strength and a branch length of 50 mm or more can be provided with a consistent wall thickness and at low cost.

Brief Description of the Drawings

[0034] [Figure 1] It is a perspective view showing the schematic configuration of the T-shaped pipe 1 of one embodiment of the present invention. [Diagram 2] It is a cross-sectional view showing a cross-section obtained by dividing the piping portion 10 and the branch portion 20 of the T-shaped pipe 1 of one embodiment of the present invention into two. [Diagram 3] It is a view showing the manufacturing process of the T-shaped pipe 1 of one embodiment of the present invention. [Figure 4] It is an external view showing the appearance of the raw material A before and after mirror finishing. [Diagram 5] It is a perspective view showing other configurations of the T-shaped pipe 1 of one embodiment of the present invention. [Figure 6] It is an external view showing the schematic configuration of the conventional molding apparatus 100. [Figure 7] It is a view showing the manufacturing process of the conventional T-shaped pipe. [Figure 8] It is an external view showing the appearance of the raw material A before and after mirror finishing.

Modes for Carrying Out the Invention

[0035] Hereinafter, embodiments of the present invention will be described in detail with reference to the drawings.

[0036] <Configuration of the T-shaped pipe 1> FIG. 1 is a view showing the schematic configuration of the T-shaped pipe 1 of one embodiment of the present invention. FIG. 1(a) is a perspective view, and FIG. 1(b) is a front view seen in the X direction of FIG. 1(a). FIG. 2 is a cross-sectional view showing a cross-section obtained by dividing the piping portion 10 and the branch portion 20 of the T-shaped pipe 1 of one embodiment of the present invention into two. The T-shaped pipe 1 includes a piping portion 10 and a branch portion 20.

[0037] The piping section 10 is formed in a cylindrical shape with both ends open. The branching section 20 has a base end connected to the central portion of the piping section 10 and is formed in a cylindrical shape with the tip end open. The central axis of the branching section 20 is orthogonal to the central axis of the piping section 10. That is, it is formed in a T shape by the piping section 10 and the branching section 20. The piping section 10 and the branching section 20 are formed of the same stainless steel member, for example, SUS304 or SUS316L.

[0038] Also, the piping section 10 and the branching section 20 have the same wall thickness and outer diameter. Further, according to the present embodiment, the lengths from the intersection of the central axis of the piping section 10 and the central axis of the branching section 20 to the centers of both ends of the piping section 10 and the length to the center of the tip end of the branching section 20 are set equal to each other. In the present embodiment, the length of the branching section 20 is set to 50 mm. Note that the length of the branching section 20 can be appropriately set according to the design of the mold 200 described later. In particular, since the length of the branching section 20 is ensured by setting it to 50 mm or more, there is no need to compensate for the length of the branching section 20 by welding or the like.

[0039] Also, the wall thickness deviation rate represented by (maximum wall thickness - minimum wall thickness) / (average wall thickness)×100 is 5% or less. The wall thickness deviation rate is a parameter indicating the stability of the wall thickness, and a lower value is preferable. The wall thickness deviation rate is preferably 4% or less, and more preferably 3% or less.

[0040] On both sides of the piping section 10 in the central axis direction at the connection portion between the piping section 10 and the branching section 20, curved surfaces with a predetermined curvature are formed. This curvature can be appropriately set according to the design of the mold 200 described later, but in the present embodiment, it is set to 5 mm or less.

[0041] <Manufacturing method of the T-shaped pipe 1> FIG. 3 is a diagram showing the schematic configuration of the molding apparatus 100 used for manufacturing the T-shaped pipe 1 and the manufacturing process of the T-shaped pipe 1 according to an embodiment of the present invention.

[0042] Regarding the molding apparatus 100, since the apparatus shown in FIG. 6 is used, detailed description thereof will be omitted.

