Electrochemical cell and method of manufacturing the same

The electrochemical cell design with a large resin film and integrated flat electrode terminals addresses sealing and thickness issues, ensuring reliable performance and manufacturing efficiency by preventing electrolyte leakage and short circuits.

JP7554932B2Active Publication Date: 2024-09-20SEIKO INSTR INC
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023531398
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-06-30
Filing Date
2022-03-07
Publication Date
2024-09-20
Estimated Expiration
2042-03-07

AI Technical Summary

Technical Problem

Existing electrochemical cells face challenges in achieving reliable sealing without increasing the risk of electrolyte leakage, moisture intrusion, and internal short circuits due to limitations in sealant film area and thermal effects during welding, as well as unnecessary thickness from stepped electrode terminals.

Method used

The electrochemical cell design incorporates a resin film that covers the entire bottom surface of the case, with a bent or curved lid plate to create a gap for electrolyte injection, and integrates electrode terminals into a flat structure to prevent thermal issues and reduce thickness.

Benefits of technology

This design ensures reliable sealing, prevents electrolyte leakage and moisture intrusion, reduces the risk of internal short circuits, and maintains a minimal cell thickness, enhancing the overall performance and manufacturing efficiency of the electrochemical cell.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007554932000005
    Figure 0007554932000005
  • Figure 0007554932000018
    Figure 0007554932000018
  • Figure 0007554932000021
    Figure 0007554932000021
Patent Text Reader

Abstract

An electrochemical cell according to the present invention is characterized by comprising an outer package which is provided with: a case that has a lateral part and bottom parts, one of the bottom parts being an opening, while the other one of the bottom parts being provided with a through hole; a cover plate that is welded to the opening so as to seal the opening; and an electrode plate which closes the through hole by the intermediary of a resin film that is fusion bonded to a peripheral part of the through hole.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to an electrochemical cell and a method for manufacturing the same. This application claims priority based on Japanese Patent Application No. 2021-108595, filed in Japan on June 30, 2021, the contents of which are incorporated herein by reference. [Background technology]

[0002] Electrochemical cells such as lithium ion secondary batteries and electrochemical capacitors have traditionally been widely used as power sources for small devices such as smartphones, wearable devices, and hearing aids. In this type of electrochemical cell, in order to increase the battery capacity and the charging and discharging currents, it is necessary to make the area of ​​the electrodes facing each other in the electrochemical cell as large as possible. Known electrochemical cell structures include a pair of strip-shaped positive and negative electrodes wound with a separator therebetween, or folded and housed in a case, with an electrolyte sealed in the case.

[0003] For example, Patent Document 1 listed below describes a battery (electrochemical cell) that includes an electrode body consisting of a positive electrode and a negative electrode, and an exterior body consisting of a first laminate member and a second laminate member, and has an outer periphery wall formed by bending the outer periphery of the first laminate member and the outer periphery of the second laminate member around the outer periphery of the exterior body. The exterior body is made of a layered laminate member of metal foil and a resin layer, and is sealed by folding the outer walls of the first and second laminate members together and heat fusing them, thereby providing a battery that can increase capacity per volume. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2018-085214 A Summary of the Invention [Problem to be solved by the invention]

[0005] Meanwhile, there is known a button-type electrochemical cell in which an electrode body having a laminated structure of positive and negative electrodes is enclosed in a metal case. Fig. 19 shows an exploded cross section of a button-type electrochemical cell 103 configured to house an electrode body 101 inside a cylindrical container-type metal case 100 and close the upper opening of the metal case 100 with a metallic cover plate 102. For example, as shown in Fig. 20, the electrochemical cell 103 is configured by welding the cover plate 102 to the periphery of the opening of the metal case 100 and providing an electrode plate 106 so as to close a through hole 105 formed in the center of the cover plate 102. In the case of the electrochemical cell 103 described above, it is necessary to attach the electrode plate 106 while taking into consideration the prevention of short circuits with the metal case 100, the prevention of leakage of the electrolyte contained inside the cell, the prevention of moisture intrusion, etc. For this reason, a ring-shaped sealant film 108 having a diameter larger than that of the electrode plate 106 is heat-sealed to the electrode plate 106, and the peripheral side of the sealant film 108 is heat-sealed to the upper surface of the cover plate 102, thereby forming an electrochemical cell 103 with ensured sealing properties. In order to improve the sealing performance, a sealant film 109 having the same shape as the sealant film 108 may be prepared separately and heat-sealed onto the electrode plate 106 and the sealant film 108 as shown in FIG.

[0006] 20, a recess 110 is formed in the center of the cover plate 102 so as to surround the periphery of a through-hole 105, and a sealant film 108 is heat-sealed to the bottom surface of the recess 110. When this structure is adopted, the area of ​​the sealant film 108 needs to be as large as possible in order to improve the reliability of the sealing structure for preventing leakage of the electrolyte, etc. However, since the size of the recess 110 formed in the cover plate 102 places a restriction on the size of the sealant film 108, there is a problem that it is not possible to increase the fusion area of ​​the sealant film 108. The same problem occurs when the sealant film 109 is added.

[0007] FIG. 21 is an exploded cross-sectional view showing an electrochemical cell 120 having a similar structure to the electrochemical cell 103 described above, and shows a structure in which a flat cover plate 121 is welded to a metal case 100 as shown in FIG. 22, since the cover plate 121 does not have a recess or the like, it is expected that the sealant film 108 can be made large. However, since the outer peripheral edge of the cover plate 121 is welded to the peripheral edge of the opening of the metal case 100, there is a high possibility that the heat during welding will act on the outer peripheral edge of the cover plate 121. Therefore, even if the sealant film 108 is made large, there is a possibility that the peripheral side of the sealant film 108 will re-melt due to the influence of the heat during welding, and there is a possibility that a poorly fused portion will occur.

[0008] Fig. 23 shows a structure in which an electrode terminal 122 is attached to the electrochemical cell 103 having the configuration shown in Fig. 20. In the electrochemical cell 103, the electrode plate 106 is provided on the inner side of the recess 110, so it is necessary to bend the base end 122A of the electrode terminal 122 into an L-shape to provide a step portion 122B before connecting it to the electrode plate 106. Also, in order to prevent a short circuit between the electrode terminal 122 and the cover plate 102, it is necessary to insert an insulating tape 123 between the electrode terminal 122 and the cover plate 102. This necessitates an additional step for attaching the insulating tape 123, which increases the number of manufacturing steps. In addition, if the step portion 122B of the electrode terminal 122 is made larger, the total thickness of the electrochemical cell 103 including the electrode terminal 122 becomes unnecessarily thick.

