Electrochemical Cell
The electrolyte layer's thinning end portion addresses damage issues in electrochemical cells by reducing thermal stress, enhancing heat retention and preventing cracks.
Patent Information
- Application Number
- JP2024506000
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2022-03-08
- Filing Date
- 2023-02-16
- Publication Date
- 2024-11-01
- Estimated Expiration
- 2043-02-16
AI Technical Summary
Existing electrochemical cells face issues with damage to the electrolyte layer due to heat radiation from the metal support, leading to potential cracks and corner cracks.
The electrolyte layer is designed with a first end portion that covers the metal support's main surface, gradually thinning as it approaches the sides, thereby reducing thermal stress and preventing damage.
This design effectively suppresses damage to the electrolyte layer while improving heat retention in the electrochemical cell.
Smart Images

Figure 0007577244000001 
Figure 0007577244000002 
Figure 0007577244000003
Abstract
Description
[Technical field]
[0001] The present invention relates to electrochemical cells. [Background technology]
[0002] In electrochemical cells (electrolysis cells, fuel cells, etc.), a structure in which a cell body is supported by a metal support is known. For example, the electrochemical cell described in Patent Document 1 includes a cell body in which a first electrode layer, an electrolyte layer, and a second electrode layer are laminated in this order on a main surface of a metal support. The electrolyte layer covers the first electrode layer, and an end of the electrolyte layer is connected to the main surface of the cell body. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Patent Publication No. 2020-155337 Summary of the Invention [Problem to be solved by the invention]
[0004] In order to improve the heat retention of an electrochemical cell, it is effective to suppress heat radiation from the metal support by covering the main surface of the metal support with the end of the electrolyte layer. However, if the end of the electrolyte layer is formed up to the end of the main surface of the metal support, damage (such as corner breaks and cracks) is likely to occur at the end of the electrolyte layer.
[0005] An object of the present invention is to provide an electrochemical cell capable of suppressing damage to an electrolyte layer. [Means for solving the problem]
[0006] An electrochemical cell according to one aspect of the present invention includes a cell body and a metal support. The cell body has a first electrode layer, a second electrode layer, and an electrolyte layer disposed between the first and second electrode layers. The metal support has a main surface that supports the cell body and a plurality of supply holes. The electrolyte layer has a first end that covers a first side of the main surface. The first end becomes thinner as it approaches the first side in a direction parallel to the main surface. Effect of the Invention
[0007] According to the present invention, it is possible to provide an electrochemical cell capable of suppressing damage to an electrolyte layer. [Brief description of the drawings]
[0008] [Figure 1] FIG. 1 is a plan view of an electrolysis cell according to an embodiment. [Diagram 2] FIG. 2 is a cross-sectional view taken along line AA of FIG. [Diagram 3] FIG. 3 is a partially enlarged view of FIG. [Figure 4] FIG. 4 is a partially enlarged view of FIG. [Diagram 5] FIG. 5 is a cross-sectional view of an electrolyte layer according to the fourth modification. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] (Electrolysis cell 1) Fig. 1 is a plan view of an electrolysis cell 1 according to an embodiment. Fig. 2 is a cross-sectional view taken along line AA in Fig. 1. The electrolysis cell 1 is an example of the "electrochemical cell" according to the present invention.
[0010] The electrolysis cell 1 is formed in a plate shape. The electrolysis cell 1 is formed in a rectangular shape extending in the longitudinal direction (Y-axis direction) in a plan view.
[0011] As shown in FIG. 2, the electrolysis cell 1 includes a cell main body 10, a metal support 20, and a flow path member 30.
[0012] [Cell body 10] The cell main body 10 has a hydrogen electrode layer 6 (cathode), an electrolyte layer 7, a reaction prevention layer 8, and an oxygen electrode layer 9 (anode). The hydrogen electrode layer 6, electrolyte layer 7, reaction prevention layer 8, and oxygen electrode layer 9 are laminated in this order from the metal support 20 side. The hydrogen electrode layer 6, electrolyte layer 7, and oxygen electrode layer 9 are essential components, while the reaction prevention layer 8 is optional.
