Test chip and manufacturing method thereof
The test chip design optimizes liquid flow paths through multiple layers to address uneven color development, ensuring precise and quantitative analysis by maintaining the coloring area centrally, thus improving the reliability of test results.
Patent Information
- Application Number
- JP2021001630
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2020-04-28
- Filing Date
- 2021-01-07
- Publication Date
- 2024-10-03
- Estimated Expiration
- 2041-01-07
AI Technical Summary
Conventional test chips experience uneven color development near the edge of the detection area, leading to unreliable test results and difficulty in quantifying the presence of target substances.
The test chip design includes a first and second layer with optimized liquid flow paths, utilizing capillary action to direct the liquid flow from the liquid receiving part to the detection confirmation part through the thickness of the sheet, with features such as annular structures and multiple flow paths to ensure even distribution.
This design significantly suppresses uneven color development, allowing for precise and quantitative analysis of target substances by maintaining the coloring area near the center of the detection confirmation part, enhancing the reliability of test results.
Smart Images

Figure 0007561041000007 
Figure 0007561041000008 
Figure 0007561041000009
Abstract
Description
[Technical field]
[0001] The present invention relates to a test chip and a method for manufacturing the same. [Background technology]
[0002] The idea that diagnosis can be performed in close proximity to patients (on-site diagnosis) is becoming more and more important in clinical settings. Based on this idea, test chips that enable practical analysis by providing micro-sized channels and reaction spots on a sheet-like substrate have been developed.
[0003] An example of the above-mentioned test chip has a mechanism in which, when a test liquid containing a target substance such as an antigen is introduced, the test liquid flows through a flow path, and a labeling medium such as an antibody that has been prepared in advance reacts with the target substance, thereby confirming the presence of the target substance by developing color (coloring). A typical example is a pregnancy test.
[0004] As an example of the above-mentioned test chip, a microfluidic device has already been reported in which a paper substrate is used to form channels and reaction spots on the paper using a wax printer or an inkjet printer (Non-Patent Document 1). Such devices are also called "μ-PADs (microfluidic paper-based analytical devices)" and have many advantages, such as (1) low cost, (2) pumpless, (3) no need for large-scale equipment, and (4) easy disposal. Research into improving such μ-PADs is being conducted worldwide.
[0005] For example, Patent Document 1 discloses that a test chip can be manufactured simply and at low cost by printing the outer edges of the flow paths and reaction spots described above on paper with ultraviolet-curable ink and then curing the ink by irradiating it with ultraviolet light. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] International Publication No. 2012 / 160857 [Non-patent literature]
[0007] [Non-Patent Document 1] Whiteside et al., Analytical Chemistry, Vol. 82, No. 1, January 1, 2010 Summary of the Invention [Problem to be solved by the invention]
[0008] However, conventional test chips including the technology of Patent Document 1 described above are prone to uneven color development, which may lead to variations in test results (insufficient reproducibility). As one example, there is a problem in which color development occurs near the edge of the detection area, making it difficult to visually observe. Such a problem may have a negative impact on the diagnosis of important diseases. For this reason, conventional test chips have room for improvement in terms of suppressing uneven color development.
[0009] Furthermore, in addition to confirming the presence or absence of the target substance, it is expected that the above-mentioned test chips such as μ-PADs will also be able to quantify it. In this regard, if the above-mentioned unevenness in color development (color development) can be suppressed, it will be possible to specify the area of the colored portion in the test chip and apply pixel analysis technology to achieve quantification. From this perspective, suppression of uneven color development is also desirable.
[0010] The present invention aims to solve the above-mentioned problems in the prior art and to achieve the following objectives. That is, the present invention aims to provide a test chip in which a target substance contained in a test liquid reacts with a labeling medium that has been added in advance, and the presence of the target substance is confirmed by the color produced by the reaction, in which color development is significantly suppressed. Another objective of the present invention is to provide a method for producing the test chip, which allows the above-mentioned test chip to be produced easily, highly accurately, and at low cost. [Means for solving the problem]
[0011] In solving the above problem, the inventors first discovered that the problem with conventional test chips, in which color development occurs near the edge of the detection area, is caused by the force of the liquid flow reaching the detection area.
[0012] After extensive research, the inventors discovered that by optimizing the liquid flow path so that the liquid reaches the detection area from the thickness direction of the sheet, color development can be caused to occur near the center of the detection area, which led to the present invention.
[0013] The means for achieving the above object are as follows.
[0014] <1> A sheet-shaped test chip, A first layer on the front side and a second layer on the back side, the first layer and the second layer are adjacent; Either the first layer or the second layer has a liquid receiving portion A, The first layer has at least a detection confirmation portion B, The second layer has at least a liquid flow section D adjacent to the detection confirmation section B and a liquid flow path E connected to the liquid flow section D, When the first layer has a liquid receiving portion A, the liquid receiving portion A is separated from the detection confirmation portion B, When a test liquid is dropped onto the liquid receiving section (A), the test liquid flows to the detection confirmation section (B) by capillary action through the liquid receiving section (A), the liquid flow path (E) and the liquid flow section (D) in this order, An inspection chip, characterized in that the first layer is formed on one surface of a sheet-like material, and the second layer is formed on the other surface of the sheet-like material.
[0015] <2> A sheet-shaped test chip, A first layer on the front side and a second layer on the back side, the first layer and the second layer are adjacent; Either the first layer or the second layer has a liquid receiving portion A, The first layer has at least a detection confirmation portion B, The second layer has at least a liquid flow section D adjacent to the detection confirmation section B and a liquid flow path E connected to the liquid flow section D, When the first layer has a liquid receiving portion A, the liquid receiving portion A is separated from the detection confirmation portion B, When a test liquid is dropped onto the liquid receiving section (A), the test liquid flows to the detection confirmation section (B) by capillary action through the liquid receiving section (A), the liquid flow path (E) and the liquid flow section (D) in this order, The test chip is characterized in that the liquid flow section D has a ring-shaped structure with a liquid non-flow section D' formed on the inside.
[0016] <3> A sheet-shaped test chip, A first layer on the front side and a second layer on the back side, the first layer and the second layer are adjacent; Either the first layer or the second layer has a liquid receiving portion A, The first layer has at least a detection confirmation portion B, The second layer has at least a liquid flow section D adjacent to the detection confirmation section B and a liquid flow path E connected to the liquid flow section D, When the first layer has a liquid receiving portion A, the liquid receiving portion A is separated from the detection confirmation portion B, When a test liquid is dropped onto the liquid receiving section (A), the test liquid flows to the detection confirmation section (B) by capillary action through the liquid receiving section (A), the liquid flow path (E) and the liquid flow section (D) in this order, The test chip, characterized in that the second layer has a plurality of the liquid flow paths E.
[0017] <4> At least two of the liquid flow paths E are connected to the liquid flow section D so as to face each other. <3> The inspection chip according to claim 1.
[0018] <5> At least two of the liquid flow paths E have substantially the same shape. <3> or <4> The inspection chip according to claim 1.
[0019] <6> The first layer has the liquid receiving portion A separated from the detection confirmation portion B, The second layer has a liquid flow section C adjacent to the liquid receiving section A, When a test liquid is dropped onto the liquid receiving section A, the test liquid flows to the detection confirmation section B by capillary action through the liquid receiving section A, the liquid flow section C, the liquid flow path E and the liquid flow section D in this order. <1> ~ <5> 13. The test chip according to claim 12,
[0020] <7> the first layer has the liquid receiving portion A separated from the detection confirmation portion B, and further has a liquid flow path F connected to the liquid receiving portion A; When a test liquid is dropped onto the liquid receiving section A, the test liquid flows to the detection confirmation section B by capillary action through the liquid receiving section A, the liquid flow path F, the liquid flow path E and the liquid flow section D in this order. <1> ~ <5> 13. The test chip according to claim 12,
[0021] <8> The second layer has the liquid receiving portion A. <1> ~ <5> 13. The test chip according to claim 12,
[0022] <9> the liquid receiving portion A, any one of the liquid flow portions C, any one of the liquid flow paths F, the liquid flow path E, the liquid flow portion D, and the detection confirmation portion B are made of a material M in which the flow of the test liquid is manifested by capillary action; The portion other than the material M is made of a material M' that is obtained by impregnating the material M with a hydrophobic material, and through which the test liquid does not flow. <1> ~ <8> 13. The test chip according to claim 12,
[0023] <10> The material M is filter paper. <9> The inspection chip according to claim 1.