[0009] Fig. 24 shows a structure in which an electrode terminal 122 is attached to an electrochemical cell 120 having the configuration shown in Fig. 22. The electrode plate 106 is attached to the upper surface of a flat cover plate 121, and a base end 122A of the electrode terminal 122 is connected to the upper surface of this electrode plate. Although the tip side of the electrode plate 106 extends slightly above the electrode plate 106, it is necessary to provide an insulating tape 125 between the electrode plate 106 and the cover plate 121 to prevent a short circuit. For this reason, as in the previous example, a separate process of attaching insulating tape 125 is required, which increases the number of manufacturing steps. In the configuration shown in Fig. 24, although it is possible to make step portion 122B slightly smaller than in the structure shown in Fig. 23, insulating tape 125 is still required.

[0010] The present invention has been made in consideration of the background of the conventional technology described above, and aims to provide an electrochemical cell in which an electrode body is housed in a case, and a method for manufacturing the same, in which a highly reliable configuration can be applied to the structure of the part where the case and the electrode body are fused with a resin film. Another object of the present invention is to provide an electrochemical cell in which the electrode plates provided in the electrochemical cell have no stepped portions and the total thickness of the electrochemical cell is not unnecessarily increased, and a method for manufacturing the same. [Means for solving the problem]

[0011] (1) The electrochemical cell according to the present invention comprises an exterior body including a case having sides and a bottom, one of the bottoms being an opening and the other bottom having a through-hole, a cover plate welded to the opening to seal the opening, and an electrode plate that closes the through-hole via a resin film fused to the periphery of the through-hole. A bend correction portion or a curve correction portion is provided on a part of the cover plate. It is characterized by:

[0012] With the above-mentioned configuration, even if the resin film provided on the bottom of the case is made sufficiently large to correspond to the bottom of the case, there is no problem with the sealing of the fused resin film. This is because, when welding a cover plate to the opening of the case, the position where the cover plate is welded and the position of the peripheral edge of the resin film can be set at a position sufficiently separated from the side in the height direction of the side. The area of ​​the resin film can be increased so as to reach the outer periphery of the bottom, and the resin film is less susceptible to the thermal effects caused when the cover plate is welded, so that the fused resin film provides good sealing properties, prevents moisture intrusion, and is less susceptible to electrolyte leakage, making it possible to provide a highly reliable electrochemical cell. By providing a bent or curved portion in part of the cover plate, when the opening of the case is closed with the cover plate, a gap can be formed between the opening of the case and the cover plate, and this gap can be used to inject the electrolyte. Since the cover plate is welded to close the opening of the case, any cover plate having bent or curved portions is straightened into a flat plate after welding, resulting in a cover plate having a straightened bent or curved portion.

[0013] (2) In the electrochemical cell according to the present invention, a configuration can be adopted in which the case and the cover plate are made of metal, an electrode body is housed in the outer casing, and one of the positive electrode body and the negative electrode body constituting the electrode body is electrically connected to the case and the other is electrically connected to the electrode plate.

[0014] By connecting the positive and negative electrodes of the electrode body to a case or an electrode plate, one electrode of the electrochemical cell can be the case and the other electrode can be the electrode plate. Since a resin film having a large area and no sealing problems is interposed between the case and the electrode plate as described above, a highly reliable electrochemical cell can be provided that is less susceptible to problems such as an internal short circuit between the positive and negative electrodes. The positive or negative electrode of the electrode body can be connected to the electrode plate through a through hole provided in the resin film, thereby enabling connection between the positive or negative side of the electrode body and the electrode plate.

[0015] (3) In the electrochemical cell according to the present invention, a configuration can be employed in which the resin film is formed on almost the entire surface of the bottom portion except for the position of the through-hole.

[0016] Since a resin film that has a large area equivalent to almost the entire bottom surface and does not cause problems in sealing is interposed between the case and the electrode plate, a highly reliable electrochemical cell can be provided that is less susceptible to problems such as internal short circuits between the positive and negative electrodes.

[0017] (4) In the electrochemical cell according to the present invention, it is preferable that the electrode plates are formed so as to have substantially the same outer periphery as the resin film.

[0018] This structure makes it possible to provide an electrochemical cell with large area electrode plates.

[0019] (5) In the electrochemical cell according to the present invention, it is preferable that the electrode plate includes an electrode terminal protruding from an outer periphery of the bottom of the case.

[0020] The electrode terminals protruding from the bottom of the case can be formed in a flat plate shape without any steps, so that even if the cell is configured with electrode terminals, it is possible to provide an electrochemical cell whose total thickness is not increased more than necessary. By integrating the electrode portion and the electrode terminal into a flat plate shape, it is possible to provide an electrochemical cell whose total thickness is not increased more than necessary.

[0021] (6) In the electrochemical cell according to the present invention, it is preferable that a protective portion protruding outward from an outer circumferential edge of the resin film is formed on a portion of the outer circumferential edge of the resin film that contacts the base end of the electrode terminal.

[0022] The protective portion provided on the outer peripheral edge of the resin film protects the base ends of the electrode terminals from contacting the case, thereby making it possible to provide an electrochemical cell that is less susceptible to short circuits between the electrode terminals and the case.

[0025] ( 7 The method for producing an electrochemical cell according to the present invention comprises an exterior body having a case having sides and a bottom, one of the bottoms being an opening and a through-hole formed in the other bottom, a cover plate welded to the opening and sealing the opening, and an electrode plate closing the through-hole via a resin film fused to the peripheral portion of the through-hole, and when producing an electrochemical cell having an electrode body housed in the exterior body, the method comprises the steps of: housing the electrode body inside the case, covering the peripheral portion of the opening of the case with a cover plate having a bent or curved portion on at least a part of its outer periphery, injecting an electrolyte into the case by utilizing a gap generated at the peripheral portion of the opening of the case due to the presence of the bent or curved portion, and after the electrolyte has been injected, welding the peripheral portion of the opening of the case to the outer periphery of the cover plate.

[0026] A cover plate having a bent or curved portion at least in part of the outer periphery is placed on the periphery of the opening of the case, and the electrolyte can be poured into the case by utilizing a gap generated on the periphery of the opening of the case. When the cover plate is welded to the periphery of the opening of the case, this gap can be closed by welding it so as to be forcibly closed.

[0027] ( 8In the method for manufacturing an electrochemical cell according to the present invention, when welding the opening peripheral portion of the case and the outer peripheral portion of the cover plate, the outer peripheral portion of the cover plate is pressed against the opening peripheral portion of the case, and the outer peripheral portion of the cover plate is welded to the opening peripheral portion of the case along the pressed portion. The method can be adopted.

[0028] By pressing the cover plate against the opening of the case so as to close it, and welding the cover plate to the periphery of the opening of the case, the cover plate can be welded so that the opening of the case is completely closed by the cover plate, thereby creating a sealed case structure.

[0029] ( 9 ) In the method for manufacturing an electrochemical cell according to the present invention, it is preferable that either the positive electrode or the negative electrode formed on the electrode body is electrically connected to the cover plate, and the other of the positive electrode tab or the negative electrode tab is electrically connected to the electrode plate via the through hole.

[0030] One of the positive and negative electrodes of the electrode body is connected to the cover plate and the other to the electrode plate, completing a battery with one electrode on the cover plate and the other electrode on the electrode plate.