[0043] The mold 200 is different from the conventional mold 200 shown in FIG. 6 in that the lower mold 202 is different, and a cylindrical recess 202c is formed that is taller than the cylindrical recess 202b shown in FIG. 6. Specifically, the cylindrical recess 202c is set to be longer than 1 / 2 the length of the raw material A in the central axis direction by at least the thickness of the raw material A. The length of the cylindrical recess 202c can be appropriately set according to the dimensions of the T-shaped pipe 1 to be manufactured. For example, if the length of the branching portion 20 of the T-shaped pipe 1 is 50 mm, the length of the cylindrical recess 202c is set to 50 mm plus the thickness of the raw material. As a result, in the manufacturing process of the T-shaped pipe 1, by cutting a part of the tip of the bulging portion of the raw material A, which will be described later with reference to FIG. 3(g), the tip of the bulging portion can be opened while maintaining the dimensions.

[0044] Water is used as the liquid sent from the injection unit 105, and the water is injected into the mold 200 through the holes 110b, 110b. Note that the water mentioned here does not mean pure water that does not contain any foreign matter or metal ions, but may contain a small amount of impurities.

[0045] Next, a method for manufacturing the T-shaped pipe 1 will be described. In the initial state, the molding apparatus 100 raises the upper die 201 to open the lower die 202. First, as shown in FIG. 3(a), the raw material A is positioned between the upper die 201 and the lower die 202, and the raw material A is set in the lower die 202. Next, as shown in FIG. 3(b), the upper die 201 is lowered to press the raw material A between the upper die 201 and the lower die 202. Up to this point, the process is the same as the conventional process shown in FIG. 7. Next, as shown in FIG. 3(c), the left and right pistons 110a, 110a are advanced to seal both ends of the raw material A, and water is injected into the raw material A. By injecting water and increasing the internal pressure of the raw material A, the center of the raw material A is bulged toward the inside of the cylindrical recess 202c, as shown in FIG. 3(d).

[0046] Next, water is further injected to increase the internal pressure of raw material A, and as shown in FIG. 3(e), the pistons 110a, 110a are advanced to compress raw material A from both sides, and the center of raw material A is expanded toward the inside of the cylindrical recess 202c. By injecting water, the internal pressure can be increased more than by injecting oil. Then, water is injected stepwise into raw material A to increase the internal pressure, and the pistons 110a, 110a are advanced stepwise multiple times, so that the central part expanding from raw material A is brought into close contact with the wall surface of the cylindrical recess 202c. In this way, by injecting water and compressing by the pistons 110a, 110a multiple times, raw material A is molded into a T-shape conforming to the internal shape of the mold 200. At that time, it is possible to suppress deviation in thickness, and the deviation in thickness expressed by (maximum thickness-minimum thickness) / (average thickness)×100 can be made to be 5% or less.

[0047] After molding, as shown in Fig. 3(f), the pistons 110a, 110a are retracted and the upper die 201 is raised to remove the raw material A formed into a T-shape. At this point, as shown in Fig. 4(a), the tip of the bulging portion of raw material A is closed, and the wall thickness is thicker than, for example, 1.2 mm, for example, 2.0 mm.

[0048] Next, as shown in Fig. 3(g), a part of the bulging portion in raw material A is cut to open the tip of the bulging portion. Finally, the outer and inner surfaces of raw material A are polished to adjust the wall thickness and are surface-treated to give a mirror finish. As a result, a T-shaped pipe 1 having a glossy surface and inner surface is manufactured as shown in Fig. 4(b). In this way, according to the T-shaped pipe 1 of this embodiment, the piping portion 10 and the branching portion 20 are integrally molded, and the branching portion 20 is seamless with respect to the piping portion 10.

[0049] <Comparison with T-shaped pipes manufactured by welding> According to the T-shaped pipe 1 of this embodiment, as described above, the piping section 10 and the branching section 20 are integrally formed, and the branching section 20 is seamless with respect to the piping section 10. Therefore, welding is not required. However, when injecting oil to bulge the center of the raw material A as in the conventional manufacturing method, it is difficult to sufficiently increase the internal pressure of the raw material A, and it is difficult to obtain the length of the bulging section. More specifically, it is difficult to bulge by 50 mm or more. For this reason, since the bulging section alone does not reach the dimension of the branching section 20, in order to make up for the insufficient length, raw material B is welded to raw material A as shown in FIG. 7(h).

