Method for forming narrow trenches
By employing solubility-shifting materials to alter the solubility of adjacent structures, the method addresses overlay errors and misalignment in photolithography, enhancing pattern precision and reducing complexity in microfabrication.
Patent Information
- Application Number
- JP2022516287
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-09-19
- Filing Date
- 2020-09-17
- Publication Date
- 2024-09-20
- Estimated Expiration
- 2040-09-17
AI Technical Summary
Existing microfabrication techniques face challenges in forming precise patterns on substrates due to overlay errors and misalignment in photolithography, leading to reduced throughput and increased complexity in pattern stitching.
The use of solubility-shifting materials, such as thermal or photoacid generators, is applied to diffuse and alter the solubility of adjacent structures, allowing for the formation of precise patterns and gaps between features even in the presence of misalignment, through methods like 'snap-to' and 'snap-away' techniques.
This approach effectively mitigates overlay errors and misalignment issues, enabling the formation of sub-resolution trenches and slot contacts, improving pattern precision and reducing the complexity of pattern stitching in microfabrication processes.
Smart Images

Figure 0007554539000006 
Figure 0007554539000031 
Figure 0007554539000049
Abstract
Description
[Technical field]
[0001] This disclosure claims the benefit of priority to U.S. Provisional Application No. 62 / 902,434, filed Sep. 19, 2019, the contents of which are incorporated herein by reference in their entirety.
[0002] This application relates to the field of microfabrication, including the microfabrication of integrated circuits and processes in patterning semiconductor substrates. [Background technology]
[0003] In material processing methods (e.g., photolithography), forming a patterned layer typically involves applying a thin layer of radiation-sensitive material, such as photoresist, to the top surface of a substrate. This radiation-sensitive material is transferred to a patterned mask, which is used to etch or transfer the pattern to an underlying layer of the substrate. Typically, the patterning step of the radiation-sensitive material involves exposing the radiation-sensitive material to a radiation source through a reticle (and associated optics), for example, using a photolithography system. This exposure creates a latent pattern in the radiation-sensitive material, which is then developed. The term developing refers to dissolving and removing parts of the radiation-sensitive material to form a geometric or relief pattern. For example, the developing step may involve removing the irradiated areas (in the case of a positive photoresist) or the unirradiated areas (in the case of a negative resist) of the radiation-sensitive material using a developing solvent. The relief pattern can then function as a mask layer. Summary of the Invention [Problem to be solved by the invention]
[0004] The present disclosure relates to forming a pattern on a substrate. [Means for solving the problem]
[0005] A first aspect is a method of forming a pattern on a substrate. The method includes forming a first layer on an underlayer of the substrate, the first layer being patterned to have a first structure. A graft material is deposited on a side of the first structure, the graft material having a solubility-shifting material. The graft material diffuses a predetermined distance to an adjacent structure adjacent the solubility-shifting material, the solubility-shifting material changing the solubility of the adjacent structure in a developer. The developer is used to remove soluble portions of the adjacent structure to form a second structure.
[0006] In an embodiment, the first structure comprises a first opening in the first layer. The adjacent structure is part of the first layer, and the first layer may comprise a photoresist material. The second structure comprises a second opening in the first layer, and a latent pattern of the second openings is formed by patterned exposure of the first layer to actinic radiation prior to the step of diffusing the solubility-shifting material. In one example, the solubility-shifting material renders the adjacent structure insoluble to the developer, and the first opening is spaced from the second opening by at least the predetermined distance. In another example, the solubility-shifting material renders the adjacent structure soluble to the developer, and the first opening is bonded to the second opening.
[0007] In an embodiment, the first structure comprises a mandrel or a line. The adjacent structure may be part of the first layer. The step of depositing the graft material is accomplished by coating the substrate with a solution containing the graft material, and the graft material is deposited on all uncoated surfaces of the substrate. After the step of diffusing the solubility-shifting material, the method further comprises the steps of removing the graft material from the substrate, and depositing a photoresist material on the substrate to form a latent pattern of the second structure, the photoresist material abutting the first structure. For example, the solubility-shifting material renders the abutting portion of the fill material soluble in the developer, and the first structure is spaced from the second structure by at least the predetermined distance.
[0008] A second aspect is a method of forming a pattern on a substrate. The method includes forming a patterned first layer on an underlayer of the substrate, the patterned first layer having a first material and the underlayer having a second material that is chemically different from the first material. The patterned first layer has a first structure. A graft material is deposited on the substrate, the graft material selectively adhering to an uncoated surface of the first structure. The graft material includes a solubility shift material. A filler material is deposited on the substrate, the filler material abutting the graft material. The solubility shift material diffuses a predetermined distance into the abutting portion of the filler material, the solubility shift material changing the solubility of the abutting portion of the filler material in a developer. The soluble portion of the filler material is removed using the developer, and the remaining portion of the filler material forms a second structure.
[0009] In one embodiment, the solubility-shifting material renders the abutting portion of the fill material soluble in the developer and the first structure is spaced from the second structure by at least the predetermined distance, while in another embodiment, the solubility-shifting material renders the abutting portion of the fill material insoluble in the developer and the first structure is in contact with the second structure.
[0010] In some embodiments, the solubility-shifting material comprises a thermal acid generator, and the method further comprises activating the thermal acid generator by heating before diffusing the solubility-shifting material into the filler material. In some embodiments, the solubility-shifting material comprises a photoacid generator, and the method further comprises activating the photoacid generator by actinic radiation before diffusing the solubility-shifting material into the filler material. For example, the actinic radiation is performed using a photomask, and the solubility-shifting material is activated by patterned exposure to actinic radiation. In some embodiments, the solubility-shifting material comprises a base that neutralizes an acid.
[0011] In some embodiments, the fill material comprises a photoresist material, and the method further comprises forming a latent pattern of the second structures in the photoresist material via patterned exposure to actinic radiation prior to diffusing the solubility-shifting material into the fill material, and in some instances, the latent pattern overlaps the abutting portions of the photoresist material.
[0012] In one embodiment, the first structure comprises a mandrel or a line, which may be cured prior to deposition of the graft material onto the substrate.
