Circuit board manufacturing method and circuit board

The described method for manufacturing micro-LED circuit boards addresses the high cost and time issues by using transfer and peel-off techniques, enabling efficient and cost-effective batch processing of pixel circuit chips.

JP7573407B2Active Publication Date: 2024-10-25KK TOKAI RIKA DENKI SEISAKUSHO
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2020174023
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-10-15
Publication Date
2024-10-25
Estimated Expiration
2040-10-15

AI Technical Summary

Technical Problem

Manufacturing circuit boards for driving micro-LEDs requires large-scale equipment and is costly, and the process of using a flip chip bonder is time-consuming due to the need to mount chips one by one in their original shape.

Method used

A method involving forming pixel circuits on a wafer, attaching it to a transfer substrate, thinning and etching the wafer, transferring pixel circuit chips, and peeling them onto a mounting substrate using UV tape and laser lift-off techniques to facilitate batch mounting without expensive equipment.

Benefits of technology

This method allows for the manufacturing of circuit boards for micro-LEDs in a shorter time and at lower cost without the need for large-scale equipment, enabling efficient batch processing of pixel circuit chips.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007573407000001
    Figure 0007573407000001
  • Figure 0007573407000002
    Figure 0007573407000002
  • Figure 0007573407000003
    Figure 0007573407000003
Patent Text Reader

Abstract

To shorten the manufacturing time without using a large-scaled facility that costs high.SOLUTION: A manufacturing method for a circuit board includes: forming a pixel circuit 2a on a surface of a wafer 1 and forming electrode pads 1d and 1e for connection on the pixel circuit; attaching the surface of the wafer to a first transfer substrate 3 through the pixel circuit and then thinning the wafer; etching the wafer so as to leave a wafer part 1c in a region continuing to the pixel circuit, thereby transferring a pixel circuit chip 2 consisting of the separated wafer part and the pixel circuit including the electrode pad to the first transfer substrate; attaching the first transfer substrate to a second transfer substrate 7 through the pixel circuit chip and then separating the first transfer substrate, thereby inverting the pixel circuit chip and transferring it to the second transfer substrate; attaching the second transfer substrate to a mount substrate 8 through the pixel circuit chip and then attaching and mounting the pixel circuit chip to the substrate; and separating the second transfer substrate from the substrate.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a manufacturing method of a circuit board having a pixel circuit chip that drives a micro LED, and the circuit board, and more particularly to a manufacturing method of a circuit board and the circuit board that can shorten manufacturing time without using costly large-scale equipment. [Background technology]

[0002] Compared to liquid crystal displays and organic EL (Electro Luminescence) displays, micro LED (Light Emitting Diode) displays have advantages in terms of device characteristics such as high brightness, high contrast, and high reliability. In addition, they are expected to be applied to next-generation displays, including flexible displays.

[0003] Examples of circuit boards (backplanes) for driving micro LEDs include circuit boards equipped with low temperature polycrystalline silicon thin film transistors (LTPS-TFTs) and circuit boards equipped with oxide TFTs (see, for example, Patent Document 1).

[0004] Meanwhile, as a conventional method for mounting a bare integrated circuit chip on a circuit board while it is still in the chip shape, a method for mounting a bare integrated circuit chip on a printed circuit board (circuit board) and a flip chip bonder used for this method have been known (see, for example, Patent Document 2). [Prior art documents] [Patent documents]

[0005] [Patent Document 1] JP 2018-185515 A [Patent Document 2] Japanese Unexamined Patent Publication No. 7-153784 Summary of the Invention [Problem to be solved by the invention]

[0006] However, when manufacturing a circuit board having a low-temperature polycrystalline silicon TFT or an oxide TFT as a circuit board for driving a micro LED, a problem occurs in that large-scale equipment is generally required, which is costly.

[0007] On the other hand, when considering manufacturing a circuit board for driving micro LEDs having a configuration different from that of a circuit board having low-temperature polycrystalline silicon TFTs or oxide TFTs in order to avoid the use of large-scale equipment, if a process using a flip-chip bonder as described in Patent Document 2 is incorporated, the chips are taken out one by one while still in their chip shape and mounted on a circuit board, which causes a problem of long manufacturing time.

[0008] Therefore, the present invention aims to address such problems and provide a circuit board manufacturing method and a circuit board that can shorten the manufacturing time when manufacturing a circuit board for driving a micro LED without using costly large-scale equipment. [Means for solving the problem]

[0009] In order to achieve the above object, the manufacturing method of the circuit board of the present invention is a manufacturing method of a circuit board including a pixel circuit chip including a pixel circuit for driving a micro LED, the manufacturing method including: forming pixel circuits on a surface of a silicon wafer according to a predetermined arrangement; forming electrode pads for connection on the pixel circuits; attaching the surface of the wafer to a first transfer substrate via the pixel circuits, and then thinning the wafer; etching the thinned wafer so as to leave a wafer portion in a region connected to the pixel circuits, thereby transferring a pixel circuit chip consisting of a separated wafer portion and a pixel circuit having the electrode pads to the first transfer substrate; attaching the first transfer substrate to a second transfer substrate via the pixel circuit chip, and then peeling off the first transfer substrate to invert and transfer the pixel circuit chip to the second transfer substrate; attaching the second transfer substrate to a substrate for mounting via the pixel circuit chip, and then adhering and mounting the pixel circuit chip to the substrate; and peeling off the second transfer substrate from the substrate.