[0050] When welding the piping and branching parts that make up the T-shaped pipe, it is necessary to take into consideration the brittleness caused by high temperatures, so advanced joining techniques are required. In addition, it is desirable to keep the central axis of the branching part and the central axis of the cylinder to be joined in the same state during welding, but it is relatively difficult to perform welding while maintaining this state. If there is even a slight misalignment between the central axis of the branching part and the central axis of the joined cylinder, a slight step will be formed between the surface of the branching part and the surface of the cylinder. For this reason, it is necessary to maintain the required wall thickness when the wall thickness is thinned by performing surface treatment so that the surface of the branching part and the surface of the cylinder are flush with each other and at the same time the roundness of both is increased. For this reason, it is necessary to use a cylinder with a thick wall thickness as the cylinder to be joined to the raw cylinder.

[0051] Furthermore, when welding the piping section and the branch section that constitute the T-shaped pipe, beads and burns occur at the welded parts, so it is necessary to carry out a surface treatment to remove the beads and burns.

[0052] <Surface treatment method> Common methods of surface treatment include grinding (mechanical method), pickling (chemical method), and electrolysis (electrochemical method).

[0053] Grinding methods (mechanical methods) involve physically grinding away the burnt areas and include sanding and blasting. Removing the burnt areas through physical grinding can result in a beautifully finished appearance. However, in the case of metals with a passive film, the film becomes destroyed, which can lead to corrosion. For this reason, when removing the burnt areas using mechanical methods, it is necessary to carry out a passivation treatment.

[0054] Pickling (chemical method) is a method in which steel is immersed in strong acids such as sulfuric acid or hydrochloric acid to remove impurities such as burns, rust, and dirt. Pickling (chemical method) also has the effect of re-forming the passive film on stainless steel. However, pickling leaves the finished surface matte and unpolished, so it is not suitable for products that require a glossy finish.

[0055] The electrolysis method (electrochemical method) is a surface treatment method for removing weld burns by utilizing the anodic reaction during electrolysis, and there are AC and DC methods depending on the current used, as well as neutral and acidic electrolysis methods depending on the type of electrolyte used.

[0056] The AC method has low dissolving power for stainless steel and destroys the passive film, so a passivation treatment is required.

[0057] The DC method not only produces a mirror-like finish on the stainless steel, but also provides the effect of a passivation treatment.

[0058] The neutral electrolysis method uses a neutral salt electrolyte and has the advantage of being highly safe, but it also has the disadvantages of being slow to remove the burnt metal and of dissolving hexavalent chromium, which is harmful to the human body, from the stainless steel.

[0059] The acid electrolysis method uses an acidic electrolyte, which has a faster burn-off speed and superior polishing power compared to the neutral electrolysis method. Another advantage is that it generates less hexavalent chromium. However, because the electrolyte is acidic, it is unsafe and the acidic solution must be thoroughly washed with water.

[0060] By carrying out surface treatment using one or more of the above-mentioned methods, the surface of the T-shaped pipe becomes a mirror-like surface, to the extent that it is difficult to visually recognize the seams of the welded parts.

[0061] Next, we will explain the differences in appearance (or crystal structure or chemical composition) between when the above-mentioned surface treatment is applied to raw materials formed by the manufacturing process of this embodiment and when it is applied to raw materials created by welding.

[0062] For example, when a grinding method (mechanical method) is applied to a raw material formed by the manufacturing process of this embodiment, the branched portion of the raw material has a high degree of circularity, so that a branched portion of uniform thickness can be formed by grinding evenly. On the other hand, when a welded raw material is subjected to the grinding method, even a slight deviation between the central axis of the branched portion and the central axis of the joined cylinder will result in a slight step between the surface of the branched portion and the surface of the cylinder. Since this step portion is made flush by grinding, it is likely to be thinner than other portions. In addition, in the pickling method (chemical method) and the electrolytic method (electrochemical method), since the entire surface of the raw material is treated, if a slight step is formed between the surface of the branched portion and the surface of the cylinder, the step may remain even after the treatment. For this reason, it may be necessary to perform partial polishing to eliminate the step.

[0063] In contrast, according to the present embodiment, since welding is not required, there is no influence caused by welding as described above.

