Laser processing inside materials
The laser system corrects spherical and coma aberrations by mechanically adjusting the sample or optical elements, ensuring precise laser processing within high-index materials like diamonds, enabling both visible and invisible marks for security applications.
Patent Information
- Application Number
- JP2023020405
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-02-06
- Filing Date
- 2023-02-14
- Publication Date
- 2024-10-17
- Estimated Expiration
- 2040-01-09
AI Technical Summary
Existing laser machining techniques face challenges in controlling the size and shape of the laser focus within materials due to aberrations caused by refractive index mismatches at the material surface, particularly in high-index materials like diamonds, which affect processing efficiency and accuracy.
A laser system with optical elements configured to correct both spherical and coma aberrations by measuring the tilt of the sample surface and mechanically adjusting the sample holder or optical elements to compensate for aberrations, combined with adaptive optics for further refinement.
The system enables precise, deterministic laser processing at various depths within materials like diamonds, allowing for the creation of visible and invisible marks for security purposes, while maintaining focus integrity and reducing surface alteration.
Smart Images

Figure 0007569397000006 
Figure 0007569397000007 
Figure 0007569397000008
Abstract
Description
[Technical field]
[0001] The present invention relates to a laser system for internal laser processing of materials, and in particular to a system for creating modified areas within a sample. The laser system is particularly useful for marking gemstone rough, and particularly diamond rough. [Background technology]
[0002] Laser machining is a process that is widely used in industry. Research and development in this area over the last decade or so has led to much smaller scales of laser processing. This is made possible by using pulsed lasers with pulse durations ranging from a few hundred femtoseconds to a few picoseconds, focused with high numerical aperture lenses. The combination of energy confinement in the time and spatial dimensions results in high instantaneous focal intensity that creates material modification by nonlinear optical processes. Thus, the effect of the process can be limited to the focal region.
[0003] It is therefore desirable to improve the degree of control afforded to laser processing techniques by improving the control over the size and shape of the laser focus within the material. However, the presence of material in the path of the laser beam inevitably affects the laser (e.g. by refraction and / or reflection).
[0004] As a result, when attempting to focus inside a material, the material itself interferes with focusing the laser inside the material.
[0005] Three-dimensional laser micromachining in diamond has previously been described by Simmonds et al. (Optical Express, Vol. 19, 12 November 2011) using a dual adaptive optics system. It is described that a dual adaptive optics system facilitates femtosecond laser machining of controlled three-dimensional structures deep within the bulk of diamond. A deformable mirror is used in parallel with a liquid crystal spatial light modulator to compensate for the extreme aberrations caused by the refractive index mismatch between diamond and the target immersion medium. Aberration compensation is shown to be important for the deterministic generation of micron-scale features deeper than 50 μm, and the dual adaptive optics approach demonstrates improved machining efficiency compared to experiments using a single adaptive element. Summary of the Invention
[0006] Light focused from an objective lens into a sample will deviate from the ideal focus due to refraction at the sample's surface. The greater the difference between the refractive index of the immersion medium (e.g., air, oil, etc.) and the refractive index of the sample, the greater the effect of the aberrations on the focus. The correction determined therefore accounts for the effect of refraction at the sample's surface to counteract the deleterious aberration effects of the sample. Different factors can contribute to different types of aberrations (or aberration modes) on the focus.
[0007] The mismatch between the refractive index of the sample and the immersion medium of the focusing objective lens results in spherical aberration, which impairs the resolution and power efficiency of the process and increases the depth of focus. This problem becomes particularly pronounced for processing in diamond due to the high refractive index of the material (2.4) and the need to use optics with high numerical aperture (NA) to obtain the highest resolution. As described in the Background section, Simmonds et al. present a dual adaptive optics approach to compensate for depth-dependent spherical aberration, enabling the processing of small features deep inside high refractive index samples such as diamond.
[0008] There is another type of aberration known as coma. If a surface is tilted relative to a focusing objective lens, ideal focusing is generally not possible and coma will distort the focus. Usually the plane of incidence is made as horizontal as possible and the resulting distortion is acceptable, but for some applications (e.g. focusing inside a gemstone) it may be difficult to obtain a perfectly horizontal plane or it may be advantageous to focus through a tilted surface. Thus, by measuring the tilt of the sample and applying a correction, the effect of the tilt on the focus can be counteracted.
[0009] It is therefore understood that it is desirable to correct both spherical aberration and coma to improve focusing efficiency, especially for precise subsurface processing of materials with high refractive index, such as rough diamond. The spherical aberration may be corrected by one or more optical elements. For coma, a laser system is provided that includes a tilt measurement device configured to measure the tilt angle of the surface of the sample relative to the optical axis of the laser beam entering the surface. The coma due to the tilt angle may then be corrected. One option is to use active optical elements to correct both the spherical aberration and the coma. However, another option involves separating the spherical aberration correction from the coma correction. One or more optical elements may be provided that include components configured to correct the spherical aberration due to the refractive index mismatch at the surface of the sample where the laser beam enters, such that the laser beam is focused to a target location inside the sample. Further, a tilt measurement device configured to measure the tilt angle of the surface of the sample relative to the optical axis of the laser beam entering the surface can be provided, and a drive mechanism is provided for moving the sample holder and / or one or more of the optical elements based on the measured tilt angle to correct coma aberration due to the tilt angle.
[0010] Thus, according to one aspect described herein, there is provided a laser system for modifying a sample to form a modified region at a target location disposed within a subsurface of the sample, the laser system comprising: a laser light source configured to provide a laser beam; a sample holder for supporting the sample; one or more optical elements configured to direct a laser beam from the laser source into the sample when the sample is supported by the sample holder, the one or more optical elements being configured to focus the laser beam into the sample and including a component configured to correct for spherical aberration due to a refractive index mismatch at a surface of the sample where the laser beam enters, such that the laser beam is focused at a target location within the sample; a tilt measurement device configured to measure the tilt angle of a surface of the sample relative to an optical axis of a laser beam entering the surface; a driving mechanism for moving one or more of the sample holder and / or optical elements based on the measured tilt angle to correct coma aberration caused by the tilt angle; has.
[0011] The driving mechanism may be configured to correct coma by moving the sample holder based on the measured tilt angle to reduce the tilt angle of the sample's surface. That is, the sample holder can be rotated to reduce or eliminate coma, thus reducing or eliminating the tilt of the sample. Alternatively, or in addition, the driving mechanism can be configured to move one or more of the optical elements to tilt the optical axis of the laser beam entering from the sample's surface, thus reducing the tilt angle and correcting coma. For example, one or more of the optical elements can be rotated to reduce or eliminate the tilt of the laser beam relative to the sample's surface, thus reducing or eliminating coma.
[0012] As a further alternative, the drive mechanism may be configured to move one or more of the optical elements to produce an amount of coma that cancels sample-induced coma due to the tilt angle, in which case the tilt angle is not cancelled, but rather the coma induced in the sample due to tilt is compensated for by introducing equal and opposite coma into the laser beam.
[0013] Therefore, it will be appreciated that coma can be reduced or eliminated by mechanically moving (rotating and / or translating) one or more optical elements in the sample and / or laser system based on the tilt measurement.
[0014] Spherical aberration may also be corrected in several different ways. In one configuration, the one or more optical elements include a lens with an adjustable correction collar to correct the spherical aberration at the target location inside the sample. Alternatively, the one or more optical elements may include a lens with a fixed correction for the spherical aberration at the target location inside the sample. As a further alternative, the one or more optical elements may include a lens and a phase plate configured to correct the spherical aberration at the target location inside the sample. Yet another alternative is where the one or more optical elements include a combination of lenses configured to introduce a spherical aberration into the laser beam that partially or fully offsets the spherical aberration due to the refractive index mismatch at the surface of the sample. Yet another alternative is where the one or more optical elements include an adaptive optics element configured to correct the spherical aberration at the target location inside the sample. The adaptive optics element (or active optics element) may include a spatial light modulator (SLM). Examples of spatial light modulators include liquid crystal SLMs, such as liquid crystal on silicon SLMs (LCOS SLMs). Other examples include mirror-based adaptive optics elements, such as digital micromirror devices / deformable mirror devices. These mirror-based devices are sometimes referred to as mirror-based SLMs. Therefore, spatial light modulator can be used as a blanket term for such devices and is not necessarily limited to liquid crystal or mirror-based SLM devices.
