Spray pyrolysis apparatus
The spray pyrolysis apparatus addresses the issue of high gas flow rates by generating a swirling flow and using multiple combustion tubes to achieve low-density, high-strength hollow particles through controlled gas discharge and dispersion, ensuring adequate reaction time and temperature uniformity.
Patent Information
- Application Number
- JP2021026273
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-02-22
- Publication Date
- 2024-09-19
- Estimated Expiration
- 2041-02-22
AI Technical Summary
Existing internal combustion type spray pyrolysis equipment faces challenges in securing sufficient processing time and temperature uniformity due to increased gas flow rates, leading to hollow particles with high density and low strength.
The apparatus is designed with a combustion tube arrangement that generates a swirling flow by positioning the combustion gas discharge direction non-intersecting with the furnace axis, using a throttle to control gas flow velocity, and employing multiple combustion tubes to maintain heat and residence time, ensuring sufficient heat exchange and dispersion of mist and particles.
This configuration produces hollow particles with low density and high strength by ensuring adequate reaction time and temperature uniformity, enhancing the quality and reproducibility of the synthesis process.
Smart Images

Figure 0007554136000004 
Figure 0007554136000012 
Figure 0007554136000009
Abstract
Description
[Technical field]
[0001] The present invention relates to a spray pyrolysis apparatus. [Background technology]
[0002] A manufacturing device that utilizes the spray pyrolysis method is used as a manufacturing device for hollow particles. The internal combustion spray pyrolysis device used in this manufacturing method has a furnace body consisting of a vertical tube. A combustion tube is connected to a part of the outer periphery of the furnace body, and a combustion burner for generating combustion gas is installed in the combustion tube. A spray device (spray nozzle) for spraying an aqueous solution is installed in the furnace body. The nozzle used here is called a two-fluid, three-fluid, or four-fluid nozzle, and the aqueous solution is sprayed from the tip simultaneously with compressed air to form a mist and fine particles. These fine particles are dried inside the furnace body and become the product. In order to obtain the target specific gravity and particle size, a certain level of processing time and processing temperature are required as processing conditions.
[0003] In general, in an internal combustion type spray pyrolysis apparatus, in addition to gas caused by mist, combustion gas generated by a combustion burner also flows into the furnace body, so the total amount of gas in the furnace body is larger than in an external heat type spray pyrolysis apparatus. This causes a problem that the gas flow rate in the furnace body increases and the target processing time (residence time in the furnace) of the particles cannot be secured. As a result, particles with low strength due to insufficient melting are generated. This can be solved by making the device larger, or by arranging multiple combustion burners to generate a swirling flow in the furnace body and retain the particles in the furnace body for a long time, as in Patent Documents 1 to 3. This also suppresses temperature unevenness in the furnace body. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2004-292223 A [Patent Document 2] JP 2007-84355 A [Patent Document 3] JP 2001-137699 A Summary of the Invention [Problem to be solved by the invention]
[0005] However, even when a swirling flow is generated inside the furnace body using a combustion burner, depending on the relative positions of the combustion burner and the spray device, heat exchange between the combustion gas and the particles may not be sufficient, resulting in hollow particles with high particle density and low strength.
[0006] SUMMARY OF THE PRESENT EMBODIMENT An object of the present invention is to provide a spray pyrolysis apparatus capable of producing hollow particles having low particle density and high strength. [Means for solving the problem]
[0007] The spray pyrolysis apparatus of the present invention comprises a furnace body consisting of a vertical tube, At least one combustion tube connected to the outer circumferential surface of the furnace body; A combustion burner is disposed at an end of the combustion tube opposite to the furnace body and generates a flame toward the furnace body; A spray nozzle is disposed on the tube axis at the bottom of the furnace body and sprays the aqueous solution upward; The combustion tube is arranged so that the discharge direction of the combustion gas from the combustion tube does not intersect with the tube axis of the furnace body, The combustion tube has a throttle at a connection portion with the furnace body, When viewed from a direction perpendicular to the discharge direction and horizontally, the intersection B between the discharge direction and the tube axis of the furnace body is located at a lower limit 1 / 2 times lower than the inner diameter of the furnace body and an upper limit 3 times higher than the inner diameter of the furnace body relative to the tip A of the spray nozzle.