[0024] <11> In the material M', the impregnation rate of the hydrophobic material into the material M is 14% or more and 32% or less. <9> or <10> The inspection chip according to claim 1.
[0025] <12> a ratio of a thickness of the second layer to a thickness of the first layer (thickness of the second layer / thickness of the first layer) is 0.56 or more and 2.2 or less; <1> ~ <11> 13. The test chip according to claim 12,
[0026] <13> A color reaction caused by the detection target substance occurs in the detection confirmation section B. <1> ~ <12> 13. The test chip according to claim 12,
[0027] <14> <1> ~ <13> A method for producing the test chip according to any one of the above, a film forming step of forming a first hydrophobic film on a first substrate and a second hydrophobic film on a second substrate using a hydrophobic material; a first printing step of printing a first sacrificial substrate with a first hydrophobic film on the first substrate in a reverse design of a first layer of a test chip; a second printing step of printing a second sacrificial substrate with a second hydrophobic film on the second substrate in a reverse design of the second layer of the test chip; a first transfer step of transferring the first hydrophobic film after the first printing step onto one surface of a sheet-like material and impregnating the sheet-like material; a second transfer step of transferring the second hydrophobic film after the second printing step to the other surface of the one sheet-like material and impregnating the sheet-like material; A method for manufacturing an inspection chip, comprising:
[0028] <15> a ratio of a thickness of the second hydrophobic film to a thickness of the first hydrophobic film (thickness of the second hydrophobic film / thickness of the first hydrophobic film) is 0.56 or more and 2.2 or less; <14> A method for producing the test chip according to claim 1. Effect of the Invention
[0029] According to the present invention, a test chip in which a target substance contained in a test liquid reacts with a labeling medium previously prepared and the presence of the target substance is confirmed by the color produced by the reaction can be provided, in which color unevenness is significantly suppressed. Also, according to the present invention, a method for producing the test chip described above can be provided, which can easily, highly accurately, and at low cost. [Brief description of the drawings]
[0030] [Figure 1A] FIG. 1 is a schematic perspective view of an example of a test chip according to the present invention. [Figure 1B] FIG. 1B is a schematic perspective view of the test chip of FIG. 1A. [Diagram 2] 1B is a schematic plan view of the front and back surfaces of the test chip of FIG. 1A. [Diagram 3] FIG. 1B is a schematic cross-sectional view of the test chip of FIG. 1A. [Figure 4] FIG. 2 is a schematic exploded view of the test chip according to one embodiment of the present invention. [Diagram 5] 1A to 1C are schematic plan views of the front and back surfaces of an example of a test chip of the present invention. [Figure 6] FIG. 6 is a schematic cross-sectional view of the test chip of FIG. 5. [Figure 7] 1A to 1C are schematic plan views of the front and back surfaces of an example of a test chip of the present invention. [Figure 8] FIG. 8 is a schematic cross-sectional view of the test chip of FIG. [Figure 9] 1A to 1C are schematic plan views of the front and back surfaces of an example of a test chip of the present invention. [Figure 10] 1A to 1C are schematic plan views of the front and back surfaces of an example of a test chip of the present invention. [Figure 11] 1A to 1C are schematic plan views of the front and back surfaces of an example of a test chip of the present invention. [Figure 12] 1A to 1C are schematic plan views of the front and back surfaces of an example of a test chip of the present invention. [Figure 13] 1A to 1C are schematic plan views of the front and back surfaces of an example of a test chip of the present invention. [Figure 14] 1A to 1C are schematic plan views of the front and back surfaces of an example of a test chip of the present invention. [Figure 15] FIG. 1 is a schematic cross-sectional view of an example of a test chip of the present invention. [Figure 16] 1A and 1B are schematic plan views of the front and back surfaces of a test chip of a comparative example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0031] Hereinafter, the present invention will be described in detail based on embodiments.
[0032] (Test chip) The test chip of the present invention is a sheet-shaped test chip, A first layer on the front side and a second layer on the back side, the first layer and the second layer are adjacent; Either the first layer or the second layer has a liquid receiving portion A, The first layer has at least a detection confirmation portion B, The second layer has at least a liquid flow section D adjacent to the detection confirmation section B and a liquid flow path E connected to the liquid flow section D, When the first layer has a liquid receiving portion A, the liquid receiving portion A is separated from the detection confirmation portion B, The basic feature of this device is that when the test liquid is dropped into the liquid receiving section A, the test liquid flows by capillary action through the liquid receiving section A, the liquid flow path E and the liquid flow section D in that order to the detection confirmation section B.
[0033] In addition to the above-mentioned basic features, the test chip according to one embodiment of the present invention is further characterized in that the liquid flow part D has a ring-shaped structure with a liquid non-flow part D' formed on the inside. The details of this feature will be described later.
[0034] In addition to the above basic features, a test chip according to another embodiment of the present invention has a further feature in that the second layer has a plurality of the liquid flow paths E. Details of this feature will be described later.
[0035] In addition to the above basic features, the test chip according to another embodiment of the present invention is further characterized in that the first layer is formed on one side of a sheet-like material, and the second layer is formed on the other side of the sheet-like material. Details of this feature will be described later.
[0036] These test chips can significantly suppress uneven color development.
[0037] In the test chip of the present invention, the liquid receiving section A is a section where the test liquid is dropped. In addition, in the test chip of the present invention, the detection confirmation section B is a section where the presence or absence of a target substance such as an antigen in the test liquid dropped into the liquid receiving section A is confirmed by the presence or absence of color development. Therefore, the test chip 1 of the present invention can be provided with a medium that reacts with the target substance and / or a labeling medium that causes a color development reaction due to the target substance in an appropriate position. Also, preferably, in the test chip 1 of the present invention, a color development reaction due to the target substance occurs in the detection confirmation section B.
[0038] More specifically, examples of the above-mentioned basic features shared by the test chips of the present invention include an embodiment in which a liquid receiving section A is provided in a first layer and a second layer has a liquid flow section C (first embodiment), an embodiment in which a liquid receiving section A is provided in a first layer and a first layer further has a liquid flow path F connected to the liquid receiving section A (second embodiment), and an embodiment in which a liquid receiving section A is provided in a second layer (third embodiment).
[0039] <First aspect of basic feature> 1A and 1B are schematic perspective views of the test chip 1 having the first embodiment. The test chip 1 has a first layer 10 on the front side, that is, the side on which the person performing the test visually confirms the test results when using the test chip, and a second layer 20 on the back side. FIG. 1A is a perspective view of the test chip 1 with the front side facing up, and FIG. 1B is a perspective view of the test chip 1 with the back side facing up. As shown in FIGS. 1A and 1B, the test chip 1 is sheet-shaped. In addition, the first layer 10 and the second layer 20 in the test chip 1 are adjacent to each other without any intervening layer. The shape of the test chip 1 in a plan view is not particularly limited and can be appropriately selected depending on the purpose. For example, it may be rectangular as shown in FIGS. 1A and 1B, or it may be circular, elliptical, or the like.
[0040] Fig. 2 is a schematic plan view of the front and back surfaces of the test chip 1, and its structure corresponds to the test chip 1 shown in Fig. 1A and Fig. 1B. As shown in Fig. 2, the test chip 1 has a liquid receiving section A and a detection confirmation section B provided in a first layer 10 arranged on the front side. The liquid receiving section A and the detection confirmation section B are spaced apart in the first layer 10 of the test chip 1.