[0064] In the T-shaped pipe 1 of the present embodiment configured as described above, the pipe section 10 and the branch section 20 are seamless, and the composition of the branch section between the pipe section 10 and the branch section 20 is continuous, so that the composition is more stable than the welded section of a T-shaped pipe made by conventional welding. Therefore, while a conventional welded T-shaped pipe becomes brittle due to high temperatures, the T-shaped pipe 1 of the present embodiment does not undergo welding and is therefore not brittle due to high temperatures, so that the branch section between the pipe section 10 and the branch section 20 has high strength.

[0065] Also, in the case of a T-shaped pipe by conventional welding, in order to secure a joint area, it is necessary to increase the wall thickness of the bulging portion from the raw material. On the other hand, according to the T-shaped pipe 1 of the present embodiment, since the pipe portion 10 and the branch portion 20 are seamless, the wall thickness of the branch portion 20 can be made thinner than that of the T-shaped pipe by welding. Thereby, it becomes possible to reduce the weight of the T-shaped pipe 1.

[0066] Further, the curvature of the root portion between the lower semi-cylindrical recess 202a and the cylindrical recess 202b in the lower mold 202 of the mold 200 is reflected in the curvature R of the root portion between the pipe portion 10 and the branch portion 20 after molding. Therefore, by designing the mold 200, the curvature R of the root portion between the pipe portion 10 and the branch portion 20 can be arbitrarily set. Note that it is desirable to set the curvature R such that 0 < R ≤ 5 mm. By setting the curvature R to 5 mm or less in this way, for example, when arranging pipes on a flat plate, forming a circular hole in the flat plate, and passing the branch portion 20 through this circular hole, it is possible to reduce the occurrence of an event such that the portion with the curvature R abuts against the edge of the circular hole and the pipe portion 10 is separated from the plate surface of the flat plate.

[0067] As described above, the embodiments of the present invention have been described. However, the embodiments of the present invention are not limited to the above-described embodiments. For example, according to the embodiment shown in FIG. 1, the pipe portion 10 and the branch portion 20 of the T-shaped pipe 1 have the same diameter, but the branch portion 20 may have a smaller diameter than the pipe portion 10. In this case, even if the central axis of the branch portion 20 and the central axis of the pipe portion 10 are orthogonal, as shown in FIG. 5, the central axis of the branch portion 20 may be offset in the radial direction of the pipe portion 10 with respect to the central axis of the pipe portion 10 without being orthogonal to the central axis of the pipe portion 10.

[0068] Note that those skilled in the art can conceive of various modification examples and correction examples within the scope of the idea of the present invention. Therefore, those modification examples and correction examples are understood to belong to the scope of the present invention. For example, with respect to the above-described embodiments, those obtained by appropriately adding, deleting, or changing the design of components by those skilled in the art, or those obtained by adding, omitting, or changing conditions of steps, are also included in the scope of the present invention as long as they have the gist of the present invention. [Explanation of symbols]

[0069] 1 T-tube 10 Piping section 20 Branch 100 Molding equipment 101 Installation section 102 Upper mold installation section 103 Lower mold installation section 105 Injection part 110 Compression section 110a piston 110b Hole 200 Molds 201 Upper mold 201a Upper semi-cylindrical recess 202 Lower mold 202a Lower semi-cylindrical recess 202b Cylindrical recess 202c Cylindrical recess 203 Space

Claims

1. A cylindrical piping portion having a central axis extending linearly, and a cylindrical branch portion extending perpendicularly to the central axis from a central portion of the piping portion, The piping portion and the branching portion are formed by integral molding using the same material, The length of the branch is 50 mm or more, A non-welded T-pipe having a wall thickness deviation of 5% or less, which is expressed as (maximum wall thickness - minimum wall thickness) / (average wall thickness) x 100.

2. The non-welded T-shaped pipe according to claim 1, The non-welded T-pipe is formed by filling a cylindrical raw material made of stainless steel with water and integrally forming the piping section and the branch section by a hydraulic bulge process.

3. The non-welded T-shaped pipe according to claim 1, A non-welded T-pipe with a mirror finish on the front and back.

4. The non-welded T-shaped pipe according to any one of claims 1 to 3, A non-welded T-pipe, wherein the curvature of the base portion of the branched portion is 5 mm or less.

Citation Information

Patent Citations

  • Hydroform process for metallic pipe

    JP2001150050A

  • Article formed by hydrostatic bulging and hydrostatic bulge forming method

    JP2006088165A