[0008] According to this configuration, by shifting the direction of the combustion gas discharge from the tube axis of the furnace body, the combustion gas discharged from the combustion tube does not rise straight up when passing through the furnace body, but rises while generating a swirling flow. The mist and particles sprayed into the furnace body rise inside the furnace body on this swirling flow, and sufficient reaction time (treatment time) can be secured. In addition, by arranging the combustion tube so that the intersection B between the direction of the combustion gas discharge and the tube axis of the furnace body is located in the above-mentioned range with respect to the tip A of the spray nozzle, the mist and particles sprayed from the spray nozzle can be sufficiently dispersed by the swirling flow. As a result, heat exchange between the combustion gas and the particles is sufficiently performed, and hollow particles with low particle density and high strength can be manufactured.
[0009] In the spray pyrolysis apparatus of the present invention, the combustion tubes are provided in a plurality of groups at different positions in the vertical direction, the plurality of combustion tube groups includes a first combustion tube group that is closest to the spray nozzle in a vertical direction, When viewed from a direction perpendicular to a first discharge direction from the combustion tubes belonging to the first combustion tube group and from a horizontal direction, an intersection B1 between the first discharge direction and a tube axis of the furnace body is located at a lower limit of 1 / 2 times the inner diameter of the furnace body and an upper limit of 1 / 2 times the inner diameter of the furnace body with respect to a tip A of the spray nozzle, The combustion tube groups other than the first combustion tube group may be positioned above the first combustion tube group.
[0010] According to this configuration, the combustion gas discharged from the multiple combustion tubes is linked with each other, so that a sufficient swirling flow can be generated in the furnace body. Also, by providing multiple combustion tubes, the amount of heat dissipated by the furnace body can be added, and the temperature and retention time required for the synthesis of hollow particles can be reproducibly and stably secured.
[0011] In the spray pyrolysis apparatus of the present invention, the inner diameter of the discharge port of the throttle may be equal to or smaller than half the inner diameter of the furnace body.
[0012] By providing a throttle, the flow rate of the combustion gas discharged from the combustion tube can be increased. For example, when the composition is changed and the firing temperature is lowered, the amount of combustion burner is reduced, and the flow rate of the combustion gas discharged from the combustion tube decreases with the decrease in the amount of combustion gas, resulting in insufficient swirling flow. Therefore, by providing a throttle, even if the amount of combustion gas decreases when the firing temperature is lowered, the flow rate of the combustion gas discharged from the combustion tube can be maintained and sufficient swirling flow can be generated. [Brief description of the drawings]
[0013] [Figure 1] 1 is a schematic cross-sectional view showing an example of a spray pyrolysis apparatus according to the present invention. [Diagram 2] FIG. 1 is a plan view showing an example of a spray pyrolysis apparatus according to the present invention. [Diagram 3] FIG. 13 is a plan view showing a spray pyrolysis apparatus according to another embodiment; [Figure 4] FIG. 13 is a plan view showing a spray pyrolysis apparatus according to another embodiment; [Diagram 5] Cross-sectional schematic diagram showing the relative positions of the combustion tube and the spray nozzle [Figure 6] Schematic cross-sectional view showing the relative positions of multiple combustion tubes and spray nozzles [Figure 7] FIG. 1 is a plan view showing a schematic configuration of a furnace body and a combustion tube according to an embodiment; [Figure 8] FIG. 1 is a plan view showing a schematic configuration of a furnace body and a combustion tube according to a comparative example; [Figure 9] FIG. 1 is a plan view showing a schematic configuration of a furnace body and a combustion tube according to a comparative example; [Figure 10] 1 is a plan view and a side view of a spray pyrolysis device according to another embodiment; [Figure 11] 1 is a plan view and a side view of a spray pyrolysis device according to another embodiment; [Figure 12] 1 is a plan view and a side view of a spray pyrolysis device according to another embodiment; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0014] Hereinafter, one embodiment of the spray pyrolysis apparatus will be described with reference to Figures 1 to 5. Note that in each figure, the dimensional ratios in the drawing do not necessarily match the actual dimensional ratios, and the dimensional ratios between the drawings do not necessarily match either.
[0015] Fig. 1 is a schematic cross-sectional view showing an example of a spray pyrolysis apparatus according to the present invention. Fig. 2 is a plan view showing an example of a spray pyrolysis apparatus according to the present invention. The spray pyrolysis apparatus 100 of this embodiment is an internal combustion type, and includes a furnace body 1 consisting of a vertical tube, and at least one combustion tube 2 connected to the outer circumferential surface of the furnace body 1.