[0031] ( 10 ) In the method for producing an electrochemical cell according to the present invention, the electrode plate is characterized in that it has an electrode portion that closes the through hole of the resin film and covers the outer peripheral edge of the resin film, and an electrode terminal that protrudes outward from the electrode portion and protrudes outward beyond the outer peripheral edge of the resin film. 7 )~( 9 2. A method for producing an electrochemical cell according to claim 1 .

[0032] The electrode plate may have a structure in which the electrode portion and the electrode terminal are integrally formed. By forming the electrode portion and the electrode terminal as an integral structure and making the whole into a flat plate, an electrochemical cell having a total thickness that is not unnecessarily large can be provided.

[0033] ( 11) In the method for manufacturing an electrochemical cell according to the present invention, it is preferable to use a resin film in which a protective portion is formed on the outer periphery of the resin film, in a portion that contacts the base end of the electrode terminal, and protrudes outward from the outer periphery of the resin film.

[0034] The protective portion provided on the outer peripheral edge of the resin film protects the base ends of the electrode terminals from contacting the case, thereby making it possible to provide an electrochemical cell that is less susceptible to short circuits between the electrode terminals and the case. Effect of the Invention

[0035] In the electrochemical cell according to the present invention, even if the area of ​​the resin film provided on the bottom of the case is made sufficiently large corresponding to the area of ​​the bottom of the case, no problem occurs in the sealing property of the fused resin film. This is because, when a cover plate is welded to the opening of the case, the position where the cover plate is welded and the position of the peripheral edge of the resin film can be set at a position sufficiently separated from the side in the height direction of the side. The area of ​​the resin film can be increased so as to reach the outer periphery of the bottom or the outer periphery of the ceiling wall, and the resin film is less susceptible to the thermal effects when the cover plate is welded. This provides a highly reliable electrochemical cell that has good sealing properties, prevents moisture intrusion, and does not cause electrolyte leakage. [Brief description of the drawings]

[0036] [Figure 1] 1 is a cross-sectional view showing an electrochemical cell of a first embodiment according to the present invention. [Diagram 2] FIG. 4 is a cross-sectional view showing an electrochemical cell according to a second embodiment of the present invention. [Diagram 3] FIG. 4 is a cross-sectional view showing an electrochemical cell according to a third embodiment of the present invention. [Figure 4] FIG. 11 is a cross-sectional view showing an electrochemical cell according to a fourth embodiment of the present invention. [Diagram 5] FIG. 11 is a cross-sectional view showing an electrochemical cell according to a fifth embodiment of the present invention. [Figure 6]FIG. 6 is a plan view of the electrochemical cell shown in FIG. [Figure 7] FIG. 6 is a plan view showing a resin film applied to the electrochemical cell shown in FIG. [Figure 8] FIG. 11 is a cross-sectional view showing an electrochemical cell according to a sixth embodiment of the present invention. [Figure 9] FIG. 23 is a plan view showing an example of an electrode and a resin film applied to the electrochemical cell of the sixth embodiment. [Figure 10] FIG. 13 is a plan view showing a second example of a resin film applied to the electrochemical cell of the fifth embodiment. [Figure 11] FIG. 13 is a plan view showing a second example of a resin film and electrodes that are applied to the electrochemical cell of the fifth embodiment. [Figure 12] FIG. 13 is a partial cross-sectional view illustrating a state in which an electrode body is connected to a metal case and a lid body and housed in the metal case in an electrochemical cell of a seventh embodiment according to the present invention. [Figure 13] FIG. 13 is a plan view of the cover plate shown in FIG. [Figure 14] 13 is a cross-sectional view showing a state in which the electrode body is housed in the metal case from the state shown in FIG. 12 and a cover plate is temporarily fixed to the opening of the metal case. [Figure 15] 16 is a plan view showing a temporary fixing position of the electrode body shown in FIG. 15. [Figure 16] 15 is a partial cross-sectional view showing a state in which a roller of a welding machine is disposed to weld the metal case and the cover plate shown in FIG. 14 . FIG. [Figure 17] 17 is a plan view showing a state in which the welding member is rotated from the state shown in FIG. 16 to weld the cover plate to the metal case. FIG. [Figure 18] 13 is a perspective view showing a specific example of the electrode body shown in FIG. 12. [Figure 19] FIG. 1 is a cross-sectional view showing a state before a cover plate is welded to a metal case in an example of a conventional electrochemical cell. [Figure 20] FIG. 1 is a cross-sectional view showing a state in which a cover plate is welded to a metal case in an example of a conventional electrochemical cell. [Figure 21]FIG. 11 is a cross-sectional view showing a state before a cover plate is welded to a metal case in another example of a conventional electrochemical cell. [Figure 22] FIG. 11 is a cross-sectional view showing a state in which a cover plate is welded to a metal case in another example of a conventional electrochemical cell. [Diagram 23] FIG. 1 is a cross-sectional view showing a state in which an electrode terminal is attached to a cover plate having a recess in a conventional electrochemical cell. [Figure 24] FIG. 1 is a cross-sectional view showing a state in which an electrode terminal is attached to a flat cover plate in a conventional electrochemical cell. [Diagram 25] FIG. 13 is an explanatory diagram showing a case where an electrode assembly is housed in a metal case in a conventional electrochemical cell. [Figure 26] FIG. 1 is an exploded view showing an example of a cover plate applied to a conventional electrochemical cell. [Figure 27] FIG. 11 is a cross-sectional view showing a state in which an electrode assembly is housed in a metal case in another example of a conventional electrochemical cell and a cover plate is welded to the metal case. [Figure 28] FIG. 11 is a cross-sectional view showing a state in which an electrode assembly is housed in a metal case in another example of a conventional electrochemical cell and a cover plate is welded to the metal case. [Figure 29] FIG. 13 is an explanatory diagram showing a case where an electrolyte is filled in another example of a conventional electrochemical cell. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0037] Hereinafter, a first embodiment of an electrochemical cell according to the present invention will be described with reference to the drawings. In the embodiment described below, a button-type secondary battery (hereinafter, simply referred to as a "battery") is given as an example of an electrochemical cell, and the battery will be described. Note that in the drawings used in the following description, the scale of each component may be appropriately changed in order to make each component recognizable.

[0038] First Embodiment 1 is a cross-sectional view for explaining a first embodiment of an electrochemical cell according to the present invention, and the electrochemical cell (battery) 1 of the first embodiment is a button battery having a circular shape in a plan view. The battery 1 includes an electrode assembly 3 housed inside an exterior body 2 made of a metal can. Although not shown in Fig. 1, an electrolyte is filled inside the exterior body 2. As the electrolyte, an electrolyte in which a supporting salt is dissolved in a non-aqueous solvent is preferably used.

