METHOD FOR MACHINING A METAL-CERAMIC SUBSTRATE AND METAL-CERAMIC SUBSTRATE - Patent application

The method for machining metal-ceramic substrates with controlled depth variations and temperature management addresses the issue of accidental breakage during transport, ensuring stable and efficient separation of metal-ceramic substrates.

JP7564380B2Active Publication Date: 2024-10-08ROGERS GERMANY
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2023553410
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-03-03
Filing Date
2022-03-02
Publication Date
2024-10-08
Estimated Expiration
2042-03-02

AI Technical Summary

Technical Problem

Existing methods for creating predetermined break points in metal-ceramic substrates, such as master cards, often result in accidental damage during transport due to insufficient stability and unintended breakage.

Method used

A method for machining metal-ceramic substrates involves forming a predetermined breaking point with distinct first and second depths, ensuring stability and controlled breakage by adjusting the bottom of the break point with specific depth ratios and orientations, using ultrashort pulse lasers and temperature control.

Benefits of technology

This approach enhances the stability of metal-ceramic substrates during transport, reducing accidental damage and improving the efficiency of separation, while maintaining structural integrity and thermal resistance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007564380000001
    Figure 0007564380000001
  • Figure 0007564380000002
    Figure 0007564380000002
  • Figure 0007564380000003
    Figure 0007564380000003
Patent Text Reader

Abstract

A method for machining a metal-ceramic substrate (1), in particular for forming a predetermined breaking point, comprising providing a metal-ceramic substrate (1) and forming a predetermined breaking point (7) in the metal-ceramic substrate (1), the predetermined breaking point (7) having, along its direction (V), at least a first portion (A1) having a first depth (T1) and at least a second portion (A2) having a second depth (T2), the second depth (T2) being different from the first depth (T1).
Need to check novelty before this filing date? Find Prior Art

Description

[Technical Field]

[0001] The present invention relates to a method for machining a metal-ceramic substrate and to a metal-ceramic substrate having a predetermined break point. [Background technology]

[0002] Electronic modules, for example power electronic modules, are well known from the prior art. Such electronic modules typically use switchable or controllable electronic components interconnected via conductive tracks on a shared metal-ceramic substrate. The essential components of the metal-ceramic substrate are an insulating layer, which in the case of a metal-ceramic substrate is made from a material that comprises ceramic, and a metallization layer, which is preferably structured on one component side of the metal-ceramic substrate and configured to form conductive paths.

[0003] Typically, the metal-ceramic substrate is realized as a master card, which is separated into smaller metal-ceramic substrates after or before structuring. Such a master card is treated with laser light to generate predetermined break and / or separation points. The individual metal-ceramic substrates can then be separated from the master card, for example, by separating them. Here, the use of ultrashort pulsed lasers has proven advantageous, as described, for example, in US Pat. No. 6,299,499. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] International Publication No. 2017 / 108950 Summary of the Invention

[0005] Based on this prior art, the present invention aims to improve the production of predetermined breaking points in metal-ceramic substrates, in particular master cards. [Problem to be solved by the invention]

[0006] This problem is solved by a method for machining a metal-ceramic substrate according to claim 1 and by a metal-ceramic substrate according to claim 10. Further embodiments can be found in the subsequent claims and in the description. [Means for solving the problem]

[0007] According to a first aspect of the present invention, a method for machining a metal-ceramic substrate comprises the steps of: Providing a metal ceramic substrate; forming a predetermined break point in the metal ceramic substrate; Including, The predetermined breaking point has at least a first portion having a first depth and at least a second portion having a second depth along the direction, the second depth being different from the first depth.

[0008] In contrast to the predetermined breaking point known in the prior art, the present invention realizes that the first and second sections provide a first and second depth relative to the predetermined breaking point, thereby adjusting the bottom of the predetermined breaking point toward the predetermined breaking point. Accordingly, by adjusting the bottom of the predetermined breaking point, particularly by using a first section having a first depth and a second section having a second depth different from the first depth, it is possible to break the corresponding metal-ceramic substrate as completely as possible while also providing the desired stability, thereby ensuring safe transport without unintentional breakage of the metal-ceramic substrate during transport, especially in the area of ​​the predetermined breaking point. This reduces the total amount of rejected metal-ceramic substrates accidentally damaged by unintentional or accidental breakage. These are preferably metal-ceramic substrates in the form of master cards.