[0016] The material of the outer wall of the furnace body 1 and the combustion tube 2 is preferably a heat-resistant metal, such as iron, stainless steel, Inconel, Hastelloy, titanium, etc. The furnace body 1 and the combustion tube 2 are preferably substantially cylindrical in shape, because they can be connected by flanges, and because they can suppress temperature unevenness in the cross-sectional direction within the furnace body 1 and unevenness in heat dissipation in the cross-sectional direction from the furnace body 1 and the combustion tube 2.
[0017] The material for the furnace body 1 and the inner wall of the combustion tube 2 may be any material having the necessary heat resistance, such as ceramics, metal, brick, or monolithic refractory material.
[0018] The furnace body 1 is composed of a vertical tube extending in the vertical direction. The combustion tube 2 is preferably connected to the furnace body 1 at an angle of 5 to 90 degrees, with the vertical downward angle being 0 degrees. If this angle is 5 degrees or more, the speed of the swirling flow becomes sufficiently high, the generation of non-uniform turbulence in the furnace body 1 can be prevented, and the variation in the obtained particle characteristics can be suppressed. If the angle is 90 degrees or less, the discharge of hot air is promoted and heat build-up can be suppressed.
[0019] A combustion burner 3 that generates a flame toward the furnace body 1 is disposed at an end 2a of the combustion tube 2 opposite to the furnace body 1. Either liquid fuel or gaseous fuel can be used as the fuel used for the combustion burner 3. Specifically, gaseous fuels such as LPG, city gas, and vaporized organic matter, and liquid fuels such as kerosene, light oil, heavy oil, and recycled oil can be used.
[0020] The length of the combustion tube 2 is preferably set so that the flame generated from the combustion burner 3 does not come into direct contact with the spray mist. However, if the distance between the flame generated from the combustion burner 3 and the spray mist is too long, the thermal efficiency becomes insufficient.
[0021] A spray nozzle 4 for spraying the aqueous solution upward is disposed at the bottom of the furnace body 1. The spray nozzle 4 is disposed on the tube axis 1c of the furnace body 1. The spray nozzle 4 is preferably a 2-4 fluid nozzle, and the aqueous solution may be sprayed by using compressed air as carrier air and doubly disposing the spray nozzle 4 so that an air shield is formed around the spray mist. In addition, the spray nozzle 4 may be protected by a heat insulating material or the like as necessary, taking heat resistance into consideration.
[0022] The combustion tube 2 is connected to the furnace body 1 at the end 2b. A constriction 21 is provided at the connection part of the combustion tube 2 with the furnace body 1. The constriction 21 is tapered, and the inner diameter gradually becomes smaller toward the furnace body 1. By providing the constriction 21, the flow rate of the combustion gas discharged from the combustion tube 2 can be increased. The inner diameter d21 (see FIG. 2) of the discharge port 21a of the constriction 21 is preferably 1 / 2 or less of the inner diameter d1 (see FIG. 1) of the furnace body 1.
[0023] In this specification, the "throttle" may be any structure capable of increasing the flow velocity near the discharge port of the combustion tube 2, and is not limited to the tapered throttle 21 as in this embodiment. The "throttle" may be, for example, a throttle-like structure that increases the flow velocity near the discharge port of the combustion tube 2 by locally reducing the cross-sectional area of the combustion tube 2.
[0024] The orifice 21 may be provided on the end 2b side of the combustion tube 2, and the position of the discharge port 21a of the orifice 21 may be any of the discharge port of the combustion tube 2 (see FIG. 3), the inside of the combustion tube 2 (see FIG. 4), and the inside of the furnace body 1 (see FIG. 2). The material of the orifice 21 may be heat-resistant bricks, fire-resistant bricks, monolithic refractories, ceramics, metals, etc., and is appropriately selected depending on the operating temperature, operating environment, etc.
[0025] The gradient θ of the orifice 21 is not particularly limited, but taking into consideration the ease of flow of the combustion gas generated from the combustion burner 3 (resistance due to the orifice 21) and the heat storage in the combustion tube 2 (if the gradient θ is large, the resistance of the combustion gas increases and heat becomes trapped inside the combustion tube 2), it is preferable that it be 5 to 75°.