[0013] A third aspect is a method of forming a pattern on a substrate. The method includes forming a patterned first layer on an underlayer of the substrate, the patterned first layer having a first structure. A graft material is deposited on the substrate, the graft material selectively adhering to uncoated surfaces of the first structure to obtain a predetermined thickness of the graft material on the sidewalls of the first structure. A second structure is formed on the substrate from a photoresist, the second structure abutting the graft material. The graft material is removed, and the first structure is spaced from the second structure by a distance corresponding to the predetermined thickness.
[0014] Aspects of the present disclosure are best understood from the following detailed description taken in conjunction with the accompanying drawings, in which: It is noted that, in accordance with standard industry practice, the various features have not been illustrated to scale, and in fact the dimensions of the various features may be expanded or reduced for clarity of presentation. [Brief description of the drawings]
[0015] [Figure 1] 1 is a flowchart of a method for forming a pattern on a substrate according to an embodiment of the present disclosure. [Diagram 2] 1 is a flowchart of a method for forming a pattern on a substrate according to an embodiment of the present disclosure. [Figure 3A] 1A-1D depict schematic cross-sectional views of a substrate at various intermediate stages of patterning with a thermal acid generator (TAG) according to embodiments of the present disclosure. [Figure 3A1] 1A-1D depict schematic top-down views of a substrate at various intermediate stages of patterning with a thermal acid generator (TAG) according to embodiments of the present disclosure. [Figure 3B] 1A-1D depict schematic cross-sectional views of a substrate at various intermediate stages of patterning with a thermal acid generator (TAG) according to embodiments of the present disclosure. [Figure 3B1] 1A-1D depict schematic top-down views of a substrate at various intermediate stages of patterning with a thermal acid generator (TAG) according to embodiments of the present disclosure. [Figure 3C] 1A-1D depict schematic cross-sectional views of a substrate at various intermediate stages of patterning with a thermal acid generator (TAG) according to embodiments of the present disclosure. [Figure 3C1] 1A-1D depict schematic top-down views of a substrate at various intermediate stages of patterning with a thermal acid generator (TAG) according to embodiments of the present disclosure. [Figure 3D] 1A-1D depict schematic cross-sectional views of a substrate at various intermediate stages of patterning with a thermal acid generator (TAG) according to embodiments of the present disclosure. [Figure 3D1] 1A-1D depict schematic top-down views of a substrate at various intermediate stages of patterning with a thermal acid generator (TAG) according to embodiments of the present disclosure. [Figure 3E] 1A-1D depict schematic cross-sectional views of a substrate at various intermediate stages of patterning with a thermal acid generator (TAG) according to embodiments of the present disclosure. [Figure 3E1] 1A-1D depict schematic top-down views of a substrate at various intermediate stages of patterning with a thermal acid generator (TAG) according to embodiments of the present disclosure. [Figure 4A] 1A-1D depict schematic cross-sectional views of a substrate at various intermediate stages of patterning with a photoacid generator (PAG), according to embodiments of the present disclosure. [Figure 4A1] 1A-1D depict schematic top-down views of a substrate at various intermediate stages of patterning with a photoacid generator (PAG), according to embodiments of the present disclosure. [Figure 4B] 1A-1D depict schematic cross-sectional views of a substrate at various intermediate stages of patterning with a photoacid generator (PAG), according to embodiments of the present disclosure. [Figure 4B1] 1A-1D depict schematic top-down views of a substrate at various intermediate stages of patterning with a photoacid generator (PAG), according to embodiments of the present disclosure. [Figure 4C] 1A-1D depict schematic cross-sectional views of a substrate at various intermediate stages of patterning with a photoacid generator (PAG), according to embodiments of the present disclosure. [Figure 4C1]1A-1D depict schematic top-down views of a substrate at various intermediate stages of patterning with a photoacid generator (PAG), according to embodiments of the present disclosure. [Figure 4D] 1A-1D depict schematic cross-sectional views of a substrate at various intermediate stages of patterning with a photoacid generator (PAG), according to embodiments of the present disclosure. [Figure 4D1] 1A-1D depict schematic top-down views of a substrate at various intermediate stages of patterning with a photoacid generator (PAG), according to embodiments of the present disclosure. [Figure 4E] 1A-1D depict schematic cross-sectional views of a substrate at various intermediate stages of patterning with a photoacid generator (PAG), according to embodiments of the present disclosure. [Figure 4E1] 1A-1D depict schematic top-down views of a substrate at various intermediate stages of patterning with a photoacid generator (PAG), according to embodiments of the present disclosure. [Figure 4F] 1A-1D depict schematic cross-sectional views of a substrate at various intermediate stages of patterning with a photoacid generator (PAG), according to embodiments of the present disclosure. [Figure 4F1] 1A-1D depict schematic top-down views of a substrate at various intermediate stages of patterning with a photoacid generator (PAG), according to embodiments of the present disclosure. [Figure 5A] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 5B] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 5C] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 5D]FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 5E] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 5F] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 5M] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 5N] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 5P] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 5Q] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 6A] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 6B]FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 6C] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 6D] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 6E] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 6F] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 6M] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 6N] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 6P] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 6Q]FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 7A] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 7B] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 7C] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 7D] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 7M] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 7N] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 7P] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 7Q]FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 8A] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 8B] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 8C] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 8D] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 8M] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 8N] FIG. 13 illustrates an example of using functional graft materials to form gaps or connections between structures or openings even in the event of overlay errors or photolithographic misalignment, according to an embodiment of the present disclosure. [Figure 9A] 1A-1D show schematic three-dimensional (3D) views of a substrate at various intermediate stages of pattern formation according to embodiments of the present disclosure. [Figure 9A1] 1A-1D show schematic top-down views of a substrate at various intermediate stages of pattern formation according to embodiments of the present disclosure. [Figure 9B] 1A-1D show schematic three-dimensional (3D) views of a substrate at various intermediate stages of pattern formation according to embodiments of the present disclosure. [Figure 9B1] 1A-1D show schematic top-down views of a substrate at various intermediate stages of pattern formation according to embodiments of the present