Wiring board and manufacturing method thereof

A multilayer wiring structure with photosensitive resin layers and dummy patterns addresses the challenges of FC-BGA wiring board manufacturing, improving electrical and insulation reliability by stabilizing surface undulations and reducing height variations.

JP7567490B2Active Publication Date: 2024-10-16TOPPAN HOLDINGS INC
View PDF 10 Cites 0 Cited by

Patent Information

Application Number
JP2021004418
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-01-14
Publication Date
2024-10-16
Estimated Expiration
2041-01-14

AI Technical Summary

Technical Problem

The existing methods for manufacturing FC-BGA wiring boards face challenges such as high equipment costs, limited yield due to silicon wafer limitations, transmission characteristic deterioration, and issues with fine wiring formation leading to warping, distortion, and electrical connection failures due to undulations and height variations in the insulating resin layer.

Method used

A multilayer wiring structure is formed using a second wiring board with photosensitive resin layers, conductive material-filled resin trenches, seed adhesion and seed layers, and dummy patterns to stabilize the surface, ensuring uniformity and reliability of connections.

Benefits of technology

The solution improves electrical connection reliability and insulation reliability by controlling height variations and surface undulations, reducing the risk of disconnections and short circuits, thereby enhancing the overall reliability of the wiring board.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007567490000007
    Figure 0007567490000007
  • Figure 0007567490000008
    Figure 0007567490000008
  • Figure 0007567490000009
    Figure 0007567490000009
Patent Text Reader

Abstract

To provide a wiring board and a manufacturing method of the wiring board with high connection reliability of a wiring portion against warping of the board during heating and stress inside a rewiring layer in a method of forming a fine rewiring layer on a support board and mounting a semiconductor element.SOLUTION: In a wiring board that includes a semiconductor element, and a second wiring board on which a wiring pattern thicker than the semiconductor element, which is bonded to the semiconductor element is formed, and in which a first wiring board is bonded to the surface opposite to the mounting surface of the semiconductor element of the second wiring board, a dummy pattern consisting of a plurality of islands 3A made of photosensitive resin is arranged at intervals of 1.5 mm or less in a large area pattern portion of 1.5 mm or more on a side of a wiring portion made of a conductive material on the second wiring board, and a flat rewiring layer is formed by suppressing surface waviness due to polishing of each rewiring layer composed of the wiring portion and a photosensitive resin layer.SELECTED DRAWING: Figure 7
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a wiring board and a manufacturing method thereof. [Background technology]

[0002] In recent years, with the progress of high speed and high integration of semiconductor devices, there is a demand for narrower pitch of connection terminals with semiconductor elements and finer board wiring for FC-BGA (Flip Chip Ball-l Grid Array) wiring boards. On the other hand, there is a demand for connection between FC-BGA wiring boards and motherboards with connection terminals at almost the same pitch as before.

[0003] In order to narrow the pitch of the connection terminals with the semiconductor elements in the FC-BGA wiring board and to miniaturize the board wiring, a method is known in which wiring is formed on a silicon substrate to serve as a substrate (silicon interposer) for connecting the semiconductor elements, and these are then connected to the FC-BGA substrate. Patent Document 1 discloses a method of forming fine wiring after planarizing the surface by polishing (chemical mechanical polishing) or the like. Patent Document 2 discloses a method of forming a narrow-pitch wiring board by forming a fine wiring layer on a support substrate, mounting the layer on an FC-BGA wiring board, and then peeling off the support substrate. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2014-225671 A [Patent Document 2] International Publication No. 2018 / 047861 [Patent Document 3] Patent No. 6247032 Summary of the Invention [Problem to be solved by the invention]

[0005] Silicon interposers are manufactured using silicon wafers with semiconductor front-end processing equipment. Silicon wafers are limited in shape and size. For this reason, only a small number of interposers can be manufactured from one wafer, and the equipment costs are high, so the interposers are also expensive. In addition, since silicon wafers are semiconductors, there is a problem in that the transmission characteristics deteriorate. Furthermore, in the method of flattening the FC-BGA wiring substrate and forming fine wiring on it, the degradation in transmission characteristics seen with silicon interposers is small, but there are problems with reduced yield within the same substrate due to the combination of manufacturing defects in the FC-BGA wiring substrate and defects during the highly difficult formation of the fine wiring, as well as problems in mounting semiconductor elements due to warping and distortion of the FC-BGA wiring substrate.

[0006] On the other hand, when fine wiring is formed on a support substrate, a semiconductor element is mounted on the fine wiring, and then the support substrate is peeled off and the semiconductor element is mounted on an FC-BGA wiring substrate via the fine wiring, the following problems arise. For example, there is a method in which a fine wiring pattern is formed using a semi-additive method, the fine wiring is covered with a photosensitive insulating resin layer, vias are opened to form connections with the wiring pattern to be layered on top, and the required number of layers are layered.

[0007] In this case, depending on the presence or absence of wiring patterns and their density, the height of the insulating resin layer in the areas without wiring patterns becomes lower, causing undulations on the surface of the coated insulating resin layer, which causes problems such as variations in the dimensions of the laminated wiring patterns and electrical connection failures caused by variations in the height between connection terminals when mounting with semiconductor elements. This problem is also present in the process of forming fine wiring on a support substrate, mounting this on an FC-BGA wiring board, and then mounting it on a semiconductor element.

[0008] In some cases, fine wiring patterns are fabricated by a damascene process using CMP, in which a trench pattern is formed in a photosensitive insulating resin layer, filled with a conductive material, and then processed by CMP. In this case, when a wiring section consisting of a wiring pattern, a connection via section, a land section, a ground pattern section, a dummy pattern section, and an accessory pattern section consisting of an alignment mark and an auxiliary pattern used to fabricate a wiring board are formed by CMP, a large-area pattern section consisting of a single material consisting of a conductive material or a photosensitive resin with a minimum width of 1.5 mm or more may be excessively polished, resulting in a concave cross-sectional shape. The depth of this concave shape tends to be deeper as the linear dimension of the wiring section is longer, and the depth of the concave shape varies from a few tenths of a micrometer to a few micrometers, depending on the linear dimension of the wiring section.