[0009] In particular, the first and / or second depths are intended to be measured from the bottom of the predetermined breakpoint in the first and second sections, respectively, to an imaginary plane extending perpendicularly to the main extension plane, also extending above the metal-ceramic substrate or ceramic layer. The first and second sections refer in particular to sections at the bottom of the predetermined breakpoint that do not have an obliquely inclined course relative to the main extension plane. In this context, the first and / or second sections may also be point-shaped in each case, especially if the second section is immediately followed by an obliquely extending bottom. For example, they may have a zigzag-shaped course at the bottom of the predetermined breakpoint. Preferably, between the first and second sections, an inclined region is provided in each case in which the bottom of the predetermined breakpoint extends obliquely relative to the main extension plane.

[0010] In other words, the first and second sections do not include sections of the predetermined breaking point where the base of the predetermined breaking point extends obliquely relative to the main extension plane. The parts of the base of the predetermined breaking point that are not counted as the first and second sections, i.e., the inclined parts, may extend, for example, perpendicular to the main extension plane and / or at an angle of 30° to 60°, preferably 40° to 50°, more preferably 42° to 48° relative to the main extension plane. In particular, each obliquely extending section of the base of the predetermined breaking point forms an essentially constant inclination along its extension direction, i.e., in particular, does not deviate from the average value of all inclination angles by more than 10%, preferably 5%, more preferably 2%.

[0011] Preferably, the first depth has a value between 0.01 mm and 0.12 mm, preferably between 0.02 mm and 0.1 mm, more preferably between 0.02 mm and 0.08 mm, while the second depth has a value between 0.01 mm and 0.16 mm, preferably between 0.02 mm and 0.12 mm, more preferably between 0.02 mm and 0.1 mm.

[0012] Furthermore, the metal-ceramic substrate comprises at least one metal layer bonded to the upper side of the ceramic element or layer, the metal layer and the ceramic element extending along the main extension plane and arranged one above the other along a stacking direction extending perpendicular to the main extension plane.

[0013] Possible materials for the metal layer are copper, aluminum, molybdenum, tungsten and / or their alloys, such as, for example, CuZr, AlSi or AlMgSi, as well as laminates, such as, for example, CuW, CuMo, CuAl and / or AlCu, or MMCs (metal matrix composites), such as, for example, CuW, CuMo or AlSiC. Furthermore, the metal layer on the produced metal-ceramic substrate is preferably surface-modified, in particular as a structural metallization. As surface modification, for example, sealing with noble metals, in particular silver and / or gold, or (electroless) nickel or ENIG ("electroless nickel immersion gold"), or edge encapsulation on the metal layer to suppress crack formation or expansion, are conceivable.

[0014] Preferably, the ceramic element comprises Al2O3, Si3N4, AlN, HPSX ceramic (i.e., a ceramic with an Al2O3 matrix consisting of x percentage of ZrO2, e.g., Al2O3 with 9% ZrO2=HPS9 or Al2O3 with 25% ZrO2=HPS25), SiC, BeO, MgO, high-density MgO (more than 90% of theoretical density), or TSZ (tetragonal stabilized zirconium oxide). The ceramic element may also be configured as a composite or hybrid ceramic, in which several ceramic layers, each differing in terms of material composition, are placed one on top of the other and bonded to form the ceramic element in order to combine various desired properties. Preferably, a ceramic is used that is as thermally conductive as possible in order to achieve the lowest possible thermal resistance.

[0015] Preferably, the metal layer is bonded to the insulating layer by an AMB process and / or a DCB process and / or hot isostatic pressing. Bonding by a diffusion bonding process or by a thick film coating process is also conceivable.

[0016] Those skilled in the art will understand that the "DCB process" (direct copper bonding technology) or "DAB process" (direct aluminum bonding technology) refers to such a process used to bond metal layers or sheets (e.g., copper sheets or foils, or aluminum sheets or foils) to each other and / or to ceramic or ceramic layers, for example, by using a metal or copper sheet or metal or copper foil having a layer or coating (fusing layer) on the surface side. In this process, described for example in U.S. Pat. No. 3,744,120 or German Patent No. 2,319,854, this layer or coating (fusing layer) forms a eutectic at a melting temperature lower than that of the metal (e.g., copper), so that by placing the foil on the ceramic and heating all layers, they can be bonded to each other by melting the metal or copper essentially only in the region of the fusing layer or oxide layer.

[0017] Specifically, the DCB process involves, for example: - oxidizing the copper foil so that a uniform copper oxide layer is formed; - Placing copper foil on the ceramic layer; heating the composite to a process temperature of between about 1025°C and 1083°C, e.g., about 1071°C; -cooling to ambient temperature, The process has the above steps.