[0041] Furthermore, the first layer 10 of the test chip 1 is provided with a liquid non-flowing portion X as a portion other than the liquid receiving portion A and the detection confirmation portion B. The liquid receiving portion A and the detection confirmation portion B are made of, for example, a material M that allows the flow of the test liquid by capillary action. The liquid non-flowing portion X is made of, for example, a material M' that does not allow the flow of the test liquid.
[0042] As shown in FIG. 2, the second layer 20 of the test chip 1 is provided with a liquid circulating section C, a liquid circulating section D, and a liquid flow path E on the back side. The liquid flow path E is connected to the liquid circulating section D and is also connected to the liquid circulating section C. The second layer 20 of the test chip 1 is further provided with a liquid non-circulating section Y as a portion other than the liquid circulating section C, the liquid flow path E, and the liquid circulating section D. The liquid circulating section C, the liquid flow path E, and the liquid circulating section D are made of a material M that allows the flow of the test liquid to occur due to capillary action, similar to the above-mentioned liquid receiving section A and detection confirmation section B. The liquid non-circulating section Y is made of a material M' that does not allow the flow of the test liquid to occur, similar to the above-mentioned liquid non-circulating section X.
[0043] 3 shows a schematic cross-sectional view of the test chip 1 of FIG. 2 cut along line a-a'. As shown in FIG. 3, in the test chip 1 having the first embodiment, the liquid receiving section A of the first layer 10 and the liquid flow section C of the second layer 20 are adjacent to each other, and the detection confirmation section B of the first layer 10 and the liquid flow section D of the second layer 20 are adjacent to each other. That is, in the test chip 1 having the first embodiment, the liquid receiving section A, the liquid flow section C, the liquid flow path E, the liquid flow section D, and the detection confirmation section B are adjacent to each other or connected in this order. In other words, the test chip 1 having the first embodiment is configured such that when the test liquid is dropped into the liquid receiving section A, the test liquid passes through the liquid receiving section A, the liquid flow section C, the liquid flow path E, and the liquid flow section D in this order by capillary action, and finally flows to the detection confirmation section B.
[0044] Here, in the conventional test chip, the liquid receiving section and the detection confirmation section (detection area) are simply connected by a flow path on the substrate, so that when the test liquid is dropped into the liquid receiving section, the force of the liquid flow that advances in the surface direction of the substrate and reaches the detection area causes the color to be unevenly distributed near the end of the detection area (especially near the end farther from the liquid receiving section). On the other hand, since the above test chip 1 has the above-mentioned configuration, the test liquid dropped into the liquid receiving section A can finally reach the detection confirmation section B in the thickness direction of the test chip 1 (the direction from the liquid flow section D toward the detection confirmation section B). Therefore, in the test chip 1 having the first embodiment, the coloring point can be kept near the center of the detection confirmation section B, so that the coloring unevenness can be significantly suppressed.
[0045] As described above, the liquid receiving portion A and the detection confirmation portion B in the first layer 10, and the liquid flow portion C, the liquid flow portion D and the liquid flow path E in the second layer 20 are made of, for example, a material M that allows the flow of the test liquid by capillary action. On the other hand, the liquid non-flow portion X in the first layer 10 and the liquid non-flow portion Y in the second layer 20 are made of, for example, a material M' that is obtained by impregnating the material M with a hydrophobic material and does not allow the flow of the test liquid.
[0046] FIG. 4 shows a schematic exploded view of the test chip 1 of FIG. 1A and FIG. 1B. As shown on the left side of FIG. 4, the test chip 1 is typically composed of the above-mentioned material M, a pre-first layer 10' made of a hydrophobic material 50 having the design of the first layer 10, and a pre-second layer 20' made of a hydrophobic material 50 having the design of the second layer 20. As shown on the left side of FIG. 4, the test chip 1 has a configuration in which the pre-first layer 10' and the pre-second layer 20' are impregnated from both sides of the material M. As shown on the right side of FIG. 4, from the viewpoint of materials, the test chip 1 is composed of, for example, a material M and a material M' obtained by impregnating the material M with a hydrophobic material 50.
[0047] The material M is not particularly limited as long as it generates capillary action, and examples thereof include paper such as filter paper, nonwoven fabric, nitrocellulose, polypropylene, etc. Among these, from the viewpoint of more conveniently and inexpensively producing the test chip, the material M is preferably filter paper. The thickness and basis weight (density) of the material M can be appropriately selected in consideration of the viscosity of the test liquid, etc.
[0048] The hydrophobic material is not particularly limited as long as it can be impregnated into the material M and inhibits the capillary phenomenon in the material M, and examples of the hydrophobic material include wax and a composition containing the wax. From the viewpoint of ease of production, the hydrophobic material preferably has a melting point of 90° C. or less.
[0049] In the above test chip, the material M' of the liquid non-flowing portion X on the front side is preferably colored so that the person conducting the test can easily visually recognize the liquid receiving portion A and the detection confirmation portion B on the front side. On the other hand, the material M' of the liquid non-flowing portion Y on the back side of the above test chip may be colored, or may be white or transparent, or may not be colored.
[0050] The coloring of the material M' can be achieved, for example, by impregnating the material M with a colorant in addition to the hydrophobic material. Such a colorant is preferably hydrophobic, and examples of such a colorant include pigments such as carbon black (black pigment). In addition, it is preferable to select a colorant that does not adversely affect the reagent used in the test chip.
[0051] The shape of the liquid receiving portion A in a plan view is not particularly limited and can be appropriately selected depending on the purpose. For example, it may be circular as shown in FIG. 2, or it may be elliptical, rectangular, or the like.
[0052] The shape of the detection confirmation portion B in a plan view is not particularly limited and can be appropriately selected depending on the purpose. It may be circular as shown in FIG. 2, or may be elliptical, rectangular, or the like.
[0053] The shape of the liquid flow section C in a plan view is not particularly limited and can be appropriately selected depending on the purpose, but it is preferably the same shape as the liquid receiving section A. In addition, it is preferable that the liquid flow section C has a shape that substantially coincides with the liquid receiving section A in a plan view of the test chip.
[0054] The shape of the liquid flow section D in a plan view is not particularly limited and can be appropriately selected depending on the purpose, but it is preferably the same shape as the detection confirmation section B. In addition, it is preferable that the liquid flow section D has a shape that substantially coincides with the detection confirmation section B in a plan view of the test chip.
[0055] The thickness of the test chip of the present invention is not particularly limited, but can be, for example, 100 to 300 μm.
[0056] Although not shown, the test chip of the present invention may have multiple sets of combinations of the detection confirmation unit B, the liquid flow unit D, and the liquid flow path E. In this case, the presence or absence of multiple detection target substances can be confirmed simultaneously in one test.
[0057] <Second aspect of basic feature> Fig. 5 is a schematic plan view of the front and back surfaces of the test chip 1 having the second embodiment. As shown in Fig. 5, the test chip 1 has a liquid receiving section A and a detection confirmation section B provided in a first layer 10 arranged on the front side. The liquid receiving section A and the detection confirmation section B are spaced apart in the first layer 10 of the test chip 1. The test chip 1 also has a liquid flow path F connected to the liquid receiving section A in the first layer 10 arranged on the front side.
[0058] Furthermore, the first layer 10 of the test chip 1 is provided with a liquid non-flowing section X as a portion other than the liquid receiving section A, the detection confirmation section B, and the liquid flow path F. The liquid receiving section A, the detection confirmation section B, and the liquid flow path F are made of, for example, a material M that allows the flow of the test liquid by capillary action. The liquid non-flowing section X is made of, for example, a material M' that does not allow the flow of the test liquid.