[0015] The one or more optical elements may be pre-configured to correct spherical aberration at a certain target depth within a particular type of material. Alternatively, the one or more optical elements may be adjustable to correct spherical aberration within different sample materials and / or at different target depths. For example, the laser system may include a spherical aberration controller configured to automatically adjust the one or more optical elements to correct spherical aberration based on one or both of a database of available corrections and optical measurements of the sample.
[0016] Advantageously, the laser source is configured to provide pulsed laser light of less than 10 picoseconds, more preferably less than 1 picosecond. The very short pulsed laser light can be precisely focused to allow precise processing of the subsurface of the material without altering the surface of the sample. The laser source may also be configured to provide pulsed laser light with pulse energies between 10 nJ and 300 nJ. The particular energy will depend on the material sample being processed.
[0017] Furthermore, the one or more optical elements are configured to focus the laser beam inside the sample with a numerical aperture of at least 0.8, 1, or 1.2. For highly repeatable deterministic marking, the laser should be focused with a high numerical aperture below the sample surface. This may be possible with an air, water, or oil immersion objective. However, when focusing with a high numerical aperture below the sample surface, aberrations are of major concern. Thus, correction as described herein is necessary.
[0018] The laser system may be configured to mark gemstones, such as diamonds. In this regard, the optics and control hardware / software may be pre-configured to mark such gemstones. For example, the sample holder may be configured to hold gemstones, and the optics may be configured for a particular gemstone material, such as diamonds.
[0019] One advantageous feature of the systems and methods as described herein is that they can efficiently machine very small and larger marks at a range of different depths into materials such as diamonds. This can be advantageous for security marking of rough diamonds. It would be advantageous to be able to provide a mark visible under a 10x loupe to identify the rough diamond. However, such a visible mark can be copied. Therefore, the systems described herein can also provide a second mark that is not visible under a 10x loupe but is visible at higher magnifications to provide additional security.
[0020] In light of the above, a first mark disposed at a first depth below a surface of the rough diamond; a second mark disposed at a second depth below the surface of the rough diamond; and Also provided is a rough diamond having the first mark is visible under a 10x loupe; The second mark is not visible under a 10x loupe but is visible at higher magnifications.
[0021] The first and second marks may be disposed at different depths below the surface. For example, the difference between the depth of the first and second marks may be at least 30 micrometers. Furthermore, the first and second marks may overlap when viewed through the surface. In this regard, the systems described herein are capable of processing such marks of significantly different sizes and at significantly different depths. By providing these marks at different depths at the same lateral position, the first visible mark may be used to locate the second mark, which is more difficult to find without the first mark as a guide and is only visible under higher magnification.
[0022] The first mark may have at least one line or dot having a width parallel to the surface greater than 2 micrometers and / or a plurality of lines with a separation of less than 10 micrometers in a direction parallel to the surface. The outer dimensions of the first mark may be greater than 100 micrometers, more preferably greater than 200 micrometers. In contrast, the second mark consists of one or more lines or dots having a width parallel to the surface of 2 micrometers or less, more preferably 1 micrometer or less.
[0023] It should be noted that the configurations described above reduce or eliminate coma by mechanically moving (rotating or translating) one or more optical elements in the sample and / or laser system based on the tilt measurement. This is in contrast to an alternative configuration in which active optical elements such as a spatial light modulator (SLM) are used to correct coma. In such an alternative configuration, a sample to be modified by a laser is placed in a laser system, the tilt of the surface of the sample through which the focused laser passes is measured, a correction to be applied to the active optical elements of the laser system is determined using at least the measured tilt, and a correction is applied to the active optical elements to modify the wavefront characteristics of the laser to counteract the effect of coma on the laser focus, such that the laser that modifies the sample at the target location to generate the modified area uses a laser with the corrected wavefront characteristics. In one configuration, an active optical element such as an SLM may be used to correct both spherical aberration and coma. However, the configuration described herein provides a mechanical drive mechanism to move one or more of the sample holder and / or optical elements based on the measured tilt angle to correct the coma due to the tilt angle, while separating these aberration corrections so that the spherical aberration can be corrected by one or more of the other methods described herein. This can be advantageous in certain applications, for example in applications where the available active optical elements (e.g., spatial light modulators) do not have sufficient range or freedom to correct the aberrations. In certain applications, mechanical drive techniques can be provided in combination with active optical elements to increase the range and freedom of the laser system to correct the aberrations.
[0024] To assist in understanding the present disclosure and to show how embodiments may be carried into practice, reference is made by way of example to the accompanying drawings, in which: [Brief description of the drawings]
[0025] [Figure 1] FIG. 1 is a schematic diagram of a portion of the laser system, showing tilt of the sample introducing coma aberration. [Diagram 2] A schematic diagram of the laser system including a laser, two optical elements, and a sample holder supporting the sample. [Diagram 3] Figure 2 shows the laser system showing the sample holder (and the sample supported by the sample holder), which can be configured to rotate to reduce or eliminate sample tilt and correct for coma. [Figure 4] FIG. 3 shows the laser system of FIG. 2 illustrating that the optical components of the system can be configured to rotate to reduce or eliminate tilt of the sample (relative to the laser beam) and correct for coma aberration. [Diagram 5] 1 is a schematic diagram showing a laser system including a laser, three optical elements, and a sample holder supporting a sample, where at least one of the optical elements can be moved to generate an amount of coma that offsets the induced sample coma due to the tilt angle. [Figure 6] Schematic diagram showing markings formed inside a diamond sample at two different depths and with varying degrees of aberration correction: (A) depth 1 (e.g. 100 micrometers), no aberration correction, more pulses (e.g. 10,000), higher pulse energy, more non-deterministic marking; (B) depth 1, aberration correction applied, fewer pulses (e.g. 5), lower pulse energy, less deterministic marking; (C) depth 2 (e.g. 200 micrometers), same aberration correction as in B, more pulses (e.g. 10,000), higher pulse energy, more non-deterministic marking; (D) depth 2, novel aberration correction applied to depth 2 compared to B, fewer pulses (e.g. 5), lower pulse energy, less deterministic marking. [Figure 7A] FIG. 2 shows a graphite track written inside a diamond substrate from one view point. [Figure 7B] FIG. 2 shows another view of the graphite tracks written inside the diamond substrate. [Figure 7C]FIG. 2 shows another view of the graphite tracks written inside the diamond substrate. [Figure 7D] FIG. 2 shows another view of the graphite tracks written inside the diamond substrate. [Figure 8A] 1 is a schematic diagram showing an example of a distorted focus inside a substrate without using aberration correction. [Figure 8B] 1 is a schematic diagram showing an example of focal spot inside a substrate achieved using aberration correction; [Figure 9A] FIG. 1 shows features written on a diamond substrate: the left set of features were written using aberration correction techniques, and the right set of features were written without aberration correction techniques. [Figure 9B] FIG. 1 shows features written on a diamond substrate: the left set of features were written using aberration correction techniques, and the right set of features were written without aberration correction techniques. [Figure 10] Figure 2 shows an alternative laser system for laser repair of samples. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0026] Described herein is a laser system configured to apply aberration correction for high numerical aperture laser marking in the bulk of samples such as diamonds and other gemstone rough.