[0009] As a result, the surface of the substrate on which the wiring section is formed using CMP has ripples that are recessed by a few tenths of a micron to several microns from the surface of the photosensitive insulating resin layer, and when the next redistribution layer (wiring section) is formed by stacking it on top of this redistribution layer (wiring section), the photosensitive insulating resin layer is applied in accordance with the ripples of the lower layer, causing ripples in the trench pattern as well. When the trench pattern formed on top is covered with a conductor layer and the covered conductor layer is polished by CMP to form wiring sections and accessory pattern sections, there is a problem that in the deep undulation parts of the lower layer, the polishing does not reach the surface of the trench pattern of the photosensitive insulating resin layer, and the pattern may not be formed. Furthermore, the connection terminals formed on the ripples of each layer also vary in height, which may cause poor electrical connection due to the variation in height between the connection terminals when mounting the semiconductor element.

[0010] The present invention has been made in view of the above-mentioned circumstances, and an object of the present invention is to provide a wiring board with high connection reliability of wiring portions and a method for manufacturing the same. [Means for solving the problem]

[0011] As a means for solving the above-mentioned problems, the invention described in claim 1 of the present invention provides a wiring board including a second wiring board bonded to a semiconductor element, and a first wiring board mounted on an opposing surface of the second wiring board opposite to the mounting surface of the semiconductor element, the widths of the wirings constituting the first wiring board, the second wiring board, and the semiconductor element become narrower in that order when compared with the narrowest one, the second wiring board is configured to configure a multilayer wiring by laminating two or more rewiring layers, each of the wiring layers includes a photosensitive resin layer made of a photosensitive resin, an opening portion opened in the photosensitive resin layer forms a resin trench portion, and a conductive material is filled as a part of the resin trench portion, the wiring board includes a wiring pattern portion and the wiring board includes a wiring pattern portion and a wiring pattern portion. The rewiring layer has a photosensitive resin solid pattern portion arranged to surround the turn, and a ground pattern consisting of a large-area pattern with a narrowest part having a width of 1.5 mm or more arranged to surround the photosensitive resin solid pattern portion, a seed adhesion layer and a seed layer are formed in this order on the bottom surface of the resin trench portion, and the rewiring layer has a wiring portion consisting of a conductor layer formed by filling the inside of the resin trench portion with a conductive material, the multilayer wiring is constructed by stacking two or more conductor layers that become the wiring portion, and each rewiring layer consisting of the wiring portion and the photosensitive resin layer has a dummy pattern consisting of a plurality of island-shaped photosensitive resin patterns made of photosensitive resin arranged at intervals of 1.5 mm or less within the ground pattern.

[0012] When the photosensitive resin solid pattern portion is a large-area pattern having a narrowest width of 1.5 mm or more, the resin solid pattern portion has a dummy pattern consisting of a plurality of island-shaped conductive patterns made of a conductive material arranged at intervals of 1.5 mm or less.

[0013] Another aspect of the present invention is a method for manufacturing a wiring board, comprising: a second wiring board bonded to a semiconductor element; the second wiring board is configured by stacking two or more redistribution layers to form a multilayer wiring; each of the wiring layers is provided with a photosensitive resin layer made of a photosensitive resin; an opening portion opened in the photosensitive resin layer forms a resin trench portion; a part of the resin trench portion forms a wiring pattern portion filled with a conductive material; a seed adhesion layer and a seed layer are formed in this order on a bottom surface of the resin trench portion; and a conductive material is filled inside the resin trench portion to form a wiring portion made of a conductor layer; and the method for forming the redistribution layer includes the steps of: forming a resin trench portion in the photosensitive resin layer; The method includes the steps of providing a seed adhesion layer and a seed layer on the resin trench portion and the photosensitive resin layer, laminating a conductive material on the seed layer as a solid film, polishing the conductive material formed as the solid film from the laminated surface of the substrate by a first polishing step, thereby polishing and removing unnecessary conductive material laminated on the surface of the photosensitive resin layer while leaving the conductive material in the resin trench portion, and removing the seed adhesion layer, the seed layer, and the conductor layer made of a conductive material and the surface of the photosensitive resin layer on the substrate surface exposed by the first polishing step by a second polishing step, thereby forming a redistribution layer having a structure in which the resin trench portion is filled with a conductive material. The redistribution layer forming step is repeated for the required number of layers to form a two-layer laminate of redistribution layers. Effect of the Invention

[0014] According to the aspects of the present invention, in a second wiring board on which fine wiring layers are formed and semiconductor elements are mounted, it is possible to improve the electrical connection reliability of via connections between wiring layers and the insulation reliability between wirings. Therefore, according to the aspects of the present invention, it is possible to improve the reliability of the wiring board without breaks or shorts. [Brief description of the drawings]