[0010] In addition, in order to achieve the above object, the circuit board of the present invention comprises a pixel circuit chip having a pixel circuit for driving a micro LED, a connection electrode pad provided on one side of the pixel circuit, and a wafer portion provided on the other side of the pixel circuit and in which a silicon wafer is separated by etching, and a substrate on which the pixel circuit chip is mounted in a predetermined arrangement so as to be connected to the electrode pad. Effect of the Invention

[0011] According to the circuit board manufacturing method of the present invention, a circuit board for driving a micro LED, which has a configuration different from that of a circuit board having a low-temperature polycrystalline silicon TFT or an oxide TFT, is manufactured by the above manufacturing method, so there is no need to use costly large-scale equipment. In addition, since a predetermined number of the pixel circuit chips are mounted at once, the manufacturing time can be shortened.

[0012] According to the circuit board of the present invention, a circuit board can be provided that is manufactured by the manufacturing method of the present invention in a shortened manufacturing time without using costly large-scale equipment. [Brief description of the drawings]

[0013] [Figure 1] 3 is a flow chart showing steps of a method for manufacturing a circuit board according to the present invention. [Diagram 2] FIG. 2 is a plan view of a wafer on which pixel circuits are formed. [Diagram 3] 3 is an enlarged view of the area surrounded by the dashed line shown in FIG. 2, where (a) is a plan view and (b) is a cross-sectional view taken along line AA in (a). [Figure 4] FIG. 2 is a block diagram showing a schematic configuration of a pixel circuit. [Diagram 5] 1A and 1B are explanatory diagrams showing the configuration of a wafer including a pixel circuit on which a pair of electrode pads are formed, where (a) is a plan view and (b) is a cross-sectional view taken along line AA of (a). [Figure 6] FIG. 2 is an explanatory diagram showing a process of attaching the surface of a wafer to a first transfer substrate 3 via pixel circuits. [Figure 7] FIG. 1 is a schematic cross-sectional view showing the structure of a UV tape. [Figure 8] FIG. 2 is an explanatory diagram showing a process of thinning a wafer. [Figure 9] 11A to 11C are explanatory diagrams showing a transfer process accompanying separation of pixel circuit chips by wet etching. [Figure 10] FIG. 11 is an explanatory diagram showing a process of attaching a first transfer substrate to a second transfer substrate via a pixel circuit chip. [Figure 11] FIG. 13 is an explanatory diagram showing a step of inverting the pixel circuit chip and transferring it to a second transfer substrate. [Figure 12] 1A to 1C are explanatory diagrams showing a process of bonding and mounting a pixel circuit chip on a substrate. [Figure 13] FIG. 11 is an explanatory view showing a step of peeling off the second transfer substrate from the substrate. [Figure 14] 1A and 1B are explanatory views showing the configuration of a circuit board according to the present invention, in which FIG. [Figure 15] FIG. 2 is an explanatory diagram showing the configuration of a first micro LED display having a circuit board according to the present invention. [Figure 16] FIG. 1 is an explanatory diagram showing the configuration of a micro LED. [Figure 17] FIG. 10 is an explanatory diagram showing the configuration of a second micro LED display having a circuit board according to the present invention. [Figure 18] FIG. 2 is an explanatory diagram showing a configuration of a phosphor cell. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] Hereinafter, an embodiment of the present invention will be described in detail with reference to the accompanying drawings. Fig. 1 is a flow chart showing the steps of a method for manufacturing a circuit board according to the present invention. Fig. 2 is a plan view of a wafer having pixel circuits formed on its surface. Fig. 3 is an enlarged view of the area surrounded by dashed line R1 shown in Fig. 2, where (a) is a plan view and (b) is a cross-sectional view taken along line AA in (a). Note that the drawings described in the following embodiments may differ from the actual dimensional ratios in order to facilitate understanding of the components.

[0015] First, in forming the pixel circuit shown in FIG. 1 (step S1), a process is performed to form pixel circuits 2a shown in FIG. 3 according to a predetermined arrangement on the surface of a wafer 1 shown in FIG. 2 by applying semiconductor technology.

[0016] Here, as shown in FIG. 3(a), pixel circuits 2a for driving micro LEDs are formed on a wafer 1 at pitch intervals of P1 and P2. The pixel circuits 2a have electronic circuits composed of minute semiconductor elements formed on a silicon wafer 1, which is a substrate for manufacturing semiconductor devices. For ease of explanation, FIG. 3(a) shows an example in which the pixel circuits 2a are arranged in 4 rows and 4 columns. The wafer 1 is composed of, for example, a silicon substrate 1b having a silicon oxide film 1a (see FIG. 3(b)). T1 indicates the thickness of the wafer 1. In general, the thickness of T1 may be about 700 μm.

[0017] The above values ​​of the pitch intervals P1 and P2 are set in consideration of the final display specifications (pixel pitch). For example, the values ​​specified by P1 and P2 correspond to the minimum pixel pitch size of the target display. In practice, for example, hundreds of thousands of pixel circuits 2a are formed on the wafer 1 according to the chip specifications.

[0018] Furthermore, when configuring pixels for a larger display, for example, if the pixel pitch is an integer multiple of the array pitch, the integration density of the pixel circuits 2a formed on the wafer 1 increases accordingly, so that the pixel circuit chip 2 described below can be selectively mounted on a mounting substrate 8 (see FIG. 13(b)) to effectively utilize the pixel circuits 2a formed on the surface of the wafer 1. Details will be described later with reference to FIG.

[0019] 3, the silicon oxide film 1a of the wafer 1 is divided into a circuit formation region (silicon (Si) chip region) R2 where the pixel circuits 2a are actually formed, and a circuit non-formation region (scribe (SCB) region) R3 where the pixel circuits 2a are not formed. However, the circuit formation region R2 shown in FIG. 3(a) indicates the pixel circuits 2a and the region of the silicon oxide film 1a below the pixel circuits 2a.