[0027] Focusing an ultrashort (sub-10 picosecond (less than 10 picoseconds), preferably sub-picosecond (less than 1 picoseconds)) pulsed laser beneath the surface of the diamond can create isolated visible marks without altering the diamond surface. Tight focusing combined with short pulse length results in a sufficiently high electric field for nonlinear absorption of the light at the focal point, either by multiphoton absorption or tunnel ionization followed by avalanche ionization. The nonlinear nature of the process means that the structural modification is confined to the focal volume of the laser, with no damage to the surrounding areas or surface of the material sample. The ultrashort nature of the pulse means that all the energy is transferred to the modification before any diffusion via heat can occur, allowing very small sub-micron marks.
[0028] As the laser breaks down the diamond lattice, small pockets of sp2-bonded carbon are induced, resulting in high local stresses accompanied by local cracking of the diamond, primarily along the 111 planes. The marks appear as dark (opaque) against a transparent background, due in part to absorption in the graphitized regions, but also to scattering from local non-uniformities in the structure.
[0029] Laser written marks can be used as permanent features for identification or hall marking of rough diamonds using QR codes, other types of codes, patterns, serial numbers, or other unique designs. Because the marks are conductive, they can also be used as laser written wires. Because the marks create localized strains that generate birefringence in the diamond, they can also be used to make optical structures such as waveguides.
[0030] For highly repeatable deterministic marking, the laser should be focused with a high numerical aperture below the diamond surface. This may be possible with air, water or oil immersion objectives. Typically, the numerical aperture NA should be greater than 0.8, preferably greater than 1, and most preferably greater than 1.2. The numerical aperture is typically less than 2.0, and more typically less than or equal to 1.5.
[0031] Aberrations are a major concern when focusing with high numerical apertures below the diamond surface. There is significant refraction of the light rays due to the large refractive index difference at the diamond surface, which is large regardless of the immersion medium chosen for the objective lens. Light rays incident at different angles are refracted differently due to Snell's law and no longer completely overlap at the focusing stage. Thus, the system is no longer purely diffraction limited and the laser focus is distorted. The distortion of the laser focus impairs resolution and negates the benefits of using a high NA lens.
[0032] When aberrations are present, the laser processing below the diamond surface becomes unstable and uncontrolled, making it impossible to deterministically produce submicron marks (submicron in the transverse direction perpendicular to the optical axis of the system) for a given pulse energy and dose. The aberrations are actually spherical aberrations, primarily from refraction at the diamond surface. The amount of spherical aberration can be calculated analytically (see Booth, 1998, Journal of Microscopy). Aberrations have been found to increase with depth inside the sample, the NA of the focusing lens, and the refractive index (RI) mismatch.
[0033] Another important aberration is first-order coma, which is associated with tilting an interface that is not perfectly perpendicular to the optical axis of the system, onto which the laser is focused. Figure 1 is a schematic diagram of a portion of a laser system showing the tilt of a sample that introduces coma.
[0034] It has previously been shown that these aberrations can be successfully corrected using adaptive optics such as liquid crystal spatial light modulators (SLMs) to impose an equal and opposite phase dispersion on the laser beam before the objective lens, restoring diffraction-limited focusing performance and enabling highly repeatable deterministic marking of submicron features for a given pulse energy and dose (see Simmonds, Optic Express, 2011 and Salter Booth patent application, 2017).
[0035] Although adaptive optics aberration correction provides a versatile solution to deterministic laser marking inside diamond, it is not the only solution. As described herein, there are other practical implementations that can provide nearly aberration-free performance and reliable laser marking.
[0036] A schematic of the laser system including a laser, two optical elements, and a sample holder supporting the sample is shown in Figure 2. Instead of using adaptive optics to correct the depth-dependent spherical aberration, other options are available: a. Many microscope objective lenses are available for purchase that contain a correction collar to eliminate spherical aberration when focusing inside the glass. Typically, a glass element inside the lens can move along the optical axis as the correction collar rotates to adjust the spherical aberration for a particular depth inside the glass. The phase of this spherical aberration can be close to the phase of the spherical aberration at a different depth that is focused inside the gemstone, and is then used to reduce the spherical aberration at that depth. b. Many microscope objectives are available that have air as the immersion medium and have a fixed correction for a particular depth inside the glass. The phase of this spherical aberration may be close to the phase of the spherical aberration at a different depth that is focused inside the gemstone and is then used to reduce the spherical aberration at that depth. c. A fixed phase plate can be purchased that exhibits any desired arbitrary phase, so one can calculate the phase required for a particular depth and objective lens, and then use this phase plate with this lens to focus at this depth inside the gemstone with no spherical aberration. d. In front of the objective lens, a combination of lenses may be aligned and adjusted in a manner similar to (a) to impart a spherical aberration to the laser beam in front of the objective lens that partially or completely offsets the spherical aberration produced by refraction at the diamond interface.
[0037] Furthermore, instead of using adaptive optics to correct the depth-dependent coma associated with sample tilt, other options are available: a mechanism for measuring the tilt of the sample (e.g., an optical microscope) and then adjusting the tilt of the sample using a mechanical mount such as a goniometer or tip / tilt stage until the tilt is less than a certain value, ideally less than 0.5 degrees, but less than 1 degree and certainly less than 2 degrees. Figure 3 shows the laser system of Figure 2 where the sample holder (and the sample supported by the sample holder) can be configured to rotate to reduce or eliminate the tilt of the sample to correct for coma. b. A mechanism (e.g., an optical microscope) for measuring the tilt of the sample, and then a mechanical mechanism for adjusting the tilt of the objective lens relative to the sample to less than the value described above. As the lens is tilted, the angles of the laser and / or other optical components may also be changed to keep the laser beam perpendicular to the back axis of the objective lens. Figure 4 shows the laser system of Figure 2 in which the optical components can be configured to rotate to reduce or eliminate the tilt of the sample and correct for coma. c. Certain optical elements, such as lenses, can also generate coma. Once the tilt of the sample is measured, the coma can be compensated for by moving the lens perpendicular to the optical axis to create the amount of coma necessary to offset the sample induced aberration. Figure 5 shows a schematic of a laser system including a laser, three optical elements, and a sample holder supporting a sample, where at least one of the optical elements can be moved to create an amount of coma that offsets the sample induced coma due to the tilt angle. d. Spatial Light Modulator (SLM) or other adaptive / active optics to correct depth-dependent spherical aberration (only) and mechanical mounting to eliminate sample tilt and coma. For example, one of the optical elements in the laser system of Figure 5 can be an SLM configured to correct spherical aberration.
[0038] The configurations and methods described herein provide for the correction / elimination of both spherical and coma aberrations for precise deterministic marking of the interior of samples such as gemstones. Any of the previously described options can be combined into a system for gemstone marking. The laser system also has an ultrashort pulsed laser, a high NA objective lens, and a 3D translation stage for mounting the gemstone sample. Spherical aberration correction can be achieved using fixed elements to allow marking at a specified depth of a specified material. However, coma correction requires some adaptability to account for errors in sample mounting.
[0039] FIG. 6 is a schematic diagram showing markings made within a diamond sample at two different depths and with varying degrees of aberration correction.
[0040] Figure 6(A) shows a marking at a depth of 1, e.g. 100 micrometers, without aberration correction. The laser focus inside the diamond sample is elongated in the depth direction with reduced energy density. Therefore, a large number of pulses (e.g. 10,000) and high pulse energy are required to form the marking in the diamond sample. The result is a large non-deterministic marking as shown.
[0041] In contrast, Figure 6(B) shows a marking at depth 1 with the aberration correction described herein applied. The laser is precisely focused inside the diamond sample to form the marking, requiring only a small number of pulses (e.g., 5) and low pulse energy. The result is a small deterministic marking as shown.
[0042] Figure 6(C) shows a marking at a depth 2, e.g. 200 micrometers, with the same aberration correction as in B applied. Due to the increased depth, the aberration correction is insufficient. Therefore, the laser focus inside the diamond sample is elongated in the depth direction with reduced energy density. Therefore, a large number of pulses (e.g. 10,000) and high pulse energy are required to form the marking in the diamond sample. The result is a large non-deterministic marking as shown.