[0026] 2, the combustion tube 2 is disposed so that the discharge direction 20 of the combustion gas from the combustion tube 2 does not intersect with the tube axis 1c of the furnace body 1. In this embodiment, the discharge direction 20 of the combustion gas is the tube axis direction of the combustion tube 2 and also the axial direction of the throttle 21.
[0027] By misaligning the discharge direction 20 of the combustion gas with the tube axis 1c of the furnace body 1 in this way, the combustion gas discharged from the combustion tube 2 does not rise straight up when passing through the furnace body 1, but rather rises by generating a swirling flow. The mist and particles sprayed into the furnace body 1 ride on this swirling flow and rise inside the furnace body 1, ensuring sufficient reaction time (treatment time).
[0028] The discharge direction 20 of the combustion gas is preferably parallel to the tangent direction of the inner peripheral surface of the furnace body 1. This allows the combustion gas to efficiently generate a swirling flow.
[0029] FIG. 5 is a schematic diagram for explaining the positional relationship between the combustion tube 2 and the spray nozzle 4. For convenience of explanation, the orifice 21 is omitted in FIG. 5. When viewed in a direction perpendicular to the discharge direction 20 of the combustion gas and in a horizontal direction, specifically, in a direction perpendicular to the paper surface of FIG. 5, the intersection B between the discharge direction 20 and the tube axis 1c of the furnace body 1 is located at a lower limit of 1 / 2 times the inner diameter d1 of the furnace body 1 and an upper limit of 3 times the inner diameter d1 of the furnace body 1 with respect to the tip A of the spray nozzle 4. If the intersection B is located lower than 1 / 2 times the inner diameter d1 with respect to the tip A, the temperature of the nozzle tip (the surrounding area after the mist is discharged) will be lowered and the drying speed of the mist will be slowed, so that the mist will collide with the furnace wall or the mist will interfere with each other, resulting in a deterioration in the quality of the particles. If the output of the combustion burner 3 is increased in order to raise the temperature of the nozzle tip, the temperature inside the furnace body 1 (furnace temperature) will become too high, resulting in a deterioration in the quality of the particles. Furthermore, if intersection B is located above tip A by more than three times the inner diameter d1, the mist or particles sprayed from spray nozzle 4 cannot be sufficiently dispersed by the swirling flow.
[0030] A bag filter for collecting the generated hollow particles can be installed on the upper part of the spray pyrolysis apparatus 100. A cyclone may be installed in front of the bag filter to reduce the load on the bag filter and to collect coarse particles and foreign matter. In addition, it is preferable to install a heat exchanger, since it is possible to utilize residual heat and reduce the amount of exhaust gas. Furthermore, a dust removal and purification device such as a scrubber may be installed in the rear of the bag filter as necessary.
[0031] By using the spray pyrolysis apparatus 100 of this embodiment, the sprayed mist and particles are carried by the swirling flow and react in the reactor for a long time, so that micro hollow particles can be obtained stably and efficiently. When spray pyrolysis is performed using a raw material liquid that is a raw material for inorganic oxides, if the raw material droplets do not directly contact the flame, a drying reaction will proceed first, and the mist will become hollow particles. If the pyrolysis reaction proceeds next, inorganic oxide hollow particles will be obtained. Here, examples of inorganic oxides include metal oxides, oxides made of alumina, silica, calcia, magnesia, aluminum, and silicon, and more specifically, oxides made of alumina, silica, aluminum, and silicon, titanium oxide, magnesium oxide, calcium oxide, sodium oxide, potassium oxide, lithium oxide, boron oxide, phosphorus oxide, zirconium oxide, barium oxide, cerium oxide, yttrium oxide, and the like, and also include composite oxides that combine these oxides.
[0032] Examples of solvents for dissolving or dispersing the raw materials of the elements constituting these oxides include water and organic solvents, but water is preferred from the viewpoints of environmental impact and production costs. Acids or alkalis may be added as pH adjusters for the solution. Examples of acids that can be used include hydrochloric acid, nitric acid, sulfuric acid, and organic acids, and examples of alkalis include sodium hydroxide, calcium hydroxide, hydroxide hydrate, and the like. Potassium chloride, etc. may also be used.