[0015] [Figure 1] 1 is a cross-sectional view showing a state in which a release layer is formed on a support substrate. [Figure 2A] FIG. 4 is a cross-sectional view showing a state in which a photosensitive resin layer has been formed. [Figure 2B]FIG. 2 is a cross-sectional view showing a state in which a seed adhesion layer is formed. [Figure 2C] FIG. 2 is a cross-sectional view showing a state in which a seed layer is formed. [Figure 2D] FIG. 4 is a cross-sectional view showing a state in which a conductor layer is formed. [Figure 2E] FIG. 11 is a cross-sectional view showing a state in which the conductor layer and the seed layer have been polished by surface polishing. [Figure 2F] 13 is a cross-sectional view showing a state in which the conductor layer, the seed adhesion layer, and the photosensitive resin layer are polished by surface polishing to form connection terminals for bonding to a first wiring board. FIG. [Figure 3A] 11 is a cross-sectional view showing a state in which a photosensitive resin layer is formed in a connection via portion. FIG. [Figure 3B] 10 is a cross-sectional view showing a state in which a photosensitive resin layer is formed on a connection via portion and a wiring portion. FIG. [Figure 3C] FIG. 2 is a cross-sectional view showing a state in which a seed adhesion layer is formed. [Figure 3D] FIG. 2 is a cross-sectional view showing a state in which a seed layer is formed. [Figure 3E] FIG. 4 is a cross-sectional view showing a state in which a conductor layer is formed. [Figure 3F] 11 is a cross-sectional view showing a state in which a connection via portion and a wiring portion are formed by surface polishing. FIG. [Figure 4] FIG. 3B is a cross-sectional view showing a state in which a multilayer wiring is formed by repeating steps from FIG. 3A to FIG. 3F. [Figure 5A] FIG. 4 is a cross-sectional view showing a state in which a photosensitive resin layer has been formed. [Figure 5B] FIG. 2 is a cross-sectional view showing a state in which a seed adhesion layer is formed. [Figure 5C] FIG. 2 is a cross-sectional view showing a state in which a seed layer is formed. [Figure 5D] FIG. 2 is a cross-sectional view showing a state in which a resist pattern is formed. [Figure 5E] FIG. 4 is a cross-sectional view showing a state in which a conductor layer is formed. [Figure 5F] FIG. 4 is a cross-sectional view showing a state after the resist pattern has been removed. [Figure 5G] 11 is a cross-sectional view showing a state in which an unnecessary seed adhesion layer and a seed layer are etched away. FIG. [Figure 5H] 1A and 1B are diagrams showing island-shaped dummy patterns arranged in a large area pattern portion made of a conductive material pattern or a photosensitive insulating resin pattern; [Figure 5I] 1 is a cross-sectional view showing a state in which a wiring board on a support board is completed after surface treatment and solder joints are formed. [Figure 6A] 4 is a cross-sectional view showing a state in which a semiconductor element is bonded to a second wiring board. FIG. [Figure 6B] 11 is a cross-sectional view showing a state in which the gap between a second wiring board and a semiconductor element is filled with underfill. [Figure 6C] 11 is a cross-sectional view showing a state in which a semiconductor element on a second wiring substrate is molded with a sealing resin. [Figure 6D] FIG. 11 is a cross-sectional view showing a state in which a peeling layer is irradiated with laser light. [Figure 6E] FIG. 11 is a cross-sectional view showing a state in which the support substrate has been removed. [Figure 6F] FIG. 2 is a cross-sectional view showing a state in which a semiconductor element is mounted. [Figure 7] 4 is a cross-sectional view showing a state in which a semiconductor element, a second wiring board, and a first wiring board are bonded together. FIG. [Figure 8] The image of one piece and an enlarged view of part ab in the image are shown below. The wiring part is a collection of patterns of several μm in size, and is shown as a solid area in the one piece image. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the following description of the drawings, the same or similar parts are denoted by the same or similar reference numerals. However, it should be noted that the drawings are schematic, and the relationship between thickness and planar dimensions, the thickness ratio of each layer, etc., differ from the actual ones. Therefore, the specific thickness and dimensions should be determined by taking into consideration the following explanation. In addition, it goes without saying that the drawings include parts whose dimensional relationships and ratios differ from each other. The embodiments described below are merely examples of devices and methods for embodying the technical idea of ​​the present invention, and the technical idea of ​​the present invention does not limit the materials, shapes, structures, arrangements, etc. of the components to those described below. The technical idea of ​​the present invention can be modified in various ways within the technical scope defined by the claims.

[0017] Hereinafter, an example of a manufacturing process for a wiring board using a support substrate according to one embodiment of the present invention will be described with reference to FIGS. 1, a release layer 2 is formed on one surface of a support substrate 1. The release layer 2 is formed in order to release the support substrate 1 in a later step. The release layer 2 may be, for example, a resin that becomes peelable by absorbing light such as UV light and generating heat or by being altered, or a resin that becomes peelable by foaming due to heat. When a resin that becomes peelable by light such as UV light, for example laser light, is used as the release layer 2, the support substrate 1 can be irradiated with light from the surface opposite to the side where the release layer 2 is provided, and the support substrate 1 can be removed from the bonded body of the wiring substrate 11 and the semiconductor element 15 on the support substrate.

[0018] The material of the release layer 2 can be selected from organic resins such as epoxy resin, polyimide resin, polyurethane resin, silicone resin, polyester resin, oxetane resin, maleimide resin, and acrylic resin, and inorganic layers such as amorphous silicon, gallium nitride, and metal oxide film. Furthermore, the release layer 2 may contain additives such as a photodecomposition promoter, a light absorber, a sensitizer, and a filler. Furthermore, the release layer 2 may be composed of multiple layers, and for example, for the purpose of protecting the multilayer rewiring layer (second wiring board) formed on the support substrate 1, a protective layer may be further provided on the release layer 2, or a layer that improves adhesion to the support substrate 1 may be provided under the release layer 2. Furthermore, a laser reflecting layer or a metal layer may be provided between the peeling layer 2 and the multi-layer rewiring layer, and the configuration is not limited to that of this embodiment.

[0019] Since light may be irradiated to the peeling layer 2 through the support substrate 1, the support substrate 1 is preferably transparent, and glass, for example, can be used as the support substrate 1. A glass substrate has excellent flatness and high rigidity, and is therefore suitable for forming a fine pattern of the wiring substrate 11 on the support substrate 1. Glass has a small CTE (coefficient of thermal expansion) and is not easily distorted, and is therefore excellent in ensuring pattern arrangement accuracy and flatness. When glass is used as the support substrate 1, it is desirable for the glass to have a large thickness in order to suppress the occurrence of warping in the manufacturing process, and the thickness is, for example, 0.7 mm or more, preferably 1.1 mm or more. The CTE of glass is preferably 3 ppm or more and 15 ppm or less, and from the viewpoint of the CTE of the semiconductor element 15 and the wiring substrate 12 for FC-GBA, the CTE of glass is more preferably about 9 ppm.

[0020] Examples of glass include quartz glass, borosilicate glass, alkali-free glass, soda glass, sapphire glass, etc. On the other hand, when the support substrate 1 does not need to be transparent when peeling off the support substrate 1, for example, when a resin that foams by heat is used for the peeling layer 2, the support substrate 1 can be made of a material with little distortion, such as a substrate made of metal or ceramics. In one embodiment of the present invention, the release layer 2 is made of a resin that absorbs UV light and becomes peelable, and the support substrate 1 is made of glass.

[0021] Next, as shown in FIG. 2A, a photosensitive resin layer 3 is formed on the release layer 2. In this embodiment, the photosensitive resin layer 3 is formed, for example, by spin coating a photosensitive epoxy resin. Photosensitive epoxy resin can be cured at a relatively low temperature and shrinks little due to curing after formation, so it is excellent for subsequent fine pattern formation. When a liquid photosensitive resin is used for its formation, the photosensitive resin layer 3 can be formed by slit coating, curtain coating, die coating, spray coating, electrostatic coating, inkjet coating, gravure coating, screen printing, gravure offset printing, spin coating, or doctor coating. When a film-like photosensitive resin is used for the formation of the photosensitive resin layer 3, lamination, vacuum lamination, vacuum pressing, or the like can be applied. For the photosensitive resin layer 3, for example, a photosensitive polyimide resin, a photosensitive benzocyclobutene resin, a photosensitive epoxy resin, or a modified product thereof can be used as an insulating resin.