[0043] Finally, Figure 6(D) shows the marking at depth 2 with the new aberration correction applied for depth 2 compared to B. The laser is precisely focused inside the diamond sample to form the marking while requiring only a small number of pulses (e.g. 5) and low pulse energy. The result is a small deterministic marking as shown.
[0044] Thus, it will be apparent that one of the advantageous features of the systems and methods described herein is that they can efficiently machine very small and larger marks at a range of different depths into materials such as diamonds. This can be advantageous for security marking of rough diamonds. It would be advantageous to be able to provide a mark visible under a 10x loupe to identify the rough diamond. However, such a visible mark can be copied. Therefore, the systems described herein can also provide a second mark that is not visible under a 10x loupe but is visible at higher magnifications to enhance security.
[0045] In light of the above, a first mark disposed at a first depth below a surface of the rough diamond; and a second mark disposed at a second depth below the surface of the diamond; the first mark is visible under a 10x loupe; The second mark is not visible under a 10x loupe but is visible at higher magnifications.
[0046] The first and second marks may be formed from sp2 carbon of graphite within an sp3 carbon diamond lattice. Using the laser system described herein, marks of different sizes may be easily fabricated. The first and second marks may be disposed at different depths below the surface. For example, the difference between the depth of the first mark and the depth of the second mark may be at least 30 micrometers. Furthermore, the first and second marks may overlap when viewed through the surface. In this regard, the system as described herein may fabricate such marks of significantly different sizes at significantly different depths. By providing these marks at different depths at the same lateral position (at least within the same field of view), the first visible mark may be used to locate the second mark, which is more difficult to find without the first mark as a guide and is only visible under higher magnification.
[0047] The first mark may have at least one line or dot having a width parallel to the surface greater than 2 micrometers and / or a plurality of lines with a separation of less than 10 micrometers in a direction parallel to the surface. The outer dimension of the first mark may be greater than 200 micrometers. In contrast, the second mark consists of one or more lines or dots having a width parallel to the surface of 2 micrometers or less, more preferably 1 micrometer or less.
[0048] The disclosed aberration correction system and method can achieve a laser focus with a Strehl ratio greater than 0.5 inside a sample. The method can include modifying the sample using a laser focus with a Strehl ratio greater than 0.5. The focus can have a Strehl ratio greater than 0.6, a Strehl ratio greater than 0.7, a Strehl ratio greater than 0.8, or a Strehl ratio greater than 0.9. The Strehl ratio can be understood as a measure of how close a focus is to an ideal (i.e., diffraction-limited) focus. A laser focus limited only by the intrinsic diffraction of the focusing system (i.e., a laser focus of diffraction-limited size) would have a Strehl ratio of 1. In practice, intrinsic imperfections in the optical system would result in a focus with a Strehl ratio less than 1 that is not diffraction-limited size. For a high NA lens, a Strehl ratio of about 0.1 is typical for a laser focused to a depth of, say, 100 μm in a diamond sample. Thus, the Strehl ratio may be understood as a measure of the effect of aberrations on the laser focus, with the closer the Strehl ratio is to 1, the smaller the effect of aberrations and imperfections in the system. The Strehl ratio may also be understood as a measure of the efficiency of a given focus.
[0049] The Strehl ratio can be defined as the intensity of a peak focus relative to the peak focus intensity when the system is free of aberrations. A focus limited solely by diffraction has a peak intensity I0, whereas a real system has a peak intensity I pWhen the Strehl ratio is the ratio I p When a system has aberrations, wavefront errors cause the light to diffract away from the focus, resulting in an actual peak intensity I p is reduced from the theoretical maximum I0, and hence the Strehl ratio is reduced. If the wavefront error is characterized as an aberration phase function φ, then the Strehl ratio S is given by
number
[0050] The method may include measuring a laser focus inside the sample, e.g. by photoluminescence inside the sample, and modifying a correction applied to the active optics based on the measured focus, thereby improving the focusing efficiency and / or increasing the Strehl ratio of the focusing.
[0051] The sample may have a flat surface on which the laser beam is incident, which introduces the aberrations.
[0052] The modified region may be any region within the sample that has been altered by exposure to a laser. In general, the modified region will have different properties than the bulk material that surrounds it, and may have different optical properties, structural properties, mechanical properties, electrical properties, etc.
[0053] An active optical element is any element that can dynamically modify the properties of incident light. For example, liquid crystal spatial light modulators (SLMs), deformable mirrors (or microdeformable mirrors), and adaptive lenses are active optical elements that can be used to dynamically impose a spatially varying modulation on a laser beam profile, thereby controlling, for example, its phase and / or propagation properties.
[0054] Measuring the tilt of the sample may include measuring the tilt of the sample surface relative to the propagation of the laser beam and / or measuring the tilt (i.e., tilt) relative to both horizontal directions (i.e., the two lateral dimensions perpendicular to the laser beam propagation). Measuring the tilt of the sample may include measuring the tilt of the sample surface relative to the cross-section of the objective lens. Thus, measuring the sample provides information about aberrations that may affect the focusing of the system.
[0055] The measurement may be performed by any suitable means and may include reflection from the sample surface. The measurement may include reflection from multiple points on the incident surface of the sample.
[0056] The measurement may be performed by imaging. The exact axial position of the best focus (i.e. the sharpest image) of the surface of the sample may be found at three different positions. This may be exactly about 0.5 μm in the axial direction. The three points may be separated by about 0.2 mm in the transverse direction. This separation distance may be large enough to allow accurate measurement of the tilt, given the range of tilt expected to be significant. For example, for a diamond tilt in the range of more than 0.5 degrees, there may be a large effect on the quality of focus inside the sample.
[0057] Other methods may be used to measure. If the system uses an oil immersion objective, a similar method may be used to make the same measurement as above, but instead of using the sharpest focus to see the axial position of the sample surface (which may be a problem with some samples where the surface is polished and there is nothing clear to image), a laser may be used to boil the immersion oil. That is, the laser boils the oil when focused into the immersion oil, and nothing is visible when the laser focus moves inside the sample. In this case, the pulse energy will be below the threshold for processing the inside of the sample. This method has almost the same axial accuracy as the imaging method, but may be easier to implement in some cases. However, it only works for oil-based lenses.
[0058] Another method for measuring the axial position of the sample surface relies on reflection from the surface. The reflection can be from the processing laser itself (when the pulse energy is sub-processing threshold) or from an alternative light source (e.g. laser or LED). The surface of the sample can be located where the reflected signal is maximum.
[0059] Another method may involve examining the third harmonic generation (THG) from the sample surface, which is also maximized when the surface is at the focus of the lens. Interferometric measurements using reflected light may be used to measure the surface position very accurately (an alternative coherent light source is required for the interferometer).
[0060] Another alternative method involves imaging the reflection of a laser beam from the diamond surface onto a camera, and the lateral displacement of the reflection on the camera allows the tilt of the sample to be determined from a single measurement.
[0061] Determining a correction to apply uses at least the measured tilt. This may also include determining a correction based on a depth of the modified region below the sample surface. Determining a correction may include using information about the optical properties of the sample material to account for refraction.
[0062] The method may include measuring a position of the sample within the laser system, and using the measured position to determine a correction to apply, and applying the correction to modify the wavefront characteristics of the laser to counteract the effects of spherical aberration on the laser focus. The method may include measuring a position of a laser incidence surface of the sample to determine a depth of focus. The method may further include determining the correction based at least in part on the depth of focus.
[0063] Thus, the correction may not only correct for coma due to tilt of the sample, but may also account for spherical aberration. The amount of spherical aberration may be proportional to the focal depth. Spherical aberration distorts the focal spot into a cusp shape, which causes the peak intensity of the focal spot to move axially away from the ideal position toward the aberrated surface. A focal spot affected by spherical aberration will therefore have a peak intensity near the sample surface. This movement of the focal spot is also known as defocus. By measuring the position of the sample, a correction may be determined to counteract the effect of spherical aberration. The method may include varying the axial position of the sample to account for the movement of the peak intensity of the focal spot. The method may include varying the axial position of the sample to account for the defocus component of the spherical aberration.