[0059] As shown in FIG. 5, the second layer 20 of the test chip 1 is provided with a liquid flow section D and a liquid flow path E on the back side. The liquid flow path E is connected to the liquid flow section D. Furthermore, the second layer 20 of the test chip 1 is provided with a liquid non-flow section Y as a portion other than the liquid flow path E and the liquid flow section D. The liquid flow path E and the liquid flow section D are made of a material M that allows the flow of the test liquid to occur due to capillary action, similar to the above-mentioned liquid receiving section A, detection confirmation section B, and liquid flow path F. The liquid non-flow section Y is made of a material M' that does not allow the flow of the test liquid to occur, similar to the above-mentioned liquid non-flow section X.
[0060] FIG. 6 shows a schematic cross-sectional view of the test chip 1 of FIG. 5 cut along the line b-b'. As shown in FIG. 6, in the test chip 1 having the second embodiment, the detection confirmation section B of the first layer 10 and the liquid flow section D of the second layer 20 are adjacent to each other, and the liquid flow path F of the first layer 10 and the liquid flow path E of the second layer 20 are connected to each other. That is, in the test chip 1 having the second embodiment, the liquid receiving section A, the liquid flow path F, the liquid flow path E, the liquid flow section D, and the detection confirmation section B are adjacent to each other or connected in this order. In other words, the test chip 1 having the second embodiment is configured such that when the test liquid is dropped into the liquid receiving section A, the test liquid passes through the liquid receiving section A, the liquid flow path F, the liquid flow path E, and the liquid flow section D in this order by capillary action, and finally flows to the detection confirmation section B. Therefore, in the test chip 1 having the second embodiment, similarly to the first embodiment, the test liquid dropped into the liquid receiving section A can finally reach the detection confirmation section B in the thickness direction of the test chip 1 (the direction from the liquid flow section D toward the detection confirmation section B). Therefore, also in the test chip 1 having the second embodiment, the coloring portion can be confined to the vicinity of the center of the detection confirmation section B, so that coloring unevenness can be significantly suppressed.
[0061] As described above, the liquid receiving portion A, the detection confirmation portion B, and the liquid flow path F in the first layer 10, and the liquid flow path portion D and the liquid flow path E in the second layer 20 are made of, for example, a material M that allows the flow of the test liquid by capillary action. On the other hand, the liquid non-flow portion X in the first layer 10 and the liquid non-flow portion Y in the second layer 20 are made of, for example, a material M' that is obtained by impregnating the above-mentioned material M with a hydrophobic material and does not allow the flow of the test liquid.
[0062] In the above test chip, the material M' of the liquid non-flowing portion X on the front side is preferably colored so that the person conducting the test can easily visually recognize the liquid receiving portion A and the detection confirmation portion B on the front side. On the other hand, the material M' of the liquid non-flowing portion Y on the back side of the above test chip may be colored, or may be white or transparent, or may not be colored.
[0063] Other than the above, explanation of matters common to the first embodiment will be omitted.
[0064] <Third aspect of basic feature> Fig. 7 is a schematic plan view of the front and back surfaces of the test chip 1 having the third embodiment. As shown in Fig. 7, the test chip 1 has a detection confirmation part B provided on the first layer 10 arranged on the front side, and no liquid receiving part A is provided.
[0065] Furthermore, the first layer 10 of the test chip 1 is provided with a liquid non-flowing portion X as a portion other than the detection confirmation portion B. The detection confirmation portion B is made of, for example, a material M that allows the flow of the test liquid by capillary action. The liquid non-flowing portion X is made of, for example, a material M' that does not allow the flow of the test liquid.
[0066] As shown in FIG. 7, the second layer 20 of the test chip 1 is provided on the back side with a liquid receiving section A, a liquid flow section D, and a liquid flow path E. The liquid flow path E is connected to the liquid flow section D and is also connected to the liquid receiving section A. The second layer 20 of the test chip 1 is further provided with a liquid non-flow section Y as a portion other than the liquid receiving section A, the liquid flow path E, and the liquid flow section D. The liquid receiving section A, the liquid flow path E, and the liquid flow section D are made of a material M that allows the flow of the test liquid to occur due to capillary action, similar to the detection confirmation section B described above. The liquid non-flow section Y is made of a material M' that does not allow the flow of the test liquid to occur, similar to the liquid non-flow section X described above.
[0067] FIG. 8 shows a schematic cross-sectional view of the test chip 1 of FIG. 7 cut along the c-c' line. As shown in FIG. 8, in the test chip 1 having the third embodiment, the detection confirmation section B of the first layer 10 and the liquid flow section D of the second layer 20 are adjacent to each other. That is, in the test chip 1 having the third embodiment, the liquid receiving section A, the liquid flow path E, the liquid flow section D, and the detection confirmation section B are adjacent to each other or connected in this order. In other words, the test chip 1 having the third embodiment is configured such that when the test liquid is dropped into the liquid receiving section A, the test liquid passes through the liquid receiving section A, the liquid flow path E, and the liquid flow section D in this order by capillary action, and finally flows to the detection confirmation section B. Therefore, in the test chip 1 having the third embodiment, the test liquid dropped into the liquid receiving section A can finally reach the detection confirmation section B in the thickness direction of the test chip 1 (the direction from the liquid flow section D toward the detection confirmation section B) as in the first embodiment. Therefore, even in the test chip 1 having the third embodiment, the coloring portion can be limited to the vicinity of the center of the detection confirmation part B, so that uneven coloring can be significantly suppressed.
[0068] As described above, the detection confirmation section B in the first layer 10, and the liquid receiving section A, liquid flow section D, and liquid flow path E in the second layer 20 are made of, for example, a material M that allows the flow of the test liquid by capillary action. On the other hand, the liquid non-flow section X in the first layer 10 and the liquid non-flow section Y in the second layer 20 are made of, for example, a material M' that is obtained by impregnating the material M with a hydrophobic material and does not allow the flow of the test liquid.
[0069] In the above test chip, it is preferable that the material M' of the liquid non-circulating portion X on the front side and the liquid non-circulating portion Y on the back side be colored so that the person conducting the test can easily visually identify the liquid receiving portion A and the detection confirmation portion B on the front side.
[0070] The test chip having the third embodiment is particularly useful, for example, when it is desired to arrange the liquid receiving portion A and the detection confirmation portion B on different surfaces from the viewpoint of fail-safe.
[0071] Other than the above, explanation of matters common to the first embodiment will be omitted.
[0072] Furthermore, the test chip of the present invention can have the following characteristics as appropriate. Below, the description will be given based on the case having the above-mentioned first aspect as a basic feature, but any of the characteristics can be applied to the cases having the second and third aspects.
[0073] 9 is a schematic plan view of the front and back surfaces of the test chip 1 of one embodiment. The test chip 1 shown in FIG. 9 is similar to that shown in FIG. 2, except that the liquid flow section D provided in the second layer 20 arranged on the back side has a ring structure and a liquid non-flow section D' is formed on the inside. In this test chip 1, due to the presence of the liquid non-flow section D', when the test liquid advances from the liquid flow section D toward the detection confirmation section B, a liquid flow can be formed in the detection confirmation section B from the outside toward the center. Therefore, the coloring area can be further confined near the center of the detection confirmation section B, and color unevenness can be further significantly suppressed.
[0074] In the test chip 1 as described above, the liquid flow section D, which is an annular structure, can have any contour shape, such as a circle, an ellipse, a rectangle, etc., but preferably has a contour shape that substantially matches that of the detection confirmation section B in a planar view of the test chip. Also, it is preferable that the liquid non-flow section D' has a shape that is a scaled-down version of the contour shape of the liquid flow section D in a planar view of the test chip. Furthermore, it is preferable that the liquid non-flow section D' is white or transparent, or is not colored, so as not to impede confirmation of color development in the detection confirmation section B.