[0018] For example, an active solder process for joining a metal layer or foil, particularly a copper layer or foil, to a ceramic material is understood to be a process particularly used in the manufacture of metal-ceramic substrates. The bond is formed between a metal foil, such as a copper foil, and a ceramic substrate, such as an aluminum nitride ceramic, at a temperature between approximately 650 and 1000°C using a solder containing an active metal in addition to the main components, such as copper, silver, and / or gold. The active metal is, for example, at least one element from the Hf, Ti, Zr, Nb, or Ce group, and establishes a bond between the brazing solder and the ceramic through a chemical reaction. The bond between the brazing solder and the metal is a metal brazing solder joint. Alternatively, a thick coating process is also considered for the bonding.

[0019] In hot isostatic pressing, the container, particularly the metal container, is preferably subjected in a heated and pressurized apparatus to a gas pressure of 100 to 2000 bar (10 to 200 MPa), preferably 150 to 1200 bar (15 to 120 MPa), more preferably 300 to 1000 bar (30 to 100 MPa), and a process temperature of up to 300°C, up to the melting temperature of the metal layer and / or further metal layer, particularly below the melting temperature of the metal layer and / or further metal layer. It has thus been found advantageously possible to bond the metal layer, i.e., the metal layer and / or further metal layer of the metal container, to the ceramic element without reaching the temperatures required for direct metal joining processes, such as the DCB or DAB process, and / or without the solder substrate used for active soldering. Furthermore, the use or advantage of an appropriate gas pressure may allow for the production of metal-ceramic substrates that are as void-free as possible, i.e., without the inclusion of gas between the metal layer and the ceramic element. In particular, the process parameters described in DE 10 2013 113 734 A1 and explicitly referred to in connection with hot isostatic pressing are used.

[0020] Preferably, the particles generated during the generation of the predetermined break point are sucked by a suction device. Such a suction device generates a suction flow that is specifically designed to suck the ceramic particles, especially those generated by sublimation, from the upper side of the metal-ceramic substrate during the treatment. Preferably, in this case, the suction device is arranged essentially at the level of the metal-ceramic substrate and directs the suction flow essentially parallel to the main extension plane of the substrate, especially near the substrate surface. As a result, the ceramic particles formed by sublimation are sucked laterally during the treatment with the laser pulses.

[0021] Preferably, the metal-ceramic substrate is positioned stationary during the formation of the predetermined break point, and / or the laser beam moves over the metal-ceramic substrate to form the predetermined break point. That is, the metal-ceramic substrate is preferably positioned stationary during the process in order to generate the predetermined break point for separating the metal-ceramic substrate. "Stationary" means fixed in a desired location or rotatably / pivotally fixed in a desired location. For this purpose, the metal-ceramic substrate, preferably provided as a master card, is fixed in a holding element. Such a holding element may, for example, comprise a suction device below the metal-ceramic substrate, which fixes the metal-ceramic substrate in the holding element during the process by means of a corresponding vacuum. Positioning the metal-ceramic substrate stationary or stationary during the generation of the predetermined break point advantageously allows for the generation of a finely structured and precisely shaped predetermined break point, especially when multiple passes of the laser beam are performed over the metal-ceramic substrate. Preferably, the laser beam of the UKP system moves along the planned course of the predetermined break point, preferably making several passes. The laser beam traversing the metal-ceramic substrate has a processing speed of between 0.1 and 2 m per second, preferably between 0.8 and 1.5 m per second.

[0022] Preferably, the first and second sections are realized outside the intersection of the two predetermined breaking points, thereby ensuring a favorable fracture behavior throughout the entire master card, and the targeted weakening is not set only in the area of ​​the intersections located above and below. In particular, it is intended that the first or second sections are not formed only at the intersections of the two predetermined breaking points. In particular, in order to divide the master card into a checkerboard pattern by the predetermined breaking points, the predetermined breaking points that intersect at the intersections run perpendicular to each other.

[0023] Preferably, the ratio of the first depth T1 to the second depth T2 is between 0.05 and 1, preferably between 0.2 and 0.8, more preferably between 0.4 and 0.6. In particular, it has been found that at a second depth that is approximately twice as large as the first depth, a metal-ceramic substrate can be provided that has a predetermined breaking point that is particularly suitable for handling, while at the same time having a sufficiently good breaking behavior along the predetermined breaking point.