[0064] The method may therefore include applying corrections to account for the effects of both coma and spherical aberration due to refraction at the surface of the sample.
[0065] The method may include measuring the sample after forming the modified area and refining the correction based on the further measurement. The method may include measuring the modified area of the sample and refining the correction based on the measurement of the modified area. Thus, the method may include a feedback stage during which the correction is improved, for example to more precisely control the size and shape of the focal spot to further reduce the effect of aberrations (e.g. coma and / or spherical aberration) on the focal spot. By improving the correction, a larger Strehl ratio may be achieved. The further measurement may use a nonlinear photoluminescence excitation, which may be from an intrinsic defect inside the sample. The method may include sensing the effect of the laser modification on the sample using photoluminescence, plasma emission or absorption, or reflection or transmission properties.
[0066] Determining the correction may include using the measured tilt in a calculation to correct for coma and, if applicable, using the measured position to correct for spherical aberration. In this way, for each sample, a suitable correction may be calculated.
[0067] Determining the correction may comprise selecting a correction from a database of available corrections. Thus, the method may include selecting a particular correction to apply, for example when the tilt of the sample is within a predetermined range and / or when the position of the sample is within a predetermined range. The database may comprise a number of corrections, each for a predetermined range of coefficients.
[0068] The corrections may be defined by expanding orthogonal modes. Each mode may define an aberration mode. The corrections may be pure modes or a superposition of modes. The corrections may be defined by Zernike polynomials or expansions of Zernike polynomials.
[0069] The compensation may have a phase field for modulating a laser beam profile to a desired profile. For example, the method may use a liquid crystal spatial light modulator (SLM) and the compensation may represent a display field for the SLM. The method may use a deformable mirror (DM) and the compensation may be configured for a deformable mirror. The compensation may be configured for an adaptive lens.
[0070] The step of determining the correction may be based at least in part on the pulse energy of the laser. Thus, the correction may take into account horizontal and vertical coma, spherical aberration, and pulse energy. The pulse energy may be selected based on the correction. The method may include determining a pulse energy to be used based on the correction and the sample, and may include modifying the sample using a laser pulse of the determined pulse energy.
[0071] If the correction is sufficient, the same pulse energy may be used to process anywhere inside the sample and produce the same results. This is generally the case for the range of aberrations taken into account in this disclosure. However, if the correction is insufficient, the pulse energy may be increased.
[0072] If the correction is insufficient, the pulse energy may be increased for processing. If there are significant aberrations and the correction is far from canceling the aberrations completely, the pulse energy may be increased considerably. In some materials (e.g., especially diamond), if the correction is insufficient, accurate and reliable processing is not possible, no matter how much the pulse energy is increased. For example, at a depth of about 250 μm in diamond, single pulse laser processing is not experimentally observed, even if the spherical aberration is perfectly corrected except for a small coma aberration (e.g., about 1 radian). The pulse energy may be increased very much and still the processing may not be achieved with a single pulse. In such cases, processing cannot be achieved deterministically. Instead, the dose (i.e., the number of pulses per modified area) must be increased, and the resulting processing is large (e.g., larger than 5 μm) and poorly defined. Moreover, there may be unpredictable variations in the required dose at different positions inside the diamond.
[0073] Determining the correction may include optimizing a predetermined function. The method may include using an algorithm to determine the correction based on various factors related to the sample. The factors may include coma, spherical aberration, and pulse energy. Determining the correction may include selecting a desired correction from a three-dimensional search space, a four-dimensional search space, or a higher dimensional search space based on factors including any combination of vertical coma, horizontal coma, spherical aberration, and pulse energy. The method may include minimizing a cost function (and / or maximizing a merit function).
[0074] The method may include simultaneously modifying spatially separated regions within the sample.The method may include sequentially modifying separate regions within the sample using the same pulse energy to modify each region.
[0075] The method may include a laser modifying the sample using an array of multiple laser beams and focal spots. The method may include simultaneously modifying spatially separated areas of the sample using respective laser beams. The method may include using multiple pulses, each pulse from a respective laser beam, to modify a desired area of the sample. The method may include forming multiple beams prior to correction, and thus performing aberration correction for the spatially separated multiple laser beams using a single optical system. The method may include creating multiple laser beams to simultaneously perform aberration correction and generate multiple beams.
[0076] The step of forming the modified region may include modifying the material using nonlinear optical interactions. The method may include modifying only the material within the bulk of the sample. Thus, the method may not include modifying the surface of the sample. The method may include modifying the sample at a depth of more than 50 micrometers, 150 micrometers, or 300 micrometers.
[0077] The method may include forming a complex structure within the sample. For example, the method may include forming an array of features within the sample. The method may include moving the sample during laser modification to create linear, curved, or any suitable shape line features within the sample. The method may include scanning the laser during laser modification to create linear, curved, or any suitable shape line features within the sample. The method may include forming an optical volume in the form of spaced apart points and / or forming a diffractive element. The method may include modifying spatially separated regions within a bulk of the material. The method may include creating visible features within the sample. The method may include forming structures within the sample. The method may include forming large features, for example, larger than 5 micrometers or larger than 20 micrometers in at least one dimension. The method may include modifying a predetermined region of the sample to generate a desired stress field within the sample. The method may include creating features within the sample that shift the phase of incident light, which may be visible under phase contrast microscopy or may scatter light so as to be visible under dark field microscopy. The method may include modifying the refractive index of the sample in a predetermined region, which may be accomplished by exposing the region to a laser or by exposing a nearby region to a laser to change the strain field in the predetermined region.
[0078] The method may include using a high numerical aperture (NA) lens to focus a laser inside the sample, which may exacerbate the effects of spherical aberration. The method may include using an objective lens without an immersion medium (i.e., a dry lens) or an objective lens with an immersion medium (e.g., oil). The method may include using an objective lens with a numerical aperture greater than about 0.5. The method may include using an objective lens with a numerical aperture greater than about 0.8. The method may include using a dry objective lens with a NA greater than 0.8 or an oil immersion objective lens with a NA greater than 1.2.
[0079] The method may include modifying a gemstone or crystal lattice. In particular, the method may include using a sample having diamond. The diamond may be in the form of gemstone. The method may be used to mark the gemstone, for example as a security device.
[0080] The method may comprise the step of producing an electrical conductor inside a sample, in particular diamond. The diamond may be a substrate of grown diamond. The method may comprise the step of coating the sample (e.g. diamond) with a metal, for example to provide an electrical connection to the electrical conductor inside the sample. The method may comprise the step of modifying the diamond structure by converting carbon from sp3 to sp2 phase. The method may include the step of modifying an internal region of the diamond adjacent to the surface of the diamond.
[0081] The corrections may be defined by expanding the orthogonal modes. Each mode may define an aberration mode. The corrections may be pure modes or a superposition of modes. The corrections may be defined by Zernike polynomials or an expansion of Zernike polynomials. The corrections may be defined as a superposition of modes using an orthogonal basis other than Zernike polynomials. The corrections may be, for example, an analytical solution for a particular geometry or a numerical solution for a particular focusing geometry. The corrections may be determined by iterative optimization using methods of focus feedback. The corrections may be defined as a superposition of modes using an orthogonal basis other than Zernike polynomials. The corrections may be, for example, an analytical solution for a particular geometry or a numerical solution for a particular focusing geometry. The corrections may be determined by iterative optimization using methods of focus feedback.
[0082] The method may include calculating coefficients of a Zernike expansion to characterize the aberration mode and determine a correction. Applying the correction may include applying a superposition of Zernike modes. The magnitude of the Zernike mode may be defined by the correction. The correction may be for a single mode or a superposition of modes.