[0020] Moreover, the non-circuit forming region R3 is formed only of a silicon oxide film (SiO2) 1a. Although it depends on the design rule of the wafer 1 and the configuration of the circuit board to be actually manufactured, the thickness T2 of the pixel circuit 2a is, for example, about 4 to 5 μm. By forming the region below the pixel circuit 2a in the circuit forming region R2 as having the same film configuration as the non-circuit forming region R3, the etching process described below can be performed more easily.

[0021] FIG. 4 is a block diagram showing a schematic configuration of the pixel circuit 2a. As shown in FIG. 4, the pixel circuit 2a drives a micro LED and includes a pixel driving circuit 2b and a scan circuit 2c. In this embodiment, the pixel circuit 2a combines three types of micro LEDs, for example, R (red), G (green), and B (blue), into one pixel unit, and drives the micro LED for each pixel unit. However, the pixel circuit 2a may be configured to drive not only one micro LED pixel but also multiple micro LED pixels. In addition, the pixel circuit 2a may be configured to be used in both a first method adopted in the first micro LED display 100 described later and a second method adopted in the second micro LED display 101.

[0022] The pixel driving circuit 2b is a circuit for converting the data voltages of each of RGB into currents for driving micro LEDs 10R, 10G, and 10B (see FIG. 15) described later. The scan circuit 2c is a circuit for outputting control signals for driving the pixel driving circuit 2b.

[0023] Here, the pixel circuit 2a includes, for example, three lines for transferring RGB data voltage values, one line for a selection (SEL) signal for switching on or off the light for each pixel unit, and one line for a control signal for defining the timing of light emission. The arrows pointing to input to the scan circuit 2c and the arrows pointing to output from the scan circuit 2c indicate the flow of the control signal.

[0024] In the pixel circuit 2a, pixel control signals are output according to the timing of the control signals output from the scan circuit 2c, and are input to the pixel drive circuit 2b as indicated by the white arrows (see FIG. 4). In the pixel circuit 2a, each voltage data of RGB is converted into current data for driving the LEDs, and the micro LEDs 10R, 10G, and 10B shown in FIG. 15 are current-driven at a predetermined timing. As a result, the micro LEDs 10R, 10G, and 10B emit light according to the magnitude of the current passed therethrough, enabling full-color display.

[0025] Next, in the electrode pad formation (step S2), a process is performed to form electrode pads 2d and 2e for electrical connection on the pixel circuit 2a.

[0026] 5 is an explanatory diagram showing the structure of a wafer 1 including a pixel circuit 2a on which a pair of electrode pads 2d, 2e are formed, where (a) is a plan view and (b) is a cross-sectional view taken along the line AA in (a). In particular, (a) is an enlarged plan view of the region R1 after the pair of electrode pads 2d, 2e are formed on the pixel circuit 2a. For example, the pair of electrode pads 2d, 2e (hereinafter, the electrode pads 2d, 2e may be collectively referred to as "electrode portion 2f") may be an n-side electrode pad (cathode electrode) and a p-side electrode pad (anode electrode) for the electrode pad 2d.

[0027] In step S2, in order to collectively transfer and mount a plurality of pixel circuits 2a after forming the pixel circuits 2a on the wafer 1, it is necessary to form electrode pads 2d, 2e such as UBM (Under Bump Metal) electrodes in advance using an electrolytic plating method or an electroless plating method. Since the pixel circuits 2a themselves are very small (each side of the external size of the chip is 100 to 200 μm), it is preferable that each side of the external size of the electrode pads formed on the pixel circuits 2a is, for example, 10 to 20 μm.

[0028] When dealing with such extremely small chip sizes and pad sizes, the electrolytic plating method is not efficient because it is necessary to form a separate electrode for applying an electrolytic voltage. Also, since the electrolytic plating method requires a more complicated processing process for forming the electrode, it is preferable to use an electroless plating method for forming the electrode portion 2f in terms of wiring space, processing, and cost.

[0029] In this way, by performing step S2 after forming pixel circuits 2a on wafer 1 in step S1 described above, when mounting each pixel circuit chip 2 on a mounting substrate 8 (see FIG. 12(a)) in step S8 described below, it becomes possible to collectively transfer and mount each pixel circuit chip 2 onto substrate 8. In this case, substrate 8 has an electrode configuration having bump electrodes 8a, 8b to enable this collectively transfer and mount.

[0030] Next, in step S3, a process of attaching the surface of the wafer 1 to a first transfer substrate is performed. Note that the surface of the silicon oxide film 1a laminated on the silicon substrate 1b corresponds to the surface of the wafer 1.

[0031] 6 is an explanatory diagram showing a process of attaching the surface of the wafer 1 to a first transfer substrate 3 via the pixel circuits 2a. The first transfer substrate 3 is used for transferring the pixel circuits 2a formed on the surface of the wafer 1. The first transfer substrate 3 includes a glass substrate 31 and a UV tape 32, and the UV tape 32 is separately attached onto one surface of the glass substrate 31.

[0032] 7 is a schematic cross-sectional view showing the structure of the UV tape 32. The UV tape 32 is a tape whose adhesive strength decreases when irradiated with ultraviolet light, and includes a base film 32a and an adhesive layer 32b. The base film 32a is made of polyethylene terephthalate (PET).

[0033] The adhesive layer 32b contains components such as acrylic polymers and oligomers (polymers in which a relatively small number of monomers are bonded). The thickness of the adhesive layer 32b is approximately 50 μm. The adhesive layer 32b also contains a photopolymerization initiator that initiates photopolymerization when irradiated with ultraviolet light. When irradiated with ultraviolet light, the components of the adhesive layer 32b are photopolymerized, causing the adhesive layer 32b to lose its flexibility and its adhesive strength to decrease.