[0033] In the example shown in Figs. 1 to 5, only one combustion tube 2 is provided, but multiple combustion tubes 2 may be provided at the same height, and multiple groups may be provided at different positions in the vertical direction (hereinafter, multiple combustion tubes provided at the same height will be referred to as the 0th combustion tube group). Note that even when only one combustion tube is provided at the same height, it is still referred to as a "group." By linking the combustion gases discharged from the multiple combustion tubes 2 with each other, a sufficient swirling flow can be generated in the furnace body 1. In addition, by providing multiple combustion tubes 2, the amount of heat equivalent to the heat dissipated by the furnace body 1 can be applied, and the temperature and retention time required for the synthesis of hollow particles can be reproducibly and stably ensured.
[0034] FIG. 6 shows an example in which two combustion tubes, a first combustion tube 2A and a second combustion tube 2B, are provided. In FIG. 6, the orifice 21 is omitted for convenience of explanation. The first combustion tube 2A belonging to the first combustion tube group is disposed closer to the spray nozzle 4 than the second combustion tube 2B belonging to the second combustion tube group, that is, the first combustion tube group is disposed closest to the spray nozzle 4 in the vertical direction. The direction of discharge of the combustion gas from the first combustion tube 2A is defined as a first discharge direction 20A. In this case, when viewed from a direction perpendicular to the first discharge direction 20A and a horizontal direction, the intersection B1 between the first discharge direction 20A and the tube axis 1c of the furnace body 1 is located at a lower limit 1 / 2 times lower than the inner diameter d1 of the furnace body 1 and at an upper limit 1 / 2 times higher than the inner diameter d1 of the furnace body 1 with respect to the tip A of the spray nozzle 4.
[0035] The second combustion tube 2B is disposed above the first combustion tube 2A. The direction of the combustion gas discharged from the second combustion tube 2B is defined as a second discharge direction 20B. When viewed from a direction perpendicular to the second discharge direction 20B and from a horizontal direction, the intersection B2 of the second discharge direction 20B and the tube axis 1c of the furnace body 1 is located above the tip A of the spray nozzle 4 by three times the inner diameter d1 of the furnace body 1, with the upper limit being set therebetween.
[0036] In addition, when three or more combustion tube groups are provided, the third and subsequent combustion tube groups are arranged above the second combustion tube group. For example, if the direction of combustion gas discharged from the combustion tubes belonging to the third combustion tube group is the third discharge direction, when viewed from a direction perpendicular to the third discharge direction and from a horizontal direction, the intersection point between the third discharge direction and the tube axis 1c of the furnace body 1 is located at an upper limit three times the inner diameter d1 of the furnace body 1 relative to the intersection point B2. The fourth and subsequent combustion tube groups are similar to the third combustion tube group. That is, if n is an integer of 3 or more, the intersection point B(n) between the (n)th discharge direction and the tube axis 1c of the furnace body 1 is located at an upper limit three times the inner diameter d1 of the furnace body 1 relative to the intersection point B(n-1) between the (n-1)th discharge direction and the tube axis 1c of the furnace body 1. EXAMPLES
[0037] In the following, specific examples are presented to explain the present invention in more detail, but the present invention is not limited to these examples.
[0038] Examples 1 to 4 A spray pyrolysis apparatus having a furnace body 1 and a combustion tube 2 as shown in Fig. 7 was installed. The inner diameter of the furnace body 1 was 500 mm. The inner diameter of the combustion tube 2 was 500 mm, and the inner diameter near the outlet of the combustion tube 2 was 250 mm due to a tapered structure (throttled portion length 400 mm, gradient 17°). The material of the combustion tube 2 was steel as the base material and monolithic refractory as the lining fireproof material.
[0039] Comparative Examples 1 to 4 A spray pyrolysis apparatus having a furnace body 1 and a combustion tube 2 shown in Figures 8 and 9 was installed. The inner diameter of the furnace body 1 was 500 mm. The inner diameter of the combustion tube 2 was 500 mm or 250 mm, and no throttle structure was provided.
[0040] Next, 1992g of tetraethyl orthosilicate, 131g of aluminum nitrate nonahydrate, 455g of magnesium nitrate hexahydrate, 516g of calcium nitrate tetrahydrate, 1666g of sodium tetraborate decahydrate, and 1L of concentrated nitric acid were mixed in 100L of ion-exchanged water and charged into the solution tank and stirred. The charged raw material solution was sprayed in the form of mist through the spray nozzle 4 by the liquid delivery pump and passed through the furnace body 1.