[0083] The correction can counteract the effect on focusing of a tilt aberration mode caused by the sample, the tilt aberration mode being different from a coma aberration mode caused by tilting the sample. The different aberration modes are characterized by different orders of phase change they introduce. The tilt aberration modes are characterized by different orders of phase change from the coma aberration modes. The spherical aberration modes are characterized by different orders of phase change from the coma aberration modes and the tilt aberration modes. Determining the correction can include determining an aberration mode that would be introduced into the laser focus by the sample.
[0084] For example, tilt aberration can be expressed as a phase change in the pupil of an optical system proportional to r cos(θ-ε), where (r,θ) is the polar coordinate in the pupil plane and ε is the orientation of the tilt. Coma aberration can be expressed as a phase change in the pupil of an optical system proportional to r cos(θ-ε), where (r,θ) is the polar coordinate in the pupil plane and ε is the orientation of the tilt. 3 It has components of the form cos(θ-ε), with the phase varying as the cube of the radial coordinate. Higher order radial terms with odd powers are also possible.
[0085] The method may include using a pulsed laser having a pulse energy between 10 nJ and 300 nJ. The pulse energy may be between 80 nJ and 150 nJ. The pulse energy may be greater than a threshold for modification of the sample material. The method may include using a laser having a wavelength in the UV spectrum, the visible spectrum, or the infrared spectrum. The method may include using a laser having a wavelength in the near infrared spectrum.
[0086] The method may include laser modifying the sample using a single laser pulse. The method may include modifying the sample using multiple pulses. The pulses may be femtosecond or picosecond pulses. The method may include varying pulse energy between doses.
[0087] The method may include modifying an area less than 1 micrometer in a direction of propagation.The method may include modifying an area less than 1 micrometer in each of the x, y and z directions.
[0088] The bulk of the sample may be diamond. The modified region may comprise an electrical conductor. The modified region may comprise a security code. The modified region may comprise a diffraction grating. The modified region may be less than 1 micrometer in all dimensions (i.e. less than 1 micrometer in width, height and depth). The modified region may be less than 100 micrometers, preferably less than 200 micrometers, more preferably less than 500 micrometers from the nearest surface of the sample.
[0089] Thus provided is a system and method for high resolution laser processing inside transparent materials that incorporates aberration correction to compensate for the effects of refraction at the material surface. The system uses feedback from material measurements to obtain the required level of material modification to optimize aberration correction and focal strength. A particular application is for machining features inside diamond.
[0090] Applications of the disclosed systems and methods include the creation of light guides inside glass by localized increase in refractive index. Similar structures can be created in crystals such as KDP or lithium niobate using localized increase in refractive index due to stress fields around damaged tracks in the medium. Microfluidic devices can be created by photoexposure of glass followed by chemical etching. Nonlinear photopolymerization can be used to create complex 3D polymer structures from suitable solutions.
[0091] The disclosed systems and methods can be used to create modified regions within a material that are approximately the same size as a diffraction-limited laser focus, which can be less than 1 micron in all dimensions.
[0092] (Diamond processing) When a femtosecond pulsed laser is tightly focused inside a diamond, nonlinear optical interactions modify the crystal lattice in various ways depending on the energy density at the focus. At low energies there is a small disruption of the crystal lattice, which can be used to generate color centers after annealing. At higher energies there is such a large amount of lattice disruption that there is a large conversion of carbon from the sp3 phase (diamond crystal structure) to the sp2 phase (graphite). Typically the laser modified areas take the form of amorphous carbon, which is a combination of sp2 and sp3 phases.
[0093] The fabrication of fine optical features in diamond uses a short pulsed laser and a high numerical aperture (NA) objective lens. This ensures that the surface of the material is not damaged and that the features are well confined in three dimensions inside the material. A single laser exposure can create a point-like feature of the modified material. Complex structures, which can be two- or three-dimensional, can be built using a collection of point-like features. Alternatively, linear structures can consist of closely spaced features.
[0094] There are two modes of subsurface laser processing inside diamond: (i) at very low pulse energies, highly nonlinear interactions create a population of lattice vacancies at the laser focus, and (ii) at higher pulse energies, destroying the diamond lattice and leaving a conductive graphitic phase. Modifications of mode (i) are invisible by transmission microscopy, only visible by fluorescence microscopy. They are important precursors for the formation of coherent NV (nitrogen vacancy) centers for quantum applications. Modifications of mode (ii) have small (< several hundreds of nm) clusters of sp2 bonded carbon with microcracks in the diamond lattice. Tracing diamond with a mode (ii) laser focus writes continuous tracks of sp2 bonded carbon, which can be used as conductive wires.
[0095] Features formed without diamond movement during exposure have the shape of an ellipsoid. The extent of the modification is longer along the propagation direction of the processing laser and depends on the NA (numerical aperture) of the objective lens used. The size of the feature also depends on the pulse energy and dose (number of pulses in an exposure) used. If the wavefront is well corrected as described here, a highly consistent modification from exposure to exposure is possible. If the wavefront is not well corrected as described here, different exposures under identical conditions will result in very non-uniform modifications (in size and shape).
[0096] High NA (NA > approx. 0.8) optics were used to reliably machine both types of features step by step without axial expansion (<2 μm along the optical axis). Processing with low NA (approx. 0.5) is also possible, but is highly position-dependent and inconsistent. High NA allows highly reproducible processing over large volumes with exactly the same pulse energy and laser dose. The processing is position-independent, which is important for industrial applications.
[0097] Other demonstrations have consisted of arrays of graphite point-like features. In other applications, continuous graphite structures have been produced that can be used as electrical conductors.
[0098] By tracing the laser focus on the diamond (or by scanning the laser across a fixed diamond sample), continuous tracks of laser modified material can be created. The tracks in processing mode (ii) contain sp2 bonded carbon and are electrically conductive. These tracks can be used to form conductive wires that run through the diamond in three dimensions. For example, FIG. 7 shows various continuous graphite tracks 110 tracing 2D and 3D paths below the surface 120 of a diamond sample. FIG. 7A shows a top view of the graphite track 110. FIGS. 7B and 7C show side views of the graphite track 110, and FIG. 7D shows an imaged perspective view of the written graphite track 110. Scale 125 indicates 5 μm. The dashed ovals in FIG. 7C show portions of graphite tracks that have been processed to increasing depths.
[0099] Such graphite tracks 110 can act as conductive wires, which are useful for the production of diamond-based sensors for radiation or chemical sensing. In one implementation, a voltage may be applied to both ends of a wire passing through the diamond to set up a local electric field inside the diamond. When ionizing radiation is incident on the diamond, free charges are created that pass through the diamond and are collected by electrodes. In another implementation, the embedded wires can be used for electrochemistry, taking advantage of the wide potential window of diamond. The embedded wires can be used to generate an electric field near the surface of the diamond, which is then immersed in a solution. Such laser-written embedded wires can be connected to external electronics by bringing them up to the diamond surface and later coated with metal for efficient electrical connection.
[0100] (Aberration correction) In the ideal case, the size of the laser focus should be diffraction limited, i.e. the smallest spot size possible for a given wavelength, the refractive index of the objective lens, and the numerical aperture. However, this limit is often not achieved due to the effects of aberrations. Aberrations are deviations from the ideal focusing performance of an optical system. In terms of ray optics, aberrations cause the rays in the focusing cone to not meet at the same point. In terms of radio optics, aberrations cause the wavefront converging at the focus to not take the shape of a spherical cap, which is necessary to focus to a diffraction-limited spot. In this case of radio optics, aberrations are often quantified in terms of the optical phase error between the ideal and distorted wavefronts, and different types of distortion are characterized by different phase errors. The focus is broadened or blurred by the effects of aberrations, reducing the peak intensity. Due to the nature of focusing, the broadening is mainly along the optical axis.
[0101] FIG. 8A shows an example of a particular type of aberration mode, spherical aberration. In laser processing, aberrations are often caused by refraction of light rays at the surface of a transparent material that is to be processed inside. This may occur, for example, at the interface between the immersion medium of the objective lens (typically air, oil or other medium) and the processing material. Light rays 210 entering the sample 220 are refracted by the sample surface 222, and the resulting focal spot 230 is distorted and elongated. A flat wavefront 240 means that parallel light rays 210 enter the high NA lens 250, which would be ideally focused without the sample 220.