[0034] Therefore, in step S3, a process is performed in which the surface of the wafer 1 is attached to the UV tape 32 of the first transfer substrate 3 so that the pixel circuit chip 2 can be easily peeled off from the first transfer substrate 3 having the adhesive layer 32b by ultraviolet light irradiation in step S7 described later.

[0035] Next, in wafer thinning (step S4), a backgrinding process is performed to thin the wafer 1. Note that backgrinding refers to a processing method for thinning the thickness of a silicon wafer by polishing the back surface of the wafer.

[0036] 8 is an explanatory diagram showing the process of thinning the wafer. In step 4, the wafer 1 is thinned using a mechanical polishing means. In this embodiment, the wafer 1 is attached to the UV tape 32 of the first transfer substrate 3, thereby fixing the wafer 1 during polishing and preventing defects such as chipping or cracking.

[0037] By performing step 4, the wafer 1 is thinned from its normal thickness T1 (for example, about 700 μm (see FIG. 6)) to a thickness T3 of 10 to 30 μm depending on the application, as shown in FIG. 8. Since the thickness of a micro LED is usually about 10 to 30 μm, the thickness of the pixel circuit 2a is adjusted accordingly.

[0038] In step S4, UV tape 32 was used for bonding onto glass substrate 31, but this is because, in addition to fixing wafer 1, it is also assumed that the UV irradiation weakens the adhesiveness of the tape surface (adhesive layer 32b) and makes it easier to replace when first transfer substrate 3 is peeled off and pixel circuit chip 2 is inverted and transferred to second transfer substrate 7 in step S7 described later. Note that, as long as replacement is possible, other adhesive tapes and adhesives may be used instead of UV tape 32.

[0039] Next, in step S5, a transfer process is performed in association with the separation of the pixel circuit chips by etching. In step S5, for example, wet etching is used as the etching. Wet etching is a processing technique used, for example, when fabricating fine circuits such as semiconductor integrated circuits, in which a circuit board is immersed in a chemical solution (chemical liquid) and unnecessary parts are removed in the chemical liquid to process the shape.

[0040] 9A to 9E are explanatory diagrams showing the transfer process associated with separation of the pixel circuit chips 2 by wet etching. Specifically, Fig. 9A to Fig. 9E are process diagrams showing the wet etching process for separating each pixel circuit chip 2 from the wafer 1 and transferring it to the first transfer substrate 3.

[0041] 9(a) is a diagram showing a state in which the wafer 1 has been thinned to a thickness of 10 to 30 μm in the above-mentioned step S4. In this state, the wafer 1 on which the pixel circuits 2a are formed and the first transfer substrate 3 are bonded together.

[0042] Next, the wet etching method will be described. In FIG. 9(b), in step S5, first, a coating layer 4 of, for example, chromium is laminated on the back surface of the wafer 1, and then, for example, a positive resist layer 5 is coated on the coating layer 4. The coating layer 4 is laminated in order to improve adhesion with the resist layer 5.

[0043] 9(c), in step S5, an exposure device (not shown) is used to mask the light-shielding portion with a light-shielding mask 6, and then the exposure light L1 is irradiated and exposed. Note that in the figure, the exposure light L1 is diagrammatically represented by an arrow.

[0044] 9(d), in the wet etching in step S5, the resist layer 5 and the coating layer 4 that are not shielded by the mask 6 are exposed to light, and then the silicon substrate 1b of the wafer 1 is etched using, for example, nitric hydrofluoric acid. Then, the silicon oxide film 1a is etched using, for example, BHF (buffered hydrofluoric acid). For the coating layer 4 and the resist layer 5, for example, a negative resist layer may be used, or a material other than chromium may be used after appropriate consideration of the adhesion between the silicon substrate 1b and the resist layer 5.

[0045] In addition, the chemical solution used in the wet etching is not particularly limited as long as it can etch the silicon substrate 1b and the silicon oxide film 1a. However, it is necessary to adjust the etching time and the portion and width of the initial etching in consideration of conditions such as the outer shape of the pixel circuit 2a and the thickness of the silicon substrate 1b.

[0046] In Fig. 9(d), the wet etching process is represented by an arrow WE. For simplicity, Fig. 9(d) shows a columnar shape, but in reality, the wafer portion 1c will eventually have a trapezoidal shape, as shown in Fig. 9(e).

[0047] FIG. 9(e) shows the shapes of the first transfer substrate 3 and the pixel circuit chip 2 after wet etching and peeling off the resist layer 5 and the coating layer 4 on the wafer portion 1c.

[0048] In step S5, wet etching is performed on the thinned wafer 1 so as to leave a wafer portion 1c (see FIG. 9(e)) in an area connected to the pixel circuit 2a. As a result, in step S5, a pixel circuit chip 2 consisting of the separated wafer portion 1c and the pixel circuit 2a having the electrode pads 2d, 2e can be transferred to the first transfer substrate 3. The wafer portion 1c is composed of a silicon oxide film 1a and a silicon substrate 1b.

[0049] In step S5, by using a wet etching method, a large amount of chips can be separated in a shorter time than, for example, a laser dicing method.

[0050] Furthermore, in the wet etching method, the processes other than the formation of the chromium coating layer 4 are mainly chemical treatments, so there is no need to use large-scale equipment, and processing can be performed at lower cost and in a smaller space.

[0051] Since the wet etching method is an isotropic etching, as described above, in Fig. 9(e), the shape of the wafer portion 1c of the pixel circuit chip 2 after the wet etching process is a trapezoid (tapered) shape. That is, the process S5 is characterized in that the wafer portion 1c is made trapezoidal by performing wet etching. However, the trapezoidal shape shown in Fig. 9(e) is only an example, and the shape is not limited to this.