[0024] Furthermore, it is particularly preferred that the first depth of the first section remains substantially constant over a first length dimensioned in the direction of the predetermined break point, and / or the second depth of the second section remains substantially constant over a second length dimensioned in the direction of the predetermined break point. The generation of corresponding adjustments, in particular where the first length and / or the second length are constant over a period of time, can be achieved quickly and without great effort.

[0025] Preferably, the first length has a value between 0.05 mm and 5.0 mm, preferably between 0.05 mm and 2.0 mm, more preferably between 0.05 mm and 0.01 mm, while the second length has a value between 0.05 mm and 5.0 mm, preferably between 0.05 mm and 2.0 mm, more preferably between 0.05 mm and 0.01 mm.

[0026] Furthermore, it is particularly preferred that the ratio of the first length to the second length is less than 1.5, preferably less than 0.5, and more preferably less than 0.25. It is particularly preferred to realize that the first length is approximately equal to the second length, so that, with respect to its adjustment, a particularly symmetrical course of the bottom of the predetermined breaking point is obtained. In particular, the spacing also includes a ratio in which the first section is point-shaped, and therefore the ratio is substantially 0. In these embodiments, the bottom section is perpendicular to the main extension plane and forms a substantially triangular shape in a cross section passing through the direction of the section.

[0027] It is particularly preferred if predetermined breaking points are generated on the upper and lower metal-ceramic substrates, which are arranged substantially coincident with one another in a direction extending perpendicular to the main extension plane, in this connection it is conceivable that the upper first and second sections are arranged in the same position or offset relative to the corresponding lower first and second sections in said direction.

[0028] Preferably, the first and second sections are provided so as to alternate periodically, in other words, the first and second sections alternate continuously along the direction, away from the connecting inclined course of the arch at the predetermined breaking point. Preferably, an inclined area is formed between the first and second sections.

[0029] Preferably, the predetermined break point has a third depth in a direction perpendicular to the direction, preferably different from the first and / or second depths, thereby forming, for example, a W-shape or W-shaped profile of the predetermined break point in a plane or cross section perpendicular to the direction. Such an increase in depth can be achieved, for example, by slightly offsetting the laser beam between several passes relative to further passes by the laser beam that lead to the formation of the predetermined break point.

[0030] Preferably, the predetermined breaking point in the first section or the second section has a trapezoidal or triangular shape in a plane parallel to the direction, which results in a substantially advantageous bottom section for the predetermined breaking point.

[0031] Preferably, the predetermined breaking point is produced by machining with laser light, in particular with an ultrashort pulse laser, and in the course of forming the predetermined breaking point the metal-ceramic substrate is subjected to a temperature treatment before, during and / or after the machining, in particular cooling, in particular after the machining, at a cooling rate of less than 4°C / min, preferably less than 2°C / min, more preferably less than 0.5°C / min. It has been found that a targeted temperature treatment, in particular a targeted cooling of the metal-ceramic substrate, can prevent thermomechanical stresses in the produced metal-ceramic substrate and can permanently improve the thermal shock resistance of the broken metal-ceramic substrate.

[0032] Preferably, a UKP laser is used as the laser source, providing optical pulses with a pulse duration of 0.1 to 800 ps, ​​preferably 1 to 500 ps, ​​and more preferably 10 to 50 ps. It has proven particularly advantageous to generate predetermined fracture points with such pulses, particularly at processing speeds between 0.2 and 8 m / s, which have a particularly favorable ratio between molten ceramic and crack formation within the predetermined fracture point, thereby ensuring particularly reliable or successful fracture along the predetermined fracture point without damage to the selected metal-ceramic substrate during fracture. In particular, compared to processing with a CO laser, this method reduces stresses on the metal-ceramic substrate, which can affect the mechanical properties of the ceramic and otherwise easily expand due to the metallization of the metal-ceramic substrate. This can lead to scrapping or at least affect the service life of the metal-ceramic substrate. This effect of using ultrashort pulsed laser light has been shown to be particularly pronounced when the use of pulsed laser light is accompanied by a temperature treatment. In particular, the success rate of fracture of the metal-ceramic substrate can be further improved.

[0033] Another object of the invention is a metal-ceramic substrate with a predetermined breaking point, manufactured by the process according to the invention. All of the properties and advantages described for the method apply equally to the metal-ceramic substrate. In particular, the metal-ceramic substrate is identified, in particular as a master card, by having a first portion with a first depth and a second portion with a second depth, the first depth being different from the second depth.