[0075] Fig. 10 is a schematic plan view of the front and back surfaces of a test chip 1 of another embodiment. The test chip 1 shown in Fig. 10 is similar to that shown in Fig. 2, except that the second layer 20 arranged on the back surface side has a plurality of liquid flow paths E (two paths, E1 and E2, in Fig. 10). In this test chip 1, the presence of a plurality of liquid flow paths E allows the momentum of the liquid flow from each liquid flow path E to be offset when the test liquid advances from the liquid flow section D toward the detection confirmation section B, thereby promoting the liquid flow in the thickness direction of the test chip 1. Therefore, the coloring area can be further confined near the center of the detection confirmation section B, and color unevenness can be further significantly suppressed.
[0076] Regarding the above-mentioned features, in the case of a test chip having the second embodiment, a plurality of liquid flow paths F can be provided in the same number as the number of liquid flow paths E, and the plurality of liquid flow paths F in the first layer 10 can be connected to the plurality of liquid flow paths E in the second layer 20, respectively.
[0077] Fig. 11 is a schematic plan view of the front and back surfaces of a test chip 1 of another embodiment. The test chip 1 shown in Fig. 11 combines the features shown in Fig. 9 and the features shown in Fig. 10. With this test chip 1 as well, color unevenness can be more significantly suppressed.
[0078] Fig. 12 is a schematic plan view of the front and back surfaces of a test chip 1 of another embodiment. The test chip 1 shown in Fig. 12 is generally similar to Fig. 11, except that the second layer 20 arranged on the back surface side has three liquid flow paths E (E3 in addition to E1 and E2). In this case, in the test chip 1 shown in Fig. 12, the three liquid flow paths E are connected to the liquid circulation section D so as to face each other. In such a test chip 1, uneven color development can also be more significantly suppressed.
[0079] Fig. 13 is a schematic plan view of the front and back surfaces of a test chip 1 of another embodiment. The test chip 1 shown in Fig. 13 is generally similar to that shown in Fig. 12, except that it has a feature that the liquid flow path E3 branches into two (E31 and E32) and is connected to the liquid flow section D. With this test chip 1 as well, it is possible to more significantly suppress uneven color development.
[0080] Fig. 14 is a schematic plan view of the front and back surfaces of a test chip 1 of another embodiment. The test chip 1 shown in Fig. 14 is generally similar to Fig. 11, except that it has two more liquid flow paths E (E3 and E4) in addition to the liquid flow paths E1 and E2. In the test chip 1 shown in Fig. 14, the four liquid flow paths E are connected to the liquid circulation section D so as to face each other. With this test chip 1 as well, color unevenness can be more significantly suppressed.
[0081] In the test chip 1 as described above, the number of liquid flow paths E (and liquid flow paths F in the case of the second embodiment) is preferably 4 or less, more preferably 3 or less, and even more preferably 2, from the viewpoint of suppressing an increase in the amount of test liquid required for testing. Moreover, the number of connection points of the liquid flow paths E to the liquid flow section D is preferably 4 or less, more preferably 3 or less, and even more preferably 2.
[0082] In the test chip 1 as described above, it is preferable that at least two of the multiple liquid flow paths E are connected to the liquid circulation section D so as to face each other, as shown in Figures 10 to 14. This allows the liquid flows from the liquid flow paths E to gather near the center of the liquid circulation section D when the test liquid advances from the liquid flow path D toward the detection and confirmation section B, and promotes the liquid flow in the thickness direction of the test chip 1. This allows the color development area to be further confined near the center of the detection and confirmation section B, thereby more significantly suppressing color development unevenness.
[0083] In the above-described test chip 1, it is preferable that at least two of the multiple liquid flow paths E have substantially the same shape, as shown in Figures 10 to 14. In this case, the liquid flowing through the liquid flow path E can reach the liquid flow section D and the detection confirmation section B substantially simultaneously, so that drift can be avoided and uneven color development can be more significantly suppressed.
[0084] When the above-mentioned test chip 1 is made of a material M (a material in which the flow of the test liquid is realized by capillary action) and a material M' (a material in which the flow of the test liquid is not realized, which is obtained by impregnating the material M with a hydrophobic material), it is preferable that the impregnation rate of the hydrophobic material in the material M' is within a range of 14% to 32%. By manufacturing the test chip so that the impregnation rate is 14% or more, the wall surface of the flow path of the test liquid (the interface between the material M and the material M') becomes sufficiently uniform, and the flow of the liquid from the liquid receiving part A to the detection confirmation part B can be made smoother. In addition, by manufacturing the test chip so that the impregnation rate is 32% or less, problems such as blockages occurring when the material M is impregnated with a hydrophobic material can be sufficiently avoided, and the test chip having the desired flow path structure can be more reliably obtained.
[0085] The above impregnation rate refers to the impregnation rate of the material M' in a region of the test chip 1 that is made of the material M' over the entire thickness direction. The above-mentioned impregnation rate can be considered to be 100% for a material M' obtained by immersing the material M in a hydrophobic material that has been heated to a sufficiently low viscosity (for example, heated to 120°C) and leaving it for a sufficient time (for example, 3 minutes) while maintaining the temperature. More specifically, the above-mentioned impregnation rate can be obtained by the method described in the examples. The impregnation rate can be adjusted, for example, by adjusting the amount of hydrophobic material to be impregnated (such as the thickness of the hydrophobic film).
[0086] In the test chip 1 as described above, the ratio of the thickness of the second layer 20 (t2) to the thickness of the first layer 10 (t1) (thickness of the second layer / thickness of the first layer), i.e., t2 / t1, is preferably 0.56 or more and 2.2 or less. By manufacturing the test chip so that t2 / t1 is 0.56 or more and 2.2 or less, the desired flow channel structure can be more reliably formed in the obtained test chip. In particular, when the test chip is manufactured by the test chip manufacturing method described later, by manufacturing the test chip so that t2 / t1 is 0.56 or more and 2.2 or less, problems such as blockages when impregnating the sheet-like material with a hydrophobic material can be sufficiently avoided, and the speed and / or speed stability of the flow of the liquid from the liquid receiving part A to the detection confirmation part B can be effectively increased. From the same viewpoint, t2 / t1 is more than 1.0, that is, as shown in FIG. 15, it is more preferable that the thickness t2 of the second layer 20 is larger than the thickness t1 of the first layer 10, more preferably 1.3 or more, and even more preferably 1.8 or more. Furthermore, t2 / t1 is not particularly limited and can be set to 3.0 or less.
[0087] The above-mentioned test chip 1 can be manufactured, for example, by forming a predetermined portion (such as the detection confirmation portion B) on a sheet-like material to form the first layer 10, forming a predetermined portion (such as the liquid flow portion D) on another sheet-like material to form the second layer 20, and stacking these two sheet-like materials. Alternatively, the above-mentioned test chip 1 can be manufactured by forming a predetermined portion on a part of a sheet-like material to form the first layer 10, forming a predetermined portion on another part of the sheet-like material to form the second layer 20, and folding the sheet-like material while adjusting the positions of the first layer and the second layer. However, it is preferable to manufacture the test chip 1 of this embodiment by forming the first layer on one side of a sheet-like material and forming the second layer on the other side. The test chip of this embodiment, in which a first layer and a second layer are formed on both sides of a single sheet-like material, has various advantages, such as: (1) it avoids the trouble and cost of stacking (or folding); (2) the flow of the test liquid by capillary action is ensured between the first and second layers; and (3) it is easy to dispose of because no tools or the like are required to hold the stacked (or folded) sheet-like material. The test chip 1 in which the first layer and the second layer are formed on both sides of a single sheet-like material can be manufactured, for example, by a method for manufacturing a test chip, which will be described later.
[0088] (Method of manufacturing the test chip) A method for producing a test chip according to an embodiment of the present invention is a method for producing the test chip described above, a film forming step of forming a first hydrophobic film on a first substrate and a second hydrophobic film on a second substrate using a hydrophobic material; a first printing step of printing a first sacrificial substrate with a first hydrophobic film on the first substrate in a reverse design of a first layer of a test chip; a second printing step of printing a second sacrificial substrate with a second hydrophobic film on the second substrate in a reverse design of the second layer of the test chip; a first transfer step of transferring the first hydrophobic film after the first printing step onto one surface of a sheet-like material and impregnating the sheet-like material; a second transfer step of transferring the second hydrophobic film after the second printing step to the other surface of the one sheet-like material and impregnating the sheet-like material; The present invention is characterized by comprising: According to this manufacturing method, the above-mentioned test chip can be manufactured easily, highly accurately, and at low cost.