[0052] 9(e), the area where one surface of the wafer portion 1c is in contact with the pixel circuit 2a is larger than the area of ​​the Si surface where the silicon substrate 1b is exposed. In the case of forming the trapezoidal shape in this way, the area of ​​the Si surface can be processed to be small, and therefore, in the step S8 described later, when bonding to the substrate 8, the bonding area with the adhesive layer 72 can be reduced, which has the advantage of making it easier to separate from the adhesive by laser irradiation.

[0053] Next, in step S6, a process of attaching the first transfer substrate 3 to the second transfer substrate 7 via the pixel circuit chip 2 is performed.

[0054] Fig. 10 is an explanatory diagram showing the process of attaching the first transfer substrate 3 to the second transfer substrate 7 via the pixel circuit chips 2. Fig. 10 shows the state after a plurality of pixel circuit chips 2 have been attached to the second transfer substrate 7. The second transfer substrate 7 has an adhesive layer 72 on one surface of a glass substrate 71.

[0055] 10, the electrode pad surface of the pixel circuit chip 2 is attached to the glass substrate 31 via the UV tape 32 on the first transfer substrate 3. In this state, mounting on the substrate 8 cannot be performed in the subsequent step S8, so the electrode pad surface of the pixel circuit chip 2 needs to be turned over.

[0056] Therefore, in step S6, the pixel circuit chip 2 is bonded to the second transfer substrate 7 having a glass substrate 71 and an adhesive layer 72 thereon. The adhesive layer 72 is made of, for example, a thermosetting adhesive.

[0057] Next, in step S7, the first transfer substrate 3 is peeled off, and the pixel circuit chip 2 including the wafer portion 1c is inverted and transferred to a second transfer substrate 7.

[0058] 11 is an explanatory diagram showing the process of inverting the pixel circuit chip 2 and transferring it to the second transfer substrate 7. In step S7, for example, an ultraviolet irradiation device (not shown) is used to irradiate the first transfer substrate 3 with ultraviolet light having a central wavelength of 365 nm. FIG. 11(a) shows the state in which the first transfer substrate 3 is irradiated with ultraviolet light UV. In the figure, the process of irradiating ultraviolet light UV is diagrammatically represented by arrows.

[0059] Specifically, in step S7, ultraviolet light UV is applied from the glass substrate 31 side to reduce the adhesive strength of the UV tape 32, and the first transfer substrate 3 is peeled off. In other words, the pixel circuit chip 2 is peeled off from the first transfer substrate 3. This is because the adhesive strength of the adhesive layer 72 of the second transfer substrate 7 to the pixel circuit chip 2 is stronger than the adhesive strength of the adhesive layer 32b (see FIG. 7) of the first transfer substrate 3 to the pixel circuit chip 2. FIG. 11(b) shows the pixel circuit chip 2 transferred to the second transfer substrate 7 after being inverted.

[0060] Next, in the process of adhering and mounting the pixel circuit chip on a mounting substrate (step S8), the second transfer substrate 7 is attached to the mounting substrate 8 via the pixel circuit chip 2, and then the pixel circuit chip 2 is adhered to the substrate 8 for mounting. This substrate 8 controls the pixel circuit chip 2, and is, for example, a flexible printed circuit board (FPC (Flexible Printed Circuits) board). A flexible printed circuit board is a film-like circuit board made of an insulating base film (for example, polyimide) and a wiring layer on which an electric circuit is formed. Note that controlling the pixel circuit chip 2 means controlling the pixel circuit 2a in the pixel circuit chip 2.

[0061] FIG. 12 is an explanatory diagram showing a process of bonding and mounting the pixel circuit chip 2 on the substrate 8. FIGS. 12(a) and 12(b) are process diagrams showing the mounting of the pixel circuit chip 2 on the substrate 8. In step S8, the substrate 8 designed to be bonded to the electrode pad pattern of the pixel circuit 2a of the pixel circuit chip 2 is prepared in advance (see FIG. 12(a)). Then, in step S8, after alignment with the pixel circuit chip 2, mounting is performed by bonding connection (see FIG. 12(b)). The pattern surface of the FPC electrode may be subjected to a surface treatment using, for example, Au, Sn, or the like, and the electrodes may be bonded to the electrode portion 2f on the pixel circuit 2a side by a method such as thermocompression bonding. Bump electrodes 8a, 8b of Au, or the like may be formed on the electrode pattern on the FPC side.

[0062] Next, in step S9, a process of peeling the second transfer substrate 7 from the substrate 8 is performed by laser lift-off. In other words, the pixel circuit chip 2 is peeled off from the second transfer substrate 7. The second transfer substrate 7 can be easily peeled off from the substrate 8 by laser lift-off.

[0063] Fig. 13 is an explanatory diagram showing a step of peeling off the second transfer substrate 7 from the substrate 8. Specifically, Fig. 13(a) illustrates a state during laser lift-off, and (b) illustrates a state after laser lift-off has been performed.

[0064] 13(a), the LLO (Laser Lift Off) method is used to irradiate the adhesive layer 72 with a laser from the rear surface of the second transfer substrate 7, and the pixel circuit chip 2 can be separated by irradiating the adhesive layer 72 with a laser. In this case, in the LLO (Laser Lift Off) method, a laser beam L2 is irradiated toward the adhesive layer 72 region attached to the exposed Si surface of the silicon substrate 1b of the wafer portion 1c. For ease of explanation, in order to distinguish between the individual pixel circuit chips 2, in FIG. 13, the individual pixel circuit chips 2 are referred to as pixel circuit chips 21, 22, 23, and 24.

[0065] In detail, when laser light L2 of a specific frequency is irradiated to the interface between the adhesive layer 72 and the glass substrate 71 by the above-mentioned LLO method, the temperature of the interface between the adhesive layer 72 and the glass substrate 71 rises, and the layer portion bonding the adhesive layer 72 to the glass substrate 71 is baked (destroyed), and as a result, it becomes possible to easily peel off the second transfer substrate 7.