[0022] Next, a resin trench portion 21 consisting of an opening is provided in the photosensitive resin layer 3 by photolithography (see FIG. 2A). The opening constituting the resin trench portion 21 is filled with a conductive material to become a wiring portion consisting of a wiring pattern, a land, and a connection via, a ground pattern portion, a dummy pattern portion, and an accessory pattern portion consisting of an alignment mark and an auxiliary pattern used to fabricate a wiring board. The land portion is formed in an opening of φ100 μm or less. The alignment mark is formed as a cross or circular pattern with a linear dimension of several hundred μm to about 2 mm, or an opening of an aggregate of these.

[0023] The minimum line width of the wiring pattern may be selected depending on the form of the product. As an example, a semiconductor element with a wiring width of 14 nm may be electrically connected to a second wiring board with a wiring width of 2 μm and a bump pitch of 50 μm, and further electrically connected to a first wiring board with a wiring width of 10 μm and a bump pitch of 160 μm, making it easy to use as a semiconductor device. In the second wiring board, when the wiring width is 3 μm or less, the semi-additive method that has been used to form wiring up to now becomes difficult to use, and the damascene method using CMP becomes effective. The ground pattern is made of a large opening having an irregular shape and a narrowest width of 1.5 mm or more, and surrounds the wiring pattern via a solid photosensitive resin pattern.

[0024] In one embodiment of the present invention, as shown in FIG. 8, a wiring board is formed in which a wiring portion, an accessory pattern 27, a ground pattern 30A, a photosensitive resin solid pattern 30B, and a dummy pattern 28 are arranged. As shown in Fig. 5H, a ground pattern 30A made of a conductive material is formed in a large-area opening surrounded by a photosensitive resin layer 3. A dummy pattern 28 made of a plurality of photosensitive resin layers 3 is disposed in the opening of the ground pattern 30A. The opening of the ground pattern is filled with a conductive material. The wiring pattern is omitted in Fig. 5H. The outline of the ground pattern 21A is indefinite and is disposed to surround the wiring pattern portion as shown in Fig. 5H. It is also possible to reverse the positional relationship between the conductive material portion and the photosensitive resin portion, and to place the dummy pattern 28 made of a conductive material on the photosensitive resin solid pattern 30B surrounded by the conductive material.

[0025] The dummy patterns 21 shown in Fig. 5H are configured to be arranged in a predetermined array pattern. The distance between the outer periphery of adjacent dummy patterns 28 and ground pattern 30A is set to 1.5 mm or less. The number of dummy patterns 28 arranged per unit area is one or more in a square with sides of 3 mm, so the patterns should be arranged at a density of 0.11 (= 1 / 9) / mm2 or more. The dimensions and shape of the dummy pattern 28 are not particularly specified, but the dimensions are 50 μm to 500 μm, and the pattern shape can be a circle, octagon, ellipse, square, etc. The arrangement interval of the dummy patterns 28 is 1.5 mm or less, preferably 1 mm or less, and the lower limit is 500 μm or more.

[0026] If the spacing between the islands 3A constituting the dummy pattern is greater than 1.5 mm, when the conductor layer 6 deposited on the photosensitive resin layer 3 is polished away by polishing, the amount of depression of the conductive material between the dummy patterns will be greater than 0.1 μm, causing a waviness of greater than −0.1 μm in the redistribution layer, which will be an obstacle when stacking and forming the next redistribution layer. The upper end surface of the dummy pattern 28 thus formed is flush with the other surface of the photosensitive resin layer 3 . In order to remove resin residues remaining after development, a plasma treatment may be performed on the resin trench portion 21. The thickness of the photosensitive resin layer 3 is set according to the thickness of the conductive layer to be formed in the opening, and in one embodiment of the present invention, the photosensitive resin layer 3 is formed to a thickness of, for example, 8 μm.

[0027] In addition, in one embodiment of the invention, in a structure in which a rewiring layer formed on the peeling layer 2 becomes the mounting surface of the semiconductor element 15, and the surface opposite the peeling layer 2 formed by lamination becomes the mounting surface of the first wiring board 12, dummy patterns 28 of φ200 μm are arranged at 1 mm intervals with respect to accessory patterns 27 such as alignment marks, ground pattern 30A, and solid photosensitive resin pattern 30B. A structure in which the redistribution layer formed on the peeling layer 2 becomes the mounting surface of the first wiring board 12, and the surface opposite the peeling layer 2 formed by lamination becomes the mounting surface of the semiconductor element 15, is also the same as the structure of the wiring board 11 on the support substrate 1 obtained in the present invention, and is included in the scope of the present claims.

[0028] Next, as shown in FIGS. 2B and 2C, a seed adhesion layer 4 and a seed layer 5 are formed in this order in a vacuum. The seed adhesion layer 4 is a layer that improves the adhesion of the seed layer 5 to the photosensitive resin layer 3 and prevents peeling of the seed layer 5. The seed layer 5 acts as a power supply layer for electrolytic plating in the wiring portion shape. The seed adhesion layer 4 and the seed layer 5 are formed by, for example, a sputtering method or a vapor deposition method, and the material thereof may be, for example, Cu, Ni, Al, Ti, Cr, Mo, W, Ta, Au, Ir, Ru, Pd, Pt, AlSi, AlSiCu, AiCu, NIFe, ITO, IZO, AZO, ZnO, PZT, TiN, Cu3N4, Cu alloy, or a combination of a plurality of these. In this embodiment, in consideration of electrical characteristics, ease of manufacture, and cost, a titanium layer is formed as the seed adhesion layer 4, and then a copper layer is formed as the seed layer 5 by a sputtering method. The total thickness of the titanium layer and the copper layer is preferably 1 μm or less as a power supply layer for electrolytic plating. In one embodiment of the present invention, Ti: 50 nm, Cu: 300 nm are formed.