[0041] The combustion tube 2 includes at least one combustion tube (first combustion tube) and up to three combustion tubes (first to third combustion tubes). The installation positions of each combustion tube 2 relative to the tip of the spray nozzle 4, that is, the position of the intersection (B1 in FIG. 6) between the discharge direction of the first combustion tube and the tube axis 1c of the furnace body 1 when the position of the tip A of the spray nozzle 4 is set to "0", the position of the intersection (B2 in FIG. 6) between the discharge direction of the second combustion tube and the tube axis 1c of the furnace body 1, and the position of the intersection (not shown in FIG. 6) between the discharge direction of the third combustion tube and the tube axis 1c of the furnace body 1 are as shown in Table 1. In Table 1, "+" indicates upward and "-" indicates downward. In Example 4 and Comparative Example 4, the third combustion tube is provided, but the third combustion tube is provided at the same height as the second combustion tube, and the third combustion tube and the second combustion tube belong to the second combustion tube group described above.
[0042] The combustion burner 3 was an LPG burner, and the temperature inside the furnace was controlled by the amount of LPG burner fired to keep it at 900° C. The raw material solution was sprayed from the spray nozzle 4 at 30 L / h, and the particles were rapidly cooled to 300° C. at the outlet of the furnace body 1 with cooling air, and the hollow particles were collected in a bag filter at the downstream stage.
[0043] The recovered hollow particles were evaluated as follows, and the evaluation results are shown in Table 2. Measurement of average particle size The average particle diameter of the inorganic oxide hollow particles was determined by creating a volumetric particle size distribution in accordance with JIS R 1629 using a Microtrac (manufactured by Nikkiso Co., Ltd.) as a particle size distribution measuring device, and determining the particle diameter (d50) corresponding to 50% of the cumulative distribution curve.
[0044] Particle density measurement The particle density of the inorganic oxide hollow particles was measured in accordance with JIS R 1620 using a dry automatic density meter "AccuPic (manufactured by Shimadzu Corporation)."
[0045] Measurement of particle strength Particle strength was measured by the following powder pressing method. (1) A sample was prepared by mixing inorganic oxide hollow particles and ethanol in a weight ratio of 4:1. (2) The sample was placed in a pressure molding machine and a specified pressure (10 MPa, 20 MPa, 30 MPa) was applied using a hydraulic press. (3) The specimen was left to stand for one minute with the specified pressure applied. (4) The sample was removed from the pressure molder and dried at 80°C for 2 hours. (5) The density of the inorganic oxide hollow particles after pressing was measured using a density measuring device (AccuPic, manufactured by Shimadzu Corporation). Then, from the density of the inorganic oxide hollow particles before and after pressure application, the remaining rate for each predetermined pressure was calculated using the following formula, and the pressure at which 50% remained was read from a graph of the remaining rate versus applied pressure. Survival rate P[%]=(1-ρ / y) / ρ×(1 / x-1 / y)×100 (In the formula, ρ represents the density after compression, y represents the true density of the hollow shell, and x represents the density before compression.) The true density of the hollow shell was measured with a density measuring device after heating at or above the melting point in a box-type electric furnace for 6 hours and cooling in order to remove voids.
[0046] [Table 1]
[0047] [Table 2]
[0048] As can be seen from Tables 1 and 2, in Examples 1 to 4, the flow rate of the combustion gas was appropriate due to the throttle structure and the installation of the first combustion tube (combustion burner) at an appropriate position, so that a swirling flow was generated in the furnace body and the residence time was ensured. As a result, hollow particles with low particle density and high particle strength were produced.
[0049] The spray pyrolysis apparatus 100 is not limited to the configuration of the above-mentioned embodiment, and is not limited to the above-mentioned action and effect. Of course, the spray pyrolysis apparatus 100 can be modified in various ways without departing from the scope of the present invention. For example, the configurations and methods of the above-mentioned embodiments may be arbitrarily adopted and combined, and further, one or more of the configurations and methods of the various modified examples described below may be arbitrarily selected and adopted in the configurations and methods of the above-mentioned embodiment.
[0050] In the above embodiment, the combustion tube 2 is connected to the furnace body 1 at an angle of 90°, and the orifice 21 is tapered such that the axis of the orifice 21 coincides with the axis of the combustion tube 2 as shown in FIG. 10(a), but is not limited thereto. For example, the outlet 21a of the orifice 21 may be a square shape as shown in FIG. 10(b), or may be a polygonal shape such as a hexagon. Also, for example, as shown in FIG. 10(c), the combustion tube 2 may be connected to the furnace body 1 at an angle of less than 90°. Also, for example, as shown in FIG. 10(d), the orifice 21 may be shaped such that the axis of the orifice 21 is shifted from the axis of the combustion tube 2.