[0102] 8B shows the case where the phase of the wavefront 240 has already been corrected by an active optical element, such as an SLM, to counteract the refraction at the sample surface 222. As a result, without the sample 220, the light rays 210 exiting the lens do not result in an ideal focus. However, with the sample present, the light rays 210 are refracted at the surface 222 resulting in an improved focus 232. Thus, by shaping the incoming wavefront, aberrations are cancelled out, allowing for precise focusing and reliable machining of sub-micrometer features.
[0103] FIG. 9A shows feature 310 (left) created by focusing using aberration correction to a depth of 50 μm inside the diamond. Feature 320 (right) is the same structure made without aberration correction. In order to fully explore all the processes, the laser pulse energy had to be increased significantly. The processing laser was incident along the z-axis. It can be seen that the processing of feature 310 is much better controlled than that of feature 320. FIG. 9B shows the same feature from the side. It can be seen that the feature created using aberration correction is significantly more controlled in the propagation direction (i.e., z-direction).
[0104] When the sample interface is perpendicular to the optical axis, the aberration consists of spherical aberration plus refocusing effects (focus shift along the optical axis). The magnitude of these effects is proportional to the focal depth. This type of spherical aberration is given by
number
[0105] If the surface normal is tilted with respect to the optical axis, then other aberrations such as coma (which involves wavefront tilt and results in a lateral focus shift) are introduced. These effects are proportional to both the depth of focus and the tilt angle of the surface. The additional aberration due to a slight tilt of the surface is given by:
number
[0106] The combination of spherical aberration and coma reduces the focal intensity and distorts the intensity distribution, adversely affecting processing efficiency and accuracy.
[0107] Due to the high refractive index of diamond (2.4 compared to 1.0 for air and about 1.5 for immersion oil), the effects of refraction at the diamond surface are large. This means that aberration correction should enable the production of fine features at depths that would otherwise be impossible. Aberration correction is easily achieved using a liquid crystal spatial light modulator (SLM), but could also be achieved using a deformable mirror. According to the configurations herein, such active optical elements can be used for spherical aberration correction. Coma aberration is corrected by mechanical movement of the sample and / or the optical elements.
[0108] Although static correction methods are possible, various tests have shown that static correction is not effective at correcting aberrations between nominally similar samples due to slight variations in material composition and positioning; instead, fine-tuned aberration correction is required.
[0109] When using dry objective lenses to focus deep into diamond, the aberration correction demands increase. When using oil immersion lenses to focus the laser, the refractive index difference is smaller than with dry lenses, so the aberration correction requirements are less. However, corrections are still necessary to get viable results.
[0110] The phase pattern calculated from the above equation can be applied to an aberration correction device (i.e. active optical element) such as a spatial light modulator (SLM) to correct the aberrations induced by the sample. Since the phase modulation range of an SLM is typically limited to one wavelength (or a small number of wavelengths), the phase is usually wrapped to fall within the usable range. For example, if only a single wavelength is usable, then a phase of 2π radians corresponds to one wavelength, so the applied phase function is φ modulo 2π. SA As previously mentioned, in accordance with configurations herein, such active optical elements can be used to correct spherical aberration, with coma being corrected by mechanical motion of the sample and / or optical elements.
[0111] The phase pattern applied to the SLM can be simplified by noting that the spherical aberration term contains defocus, which is another aberration mode or component that moves the focus (i.e. the peak light intensity) along the optical axis but does not change its shape. By removing the defocus component from the correction, the size of the phase correction is reduced and therefore the SLM can be used more efficiently for aberration correction. The defocus component of the spherical aberration can be compensated for by moving the sample by an appropriate amount.
[0112] Instead of using analytical expressions directly, the aberrations can be considered as a set of basis functions. Generally, Zernike polynomials are used for this purpose. Thus, the aberrations can be described as a sum of aberration modes. For example, spherical aberration can be expressed as an expansion of Zernike polynomial terms. The use of these functions aids in the design of feedback systems for the measurement and correction of unknown aberrations.
[0113] The methods described herein further relate to focusing through non-planar surfaces. This may include through curved surfaces or near / over edges. Again, an accurate prediction of the surface topography can be used to predict a near optimal starting phase pattern and can be used as a good starting point for subsequent optimization using focus feedback. Machining across or near an edge involves segmenting the pupil. The methods described herein can be employed to set the phase to correct spherical aberration and coma in the segmented pupil. Focusing through curved surfaces requires correcting a combination of spherical aberration, astigmatism, and coma.
[0114] (Adaptive focus control) To maintain a consistent quality of processing between different locations (especially depths) inside the sample and between different samples, an adaptive control system needs to be implemented that can maintain the right combination of aberration correction and pulse energy. This can use a feedback method from the focal region to the wavefront and energy control device.
[0115] The first measurement of the surface position and tilt based on the reflection from the material surface described above predicts the corrections required to counter spherical aberration and coma. In one implementation, measuring the position relative to the best optical focus at three points, not all on the same axis, can provide information about the relative tilt of the sample. This can make it possible to predict the aberration corrections for coma and spherical aberration at a particular depth in a sample, such as diamond.
[0116] By observing the processing at the focus by microscopy, finer compensation can be performed. A combination of measurements is possible. Using a transmission microscope it is possible to observe the change in absorption or the change in the optical phase at the focus due to refractive index modification. This indicates the extent to which the material has been modified by the laser pulse and can provide a feedback signal for aberration correction and optimization of the pulse energy. Photoluminescence or plasma emission from the focus can provide an alternative feedback signal.
[0117] To reduce the number of measurements required for the optimization process (time required), algorithms can be used in which the coefficients of the aberration modes (in particular spherical aberration and coma) and the pulse energy are considered as unknown coordinates in the search space.
[0118] The optimization process can be mathematically expressed as the minimization of a cost function f (or alternatively the maximization of a merit function g) related to the aberration components and the pulse energy, collectively represented by the symbol P. The optimal value of P is the cost function that is to be minimized.
number
number
[0119] Alternatively, the processing laser may be used below threshold to nonlinearly excite photoluminescence (PL) from intrinsic defects contained in the sample for structural modification. When aberrations are minimized, the detected PL is maximized. Similarly, when aberrations are corrected, the luminescence or fluorescence emission in a confocal microscope is maximized. Therefore, these signals can be used as a feedback mechanism to enable optimization of the cost / merit function.
[0120] Different ways of performing the optimization process are possible. If the refractive index and NA are known, the minimum number of unknown parameters that need to be optimized by tilting planes for laser processing is three: one coefficient of spherical aberration and two related to coma (i.e. two orthogonal coma components). Therefore, the process can be considered as a three-dimensional optimization problem. Another variable in the form of pulse energy can be considered, which extends the process to a four-dimensional optimization. If there are more unknowns, more variables (dimensions) will need to be taken into account in the optimization process.
[0121] Although the adaptive optimization could be performed point by point for all machined locations, it would be more practical to perform fewer optimization measurements over the field of the machining and to perform parameter interpolation over this field. This field could be a line or curve, a lateral surface, or it could extend in three dimensions. With sufficient surface measurements, a properly corrected focus (i.e. a focus with a sufficiently large Strehl ratio) can be achieved. However, the optimization procedure may be performed for each new sample.
[0122] (larger marking) Larger scale structures and markings are also possible. This may include point-like features or solid lines to create alphanumeric characters, bar codes, QR codes, or images. Such features may be grouped to form diffractive elements, holograms, or diffraction gratings. Depth ranges and areas may be up to the size of the gemstone being used (typically in the range of 3 mm in the lateral x and y directions and 1 mm in the z direction of propagation). Feature sizes may be up to 5 μm in the lateral (x and y directions) and 20 μm in the z direction of propagation. In practice, the reliable creation of larger features may be achieved by stitching together a combination of smaller scale modifications. When generating large features, care must be taken to manage the stress loading of the surrounding sample (e.g. diamond) to avoid the formation of large irregular cracks. This may be achieved by a sparse matrix of small (approximately 1 μm in scale) features that are combined to form features that appear optically large but have only minimal volumetric transformation from diamond to graphite.