[0029] Next, as shown in FIG. 2D, a conductor layer 6 is formed by electrolytic plating. The conductor layer 6 serves as an electrode for bonding to the FC-BGA substrate 12. Examples of electrolytic plating include electrolytic nickel plating, electrolytic copper plating, electrolytic chromium plating, electrolytic Pd plating, electrolytic gold plating, electrolytic iridium plating, etc. Copper electrolytic plating is preferable because it is simple, inexpensive, and has good electrical conductivity. The thickness of the electrolytic copper plating, which serves as an electrode for bonding to first wiring board 12, is desirably 1 μm or more from the viewpoint of solder bonding, and 30 μm or less from the viewpoint of productivity. In one embodiment of the present invention, the trench portion 21 of the photosensitive resin layer 3 is filled with Cu to a thickness of 9 μm, and the upper portion of the photosensitive resin layer 3 is also filled with Cu to a thickness of 9 μm.

[0030] Next, as shown in FIG. 2E, the copper layer on the surface of the photosensitive resin layer is polished and removed by CMP (chemical mechanical polishing) having chemical polishing properties for the conductive material of the conductor layer 6. That is, the first polishing is performed so that the seed adhesion layer 4 covering the top part of the resin trench part 21 and the conductor layer 6 filled in the opening of the resin trench part 21 become the surface. The abrasive used in the chemical mechanical polishing contains a chemical polishing component and a physical polishing component, and a prescription in which the chemical polishing component is dominant is preferable. A prescription in which the effect of the physical polishing component is adjusted to be high can also be used, but since layers with different hardness consisting of the conductor layer 6, the seed adhesion layer 4, and the photosensitive resin layer 3 come to the surface with polishing, it becomes difficult to control the height of the wiring and the unevenness of the surface. In one embodiment of the present invention, Cu: 9 μm of the upper conductor layer 6 of the photosensitive resin layer 3 and Cu: 300 nm of the seed layer 5 are removed by the first polishing using an abrasive containing a predominantly chemical abrasive component.

[0031] Next, as shown in FIG. 2F, the seed adhesion layer 4 and the surface layer of the photosensitive resin layer 3 are removed by a second polishing step in which the photosensitive resin layer 3, the conductor layer 6, and the seed layer 5 are physically polished and removed. The second polishing step is performed by polishing the dissimilar materials of the seed adhesion layer 4 and the photosensitive resin layer 3. Since the photosensitive resin layer 3 cannot be polished by chemical polishing, physical polishing using an abrasive such as filler is effective. Since the parts with high surface irregularities are polished first in physical polishing, the second polishing step is effective in reducing the surface irregularities caused by the first polishing step. As for the abrasive, a formulation in which a small amount of a chemical abrasive component for conductive materials is added to an abrasive predominantly for physical polishing, and which imparts surface smoothness to the conductor layer 6, is desirable. By adjusting the polishing speed of the conductor layer 6 and the photosensitive resin layer 3 and increasing the polishing speed of the photosensitive resin layer 3, a shape in which the wiring portion is higher than the photosensitive resin layer 3 is realized.

[0032] In addition, in the portion where the opening width of the resin trench portion 21 is wide and the conductor layer 6 is processed into a concave shape by the first polishing, the depth of the concave shape can be reduced by preferentially polishing the photosensitive resin layer 3 and the seed adhesion layer 4 located at the ends of the concave shape. In this way, for the resin trench portion 21 consisting of patterns with various opening widths, such as the bump portion 17, the land portion 27, and the accessory pattern 27, the rewiring layer in which the depth of the concave shape is reduced to a few tenths of a micrometer to just under 1 micrometer by the first polishing, and the surface layer is polished to a few tenths of a micrometer by the second polishing, so that the variation in the height of the wiring portion, ground pattern portion, and photosensitive resin solid pattern portion from the virtual plane can be controlled to a range of -0.1 to +0.1 μm.

[0033] Here, the film thickness was measured using a stylus-type film thickness meter or a laser microscope, and the variation in height at each measurement point was calculated based on the height of the photosensitive resin layer 3. The equation for the virtual plane is shown in 1 below. The three-dimensional measurement value over the entire area is (x i , y i、 z i ) and the measurement unit is given in μm.

[0034]

number

[0035] Each measurement point (x i , y i、 z i The constants (a, b, c) should be determined so that the distance between each measurement point (x i , y i、 z i ) and the height between the least squares plane E i Let F be the sum of squares of all points. F is expressed by the following formula.

[0036]

number

[0037] Then, constants (a, b, c) are determined so as to minimize the F value. In other words, the simultaneous equations with three unknowns (see the equation below) are solved so that the partial differentiation value of the above equation with respect to the constants (a, b, c) is 0.

[0038]

number

[0039] In practice, the constants (a, b, c) can be calculated by a matrix calculation using a computer. Furthermore, three times the root mean square distance from the virtual plane can be calculated from the following formula. The following formula indicates that the following value, which indicates the flatness of the redistribution layer, is ±0.1*3μm or less.

[0040]

number

[0041] This formula means that three times the standard deviation of the distance between the plane and each measurement point, as determined from each measurement point, is 0.3 μm or less. n is the number of measurement points on the first main surface, and it is desirable for n to be at least 5 × 5 = 25 or more lattice points. More desirably, n is 10 × 10 = 100 or more. If the number of measurement points n is less than 25, the number of samples is small and it is difficult to measure the true value. The bumps obtained by polishing in this manner become connection terminals for the FC-BGA substrate 12 and the semiconductor element 15.

[0042] Next, as shown in FIG. 3A, a photosensitive resin layer 3 is formed on the upper surface in the same manner as in FIG. 2A. The thickness of the photosensitive resin layer 3 to be formed is set according to the thickness of the conductor layer to be formed in the opening, and in one embodiment of the present invention, the photosensitive resin layer 3 is formed with a thickness of, for example, 2 μm. The opening shape of the via portion in plan view is set from the viewpoint of connection with the conductor layer 6, and in one embodiment of the present invention, an opening shape of, for example, φ10 μm is formed. This opening has the shape of a connection via portion 19 that connects upper and lower rewiring layers of the multilayer rewiring layer.

[0043] Furthermore, as shown in FIG. 3B, a photosensitive resin layer 3 is formed on the upper surface thereof in the same manner as in FIG. 2A. The thickness of the photosensitive resin layer 3 to be formed is set according to the thickness of the conductor layer to be formed in the opening, and in one embodiment of the present invention, the photosensitive resin layer 3 is formed to a thickness of, for example, 2.5 μm. The resin trench portion 21 is made up of a wiring portion consisting of a land portion 26 and a wiring pattern portion 25, an accessory pattern portion 27 consisting of an alignment mark or the like, and a ground pattern 30A.