[0089] <Film formation process> In the film formation step, a first hydrophobic film is formed on a first substrate using a hydrophobic material, and a second hydrophobic film is formed on a second substrate.
[0090] A colorant can be blended into the hydrophobic material. A viscosity adjusting component (e.g., resin, etc.), a dispersion aid, a filler, etc. can be appropriately blended into the hydrophobic material. The hydrophobic material and the colorant are as described above with respect to the test chip.
[0091] The above-mentioned hydrophobic material is preferably heated and melted before forming the film. The heating temperature can be appropriately set in consideration of the melting points of the hydrophobic material and the viscosity adjusting component. In addition, the viscosity of the hydrophobic material when melted can be appropriately selected in consideration of the thickness and basis weight (density) of the sheet-like material to be used later, so that the sheet-like material can be impregnated with the hydrophobic material as desired.
[0092] The viscosity of the hydrophobic material is not particularly limited, but from the viewpoint of sufficiently avoiding problems such as blockage during impregnation, the viscosity is set to 140° C. and a shear rate of 3000 s -1 is preferably 100 mPa·s or less, more preferably 50 mPa·s or less, and even more preferably 30 mPa·s or less.
[0093] The first and second substrates are not components of the final test chip, but are one of the components used for manufacturing the test chip. For the first and second substrates, for example, polyesters such as polyethylene terephthalate (PET) and polyethylene naphthalate (PEN), polyphenylene sulfide (PPS), and films made of cellophane can be used. The first and second substrates may have any shape, such as a ribbon shape or a film shape. The first and second substrates may be the same substrate.
[0094] In the film forming step, the hydrophobic film can be formed on the first substrate and the second substrate by applying the above-mentioned hydrophobic material. It is preferable to heat and hold the first substrate and the second substrate before applying the hydrophobic material. The thickness of the first hydrophobic film and the second hydrophobic film to be formed can be appropriately selected in consideration of the thickness of the sheet-like material to be used later.
[0095] In particular, the ratio of the thickness (t2') of the second hydrophobic film to the thickness (t1') of the first hydrophobic film (thickness of the second hydrophobic film / thickness of the first hydrophobic film), i.e., t2' / t1', is preferably 0.56 or more and 2.2 or less. By setting t2' / t1' to 0.56 or more and 2.2 or less, problems such as blockages when impregnating a hydrophobic material into a sheet-like material in a later process can be sufficiently avoided, and the speed and / or speed stability of the liquid flow from the liquid receiving part A to the detection confirmation part B can be sufficiently increased. From the same viewpoint, t2' / t1' is more preferably more than 1.0, even more preferably 1.3 or more, and even more preferably 1.8 or more. In addition, t2' / t1' is not particularly limited, and can be 3.0 or less.
[0096] <First printing process and second printing process> In a first printing step, the first hydrophobic film formed on the first substrate is used to print a first sacrificial substrate, and in a second printing step, the second hydrophobic film formed on the second substrate is used to print a second sacrificial substrate.
[0097] The first sacrificial substrate and the second sacrificial substrate are not components of the final test chip, but are one of the components used for manufacturing the test chip. The first sacrificial substrate and the second sacrificial substrate are preferably versatile and can be printed with high precision, such as fine paper, coated paper, synthetic paper, etc. The first sacrificial substrate and the second sacrificial substrate may be the same substrate.
[0098] Printing on the first sacrificial substrate and printing on the second sacrificial substrate are not particularly limited, but for example, a label writer commonly used as an office product can be suitably used. In the first printing step, the first hydrophobic film on the first substrate is used to print on the first sacrificial substrate so as to form an inverted design of the first layer of the test chip. In the second printing step, the second hydrophobic film on the second substrate is used to print on the second sacrificial substrate so as to form an inverted design of the second layer of the test chip. In this regard, taking the manufacture of the test chip shown in FIG. 2 as an example, the design printed on the first sacrificial substrate is a design having a printed film corresponding to the liquid receiving portion A and the detection confirmation portion B. In addition, the design printed on the second sacrificial substrate is a design having a printed film corresponding to the liquid flow portion C, the liquid flow portion D, and the liquid flow path E.
[0099] The design to be printed may be created in advance using a personal computer or the like, and the data may be input to the printing device. The first printing step and the second printing step may be performed simultaneously.
[0100] <First transfer step and second transfer step> In the first transfer step, the first hydrophobic film after the first printing step is transferred to one side of one sheet-like material and is impregnated into the sheet-like material. In the second transfer step, the second hydrophobic film after the second printing step is transferred to the other side of the sheet-like material and is impregnated into the sheet-like material. This forms a first layer derived from the first hydrophobic film and a second layer derived from the second hydrophobic film.
[0101] A transfer device such as a laminator may be used for transferring the hydrophobic film. In addition, when transferring the first hydrophobic film onto the first substrate and the second hydrophobic film onto the second substrate, it is preferable to appropriately adjust the transfer positions of each film according to the design of the desired test chip.
[0102] The sheet-like material is as described above with respect to the material M.
[0103] The impregnation of the sheet-like material with the hydrophobic film can be achieved, for example, by heating. In this regard, for example, by using a transfer device such as a heatable laminator, both the transfer and the impregnation of the hydrophobic film can be performed.
[0104] Here, in the first transfer step and the second transfer step, the first hydrophobic film transferred from the first substrate and the second hydrophobic film transferred from the second substrate are at least partially in contact with each other in the material M by the above-mentioned impregnation. In other words, in a portion of the sheet-like material where the hydrophobic film is transferred to both sides in the thickness direction, the hydrophobic film is impregnated throughout the entire thickness direction. On the other hand, in a portion of the sheet-like material where the hydrophobic film is transferred only to one surface in the thickness direction, the hydrophobic film is not impregnated to the other surface. Such adjustment can be performed, for example, by appropriately adjusting the viscosity of the hydrophobic material, the thickness of the sheet-like material, the thickness of the hydrophobic film, etc.
[0105] In the first and second transfer steps, the transferred hydrophobic film can be entirely impregnated into the sheet-like material. In this case, the thickness of the sheet-like material hardly changes before and after the first and second transfer steps (however, there is a possibility that the thickness may decrease due to the effect of compression by a laminator, etc.).
[0106] The first transfer step may be performed before the second transfer step or after the second transfer step. Alternatively, the first transfer step and the second transfer step may be performed simultaneously. In that case, the sheet-like material can be sandwiched between the first substrate and the second substrate so that the hydrophobic film is in contact with the sheet-like material.
[0107] Furthermore, if the conditions of the first transfer process and the second transfer process are equivalent, the thickness ratio (t2 / t1) of the first layer and the second layer formed after impregnation is maintained from the thickness ratio (t2' / t1') of each hydrophobic film before impregnation.
[0108] After the first and second transfer steps, the first and second substrates can be peeled off as appropriate, thus finally obtaining the test chip of this embodiment.
[0109] In the manufacturing method of the test chip of this embodiment, the specified printing and transfer processes described above are performed, so that even if a sheet-like material with a relatively rough surface, such as commercially available filter paper, is used, there is little transfer failure or void occurrence, and the test chip can be manufactured with higher precision.
[0110] Furthermore, in the method for producing the test chip of this embodiment, the first and second layers having a desired design can be formed without using a mold or the like, making on-demand production possible.