[0051] When multiple combustion tubes are provided, they may be provided at different heights or at the same height. When multiple combustion tubes are provided at the same height, the multiple combustion tubes are provided at intervals in the circumferential direction of the furnace body 1. In the example shown in Figure 11, three combustion tubes 2 are provided at different heights and are provided at equal intervals in the circumferential direction of the furnace body 1.
[0052] In the above embodiment, the combustion tube 2, the first combustion tube 2A, and the second combustion tube 2B are provided one by one, but this is not limited to this. For example, a plurality of combustion tubes 2 may be provided at the same height. Similarly, a plurality of first combustion tubes 2A may be provided at the same height.
[0053] Also, for example, as shown in FIG. 12, the multiple combustion tubes 2 may each be connected to the furnace body 1 at an angle of less than 90°. [Explanation of symbols]
[0054] 100: Spray pyrolysis equipment 1: Furnace body 1c: Tube axis of furnace body 2: Combustion tube 2A: First combustion tube 2B: Second combustion tube 2a: End of combustion tube 2b: End of the combustion tube 3: Combustion burner 4: Spray nozzle 20: Combustion gas discharge direction 20A: First discharge direction 20B: Second discharge direction 21: Aperture 21a: aperture outlet A: Tip of spray nozzle B: Intersection of the combustion gas discharge direction and the tube axis of the furnace body B1: Intersection of the first discharge direction and the tube axis of the furnace body B2: Intersection of the second discharge direction and the tube axis of the furnace body d1: Inner diameter of furnace body d21: Inner diameter of the aperture outlet
Claims
1. A furnace body consisting of a vertical tube; At least one combustion tube connected to the outer circumferential surface of the furnace body; A combustion burner is disposed at an end of the combustion tube opposite to the furnace body and generates a flame toward the furnace body; A spray nozzle is disposed on the tube axis at the bottom of the furnace body and sprays the aqueous solution upward; The combustion tube is arranged so that the discharge direction of the combustion gas from the combustion tube does not intersect with the tube axis of the furnace body, The combustion tube has a throttle at a connection portion with the furnace body, The combustion tubes are provided in a plurality of groups at different positions in the vertical direction, the plurality of combustion tube groups includes a first combustion tube group that is closest to the spray nozzle in a vertical direction, When viewed from a direction perpendicular to a first discharge direction from the combustion tubes belonging to the first combustion tube group and from a horizontal direction, an intersection B1 between the first discharge direction and a tube axis of the furnace body is located at a lower limit of 1 / 2 times the inner diameter of the furnace body and an upper limit of 1 / 2 times the inner diameter of the furnace body with respect to a tip A of the spray nozzle, the second combustion tube group is disposed above the first combustion tube group, When viewed from a direction perpendicular to a second discharge direction from the combustion tubes belonging to the second combustion tube group and from a horizontal direction, an intersection B2 between the second discharge direction and a tube axis of the furnace body is located at an upper limit three times the inner diameter of the furnace body 1 with respect to a tip A of the spray nozzle, The third and subsequent combustion tube groups are disposed above the second combustion tube group, A spray pyrolysis apparatus in which, when viewed from a direction perpendicular to the (n)th discharge direction from a combustion tube belonging to the (n)th combustion tube group and a horizontal direction, an intersection B(n) of the (n)th discharge direction and a tube axis of the furnace body is located up to three times the inner diameter of the furnace body relative to an intersection B(n-1) of the (n-1)th discharge direction and a tube axis of the furnace body, where n is an integer of 3 or more.
2. 2. The spray pyrolysis apparatus according to claim 1, wherein an inner diameter of the outlet of the throttle is equal to or smaller than half an inner diameter of the furnace body.
3. 3. The spray pyrolysis apparatus according to claim 1, wherein the gradient θ of the throttle is 5 to 75°.
Citation Information
Patent Citations
Treatment of mineral at high temperature
JP1990157037A
Spray type pyrolyzing / synthesizing device
JP2001137699A
Powder production apparatus
JP2004292223A
Powder production apparatus
JP2007084355A
Spray thermal decomposition device
JP2019025385A