[0034] Further advantages and features will become apparent from the following description of preferred embodiments of the subject matter of the present invention, with reference to the accompanying drawings, in which: Figure 1 is a perspective view of a device for carrying out a method of manufacturing a device according to the present invention; [Brief explanation of the drawings]

[0035] [Figure 1] 1 is a schematic diagram of a process for machining a metal-ceramic substrate according to a first exemplary embodiment of the present invention; [Figure 2a] FIG. 1 illustrates a predetermined break point according to the prior art. [Figure 2b] FIG. 10 illustrates a predetermined break point according to a second exemplary embodiment of the present invention. [Figure 2c] FIG. 10 illustrates a predetermined break point according to a third exemplary embodiment of the present invention. DETAILED DESCRIPTION OF THE INVENTION

[0036] FIG. 1 schematically illustrates a method for machining a metal-ceramic substrate 1 according to a first exemplary embodiment of the present invention. Such a metal-ceramic substrate 1 preferably serves as a carrier for electronic or electrical components, which may be connected to the metal-ceramic substrate 1. Essential components of such a metal-ceramic substrate 1 are a ceramic layer or ceramic element extending along the main extension surface HSE and a metal layer bonded to the ceramic layer. The ceramic layer is made of at least one material, including ceramic. In this case, the metal and ceramic layers are arranged one above the other along a stacking direction extending perpendicular to the main extension surface HSE and are firmly bonded in the manufactured state via the bonding surface in at least some areas. Preferably, the metal layer is then structured to form conductive paths or connection points for the electrical components. For example, this structuring is etched into the metal layer. However, a permanent bond, particularly a firmly bonded bond, must first be formed between the metal and ceramic layers.

[0037] A system for manufacturing a metal-ceramic substrate, particularly in a DCB or DAB bonding process, for permanently bonding a metal layer to a ceramic layer includes a furnace for heating a laminate of a ceramic layer and at least one metal layer, thus achieving bonding. For example, the metal layer is made of copper, and the metal layer and the ceramic layer are bonded to each other using a DCB (direct copper bonding) process. Alternatively, the metal layer can be bonded to the ceramic layer using an active soldering process or a thick film process. Bonding by a hot isostatic pressing process or by diffusion bonding is also conceivable.

[0038] After bonding, particularly by a DCB process, an active soldering process, a diffusion bonding process, a hot isostatic pressing process, and / or a thick-film coating process, the metal-ceramic substrate 1 is provided as a master card. Such a master card is then subsequently singulated to provide the singulated metal-ceramic substrate 1. For this separation, it is preferable to treat the master card with laser light 10, particularly ultrashort-pulse laser light. This allows for immediate separation by the laser light 10 and / or the formation of predetermined break points 7 along which the master card is subsequently cut to form the singulated metal-ceramic substrate 1. For ultrashort-pulse lasers, those skilled in the art will recognize, in particular, laser sources that emit laser pulses whose pulse length is less than nanoseconds. Preferably, the pulse duration is between 0.1 and 100 ps. Pulse durations in the femtosecond range, i.e., pulse lengths between 0.1 and 100 fs, are also conceivable. Alternatively, the use of a CO laser is also conceivable. In the exemplary embodiment shown in FIG. 1, the metal-ceramic substrate 1 is arranged in a holding element 40 .

[0039] In particular, the metal-ceramic substrate 1 is intended to be fixed in place by the holding element 40. In particular, the laser beam 10 is moved over the metal-ceramic substrate 1 to generate predetermined break points 7u having a specific course along the direction V on the metal-ceramic substrate 1. In other words, instead of moving or aligning the metal-ceramic substrate 1 relative to the laser beam 10, it is preferable to align the laser beam 10 so that the moving laser beam 10 over the metal-ceramic substrate 1 generates predetermined break points 7 and / or cutting lines at each irradiation point. The predetermined break points 7 may be continuous and / or intermittent, i.e., the predetermined break points 7 may exist as perforations. In this case, the laser beam 10 moving over the metal-ceramic substrate 1 has a processing speed of 0.1 to 2 m / s, preferably 0.8 to 1.5 m / s. Alternatively, the metal-ceramic substrate 1 may be displaced to change the position of the laser beam 10 irradiating the metal-ceramic substrate 1.

[0040] In particular, in order to align the laser beam 10, it is considered that the laser beam 10 is directed to a mirror element 30. After being reflected by the mirror element 30, the laser beam 10 is irradiated onto the metal-ceramic substrate 1. In this connection, it is particularly realized that the mirror element 30 is pivotally mounted, in particular pivotally mounted around at least two axes, in order to align the laser beam 10 with a specific processing area or specific areas on the metal-ceramic substrate 1. Furthermore, it is preferable to arrange a lens 20, preferably an f-theta lens, between the mirror element 30 and the metal-ceramic substrate 1. In particular, the lens 20 extends, in particular as a master card, over a length corresponding to the length and / or width of the metal-ceramic substrate 1, substantially along a plane substantially perpendicular to the irradiation direction of the laser beam 10. In other words, the laser beam 10 traveling over the metal-ceramic substrate 1 always passes through the same lens 20, regardless of the processing area.