[0066] More specifically, in the LLO method, pulsed laser light L2 is irradiated from the rear surface of the second transfer substrate 7 to peel off each of the pixel circuit chips 21, 22, 23, 24 from the second transfer substrate 7. In step S9, specifically, a laser lift-off device (not shown) is used to adjust parameters such as laser power, the irradiation area of ​​the laser light L2, and the number of irradiations based on pulse irradiation, to peel off the pixel circuit chips 21, 22, 23, 24 from the second transfer substrate 7. Here, the parameters include, for example, a pulse laser of 1 Hz to 100 kHz (pulse width: 1 psec to 10 nsec), 100 to 1000 mJ / cm 2 The optimum conditions are selected from among the energy densities of the order of magnitude.

[0067] When performing laser lift-off in step S9, it is preferable to use, for example, a picosecond pulse laser with a wavelength of 266 nm, which is the fourth harmonic (FHG: Fourth-Harmonic Generation), generated by a solid-state UV region YAG (Yttrium Aluminum Garnet) laser oscillator.

[0068] Next, in step S9, the second transfer substrate 7 is peeled off from the substrate 8, thereby forming a circuit board 9 manufactured by the circuit board manufacturing method of the present invention, as shown in FIG. 13(b).

[0069] 14 is an explanatory diagram showing the configuration of a circuit board according to the present invention, where (a) is a plan view and (b) is a front view. In FIG. 14, a pixel circuit chip 2 mounted on a substrate 8 is a circuit board 9 manufactured by the circuit board manufacturing method of the present invention. That is, the circuit board 9 includes a pixel circuit 2a for driving a micro LED, electrode pads 2d and 2e for connection provided on one side of the pixel circuit 2a, a pixel circuit chip 2 having a wafer portion 1c in a state in which a silicon wafer 1 is separated by etching provided on the other side of the pixel circuit 2a, and a substrate 8 on which the pixel circuit chip 2 is mounted according to a predetermined arrangement such that the electrode pad 2d is connected to the bump electrode 8a and the electrode pad 2e is connected to the bump electrode 8b.

[0070] Specifically, the circuit board 9 has a configuration including, for example, an FPC backplane (substrate 8) and a silicon chip (pixel circuit chip 2). This configuration does not require large-scale capital investment, unlike backplanes using conventional low-temperature polycrystalline silicon TFTs or oxide TFTs.

[0071] As described above, it is preferable that the wafer portion 1c of the circuit board 9 has a trapezoidal shape so that separation from the adhesive by laser irradiation can be more easily performed in step S9.

[0072] In step S9, laser lift-off is used as a means for peeling off the second transfer substrate 7 from the substrate 8. However, a means for selectively performing laser lift-off on each of the pixel circuit chips 21, 22, 23, 24 may also be adopted.

[0073] In this embodiment, when a carrier material such as the second transfer substrate 7 is used, for example, the arrangement pitch P1 (see FIG. 3) of the pixel circuits 2a of the pixel circuit chip 2 to be transferred does not need to be the same as the pixel pitch of the substrate 8. That is, in this embodiment, for example, the pixel pitch on the substrate 8 may be an integer multiple of the arrangement pitch P1 of the pixel circuits 2a. For example, in FIG. 13(a), if the pixel pitch is twice the arrangement pitch P1, this means that the arrangement pitch P1 is a half pitch with respect to the pixel pitch. In this case, in step S9, only the pixel circuit chips 21 and 23 may be peeled off from the second transfer substrate 7 by selective laser lift-off, and only the pixel circuit chips 21 and 23 may be mounted on the substrate 8. Note that the pixel circuit chips 22 and 24 remain on the second transfer substrate 7.

[0074] Then, using this second transfer substrate 7, the pixel circuit chips 22, 24 remaining on the other substrate 8 may be peeled off from the second transfer substrate 7 by selective laser lift-off, so that only the pixel circuit chips 21, 23 are mounted on the substrate 8.

[0075] As a result, in the above step S9, only the pixel circuit chip 2 to be used for mounting can be lifted off, and the remaining pixel circuit chip 2 can be used for the next mounting substrate, leading to cost reduction. In other words, in step S9, the pixel circuit chip 2 transferred to the second transfer substrate 7 can be effectively utilized according to the integration degree. This means that the pixel circuits 2a formed on the surface of the wafer 1 can be effectively utilized.

[0076] In step S9, ultraviolet light irradiation may be used as a means for peeling off the second transfer substrate 7 from the substrate 8. As described above, when the UV tape 32 shown in Fig. 7 is used instead of the adhesive layer 72, ultraviolet light irradiation weakens the adhesive strength of the adhesive layer 32b of the UV tape 32, making it possible to easily peel off the second transfer substrate 7. In this case, the laser light L2 shown in Fig. 13(a) is replaced with ultraviolet light UV (not shown).

[0077] Also, in step S9, as a means for peeling off the second transfer substrate 7 from the substrate 8, selective ultraviolet irradiation may be used in the same manner as selective laser lift-off, in which only the pixel circuit chip 2 to be used for mounting is mounted on the substrate 8, and then the second transfer substrate 7 is peeled off. This allows the pixel circuit chip 2 remaining on the second transfer substrate 7 to be used for the next substrate to be mounted, even by selective ultraviolet irradiation, leading to cost reduction. In other words, in step S9, the pixel circuit chip 2 transferred to the second transfer substrate 7 can be effectively utilized according to the degree of integration, even by selective ultraviolet irradiation.

[0078] As described above, by performing a series of processes from step S1 to step S9 shown in FIG. 1 based on the circuit board manufacturing method of the present invention, it is possible to manufacture a circuit board 9 having a pixel circuit chip 2 mounted on a substrate 8.