[0013] [Hydrogen electrode layer 6] The hydrogen electrode layer 6 is disposed between the metal support 20 and the electrolyte layer 7. The hydrogen electrode layer 6 is supported by the metal support 20. In detail, the hydrogen electrode layer 6 is disposed on a first main surface 20S of the metal support 20. The hydrogen electrode layer 6 covers an area of the first main surface 20S of the metal support 20 in which a plurality of supply holes 21 are provided. The hydrogen electrode layer 6 may extend into each supply hole 21. The hydrogen electrode layer 6 is an example of a "first electrode layer" according to the present invention.
[0014] A source gas is supplied to the hydrogen electrode 6 through each supply hole 21. The source gas contains at least H2O.
[0015] When the raw material gas contains only H2O, the hydrogen electrode 6 produces H2 from the raw material gas in accordance with the electrochemical reaction of water electrolysis shown in the following formula (1). Hydrogen electrode 6: H2O+2e - →H2+O 2- (1)
[0016] When the raw gas contains CO in addition to H2O, the hydrogen electrode 6 converts the raw gas into H2, CO, and O2 in accordance with the electrochemical reactions of co-electrolysis shown in the following formulas (2), (3), and (4). 2- Generate. Hydrogen electrode 6: CO2+H2O+4e - →CO+H2+2O 2- (2) Electrochemical reaction of H2O: H2O+2e - →H2+O 2- (3) Electrochemical reaction of CO2: CO2+2e - →CO+O 2- (4)
[0017] The hydrogen electrode layer 6 is made of a porous material having electronic conductivity. The hydrogen electrode layer 6 may have oxide ion conductivity. The hydrogen electrode layer 6 may be made of, for example, 8 mol% yttria-stabilized zirconia (8YSZ), calcia-stabilized zirconia (CSZ), scandia-stabilized zirconia (ScSZ), gadolinium-doped ceria (GDC), samarium-doped ceria (SDC), (La,Sr)(Cr,Mn)O3, (La,Sr)TiO3, Sr2(Fe,Mo)2O6, (La,Sr)VO3, (La,Sr)FeO3, a mixed material of two or more of these, or a composite of one or more of these and NiO.
[0018] The porosity of the hydrogen electrode layer 6 is not particularly limited, but may be, for example, 5% to 70%. The thickness of the hydrogen electrode layer 6 is not particularly limited, but may be, for example, 1 μm to 100 μm.
[0019] The method for forming the hydrogen electrode layer 6 is not particularly limited, and may be a firing method, a spray coating method (such as a thermal spray method, an aerosol deposition method, an aerosol gas deposition method, a powder jet deposition method, a particle jet deposition method, or a cold spray method), a PVD method (such as a sputtering method or a pulsed laser deposition method), or a CVD method.
[0020] [Electrolyte layer 7] The electrolyte layer 7 is disposed between the hydrogen electrode layer 6 and the oxygen electrode layer 9. The electrolyte layer 7 covers the entire hydrogen electrode layer 6. In this embodiment, the electrolyte layer 7 is disposed between the hydrogen electrode layer 6 and the reaction prevention layer 8, and is connected to both the hydrogen electrode layer 6 and the reaction prevention layer 8.
[0021] The outer periphery of the electrolyte layer 7 is joined to the first main surface 20S of the metal support 20. This ensures airtightness between the hydrogen electrode layer 6 side and the oxygen electrode layer 9 side, eliminating the need to provide a separate seal between the metal support 20 and the electrolyte layer 7. The outer periphery of the electrolyte layer 7 refers to the portion of the electrolyte layer 7 that is connected to the first main surface 20S of the metal support 20.
[0022] 1, the electrolyte layer 7 has a first end 71 and a second end 72. The first and second ends 71, 72 are both ends of the electrolyte layer 7 in the short-side direction (X-axis direction). Each of the first and second ends 71, 72 extends along the long-side direction.