[0039] The exterior body 2 consists of an open-top metal case 2A having a bottom (bottom wall) 2a and a side (side wall) 2b, and a metal cover plate 2B fixed to the periphery of the opening by a joining method such as welding so as to close the top opening of the case 2A. The case 2A is made of a stainless steel plate with excellent corrosion resistance, such as SUS316, and functions as one electrode of the battery 1. A through hole 2d having an inner diameter approximately a fraction of the outer diameter of the bottom 2a is formed in the center of the bottom 2a of the case 2A, and a metal electrode plate 6 is attached to the underside of the bottom 2a via a ring-shaped resin film (sealant film) 5. A through hole 5a having the same inner diameter as the through hole 2d of the bottom 2a is formed in the center of the resin film 5, and the resin film 5 is fused to the lower surface of the bottom 2a with the through hole 5a aligned with the through hole 2d. The outer diameter of the resin film 5 is formed to be almost the same as the outer diameter of the bottom 2a. Therefore, the resin film 5 is fused to the bottom 2a so as to cover almost the entire lower surface except for the through hole 2d of the bottom 2a. In addition, the outer peripheral edge of the resin film 5 reaches the outer peripheral portion of the bottom 2a and covers the outer peripheral portion of the side portion 2a. In other words, almost the entire bottom surface of the exterior body 2 is covered by the resin film 5.

[0040] The electrode plate 6 is made of a metal disk, and its outer diameter is formed to be the same as that of the resin film 5. Therefore, the electrode plate 6 is provided so as to cover the entire lower surface of the resin film 5, including the through-hole 5a of the resin film 5. The electrode plate 6 is made of a stainless steel plate having excellent corrosion resistance, such as SUS316, and functions as the other electrode of the battery 1.

[0041] The resin film (sealant film) 5 is made of a material that can be attached to the metallic bottom 2a and the electrode plate 6 by fusion, which will be described later. The resin film 5 has a base layer made of a sheet or nonwoven fabric made of a high melting point resin such as PET (polyethylene terephthalate), PPS (polyphenylene sulfide), nylon, or polyethylene naphthalate (PEN). The resin film 5 can have a three-layer structure with fusion layers made of low melting point resins such as simple substances or copolymers of thermoplastic resins such as modified PP (polypropylene) and PE (polyethylene) provided on both sides of the base layer. The high melting point resin referred to here means a resin having a melting point higher than the general heat fusion temperature (150 to 200°C), and the low melting point resin is preferably a resin having a melting point lower than the high melting point resin, in other words, a resin having a melting point lower than the general heat fusion temperature. Also, the resin film 5 may have a single layer structure made of a heat fusion-compatible resin. The resin film 5 may be fused by other fusion means (welding means) such as ultrasonic welding, laser welding, and high frequency welding, in addition to heat fusion.

[0042] The electrode body 3 has, for example, a structure in which a negative electrode body and a positive electrode body are laminated, with a positive electrode tab extending from one side and a negative electrode tab extending from the other side. Although omitted in Fig. 1, the positive electrode tab of the electrode body 3 is electrically connected to the cover plate 2B or the case 2A, the negative electrode tab of the electrode body 3 is electrically connected to the electrode plate 6, and the inside of the exterior body 2 is filled with an electrolyte to form the battery 1.

[0043] To manufacture the battery 1 shown in Fig. 1, the resin film 5 and electrode plate 6 are aligned and attached to the lower surface side of the bottom of the case 2A, heated to a temperature at which heat fusion is possible for the required time, and then cooled to room temperature. In this state, the resin film 5 and electrode plate 6 are fused to the bottom side of the case 2A, covering the lower surface side of the bottom, but the top side of the case 2A is open because the cover plate 2B is not welded, and the electrode body 3 is not housed therein.

[0044] The negative electrode tab of the electrode body 3 is connected to the electrode plate 6 by a joining method such as welding, and the positive electrode tab of the electrode body 3 is connected to the cover plate 2B by a joining method such as welding, and the electrode body 3 is housed inside the case 2A. After the electrode body 3 is housed in the case 2A with some leeway in the length of the negative electrode tab and the positive electrode tab, an electrolyte is poured in from the opening on the top side of the case 2A. After the electrolyte is poured in, the opening of case 2A is closed with cover plate 2B, and the outer peripheral edge of cover plate 2B is welded around the entire circumference while applying pressure with a welding machine from the direction indicated by the downward arrow in Fig. 1, thereby obtaining battery 1 having the structure shown in Fig. 1. The welding method that can be used may be resistance welding, laser welding, or the like.

[0045] When manufacturing the battery 1 shown in FIG. 1, the outer peripheral edge of the cover plate 2B is joined by a welding method such as resistance welding. However, since the welding position and the outer peripheral edge of the resin film 5 are separated by the side portion 2b, there is no problem such as the heat-sealed portion of the resin film 5 peeling off due to the heat during welding. Therefore, in the configuration shown in FIG. 1, a resin film 5 with a large area that covers the entire lower surface of the bottom portion 2a can be used, and the resin film 5 can be used to fusion-bond the electrode plate 6 to the bottom portion 2a with good sealing properties.

[0046] In contrast, in the electrochemical cell 120 of the conventional structure shown in FIG. 22, if the sealant film 108 is made large, the periphery of the sealant film 108 comes close to the welded portion, so there is a problem that the sealant film 108 cannot be made large. 1, the structure in which the electrode plate 6 is attached by the resin film 5 is highly reliable, and a structure with excellent sealing properties can be provided by the resin film 5. Therefore, in the battery 1, the intrusion of moisture and leakage of electrolyte through the attached portion of the resin film 5 can be prevented, and a highly reliable structure can be provided.

[0047] In the structure of Fig. 1, an upper opening type case 2A having a bottom 2a and a side 2b is used, but a battery may be constructed by turning the structure of Fig. 1 upside down and using a lower opening type case having sides and a ceiling (bottom), with the lower opening closed by a cover plate. In that case, a resin film 5 and an electrode plate 6 are attached to the upper surface of the ceiling wall.

[0048] <Second embodiment> 2 shows a battery (electrochemical cell) 10 of a second embodiment, which uses a bottom-opening metal case 12A having sides 12b and a ceiling wall (bottom) 12a, with the bottom opening of the case 12A closed with a cover plate 12B. An electrode plate 16 is fused to the upper surface of the ceiling wall 12a via a resin film 15. A through hole 15a is formed in the resin film 15. The battery 10 shown in Fig. 2 has a configuration in which the battery 1 shown in Fig. 1 has been turned upside down, and a flat cover plate 12B is welded to close the bottom opening of the case 12A. The outer peripheral edge of the cover plate 12 is welded to the periphery of the bottom opening of the case 12A, closing the bottom opening of the case 12A. The configuration shown in Figure 2 is the same as the configuration in Figure 1 except that the relationship between case 2A and cover plate 2B shown in Figure 1 is inverted upside down, and resin film 15 and electrode plate 16 are fused to ceiling wall 12a.

[0049] The battery 10 of the second embodiment shown in FIG. 2 can also obtain the same effects as the battery 1 of the first embodiment shown in FIG. 1, such as the ability to increase the area of ​​the resin film 15 and the excellent sealing properties of the resin film 15.