disclosure. [Figure 9C] 1A-1D show schematic three-dimensional (3D) views of a substrate at various intermediate stages of pattern formation according to embodiments of the present disclosure. [Figure 9C1] 1A-1D show schematic top-down views of a substrate at various intermediate stages of pattern formation according to embodiments of the present disclosure. [Figure 9D] 1A-1D show schematic three-dimensional (3D) views of a substrate at various intermediate stages of pattern formation according to embodiments of the present disclosure. [Figure 9D1] 1A-1D show schematic top-down views of a substrate at various intermediate stages of pattern formation according to embodiments of the present disclosure. [Figure 9E] 1A-1D show schematic three-dimensional (3D) views of a substrate at various intermediate stages of pattern formation according to embodiments of the present disclosure. [Figure 9E1] 1A-1D show schematic top-down views of a substrate at various intermediate stages of pattern formation according to embodiments of the present disclosure. [Figure 9F] 1A-1D show schematic three-dimensional (3D) views of a substrate at various intermediate stages of pattern formation according to embodiments of the present disclosure. [Figure 9F1] 1A-1D show schematic top-down views of a substrate at various intermediate stages of pattern formation according to embodiments of the present disclosure. [Figure 10A] 10 illustrates the formation of a pattern on a substrate according to the exemplary process of FIG. [Figure 10B] 10 illustrates the formation of a pattern on a substrate according to the exemplary process of FIG. [Figure 10C] 10 illustrates the formation of a pattern on a substrate according to the exemplary process of FIG. [Figure 11]1 is a flow chart of a method for forming a pattern on a substrate according to one embodiment of the present disclosure. [Figure 12A] 1A-1D show schematic 3D and top view diagrams of a substrate at various intermediate stages of pattern formation according to an embodiment of the present disclosure. [Figure 12B] 1A-1D show schematic 3D and top view diagrams of a substrate at various intermediate stages of pattern formation according to an embodiment of the present disclosure. [Figure 12C] 1A-1D show schematic 3D and top view diagrams of a substrate at various intermediate stages of pattern formation according to an embodiment of the present disclosure. [Figure 12D] 1A-1D show schematic 3D and top view diagrams of a substrate at various intermediate stages of pattern formation according to an embodiment of the present disclosure. [Figure 12E] 1A-1D show schematic 3D and top view diagrams of a substrate at various intermediate stages of pattern formation according to an embodiment of the present disclosure. [Figure 12F] 1A-1D show schematic 3D and top view diagrams of a substrate at various intermediate stages of pattern formation according to an embodiment of the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0016] In the following disclosure, many different embodiments or examples are provided that embody different features of the provided subject matter. In the following, specific examples of components and arrangements are described for the sake of brevity of the disclosure. It should be understood that these are merely examples and are not intended to be limiting. For example, in the following description, forming a first feature above or on top of a second feature may have an embodiment in which the first and second features are formed in direct contact, and may have an embodiment in which an additional feature is formed between the first and second features, and the first and second features are not in direct contact. Also, in the present disclosure, reference numerals and / or terms may be repeated in various examples. This repetition is for simplicity and clarity, and does not in itself represent a relationship between the various embodiments and / or configurations described. Furthermore, spatial relative terms such as "top", "bottom", "lower", "lower", "lower", "top", and "upper" are used for ease of description and to describe the relationship of one element or feature to another element or feature as shown in the drawings. The spatially relative terms are intended to encompass different orientations of the device during use or operation in addition to the orientation depicted in the figures. The device may be in other orientations (rotated 90 degrees or at other orientations) and the spatially relative terms used herein may be interpreted accordingly.
[0017] The order of discussion of the different steps described herein is presented for clarity. Generally, these steps can be performed in any suitable order. Also, although different features, techniques, configurations, etc. in the present application may each be described in different parts of the present disclosure, it is intended that each concept can be implemented independently of each other or in combination with each other. Thus, the present invention can be implemented and viewed in many different ways.
[0018] One approach to printing features at sub-resolution pitch is to split the pattern between two masks at a relaxed pitch and recombine it in successive lithography and etch steps. However, this approach can result in overlay errors and edge placement errors (EPE). One problem with this approach is that the throughput is reduced if the pattern is split into two exposures and etches. The second problem is misregistration due to multi-patterning. Anti-spacers are a self-aligning process that is not subject to resolution limitations and can address both of these challenges simultaneously. Also, similar techniques for anti-spacer formation described in this application can be used for "snap to" and "snap away" techniques. Also, in snap techniques, the effect of overlay is mitigated by using reactive chemical species at the edge set.
[0019] In the anti-spacer technique, the diffusion length of the reactive species is used to define the critical dimension (CD), for example, to form either a narrow trench or a slot contact. The CD can be tuned through molecular weight modification of the reactive species, molecular structure of the reactive species, and thermal treatment temperature / time. If the reactive species can be spatially controlled by exposure through a mask or selective deposition, a narrow slot contact can be formed instead of a narrow trench. Another approach to forming a narrow slot contact is to use a keep / cut mask after the formation of the narrow trench. However, this technique introduces another lithography exposure and film stack. For ease of explanation, this disclosure focuses on the use of acid as the reactive species as an example.
[0020] The techniques described herein include a process flow for patterning a substrate using the diffusion length of a solubility-shifting material to form narrow trenches or provide buffers (i.e., slot contacts) between adjacent structures or openings. The techniques described include forming a patterned first layer having a first structure, depositing a graft material including a solubility-shifting material on the side surface of the first structure, diffusing the solubility-shifting material into the adjacent structures, and removing the soluble portions of the adjacent structures. By controlling the diffusion conditions and times, sub-resolution CDs can be defined and exploited for "snap-to" and "snap-away" techniques.
[0021] 1 is a flow chart of a method 100 of forming a pattern on a substrate according to one embodiment of the present disclosure. Method 100 begins at step S101, where a first layer is formed on an underlying layer of a substrate and patterned to have a first structure. The first structure can include, for example, first layer mandrels / lines (e.g., FIGS. 3-6 and 9-10), or openings (e.g., FIGS. 7-8).
[0022] In step S102, a graft material comprising a solubility-shifting material is deposited on the side surfaces of the first structures. In some embodiments, the graft material selectively adheres to the uncoated surfaces of the first structure lines (e.g., Figures 3-6). In other embodiments, the graft material is non-selectively deposited on all of the uncoated surfaces of the substrate (e.g., Figures 7-10). For example, the graft material may be deposited on the side and bottom surfaces of the openings and the top surface of the patterned first layer (e.g., Figures 7-8). In another example, the graft material may be deposited on the side and top surfaces of the mandrel and the top surface of the underlayer (e.g., Figures 9-10).