[0023] The first end 71 is a portion of the outer periphery of the electrolyte layer 7 that extends along the first side L1 of the first main surface 20S. The second end 72 is a portion of the outer periphery of the electrolyte layer 7 that extends along the second side L2 of the first main surface 20S. The configurations of the first and second end portions 71, 72 will be described later.
[0024] The electrolyte layer 7 is formed by discharging the O 2- to the oxygen electrode layer 9. The electrolyte layer 7 is made of a dense material having oxide ion conductivity. The electrolyte layer 7 can be made of, for example, 8YSZ, LSGM (lanthanum gallate), GDC (gadolinium-doped ceria), or the like.
[0025] The electrolyte layer 7 is made of a dense material that has ion conductivity but does not have electronic conductivity. The electrolyte layer 7 can be made of, for example, YSZ (8YSZ), GDC, ScSZ, SDC, LSGM (lanthanum gallate), or the like.
[0026] The porosity of the electrolyte layer 7 is not particularly limited, but may be, for example, 0.1% to 7%. The thickness of the electrolyte layer 7 is not particularly limited, but may be, for example, 1 μm to 100 μm.
[0027] The method for forming the electrolyte layer 7 is not particularly limited, and a baking method, a spray coating method, a PVD method, a CVD method, or the like can be used.
[0028] [Reaction prevention layer 8] The reaction prevention layer 8 is disposed between the electrolyte layer 7 and the oxygen electrode layer 9. The reaction prevention layer 8 is disposed on the opposite side of the hydrogen electrode layer 6 with the electrolyte layer 7 interposed therebetween. In this embodiment, the reaction prevention layer 8 is connected to the electrolyte layer 7. The reaction prevention layer 8 has a function of suppressing the formation of a reaction layer with high electrical resistance due to a reaction between the electrolyte layer 7 and the oxygen electrode layer 9.
[0029] The reaction prevention layer 8 is made of an oxide ion conductive material, and may be made of GDC, SDC, or the like.
[0030] The porosity of the reaction prevention layer 8 is not particularly limited, but may be, for example, 0.1% to 50%. The thickness of the reaction prevention layer 8 is not particularly limited, but may be, for example, 1 μm to 50 μm.
[0031] The method for forming the reaction prevention layer 8 is not particularly limited, and a baking method, a spray coating method, a PVD method, a CVD method, or the like can be used.
[0032] [Oxygen electrode layer 9] The oxygen electrode layer 9 is disposed on the opposite side of the hydrogen electrode layer 6 with respect to the electrolyte layer 7. In this embodiment, since the electrolytic cell 1 includes the reaction prevention layer 8, the oxygen electrode layer 9 is connected to the reaction prevention layer 8. If the electrolytic cell 1 does not include the reaction prevention layer 8, the oxygen electrode layer 9 is connected onto the electrolyte layer 7. The oxygen electrode layer 9 is an example of a "second electrode layer" according to the present invention.
[0033] The oxygen electrode layer 9 reacts with O 2 transferred from the hydrogen electrode layer 6 through the electrolyte layer 7 in accordance with the chemical reaction of the following formula (2): 2- produces O2 from Oxygen electrode layer 9:2O 2- →O2+4e - (2)
[0034] The oxygen electrode layer 9 is made of a porous material having oxide ion conductivity and electron conductivity. The oxygen electrode layer 9 can be made of a compound of one or more of (La,Sr)(Co,Fe)O3, (La,Sr)FeO3, La(Ni,Fe)O3, (La,Sr)CoO3, and (Sm,Sr)CoO3 with an oxide ion conductive material (such as GDC).
[0035] The porosity of the oxygen electrode layer 9 is not particularly limited, but may be, for example, 20% to 60%. The thickness of the oxygen electrode layer 9 is not particularly limited, but may be, for example, 1 μm to 100 μm.
[0036] The method for forming the oxygen electrode layer 9 is not particularly limited, and a baking method, a spray coating method, a PVD method, a CVD method, or the like can be used.