[0079] In the above embodiment, wet etching is used as the etching in step S5, but the present invention is not limited to this, and for example, dry etching in which etching is performed in plasma may be used. Therefore, the etching includes wet etching and dry etching.

[0080] Next, a first micro LED display having a circuit board according to the present invention will be described. Fig. 15 is an explanatory diagram showing the configuration of a first micro LED display 100 having a circuit board according to the present invention. Fig. 16 is an explanatory diagram showing the configuration of a micro LED.

[0081] The first micro LED display 100 adopts a first method of combining three types of micro LEDs, R (red), G (green), and B (blue), into one pixel unit to achieve full color display.

[0082] The first micro LED display 100 includes a circuit board 9a, which includes micro LEDs 10R, 10G, and 10B as the light-emitting unit 10, a pixel circuit chip 2 as a driving unit, and a substrate 8a on which the light-emitting unit 10 and the pixel circuit chip 2 are mounted according to a predetermined arrangement. In FIG. 15, as an example, the light-emitting unit 10 and the pixel circuit chip 2 are arranged in 4 rows and 4 columns. Here, if the arrangement of the light-emitting unit 10 is m rows and n columns, and the arrangement of the pixel circuit chip 2 is m rows and n columns, m and n are natural numbers, the pixel circuit chip 2 and the light-emitting unit 10 having the same index value are associated with each other. For example, if the arrangement of the pixel circuit chips 2 located in the area surrounded by the dashed line R4 is 1 row and 1 column, and the arrangement of the light-emitting unit 10 is 1 row and 1 column, the pixel circuit chip 2 arranged in 1 row and 1 column drives the light-emitting unit 10 arranged in 1 row and 1 column. In other words, one pixel circuit chip 2 controls the emission of one light-emitting unit 10.

[0083] 16, the configuration will be described using the micro LED 10B shown in FIG. 15 as an example. The micro LED 10B is a blue light emitting diode, and has a main body 10a, an anode electrode 10b for light emission and a cathode electrode 10c on one side of the main body, and a light emitting surface 10d for emitting light from the main body 10a on the other side. The micro LED 10R has a main body 10a that is a red light emitting diode, and the micro LED 10G has a main body 10a that is a green light emitting diode.

[0084] In the circuit board 9a, the substrate 8a is connected to the pixel circuit chip 2 and the light-emitting unit 10 by wiring (not shown). In detail, the anode electrode 10b and the cathode electrode 10c of each of the micro LEDs 10R, 10G, and 10B as the light-emitting unit 10 are electrically connected via bump electrodes (not shown) provided on the substrate 8a. As a result, the micro LEDs 10R, 10G, and 10B are mounted on the substrate 8a in a state in which they can be electrically connected to each other.

[0085] With the above configuration, in the first micro LED display 100, each pixel circuit chip 2 is controlled by a separately prepared control circuit such as a driver IC (not shown), and the micro LEDs 10R, 10G, and 10B can perform full-color display in response to external power.

[0086] Next, a second micro LED display including a circuit board according to the present invention will be described. Figure 17 is an explanatory diagram showing the configuration of a second micro LED display 101 including a circuit board according to the present invention.

[0087] The second micro LED display 101 adopts a second method of achieving full color display by combining micro LEDs that emit short wavelength light such as ultraviolet light emitting diodes (UV-LEDs) with RGB phosphors.

[0088] The second micro LED display 101 includes a circuit board 9b, which is composed of phosphor cells 11 for emitting light, a pixel circuit chip 2 as a driving unit, and a substrate 8b on which the phosphor cells 11 and the pixel circuit chip 2 are mounted according to a predetermined arrangement.

[0089] Fig. 18 is an explanatory diagram showing the configuration of a phosphor cell 11. (a) is an enlarged plan view of the phosphor cell 11 shown in Fig. 17, (b) is a cross-sectional view taken along line BB in Fig. 18(a), and (c) is a front view of a micro LED 12.

[0090] As shown in FIG. 18(b), the phosphor cell 11 includes a fluorescent light-emitting layer 11a, a micro LED 12, and a planarizing film 13.

[0091] The fluorescent light-emitting layer 11a has a fluorescent material layer 11R filled with a red fluorescent pigment, a fluorescent material layer 11G filled with a green fluorescent pigment, and a fluorescent material layer 11B filled with a blue fluorescent pigment. These fluorescent pigments are examples of RGB phosphors. The fluorescent light-emitting layer 11a converts the wavelengths of the red, green, and blue fluorescent pigments into red (R), green (G), and blue (B) fluorescence, respectively, to realize a full-color display.

[0092] Specifically, the fluorescent pigments in the fluorescent material layers 11R, 11G, and 11B transition to an excited state by the light (excitation light) emitted from the micro LED 12, and then when they return to the ground state, they emit fluorescent light corresponding to the visible spectrum of red (R), green (G), and blue (B) that have been wavelength-converted by each fluorescent material. These fluorescent material layers 11R, 11G, and 11B are partitioned by partition walls 15 having a reflective metal film 14 on the surface to prevent color mixing.

[0093] As shown in FIG. 18(c), the micro LED 12 has a main body 12a, an anode electrode 12b for light emission and a cathode electrode 12c on one side of the main body, and a light emission surface 12d for emitting light from the main body 12a on the other side. The main body 12a of the micro LED 12 is manufactured using, for example, gallium nitride (GaN) as a main material. The micro LED 12 may be an ultraviolet light emitting diode (UV-LED) or an LED that emits blue light. In this embodiment, for example, in consideration of the conversion efficiency of RGB phosphors, an ultraviolet light emitting diode (UV-LED) that emits light corresponding to a peak wavelength of 385 nm may be selected.