[0044] The opening shape of the land portion 26 in plan view is set from the viewpoint of the connectivity of the laminate, and is formed to surround the outside of the opening shape of the lower connection via portion 31. In one embodiment of the present invention, the opening shape is, for example, φ25 μm. The wiring pattern portion is formed with an opening shape of, for example, L / S=2 / 2 μm. The alignment mark consists of a cross-shaped or circular pattern of several hundred μm to 2 mm, and an opening of a collection of these, and the ground pattern 30A consists of a large-area concave pattern having a width of 1 mm or more at its narrowest part surrounding the resin solid pattern portion 30B of 200 μm to 500 μm width that surrounds the wiring pattern 25.

[0045] In one embodiment of the present invention, dummy patterns 28 having a diameter of 200 μm are formed at intervals of 1 mm in the opening of a large-area ground pattern. In one embodiment of the present invention, the photosensitive resin layer 3 is coated in two layers, and each layer is formed separately into the connection via portion 31, the land portion 27, and the wiring pattern portion 25. However, it is also possible to form them in a single photolithography process by coating a single layer using gradation exposure.

[0046] 3C and 3D, the seed adhesion layer 4 and the seed layer 5 are formed in a vacuum in the same manner as in Fig. 2B and Fig. 2C. In one embodiment of the present invention, Ti: 50 nm and Cu: 300 nm are formed. Next, as shown in Fig. 3E, a conductor layer 6 is formed by electrolytic plating. The conductor layer 6 becomes the wiring portion and the accessory pattern portion. Examples of electrolytic plating include nickel electrolytic plating, copper electrolytic plating, chromium electrolytic plating, Pd electrolytic plating, gold electrolytic plating, rhodium electrolytic plating, and iridium electrolytic plating. Of these, copper electrolytic plating is preferable because it is simple, inexpensive, and has good electrical conductivity. The thickness of the electrolytic copper plating is desirably 0.5 μm or more from the viewpoint of electrical resistance of the wiring portion, and 10 μm or less from the viewpoint of productivity. In one embodiment of the present invention, Cu: 5 μm is formed in the double opening of the photosensitive resin layer 3, and Cu: 5 μm is also formed in the single opening of the photosensitive resin layer 3 and on the upper part of the photosensitive resin layer 3.

[0047] Next, as shown in Fig. 3F, the copper layer on the surface of the photosensitive resin layer is polished and removed by CMP (chemical mechanical polishing) that has a chemical polishing property for the conductive material of the conductor layer, in the same manner as in Fig. 2E and Fig. 2F. That is, processing is performed by the first polishing so that the seed adhesion layer 4 covering the top part of the resin trench part 21 and the conductor layer 6 filling the opening part of the resin trench part 21 become the surface. Furthermore, the seed adhesion layer 4 and the surface layer of the photosensitive resin layer 3 are removed by a second polishing step in which the photosensitive resin layer 3, the conductor layer 6, and the seed layer 5 are physically polished and removed. The conductor layer 6 remaining after polishing becomes the connection via portion 31, the land portion 26, the conductor portion of the wiring pattern portion 25 (wiring portion), and the accessory pattern portion 27 and the dummy pattern 28 in the ground pattern 30A or the photosensitive resin solid pattern 30B.

[0048] In one embodiment of the present invention, a rewiring layer with a concave depth of a few tenths of a micrometer to just under 1 micrometer is formed by the first polishing for resin trench portion 21 consisting of patterns with various opening widths such as wiring portion, ground pattern 30A, accessory pattern portion 27, etc. Also, by the second polishing, the variation in height from the virtual plane of the wiring portion, accessory pattern portion, and photosensitive resin layer can be controlled to within the range of -0.1 to +0.1 micrometer. Then, as shown in FIG. 4, by repeating the steps of FIG. 3A to FIG. 3F, rewiring layers are sequentially stacked to form a multilayer wiring. In one embodiment of the present invention, two rewiring layers having fine wiring portions with L / S=2 / 2 μm are formed.

[0049] Next, the process of forming electrodes for bonding to the semiconductor element 15 will be described. As shown in Fig. 5A, a photosensitive resin layer 3 is formed on the upper surface of the multilayer wiring in the same manner as in Fig. 2A. The thickness of the photosensitive resin layer 3 to be formed is set according to the thickness that covers the thickness of the lower conductor layer and provides electrical insulation between the upper and lower layers. In one embodiment of the present invention, a photosensitive resin layer 3 having a thickness of, for example, 4 µm is formed. Next, as shown in FIGS. 5B and 5C, a seed adhesion layer 4 and a seed layer 5 are sequentially formed in vacuum in the same manner as in FIGS. 2B and 2C.

[0050] Next, a resist pattern 7 is formed as shown in Fig. 5D. Thereafter, a conductor layer 6 is formed by electrolytic plating as shown in Fig. 5E. The formed conductor layer 6 becomes an electrode for bonding to a semiconductor element 15. The thickness of the electrolytic plating is desirably 1 µm or more from the viewpoint of solder bonding, and 30 µm or less from the viewpoint of productivity. In one embodiment of the present invention, for example, the resist pattern 7 has an opening shape of φ25 μm and is formed at intervals of 55 μm, and the thickness of the conductor layer is such that Cu:10 μm is formed in the opening of the photosensitive resin layer 3 and Cu:7 μm is formed on the upper surface of the photosensitive resin layer 3.

[0051] Thereafter, the resist pattern is removed as shown in Fig. 5F. Thereafter, unnecessary seed adhesion layer 4 and seed layer 5 are etched away as shown in Fig. 5G. In this state, conductor layer 6 consisting of bump portion 17 remaining on the surface becomes an electrode for bonding with semiconductor element 15. The conductive layer 6 consisting of the bump portion 17 may be used in its convex shape as is, or may be covered with a photosensitive resin containing a filler. Alternatively, a conductor layer may be formed as a solid film after FIG. 5C, and then polished to fill the conductor layer in the resin trenches, as shown in FIG. 5F. The shape of the bump portion 17 may be selected in accordance with the bonding method with the semiconductor element 15 . Then, in order to prevent oxidation of the surface of the conductor layer 6 consisting of the bump portion 17 and to improve the wettability of the solder bump 10, a surface treatment layer 9 is provided on the surface of the conductor layer 6 consisting of the bump portion 17 (see FIG. 5I).