[0037] [Metal support 20] The metal support 20 supports the cell main body 10. The metal support 20 is formed in a plate shape. The metal support 20 may be in a flat plate shape or a curved plate shape. The metal support 20 may have any thickness as long as it can maintain the strength of the electrolysis cell 1, and the thickness is not particularly limited, but may be, for example, 0.1 mm or more and 2.0 mm or less.
[0038] The metal support 20 has a plurality of supply holes 21, a first main surface 20S, and a second main surface 20T. The first main surface 20S is an example of the "main surface" according to the present invention.
[0039] Each supply hole 21 penetrates the metal support 20 from the first main surface 20S to the second main surface 20T. Each supply hole 21 opens to the first main surface 20S and the second main surface 20T. Each supply hole 21 is formed in a region of the first main surface 20S that is joined to the hydrogen electrode layer 6. Each supply hole 21 is connected to a flow path 30a formed between the metal support 20 and the flow path member 30.
[0040] Each supply hole 21 can be formed by mechanical processing (e.g., punching), laser processing, chemical processing (e.g., etching), or the like. Alternatively, when the metal support 20 is made of a porous metal, each supply hole 21 may be an air hole in the porous metal. Therefore, each supply hole 21 does not need to be formed perpendicular to the first main surface 20S and the second main surface 20T.
[0041] The cell main body 10 is joined to the first main surface 20S. The flow path member 30 is joined to the second main surface 20T. The first main surface 20S is provided on the opposite side to the second main surface 20T.
[0042] 1 shows four sides that define the first main surface 20S. The first main surface 20S is defined by a first side L1, a second side L2, a third side L3, and a fourth side L4. The first main surface 20S is a region of the outer surface of the metal support 20 that is surrounded by the first side L1, the second side L2, the third side L3, and the fourth side L4.
[0043] The planar shape of the first main surface 20S is a rectangle extending in the longitudinal direction. The first side L1 and the second side L2 are parallel to each other. The first and second sides L1 and L2 are the long sides of the first main surface 20S. The first and second sides L1 and L2 are parallel to the longitudinal direction. The third side L3 and the fourth side L4 are parallel to each other. The third and fourth sides L3 and L4 are the short sides of the first main surface 20S. The third and fourth sides L3 and L4 are parallel to the short direction. In this specification, the term "parallel" refers not only to the case where the sides are parallel in the strict sense, but also to the case where the sides can be said to be substantially parallel (with an inclination of 10 degrees or less).
[0044] The metal support 20 is made of a metal material. For example, the metal support 20 is made of an alloy material containing Cr (chromium). Examples of such metal materials include Fe-Cr alloy steel (stainless steel, etc.) and Ni-Cr alloy steel. The Cr content in the metal support 20 is not particularly limited, but may be 4% by mass or more and 30% by mass or less.
[0045] The metal support 20 may contain Ti (titanium) and / or Zr (zirconium). The Ti content in the metal support 20 is not particularly limited, but may be 0.01 mol% or more and 1.0 mol% or less. The Zr content in the metal support 20 is not particularly limited, but may be 0.01 mol% or more and 0.4 mol% or less. The metal support 20 may contain Ti as TiO2 (titania) or Zr as ZrO2 (zirconia).
[0046] The metal support 20 may have an oxide film on its surface, which is formed by oxidation of the constituent elements of the metal support 20. A typical example of the oxide film is a chromium oxide film. The oxide film covers the surface of the metal support 20 partially or entirely. The oxide film may also cover the inner wall surface of each supply hole 21 partially or entirely.
[0047] [Flow path member 30] The flow path member 30 is joined to the second main surface 20T of the metal support 20. A flow path 30a is formed between the flow path member 30 and the metal support 20. A source gas is supplied to the flow path 30a. The source gas supplied to the flow path 30a is supplied to the hydrogen electrode layer 6 of the cell main body 10 through each supply hole 21 of the metal support 20.
[0048] The flow path member 30 can be made of, for example, an alloy material. The flow path member 30 may be formed of the same material as the metal support 20. In this case, the flow path member 30 may be substantially integral with the metal support 20.