[0023] In steps S103 and S104, the solubility-shifting material is diffused a predetermined distance into an adjacent structure adjacent to the solubility-shifting material, and then the soluble portion of the adjacent structure is removed using a developer to form a second structure. The solubility-shifting material is designed to change the solubility of the adjacent structure in a particular developer. In some embodiments, the solubility-shifting material makes the adjacent structure soluble in a particular developer, and the first structure is spaced from the second structure by at least a predetermined distance (e.g., Figures 3-6 and 9-10). In some embodiments, the solubility-shifting material makes the adjacent structure insoluble in a particular developer, and the first structure comes into contact with the second structure (e.g., Figures 5-6). In some embodiments, the solubility-shifting material makes the adjacent structure soluble in a particular developer, and the first structure comes into contact with the second structure (e.g., Figures 7-8). In some embodiments, the solubility-shifting material renders adjacent structures insoluble to a particular developer, and the first structure is spaced from the second structure by at least a predetermined distance (e.g., FIGS. 7-8). Also, in some embodiments, the solubility-shifting material may be activated prior to step S103.
[0024] Referring again to steps S103 and S104, the adjacent structure is part of the first layer, and in one example, the first structure is an opening in the first layer (e.g., FIGS. 7-8). The second structure then becomes a second opening, which may be spaced apart from or in contact with the first opening. In another example, where the first structure is a mandrel or line, the adjacent structure may be part of the first layer (e.g., FIGS. 9-10), or may be a layer of photoresist material deposited on the substrate after deposition of the graft material (e.g., FIGS. 3-6). In fact, method 100 has at least eleven embodiments (e.g., FIGS. 3-10) that represent various process flows, each of which is described in more detail below.
[0025] FIG. 2 is a flow chart of a method 200 for forming a pattern on a substrate according to an embodiment of the present disclosure. The method 200 includes at least six embodiments of the method 100 in FIG. 1 (e.g., FIGS. 3-6). In step S201, a patterned first layer is formed on an underlayer of a substrate. The patterned first layer has a first material, and the underlayer has a second material, the second material being chemically different from the first material. The patterned first layer may also have a first structure, such as a mandrel or a line. For example, the mandrel may be composed of a first photoresist material. It is noted that while the description of the method 200 focuses on the first photoresist material and the mandrels, the first material may be a hard mask material and the first structure may have other structures.
[0026] In step S202, a graft material including a solubility-shifting material is deposited on the substrate, and the graft material selectively adheres to the uncoated surface of the first structure. The graft material (also called a brush) is a polymer or short-chain polymer with an attachment group. Based on the particular head group selected, the graft material can attach to the surface of a particular material without attaching to the surface of another material. The graft material may be a self-assembled monolayer (SAM). In one aspect, the graft material is preferably a polymer more than formed of hydrocarbon chains. The graft material may be deposited by spin-on deposition, physical vapor deposition, or other methods. In one embodiment, a bake process is performed after deposition of the particular graft material. The bake bonds the graft material to the first photoresist material without bonding to the underlayer. A solvent strip process may then be used to remove the unbonded material (such as the bedding material). The other side of the grafted material may have a functional group, such as a thermal acid generator (TAG), a photoacid generator (PAG), a base, or other solubility-shifting material.
[0027] In step S203, a filler material is deposited on the substrate. The filler material abuts the graft material. For example, an overcoat of filler material can be deposited on the patterned first layer. The filler material can be a second photoresist material or another filler material that responds to the solubility shift material. In an embodiment, the filler material is selected to be essentially soluble in the developer upon reaction with acid. One example of a filler material that is primarily used in this disclosure is a polymer with a protective group that reacts with acid to dissolve in a given developer.
[0028] In step S204, a solubility-shifting material is diffused into the abutting portion of the fill material by a predetermined distance, such that the solubility-shifting material changes the solubility of the abutting portion of the fill material in a particular developer. In step S205, the soluble portion of the fill material is removed using the developer, such that the remaining portion of the fill material forms the second structure. In some embodiments, the solubility-shifting material renders the abutting portion of the fill material soluble in the developer, such that the first structure is spaced apart from the second structure by at least a predetermined distance. In other embodiments, the solubility-shifting material renders the abutting portion of the fill material insoluble in the developer, such that the first structure is in contact with the second structure. In some embodiments, an activation step may be performed prior to step S204 to activate the solubility-shifting material.
[0029] 3 shows schematic cross-sectional and top views of a substrate 300 at various intermediate stages of TAG patterning according to an embodiment of the present disclosure. In particular, FIG. 3 shows a method of forming narrow trench and slot contacts using a graft material having functional groups. The functional groups are TAG, and the method may be an embodiment of the method 200 in FIG. 2. Some of the description has already been given and will be omitted here for brevity.
[0030] 3A1-3E1 are top views of the substrate 300, and FIG. 3A-3E are corresponding cross-sectional views along the cutting line Aa-Ee in the z-direction. As shown in FIG. 3A, a patterned first layer 310 is formed on an underlayer 320 of the substrate 300. The patterned first layer 310 has a first structure, such as a mandrel 311. For example, FIG. 3A and 3A1 show the obtained shape pattern after exposure and development of a first photoresist layer. It is noted that although photoresist is used here as a primary example, the initial pattern may be photoresist or other materials, such as a hard mask material.
[0031] 3B and 3B1, graft material 321 is selectively deposited onto the uncoated surface of mandrel 311. As a result, graft material 321 adheres to top surface 311' and side surface 311'' of mandrel 311, but does not adhere to the uncoated top surface 301' of underlayer 301. Corresponding to the graft material in step S202 in FIG. 2, graft material 321 has TAG as an example of a solubility-shifting material.
[0032] In Figures 3C and 3C1, a fill material 331 is deposited on the substrate to form an overcoat over the mandrels 311. Similarly, the fill material 331 may be polymeric and have protective groups that react with acid to make it more soluble in a given developer. Spin-coating is a common method of depositing such overcoats, and the resulting overcoat typically not only fills spaces but also completely covers the first patterned first layer. The overcoat may be planarized (flat as shown) or not (not shown). Additionally, the fill material is effectively free of solubility-shifting material, meaning that the fill material does not contain solubility-shifting material or that the amount of solubility-shifting material is insufficient to result in a small change in solubility.