[0123] (Laser Systems) The configuration of the laser system is shown in Figure 10. Additional components may be added, for example, to aid in aberration or position sensing, to perform additional aberration correction, or to make the system parallel and use multiple focal spots.
[0124] Laser system 400 includes a laser 410, a polarizer 420, a spatial light modulator (SLM) 430, a high NA objective lens 440, and a three-dimensional translation stage 450. A sample 460 is placed on stage 450 at the focal point of system 400.
[0125] The sample 460 is a diamond and is placed in the laser system 400 for modification with the laser 410. The sample 460 is then measured to inform the determination of the correction. In particular, the surface of the sample 460 where the laser is incident is measured and the tilt of this surface from the transverse axis is determined. The transverse direction is the 2D plane perpendicular to the main propagation direction of the laser. It is also the plane parallel to the main plane of the objective lens.
[0126] The tilt of the surface of the sample 460 is used to determine the expected coma aberration that will be introduced onto the laser focus. The expected aberration is then characterized in terms of Zernike modes and communicated to the SLM. The SLM is modified to indicate the necessary phase correction to modify the laser to counteract the aberration. According to the configuration described herein, the SLM can correct for spherical aberration, and coma is corrected by mechanical motion of the sample and / or optical elements.
[0127] The pulse energy of the laser system is also determined based on the calibration. The laser is set to the required pulse energy and then used to modify the diamond sample.
[0128] Following modification, the modified area of the sample is measured using transmission microscopy. The determined correction is then refined based on feedback obtained from this further measurement. The refined correction is applied and the sample is laser modified.
[0129] (Example) The diamond is mounted in the laser processing system. The objective lens is first moved axially (i.e., z-direction) to locate the diamond surface by maximizing the reflected light from the LED. The diamond is then moved transversely (XY) to the desired location for processing.
[0130] Fine positioning of the axial (z) position of the surface is achieved using a laser with low pulse energy (well below the bulk graphitization threshold, e.g. less than 30 nJ). The sample surface is found by moving the diamond axially in 100 nm steps. If an oil immersion lens is used, the diamond is moved to the point where the laser no longer boils the immersion oil. If an air lens is used, the diamond is moved until the laser no longer marks the diamond surface. Two more such measurements are taken, one by moving 0.2 mm in the x direction and the other by moving 0.2 mm in the y direction. These measurements cover an area of the sample and are used to determine the local surface slope.
[0131] The diamond is then moved axially to the desired depth for machining, where it is noted that the actual machining depth is approximately 2 times larger than the movement depth for the high NA oil immersion lens and approximately 2.7 times larger for the high NA air lens. This is because the SLM is used to correct aberrations due to refraction at the sample interface, except for defocus, which is more easily countered by moving the diamond axially as explained above. Based on the surface measurements, an aberration correction is applied to the SLM. This correction represents a spherical aberration correction based on the axial depth moved. Coma in the x and y directions is corrected by mechanically canceling the tilt angle or by moving the optical elements to cancel the coma based on the measured x and y surface tilts. A burst of 5 pulses is delivered to the diamond using a given pulse energy (e.g. 100 nJ for a 1.4 NA oil immersion lens using 780 nm wavelength light with a pulse duration of 250 fs). A transmission microscope is used to confirm that the diamond has been successfully renovated at the desired point. Preferred features should have dimensions (in the transverse direction) of about 0.5 μm and dimensions (in the axial direction) of about 1 μm, and should appear dark when viewed under a transmission microscope.
[0132] To check the processing, the imaging also needs to compensate for aberrations. It is then verified that the diamond can be subsequently modified using lower pulse energies and / or doses, up to the point where the modification is no longer visible. The desired pattern is then machined as desired into the diamond.
[0133] If no modification is visible when the diamond is illuminated with the first burst of pulses, the sample is moved a short distance (e.g. 5 μm) in the transverse direction and the aberration mode is adjusted in a systematic way by applying bursts of the laser for each setting. The diamond is moved axially between each burst and inspected to see if the diamond has been modified as desired. Once the correct setting is achieved, processing is carried out directly as described above without the need for further corrections.
[0134] Besides visible diamond modification, other metrics can be used to optimize aberration correction, for example, the nonlinear photoluminescence from diamond caused by laser focusing may be optimized to correct for aberrations. For this measurement, ensure that no processing is done by lowering the laser pulse energy (using the conditions described above, e.g., with a pulse energy of less than 20 nJ) or ideally by switching to a laser with a higher repetition rate and lower pulse energy (80 MHz repetition rate and pulse energy of less than 20 nJ). The characteristics of the focus are measured to determine the aberrations affecting the focus. Corrections can then be determined and applied to active optics to improve the Strehl ratio of the focus. If the surface is accurately measured, such adaptive correction procedures will rarely be necessary.
[0135] Although the above method may use a femtosecond infrared processing laser, the technique may be applied to processing systems of any wavelength or pulse width. For example, ultraviolet (UV) or continuous wave (CW) systems may be used. Generally, the processing laser induces an increase in the refractive index of the sample. However, in some materials, the laser can induce a decrease in the refractive index. The fabricated optical device may operate at a different wavelength to the writing laser. The device may be fabricated for any operating wavelength of the optical device.
[0136] The examples described herein should be understood as illustrative examples of embodiments of the present invention. Further embodiments and examples are envisioned. Any feature described in connection with any example or embodiment may be used alone or in combination with other features. In addition, any feature described in connection with any example or embodiment may be used in combination with one or more features of any other example or embodiment or any combination of any other example or embodiment. Moreover, equivalents and modifications not described herein may be employed within the scope of the present invention as defined in the claims.
Claims
1. A transparent material sample, comprising: a first mark disposed at a first depth below a surface of the sample; a second mark disposed at a second depth below the surface of the sample; and having the first mark is visible under a 10x magnifying glass; A transparent material sample, wherein said second mark is not visible under a 10x loupe, but is visible at higher magnifications.
2. The sample of claim 1 , wherein the first mark and the second mark are disposed at different depths below the surface.
3. The sample of claim 2 , wherein the difference between the depth of the first mark and the depth of the second mark is at least 30 micrometers.
4. The sample of claim 2 or 3, wherein the first mark and the second mark overlap when viewed through the surface.
5. 5. The sample of claim 1 , wherein the first mark comprises at least one line or dot having a width greater than 2 micrometers parallel to the surface and / or a plurality of lines with a separation of less than 10 micrometers in a direction parallel to the surface.
6. The sample of claim 1 , wherein the first mark has an outer dimension greater than 100 micrometers.
7. The sample described in claim 6, wherein the first mark has an outer dimension greater than 200 micrometers.
8. A sample described in any one of claims 1 to 7, wherein the second mark consists of one or more lines or dots parallel to the surface and having a width of 2 micrometers or less.
9. A sample described in any one of claims 1 to 8, wherein the second mark consists of one or more lines or dots parallel to the surface and having a width of 1 micrometer or less.
10. A sample described in any one of claims 1 to 9, wherein at least one of the first mark and the second mark has at least one line feature having a continuous line or a plurality of spaced points.
11. The sample described in claim 10, wherein the line feature is straight or curved.
12. A sample described in any one of claims 1 to 11, wherein the sample is a rough stone.
13. The sample of claim 1, wherein the sample is a crystal lattice.
14. A sample described in any one of claims 1 to 11, wherein the sample has diamond.
15. The sample of claim 1, wherein the sample is a diamond substrate.
16. A sample described in any one of claims 1 to 11, wherein the sample is a rough diamond.
Citation Information
Patent Citations
Method and system for laser marking within the volume of gemstones such as diamonds
JP2008531143A