[0049] The flow path member 30 has a frame 31 and an interconnector 32. The frame 31 is an annular member that surrounds the side of the flow path 30a. The frame 31 is joined to the second main surface 20T of the metal support 20. The interconnector 32 is a plate-like member for electrically connecting the electrolysis cell 1 to an external power source or another electrolysis cell in series. The interconnector 32 is joined to the frame 31.
[0050] Thus, in the flow path member 30 according to this embodiment, the frame 31 and the interconnector 32 are separate members, but the frame 31 and the interconnector 32 may be integral with each other.
[0051] [Configuration of first end portion 71 of electrolyte layer 7] Next, a configuration of the first end portion 71 of the electrolyte layer 7 will be described. FIG 3 is a partially enlarged view of FIG.
[0052] 3, the first end 71 is connected to the first main surface 20S of the metal support 20. The first end 71 covers the first side L1 of the first main surface 20S. In other words, the first end 71 covers the area of the first main surface 20S that is exposed from the hydrogen electrode layer 6 all the way to the end. This makes it possible to suppress heat radiation from the metal support 20, thereby improving the heat retention of the electrolysis cell 1.
[0053] 3, the first end 71 becomes thinner as it approaches the first side L1 in the short side direction parallel to the first main surface 20S. In detail, the first end 71 has a tip 71a that covers the first side L1, and the thickness of the tip 71a gradually decreases as it approaches the first side L1 in the short side direction. This makes it possible to prevent damage (such as corner breaks and cracks) from occurring on the outer edge of the tip 71a.
[0054] Here, the electrolysis cell 1, which has a rectangular planar shape, thermally expands and contracts more in the longitudinal direction than in the lateral direction. Therefore, the portion of the outer periphery of the electrolyte layer 7 along the longitudinal direction is more likely to be subjected to a large thermal stress than the portion along the lateral direction. Therefore, by making the thickness of the first end 71 thinner toward the first side L1, the portion of the electrolyte layer 7 that is particularly susceptible to damage can be effectively protected.
[0055] The tip portion 71a is a portion of the electrolyte layer 7 between the first reference line P1 and the second reference line P2. The first reference line P1 is a straight line that passes through the first side L1 and is perpendicular to the first main surface 20S. The second reference line P2 is a straight line that is located 4 μm inward from the first reference line P1 and is parallel to the first reference line P1.
[0056] The thickness of the tip portion 71a means the height of the tip portion 71a in the direction perpendicular to the first main surface 20S (Z-axis direction). The thickness of the tip portion 71a is maximum at the position where it intersects with the second reference line P2 and is minimum at the position where it intersects with the first reference line P1. The thickness of the tip portion 71a may be continuously smaller as it approaches the first side L1, or may be gradually smaller as it approaches the first side L1.
[0057] Therefore, in FIG. 3, the outer surface of the tip portion 71a is convexly curved toward the side opposite the first main surface 20S, but it may be convexly curved toward the first main surface 20S side, may be straight, or may be curved in whole or in part.
[0058] As long as the thickness of the tip 71a gradually decreases toward the first side L1, the thickness of the portion of the first end 71 other than the tip 71a is not particularly limited. The thickness of the portion other than the tip 71a may be substantially uniform, may decrease toward the tip 71a, or may increase toward the tip 71a.
[0059] As described above, in the cross section shown in Fig. 3, the thickness of the tip portion 71a gradually decreases toward the first side L1. The configuration shown in Fig. 3 is preferably observed in all cross sections of the tip portion 71a, but it is sufficient if it is observed in at least one cross section of the tip portion 71a. If the configuration shown in Fig. 3 is observed in even one cross section, it is possible to improve the heat retention of the electrolysis cell 1 at least in that portion and to suppress damage to the outer edge of that portion.
[0060] [Configuration of second end portion 72 of electrolyte layer 7] Next, the configuration of the second end portion 72 of the electrolyte layer 7 will be described. FIG 4 is a partially enlarged view of FIG.