[0033] In Figures 3D and 3D1, the TAG in the graft material 321 is diffused a predetermined distance into the abutting portion of the fill material 341, and the TAG changes the solubility of the abutting portion of the fill material in the developer. In one embodiment, a bake step is performed, which causes the acid to diffuse into the fill material 331, making the diffused portion 341 soluble. After the acid has reacted with the fill material 331 to a selected distance, the substrate 300 is baked at a higher temperature to decompose the crosslinker in the mandrels 311, further reducing the solubility of the mandrels 311. For example, the post-exposure bake (PEB) for a particular resist is about 90°C, while the TAG can be activated and diffused between 120-130°C. A given crosslinker can be activated with a bake of 150-160°C. In one embodiment, the TAG should be selected so that it does not decompose during the PEB of the initial patterning (i.e., the patterned first layer 310). In some embodiments, the crosslinker is not decomposed until after both the PEB and TAG bakes.
[0034] In this embodiment, the TAG renders the abutting portions of the fill material 341 soluble to a developer. As a result, in Figures 3E and 3E1, the abutting portions of the fill material 341 are removed. In particular, a development step is performed to remove the soluble portions (i.e., the abutting portions) of the fill material 341. This leaves narrow trenches 351 in the sidewalls 311'' of the mandrels 311 and spaces the first structure (i.e., the mandrels 311) from the second structure (i.e., the remaining fill material 331) by at least a predetermined distance. Any subsequent patterning process can then be continued, for example, by masking portions of the narrow trenches and selectively transferring them to an underlying layer.
[0035] 4 shows schematic cross-sectional and top views of a substrate 400 at various intermediate stages of patterning with PAG, according to an embodiment of the present disclosure. Similar to FIG. 3, FIG. 4 shows a method of forming narrow trench and slot contacts using a graft material with functional groups. The functional groups are PAGs, and this method can be an embodiment of method 200 of FIG. 2. Compared to TAGs, PAGs are more thermally stable and can provide spatial control via controlled exposure to actinic radiation.
[0036] Similarly, Figures 4A1-4F1 are top views of substrate 400, and Figures 4A-4F are corresponding cross-sectional views along cut line A1a'-E'e' in the z-direction. Figures 4A and 4A1 show a patterned first layer 410 with mandrels 411 on top of underlayer 401. Figures 4B and 4B1 show attachment of graft material 421, including PAG, to mandrels 411. Figures 4C and 4C1 show an overcoat of fill material 431. In Figures 4D and 4D1, a patterned photolithographic exposure is performed, where a photomask 441 is placed on substrate 400. The arrows represent incident light, such as ultraviolet light. In Figures 4E and 4E1, a bake step causes the acid resulting from the exposure to diffuse a predetermined distance into fill material 451. This predetermined distance is a function of the amount of acid generated, the bake time, and the bake temperature (for example), and thus the distance can be precisely controlled. 4F and 4F1 show the formation 461 of narrow slots (eg, narrow trenches) after a development step.
[0037] 5-8 show embodiments in which gaps (e.g., narrow trenches) or connections (e.g., slot contacts) are formed between structures or openings using functional grafting materials (e.g., TAG, PAG, or bases) even in the case of overlay errors or photolithographic misalignment. Therefore, some descriptions have already been provided and will be omitted here for process simplicity.
[0038] FIG. 5 shows schematic 3D and top views of a substrate 500 at various intermediate stages of pattern formation according to an embodiment of the present disclosure. FIG. 5A shows an incident patterned line (structure) 511 on an underlying layer 501 of the substrate 500, which corresponds to the first structure in the method 200. In this example, the line 511 is composed of a first photoresist material and is formed by photolithography. The line 511 can be developed using a positive tone developer (PTD). After formation, a process step of direct current superposition (DCS) is performed to harden the photoresist line 511 and prevent it from becoming soluble. DCS is performed in a plasma chamber by coupling a negative DC power to the upper electrode of the plasma chamber to generate a flux of ballistic electrons that impinge on the substrate 500. As a result, the exposed surfaces of the lines 511, including the top surface 511' and the two side surfaces 511, undergo a change in physical properties and become insoluble to the solvent, forming a new membrane 513 surrounding the lines 511. Cross-linking may occur within the membrane 513 during the DCS process. Other processes such as thermal freezing, gas freezing, etc. may also be utilized.
[0039] Next, in FIG. 5B, a graft material 521 having acid functional groups is coated on the lines 511 (more precisely, on the film 513). Next, in FIG. 5C, a second photoresist material 531 is deposited. In FIG. 5D, the substrate 500 is exposed to a second pattern of actinic radiation. The actinic radiation (represented by arrows) is irradiated through a photomask 543 placed over the substrate 500, resulting in the formation of a second latent pattern (not shown) in the second photoresist material 531. The acid functional groups are then activated and diffuse into the second photoresist material 531 for a predetermined distance, forming a diffusion layer 541. Inside the diffusion layer 541, the second photoresist 531 that has received sufficient acid changes its solubility with the acid. Here, the acid makes the diffusion layer 541 soluble. In the embodiment in which the acid functional groups are TAG, a bake step is performed for both activation and diffusion. In another embodiment where the acid functional group is a PAG, actinic radiation exposure (e.g., flood or patterned exposure at certain wavelengths to which the second photoresist material 531 is not sensitive) is performed for activation, followed by baking for diffusion.
[0040] In Figure 5E, the second pattern is developed, such as by PTD, to remove the soluble portions of the second photoresist layer 531, including the diffusion layer 541. As a result, the remaining insoluble second photoresist material 531 forms a second structure 551. Furthermore, a gap 553 is formed between the first structure 511 and the second structure 551. In an embodiment, the graft material 521 may be removed to further widen the gap 553, as shown in Figure 5F.