[0052] In one embodiment of the present invention, electroless Ni / Pd / Au plating is formed as the surface treatment layer 9. Note that an OSP (Organic Soiderability Preservative: surface treatment with a water-soluble flux) film may be formed on the surface treatment layer 9. Next, a solder material is placed on the surface treatment layer 9, and then melted, cooled, and fixed to obtain a joint of the solder bump 10 (see FIG. 5I). This completes the wiring board 11 formed on the support substrate 1.

[0053] Next, as shown in FIG. 6A, the wiring board 11 on the support substrate 1 and the semiconductor element 15 are bonded by the bonding portions of the solder bumps 10. The above joint is then sealed with underfill 22 as shown in FIG. 6B. The resin material constituting the underfill is, for example, one of epoxy resin, urethane resin, silicone resin, polyester resin, oxetane resin, urethane resin, silicone resin, polyester resin, oxetane resin, and maleimide resin, or a mixture of two or more of these resins, to which silica, titanium oxide, aluminum oxide, magnesium oxide, zinc oxide, or the like is added as a filler. The underfill 22 is formed by filling with a liquid resin.

[0054] Next, as shown in FIG. 6C, a sealing resin 23 for sealing the semiconductor element 15 is formed. The sealing resin 23 is made of a material different from the underfill 22, and is made of one or a mixture of two or more of epoxy resin, silicone resin, acrylic resin, urethane resin, polyester resin, and oxetane resin, to which silica, titanium oxide, aluminum oxide, magnesium oxide, zinc oxide, or the like is added as a filler, and is formed by compression molding, transfer molding, or the like.

[0055] Next, as shown in Fig. 6E, the support substrate 1 is peeled off. For example, as shown in Fig. 6D, the peeling is performed by irradiating the peeling layer 2 with UV laser light 13. By irradiating the peeling layer 2 formed at the interface with the support substrate 1 with laser light 13 from the back surface of the support substrate 1, i.e., from the surface of the support substrate 1 opposite to the semiconductor element 15, and making the peeling layer 2 into a peelable state, it becomes possible to remove the support substrate 1 as shown in Fig. 6E. Next, the seed adhesion layer 4 and the seed layer 5 formed on the surface of the outer conductor layer 6 are removed to obtain a substrate as shown in Fig. 6F. In the embodiment of the present invention, titanium is used for the seed adhesion layer 4 and copper is used for the seed layer 5, which can be dissolved and removed with an alkaline etching agent and an acidic etching agent, respectively.

[0056] In this manner, a semiconductor device as shown in FIG. 6F is obtained in which second wiring board 14, which is made up of two or more rewiring layers (multilayer wiring), and semiconductor element 15 are bonded together. Thereafter, in order to prevent oxidation of the conductor layer 6 exposed on the surface of the second wiring board 14 and to improve the wettability of the solder bump portion 17, the conductor layer 6 exposed on the surface may be subjected to a surface treatment such as electroless Ni / Pd / Au plating, OSP, electroless tin plating, or electroless Ni / Au plating.

[0057] Thereafter, as shown in FIG. 7, the semiconductor device (see FIG. 6F) obtained by the above process is bonded to an FC-BGA substrate (first wiring substrate) 12, and an underfill 22 is filled in the bonded portion. The semiconductor device and the FC-BGA substrate 12 are fixed together, and the bonded portion is sealed, completing the semiconductor device 24. EXAMPLES

[0058] Tables 1 and 2 show the results of the dummy pattern dimensions (island arrangement intervals (numbers in the horizontal columns in the tables)) of the conductor layer and the amount of recession caused by polishing, as confirmation of the effects of this embodiment. The table shows, when copper is used as the conductive material (conductive layer), the amount of depression after the first polishing, which has a high chemical abrasiveness, and the second polishing, which has a high physical abrasiveness, and whether the copper is finished in a convex or concave shape relative to the photosensitive resin. For the first polishing, a slurry for chemical polishing of copper is used, in which a copper oxidizing agent, an organic reducing agent, a rust inhibitor, a complexing agent, etc. are dispersed. For the second polishing, a slurry is used that is designed to physically polish the copper, seed layer, inorganic adhesion layer, and photosensitive resin, and contains dispersed filler made of colloidal silica with diameters of several tens of nanometers, as well as filler dispersion stabilizers and additives.

[0059] Table 1 shows the results when slurry A was used in the first polishing. Table 2 shows the results when slurry B was used in the first polishing. Slurry A has a strong copper etching property, and even in a narrow pattern area with an opening width of 20 μm in the photosensitive resin, the copper is etched, resulting in a large depression of the copper in the photosensitive resin. Slurry B is a slurry that reduces the etching ability of copper. In the narrow pattern areas of the photosensitive resin opening width of 20 μm, the copper is difficult to etch, but in areas where the opening width becomes wider and the polishing pad can easily follow it, the amount of copper recession begins to increase. The etching property of copper can be adjusted by adjusting the balance of the constituent components of the slurry.

[0060] [Table 1]

[0061] [Table 2]

[0062] The wiring portion of the second wiring board has an area of ​​200 μm or less, and the unevenness in the wiring board can be controlled within the range of −0.1 to +0.1 μm. The accessory pattern portion is made up of large-area patterns such as alignment marks, ground patterns, and dummy patterns, and also includes solid patterns made of conductive materials larger than 2 mm as shown in Tables 1 and 2. When forming a solid pattern of a large area pattern using the damascene method of the present invention, it is effective to arrange dummy patterns at intervals narrower than 1.5 mm, preferably narrower than 1 mm, as shown in Tables 1 and 2, and made of a material different from the conductive material, such as a photosensitive resin.

[0063] In this embodiment, when forming the conductor layer 6 in FIG. 2F, FIG. 3F, and FIG. 4, dummy patterns having a diameter of 200 μm are arranged in an island shape at intervals of 1 mm in the body area pattern portion having a linear dimension of the accessory pattern portion greater than 1 mm. In addition, in a large area pattern portion of the photosensitive insulating resin having a linear dimension of 1 mm or more, dummy patterns made of a conductive material and having a diameter of 200 μm were arranged in an island shape at intervals of 1 mm. This pattern arrangement enabled us to control the variation in height of each redistribution layer from the virtual plane within the range of -0.1 μm to +0.1 μm.