[0061] 4, the second end 72 is connected to the first main surface 20S of the metal support 20. The second end 72 covers the second side L2 of the first main surface 20S. In other words, the second end 72 covers the region of the first main surface 20S that is exposed from the hydrogen electrode layer 6 all the way to the end. This makes it possible to suppress heat radiation from the metal support 20, thereby improving the heat retention of the electrolysis cell 1.
[0062] As shown in FIG. 4, the second end 72 becomes thinner toward the second side L2 in the short-side direction parallel to the first main surface 20S. In detail, the second end 72 has a tip 72a covering the second side L2, and the thickness of the tip 72a becomes gradually smaller toward the second side L2 in the short-side direction. This can prevent damage (corner breaks, cracks, etc.) from occurring on the outer edge of the tip 72a. Similar to the first end 71 described above, the second end 72 is prone to large thermal stress, so by making the thickness of the second end 72 thinner toward the second side L2, the part of the electrolyte layer 7 that is particularly prone to damage can be effectively protected.
[0063] The tip portion 72a is a portion of the electrolyte layer 7 between the third reference line P3 and the fourth reference line P4. The third reference line P3 is a straight line that passes through the second side L2 and is perpendicular to the first main surface 20S. The fourth reference line P4 is located 4 μm inward from the third reference line P3 and is a straight line that is parallel to the third reference line P3.
[0064] The thickness of the tip portion 72a means the height of the tip portion 72a in a direction perpendicular to the first main surface 20S. The thickness of the tip portion 72a is maximum at the position where it intersects with the fourth reference line P4 and is minimum at the position where it intersects with the third reference line P3. The thickness of the tip portion 72a may be continuously smaller as it approaches the second side L2, or may be gradually smaller as it approaches the second side L2.
[0065] Therefore, in FIG. 4, the outer surface of the tip portion 72a is convexly curved toward the side opposite the first main surface 20S, but it may be convexly curved toward the first main surface 20S side, may be straight, or may be curved in whole or in part.
[0066] As long as the thickness of the tip 72a gradually decreases toward the second side L2, the thickness of the portion of the second end 72 other than the tip 72a is not particularly limited. The thickness of the portion other than the tip 72a may be substantially uniform, may decrease toward the tip 72a, or may increase toward the tip 72a.
[0067] As described above, in the cross section shown in Fig. 4, the thickness of the tip portion 72a gradually decreases toward the second side L2. The configuration shown in Fig. 4 is preferably observed in all cross sections of the tip portion 72a, but it is sufficient if it is observed in at least one cross section of the tip portion 72a. If the configuration shown in Fig. 4 is observed in even one cross section, it is possible to improve the heat retention of the electrolysis cell 1 at least in that portion and to suppress damage to the outer edge of that portion.
[0068] (Modification of the embodiment) Although the embodiments of the present invention have been described above, the present invention is not limited to these, and various modifications are possible without departing from the spirit of the present invention.
[0069] [Variation 1] In the above embodiment, the electrolysis cell 1 is formed into a rectangle extending in the longitudinal direction in a plan view, but is not limited thereto. The electrolysis cell 1 may be formed into a square shape in a plan view, or may be formed into a rectangle extending in the lateral direction in a plan view.
[0070] [Variation 2] In the above embodiment, the planar shape of the first main surface 20S of the metal support 20 is a rectangle extending in the longitudinal direction, but is not limited thereto. The planar shape of the first main surface 20S of the metal support 20 may be a square or a rectangle extending in the lateral direction.
[0071] [Variation 3] Third and fourth ends 73, 74 (see FIG. 1 ) extending along the short side direction of the outer periphery of the electrolyte layer 7 may have the same configuration as the first and second ends 71, 72, or may have a different configuration from the first and second ends 71, 72. When the third and fourth ends 73, 74 have the same configuration as the first and second ends 71, 72, respectively, the heat retention of the electrolysis cell 1 can be further improved and damage to the outer edge of the electrolyte layer 7 can be further suppressed.