[0041] 5M and 5N are top views of FIG. 5D and FIG. 5E, respectively. In FIG. 5M, the arrows represent the diffusion process, the dashed lines represent the areas exposed to actinic radiation in FIG. 5D, and the latent pattern is represented by 533, which will eventually become the second structure 551. FIG. 5M shows that even if the exposure (i.e., the dashed areas) is misaligned and the lines (i.e., 513 and 533) are too close, the diffusion (i.e., 541) from the graft material 521 will substantially shorten the second line 533 approaching the first line 513, causing it to "snap away" from the first line 513. In other words, in this embodiment, the acid is diffused into the second line 533, ensuring that in FIG. 5N, a gap 553 exists. This may provide many patterning advantages, such as preventing short circuit current paths between structures.
[0042] Figures 5P and 5Q are top views of structures similar to Figures 5D and 5E, respectively, according to another embodiment in which a "snap-to" structure is formed. This embodiment is similar to that already described with respect to Figures 5A-5F, except that the graft material 521 contains a base instead of an acid generator. The diffusion layer 541 is made insoluble by the base in the PTD, and the soluble portion of the second photoresist layer 531 is removed. It is noted that in Figure 5M, even though the exposure of the second lines 551 (i.e., latent pattern 533) does not reach the first lines 513, after diffusion (i.e., 541), the first lines 513 are substantially wider and the two lines touch without a gap separating them.
[0043] 6 shows schematic 3D and top views of a substrate 600 at various intermediate stages of pattern formation according to another embodiment of the present disclosure. FIG. 6 is similar to FIG. 5, so the differences will be emphasized. Here, an inverse photomask 643 is used, and photomask 643 and photomask 543 are complementary to each other. That is, in this embodiment, the exposed areas of photomask 543 are the blocked areas of photomask 643, and the exposed areas of photomask 643 are the blocked areas of photomask 543. Furthermore, the second photoresist material 631 is negative rather than positive.
[0044] Figures 6M and 6N are top views of Figures 6D and 6E, respectively, according to one embodiment in which a "snap-away" structure is formed. Similarly, in Figure 6M, the arrows represent the diffusion process while the dashed areas represent the areas exposed to actinic radiation in Figure 6D, and the latent pattern is represented at 633, which ultimately becomes the second structure 651. In this embodiment, the graft material 621 includes a base (which can neutralize excess acid). The first line 611 is developed using a PTD while the second line 651 is developed using an NTD. Note that after exposure, in FIG. 6M, the latent pattern 633 extends to the graft material 621 (so that the two lines touch), but then the acid is neutralized in the latent pattern of the second line 633 by diffusion of the base away from the first line 613, so that this material (i.e., diffusion layer 641) remains insoluble to the NTD and is then removed, ensuring a gap 653 between the first line 613 and the second line 651 in FIG. 6N.
[0045] 6P and 6Q are top views of structures similar to those of FIG. 6D and 6E, respectively, according to another embodiment in which a "snap-to" structure is formed. In this embodiment, the graft material 621 has acid functional groups (e.g., TAG or PAG). The first line 611 can be developed with a PTD or NTD, and the second line 651 with an NTD. Similarly, the bonding of the structures can be ensured even in the case of an overlay error. A latent pattern 633 is formed in a second photoresist 631 deposited on top of the substrate 600. Then, diffusion (i.e., 641) from the first line 613 ensures the bonding of the two lines. In other words, in this embodiment, acid is diffused from the first line 611, making the area 641 around the first line insoluble to the NTD. After the development of the second line 651, the first line 611 and the second line 651 are bonded. Without the diffusion step, a gap would result between the two structures.
[0046] 7 and 8 show "snap-to" and "snap-away" structures having openings (e.g., trenches) instead of lines as shown in Figures 5 and 6. Figure 7 shows schematic 3D and top views of a substrate 700 at various intermediate stages of patterning, according to another embodiment of the present disclosure. As shown, a first trench 711 is imaged between two lines 713 in a patterned first layer 710 on an underlying layer 701 of the substrate 700, The first trench 711 is then coated with a graft material 721 having base functionality. It is noted that the graft material 721 is deposited non-selectively on all uncovered surfaces, including the sidewalls 711'', the bottom surface 711' of the first trench 711, and the top surface 713' of the lines 713. If necessary, a spacer release etch can be performed. This is a directional etch that removes the graft material 721 from the horizontal surfaces (i.e., the bottom surface 711' of the first trench 711 and the top surface 713' of the lines 713), leaving behind the sidewall (i.e., 711'') deposits in the first trench 711 (not shown). Subsequent actinic radiation, diffusion, and development process steps are similar to the corresponding steps in Figures 5 and 6, although the diffusion layer is not shown in Figure 7C. As a result, a second trench 741 is formed, which is separated from the first trench 711 by a region 743 of the line 713 .
[0047] 7M and 7N are top views of FIGS. 7C and 7D, respectively, according to one embodiment in which a "snap-away" structure is formed. In FIG. 7M, the arrows represent the diffusion process while the dashed areas represent the areas exposed to actinic radiation in FIG. 7C, and the latent pattern is represented by 733, which eventually becomes the second structure 741. In this embodiment, a graft material 721 with a base is used. In FIGS. 7M and 7N, a light exposure is shown that exhibits an overlay error, which causes the first and second trenches (i.e., 711 and 741) to merge. That is, the latent pattern 715 formed by actinic radiation exposure through the photomask 731 is in contact with the graft material 721 that covers the first trench 711. However, due to diffusion from the graft material 721 (i.e., 743), the area 743 between these trenches becomes insoluble, and after development, the two trenches are separated. Also, both the first trench 711 and the second trench 741 may be formed using PTDs.
[0048] 7P and 7Q are top views of structures similar to those of FIGS. 7C and 7D, respectively, according to another embodiment in which a "snap-to" structure is formed. Similarly, the arrows represent the diffusion process, while the dashed areas represent the areas exposed to actinic radiation in FIG. 7C, and the latent pattern is represented by 733, which will eventually become the second structure 741. In this embodiment, instead of a base, a graft material 721 with an acid is used. In FIG. 7P, it is shown that the latent pattern 733 does not contact the first trench 711. The acid diffuses out of the graft material 721, and the separated portion 743 of the photoresist becomes soluble. As a result, both trenches are in contact after development. That is, in this embodiment, the latent pattern 715 is separated from the first trench 711 by the dashed areas defined by the photomask 731. However, the acid from the graft material 721 diffuses a predetermined distance, effectively "opening up" the first trench 711, ensuring that the first trench 711 and the second trench 741 merge. Also, both the first trench 711 and the second trench 741 can be formed using PTD.