[0050] To manufacture the battery 10, for example, the electrode body 3 is placed inside the case 12A before the resin film 15 and the electrode plate 16 are attached, the positive electrode tab of the electrode body 3 is welded to the cover plate 12B, and then the cover plate 12B is welded to the opening on the underside of the case 12A. After this, electrolyte is filled through the through hole 12d in the ceiling wall 12a, and then the negative electrode tab of the electrode body 3 is welded to the electrode plate 16. Then, the resin film 15 and the electrode plate 16 are fused to the outer surface (upper surface) of the ceiling wall 12a to produce the battery 10.

[0051] <Third embodiment> FIG. 3 shows the configuration of a third embodiment in which an electrode terminal 20 is attached to the battery 1 having the configuration shown in FIG. 1, and includes a flat electrode terminal 20 extending from the center of the bottom surface of the electrode plate 6 to the outside of the electrode plate 6. Since the electrode plate 6 is flat and the electrode terminal 20 is also flat, the structure shown in FIG. 3 makes it possible to provide a battery 1 with electrode terminals without making the total thickness of the battery 1 unnecessarily large. 3, there is no risk of electrode terminal 20 touching case 2A, and therefore no risk of an internal short circuit. That is, because resin film 5 is large enough to cover the entire lower surface of bottom 2a, there is no risk of electrode plate 6 touching bottom 2a or side 2b, and there is also no risk of electrode terminal 20 touching bottom 2a or side 2b, so that an internal short circuit can be prevented. In the conventional structure previously described with reference to Figures 23 and 24, insulating tape 123, 125 was required to prevent a short circuit between electrode terminal 122 and cover plate 102 or cover plate 121, but insulating tape is not required in the structure shown in Figure 3. In addition, because electrode terminal 20 is flat and has no steps, the total thickness of battery 1 is not unnecessarily increased.

[0052] <Fourth embodiment> FIG. 4 shows the configuration of a fourth embodiment in which an electrode terminal 20 is attached to a battery (electrochemical cell) 25 having a configuration similar to the battery 1 shown in FIG. 1, and the flat electrode terminal 20 is attached so as to extend from the center of the bottom surface of the electrode plate 26 outward from the electrode plate 26. A battery 25 shown in FIG. 4 differs from battery 1 in the size of electrode plate 26, but the other configurations are the same. In battery 25, electrode plate 26 is formed in a disk shape that is slightly smaller than resin film 5. Battery 25 has a configuration in which resin film 5 is larger than electrode plate 26, but does not require insulating tapes 123, 125 that were necessary in the conventional structure shown in Figures 23 and 24. 4, resin film 5 covers the outer periphery of bottom 2a, preventing short-circuiting between electrode terminal 20 and case 2A. Other effects are similar to those of battery 1 shown in FIG.

[0053] <Fifth embodiment> FIG. 5 shows the configuration of a fifth embodiment in which an electrode plate 31 is provided for a battery (electrochemical cell) 30 having a similar configuration to the battery 1 shown in FIG. In battery 30, the exterior body 2 is composed of a case 2A and a cover plate 2B, and the structure in which the electrode body 3 is housed inside the exterior body 2 is the same as that of battery 1. In addition, the structure in which a resin film 5 is fused to the lower surface (outer surface) of the bottom 2a of case 2A is also the same as that of battery 1.

[0054] The fifth embodiment is characterized in that a flat electrode plate 31 is provided, which has a disk-shaped electrode portion 31A shown in FIG. 6 having the same outer diameter as the outer diameter of the resin film 5, and a strip-shaped electrode terminal 31B extending outward from a portion of the outer peripheral edge of the electrode portion 31A. In the electrode plate 31, the electrode portion 31A is fused to the ring-shaped resin film 5, the planar shape of which is shown in Fig. 7, with their centers aligned with each other. The electrode portion 31A covers almost the entire lower surface of the resin film 5, including the through hole 5a in the resin film 5, and the outer peripheral edge of the resin film 5.

[0055] Since the electrode plate 31 is provided with the electrode terminal 31B, it is not necessary to connect a separate electrode terminal 20 to the outer surface of the electrode plate 6 as in the structure shown in FIGS. 5, the flat electrode plate 31 also serves as a terminal, so the total thickness of the battery 30 is not increased, and there is no need to connect a separate terminal. This simplifies the structure and the manufacturing process. Other effects are the same as those of the battery 1 shown in FIG. 3.

[0056] Sixth embodiment FIG. 8 shows the configuration of a sixth embodiment in which an electrode plate 36 is provided on a battery (electrochemical cell) 35 having a similar configuration to the battery 1 shown in FIG. In battery 35, the structure is equivalent in that exterior body 2 is composed of case 2A and cover plate 2B, and electrode body 3 is housed inside exterior body 2. Also, the structure in which resin film 5 is fused to the lower surface (outer surface) of bottom 2a of case 2A is also equivalent.

[0057] The structure of the sixth embodiment is characterized in that a flat electrode plate 36 is provided, which has a disk-shaped electrode portion 36A shown in Fig. 9 with an outer diameter slightly smaller than that of the resin film 5, and a rectangular electrode terminal 36B extending outward from a part of the outer periphery of the electrode portion 36A. In the electrode plate 36, the electrode portion 36A is fused to the resin film 5, the planar shape of which is shown in Fig. 9, with their centers aligned with each other.

[0058] Since the electrode plate 36 is provided with the electrode terminal 36B, it is not necessary to separately connect the electrode terminal 20 to the outer surface of the electrode plate 6 as in the structure shown in FIGS. With the configuration shown in Fig. 8, the flat electrode plate 36 also serves as a terminal, so the total thickness of the battery 35 does not increase, and there is no need to connect a separate terminal. This simplifies the structure and the manufacturing process. Other effects are the same as those of the battery 1 shown in Fig. 3.

[0059] Fig. 10 shows a second example of a resin film applicable to the structure of the fifth embodiment (see Figs. 5 and 6). The resin film 50 of this example has a disk-shaped covering portion 50A having the same outer diameter as the previous resin film 5, and a protective portion 50B having a rectangular shape in a plan view and protruding outward from a part of the outer periphery of the covering portion 50A. The length of the protective portion 50B is shorter than that of the electrode terminal 36B of the fifth embodiment, and the width of the protective portion 50B is slightly wider than that of the electrode terminal 36B of the fifth embodiment.

[0060] FIG. 11 shows the state in which the electrode portion 31A of the fifth embodiment is aligned with the center of the electrode portion 31A on the outer surface of the covering portion 50A of the resin film 50, and the electrode terminal 31B of the fifth embodiment is aligned with the protective portion 50B of the resin film 50 and then fused. As shown in FIG. 11, a protective portion 50B is disposed on the rear surface side of the base end of the electrode terminal 31B, so that it is possible to provide a configuration in which there is no risk of the electrode terminal 31B coming into contact with the metal case 2A. Therefore, by adopting the configuration shown in FIG. 11, it is possible to realize a configuration in which there is no risk of short-circuiting the electrode terminal 31B to the case 2A.