[0041] It has been found to be particularly advantageous to use a lens 20 with a focal length greater than 300 mm, preferably greater than 350 mm, and particularly preferably greater than 420 mm. By positioning the lens 20 at a distance from the metal-ceramic substrate 1 that essentially corresponds to the focal length of the lens 20, it becomes possible to form the predetermined break point or predetermined break recess 7 at a relatively slight inclination relative to the vertical direction perpendicular to the main extension surface HSE of the metal-ceramic substrate 1. Otherwise, it would be necessary to allow for an inclination angle that would essentially result in a V-shaped or notch-shaped predetermined break point 7. This applies in particular to predetermined break points 7 formed at the edge of the metal-ceramic substrate 1. Such an inclined position is caused, in particular, by the fact that the laser light 10 or laser beam cannot be uniformly irradiated perpendicularly onto the metal-ceramic substrate 1 so as to be visible across the entire area of ​​the metal-ceramic substrate 1.

[0042] However, by using a focal length of more than 300 mm, this tilt, particularly in the edge regions of the metal-ceramic substrate 1, is reduced so that the tilt angle, measured or referenced to the normal of the metal-ceramic substrate 1, is less than 12°, particularly preferably less than 10°. In particular, it can be seen that the deviation of the tilt angle compared to the direction of the predetermined breaking point 7 in the center of the metal-ceramic substrate 1 is not more than 12°. It is therefore advantageously possible to form predetermined breaking points 7 whose breaking behavior is substantially uniformly distributed over the entire metal-ceramic substrate 1.

[0043] Also provided is a suction device 25, which is arranged laterally offset from the metal-ceramic substrate 1 or the holding element 40. The suction device 25 has an opening through which gas can be sucked. In particular, the suction device 25 serves to ensure that sublimated particles are sucked from the surface or upper side of the metal-ceramic substrate 1 during the machining process. These sublimated ceramic particles are the result of plasma formation or a plasma flame 6 that is generated during the treatment of the metal-ceramic substrate 1 with ultrashort pulsed laser light. In addition to a lateral arrangement, an arrangement of the suction device 25 above the metal-ceramic substrate 1 to be divided is also conceivable, with its opening directed towards the metal-ceramic substrate 1.

[0044] In particular, it is realized that the metal-ceramic substrate 1 is subjected to a temperature treatment before and / or during and / or after machining with the laser beam 10 in the course of generating the predetermined fracture point 7. In particular, the temperature treatment is configured to control the temperature development in the metal-ceramic substrate 1 so as to avoid sudden or strong temperature changes. This advantageously reduces the formation of thermomechanically induced stresses in the metal-ceramic substrate 1. This leads to the fact that the thermal shock resistance of the produced, in particular split, metal-ceramic substrate 1 can be improved and the tendency to shell fracture, in particular the tendency to vertically extending cracks, can be reduced.

[0045] In particular, those skilled in the art will understand that by "during the process of creating the predetermined break point" the temperature increase occurs due to machining with the laser beam 10, and does not refer to temperature increases that occurred previously, such as when joining a metal layer to a ceramic layer during a DCB process and / or an active soldering process, or during heat generation after fabrication of the metal-ceramic substrate 1, such as during operation. To this end, for example, heating of the metal-ceramic substrate 1 occurs within 15 minutes, preferably within 10 minutes, and more preferably within 5 minutes, before machining 103 the metal-ceramic substrate 1 to create the predetermined break point 7. The same applies to temperature treatments after machining with the laser beam 10.

[0046] For example, for this purpose, the metal-ceramic substrate 1 is heated, in particular to a temperature above 40°C, preferably above 80°C, more preferably above 150°C, before being machined or machined by the laser light 10. In particular, the heating 102 thereby results in a heat input carried out by the laser pulse itself, preferably a short-term heat input that is proportionally reduced. In particular, for this purpose, the temperature treatment is carried out at a heating rate of less than 5°C / min, preferably less than 3°C / min, more preferably less than 0.5°C / min.