[0049] FIG. 8 shows a schematic 3D and top view of a substrate 800 at various intermediate stages of pattern formation according to another embodiment of the present disclosure. FIG. 8 shows a similar process to FIG. 7, but with an inverse photopattern, as shown by the inverse photomask 831. Thus, a PTD may be used to develop the first trench (711) and an NTD may be used to develop the second trench (741). The rest of the description has been provided previously and is omitted here for brevity. It should be noted that while FIG. 8 shows only an embodiment in which a "snap-to" structure is formed, a "snap-away" structure may also be formed using this inverse photopattern.
[0050] FIG. 9 illustrates an additional embodiment of forming narrow trenches using acid wash, which may be an embodiment of method 100 in FIG. 1. FIGS. 9A1-9F1 are top views of a substrate 900 at various intermediate stages of an example method, and FIGS. 9A-9F are corresponding cross-sectional views taken along section line A″a″-F″f″ in the z-direction. The acid wash flow is a three material process in which reactive species are driven into mandrels by immersing the substrate in a solution of reactive species to form self-assembled double patterns (SADPs).
[0051] As shown in Figures 9A and 9A1, a substrate 900 has a patterned first layer 910 on an underlayer 901. In this example, the patterned first layer 910 has lines 911 made of a first photoresist material. After forming the photoresist lines 911, in Figures 9B and 9B1, acid is deposited on the substrate 900. In Figures 9C and 9C1, a bake step is performed to activate the deprotection in the deprotected regions 931 by diffusing the acid into the lines 911. This dissolves a certain thickness of the lines (i.e., the deprotected regions 931) in a given developer. A solvent rinse step is then required to remove any remaining acid. Next, in Figures 9D and 9D1, a fill material 941, such as a second photoresist material, is deposited. The fill material 941 must be compatible with the first photoresist solvent system so that after depositing the fill material 941, for example by a common spin-coating process, the deprotected regions 931 and the lines 911 remain on the substrate 900. Also, in Figures 9E and 9E1, the fill material 941 is designed such that the overburden is removed. Then, as shown in Figures 9F and 9F1, the soluble material 931 is developed, leaving a narrow trench 961 between the lines 911 (first structure) and the remaining fill material 941 (second structure).
[0052] Figure 10 shows the formation of a pattern on a substrate according to the example process of Figure 9. Figure 10 shows how two patterns are formed on a substrate while maintaining sufficient distance between the structures. Figure 10 shows this embodiment in which an acid wash is used to ensure that the structures do not merge, however, a grafting material can also be used to prevent structures from merging due to overlay errors.
[0053] In this approach, the pattern is split into two masks and recombined in successive lithography and etching steps, with the width of the line or space being defined by the edges placed on the separate masks. The advantage of this technique is that the effect of errors is minimized through diffusion-based buffering and suitable resist. Decomposition of the layout for multiple exposure steps is a challenge in automated double patterning lithography (DPL) design flows. There is a challenge in identifying the optimal cut point on the polygon. Thus, this technique can overcome the challenges faced in layout decomposition or pattern stitching.
[0054] This method applies a trade-off between the overlay problem due to the resolution limit of the Rayleigh criterion in photolithography and sub-resolution trenches by acid diffusion to solve the post-layout degradation problem. By using acid diffusion spin-on material and bilayer patterning, the fiddle pattern overlap caused by proximity exposure can be prevented.
[0055] FIG. 10A is a top view of a substrate 1000 after patterning using the exemplary process of FIG. 9. As shown in the figure, an initial photoresist pattern L1 is printed on the substrate 1000 (L1 is represented by the area defined by the dashed line) to form a conflict-free layout (i.e., a layout in which sufficient distance is ensured between structures). The printed pattern L1 is then coated with an acid wash (e.g., FIG. 9B). After coating the acid wash over the initial photoresist pattern L1 and baking to activate the deprotection in the deprotected areas, a solvent rinse step is used to remove any remaining acid (e.g., FIG. 9C). As a result, the remaining photoresist pattern L1 forms lines 1010. The pattern L1 is then coated with a second layer of resist 1020 (also referred to as layer 2 or L2) (e.g., FIG. 9D). The L2 material needs to be compatible with the L1 photoresist solvent system. The L2 material is designed such that the overcoat regions are removed as L2 develop loss since there is no top coating on the L2 layer (i.e., the aforementioned top layer as shown in FIG. 9E). It is noted that factors in L2 design are the dissolution rate for both the ability to remove the overcoat regions of L2 during L2 development, and how much shrinkage occurs in the features during L2 development. This technique may be more successful with a height profile from bare loss without the top coating of L2, and consistency in the diffusion length of L1 (e.g., FIG. 9F). The development loss is measured as the difference in thickness before and after development of the L2 material. Advantageously, the development loss is designed to be equal to the diffusion loss due to the acid wash. The diffusion region defines a gap region with a sub-resolution trench (e.g., trench 961 in FIG. 9F), and the resolution is limited by the acid diffusion length of about 7 nm.
[0056] FIG. 10B is an enlarged view of the circle CirA in FIG. 10A, and FIG. 10C is a cross-sectional view along the cut line Gg in the z-direction. FIGS. 10B and 10C further show the gap region between the line 1010 (L1) and the line 1020 (L2). In particular, the width D of the gap region represents a certain diffusion length by the acid during the baking process. The introduction of an acid wash, in which a flow of the deprotection layer due to the pattern decomposition is formed, is a unique method to reduce the overlay error due to close proximity interactions. Thus, this objective helps to reduce the overlay error due to the resolution limit by the Rayleigh criterion. It can be used for sub-resolution trenches. The resolution is limited by the acid diffusion length of about 7 nm.
[0057] FIG. 11 is a flow chart of a method 1100 of forming a pattern on a substrate according to one embodiment of the present disclosure. The method 1100 begins at step S1101, where a patterned first layer is formed on an underlayer of a substrate. The patterned first layer has a first structure. At step S1102, a graft material is deposited on the substrate, where the graft material is selectively adhered to an uncoated surface of the first structure to obtain a predetermined thickness of the graft material on the sidewalls of the first structure. At step S1103, a second structure is formed on the substrate from photoresist abutting the graft material. The method 1100 then proceeds to step S110, where the graft material is removed and the first structure is spaced from the second structure by a distance corresponding to the predetermined thickness.