[0061] <Issues when manufacturing batteries> In the above embodiments, various configurations have been described in which the electrode plate is fused to the cover plate of the exterior body by fusing a resin film. However, when manufacturing a battery using a resin film fusing technique, there are problems as described below. 25 to 29 are diagrams illustrating problems that may arise when manufacturing a battery. 25 shows a state in which a negative electrode tab 131A of an electrode body 131 is connected to a shallow-bottom metal case 130 having a bottom 130A and a side 130B, and a positive electrode tab 131B of the electrode body 131 is connected to an electrode plate 132 fused to a cover plate 131C. In FIG. 25, resin films 133, 134 (see FIG. 26) are arranged on both the top and bottom surfaces of the electrode plate 132, the peripheral sides of the resin films 133, 134 are fused to each other, and the outer periphery of the resin film 134 is fused to the back side of the cover plate 131C. The resin film 134 is made large enough not to get in the way of the welded parts.

[0062] To manufacture a battery, it is necessary to insert electrode body 131 from the state shown in FIG. 25 into case 130 as shown in FIG. 27, inject electrolyte, and weld cover plate 131C. Specifically, after the product is brought into the state shown in FIG. 27, it is necessary to transport it to a vacuum drying device in a drying process, and after it is sufficiently dried, to inject an electrolyte and to weld a cover plate 131C. However, since the negative electrode tab 131A and the positive electrode tab 131B of the electrode body 131 are usually configured by applying an active material or the like to a thin metal foil, the strength of the tabs is weak and there is a risk of the tabs breaking during transportation in the drying process. Note that if the metal foil is replaced with a thicker one, the amount of active material decreases, which causes a problem of a decrease in the capacity of the battery, and therefore the metal foil cannot be replaced with one thicker than before.

[0063] If the cover plate 131C is temporarily fixed to the opening of the case 130 by temporary welding or the like from the state shown in FIG. 27 to that shown in FIG. 28, it is possible to prevent the tab from breaking during transportation. However, when the temporary fastening is performed, a problem occurs when injecting electrolyte 140 using an injector 138 such as a dropper, as shown in Fig. 29. That is, it is necessary to release the temporary fastening once and remove cover plate 131C from the opening of case 130, but performing this operation increases the risk of the tab breaking. After the temporary fastening is released, it is necessary to perform welding along the entire periphery of the cover plate 131C as shown in FIG. 29, and to permanently fasten the cover plate 131C to the opening on the top side of the case 130. In the prior art, it was necessary to solve the above-mentioned problems and then implement a problem-free manufacturing method, but no structure that would not cause tab breakage had been provided. In the seventh embodiment described below, it is possible to provide a manufacturing method capable of solving the above-mentioned problems and a structure corresponding to the manufacturing method.

[0064] Seventh embodiment FIG. 12 is an exploded partial cross-sectional view illustrating a suitable state for manufacturing a seventh embodiment of a battery (electrochemical cell) 60 having a similar configuration to the battery 1 shown in FIG. 1, and the battery 60 shown in FIG. 17 is obtained through the steps described below. A battery 60 of the seventh embodiment has an exterior body 2 formed by a case 2A and a cover plate 2B, and has a structure in which an electrode body 3 is housed inside the exterior body 2, which is equivalent to the structure of the battery 1 shown in Fig. 1. Furthermore, with respect to a structure in which an electrode plate 6 is fused to the outer surface (lower surface) of the bottom part 2a via a resin film 5, the battery 60 has a structure equivalent to that of the battery 1 shown in Fig. 1. The battery 60 of the seventh embodiment differs from the battery 1 shown in FIG. 1 in that it has a bent portion 2e (described later) formed in the cover plate 2B, and then the bent portion 2e is straightened during welding to return it to a flat plate shape.

[0065] The steps for manufacturing the battery 60 will be described below in order starting from FIG. As shown in Fig. 12, an electrode plate 6 is fused to a case 2A with an open top by a resin film 5. The electrode body 3 and cover plate 2B are sequentially arranged above the case 2A, and the positive electrode tab 3A of the electrode body 3 is joined to the center of the cover plate 2B, and the negative electrode tab 3B is joined to the center of the electrode plate 6 by a joining method such as ultrasonic welding. In the state shown in Fig. 12, the positive electrode of the electrode body 3 is electrically connected to the cover plate 2B by the above-mentioned tab connection, and the negative electrode of the electrode body 3 is electrically connected to the electrode plate 6 by the above-mentioned tab connection. In the structure shown in Fig. 12, a cover plate 2B having a bent portion 2e formed at a position shown by a dashed line in Fig. 13 is used. As shown in Figs. 12 and 13, the bent portion 2e is parallel to the center line S of the cover plate 2B which is circular in plan view, and is formed parallel to the center line S at a position toward the right side of the center of the cover plate 2B. As shown in Fig. 12, the cover plate 2B in this example has a structure in which the right side of the bent portion 2e is bent obliquely upward at a slight inclination angle (inclination angle α ≒ 10° in Fig. 12) relative to the left side of the bent portion 2e.

[0066] Fig. 14 shows a state in which the positive electrode tab 3A and the negative electrode tab 3B are folded from the state shown in Fig. 12 to accommodate the electrode body 3 in the case 2A. The positions (two positions on the outer periphery of the cover plate 2B) indicated by the arrows in Fig. 15, which is a plan view of the state shown in Fig. 14, are temporarily fixed by welding. The temporary fixing positions are the flat portion to the left of the bent portion 2e of the cover plate 2B shown in Fig. 15. 14, the tip 2f of the cover plate 2B is warped and slightly raised from the top opening 2i of the case 2A, creating a gap d between the top opening 2i of the case 2A and the tip 2f of the cover plate 2B. Using this gap d, electrolyte can be injected into the inside of the case 2A using an injector such as a dropper or syringe. By providing the bent portion 2e on the cover plate 2B, the gap d can be formed as described above, and the electrolyte can be poured in by utilizing this gap d. The bent portion 2e may be a curved portion whose curvature gradually changes.

[0067] As described above, even if the case 2A is transported with the cover plate 2B temporarily fixed, no load is applied to the positive electrode tab 3A and the negative electrode tab 3B, so the case 2A housing the electrode assembly 3 can be transported safely. For example, when transporting to a drying area, or from the drying area to an electrolyte injection area, or when handling in these areas, the case 2A can be transported without breaking the tabs.

[0068] Once the electrolyte injection operation is completed, as shown in Figures 16 and 17, pressure rollers 61, 61 of a welding machine are pressed against the top of the cover plate 2B, and the pressure rollers 61, 61 are rotated in the circumferential direction of the cover plate 2B while resistance welding the top opening of the case 2A to the outer circumferential edge of the cover plate 2B, thereby integrating the case 2A and the cover plate 2B to form the exterior body 2 and the battery 60. When the entire circumference of the cover plate 2B is welded to the top opening of the case 2A using the pressure rollers 61, 61, the cover plate 2B having the bent portion 2e is pressed against the top opening by the pressure rollers 61, and is welded while being straightened into a flat plate shape along the pressed portion. As a result, a straightened bend portion 2g is formed in the part of the flat cover plate 2B that corresponds to the bent portion 2e.