[0047] Preferably, the cooling is performed at a cooling rate of less than 4°C / min, preferably less than 2°C / min, more preferably less than 0.5°C / min. The temperature treatment during machining of the metal-ceramic substrate 1 means, in particular, that the laser beam or laser light 10 passes through the same position in the first and subsequent second passes, for example, when passing through a given position multiple times. By specifically adjusting the time interval between the first and second passes, the cooling of the metal-ceramic substrate 1 during machining can be performed in a targeted manner. Alternatively or additionally, in addition to setting the time interval until the second pass, it is also conceivable to further cool the metal-ceramic substrate 1. This allows the time interval until the second pass to be shortened, which can speed up the entire manufacturing process of manufacturing or machining the metal-ceramic substrate 1 while forming the predetermined breaking point 7.

[0048] To perform a targeted temperature treatment of the metal-ceramic substrate 1, the holding element 40 may have, for example, a heating element 50, preferably located at or below the predetermined break point 7 and extending perpendicular to the main extension plane HSE. In this regard, the corresponding heating element 50 may be located within the holding element 40 and / or attached to the outside of the holding element 40. For example, when the holding element 40 comprises a metal-ceramic substrate, the heating element 50 is directly adjacent to the metal-ceramic substrate 1. The holding element 40 may also preferably positively and / or non-positively fix the metal-ceramic substrate 1 in a direction parallel to the main extension plane HSE. Consequently, the holding element 40 may also be used to position the metal-ceramic substrate 1. Alternatively, and / or complementary to forming the heating element 50 inside or outside the holding element 40, the entire holding element 40 may be heated and / or selectively cooled to heat and / or cool the metal-ceramic substrate 1. For this purpose, the holding element 40 is preferably made of a material having a relatively high thermal conductivity, in particular a thermal conductivity of more than 100 W / mK, preferably more than 200 W / mK, particularly preferably more than 400 W / mK.

[0049] Preferably, the holding element 40 is heated, for example by means of heating coils or heating elements 50 which are regularly and / or irregularly distributed in or on the holding element 40. Preferably, the heating coils or heating elements 50 are arranged at least partially coincident below the planned predetermined breaking point 7 in a direction perpendicular to the main extension plane HSE.

[0050] FIG. 2a shows a predetermined breaking point 7 according to the state of the art. In particular, this is a cross-sectional view along the direction V, where the contour of the predetermined breaking point 7 can be seen, particularly at its bottom or base. The predetermined breaking point 7, particularly recessed in the ceramic layer, has a first depth T1 measured in a direction perpendicular to the main extension plane HSE between the upper surface OS of the metal-ceramic substrate 1, in particular the ceramic layer of the metal-ceramic substrate 1, into which the predetermined breaking point 7 is recessed, and the bottom. In this context, the first depth T1 is always referred to, particularly in terms of concept, as a plane that continues the upper OS of the ceramic layer, i.e., a plane that extends parallel to the upper OS. Exemplary embodiments according to the prior art show that, apart from a course extending obliquely relative to the main extension plane, the predetermined breaking point 7 according to the prior art has a substantially constant first depth T1 at the beginning and end. In this context, those skilled in the art will understand that the first constant depth T1 varies along the direction of progression V by less than 10%, less than 5%, and even less than 2%.

[0051] FIG. 2b shows a predetermined breaking point 7 according to a preferred embodiment of the present invention. In particular, the predetermined breaking point 7 in FIG. 2b has a first section A1 and a second section A2, and the first depth T1 of the first section A1 is different from the second depth T2 of the second section A2. In particular, the first section A1 or the second section A2 is understood to be such a partial section of the predetermined breaking point 7 or of the bottom of the predetermined breaking point 7, respectively, that extends along a direction V essentially parallel to the main extension plane HSE. In other words, the first section A1 and the second section A2 at the predetermined breaking point 7 exclude sections at the bottom or above the predetermined breaking point 7 that extend essentially obliquely to the main extension plane HSE, for example, connecting the top surface OS with the first section A1 and / or connecting the first section A1 with the second section A2.

[0052] In the exemplary embodiment shown in FIG. 2b, the first length L1 of the first section A1, which is dimensioned parallel to the direction V, substantially corresponds to the second length L2 of the second section A2. Furthermore, FIG. 2b shows that the second depth T2 of the second section A2 is substantially twice the first depth T1 of the first section A1. Furthermore, it is preferable that the first and second sections A1 and A2 alternate in the direction V, thereby forming a periodic pattern of the bottoms of the predetermined breaking points 7. It has been found that forming the predetermined breaking points 7 at different depths, i.e., at least the first depth T1 and the second depth T2 relative to the first distance A1 and the second section A2, is suitable for providing sufficient stability of the metal-ceramic substrate 1, particularly in the form of a master card, thereby enabling its transportation. At the same time, the different depths T1 and T2 allow for more or less exclusive breaking along the predetermined breaking points 7.