[0058] FIG. 12 shows schematic 3D and top views of a substrate 1200 at various intermediate stages of patterning according to an embodiment of the present disclosure. Although not shown in FIG. 12, a DCS process can be performed to harden the lines 1211 to prevent them from becoming soluble and form a film covering the lines 1211, as shown in FIG. 5. The process flow example of FIG. 12 is similar to the process flow example of FIG. 5, so the differences will be emphasized here. Here, the graft material 1221 does not necessarily include a solubility-shifting material. As a result, as shown in FIG. 12E, a second structure 1251 is formed in contact with the graft material 1221, with no gap between them. The graft material 1221 is then removed, leaving a gap 1261 between the two lines (i.e., 1221 and 1251) in FIG. 12F. 12 shows that even if the exposure pattern is misaligned and overlaps with graft material region 1221, the graft material 1221 is still ready to be removed to leave the desired gaps 1261 between the lines. Alternatively, graft material 1221 may have a solubility-shifting material, but no diffusion process is performed such that diffusion occurs. In other examples, graft material 1221 may have a solubility-shifting material, but the amount of solubility-shifting material is insufficient to change solubility, or a membrane formed during the DCS process may prevent diffusion of the solubility-shifting material.
[0059] Another embodiment is a selective coating flow. In a selective coating flow, the initial pattern (e.g., mandrels) can be a photoresist or hard mask material. In this initial pattern, a material is selectively attached to the mandrels relative to the floor material. This pattern is then overcoated with another material, either organic or inorganic based. The selective coating material is then removed, either via RIE etching or development, depending on the material matrix, to form the narrow trench feature.
[0060] A related flow is that of atomic layer deposition (ALD). ALD material is conformally deposited on a substrate. A spacer release etch removes the ALD material on all but the vertical surfaces, leaving sidewall spacers. This spacer material provides a buffer and inhibits structures from joining from different masks. After both structures are exposed and developed, the spacer material is carved out, such as by an etch process, leaving the desired gap between the specific structures.
[0061] Various embodiments in this application can benefit from various optimization techniques. For example, materials can be selected to have components (e.g., TGA and crosslinker) with different but non-overlapping decomposition temperatures. Solvent compatibility needs to be checked to place an overcoat without stripping the initial pattern (e.g., first photoresist and second photoresist). The initial pattern of photoresist is "frozen" or made insoluble using crosslinking to prevent dissolution of the mandrel in the subsequent developer (e.g., DCS).
[0062] The various embodiments described herein provide several advantages. For example, narrow trench or slot contacts can be formed between two structures by diffusion of a solubility-shifting material even when photomask misalignment occurs. The diffusion process can suppress overlay errors due to the Rayleigh criterion resolution limit, thus forming sub-resolution "snap-to" and "snap-away" structures.
[0063] In the above description, specific details have been described, such as the specific geometry of the processing system and various components and processes used therein. However, it should be understood that the technology of the present application may be practiced in other embodiments that deviate from these specific details, and such details are for the purpose of explanation and not limitation. The embodiments described in this application are described with reference to the accompanying drawings. Similarly, for the purpose of explanation, specific numbers, materials, and configurations are described for a thorough understanding. However, the embodiments may be practiced without such specific details. Components having substantially the same functional configuration are represented by similar reference numerals, and therefore any redundant description may be omitted.
[0064] Various techniques are described as multiple discrete operations to aid in understanding various embodiments. The order of description should not be construed to imply that these operations are order dependent. In fact, these operations need not be performed in the order described. The described operations may be performed in a different order than in the described embodiments. Various additional operations may be performed and / or described operations may be omitted in additional embodiments.
[0065] As used herein, "substrate" or "target substrate" generally refers to an object to be processed by the present invention. The substrate may include any material portion or structure of a device, particularly a semiconductor or other electronic device, and may be a base substrate structure, such as a semiconductor wafer, a reticle, or a layer on or overlying the base substrate structure, such as a thin film. Thus, substrate is not limited to any particular base structure, underlying or overlying layer, patterned or unpatterned, but rather is intended to include any such layer or base structure, and any combination of layers and / or base structures. Although the description refers to a particular type of substrate, this is for illustrative purposes only.
[0066] Moreover, those skilled in the art will appreciate that many variations may be made in the operation of the above-described techniques that achieve the same objectives of the present invention. Such variations are intended to be covered within the scope of the present disclosure. Accordingly, the above description of embodiments of the present invention is not intended to be limiting. Rather, any limitations to the embodiments of the present invention are presented in the following claims.
Claims
1. 1. A method for forming a pattern on a substrate, comprising the steps of: forming a first layer on an underlying layer of the substrate, the first layer being patterned to have a first structure; depositing a graft material on a side of the first structure, the graft material comprising a solubility-shifting material; diffusing the solubility-shifting material a predetermined distance into adjacent structures adjacent to the solubility-shifting material, the solubility-shifting material changing the solubility of the adjacent structures in a developer; removing soluble portions of the adjacent structures using the developer to form a second structure; having the first structure has a first opening in the first layer; the adjacent structure is part of the first layer; the first layer comprises a photoresist material; the second structure having a second opening in the first layer; forming a latent pattern of the second openings by patterned exposure of the first layer to actinic radiation prior to the step of diffusing the solubility-shifting material; the solubility-shifting material renders the adjacent structures insoluble to the developer; The first opening is spaced from the second opening by at least the predetermined distance.
2. The method of claim 1 , wherein the solubility-shifting material comprises a base that neutralizes an acid.
Citation Information
Patent Citations
Production of semiconductor device and semiconductor device
JP2000035672A
Pattern forming method, production of semiconductor device using same, and semiconductor device
JP2001033984A
Fine pattern forming method, fine pattern forming material and method for producing semiconductor device using the method
JP2002006512A
Method for forming fine pattern of semiconductor device by means of double patterning process utilizing acid diffusion
JP2009272623A
Pattern forming method
JP2010060693A