[0069] The bend straightened portion 2g means a portion that is straightened to a flat plate shape with traces of plastic processing when the cover plate 2B, which is a metal plate, is forcibly plastically processed into a flat plate shape after forming the one-end bend portion 2e in the cover plate 2B, which is a metal plate. Note that when a curved portion is formed instead of the bend portion 2e, the curve straightened portion is generated as a portion that is straightened to a flat plate shape with traces of plastic processing.

[0070] In addition, when welding the cover plate 2B, in order to apply laser welding, the cover plate 2B may be flattened by suppressing warping with a sufficiently transparent member such as a glass plate, and then the laser may be irradiated to weld the cover plate 2B. Alternatively, the cover plate 2B may be temporarily fixed by laser welding at several points, the warping may be corrected to form a flat plate, and the laser welding may be performed in this state.

[0071] When battery 60 is manufactured using the method described above, the joining of the positive electrode tab 3A and the negative electrode tab 3B to the case 2A and the cover plate 2B, the accommodation of the electrode body 3 in the case 2A, the injection of the electrolyte into the case 2A, and the welding of the cover plate 2B to the case 2A can be carried out smoothly and reliably. Therefore, the battery 60 can be manufactured without carrying out complicated steps or laborious operations.

[0072] For example, the positive electrode tab 3A and the negative electrode tab 3B provided on the electrode assembly 3 are generally configured by applying an active material to a thin metal foil film, and there is a risk that the tabs will break if excessive bending or tensile force is applied to the metal foil during the battery manufacturing stage. In this regard, there is little risk of a load being applied to each tab 3A, 3B during the stage of housing the electrode assembly 3 in the case 2A while bending the positive electrode tab 3A and the negative electrode tab 3B from the state shown in Fig. 12, so the problem of tab breakage during manufacturing is unlikely to occur.

[0073] Here, if one were to manufacture a battery using a flat cover plate 2B that does not have a bent portion 2e, in order to inject electrolyte into the case 2A, it would be necessary to hold the cover plate 2B at an angle so as to leave a gap at the top opening of the case 2A. Button batteries can have an outer diameter of only a few mm, and supporting the cover plate 2B at an angle can be a complicated task, and there is also a risk of damaging the positive electrode tab 3A when injecting electrolyte with a syringe. In view of this background, the procedure described above makes it possible to manufacture battery 60 without performing complex or laborious steps and without causing tab breakage.

[0074] In the batteries 1, 10, 25, 30, 35, and 60 of the first to seventh embodiments described above, a detailed description of the configuration of the electrode assembly 3 has been omitted, but the electrode assembly can employ a configuration such as that described below, as an example.

[0075] <Examples of electrode bodies> FIG. 18 is a perspective view showing one embodiment of the electrode assembly 3. This electrode assembly 65 is composed of a negative electrode assembly 67 covered with a negative electrode side separator layer 66 and a positive electrode assembly 69 covered with a positive electrode side separator layer 68. The electrode body 65 is an electrode body in which the negative electrode body 67 and the positive electrode body 69 are wound so as to be alternately stacked. Specifically, the electrode body 65 is formed by overlapping the negative electrode body 67 and the positive electrode body 69 with the negative electrode side separator layer 66 interposed therebetween and winding them in a flat shape. The negative electrode body 67 is provided with a negative electrode tab 70, and the positive electrode body 69 is provided with a positive electrode tab 71. For example, the negative electrode tab 70 is connected to the above-mentioned electrode plate 6, and the positive electrode tab 71 is connected to the above-mentioned cover plate 2B. It should be noted that the wound structure of the electrode body 65 is merely one example, and other structures such as a zigzag structure may also be adopted.

[0076] The negative electrode side separator layer 66 is formed so as to cover the entire negative electrode body 67 except for the negative electrode tab 70 and its surrounding portion on its base end side. The positive electrode side separator layer 68 is formed so as to cover the entire positive electrode body 69 except for the positive electrode tab 71 and its surrounding portion on its base end side. Therefore, the separator layers 66, 68 are disposed around and between the negative electrode body 67 and the positive electrode body 69 when the negative electrode body 67 and the positive electrode body 69 are wound, so that the negative electrode body 67 and the positive electrode body 69 are insulated and separated from each other.

[0077] In addition, in FIG. 18 , only the positions of the separator layers 66, 68 are shown, ignoring the layer thicknesses. However, the separator layers 66, 68 are arranged so as to be interposed between the negative electrode body 67 and the positive electrode body 69 at least in the entire region where the negative electrode body 67 and the positive electrode body 69 face each other, and so that the negative electrode side separator layer 66 covers the negative electrode body 67 and the positive electrode side separator layer 68 covers the positive electrode body 69. The direction in which the negative electrode body 67 and the positive electrode body 69 are wound and stacked can be referred to as the stacking direction. Note that "winding" refers to winding around a specific winding center axis.

[0078] The negative electrode body 67 is a sheet-like member including a foil-shaped negative electrode collector made of a metal material and a negative electrode active material layer coated on one or both sides of the negative electrode collector. The negative electrode collector is made of a metal foil such as copper or nickel. The thickness of the metal foil is, for example, about several μm. The negative electrode active material is, for example, a single substance or a mixture of silicon, silicon oxide, graphite, hard carbon, lithium titanate, etc. The negative electrode collector is composed of a plurality of circular negative electrode bodies and a band-shaped connection portion that connects the adjacent negative electrode bodies, and a negative electrode tab extends from the outer periphery of the negative electrode collector at one end in the arrangement direction.

[0079] As a material for forming the negative electrode active material layer, in addition to the negative electrode active material, a conductive assistant (e.g., acetylene black, etc.), a binder (e.g., a dispersion of polyvinylidene fluoride or styrene butadiene rubber (SBR), etc.), a thickener (e.g., carboxymethyl cellulose (CMC), etc.), and a solvent (e.g., any solvent such as water or N-methylpyrrolidone) can be mixed to prepare a negative electrode slurry. A coating liquid containing the constituent materials for forming the negative electrode active material layer can be called a "negative electrode slurry". The negative electrode active material layer can be formed by applying this negative electrode slurry to the negative electrode side current collector and drying it.

[0080] The positive electrode body 69 is a sheet-like member including a foil-like positive electrode collector made of a metal material and a positive electrode active material layer applied to one or both sides of the positive electrode collector. The positive electrode collector is made of a metal foil such as aluminum or stainless steel. The thickness of the metal foil is, for example, about 10 and a few μm. When the battery 1 is a lithium battery, the positive electrode active material is, for example, a composite oxide containing lithium and a transition metal, such as lithium cobalt oxide, lithium titanate, lithium manganese oxide, etc. The positive electrode current collector is composed of a plurality of circular positive electrode bodies and a band-shaped connection portion connecting adjacent positive electrode bodies, and a positive electrode tab extends from the outer periphery of the positive electrode current collector at one end in the arrangement direction.