[0111] Furthermore, in the manufacturing method of the test chip of this embodiment, the test chip can be manufactured by forming a first layer and a second layer on both sides of a single sheet-like material, respectively. Therefore, compared to, for example, a manufacturing method using two sheets of sheet-like material (or a manufacturing method by folding a single sheet-like material), this method has various advantages, such as: (1) the effort and cost of stacking (or folding) can be avoided; (2) the flow of the test liquid by capillary action is ensured between the first and second layers of the obtained test chip; and (3) since no tool or the like for maintaining the stacking (or folding) is required, the obtained test chip can be easily disposed of. EXAMPLES
[0112] Next, the present invention will be described more specifically with reference to examples and comparative examples, but the present invention is not limited to the following examples.
[0113] (Experiment 1) First, we investigated the effect of the design (channel structure) of the first and second layers of the test chip on color unevenness.
[0114] <Manufacturing of test chips> 48 parts by mass of paraffin wax (manufactured by Nippon Seiro Co., Ltd., "Paraffin Wax -155") as a hydrophobic material, 48 parts by mass of synthetic wax (manufactured by Mitsubishi Chemical Corporation, "Diacarna (registered trademark) 80") as a hydrophobic material, 2 parts by mass of ethylene-vinyl acetate copolymer resin (manufactured by Tosoh Corporation, "Ultrathene (registered trademark) 681"), and 2 parts by mass of carbon black (manufactured by Mitsubishi Chemical Corporation, "MA-100") as a colorant were blended and melt-mixed at 100°C. At that time, the components were dispersed using a sand mill. In this manner, a hydrophobic material was prepared.
[0115] A substrate (Toray Industries, Inc.'s "Lumirror (registered trademark) #5A-F531", polyester film, one side heat-resistant treated) was placed with the side that had not been heat-resistant facing up on a hot plate maintained at 120° C. Next, the above-mentioned hydrophobic material maintained in a molten state at 120° C. was applied to the substrate with a thickness of about 6 to 12 μm using a Mayer bar to form a ribbon-shaped hydrophobic film (first hydrophobic film and second hydrophobic film).
[0116] Next, using a label writer (King Jim Co., Ltd., "Tepra SR750"), the above-mentioned hydrophobic film was printed on the fine paper as the first sacrificial substrate so as to have the desired design created in advance on a personal computer. Similarly, the above-mentioned hydrophobic film was printed on the fine paper as the second sacrificial substrate so as to have the desired design created in advance on a personal computer. The above two designs printed on the fine paper correspond to the inverted designs of the front surface (first layer) and back surface (second layer) of the final test chip, respectively. The fine paper after printing is not particularly used in the subsequent process.
[0117] Here, in Comparative Example 1, the design of the front surface (first layer) and the design of the back surface (second layer) were as shown in Fig. 16. That is, in Comparative Example 1, the liquid receiving section A and the detection confirmation section B are connected by a liquid flow path on the front surface, and the designs of the front surface and the back surface are substantially the same. Also, in Examples 1-1 to 1-7, the designs of the front surface (first layer) and the back surface (second layer) were as shown in Figs. 2, 9, 10, 11, 12, 13, and 14, respectively.
[0118] Next, using the printed substrate, filter paper (Whatman grade 41) as sheet-like material M was sandwiched while appropriately adjusting the position so that the hydrophobic film was in contact with the filter paper. Then, using a laminator maintained at 90 ° C, the hydrophobic film was transferred to both sides of the filter paper at once. Each hydrophobic film was almost completely impregnated into the filter paper from both sides, and the filter paper portion directly below was hydrophobized. As a result, a first layer having a predetermined design was formed on the front side of the filter paper, and a second layer having a predetermined design was formed on the back side of the filter paper. In addition, in the part of the filter paper where the hydrophobic film was transferred to both sides in the thickness direction, the hydrophobic film was impregnated throughout the entire thickness direction, and in the part where the hydrophobic film was transferred to only one surface in the thickness direction, the impregnation was not allowed to reach the other surface. The substrates on both sides were then peeled off to finally obtain the test chip. Note that the first and second layers in all examples were derived from the same hydrophobic film, and therefore had the same thickness.
[0119] <Evaluation of color unevenness> Each of the obtained test chips was placed with the surface (first layer) facing up, and a mark was made with a water-based red highlighter pen in the center of the detection confirmation part B. Then, three drops of distilled water were dropped into the liquid receiving part A with a dropper, and the change in the red mark due to the flow of water was observed.
[0120] As a result, in Comparative Example 1 (FIG. 16), the red mark that was in the center of the detection confirmation part B moved to the periphery of the detection confirmation part B (especially the side farther from the liquid receiving part A), making it difficult to visually confirm the red color. Therefore, the test chip of Comparative Example 1 was found to have uneven color development, and therefore is not suitable for quantitative analysis.
[0121] In contrast, in Examples 1-1 to 1-7 (Figs. 2, 9 to 14), the highlighter mark at the center of detection confirmation section B remained inside the outer periphery of detection confirmation section B. In particular, in Examples 1-2 to 1-7 (Figs. 9 to 14), the highlighter mark at the center of detection confirmation section B remained closer to the center of detection confirmation section B. This is thought to be because, compared to Comparative Example 1, the liquid flow path has been optimized to allow water to flow three-dimensionally within the filter paper. Therefore, it is recognized that the test chips of Examples 1-1 to 1-7 have significantly reduced color unevenness, and therefore quantitative analysis can be expected.
[0122] (Experiment 2) Next, the relationship between the thicknesses of the first and second layers that can ensure good liquid flowability was examined.
[0123] A hydrophobic material (ink) was prepared according to the formulation shown in Table 1. [Table 1]
[0124] *1 Paraffin wax: "Paraffin Wax -135" manufactured by Nippon Seiro Co., Ltd. *2 Synthetic wax: "Diacarna (registered trademark) 30" manufactured by Mitsubishi Chemical Corporation *3 Carbon black: "MA-100" manufactured by Mitsubishi Chemical Corporation *4 Resin: Tosoh Corporation's "Ultrathene (registered trademark) 722"
[0125] A test chip was obtained in a manner similar to that described above, except that ink 1 or ink 2 was used as the hydrophobic material, Whatman grade 41 (filter paper #41) or Whatman grade 40 (filter paper #40) was used as the filter paper (material M), and the temperature of the laminator was appropriately adjusted. At that time, the design of the first layer and the second layer was as shown in FIG. 11. At that time, the thickness of the first hydrophobic film used to form the first layer and the second hydrophobic film used to form the second layer (corresponding to the ratio of the thicknesses of the first layer and the second layer) was appropriately changed.
[0126] Each of the obtained test chips was placed with the surface (first layer) facing up. Next, about 0.3 mL of a solution of aqueous fluorescent ink dissolved in distilled water was dropped with a dropper into the liquid receiving part A, and the time (flow time) from the start of the drop to the time the liquid reached the detection confirmation part B was measured. The same measurement was performed eight times, and the average value and standard deviation were calculated. The results are shown in Tables 2 to 5 for each combination of hydrophobic material and filter paper.
[0127] [Table 2]
[0128] [Table 3]
[0129] [Table 4]
[0130] [Table 5]
[0131] It can be said that the liquid flowability is good in all of the examples in Tables 2 to 5. From this, it can be considered that good liquid flowability can be ensured as long as the ratio of the thickness of the second layer to the thickness of the first layer (thickness of the second layer / thickness of the first layer) is at least within the range of 0.56 to 2.2.
[0132] (Experiment 3) Next, the impregnation rate of the hydrophobic material that can ensure good liquid flowability was examined.
[0133] The same filter paper (filter paper #41 or filter paper #40) used in Experiment 2 was cut to a size of 5 cm x 2 cm, dried at 120°C for 3 minutes, and the dry mass M0 (g) was measured. The filter paper was then immersed in the same hydrophobic material (ink 1 or ink 2) used in Experiment 2 and left at 120°C for 3 minutes. After immersion, the filter paper was sandwiched between the same type of filter paper and a slide glass and left at 120°C for 1 minute under a load of 100 gf to remove excess hydrophobic material. The mass M1 (g) of the filter paper was then measured. The maximum impregnation amount per unit area P was then calculated from (M1-M0) x 1000. max (g / m 2 ) was calculated.