[0053] In particular, it is realized that the base of the predetermined breaking point 7 is continuously, in particular continuously and periodically, adjusted along the direction V so as to form a first section A1 and a second section A2, in particular the base has a trapezoidal and / or triangular cross section in a cross section perpendicular to the main extension plane HSE and passing through the direction V.

[0054] To achieve such a predetermined break point 7, for example, the laser light 10 may pass through the ceramic layer more frequently in the second section A2 than in the first section A1. Alternatively, after the recess having the first depth T1 is created, a masking element, in particular a suitably patterned masking element, may be placed on the ceramic layer so that the light only reaches the ceramic layer through the non-shaded areas in the masking element and removes the ceramic material there. In this way, a suitably adjusted predetermined break point 7 may be achieved.

[0055] In the exemplary embodiment of the invention shown in Figure 2c, it is further realized that the second length L2 of the second section A2 is longer than the first length L1 of the first section A1. In particular, the first section A1 is substantially point-shaped so as to form a triangle at the base of the predetermined breaking point 7. [Explanation of symbols]

[0056] 1 Metal ceramic substrate 6 Plasma Flame 7 Predetermined Breaking Point 10 Laser light 20 lenses 25 Suction device 30 mirror elements 50 Heating Elements A1 First Section A2 Second Section T1 First Depth T2 Second Depth V direction OS top HSE main extension surface

Claims

1. A method for machining a metal-ceramic substrate (1), in particular for producing a predetermined breaking point, comprising the steps of: Providing a metal-ceramic substrate (1); forming a predetermined breaking point (7) in the metal-ceramic substrate (1); Including, the predetermined breaking point (7) has, along its direction (V), at least a first portion (A1) having a first depth (T1) and at least a second portion (A2) having a second depth (T2), the second depth (T2) being different from the first depth (T1), the first portion (A1) and the second portion (A2) are realized outside the intersection of two predetermined breaking points (7), a first depth (T1) of the first portion (A1) remains substantially constant over a first length (L1) dimensioned in the direction (V) of the predetermined break point (7); The method wherein the second depth (T2) of the second portion (A2) remains substantially constant over a second length (L2) dimensioned in the direction (V) of the predetermined break point (7).

2. 10. The method of claim 1 , A method, wherein the ratio between the first depth (T1) and the second depth (T2) has a value between 0.2 and 0.8, preferably between 0.3 and 0.7, particularly preferably between 0.4 and 0.

6.

3. 10. The method of claim 1 , The method, wherein the ratio of the first length (L1) to the second length (L2) is less than 1.5, preferably less than 0.5, and more preferably less than 0.

25.

4. The method according to any one of claims 1 to 3, The method, wherein the first portion (A1) and the second portion (A2) are provided in a periodically alternating manner.

5. The method according to any one of claims 1 to 4, The method, wherein the predetermined breaking point (7) preferably has a third depth in a direction perpendicular to said direction (V), different from the first depth (T1) and / or the second depth (T2).

6. The method according to any one of claims 1 to 5, The method, wherein the predetermined breaking point (7) has a trapezoidal or triangular shape in a plane parallel to said direction (V).

7. The method according to any one of claims 1 to 6, A method in which the predetermined breaking point (7) is generated by machining with a laser light (10), in particular an ultrashort pulsed (UKP) laser, and in the course of forming the predetermined breaking point (7), the metal-ceramic substrate (1) is subjected to a temperature treatment before, during and / or after the machining, in particular cooling after the machining at a cooling rate of less than 4° C. / min, preferably less than 2° C. / min, more preferably less than 0.5° C. / min.

8. A metal-ceramic substrate having a predetermined breaking point (7) produced by the method according to any one of claims 1 to 7.

Citation Information

Patent Citations

  • Dividing method for ceramic substrate

    JP1994087085A

  • Ceramic substrate, method for forming groove, and laser machining apparatus

    JP2004179556A

  • Ceramic substrate, electronic device and electronic apparatus, manufacturing method of electronic device and manufacturing method of ceramic substrate

    JP2013125855A

  • Laser scribing method and flat plate material having dicing grooves

    JP2016083697A

  • Collective ceramic substrate, manufacturing method for the substrate, ceramic substrate, and ceramic circuit substrate

    WO2009154295A1