[0081] As a material for forming the positive electrode active material layer, in addition to the above-mentioned positive electrode active material, a conductive assistant (e.g., acetylene black, etc.), a binder (e.g., polyvinylidene fluoride, etc.), and a solvent (e.g., any solvent such as N-methylpyrrolidone) can be mixed to prepare a positive electrode slurry. A coating liquid containing the constituent materials for forming the positive electrode active material layer can be called a "positive electrode slurry." The positive electrode slurry can be applied to a positive electrode side current collector and dried to form a positive electrode active material layer.

[0082] The separator layers 66, 68 are, for example, resin layers having lithium ion conductivity. The separator layers 66, 68 are formed of, for example, a polyolefin resin porous film, a glass nonwoven fabric, a resin nonwoven fabric, a laminate of cellulose fibers, or the like. Note that the separator layers 66, 68 only need to separate the positive electrode body 69 and the negative electrode body 67, so that either one of them may be omitted.

[0083] 18, the electrode body 65 of this embodiment is formed in a shape corresponding to the shape of the sealed space inside the exterior body so that it is arranged at high density inside the exterior body 2. That is, the electrode body 65 is formed in a circular shape when viewed from the stacking direction. The negative electrode body 67 has a configuration in which a plurality of circular negative electrode bodies 67a are connected via a connection part so as to be arranged in a shape such as a strip, and the positive electrode body 69 can have a configuration in which a plurality of circular positive electrode bodies 69a are connected via a connection part so as to be arranged in a shape such as a strip. Therefore, the electrode body 65 shown in FIG. 18 is formed by alternately stacking or winding the circular negative electrode current collector of the negative electrode body 67 and the circular positive electrode current collector of the positive electrode body 69. Note that, by fastening the end 66a of the separator layer 66 at a position on the upper surface side of the electrode body 65 that is inside the end of the negative electrode body 67a, it becomes easy to fold back the negative electrode tab 70. An electrode assembly 65 shown in FIG. 18 can be applied as the electrode assembly 3 in the first to seventh embodiments. [Explanation of symbols]

[0084] 1 ... battery (electrochemical cell), 2 ... exterior body, 2A ... case, 2a ... bottom, 2B ... cover plate, 2b ... side, 2d ... through hole, 2e ... bent portion, 2f ... tip portion, 2g ... bend correction portion, d ... gap, 3 ... electrode body, 5, 15 ... resin film (sealant film), 5a, 15a...through hole, 6, 16...electrode plate, 10...battery (electrochemical cell), 12...outer body, 12A...case, 12a...ceiling wall, 12B...cover plate, 12b...side portion, 12d...through hole, 20...electrode plate, 25...battery (electrochemical cell), 26...electrode plate, 30...battery (electrochemical cell), 31...electrode plate, 31A...electrode portion, 31B...electrode terminal, 35...battery (electrochemical cell), 36...electrode plate, 36A...electrode portion, 36B...electrode terminal, 50...resin film (sealant film), 50A...covering portion, 50B...protective portion, 60...battery (electrochemical cell), 61...pressure roller, 65...electrode body, 66: negative electrode side separator layer, 67: negative electrode body, 68: positive electrode side separator layer, 69: positive electrode body, 70: negative electrode tab, 71: positive electrode tab.

Claims

1. An electrochemical cell comprising an exterior body having a case having sides and a bottom, one of the bottoms being an opening and the other of the bottoms being formed with a through hole, a cover plate welded to the opening and sealing the opening, and an electrode plate closing the through hole via a resin film fused to the peripheral portion of the through hole, wherein a portion of the cover plate has a bend correction portion or a curve correction portion.

2. the case and the cover plate are made of metal; The electrode assembly is housed in the exterior housing, 2. The electrochemical cell according to claim 1, wherein one of the positive and negative electrode bodies constituting the electrode assembly is electrically connected to the case, and the other is electrically connected to the electrode plate.

3. 3. The electrochemical cell according to claim 1, wherein the resin film is formed on almost the entire surface of the bottom portion except for the position of the through hole.

4. 4. The electrochemical cell of claim 3, wherein the electrode plate is formed so as to have substantially the same periphery as the resin film.

5. 5. The electrochemical cell according to claim 1, wherein the electrode plate is provided with an electrode terminal protruding from an outer peripheral edge of the bottom of the case.

6. 6. The electrochemical cell according to claim 5, wherein a protective portion is formed on the outer peripheral edge of the resin film in a portion that contacts the base end of the electrode terminal, the protective portion protruding outward from the outer peripheral edge of the resin film.

7. The present invention relates to an electrochemical cell including an exterior body having a case having sides and a bottom, one of the bottoms being an opening and the other bottom being formed with a through-hole, a cover plate welded to the opening and sealing the opening, and an electrode plate closing the through-hole via a resin film fused to a peripheral portion of the through-hole, and the present invention relates to an electrochemical cell including an electrode assembly housed in the exterior body, the method comprising the steps of: a cover plate having a bent or curved portion on at least a portion of an outer periphery of the opening of the case is placed over the opening periphery of the case, an electrolyte is injected into the case by utilizing a gap generated at the opening periphery of the case due to the presence of the bent or curved portion, and after the electrolyte is injected, the opening periphery of the case and the outer periphery of the cover plate are welded together.

8. 8. The method for manufacturing an electrochemical cell according to claim 7, wherein, when welding the peripheral edge portion of the opening of the case and the outer periphery portion of the cover plate, the outer periphery portion of the cover plate is pressed against the peripheral edge portion of the opening of the case, and the outer periphery portion of the cover plate is welded to the peripheral edge portion of the opening of the case along the pressed portion.

9. 9. The method for manufacturing an electrochemical cell according to claim 7 or 8, characterized in that one of the positive electrode and the negative electrode formed on the electrode body is electrically connected to the cover plate, and the other of the positive electrode and the negative electrode is electrically connected to the electrode plate through the through hole.

10. The method for producing an electrochemical cell according to any one of claims 7 to 9, wherein an electrode plate having an electrode portion that closes the through-hole of the resin film and covers up to an outer peripheral edge portion of the resin film, and an electrode terminal that protrudes outward from the electrode portion and protrudes outward beyond the outer peripheral edge portion of the resin film is used as the electrode plate.

11. 11. The method for manufacturing an electrochemical cell according to claim 10, wherein a resin film is used in which a protective portion is formed on an outer peripheral edge of the resin film in a portion that contacts the base end of the electrode terminal and that protrudes outward from the outer peripheral edge of the resin film.

Citation Information

Patent Citations

  • Film armored battery and battery pack

    JP2008016368A

  • Electrochemical cell and method for manufacturing the same

    JP2011228409A

  • Electrochemical cell and manufacturing method of electrochemical cell

    JP2018085214A

  • Sealed electrical storage device

    JP2019046639A

  • Electrochemical cell and manufacturing method thereof

    JP2020072061A