[0134] In each of Tables 2 to 5, the examples in which the total thickness of the first hydrophobic film and the second hydrophobic film is the smallest and the largest are selected, respectively, and the actual impregnation amount P (g / m) per unit area in the selected examples is calculated using the ink density listed in Table 1. 2 ) was calculated. Then, (P / P max The impregnation rate (%) of the hydrophobic material into the filter paper was calculated by multiplying the impregnation rate (%) by 100. The results are shown in Table 6.
[0135] [Table 6]
[0136] From Table 6, it can be considered that as long as the impregnation rate of the hydrophobic material is within the range of at least about 14% to 32%, good liquid flowability can be ensured. [Industrial Applicability]
[0137] According to the present invention, a test chip in which a target substance contained in a test liquid reacts with a labeling medium previously prepared and the presence of the target substance is confirmed by the color produced by the reaction can be provided, in which color unevenness is significantly suppressed. Also, according to the present invention, a method for producing the test chip described above can be provided, which can easily, highly accurately, and at low cost. [Explanation of symbols]
[0138] 1. Test chip 10 1st layer 10' Pre 1st layer 20 2nd layer 20' Pre 2nd layer 50 Hydrophobic Materials A Liquid receiving part B Detection confirmation section C, D liquid flow section D' Liquid non-flow area E, E1, E2, E3, E4, E31, E32 Liquid flow path F Liquid flow path M: Material in which the flow of the test liquid is expressed M' Material that does not allow the test liquid to flow X, Y liquid non-flow area
Claims
1. A sheet-shaped test chip, A first layer on the front side and a second layer on the back side, the first layer and the second layer are adjacent; Either the first layer or the second layer has a liquid receiving portion A, The first layer has at least a detection confirmation portion B, The second layer has at least a liquid flow section D adjacent to the detection confirmation section B and a liquid flow path E connected to the liquid flow section D, When the first layer has a liquid receiving portion A, the liquid receiving portion A is separated from the detection confirmation portion B, When a test liquid is dropped onto the liquid receiving section A, the test liquid flows to the detection confirmation section B by capillary action through the liquid receiving section A, the liquid flow path E, and the liquid flow section D in this order, An inspection chip, characterized in that the first layer is formed on one surface of a sheet-like material, and the second layer is formed on the other surface of the sheet-like material.
2. A sheet-shaped test chip, A first layer on the front side and a second layer on the back side, the first layer and the second layer are adjacent; Either the first layer or the second layer has a liquid receiving portion A, The first layer has at least a detection confirmation portion B, The second layer has at least a liquid flow section D adjacent to the detection confirmation section B and a liquid flow path E connected to the liquid flow section D, When the first layer has a liquid receiving portion A, the liquid receiving portion A is separated from the detection confirmation portion B, When a test liquid is dropped onto the liquid receiving section A, the test liquid flows to the detection confirmation section B by capillary action through the liquid receiving section A, the liquid flow path E, and the liquid flow section D in this order, The test chip is characterized in that the liquid flow section D has a ring-shaped structure with a liquid non-flow section D' formed inside.
3. A sheet-shaped test chip, A first layer on the front side and a second layer on the back side, the first layer and the second layer are adjacent; Either the first layer or the second layer has a liquid receiving portion A, The first layer has at least a detection confirmation portion B, The second layer has at least a liquid flow section D adjacent to the detection confirmation section B and a liquid flow path E connected to the liquid flow section D, When the first layer has a liquid receiving portion A, the liquid receiving portion A is separated from the detection confirmation portion B, When a test liquid is dropped onto the liquid receiving section A, the test liquid flows to the detection confirmation section B by capillary action through the liquid receiving section A, the liquid flow path E, and the liquid flow section D in this order, The test chip according to claim 1, wherein the number of liquid flow paths E connected to each liquid distribution portion D in the second layer is more than one.
4. The test chip according to claim 3 , wherein at least two of said liquid flow paths E are connected to said liquid circulation portion D so as to face each other.
5. The test chip according to claim 3 , wherein at least two of said liquid flow paths E have substantially the same shape.
6. The first layer has the liquid receiving portion A spaced apart from the detection confirmation portion B, The second layer has a liquid flow section C adjacent to the liquid receiving section A, The test chip according to any one of claims 1 to 5, wherein when a test liquid is dropped into the liquid receiving section A, the test liquid flows by capillary action through the liquid receiving section A, the liquid flow section C, the liquid flow path E and the liquid flow section D in this order to the detection confirmation section B.
7. the first layer has the liquid receiving portion A separated from the detection confirmation portion B, and further has a liquid flow path F connected to the liquid receiving portion A; The test chip according to any one of claims 1 to 5, wherein when a test liquid is dropped into the liquid receiving section A, the test liquid flows by capillary action through the liquid receiving section A, the liquid flow path F, the liquid flow path E and the liquid flow section D in this order to the detection confirmation section B.
8. The test chip according to any one of claims 1 to 5, wherein the second layer has the liquid receiving portion A.
9. the liquid receiving portion A, the liquid flow portion C, the liquid flow path E, the liquid flow portion D, and the detection confirmation portion B are made of a material M in which the flow of the test liquid is manifested by capillary action; 7. The test chip according to claim 6, wherein the portion other than said material M is made of a material M' which is obtained by impregnating said material M with a hydrophobic material and through which the test liquid does not pass.
10. The liquid receiving portion A, the liquid flow path F, the liquid flow path E, the liquid flow portion D, and the detection confirmation portion B are made of a material M in which the flow of the test liquid is manifested by capillary action, 8. The test chip according to claim 7, wherein the portion other than said material M is made of a material M' which is obtained by impregnating said material M with a hydrophobic material and through which the test liquid does not flow.
11. The test chip according to claim 9 or 10, wherein the material M is filter paper.
12. 12. The test chip according to claim 9, wherein an impregnation rate of said hydrophobic material into said material M' is 14% or more and 32% or less.
13. The test chip according to any one of claims 1 to 12, wherein the ratio of the thickness of the second layer to the thickness of the first layer (thickness of the second layer / thickness of the first layer) is 0.56 or more and 2.2 or less.
14. The test chip according to any one of claims 1 to 13, wherein a color reaction caused by a substance to be detected occurs in said detection confirmation part B.
15. A method for producing the test chip according to any one of claims 1 to 14, comprising the steps of: a film forming step of forming a first hydrophobic film on a first substrate and a second hydrophobic film on a second substrate using a hydrophobic material; a first printing step of printing a first sacrificial substrate with a first hydrophobic film on the first substrate in a reverse design of a first layer of a test chip; a second printing step of printing a second sacrificial substrate with a second hydrophobic film on the second substrate in a reverse design of the second layer of the test chip; a first transfer step of transferring the first hydrophobic film after the first printing step onto one surface of a sheet-like material and impregnating the sheet-like material; a second transfer step of transferring the second hydrophobic film after the second printing step to the other surface of the one sheet-like material and impregnating the sheet-like material; A method for manufacturing an inspection chip, comprising:
16. 16. The method for manufacturing a test chip according to claim 15, wherein a ratio of a thickness of the second hydrophobic film to a thickness of the first hydrophobic film (thickness of the second hydrophobic film / thickness of the first hydrophobic film) is 0.56 or more and 2.2 or less.
Citation Information
Patent Citations
Three-dimensional paper chip based on thin double-sided adhesive tape and laminating technology and preparation method of three-dimensional paper chip
CN107899626A
Three -dimensional paper base core piece
CN208465907U
Dielectric cytometry device and cell sorting method using dielectric cytometry
JP2012098063A
Method of monitoring cell motility and chemotaxis
US20030022269A1
Lateral Flow and Flow-through Bioassay Devices Based On Patterned Porous Media, Methods of Making Same, and Methods of Using Same
US20090298191A1