[0072] [Variation 4] 5, the first end 71 of the electrolyte layer 7 may have a protruding portion 71b. The protruding portion 71b is a portion of the first end 71 that protrudes outward from the first main surface 20S of the metal support 20. In other words, the protruding portion 71b is a portion of the first end 71 that is located outward from the first reference line P1 (opposite the second reference line P2). The protruding portion 71b is continuous with the tip portion 71a. The protruding portion 71b is integral with the tip portion 71a.
[0073] 5, the protrusion 71b preferably covers at least a part of the side surface 20U of the metal support 20. This allows the side surface 20U to be covered by the protrusion 71b, thereby further suppressing heat radiation from the metal support 20.
[0074] Even if the first end 71 has the protruding portion 71b, the tip 71a of the first end 71 is defined by the first and second reference lines P1, P2. Although not shown, the second end 72 of the electrolyte layer 7 may also have a protruding portion.
[0075] [Variation 5] In the above embodiment, the hydrogen electrode layer 6 functions as a cathode and the oxygen electrode layer 9 functions as an anode, but the hydrogen electrode layer 6 may function as an anode and the oxygen electrode layer 9 may function as a cathode. In this case, the constituent materials of the hydrogen electrode layer 6 and the oxygen electrode layer 9 are switched, and a source gas is passed over the outer surface of the hydrogen electrode layer 6.
[0076] [Variation 6] In the above embodiment, the electrolysis cell 1 has been described as an example of an electrochemical cell, but the electrochemical cell is not limited to the electrolysis cell. An electrochemical cell is a general term for an element in which a pair of electrodes are arranged so that an electromotive force is generated from an overall oxidation-reduction reaction in order to convert electrical energy into chemical energy, and an element for converting chemical energy into electrical energy. Therefore, the electrochemical cell includes, for example, a fuel cell that uses oxide ions or protons as a carrier. [Explanation of symbols]
[0077] 1 cell 6 Hydrogen electrode layer 7 Electrolyte layer 71 First end 71a Tip 71b Protrusion 72 Second end 72a Tip 73 Third end 74 4th end 8. Reaction prevention layer 9 Oxygen Polar Layer 10 Cell body 20 Metal support 20S 1st main surface 21 Supply hole 30 Flow path member 30a Flow path L1~L4 1st to 4th sides P1~P4 1st to 4th reference line
Claims
1. a cell body having a first electrode layer, a second electrode layer, and an electrolyte layer disposed between the first electrode layer and the second electrode layer; a metal support having a main surface for supporting the cell body and a plurality of supply holes; Equipped with the electrolyte layer has a first end covering a first side of the main surface, In a cross section of the electrolyte layer perpendicular to the main surface, the first end includes a tip portion that is disposed between a first reference line and a second reference line, the first reference line is a straight line that passes through the first side and is perpendicular to the main surface, The second reference line is located 4 μm inward from the first reference line and is a straight line parallel to the first reference line, The tip of the first end portion becomes thinner as it approaches the first side in a direction parallel to the main surface. Electrochemical cell.
2. the electrolyte layer has a second end covering a second side of the main surface, The second side is parallel to the first side, In a cross section of the electrolyte layer perpendicular to the main surface, the second end includes a tip portion that is disposed between a third reference line and a fourth reference line, the third reference line is a straight line that passes through the second side and is perpendicular to the main surface, The fourth reference line is located 4 μm inward from the third reference line and is a straight line parallel to the third reference line, The tip of the second end portion becomes thinner toward the second side in a direction parallel to the main surface.
10. The electrochemical cell of claim 1.
3. The main surface is formed in a rectangular shape, Each of the first side and the second side is a long side of the main surface.
3. The electrochemical cell of claim 2.
4. the electrolyte layer has a protruding portion protruding outward from the main surface, The protrusion covers at least a portion of a side surface of the metal support.
4. An electrochemical cell according to claim 1.
Citation Information
Patent Citations
Fuel cell and method of manufacturing same
JP2007172848A
Reaction cell, its production method, and reaction system
JP2009041044A
Electrochemical cell
JP2020155337A
Solid oxide electrochemical stack
JP2021111473A
Cell, cell stack device, module, and module accommodation device
WO2020218334A1