[0094] The planarization film 13 is formed in a flat plate shape and adheres to the peripheral side surfaces of the micro LEDs 12 to hold them.

[0095] With the above configuration, each pixel circuit chip 2 is controlled by a separately prepared control circuit such as a driver IC (not shown), and the phosphor cell 11 can perform full-color display according to the power from the outside. In this case, in the pixel circuit 2a shown in FIG. 4, since the first method is changed to the second method, the wiring (three lines) for transferring the data voltage values ​​of RGB transfers the data voltage values ​​of each micro LED 12 corresponding to the RGB of the RGB phosphor to emit the above-mentioned fluorescence. Then, in the pixel circuit 2a, each voltage data in the second method is converted into current data for driving the LED, and each micro LED 12 shown in FIG. 18(b) is current-driven at a predetermined timing. As a result, the phosphor cell 11 emits light according to the magnitude of the current passed therethrough, enabling full-color display.

[0096] Therefore, the pixel circuit 2a corresponds to a first method of combining three types of micro LEDs, for example R (red), G (green), and B (blue), into one pixel unit to realize a full-color display, and a second method of combining a micro LED that emits short-wavelength light such as an ultraviolet light-emitting diode (UV-LED) with an RGB phosphor to realize a full-color display, and is characterized in that the micro LED is driven according to the first method or the second method. As a result, the circuit board according to the present invention can be used for both the first method and the second method, thereby increasing versatility.

[0097] As described above, by using the circuit board manufacturing method of the present invention, unlike backplanes using conventional low-temperature polycrystalline silicon TFTs or oxide TFTs, large-scale capital investment is not required. Furthermore, by utilizing existing semiconductor equipment, a circuit board can be manufactured at low cost using the circuit board manufacturing method of the present invention, and a micro LED display equipped with this circuit board can be manufactured.

[0098] In addition, by simply changing the design of the size, resolution, etc. of the FPC or other substrate, and performing the selective laser lift-off or selective UV irradiation described above, it is possible to accommodate displays of different sizes and specifications. This allows for flexible response to requests for high-mix, low-volume production.

[0099] In addition, since the circuit board manufactured by the manufacturing method of the present invention uses a silicon semiconductor with excellent driving capability, the driving capability is about 10 times that of a circuit board that uses an LTPS semiconductor or an oxide semiconductor. From the viewpoint of the luminous efficiency characteristics of micro LEDs, it is possible to ensure sufficient driving capability for PWM (Pulse Width Modulation) driving, which is necessary to drive a micro LED device.

[0100] Furthermore, in the case of silicon semiconductors, if further miniaturization is possible while maintaining sufficient transistor characteristics, it is possible to mount more transistors in the same area. Therefore, in the above-mentioned embodiment, in addition to the pixel drive circuit 2b, it is possible to integrate necessary circuit functions such as a scan circuit 1c that is usually arranged outside the display area, in the pixel circuit 2a, as shown in Figure 4. Furthermore, the pixel circuit 2a may include a circuit for converting, for example, input RGB parallel data into RGB serial data, as necessary.

[0101] By integrating these functions, it is possible to reduce the number of connection terminals by minimizing the number of wires inside the display, and to reduce the number of circuits that are usually placed outside the display area. This is expected to improve reliability by reducing poor terminal connections inside the display, and reduce costs by reducing external circuits.

[0102] The above-described embodiment is shown to the extent that the present invention can be understood and practiced, and the present invention is not limited thereto. The present invention can be changed and modified in various ways without departing from the scope of the technical ideas shown in the claims. [Explanation of symbols]

[0103] 1...Wafer 1c…Wafer part 2, 21, 22, 23, 24...Pixel circuit chip 2a...Pixel circuit 2d, 2e...Electrode pads 3...First transfer substrate 7...Second transfer substrate 8, 8a, 8b...Substrate 9, 9a, 9b...Circuit board 10R, 10G, 10B, 12…Micro LED 100…The first micro LED display 101…the second micro LED display

Claims

1. A method for manufacturing a circuit board including a pixel circuit chip including a pixel circuit for driving a micro LED, comprising: forming pixel circuits on a surface of a silicon wafer according to a predetermined arrangement; forming a connection electrode pad on the pixel circuit; a surface of the wafer is attached to a first transfer substrate via the pixel circuit, and then the wafer is thinned; Etching the thinned wafer so as to leave a wafer portion connected to the pixel circuit, thereby transferring a pixel circuit chip consisting of a separated wafer portion and the pixel circuit having the electrode pad to the first transfer substrate; attaching the first transfer substrate to a second transfer substrate via the pixel circuit chip, and then peeling off the first transfer substrate to invert the pixel circuit chip and transfer it to the second transfer substrate; affixing the second transfer substrate to a mounting substrate via the pixel circuit chip, and then bonding the pixel circuit chip to the substrate for mounting; peeling the second transfer substrate from the substrate; A method for manufacturing a circuit board, comprising:

2. 2. The method for manufacturing a circuit board according to claim 1, wherein the etching is wet etching.

3. 3. The method for manufacturing a circuit board according to claim 2, wherein the wafer portion is formed into a trapezoidal shape by performing the wet etching.

4. 4. The method for manufacturing a circuit board according to claim 1, wherein a laser lift-off is used as a means for peeling off the second transfer substrate from the substrate.

5. 4. The method for manufacturing a circuit board according to claim 1, wherein ultraviolet light is used as a means for peeling off the second transfer substrate from the substrate.

Citation Information

Patent Citations

  • JP153784A

  • JP185515A

  • Formation of display transistor array panel

    JP1999142878A

  • Liquid ejecting head, its manufacturing method and liquid ejecting apparatus

    JP2009166410A

  • Display device manufacturing method, chip component transferring method, and transferring member

    JP2019015899A