[0064] In addition, by controlling the variation in height of each redistribution layer from the virtual plane to within the range of -0.1 μm to +0.1 μm, it was possible to reduce waviness during application of the photosensitive insulating resin to be laminated on the upper layer, and also to suppress variation in height of the resin trench portion 21 and variation in dimensional resolution. In addition, the variation in height of the bumps that are connected to the semiconductor element can be controlled, which is effective in improving the reliability of the electrical connection.

[0065] The materials, manufacturing methods, and configurations used are the same as those of the embodiment, but a comparative example will be described in which no island-shaped dummy patterns are arranged in the accessory pattern portion or in the large area portion of the photosensitive insulating resin having a linear dimension of 1.5 mm or more. In the comparative example, a solid pattern made of an amorphous conductive material was arranged as a ground pattern surrounding the wiring pattern. In forming the conductor layer 6 in Fig. 3F and Fig. 4, the ground pattern was recessed by a depth of more than 2 μm by the first polishing with high chemical abrasiveness, and the conductive material near the center of the pattern was lost, resulting in the exposure of the underlying photosensitive resin layer in some areas. The wiring portion was formed with the same quality as in the comparative example. The redistribution layer thus obtained had a variation in height from the surface to a virtual plane within the range of -2 μm to +0.1 μm.

[0066] In addition, because the variation in height of each redistribution layer from the virtual plane was in the range of −2 μm to +0.1 μm, the photosensitive insulating resin to be laminated on the upper layer was subjected to undulations during application, resulting in variations in the height of the resin trench portion 21 and variations in the dimensional resolution. In addition, the valleys of the undulations were not polished properly, resulting in some areas where copper remained as a solid film, thereby reducing the pattern resolution. The above embodiment is merely an example, and other specific details and the like can of course be modified as appropriate.

[0067] The present invention can be used in a semiconductor device having a wiring board equipped with an interposer or the like interposed between a main board and a semiconductor element. [Explanation of symbols]

[0068] 1 Support substrate 2. Peel layer 3 Photosensitive resin layer 4 Seed adhesion layer 5 Seed layer 6 Conductor Layer 7 Resist Pattern 9 Surface treatment layer 10 Solder Bumps 11 Wiring board 12 Semiconductor element (first wiring board) 14 Wiring board (second wiring board) 15 Semiconductor elements 17 Bump section 21 Resin trench part 22 Underfill 23 Sealing resin 24 Semiconductor Devices 25 Wiring Pattern 26 Rand 27 Accessory Patterns 28 Dummy Pattern 29 Wiring section 30A Ground Pattern 30B Photosensitive resin solid pattern 31 Via

Claims

1. a second wiring board joined to the semiconductor element; a first wiring board mounted on an opposing surface of the second wiring board opposite to a mounting surface on which the semiconductor element is mounted, The widths of the wiring constituting each of the first wiring board, the second wiring board, and the semiconductor element become thinner in that order when compared at their thinnest positions. The second wiring board has two or more rewiring layers stacked to form a multilayer wiring; Each of the wiring layers includes a photosensitive resin layer made of a photosensitive resin, and an opening in the photosensitive resin layer forms a resin trench portion; a wiring pattern portion filled with a conductive material as a part of the resin trench portion, a photosensitive resin solid pattern portion arranged so as to surround the wiring pattern portion, and a ground pattern consisting of a large-area pattern with a narrowest portion having a width of 1.5 mm or more arranged so as to surround the photosensitive resin solid pattern portion; a seed adhesion layer and a seed layer are formed in this order on a bottom surface of the resin trench portion, and a wiring portion made of a conductor layer formed by filling the inside of the resin trench portion with a conductive material is provided; The multilayer wiring is formed by laminating two or more conductor layers that become the wiring portion, Each rewiring layer including the wiring portion and the photosensitive resin layer has a dummy pattern including a plurality of island-shaped photosensitive resin patterns arranged at intervals of 1.5 mm or less within the ground pattern. A wiring board comprising:

2. The wiring board described in claim 1, characterized in that when the photosensitive resin solid pattern portion is a large-area pattern whose narrowest part is 1.5 mm or more in width, the wiring board has a dummy pattern consisting of a plurality of island-shaped conductor patterns made of a conductive material arranged at intervals of 1.5 mm or less within the photosensitive resin solid pattern portion.

3. The wiring board according to claim 1 or 2, characterized in that a connection via portion connecting adjacent redistribution layers has a seed adhesion layer on one side on which the first wiring board or the second wiring board is mounted, and on a side surface.

4. 4. The wiring board according to claim 1, wherein the conductive material contains copper.

5. 5. The wiring board according to claim 1, wherein the seed layer of the second wiring board is a layer containing copper.

6. 6. The wiring board according to claim 1, wherein the seed adhesion layer of the second wiring board is a layer containing titanium.

7. A wiring board including a second wiring board bonded to a semiconductor element, the second wiring board including two or more rewiring layers stacked to form a multilayer wiring, each of the wiring layers including a photosensitive resin layer made of a photosensitive resin, an opening portion formed in the photosensitive resin layer forming a resin trench portion, a part of the resin trench portion forms a wiring pattern portion filled with a conductive material, a seed adhesion layer and a seed layer are formed in this order on a bottom surface of the resin trench portion, and the resin trench portion is filled with a conductive material to form a wiring portion made of a conductor layer, The method for forming a redistribution layer includes the steps of: forming a resin trench portion in the photosensitive resin layer; providing a seed adhesion layer and a seed layer on the resin trench portion and the photosensitive resin layer; forming a solid film of a conductive material on the seed layer; a first polishing step of polishing the conductive material formed as the solid film from the laminated surface of the substrate, thereby polishing and removing unnecessary conductive material formed on the surface of the photosensitive resin layer while leaving the conductive material in the resin trench portion; a step of removing the seed adhesion layer, the seed layer, the conductor layer made of a conductive material, and the surface of the photosensitive resin layer on the substrate surface exposed by the first polishing by a second polishing, and forming a rewiring layer having a structure in which the resin trench portion is filled with a conductive material; Equipped with A method for manufacturing a wiring board, comprising repeating the above-mentioned step of forming a rewiring layer for a required number of layers to form a two-layered rewiring layer.

Citation Information

Patent Citations

  • Remote control device for camera

    JP1987047032A

  • Printed wiring board

    JP1995154039A

  • Multilayer printed-wiring board

    JP1997008465A

  • Multilayer wiring substrate

    JP2007150060A

  • Wiring board and semiconductor device

    JP2014225671A